Glass recycling process
By bonding non-breakable components to the glazing surface before breaking and separating glued pieces, the recycling process effectively addresses the challenge of recycling glass with non-glass components, ensuring efficient and cost-effective separation of glass and non-glass materials.
Patent Information
- Application Number
- FR2023004299
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-28
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2043-04-28
AI Technical Summary
The recycling of glass objects containing non-glass components, such as defrosting resistors in automobile glazing, is challenging due to the risk of the metallic materials melting and altering the glass composition or tin bath, and conventional separation processes are inefficient and costly.
A glass recycling process involving a preliminary step of bonding non-breakable components to the glazing surface, followed by breaking and separating the glued pieces from unglued pieces, allowing for easy segregation of glass and non-glass materials.
Enables efficient and cost-effective recycling of glass substrates with non-glass components by facilitating the separation of glass and non-glass materials, preserving the chemical composition of the recycled glass.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Title of the invention: Method for recycling glazing Field of invention
[0001] The present invention relates to the recycling of flat glass glazing.
[0002] In particular, the invention relates to the recycling of glazing composed of a glass substrate on which a component made of non-glass material is assembled. Prior art
[0003] Glass is generally manufactured by melting raw materials including silica. It is also possible to make it by melting pieces of recycled glass. This process using recycled glass requires less energy to produce the same quantity of glass than the process requiring the melting of raw materials and their transformation to form the desired glass composition. Manufacturing glass from recycled glass is therefore particularly advantageous and has a lower CO2 impact.
[0004] To manufacture glass from recycled glass, it is necessary to have recycled glass having the desired chemical composition for the glass to be manufactured. A particular difficulty arises for the recycling of objects composed of both glass and components made of a material that is not glass. If these components are infusible, they may float on the molten glass, and will have to be removed. If, on the other hand, these components are fusible at the melting temperature of the glass, they risk melting at the same time as the recycled glass and mixing with it, changing its chemical composition, or even interacting chemically with the molten glass or the tin bath. It is therefore generally not desirable to recycle such objects composed of both glass and fusible non-glass components.
[0005] Such a difficulty may arise in particular for the recycling of automotive glazing, and in particular vehicle rear windows. Vehicle rear windows in fact most often comprise a defrosting resistor formed of electrically conductive tracks, deposited on one face of a glass substrate of the rear window. These tracks are often formed by an electrically conductive silver paste, which is deposited by screen printing on the glass substrate and solidified by baking at high temperature. When the vehicle is in use, these tracks may be crossed by an electric current in order to heat up to allow the rear window to be demisted or defrosted.Typically, on a rear window, the defrosting resistor is made up of thin tracks offering high electrical resistance, allowing the rear window to be defrosted or demisted, and thick tracks, offering lower electrical resistance, which ensure the connection. electric thin tracks.
[0006] Such defrosting resistors can also be provided on the windshields of vehicles or even, in certain cases, on the side windows of vehicles.
[0007] The recycling of such vehicle glazing poses a problem, the metallic material contained in the defrosting resistor being liable to melt with the recycled glass, modifying its composition in an unacceptable way or altering the properties of the tin bath.
[0008] To enable, however, the recycling of glass substrates of vehicle rear windows, documents US20200165697A1, WO2009087908A1, US2022228235 and WO2020240126 are known, for example, describing chemical processes for dissociating a metal component from the glass with which it is associated. However, it is not very effective to subject the entire rear window glazing to such a separation process.
[0009] It is also known to sort pieces of glass, depending on whether or not they are associated with components made of non-glass material. Such sorting is however complicated and expensive.
[0010] The present invention aims to overcome these drawbacks of the prior art.
[0011] In particular, the invention aims to provide a glass recycling method allowing optimized recycling of flat glass glazing composed of a glass substrate on which a component made of non-glass material is assembled.
[0012] A particular objective of the invention is to enable the optimized recycling of automotive glazing, and in particular of motor vehicle rear windows equipped with defrosting resistors comprising metallic materials.
[0013] Yet another objective of the invention is to propose such a recycling process which makes it possible to obtain recycled glass, which has chemical characteristics as close as possible to those desired.
[0014] Yet another objective of the invention is to provide such a recycling method which is easy to implement. Statement of the invention
[0015] These objectives, as well as others which will become more clearly apparent hereinafter, are achieved using a method for recycling a glazing unit comprising a glass substrate and at least one component made of non-glass material secured to the glass substrate, this method comprising a step of breaking the glazing unit, followed by a step of separating the pieces of glazing unit, to separate the pieces of glazing secured to a substantial quantity of the non-glass material, from the pieces of glazing unit which are not secured to a substantial quantity of the non-glass material. According to the invention, this method comprises a preliminary step, before the step of breaking the glazing unit, of bonding on a part of the surface of the glazing of at least one non-breakable component, at the level of at least one zone of the glazing on which at least one of the components made of non-glass material is secured, and the separation step comprises the separation of the non-breakable components, with the pieces of glazing which are stuck there, from the other pieces of glazing which are not stuck to the non-breakable component.
[0016] Advantageously, the glazing is automotive glazing.
[0017] Advantageously, the glazing is a rear window of a motor vehicle, comprising a defrosting resistor constituting one of the components made of non-glass material.
[0018] According to an advantageous embodiment, the component made of non-glass material is a component screen-printed on the glass substrate, to form said glazing.
[0019] Preferably, the non-glass component comprises a metal alloy screen-printed onto the glass substrate.
[0020] According to an advantageous embodiment, the non-breakable component is a flexible adhesive film.
[0021] Preferably, this flexible adhesive film is made of plastic material.
[0022] According to a preferred embodiment, the non-breakable component is bonded to a face of said glass substrate on which the component made of non-glass material is secured.
[0023] According to another possible embodiment, one of the non-breakable components is bonded to each of the two opposite faces of the glass substrate, at least one of the areas of the glazing on which at least one of the components made of non-glass material is secured. Description of figures
[0024] The invention will be better understood on reading the following description of preferred embodiments, given as a simple figurative and non-limiting example, and accompanied by the figures among which: - [Fig.l] represents a glazing constituting a rear window of a motor vehicle. - [Fig.2] represents the glazing of [Fig.l], after it has been broken. - [Fig.3] represents the glazing of [Fig.l] on which have been stuck non-breakable adhesive components, according to one embodiment of the method of the invention. - [Fig.4] shows the glazing of [Fig.3], to which the non-breakable adhesive components have been bonded, after it has been broken. - [Fig.5] shows the non-breakable adhesive components and the fragments of the glazing in [Fig.4] that adhere to them. - [Fig.6] is a graph showing the steps of a recycling process according to one embodiment of the invention. Description of the embodiments
[0025] [Fig.l] represents, in front view, a glazing 1 constituting a rear window of a motor vehicle.
[0026] Motor vehicle glazings, such as windshields or rear windows of a motor vehicle, may consist of several glass substrates superimposed on each other, between which layers of non-glass materials, such as plastic materials, may be interposed. The term "glazing" used in the present description preferably applies to a single glass substrate. However, it may also apply to a composite assembly comprising several superimposed glass substrates.
[0027] The glazing 1 is formed from a glass substrate 10, onto which components made of non-glass material are secured.
[0028] A glass substrate, within the meaning of the present description, is a flat glass plate, made of a glass material, that is to say a non-crystalline solid material exhibiting the glass transition phenomenon. Preferably, this glass substrate is transparent, that is to say it allows specular transmission of radiation at least in the wavelength ranges useful for the intended application of the element. In this case, the glass substrates used as glazing for motor vehicles are normally transparent at least in the visible wavelength range. The glass substrate may also be covered by components such as enamels, which may themselves be made of a glass material which does not prevent the recycling of the glass substrate.
[0029] Components made of non-glass material, within the meaning of the present description, are components which are not formed mainly or essentially of a glass material, which can be secured to a glass substrate.
[0030] The glass substrate may, in a known manner, be covered on one of its faces or on both of its faces with a thin coating layer. Such a coating, which may be made of a non-glass material, generally has a very thin thickness, and its mass therefore forms only a tiny proportion of the total mass of the glazing. The small proportion of non-glass material that such a coating brings into a glazing is generally not considered to constitute an obstacle to the recycling of this glazing.
[0031] In the embodiment shown, components made of non-glass material constitute a defrosting resistor 2, formed of electrically conductive tracks, deposited on one face of the glass substrate. These tracks are formed by a electrically conductive material, which is deposited for example by screen printing on the glass substrate and solidified and bonded to the glass substrate by high temperature firing.
[0032] The mass of such a non-glass component remains low, in comparison with the total mass of the glazing. It is however sufficiently significant to affect the recycling conditions of this glazing. For example, it may be considered that a glazing comprising a glass substrate and a non-glass component comprises a significant quantity of non-glass material when the mass of this non-glass component represents more than 200 ppm (parts per million) of the total mass of the glazing. Such a definition is however only indicative, and may vary, for example, depending on the recycling process implemented.
[0033] The electrically conductive material used in the defrosting resistor 2 may be an at least partially metallic alloy which, in the embodiment shown, comprises a mixture of at least 80% silver and a glass frit, which facilitates its adhesion to the glass substrate. This coating thus has a high hardness and cannot be easily removed from the glass substrate.
[0034] Conventionally, the defrosting resistor 2 of the glazing 1 is composed of thin tracks offering a high electrical resistance, and thick tracks, offering a lower electrical resistance. The thick tracks form the lateral collectors 21, 22 and 23, placed along two lateral edges of the glass substrate. The lateral collector 21 being located along one of the edges, is connected to the lateral collectors 22 and 23, located along the other edge, by a plurality of thin tracks forming the heating wires 24.
[0035] The lateral collectors 21, 22 and 23 are intended to ensure efficient conduction of the electric current, without opposing any significant resistance. These collectors therefore have large dimensions, using a relatively large quantity of non-glass material.
[0036] On the contrary, the heating wires 24 are intended to heat up when an electric current passes through them. They must therefore offer a high resistance and consequently have a very small cross-section. These heating wires 24 are therefore formed by a very small quantity of non-glass material.
[0037] A large part of the non-glass material used to form the defrosting resistor 2 is therefore placed in the collectors 21, 22 and 23. Although the heating wires 24 cover a larger surface area of the glazing 1, the mass of non-glass material that they use is, on the contrary, relatively low.
[0038] To recycle the glazing 1, it is necessary to break it to melt the pieces. [Fig.2] thus represents the glazing 1 of [Fig.l] broken into pieces 100. Among these pieces 100, the vast majority is made up solely of glass material, or has only a very small proportion of non-glass material associated with the glass material. on the contrary, the pieces 100 corresponding to the parts of the glazing 1 comprising the collectors 21, 22 and 23 have a more significant proportion of non-glass material.
[0039] Processing all of the pieces of glass 100 to separate the non-glass material from the glass material would be inefficient. Efficient recycling of the glass would require separating the pieces 100 comprising exclusively or almost exclusively glass material, which can be recycled directly, from the pieces 100 comprising a significant portion of non-glass material, which can undergo processing to separate the glass material from the non-glass material. Such sorting of the pieces 100 is, however, very complicated and expensive.
[0040] To facilitate the separation of pieces of glass 100 composed exclusively or almost exclusively of glass material from pieces 100 comprising a significant portion of non-glass materials, the invention proposes a particular method for recycling glass.
[0041] According to the invention, the method for recycling glass comprises, before a step 92 of breaking the glazing, a prior step 91 of bonding non-breakable components to a portion of the surface of this glazing. A non-breakable component, within the meaning of the present description, is a component that can be secured to a glazing and does not break when the glazing is broken. Such a non-breakable component may be a rigid component, for example metallic, having mechanical characteristics that prevent it from breaking under the effect of an impact breaking the glazing. It may also be made of a flexible material, such as a plastic film, capable of deforming without breaking under the effect of an impact breaking the glazing.
[0042] According to still other possible embodiments of the invention, the bonding of non-breakable component on a part of the surface of the glazing can be done by depositing, on a part of the surface of this glazing, a liquid component solidifying after its deposition, such as for example an organic resin or a plastic coating. This liquid component constitutes a non-breakable component within the meaning of the present invention if, after its solidification and after the breaking of the glazing, it is capable of retaining the shards of the glazing to which it is secured.
[0043] According to the invention, the non-breakable component is only bonded to a portion of the surface of the glazing, in order to allow separate recycling of the portions of the glazing bonded to a non-breakable component and the portions of the glazing which are not bonded to a non-breakable component. It is particularly advantageous for the non-breakable component(s) to be bonded only to a portion of the surface of a face of the glazing less than 50% of the total surface of the face of this glazing, and even preferably less than 10% of the total surface of the face of this glazing.
[0044] [Fig. 3] represents the glazing 1 on which such components made of non-material breakable have been applied. In this case, these components made of non-breakable material consist of portions of adhesive film 31 and 32, such as adhesive tape, which are glued to one face of the glazing 1, at the collectors 21, 22 and 23.
[0045] More precisely, a portion of adhesive film 31 is glued to one face of the glazing 1, to an area of this glazing 1 on which the collector 21 is secured, and a portion of adhesive film 32 is placed on one face of the glazing 1, to an area of this glazing 1 on which the collectors 22 and 23 are secured. These portions of adhesive film 31 and 32, constituting non-breakable components, therefore cover the areas of the glazing 1 on which significant quantities of non-glass material are secured.
[0046] In the embodiment shown, it has in fact been chosen to only bond the components made of non-breakable material to the areas of the glazing 1 on which the collectors 21, 22 and 23 are secured, which concentrate a large part of the non-glass materials of the glazing 1, and not to bond them to the heating wires 24. It would also be possible, in a variant of this embodiment, to bond components made of non-breakable material to all the areas of the glazing 1 at which the non-glass components are secured, that is to say to the areas of this glazing 1 on which the collectors 21, 22 and 23 are secured as well as to the areas of this glazing 1 on which the heating wires 24 are secured.
[0047] The non-breakable components may, according to the invention, be bonded to one or other of the faces of the glazing 1, or to both faces, on the portions of this glazing which comprise non-glass components in significant quantity. In the preferred embodiment shown, however, the portions of adhesive film 31 and 32 constituting the non-breakable components are bonded to the face of the glazing 1 which comprises the deposits of non-glass material. The choice of bonding the non-breakable components to this face in fact makes it possible to delimit as precisely as possible the outline of the areas of the glazing which comprise non-glass components in significant quantity, on which to bond the non-breakable component.
[0048] Following step 91 of bonding non-breakable components to the glazing 1, the recycling method according to the invention comprises a step 92 of breaking the glazing. The glazing 1 can thus be reduced to pieces 100, as shown in [Fig. 4]. This breaking of the glazing does not result in breakage or separation of the non-breakable components formed by the portions of adhesive film 31 and 32, which remain associated with the pieces of glazing to which they were bonded.
[0049] After this step 92 of breaking the glazing 1, the method according to the invention implements a step 93 of separating the pieces 100 of the glazing 1 associated with the non-breakable components, on the one hand, and the pieces 100 of the glazing 1 which are not associated with the non-breakable components, on the other hand.
[0050] Such a separation can be done very easily. It can for example be done by removal of the non-breakable materials, taking with them the pieces of glass 100 associated with them. It is thus possible, on the broken glazing 1 shown in [Fig.4], to remove the portions of adhesive film 31 and 32, taking with them the pieces of glass 100 which are stuck to them.
[0051] According to another possible embodiment, this separation step 93 can also be implemented by sieving the pieces of glass 100. The pieces 100 which are not associated with non-breakable components then pass through the meshes of the sieve, while the non-breakable components, as well as the pieces which are stuck thereto, do not pass through these meshes.
[0052] [Fig. 5] thus shows the portions of adhesive film 31 and 32, constituting non-breakable components, glued to the pieces 100 of the portion of the glazing 1 on which they were glued. These pieces 100 are advantageously those which carry the portions of the collectors 21, 22 and 23, comprising a significant portion of non-glass material.
[0053] These pieces 100 bonded to the non-breakable components can undergo specific recycling, during a reuse step 94. They can for example be melted to form a glass material whose composition can include the non-glass material. Alternatively, they can undergo recycling steps aimed at separating the glass material from the non-glass material, to recycle them separately.
[0054] On the contrary, the pieces of the glazing 1 which are not stuck to these portions of adhesive film 31 and 32 do not comprise any non-glass material, or only comprise a small part thereof, corresponding in particular to portions of the heating wires 24. These materials can advantageously be recycled like glass not comprising any non-glass material, during a reuse step 95.
[0055] The separation of the pieces 100 of the glazing, within the meaning of the present invention, does not necessarily allow all of the pieces of the glazing which are bonded to the non-breakable material to be associated with non-glass materials, nor that all of the pieces of the glazing which are not bonded to the non-breakable material are free of non-glass materials. However, it allows, in a very easy manner, to concentrate the pieces of the glazing which are associated with the largest quantities of non-glass material.
[0056] Thus, by way of example, the inventors applied a recycling method according to one embodiment of the invention to a rear window of a motor vehicle which is composed of a glass substrate on which is secured a defrosting resistor composed of a silver alloy. The glass substrate has a mass of approximately 5 kg. The defrosting resistor is formed of a silver alloy weighing approximately 1.3 g distributed between the lateral collectors and the heating wires. The silver alloy therefore represents approximately 0.0265% of the mass of the glazing, or 265 ppm (parts per million).
[0057] The application to this rear window of the recycling process described by the figures, according to which components made of non-breakable material are only glued to the areas of the glazing on which the collectors are secured, makes it possible to easily separate the pieces of this glazing between a first part, weighing approximately 4,750 g, which contains only approximately 170 ppm of silver alloy, and a second part, weighing approximately 250 g, which contains 2,000 ppm of silver alloy. These two parts can advantageously be recycled separately.
[0058] The application to this rear window of a variant of the recycling process described by the figures, according to which components made of non-breakable material are glued to all the areas of the glazing on which the collectors and the conductive wires are secured, makes it possible to easily separate the pieces of this glazing between a first part, weighing approximately 3,950 g, which does not contain any silver alloy at all, and a second part, weighing approximately 1,050 g, which contains 1,260 ppm of silver alloy. These two parts can advantageously be recycled separately.
Claims
Claims
1. Method for recycling a glazing unit (1) comprising a glass substrate (10) and at least one component made of non-glass material (2) secured to said glass substrate (10), said method comprising a step (92) of breaking said glazing unit (1), followed by a step (93) of separating the pieces of said glazing unit, to separate the pieces (100) of said glazing unit (1) secured to a substantial quantity of said non-glass material, from the pieces (100) of said glazing unit (1) which are not secured to a substantial quantity of said non-glass material, characterized in that it comprises a preliminary step (91), before the step (92) of breaking said glazing unit (1), of bonding to a portion of the surface of said glazing unit (1) at least one non-breakable component (31, 32), at at least one area of said glazing unit (1) on which at least one of said components made of non-glass material (2) is secured,and in that said separation step (93) comprises separating said non-breakable components (31, 32), with the pieces (100) of said glazing (1) which are bonded thereto, from the other pieces (100) of said glazing (1) which are not bonded to said non-breakable components (31, 32).,
2. Recycling method according to the preceding claim, characterized in that said glazing (1) is automotive glazing.
3. Recycling method according to the preceding claim, characterized in that said glazing (1) is a rear window of a motor vehicle, comprising a defrosting resistor (2) constituting one of said components made of non-glass material.
4. Recycling method according to any one of the preceding claims, characterized in that said non-glass material component (2) is a component screen-printed on said glass substrate (10), to form said glazing (1).
5. Recycling method according to any one of the preceding claims, characterized in that said non-glass component (2) comprises a metal alloy screen-printed on said glass substrate (10).
6. A recycling method according to any one of the preceding claims, characterized in that said non-breakable component (31, 32) is a flexible adhesive film.
7. Recycling method according to claim 6, characterized in that said flexible adhesive film (31, 32) is made of plastic material.
8. Recycling method according to any one of claims 1 to 6, characterized in that said non-breakable component (31, 32) is bonded to a face of said glass substrate (10) on which said component made of non-glass material (2) is secured.
9. Recycling method according to any one of claims 1 to 6, characterized in that one of said non-breakable components (31, 32) is bonded to each of the two opposite faces of said glass substrate (10), at least in one area of said glazing (1) on which at least one of said components made of non-glass material (2) is secured.
Citation Information
Patent Citations
Integrated recovery of metals from complex substrates
US20200165697A1
Method for recycling silver present on a photovoltaic cell
US20220228235A1
Method of recycling useful metal
WO2009087908A1
Method for recycling silver present on a photovoltaic cell
WO2020240126A1
Recycling insulating and / or laminated glass panels
DE4418573C1