RESISTIVE MEMORY CELL
A CMOS-compatible resistive memory cell using V2O3 with a localized titanium-oxygen-vanadium zone addresses integration issues of Mott memories, enabling efficient resistive switching and thermal compatibility.
Patent Information
- Application Number
- FR2023004573
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-09
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2043-05-09
AI Technical Summary
Existing non-volatile resistive memories, such as Mott memories based on (V2xCrx)O3, face integration challenges in CMOS back end processes due to high thermal budgets exceeding 450°C, and require initialization steps.
A resistive memory cell using a conductive vanadium oxide (V2O3) with a localized zone of vanadium, titanium, and oxygen, formed through ion beam deposition, allowing bipolar operation and compatible with CMOS back end integration.
The proposed memory cell achieves reliable resistive switching between high and low states with improved endurance and reduced thermal requirements, maintaining resistance values without additional initialization steps.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Title of the invention: RESISTIVE MEMORY CELL TECHNICAL FIELD OF THE INVENTION
[0001] The technical field of the invention is that of resistive memories. The present invention relates to a non-volatile resistive memory cell. TECHNOLOGICAL BACKGROUND OF THE INVENTION
[0002] For applications that require information to be stored even when the power is off, non-volatile memories of the EEPROM or FLASH type are conventionally used. However, these memories have disadvantages such as long write times, a memory point density limited by the size of the transistors used or a limited number of rewrite cycles.
[0003] More recently, resistive non-volatile memories constitute a promising alternative to FLASH or EEPROM type memories.
[0004] Resistive memories are based on the use of an active medium whose electrical resistance depends on the electrical voltage applied to the terminals of the material. In other words, a resistive memory cell has two states: an HRS state ("High Resistive State" according to English terminology) corresponding to a highly resistive state and an LRS state ("Low Resistive State" according to English terminology) corresponding to a weakly resistive state. The active medium is inserted between two electrodes allowing the application of an electrical voltage and ensuring the reading and writing of the state of the resistive memory cell.
[0005] Depending on the type of active material used, different types of resistive memory can be produced: phase change materials (PCRAM or “Phase Change RAM” memories also called PCM “Phase Change Memory”), ionic conduction (CBRAM or “Conductive Bridging RAM” memories), metal oxides (OxRAM or “Oxide Resistive RAM” memories), magnetic (MRAM or “Magnetic RAM” memories), magnetic spin transfer materials (STTRAM or “Spin Torque Transfer RAM” memories) or Mott insulators.
[0006] So-called "Mott" memories are based on the use of an active layer made of Mott insulating materials, which are materials that, according to band theory, should be conductive, but in reality are insulating due to strong electronic correlations. It is possible to make the material pass from this Mott insulating state to a metallic state by applying pressure or an electric field. In Mott memories, a SET voltage applied to the memory electrodes controls the transition from the insulating state to the metallic state, and a RESET voltage applied to the memory electrodes controls the transition from the metallic state to the insulating state. It should be noted that Mott memories are of the apolar type: in other words, the sign of the SET or RESET voltage applied is irrelevant, unlike bipolar resistive memories such as CB RAM memories for example, for which it is necessary to invert the sign of the potential applied to the electrodes depending on whether one is trying to carry out a SET or RESET operation.
[0007] Among Mott insulators, crystallized vanadium sesquioxide in which part of the vanadium atoms are substituted by chromium, for example (V2xCrx)O3 (with x > 0.011), is a Mott insulator in which the phenomenon of reversible resistive switching induced by an electrical pulse is possible. It is therefore used for the production of Mott memories. The advantage of Mott resistive memories compared to other resistive RRAM memories is that they are based solely on electronic transition phenomena. Unlike certain other resistive memories with an initial state where the active material of the active storage area is insulating (pristine state), Mott memory does not require an initialization or forming step (i.e. a step during which a first electrical stress must therefore be applied to the virgin memory cell in order to generate the LRS state for the first time).
[0008] The production of thin layers of crystallized (V2xCrx)O3 (with x > 0.011) usable in a Mott memory has been obtained by physical vapor deposition (PVD) techniques such as magnetron cathode sputtering: to do this, abrasion of vanadium and chromium-based targets by argon ions under oxygen pressure is carried out in order to obtain an amorphous vanadium oxide, non-stoichiometric in oxygen and chromium. However, the material (V2.xCrx)O3 (with x > 0.011) used in Mott memories must be crystallized and perfectly stoichiometric. Consequently, the PVD deposition step is followed by an annealing step at a temperature greater than or equal to 500°C under a reducing atmosphere. Such a technique has certain drawbacks in a back-end CMOS integration logic in which the thermal budget must not exceed 450°C. Summary of the invention
[0009] The invention offers a solution to the problems mentioned above, by proposing a non-volatile resistive memory cell based on vanadium oxide which is notably more easily integrated into a CMOS back end process.
[0010] A resistive memory cell is understood to mean an electrical device having a first highly resistive state or HRS state or RESET state and a second low resistive state or LRS state or SET state. Non-volatility lies in the fact that the memory cell retains its resistive state once the SET or RESET voltage is RESET is no longer applied.
[0011] The invention more specifically relates to a resistive memory cell comprising: • A lower electrode based on titanium nitride, • An upper electrode, • An active layer having a first contact surface with the lower electrode and a second contact surface with the upper electrode, said active layer comprising a zone, called the local zone, said local zone being in a material comprising vanadium, titanium and oxygen extending from the first contact surface, the remainder of the active layer being made of conductive vanadium oxide V2O3.
[0012] Conductive vanadium oxide V2O3 is understood to mean a V2O3 material with a resistivity less than or equal to 0.1 ohm.cm.
[0013] Unlike Mott memories which rely on the use of a (V 2 xCrx)O3 material (with x > 0.011) in the Mott insulating phase, the memory cell according to the invention uses an active layer mainly made of V2O3 with a singular zone in this layer at the interface between the active layer and the lower electrode: this zone of the active layer at the lower electrode is not made of conductive vanadium oxide V2O3 and comprises a highly resistive material including vanadium, titanium and oxygen. Surprisingly, the applicant has noticed that such a cell has a resistive memory operation allowing switching between a highly resistive state HRS and a low resistive state LRS.These RESET and SET operations are carried out by applying a potential difference of reverse polarity between the upper and lower electrodes of the memory cell: in other words, unlike Mott memories, the cell according to the invention has a bipolar operation.
[0014] Surprisingly, the applicant discovered the operation of the invention by wanting to produce an insulating V2O3 material for a Mott memory by an ion beam deposition (IBD) technique; by using this deposition technique, the inventors obtained a conductive V2O3 material and therefore not suitable for a Mott memory known from the state of the art. However, by carrying out RESET / SET cycle operations on a stack including an active layer of conductive V2O3 as deposited between two electrodes, the inventors observed a resistive memory type operation.They also observed that, during the first initialization operation (or forming according to English terminology), the conductive V2O3 layer passed from a low resistive state LRS to a highly resistive state HRS with the appearance of this singular local zone based on titanium, oxygen and highly resistive vanadium. in the V2O3 layer. This particular cell structure including this zone formed from a V-Ti-O alloy gives the cell according to the invention a role of bipolar resistive memory cell. We will return in the rest of the description to the structure of this cell, to its operation and to the mechanism of creation of this localized zone in V-Ti-O, probably linked to a strong heating at the interface between the lower electrode and the active layer at the time of the forming step. It will be noted that IBD deposition techniques allow the production of crystalline or partially crystalline conductive V2O3 layers at crystallization temperatures above 280°C, therefore perfectly compatible with CMOS back-end integration.
[0015] It will be noted that the terms "lower" and "upper" are of course used for a better understanding of the invention but remain relative so that the lower electrode can be considered as the upper electrode and the upper electrode as the lower electrode by turning the memory cell over while remaining within the scope of application of the memory cell according to the invention.
[0016] In addition to the characteristics which have just been mentioned in the preceding paragraphs, the memory cell according to the invention may have one or more additional characteristics among the following, considered individually or according to all technically possible combinations: • The upper electrode is based on titanium nitride; • the local area is without contact with the second contact surface; • the thickness of the active layer is between 5 and 200 nm and preferably between 10 and 100 nm; • the local area has a dome shape whose section parallel to the plane of the layers decreases from the first contact surface; • the lower electrode based on titanium nitride comprises vanadium, titanium and oxygen in a localized area close to the first contact surface. In this case, the local area has, for example, a mushroom shape with a dome whose section parallel to the plane of the layers decreases from the first contact surface; • the first contact surface has an area less than or equal to 6000 nm 2 • 9 • the first contact surface is equal to the upper surface of the lower electrode and strictly less than the total lower surface of the active layer; • the lower electrode has a rectangular parallelepiped shape of the “Wall” type or an L shape; • conductive vanadium oxide V2O3 is crystalline or partially crystalline; • the local area is made of a crystalline or partially crystalline material.
[0017] Another object of the invention is a method of manufacturing a memory cell comprising the following steps: • Production of a lower electrode based on titanium nitride; • Deposition of a layer made of vanadium oxide V2O3 having a first contact surface with the lower electrode; • Production of an upper electrode; said method comprising a step, called the initialization step, consisting of injecting a current through the stack formed by the lower electrode, the V2O3 layer and the upper electrode, the current density being chosen to create said local zone comprising vanadium, titanium and oxygen.
[0018] In addition to the characteristics which have just been mentioned in the preceding paragraphs, the manufacturing method according to the invention may have one or more additional characteristics among the following, considered individually or according to all technically possible combinations: • The method comprises a heat treatment step during or after said deposition step until said layer of vanadium oxide V2O3 becomes conductive; • said deposited layer is made of amorphous vanadium oxide V2O3; • the current density of the initialization step is greater than or equal to 50.106 A / cm2; • the deposition of the layer made of vanadium oxide V2O3 is carried out using an ion beam deposition technique; • the method comprises a step of cleaning the lower electrode by ionic stripping (Ar, Xe, or Kr) in situ (i.e. in the same equipment as the V2O3 deposition step, without re-exposure to air) before the V2O3 deposition step; • the production of the upper electrode can be carried out in situ or after re-exposure to air. BRIEF DESCRIPTION OF THE FIGURES
[0019] The figures are presented for information purposes only and in no way limit the invention.
[0020] [Fig.l] schematically represents a 3D view of the memory cell according to the invention.
[0021] [Fig.2] represents the behavior during 1000 write (SET) and erase (RESET) cycles of a memory cell according to the invention.
[0022] [Fig.3] shows a dark-field STEM image of a cell before forming.
[0023] [Fig.4] shows a dark-field STEM image of a memory cell according to the invention.
[0024] [Fig.5], [Fig.6], [Fig.7] and [Fig.8] show analyses by energy dispersive X-ray spectroscopy EDX and by TEM microscopy of a memory cell according to the invention.
[0025] [Fig.9], [Fig.10], [Fig.11] and [Fig.l2][Fig.l3], [Fig.14] and [Fig.15] show results of write (SET) and erase (RESET) cycles for cells according to the invention with different contact surfaces and different active layer thicknesses.
[0026] [Fig. 16] schematically illustrates the operation of a memory cell according to the invention.
[0027] [Fig.17] and [Fig.18] are EELS analyses showing the presence of oxygen and vanadium in the upper part of the lower electrode of the memory cell according to the invention.
[0028] The invention and its various applications will be better understood upon reading the following description and examining the accompanying figures. DETAILED DESCRIPTION OF THE INVENTION
[0029] Unless otherwise specified, the same element appearing in different figures has a single reference.
[0030] [Fig.l] schematically represents in three dimensions a memory cell 1 according to the invention in an Oxyz reference frame, the Oxy plane defining the plane of the layers, the Oz axis defining the direction of the height of the layers, the Oy axis defining the direction of the length of the layers and the Ox axis defining the direction of the width of the layers.
[0031] Memory cell 1 comprises: • A lower electrode 2 in TiN; • A top electrode 4 in TiN; • An active layer 3 mainly made of conductive vanadium oxide V2O3 and crystallized or partially crystallized but with a singular localized zone 5 comprising titanium, vanadium and oxygen to which we will return in the following.
[0032] The upper surface of the active layer 3 is in contact with the lower surface of the upper electrode 4, along a contact surface S2.
[0033] The lower surface of the active layer 3 is in contact with the upper surface of the lower electrode 2, along a contact surface SL
[0034] The lower electrode 2 has a “wall” type architecture, that is to say it forms a parallelepiped wall of length 1, width L and height h: the area IxL of the upper surface of the electrode is strictly less than the area of the surface in lower part of the active layer 3; in other words, the area of the contact surface SI is equal to IxL. The area of the contact surface SI is strictly less than the area of the contact surface S2 (i.e. the lower electrode 2 here has a width L much less than the width of the upper electrode 4 and a length 1 less than or equal to that of the upper electrode 4). It will be noted that the lower electrode 2 can also have other shapes such as an L shape with a first upper part identical to the wall presented above and a second lower part of parallelepiped shape parallel to the plane of the layers.
[0035] The active layer 3 of the memory cell 1 according to the invention can be produced in particular by the deposition of a crystallized or partially crystallized conductive V2O3 layer using an ion beam deposition (IBD) technique. The deposition consists of the sputtering of a vanadium target by an argon ion beam. The deposition chamber is placed under vacuum (5x108 Torr) before deposition. During deposition, the partial pressure of oxygen is controlled and influences the degree of oxidation of the final material. The deposition is carried out at room temperature and does not necessarily require heat treatment, thus making the method for obtaining the memory cell according to the invention compatible with CMOS back-end integration. Even with crystallization annealing, the latter remain below 450°C, which is the maximum temperature for CMOS back-end integration.
[0036] According to another embodiment, after the IBD deposition the V2O3 is insulating (resistivity of the order of a few ohms.cm to a few tens of ohms.cm) and has an amorphous character (no diffraction peaks detectable in XRD characterization). In this case, annealing at a temperature lower than 450°C and preferably greater than or equal to 280°C is carried out in order to obtain a conductive V2O3 material (i.e. with a resistivity lower than or equal to 0.1 ohm.cm) crystallized or partially crystallized. It will be noted that the annealing step can be carried out during the manufacture of the wall-type memory cell which implements certain technological steps, such as the deposition of encapsulation dielectrics, at temperatures of the order of 300°C, temperatures at which the amorphous IBD V2O3 crystallizes.
[0037] The production of the upper and lower electrodes based on titanium nitride is done according to techniques well known to those skilled in the art. At this stage, the active layer is exclusively made of crystallized or partially crystallized conductive V2O3 while we have seen that the active layer 3 according to the invention comprises a singular localized zone 5 comprising titanium, vanadium and oxygen. The conductive V2O3 could also be obtained by other deposition techniques such as PVD deposition. It is also possible to use crystallized conductive V2O3 in which part of the vanadium is substituted by chromium as long as the V2O3 remains conductive.
[0038] To obtain this singular localized zone 5, it is appropriate to carry out a forming step (i.e. initialization) through the stack formed by the two electrodes (the lower electrode having the shape of the wall 2) and the crystallized or partially crystallized conductive V2O3 layer. It is understood that at this stage called pristine state (i.e. virgin state), the stack is in a low resistive state LRS since the V2O3 layer is conductive. The forming step consists of injecting a current with a high current density, preferably strictly greater than 50.106 A / cm2 by applying a positive voltage between the first and the second electrode (forming voltage). This step will cause the stack to switch from its pristine state LRS to a highly resistive state HRS and will cause the appearance of the localized zone 5 shown in [Fig. 1].The appearance of this zone including titanium, oxygen and vanadium can be explained by the injection of a high density current at the contact surface SI between the first electrode 2 and the active layer 3. The area of the upper surface IxL of the first wall-shaped electrode is chosen to be sufficiently small to cause local heating at the level of SI and the zone close to SI (i.e. above in the active zone 3 and below in the first electrode 2).Electrothermal simulations using the COMSOL tool show that the temperature reached at the interface between the lower electrode wall 2 and the active layer 3 can reach 2000°K: this local heating leads to the creation of zone 5 made of a V-Ti-0 alloy comprising a first dome-shaped part 6 extending from the first contact surface SI and rising inside the active layer 3 and a second part 7 located on the upper end of the lower electrode 2. In other words, zone 5 has the shape of a mushroom with its cap in the active zone 3 and its foot in the top of the lower electrode 2.
[0039] Once this forming operation has been carried out and the V-Ti-0 based zone 5 has been created, the memory cell 1 behaves like a bipolar resistive memory cell. In other words, the application of a SET voltage pulse will allow a SET operation to be carried out and a switch to a low resistive state LRS. Then the application of a RESET voltage pulse of opposite sign to the SET voltage will allow a switch to a high resistive state HRS. The memory cell has a non-volatile behavior so that it retains the resistance value once the SET or RESET voltage is no longer applied. [Fig. 2] shows the behavior during 1000 write (SET) and erase (RESET) cycles of a memory cell according to the invention with an active layer thickness of 50 nm, a length 1 of the lower wall-type electrode of 100 nm and a width L of 24 nm. The SET pulse is 1.2V for 100 ns and the opposite polarity RESET pulse of opposite polarity to the SET pulse is 1.3 V for 200 ns. On . observes good endurance (i.e. during 1000 SET / RESET cycles) of the memory cell according to the invention which switches from an LRS resistance of a few kOhms to an HRS resistance of the order of a few hundred kOhms. The endurance results show a low dispersion of the resistive states compared to other types of resistive memories such as CBRAM or OxRAM. It is noted that the SET and RESET pulses have amplitudes lower than 2 V and durations lower than 1 ps.
[0040] The highlighting of the localized zone 5 was carried out by scanning transmission electron microscopy (STEM) images (Scanning Transmission Electron Microscope according to the English terminology) illustrated in Figures 3 and 4. [Fig. 3] shows a dark-field STEM image of a cell before forming and [Fig. 4] shows a dark-field STEM image of a memory cell according to the invention after the forming step and 40 programming cycles. The circle shown in [Fig. 4] surrounds the particular zone 5 of [Fig. 1] created after the initialization step, above the lower wall electrode in TiN. This zone 5, not present in [Fig. 3] before the forming step, is an altered zone a few nanometers thick with high atomic density in the shape of a dome whose section parallel to the plane of the layers decreases from the first contact surface.It is noted that this zone 5 is indeed located inside the active layer 3 in conductive V2O3 and has a different atomic density than the part in conductive V2O3. It is also noted that this zone 5 starts from the contact surface between the active layer 3 and the lower electrode 2 in TiN then goes up in the thickness of the active layer 3 without reaching the upper surface of the active layer 3 so that zone 5 is not in contact with the upper electrode 4: the localized zone 5 remains present during the different programming cycles and can be seen as a zone in contact with the lower electrode 2 in a more global zone in conductive V2O3. The fact that the memory cell according to the invention is in a highly resistive state after the forming step indicates that zone 5 is made of a highly resistive material.Thus, the forming step induces a change in the composition of the conductive V2O3 material in this zone and the formation of a highly resistive alloy based on vanadium, titanium and oxygen. This result is supported by data from the literature which indicate high resistivities of the order of 105 Ohm.cm for TiO2-V2O3-V2O5 alloys and especially by analyses by energy dispersive X-ray spectroscopy (EDX) illustrated in figures 5 to 8 which demonstrate the presence of titanium in this particular zone 5. In each of figures 5 to 8, are represented: • On the right part an image by transmission electron microscopy. TEM (Transmission Electron Microscopy) of the memory cell according to the invention; • On the upper part, a diffraction image of the area surrounded by the rectangle present on the TEM image; • On the lower part, the EDX spectrum of the area surrounded by the rectangle present on the TEM image.
[0041] The TEM and EDX analyses show the creation of a local dome-shaped zone 6 comprising vanadium, titanium and oxygen. The presence of vanadium and oxygen is not surprising since this zone is located in a layer initially made of V2O3. On the other hand, the EDX analyses clearly show the presence of titanium in the first wall-type electrode but also in the local zone located immediately above the first electrode and noted 5 in [Fig. 1]. It can be seen that the quantity of titanium is greater at the contact interface SI between the active layer 3 and the lower electrode 2 and then gradually decreases until it disappears in the active layer 3 comprising only V2O3 on its upper part: this observation makes it possible to clearly identify the singular zone 5 which does not extend over the entire height of the active layer 3. The presence of titanium is again evident at the upper electrode 4.
[0042] Figures 17 and 18 show EELS analyses by electron energy loss spectrometry illustrating the distribution of vanadium and oxygen respectively for a stack of a memory cell according to the invention before the forming step and for a memory cell according to the invention once formed. For each [Fig. 17] and 18, the upper part shows a transmission electron microscopy image of the analyzed area: the lower electrode and the active layer are seen. In [Fig. 17], the EELS images of the uninitialized stack (bottom left for vanadium and bottom right for oxygen) show the presence of vanadium and oxygen only in the active layer. On the other hand, in [Fig. 18], the EELS images of the memory cell according to the invention (bottom left for vanadium and bottom right for oxygen) show the presence of oxygen and vanadium, in addition to titanium, in the upper part 7 of the lower electrode 2.We therefore have a local zone 5 in the shape of a mushroom (dome 6 and upper part 7 of the lower electrode) comprising vanadium, titanium and oxygen.
[0043] Figures 9 to 15 show cycling results for cells according to the invention with different SI contact surfaces and different thicknesses of active layer 3. These results show that the thickness of the conductive V2O3 layer has little impact on the memory behavior of the cell according to the invention: this thickness is however preferably between 5 and 200 nm and even more advantageously between 10 and 100 nm. The SI contact surface (i.e. corresponding to the upper surface of the lower electrode wall 2) is preferably lower at 6000 nm2.
[0044] [Fig. 16] schematically illustrates an explanation of the operating mode of the cell according to the invention. The left part of the figure shows the stack before the forming step without the presence of the highly resistive local zone 5: in this virgin configuration, the stack is low resistive. After the initialization step allowing to pass from a low resistive virgin state to a highly resistive state HRS, the memory cell according to the invention 1 is created with the presence of the highly resistive singular zone 5 comprising in particular Ti, V and O. Then, the resistive memory cell could behave like a filamentary resistive memory with the singular zone 5 playing the role of solid electrolyte.Thus, when a positive potential is applied to the lower electrode 2, mobile titanium-based ions would move from the lower electrode 2 under the effect of the electric field applied to the electrodes, causing the growth of a titanium metal filament inside the singular zone 5 based on Ti, V and O. The remainder of the active layer 3 being made of metal oxide, the memory cell according to the invention then passes into a low resistive state LRS. The transition to the high resistive state HRS consists of applying a negative voltage to the lower electrode 2, causing the total or partial dissolution of the conductive filament.
Claims
Claims
1. Resistive memory cell (1) comprising: - A lower electrode (2) based on titanium nitride, - An upper electrode (4), - An active layer (3) having a first contact surface (SI) with the lower electrode and a second contact surface (S2) with the upper electrode, said active layer (3) comprising a zone, called local zone (5), said local zone being in a material comprising vanadium, titanium and oxygen extending from the first contact surface (SI), the remainder of the active layer being made of conductive vanadium oxide V2O3.
2. Memory cell according to the preceding claim, characterized in that the upper electrode (4) is based on titanium nitride.
3. Memory cell according to one of the preceding claims, characterized in that said local zone is without contact with the second contact surface (S2).
4. Memory cell according to one of the preceding claims, characterized in that the thickness of the active layer is between 5 and 200 nm and preferably between 10 and 100 nm.
5. Resistive memory cell according to one of the preceding claims, characterized in that the local zone has a dome shape whose section parallel to the plane of the layers decreases from the first contact surface.
6. Memory cell according to one of the preceding claims, characterized in that the lower electrode based on titanium nitride comprises vanadium, titanium and oxygen in a localized area close to the first contact surface.
7. Memory cell according to one of the preceding claims, characterized in that the first contact surface has an area less than or equal to 6000 nm2.
8. Memory cell according to one of the preceding claims, characterized in that the first contact surface is equal to the upper surface of the lower electrode and is strictly less than the total lower surface of the active layer.
9. Memory cell according to one of the preceding claims, characterized in that the lower electrode has a rectangular parallelepiped shape of the “Wall” type or an L shape.
10. Memory cell according to one of the preceding claims, characterized in that the conductive vanadium oxide V2O3 is crystalline or partially crystalline.
11. Memory cell according to one of the preceding claims, characterized in that the local zone is in a crystalline or partially crystalline material.
12. Method for manufacturing a resistive memory cell according to any one of the preceding claims, characterized in that it comprises the following steps: - Production of a lower electrode based on titanium nitride - Deposition of a layer made of vanadium oxide V2O3 having a first contact surface with the lower electrode; - Production of an upper electrode; said method comprising a step, called the initialization step, consisting of injecting a current through a stack formed by the lower electrode, the V2O3 layer and the upper electrode, the current density being chosen to create said local zone comprising vanadium, titanium and oxygen.
13. Method according to the preceding claim, characterized in that it comprises a heat treatment step during or after said deposition step until said layer of vanadium oxide V2O3 becomes conductive.
14. Method of manufacturing a memory cell according to one of claims 12 to 14 characterized in that the current density of the initialization step is greater than or equal to 50.106 A / cm2.
15. Method of manufacturing a memory cell according to one of claims 12 to 14, characterized in that the deposition of the layer made of vanadium oxide V2O3 is carried out by an ion beam deposition technique.
Citation Information
Patent Citations
Resistance change memory device having threshold switching and memory switching characteristics, method of fabricating the same, and resistance change memory device including the same
US20130270509A1