Installation and process for preparing wood fuel material to supply, in particular, a gasification reactor
The process optimizes wood fuel preparation by mechanical reduction, slow drying, and screening to achieve uniform, low-humidity wood fuel, improving gasification efficiency and reducing health risks.
Patent Information
- Application Number
- FR2023004753
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-12
- Publication Date
- 2024-11-15
AI Technical Summary
Existing methods for preparing wood fuel pellets result in non-uniform materials with varying calorific values, leading to suboptimal gasification efficiency and high dust and fines production due to high-speed grinding, which also poses health risks.
A process involving mechanical reduction of wood waste to uniform, calibrated pieces, followed by slow drying and screening to achieve low humidity levels, combined with low-speed cutting and metal extraction to produce homogeneous, combustible material optimized for gasification.
The process produces wood fuel with low humidity and uniform dimensions, enhancing gasification efficiency and reducing health hazards by minimizing dust and fines, enabling sustained industrial production of energy-efficient fuel.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Title of the invention: Installation and a method for preparing wood fuel material to supply in particular a gasification reactor Technical field
[0001] The invention relates to a method and an installation for the preparation of combustible materials solely based on wood, the combustible material allowing in particular the feeding of a gasification reactor. The invention falls more broadly within the field of the treatment and recovery of wood waste. Prior art
[0002] Gasification is a thermochemical transformation process that lies between pyrolysis and combustion and allows carbonaceous or organic materials to be transformed into synthesis gas called "syngas" in the jargon of those skilled in the art. Syngas is a contraction of the terms "synthetic gas". Within a closed enclosure, also called a reactor, the gasification reaction brings the carbonaceous material to a temperature above 1,000°C in the presence of a gaseous reactant that can be carbon dioxide, water vapor or a mixture of oxygen and air and allows, through its combustion, to produce a combustible gas mixture that can be composed mainly of carbon monoxide (CO) and dihydrogen (H2). The syngas can then be used as a source of heat production, to operate turbines to produce electrical energy, etc.
[0003] Gasification is thus a particularly interesting recycling method for carbonaceous waste. Moreover, document US2017 / 0088783 describes a method for preparing waste comprising wood, paper, cardboard, plastics and food residues. This preparation process aims to produce granules which will then be used as fuel to supply a gasification unit. This preparation process grinds the waste to obtain a paste of combustible material which is then dried and then compacted and cut to form granules.
[0004] Grinding this type of waste mixture to create a fuel in the form of granules provides granules made up of very diverse organic materials whose calorific value is not equivalent, which can be an obstacle to optimizing the gasification reaction. In addition, the production of granules necessarily involves grinding the waste at high speed; the grinders used for this type of application generally rotate at 2000 rpm, which results in generating a lot of dust and fines. Thus, the organic fuel in the form of granules granular form which is obtained by the method described by document US2017 / 0088783 does not allow the gasification yield to be optimized.
[0005] The invention aims to overcome all of these drawbacks. Statement of the invention
[0006] The invention aims to produce a wood fuel in the form of calibrated pieces of wood free from pollutants.
[0007] The invention also aims to produce a wood fuel making it possible to optimize the gasification reaction.
[0008] The invention also aims to recover wood waste in order to produce electrical or thermal energy.
[0009] In particular, the invention aims to recover wood waste industrially.
[0010] With this in mind, the invention relates to a process for preparing wood fuel material to supply in particular a gasification reactor, the process comprising the following steps: - Provide wood waste of type B wood, - Mechanically reduce the size of wood waste so as to transform the wood waste into combustible material which includes pieces of wood with reduced dimensions, - Dry the calibrated combustible material by extracting the moisture from the heart of the small pieces of wood, - Sift the combustible material so as to eliminate pieces of wood and wood residues whose dimensions are greater or less than the dimensions of a given size, and - Store the calibrated and dried combustible material without moisture absorption.
[0011] The method according to the invention makes it possible to produce calibrated combustible material in a laminated format similar to wood chips which has a very low humidity level (> 10%). The humidity level and the format of the calibrated combustible material make it possible to optimize the combustion and / or gasification of this combustible material, which advantageously optimizes the efficiency of production of electrical and thermal energy. The drying cycle is adapted to optimize the extraction of moisture at the core in order to increase the calorific value of the calibrated combustible material.
[0012] The process also makes it possible to ensure production rates of calibrated combustible material on an industrial scale which makes it possible to supply a gasification reactor for more than 8000 hours per year from, for example, 16000 tonnes of wet wood per year.
[0013] In embodiments, the method may comprise a refining step by mechanically reducing the dimensions of the pieces of wood of the combustible material so as to provide a combustible material of reduced dimensions. This step makes it possible to optimize the rolling of the pieces of wood which constitute the combustible material in order to obtain pieces of wood of homogeneous dimensions.
[0014] In particular, the refining step may reduce the pieces of wood of the combustible material to dimensions which are less than 100 mm and preferably the dimensions of the pieces of wood resulting from the refining step 204 are less than 50 mm.
[0015] In embodiments, the mechanical reduction may be performed by rotary cutting of the shear having a rotational speed of less than 500 rpm, preferably the rotational speed is less than 250 rpm, and most preferably the rotational speed is less than 100 rpm. The low-speed rotary cutting provides a scissor-effect cut that is cleaner and produces less wood fines residue. This optimizes the efficiency of the preparation method of the invention.
[0016] In embodiments, the method according to the invention may comprise at least one step of extracting ferrous metals and / or non-ferrous metals. Such a step makes it possible to eliminate the metal residues, on the one hand, in order to protect the equipment which is used in the method, and on the other hand, to ensure combustion homogeneity and increase the efficiency of the gasification reactor.
[0017] In embodiments, the method according to the invention may comprise a step of recovering wood residues of dimensions smaller than the dimensions of the calibrated combustible material, said wood residues are separated from the non-wood residues and compacted so as to provide a compacted secondary fuel. This step makes it possible to optimize the efficiency of the process by producing a secondary fuel with the residues resulting from the process and in particular from the mechanical reduction steps.
[0018] In embodiments, the mechanical reduction step may produce a combustible material that comprises pieces of wood having dimensions less than 500 mm and preferably the dimensions of the pieces of wood are less than 300 mm.
[0019] In embodiments, the method according to the invention may comprise a step of storing the combustible material of reduced dimensions before the drying step so as to provide a reserve of combustible material of reduced dimensions upstream of the drying step. This step makes it possible to compensate for the differences in production rate between the drying step and the upstream and / or downstream steps.
[0020] In embodiments, the drying step is carried out according to a drying cycle having a duration greater than 5 hours and at a temperature lower than 100°C, preferably the drying cycle duration is greater than 100.
[0021] The invention also relates to an installation for preparing wood fuel material to supply in particular a gasification reactor, the installation comprising: - at least one receiving conveyor configured to receive type B wood waste, - a first mechanical reducer which is configured to mechanically reduce the dimensions of wood waste so as to transform the wood waste into combustible material which has pieces of wood of determined dimensions, the receiving conveyor conveying the wood waste to the first mechanical reducer, - at least one dryer configured to dry the combustible material of reduced dimensions according to a drying cycle having a temperature lower than 100°C and for a duration greater than 5 hours, preferably the duration of the drying cycle is greater than 100, and - at least one screen configured to separate, within the combustible material, pieces of wood and wood residues whose dimensions are greater or less than the dimensions of a given size, - at least one storage unit for dried and calibrated combustible material suitable for storing the material without moisture absorption.
[0022] In particular, by maintaining a humidity level of less than 10% within the combustible material, this material is stored without moisture absorption.
[0023] The installation according to the invention has the same advantages as those of the method according to the invention.
[0024] In embodiments, the installation according to the invention may comprise a second mechanical reducer which is configured to refine by mechanical reduction so as to produce a combustible material whose pieces of wood have dimensions smaller than the pieces of wood coming from the first mechanical reducer.
[0025] In embodiments, the screen may comprise two screening grids, a first screening grid comprising a mesh whose dimensions are smaller than the dimensions of the sized combustible material, and a second screening grid comprising a mesh whose dimensions are larger than the dimensions of the sized combustible material.
[0026] In embodiments, at least one mechanical reducer may comprise at least one rotary shear having a rotational speed of less than 500 rpm, preferably the rotational speed is less than 250 rpm, and preferably the rotational speed is less than 100 rpm. Each reducer comprises refiners are equipped with a grid and at least one knife behind the grid to avoid long pieces of long wafers in order to ensure homogeneous wafers with few fines at the outlet.
[0027] In embodiments, the dryer may include a support grate and a hot air source, the support grate configured to receive the reduced-size combustible material while the hot air source is disposed beneath the support grate so as to generate an upward flow of hot air within the dryer.
[0028] In particular, the dryer may integrate a system for conveying the calibrated combustible material so that said combustible material gradually passes through the dryer.
[0029] In embodiments, the installation according to the invention may comprise a storage unit for the dried combustible material and of reduced calibrated dimensions, the storage unit is arranged between the screen dryer and the screen dryer. This storage unit makes it possible to compensate for differences in production rate between the dryer and the other equipment of the installation.
[0030] In embodiments, the installation according to the invention may comprise at least one unit for extracting non-ferrous metals and / or ferrous metals, the extraction unit comprising an electromagnetic field generator.
[0031] In embodiments, the installation according to the invention may comprise a unit for recovering wood residues such as fines which have dimensions smaller than the dimensions of the calibrated combustible material, the recovery unit being equipped with a compactor in order to produce a compacted secondary fuel. The recovery unit makes it possible to recover the wood residues resulting from the different stages, in particular mechanical reduction.
[0032] In embodiments, the installation according to the invention may comprise a dust and fines suction system comprising suction inlets at least at the level of the mechanical reducer and the screen. The suction system makes it possible to reduce the respiratory risks of operators working within the installation. Brief description of the drawings
[0033] Other characteristics and advantages of the invention will become apparent from reading the description which follows. This is purely illustrative and must be read in conjunction with the appended drawings in which:
[0034] [Fig. 1] is a schematic representation of an installation for preparing wood fuel material according to an embodiment of the invention, the fuel material making it possible in particular to supply a unit for producing electrical and thermal energy by gasification.
[0035] [Fig.2] is a schematic representation of a flowchart illustrating the steps of a process for preparing wood combustible material according to one embodiment of the invention, the combustible material making it possible in particular to supply a unit for producing electrical and thermal energy by gasification.
[0036] [Fig.3] is a representation of combustible materials produced by a preparation process according to an embodiment of the invention. Description of the embodiments
[0037] The invention relates to an installation 10 and a method 200 which make it possible to prepare a combustible material which can in particular be used to feed a gasification reactor. Nevertheless, the combustible material can be used in other applications requiring a fuel such as domestic or industrial heating.
[0038] The inventors chose to transform only type B wood waste which corresponds to “BFVBD” (end-of-life wood and waste wood) defined according to the 2017 reference standard of ADEME (French Environment and Energy Management Agency), which is a French government agency. More specifically, ADEME defines BFVBD as end-of-life packaging wood such as logistics pallets, end-of-life furniture wood whether raw or of the particle board type, joinery wood such as OSB which is made up of layers of treated wood strips, wood from demolition, etc.
[0039] The method 200 and the installation 10 conforming to the invention make it possible to recover this non-hazardous wood waste which comes from industrial activity and local waste disposal sites.
[0040] With reference to [Fig.l], the installation 10 comprises at least one receiving conveyor 11 configured to receive type B wood waste. The receiving conveyor 11 may comprise a wide belt in order to receive and convey wooden pieces whose size may be greater than 1m3. The receiving conveyor 11 may be equipped with a densitometric detector in order to detect very large pieces of metal, such as pieces of metal greater than 1kg. When this type of metal pieces are identified, they are extracted from the receiving conveyor 11 before sending them to the rest of the processing line to avoid damaging the equipment of the processing line which is located downstream.
[0041] In the example of [Fig.l], the wood waste is conveyed to the installation 10 using a dump truck 100. The installation 10 may also comprise weighing equipment adapted to the dump trucks 100 in order to evaluate the quantity of wood waste which is introduced into the processing line of the installation 10. Wood waste storage areas may advantageously be arranged close to the installation 10 in order to ensure production independence on several weeks in case of external damage such as frost barriers, social events, etc.
[0042] The installation 10 comprises at least one first mechanical reducer 12 which is configured to mechanically reduce the dimensions of wood waste. The first mechanical reducer 12 transforms the wood waste into combustible material which has pieces of wood of determined dimensions. The pieces of wood resulting from the first mechanical reduction have dimensions less than 500 mm, preferably the dimensions of the pieces of wood are less than 300 mm. As can be seen in [Fig.l], the receiving conveyor 11 conveys the wood waste 1 to the first mechanical reducer 12.
[0043] According to one embodiment, the installation 10 comprises a second mechanical reducer 13 which is configured to refine the caliber of the combustible material. The mechanical reduction of the first caliber combustible material provides a combustible material whose dimensions of the pieces of wood are reduced or refined compared to the pieces resulting from the first reduction. For example, the dimensions of the refined pieces of wood can be between 0 mm and 100 mm, and preferably the dimensions of the refined pieces of wood can be between 0 mm and 50 mm. In this embodiment, the first mechanical reducer 12 carries out a pre-reduction of the wood waste while the second mechanical reducer refines the dimensions of the pieces of wood which constitute combustible material.
[0044] According to one embodiment, at least one mechanical reducer 12, 13, and preferably each mechanical reducer 12, 13, comprises at least one rotary shear, preferably each mechanical reducer 12, 13, comprises several rotary shears, for example, each mechanical reducer 12, 13 can comprise four rotary shears.
[0045] Each rotary shear is configured to operate at a rotational speed of less than 500 rpm, preferably the rotational speed of the shear is less than 250 rpm, and preferably the rotational speed of the shear is less than 100 rpm. The inventors have surprisingly discovered that a low rotational speed of between 15 and 50 rpm provides optimal cutting for pre-reduction and / or refining the dimensions of the pieces of wood. The use of a low rotational speed shear makes it possible to reduce the size of the wood waste according to a chisel effect which ensures a clean cut and produces a combustible material of which each unit has a laminar geometric shape as shown in [Fig. 3].
[0046] However, a combustible material whose units have a homogeneous geometric shape makes it possible to increase the efficiency of gasification or combustion, for example, of a boiler. In addition, the low rotation speed makes it possible to reduce the quantities of fines which are residues from mechanical reduction.
[0047] The inventors therefore chose a mechanical reduction technique which goes against practices in the field of wood waste processing which usually use high-speed grinders (whose speed is greater than 2000 rpm). However, high-speed grinding reduces the size of the material by a tearing effect which produces, on the one hand, units whose geometric shape is not homogeneous, and on the other hand, a significant quantity of fines and dust which have a lower calorific potential and are dangerous for operators working on the installation site.
[0048] Furthermore, each mechanical reducer 12, 13 may comprise, between the rotary shear and the output of the reducer, knives under a grid to prevent pieces of wood of dimensions larger than the required dimensions from passing into the rest of the processing line. This ensures uniformity of shape and dimensions of the pieces of wood at the output of each mechanical reducer 12, 13.
[0049] In this example, a second conveyor carries the combustible material between the first mechanical reducer 12 and the second mechanical reducer 13.
[0050] As illustrated in [Fig.l], the installation 10 comprises at least one dryer 14 configured to dry the combustible material. According to one embodiment, the installation 10 comprises two dryers 14 to allow during maintenance operations not to stop the production of calibrated combustible materials. The two dryers 14 are advantageously connected by a conveyor so that the combustible material passes successively through the two dryers 14. This makes it possible to dry a combustible material whose humidity level is greater than 35% which is considered to be very humid material.
[0051] According to the invention, a dryer 14 operates according to a slow drying cycle which has a cycle duration greater than 5 hours, preferably the duration of the drying cycle is greater than 100. Concretely, this means that a piece of wood can take between 5 hours and 14 hours to pass through the dryer 14. The inventors have discovered that optimal drying is obtained by eliminating 90% of the humidity from the combustible material for a drying cycle lasting 14 hours. The dryer projects air whose temperature is between 30 and 100°C, and preferably, the temperature of the air projected by the dryer onto the combustible material is between 40 and 70°C. Such a temperature applied according to the drying cycle durations addressed above makes it possible to optimize the drying of the combustible material.
[0052] The inventors have discovered that a slow, low-temperature drying cycle as described above makes it possible to dry the core of the pieces of wood before the surface of the latter. This is possible because the pores of the wood are not closed. However, a closing of the pores is observed when drying is applied too quickly with a temperature If the temperature is too high, for example when the temperature is above 100°C, the outer surface of the pieces of wood becomes gritted and prevents the moisture from escaping from the core to the outside of the piece of wood.
[0053] According to one embodiment, the dryer 14 comprises a support grid and a hot air source. The support grid is configured to receive the combustible material while the hot air source is arranged under the support grid so as to generate an upward flow of hot air within the dryer. For example, the combustible material may be distributed in a 20 cm thick bed on the support grid. The dryer 14 may be supplied with hot air by a hot water / air exchanger using hot water from a gasification reactor arranged near the installation 10.
[0054] Furthermore, the dryer 14 may incorporate a system for conveying the combustible material so that said combustible material gradually passes through the dryer. The conveying system may comprise scraper ladders operated by a hydraulic unit which has the advantage of advancing the combustible material at a low speed. The slow passage through the dryer 14 makes it possible to reduce its length and to provide slow, homogeneous and complete drying.
[0055] According to one embodiment, the installation 10 may comprise a storage unit 15 for the combustible material which is arranged between the dryer 14 and the screen 16. The storage unit 15 makes it possible to compensate for the differences in speed between the dryer and the equipment located upstream and downstream of it. For this, the dryer 14 may operate 24 hours a day while the rest of the line upstream and downstream of the dryer 14 may operate 10 hours a day. The storage unit 15 is configured to store the combustible material without moisture absorption. According to one embodiment, the storage unit 15 may be ventilated with air. For example, the ventilated air may be pretreated by a heat exchanger to extract the moisture therefrom.
[0056] According to one embodiment of the invention, a storage unit 150 for the combustible material of reduced dimensions can be arranged between the mechanical reducers 12, 13 and the dryer 14. This storage unit 150 makes it possible to compensate for the differences in operating rate between the mechanical reducers 12, 13 and the dryer 14.
[0057] As illustrated in [Fig.l], the installation 10 comprises at least one screen 16. The screen 16 is arranged after the dryer 14. In particular, the screen 16 is configured to separate the combustible material from the pieces of wood and the wood residues whose dimensions are greater or smaller than the dimensions of a determined caliber.
[0058] According to one embodiment, the screen 16 comprises two screening grids, a first screening grid comprising a residue extraction mesh whose dimensions are smaller than the dimensions of the calibrated combustible material. In the occurrence, the dimensions of the residue extraction mesh may be between 3 mm and 10 mm, preferably, the dimensions of the residue extraction mesh may be between 5 mm and 8 mm. The screen 16 comprises a second screening grid comprising a wood piece rejection mesh whose dimensions are greater than the dimensions of the calibrated combustible material. Here, the rejection mesh corresponds to the dimensions of the refined wood pieces, the rejection mesh thus has dimensions less than 100 mm or preferably dimensions less than 50 mm. In addition, the screen 16 may be of different types, for example, the screen 16 may be a vibrating screen, a drum screen or a cam screen.
[0059] The installation 10 has means for returning pieces of wood which do not pass the rejection mesh, the return means conveying said pieces of wood towards the second mechanical reducer 13 in order to reduce their dimensions to allow them to pass through the rejection mesh of the screen 16. Alternatively, the pieces of wood which do not pass the rejection mesh can be stored in a bin with a view to reintroducing them into the processing chain of the installation 10, for example, at the receiving conveyor 11.
[0060] According to one embodiment, the installation 10 comprises a unit 17 for recovering wood residues of dimensions smaller than the dimensions of the calibrated combustible material. In particular, the pieces of wood and the fine passing through the extraction mesh at the level of the screen 16 are recovered and conveyed to the recovery unit 17. The recovery unit 17 is in particular equipped with a compactor in order to produce a compacted secondary fuel.
[0061] In particular, the pieces of wood, fines and dust can be captured at the level of the screen 16 by suction, but also at the level of each mechanical reducer 12, 13 and then stored separately in several buffer silos 18. The fines and dust stored separately in the silos 18 are mixed according to determined proportions in order to pass through an aeraulic densitometric separator of the “Zig-Zag” type which separates the wood residues from the other fine mineral elements or residual metals pebbles ... The densitometric separator feeds a dosing screw which mixes the said residues with water. The mixture is then sent to a die press which makes it possible to produce compacted secondary fuels such as pebbles or granules.
[0062] The compacted fuels are then cooled and sieved before being stored in a compacted fuel storage silo 19 which can act as a buffer silo to supply a gasification reactor.
[0063] According to one embodiment, the installation 10 may comprise at least one unit 20, 21 for extracting and separating non-ferrous metals and / or ferrous metals. Each extraction and separation unit 20, 21 comprises means for generating an electromagnetic field such as a permanent magnet or an electromagnet. For example, an extraction unit 20 may be arranged above the second conveyor which extends between the two mechanical reducers 12, 13. The extraction unit 20 removes the ferrous elements to preserve the second mechanical reducer 13 which has a finer cut and therefore cutting members more easily exposed to damage caused by metal debris. However, according to another embodiment, the extraction unit 20 may also be positioned between the second mechanical reducer 13 and the dryer 14.
[0064] According to one embodiment, the installation 10 comprises a second extraction unit 21 which has the function of separating the ferrous and non-ferrous metals from the calibrated and dried combustion material. In this example, the second extraction unit 21 is arranged between the screen 14 and a storage unit 24. For example, the second extraction unit 21 may comprise a vibrating distributor (vibrating plate) which distributes the material over the width of the belt which extends under a pulley equipped with a magnet which runs the entire width of the belt. The polishing first extracts the ferrous metals. The distribution of the material over the width of the belt optimizes the extraction of the ferrous metals. The pulley may comprise a powerful permanent magnet comprising in particular neodymium to extract the ferrous elements.In addition, the second extraction unit 21 may also incorporate an eddy current separator which is intended for the extraction of non-ferrous metals present in the flow of combustible materials. The non-ferrous metals may include OMR, WEEE, RBA, clinker, electric cables etc.
[0065] The metals extracted from the combustible material can then be recovered in suitable recycling centers. In practice, the second extraction unit can consist of a curved conveyor which includes a neodymium pulley and an eddy current separator. The curvature of the conveyor belt keeps the pieces of wood stuck to the belt and optimizes the magnetic extraction of the metallic materials at the level of the curvature.
[0066] As illustrated in [Fig.l], the installation 10 comprises at least one storage unit 24 for the calibrated and decontaminated dried combustible material which aims to provide a buffer reserve of combustible material. The storage unit 24 is configured to store the material without moisture absorption as previously described. According to an embodiment illustrated in [Fig.l], the storage unit 24 is arranged at the end of the production line following the second extraction unit 21 and is connected to the gasification reactor by the feed conveyor 22.
[0067] It should be noted that the installation incorporates conveyors which transport the combustible material between each processing equipment (dryer, reducer mechanical, metal extractor etc.) and storage units or silos.
[0068] All the conveyors of the installation 10 can be closed belt conveyors to limit noise pollution and limit dust emissions.
[0069] The transformation of BFVBD into calibrated combustible material and into a compacted secondary product generates wood dust which is harmful to the health of operators and potentially explosive if it is left suspended in the premises. To avoid these drawbacks, according to one embodiment, the installation 10 can be equipped with a dust and fine dust extraction system 25 comprising suction inlets at least at the level of the mechanical reducer 12, 13 and the screen 16. However, it is also possible to connect the extraction system 25 to all the processing equipment of the installation 10 and in certain cases also to the various conveyors which are integrated into the installation 10. For example, the extraction system 25 can be centralized and equipped with two cyclones to capture the largest dust and a bag filter for fine dust.
[0070] It should be noted that the compacted fuel storage silo 19 is also connected to the feed conveyor 22 so as to mix the calibrated combustible material and the compacted fuel to feed the gasifier.
[0071] With reference to [Fig.2], the invention also relates to a method 200 for preparing wood fuel material to supply in particular a gasification reactor. The installation 10 allows the implementation of the method 200.
[0072] As illustrated in [Fig.2], the method comprises a step 201 of supplying wood waste of type wood B. In this example, the receiving conveyor 11 makes it possible to receive and introduce the wood waste into the production line. Upstream of its introduction into the production line, the wood waste is weighed and the quality of the material can be evaluated by measuring, for example, its humidity and by visually determining the quality of the product, in particular the quantity of body which constitutes the wood waste.
[0073] According to one embodiment, the preparation method 200 comprises at least one step 202 of extracting ferrous metals and / or non-ferrous metals. The extraction step 202 can be carried out by densimetry or for magnetic extraction. The installation 10 gives an example in which an extraction unit 20 uses the principle of magnetic extraction. The extraction step 202 makes it possible to optimize the calorific value of the combustible material produced but also to protect the equipment of the production line from potential damage. In this example, a metal extraction unit 20 comprising a powerful magnet can be arranged above a conveyor of the installation 10 (see [Fig.l]).
[0074] As illustrated in [Fig.2], the method comprises a step of mechanically reducing 203 the dimensions of the wood waste so as to transform the wood waste in combustible material which comprises pieces of wood whose dimensions are reduced. According to one embodiment, the mechanical reduction step 203 produces a combustible material which comprises pieces of wood whose dimensions are less than 500 mm and preferably the dimensions of the pieces of wood are less than 300 mm. In this example, the mechanical reduction step 203 is carried out by the first mechanical conveyor 12, it makes it possible to carry out a pre-cutting of the wood waste.
[0075] According to an embodiment illustrated in [Fig. 2], the preparation method 200 comprises a refining step 204 by mechanically reducing the dimensions of the pieces of wood of the combustible material so as to provide a combustible material of reduced dimensions. In particular, the refining step 204 reduces pieces of wood of the combustible material to dimensions which are less than 100 mm and preferably the dimensions of the pieces of wood resulting from the refining step 204 are less than 50 mm. In this example, the refining step 204 is carried out by the second mechanical reducer 13.
[0076] According to one embodiment, the mechanical reduction is carried out by rotary cutting which has a rotation speed of the shear less than 500 rpm, preferably the rotation speed is less than 250 rpm, and preferably the rotation speed is less than 100 rpm. As previously addressed, the inventors have discovered that the optimal rotation speed of the rotary cutting is between 15 and 50 rpm. The mechanical reduction 203 and refining 204 steps use a low cutting speed as previously described. The rotary cutting allows at low rotation speed to produce a chisel effect on the pieces of wood which results in a clean cut and a reduction in the quantities of fines. The mechanical reduction 203 and refining 204 steps can thus be carried out using a mechanical reducer 12, 13 capable of processing between 2000 and 4000 kg / h of combustible materials.
[0077] The succession of two mechanical reduction stages 203, 204 makes it possible to compensate for the low rotation speeds of the mechanical reducers 12, 13 and to maintain a production rate that is acceptable from an industrial point of view.
[0078] The drying step 205 aims to eliminate the moisture with which each piece of wood is soaked in order to optimize its calorific value during combustion / gasification. In this step, the calibrated combustible material is dried by extracting the moisture from the heart of the pieces of wood of reduced dimensions.
[0079] During the drying step 205, a flow of hot air is projected onto the combustible material which passes through the dryer 14. The temperature of this flow of hot air can be between 30 and 100°C, preferably, preferably, the temperature of the flow of hot air is between 40 and 70°C. Advantageously, the drying step 205 is takes place according to a slow drying cycle which can have a duration greater than 5 hours, preferably the duration of the drying cycle is greater than 10 hours. The inventors have discovered that at this temperature a drying cycle lasting 14 hours can eliminate up to 90% of the moisture contained in the laminated pieces of wood. As explained above, the combustible material passes through the dryer, for example using scraper ladders which carry said material towards the outlet of the dryer 14.
[0080] According to one embodiment, the method 200 may comprise a storage step 206 of the dry combustible material. This storage step 213 makes it possible to create a reserve of dry combustible material available to supply, for example, a gasification reactor. In the example of [Fig.l], the storage step 213 is carried out by the storage unit 23.
[0081] As illustrated in [Fig.2], the preparation method 200 comprises a step 207 of screening the combustible material so as to eliminate pieces of wood and wood residues whose dimensions are greater or less than the dimensions of a determined caliber. The screening step 207 can be carried out using a vibrating screen as previously addressed.The screening step 207 produces three fractions of material, firstly, wood residues whose dimensions are less than 10 mm and preferably less than 8 mm, specifically, these wood residues pass through the extraction mesh of the screen 16, secondly, pieces of wood which can be between 10 and 100 mm and preferably between 8 and 50 mm, and secondly, pieces of wood which do not pass the rejection mesh of the screen 16 and whose dimensions are greater than 100 mm and preferably pieces of wood whose dimensions are greater than 50 mm.
[0082] It is preferable to carry out the screening 205 on dry material to optimize the separation of wood residues such as fines and dust in particular. This is why the screen 16 is preferably arranged after the dryer 14.
[0083] According to an embodiment illustrated in [Fig.2], the method 200 may comprise a step 208 of returning pieces of wood whose dimensions are greater than the rejection mesh to the equipment which carries out the mechanical reduction steps 202, 204. In particular, said pieces of wood are preferably returned to the refining step 204. As illustrated in [Fig.l], to facilitate the returning of said pieces of wood, the screen 16 may be connected to the second mechanical reducer 13 by a conveyor. Alternatively, a skip may be placed at the outlet of the rejection mesh to collect the oversized pieces of wood, the latter will then be reintroduced into the processing chain. The returning step 208 makes it possible to optimize the efficiency of the process and ensures homogeneity of the combustible material in terms of dimensions and geometric shape. This step 208 is op- tional it is for this reason that it is represented in dotted lines on [Fig.2].
[0084] According to another embodiment illustrated in [Fig.2], the method 200 may comprise a step 209 of recovering wood residues of dimensions smaller than the dimensions of the calibrated combustible material. In practice, it is the wood residues which pass through the extraction mesh during step 207 which are recovered, for example, by suction. In order to optimize the efficiency of the method 200, these residues are then treated and compacted so as to provide a compacted secondary fuel which can also be used for gasification.
[0085] In the example of [Fig.l], the screen 16 is connected to the suction system 25 which collects the residues (fines, dust and debris) passing through the extraction mesh and conveys them to a silo 18 to carry out a storage step for the wood residues from the screening step 207. The silo 18 makes it possible to constitute a buffer reserve in order to supply a secondary production line which aims to produce, using the mechanical reduction residues, a secondary compacted product which can also be used as fuel. The method 200 can thus comprise a treatment step 210 of said wood residues. This treatment step 210 consists of eliminating all residues which are not wood derivatives and then hydrating said residues in order to create a physical binder between the residue particles for compaction.
[0086] For example, the treatment step 210 can be carried out by passing the wood residues through a densitometric separator such as a “Zig-Zag” type aeraulic separator which separates the wood from other fine elements (such as metals, stones), then conveying the cleaned residues to a mixing screw which mixes them with water. The paste which results from the treatment step 210 can then undergo a compacting step 211 to form a compacted secondary product. To obtain granules it is possible to use a pellet press such as a flat die press, however it is also possible to use a press to form compacted pallets. In the example of [Fig.l], the installation makes it possible to cool and then sieve the compacted products before storing them in a silo 19 for example to create a supply reserve for a gasification reactor.
[0087] The third fraction which is obtained using the screen 16 corresponds to the calibrated combustible material, that is to say, pieces of laminated wood with dimensions smaller than the rejection mesh and larger than the extraction mesh.
[0088] According to one embodiment, the method 200 may comprise a storage step 211 of the combustible material of reduced dimensions which can be described as wet material. In the example of the installation 10, a storage unit 150 is arranged at the outlet of the second reducer 13 to provide a reserve of combustible and wet material upstream of the drying step 205. The storage step 211 allows to compensate for the rates at which the different stages of the process 200 take place. For example, the refining stage 204 processing speed of the mechanical reducers 12, 13 can have an output mass flow rate of between 2000 and 4000 kg / h of combustible materials while the drying stage 212 of the process 200 must be slower to obtain optimal extraction of the moisture contained in each piece of wood. For example, the dryer 14 used in the installation 10 can have an output mass flow rate of between 800 and 1400 kg / h. To compensate for this lower mass flow rate value, the operating time range of the dryer 14 can be greater than those of the other equipment. For example, the dryer 14 can operate 24 / 24h while the other equipment operates according to a time range of between 10h / 24 and 14h / 24.
[0089] According to one embodiment, the method 200 may comprise a second extraction step 212 of the ferrous metals and / or the non-ferrous metals. In the example of [Fig. 2] this second extraction step 214 of the metals is arranged after the screening step 207 and before the calibrated combustible material is introduced into a gasification reactor. As described previously, the second extraction step 212 may be carried out using an extraction unit 21 which distributes the combustible material over the width of a vibrating belt, then extracts the ferrous metals using a magnetic pulley, and finally extracts the non-ferrous metals using an eddy current separator. The metals may thus be extracted and recovered at establishments specializing in the recycling of metals. The combustible material thus decontaminated may be stored as illustrated in [Fig.l], in which the installation comprises a storage unit 24 for the calibrated combustible material arranged downstream of the second extraction unit 21.
[0090] Thus, according to one embodiment, the method 200 may comprise a storage step 213 of the calibrated, dried and decontaminated combustible material. This storage step 213 is carried out dry in a ventilated storage unit 24 in order to avoid any moisture absorption. In general, the storage steps which follow the drying step are optimized by ventilation means to avoid moisture absorption which would deteriorate the quality of the combustible material with a view to its gasification or combustion.
[0091] According to one embodiment, the method 200 is carried out in geographical proximity to a gasification reactor and can thus comprise a step 214 of feeding the reactor during which the calibrated combustible material and the compacted secondary product can be mixed, for example, within a conveyor 22 to feed the gasification reactor.
[0092] As can be seen in [Fig.l], between each step of the method 200, the combustible material can be conveyed by conveyors.
[0093] The schematic representation of the method 200 in [Fig.2] includes optional steps which allow the method to be optimized, which is why they are represented in dotted lines.
Claims
Claims
1. Method for preparing (200) wood combustible material to feed in particular a gasification reactor, the method (200) comprises the following steps: - Providing (201) wood waste of type B wood, - Mechanically reducing (203) the dimensions of the wood waste so as to transform the wood waste into combustible material which comprises pieces of wood whose reduced dimensions, - Drying (205) the calibrated combustible material according to a drying cycle by extracting the humidity from the heart of the pieces of wood of reduced dimensions and - Sifting (207) the combustible material so as to eliminate the pieces of wood and wood residues whose dimensions are greater or less than the dimensions of a determined caliber, - Storing (212) the calibrated and dried combustible material.
2. Preparation method (200) according to claim 1, which comprises a refining step (204) by mechanically reducing the dimensions of the pieces of wood of the combustible material so as to provide a combustible material of reduced dimensions.
3. A preparation method (200) according to claim 2, wherein the refining step (204) reduces the pieces of wood of the combustible material to dimensions which are less than 100 mm and preferably the dimensions of the pieces of wood resulting from the refining step 204 are less than 50 mm.
4. Preparation method (200) according to one of claims 1 or 2, wherein the mechanical reduction is carried out by rotary cutting which has a rotation speed of the shears less than 500 rpm, preferably less than the rotation speed is less than 250 rpm, and preferably the rotation speed is less than 100 rpm.
5. Preparation method (200) according to one of claims 1 to 4, which comprises at least one step of extraction (202, 212) of ferrous metals and / or non-ferrous metals.
6. Preparation method (200) according to one of claims 1 to 5, which comprises a step of recovering (209) wood residues of dimensions smaller than the dimensions of the calibrated combustible material, said wood residues are separated from the non-wood residues and compacted (210) so as to provide a compacted secondary fuel.
7. Preparation method (200) according to one of claims 1 to 6, wherein the mechanical reduction step (203) produces a combustible material which comprises pieces of wood whose dimensions are less than 500 mm and preferably the dimensions of the pieces of wood are less than 300 mm.
8. Preparation method (200) according to one of claims 1 to 7, which comprises a step of storing (211) the combustible material of reduced dimensions before the drying step (205) so as to provide a reserve of combustible material of reduced dimensions upstream of the drying step (205).
9. Preparation method (200) according to one of claims 1 to 8, wherein, the drying step (205) according to a drying cycle having a duration greater than 5 hours and at a temperature less than 100°C, preferably the duration of the drying cycle is greater than 100.
10. Installation for preparing (10) wood combustible material to feed in particular a gasification reactor, the installation comprising: - at least one receiving conveyor (11) configured to receive type B wood waste, - a first mechanical reducer (12) which is configured to mechanically reduce the dimensions of wood waste so as to transform the wood waste into combustible material which has pieces of wood of determined dimensions, the receiving conveyor (11) conveying the wood waste to the first mechanical reducer (12), - at least one dryer (14) configured to dry the combustible material of reduced dimensions according to a drying cycle having a temperature lower than 100°C and for a duration greater than 5 hours, preferably the duration of the drying cycle is greater than 100,and - at least one screen (16) configured to separate within the dried combustible material pieces of wood and wood residues whose dimensions are greater than or in-, smaller than the dimensions of a given caliber, - at least one storage unit (24) adapted to store the calibrated and dried combustible material without moisture absorption.
11. Preparation installation (10) according to claim 10, which comprises a second mechanical reducer (13) which is configured to refine by mechanical reduction so as to produce a combustible material whose pieces of wood have dimensions smaller than the pieces of wood coming from the first mechanical reducer (12).
12. Preparation installation according to one of claims 10 and 11, in which the screen (14) comprises two screening grids, a first screening grid comprising a mesh whose dimensions are smaller than the dimensions of the calibrated combustible material, and a second screening grid comprising a mesh whose dimensions are greater than the dimensions of the calibrated combustible material.
13. Preparation installation (10) according to one of claims 10 to 12, wherein at least one mechanical reducer (12, 13) comprises at least one rotary shear which has a rotation speed of less than 500 rpm, preferably the rotation speed is less than 250 rpm, and preferably the rotation speed is less than 100 rpm.
14. Preparation installation (10) according to one of claims 10 to 13, in which the dryer (14) comprises a support grid and a source of hot air, the support grid configured to receive the combustible material of reduced dimensions while the source of hot air is arranged under the support grid so as to generate an upward flow of hot air within the dryer.
15. Preparation installation (10) according to claim 14, in which the dryer incorporates a system for conveying the combustible material so that said combustible material gradually passes through the dryer.
16. Preparation installation (10) according to one of claims 10 to 15, which comprises a storage unit (15) for the dried combustible material and of reduced dimensions, the storage unit (15) is arranged between the dryer (14) and the screen (16).
17. Preparation installation (10) according to one of claims 10 to 16, which comprises at least one extraction unit (20, 21) for non-ferrous metals and / or ferrous metals, the extraction unit (20, 21) including an electromagnetic field generator.
18. Preparation installation (10) according to one of claims 10 to 17, which comprises a unit (17) for recovering wood residues of dimensions smaller than the dimensions of the calibrated combustible material, the recovery unit (17) being equipped with a compactor in order to produce a compacted secondary fuel.
19. Preparation installation (10) according to one of claims 10 to 18, which comprises a dust and fines suction system (25) comprising suction openings at least at the level of the mechanical reducer (12, 13) and the screen (16).
Citation Information
Patent Citations
Method Of Gasification Of Waste, In Particular Household Waste And The Apparatus For Performing Such A Method
US20170088783A1
Process for treating woody plant materials and solid recovered fuels for the production of biomass pellets
EP3246382A1
Method and system for conversion of wet biomass to high-grade fuel pellets
EP3280785B1
Particulate waste wood fuel, method for making particulate waste wood fuel, and a method for producing energy with particulate waste wood fuel
US6193768B1