A cathode composition
Magnesium-based cathode compositions with a disordered rock salt structure, produced via low-temperature high-energy ball milling, address the limitations of lithium-rich cathodes by enhancing energy density and stability, offering a cost-effective and practical solution for battery cathodes.
Patent Information
- Application Number
- GB2024013858
- Authority / Receiving Office
- GB · GB
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2021-12-20
- Publication Date
- 2024-12-04
- Estimated Expiration
- 2041-12-20
AI Technical Summary
Lithium-rich cathode compositions for batteries face issues with defects, trapped lithium ions, and energy-intensive high-temperature synthesis, which complicates reaction control and limits energy density in disordered rock salt structures.
Development of magnesium-based cathode compositions with a disordered rock salt crystal structure, produced through low-temperature high-energy ball milling, where magnesium is the primary charge carrier, enabling improved energy density and stability by avoiding spinel or layered structures and allowing precise control over oxidation states.
The magnesium-based cathode compositions demonstrate enhanced electrochemical activity, stability, and energy density compared to lithium-based compositions, with the ability to be synthesized and cycled effectively at lower costs, using a method that maintains oxidation states and avoids high-temperature synthesis.
Smart Images

Figure 00000001_0000 
Figure 00000002_0000 
Figure 00000003_0000
Abstract
Description
TECHNICAL FIELD The present invention relates to a cathode composition. More specifically, the present invention relates to a cathode composition for a battery. The present invention further relates to a method of making the cathode composition for a battery. The present invention further relates to a cathode comprising the cathode composition and an electrochemical cell comprising the cathode. BACKGROUND Lithium-rich cathode compositions for batteries are widely known. Typically, lithium-rich cathodes require a layered structure, which can lead to problems with defects, trapped lithium ions and collapse of the layers during cycling of the battery. In addition, iithium-rich cathode compositions are usually prepared via high temperature synthesis, which is energy-intensive, expensive and can result in difficulties in controlling the reactions that take place to form the composition. More recently, lithium-rich disordered rock salt (DRS) structures have been investigated as cathode materials. However, it is currently a challenge to improve the energy density in lithium-rich DRS structures with known compositions and methods. The present invention has been devised to mitigate or overcome at least some of the above-mentioned problems. SUMMARY OF THE INVENTION In accordance with a first aspect of the present invention, there is provided a cathode composition for a battery of the general formula: MgnxNii-xO2 or Mgi+xMni-xO2; wherein the value of x is greater than 0. The present invention thereby provides stable and electrochemically-active magnesiumbased cathode compositions for batteries. In these compositions, magnesium is the main charge carrier, rather than lithium in traditional lithium-ion batteries. Magnesiumbased cathode compositions are synthetically challenging to produce; however the present inventors have shown for the first time that not only can the above magnesiumbased cathode compositions be produced, but also that they can be produced in a straightforward manner and cycled. The compositions themselves are cheaper to produce and more practical than any previously reported cathode composition. In addition, the present inventors have demonstrated electrochemical activity in these compositions for the first time. Advantageously, the magnesium ion intercalation process involves the insertion of two electrons, which enables the energy density and stability of the cathode to be significantly improved in comparison to lithium-based cathode compositions. The composition may be in the form of a single phase having a rock salt crystal structure such that an x-ray diffraction pattern of the composition using a Cu Ka radiation source has an absence of peaks below a 20 value of 35. Conventional ordered or layered lithium and manganese-rich compositions (Lh+xTmi-xCk where Tm is predominately IV1n) have lithium ions sitting in both the alkali and transition metal sites. In addition to the above, x-ray diffraction patterns of these conventional compositions will have a peak at a 20 value of 18. However, in the present invention the x-ray diffraction pattern of the cathode composition has an absence of a peak at a 20 value of 18. In other words, the single phase crystal structure of the present invention is absent of any spinel or layered structures, and is considered purely as a single phase rock salt crystal structure. The single phase crystal structure does not exhibit either a R3(bar)m and / or a C2 / m space group. In particular, the compositions are provided as a single phase rock salt crystal structure (i.e. face centred cubic lattice with the Fm3(bar)m space group), which may be a disordered rock salt crystal structure. The value of x may be equal to or less than approximately 0.3. The composition may be Mg1.2Nio.sO2. The composition may be Mg1.2Mno.3O2. The value of x may be equal to or less than approximately 0.15. In accordance with a second aspect of the present invention, there is provided a method of making the cathode composition according to the first aspect, the method comprising: providing a magnesium nickel oxide precursor or a magnesium manganese oxide precursor; high-energy milling the precursor with a plurality of milling balls at a milling speed for a milling time period to form the cathode composition; wherein the magnesium nickel oxide precursor or the magnesium manganese oxide precursor has oxidation states that are equal to the oxidation states of the respective elements in the cathode composition. Contrary to known high temperature synthesis methods, the present method of making the cathode compositions does not require high temperatures. In addition, the present method provides more control over the oxidation states of the transition metals in the compositions, since the precursors can be selected according to the required oxidation states and applying the method to the precursors results in a cathode composition based on the oxidation states of the precursors without any risk of oxidation during the milling process. The milling speed may be at least approximately 400 rpm. The mining speed may be between approximately 400 rpm and approximately 1000 rpm. The milling speed may be between approximately 400 rpm and approximately 800 rpm. The milling speed may be approximately 800 rpm. The milling time period may be between approximately 10 hours and approximately 180 hours. The milling time period may be between approximately 40 hours and approximately 100 hours. The milling time period may be between approximately 40 hours and approximately 80 hours. The milling time period may be between approximately 40 hours and approximately 60 hours. The ratio of precursor powder to milling balls by weight may be between 1:4 and 1:20. The magnesium nickel oxide precursor may comprise magnesium oxide and nickel oxide in a molar proportion of 1+x magnesium oxide to 1-x nickel oxide. The magnesium manganese oxide precursor may comprise magnesium oxide and manganese oxide in a molar proportion of 1+x magnesium oxide to 1-x manganese oxide. The plurality of milling balls may comprise tungsten carbide. The high-energy milling may be performed within a ball mill jar comprising tungsten carbide. The plurality of milling balls may comprise zirconium oxide The high-energy milling may be performed within a ball mill jar comprising zirconium oxide. Each of the plurality of milling balls may have a diameter of approximately 0.5 mm to approximately 1 cm. In accordance with a third aspect of the present invention, there is provided a cathode comprising the cathode composition according to the first aspect. In accordance with a fourth aspect of the present invention, there is provided an electrochemical cell comprising a cathode according to the third aspect, an electrolyte and an anode. Within the scope of this application, it is expressly intended that the various aspects, embodiments, examples and alternatives set out in the preceding paragraphs, in the claims and / or in the following description and drawings, and in particular the individual features thereof, may be taken independently or in any combination. That is, ali embodiments and / or features of any embodiment can be combined in any way and / or combination, unless such features are incompatible. The applicant reserves the right to change any originally filed claim or file any new claim accordingly, including the right to amend any originally filed claim to depend from and / or incorporate any feature of any other claim although not originally claimed in that manner. BRIEF DESCRIPTION OF THE DRAWINGS One or more embodiments of the invention will now be described, by way of example only, with reference to the accompanying drawings, in which: Figure 1 shows eiectric potential as a function of capacity for the cathode composition Mgi 2Nio.s02 in Example 1; Figure 2 shows electric potential as a function of capacity for the cathode composition Mg1.2Mno.gO2 in Example 2; and Figure 3 shows X-ray diffraction patterns of the cathode composition Mg1.2Mno.sO2 in Example 2. DETAILED DESCRIPTION The present invention relates to a cathode composition for a battery of the general formula: Mgi+xNi1.xO2 or Mgi+xMni.xO2; wherein the value of x is greater than 0. The composition has a disordered rock salt structure, Le. it comprises regions of rock salt having different cations, wherein the regions are disordered. In this way the rock salt effectively forms a composite rock salt material. The inventors have determined that the cathode composition can be made using a ball milling technique. Starting materials are selected according to the desired cathode material, as will be explained in more detail below. The starting materials are then subjected to ball milling for a milling time period. The ball milling process typically takes place at room temperature, or at low temperatures such that the oxidation state of the metal cations is not altered during the process. Milling parameters can be selected as appropriate. After the ball milling process is complete, the resulting material is the disordered rock salt cathode composition. The ball milling process advantageously allows the oxidation state of the metals to be maintained into the final cathode composition. In this way, the oxidation state, and hence the final cathode composition, can be carefully controlled. For the MguxNh-xCh composition, the starting materiai is a magnesium nickel oxide. The magnesium nickel oxide comprises a mixture of MgO and NiO, which is preferably provided in powder form. The ratio of the MgO and NiO is selected according to the value of x in the final composition. In particular the molar ratio of MgO to NiO is 1+x to 1-x. For the Mg-i+xMn^Oz composition, the starting material is a magnesium manganese oxide. The magnesium manganese oxide comprises a mixture of MgO and MnO, which is preferably provided in powder form. The ratio of the MgO and MnO is selected according to the value of x in the final composition. In particular the molar ratio of MgO to MnO is 1+x to 1-x. The ball milling process parameters may be any suitable parameters. In particular: The ball milling time period is a time that is sufficient to produce the cathode composition, which may be for example at least 10 hours. The material of the balls and / or the container may be any suitable material such as for example tungsten carbide or zirconium oxide. A ratio of balls to precursor may be any suitable ratio to provide sufficient milling to produce the cathode composition. For example the ratio of precursor to milling balls by weight may be between 1:4 and 1:20, though other suitable ratios may be used. The milling speed may be any suitable milling speed that is sufficient to produce the cathode composition, which may be for example at least approximately 400 rpm. The composition can be incorporated into a cathode in any suitable form. Aspects of the present invention indude a method of making the cathode composition for a battery, a cathode comprising the cathode composition, and an electrochemical cell comprising the cathode. The present invention will now be illustrated with reference to the following examples. EXAMPLE 1 Mg12Ni0.8O2 A magnesium nickel oxide (MgNiO?) precursor was prepared having a molar ratio of 1.2 MgO to 0.8 NiO. This corresponded to 8.95g (44.75 wt%) MgO and 11,05g (55.25 wt%) NiO. The precursor was provided in a 20 ml ball mill jar made of tungsten carbide. 80 tungsten carbide milling balls each having a diameter of 5 mm were also provided in the ball mill jar. High-energy milling was used to mill the precursor at a milling speed of 800 rpm for a milling time period of at least 10 hours to form a cathode composition of the formula: Mgi.2Nios02. This results in formation of 20g of Mg1.2Nio.sO2 powder inside the ball mill jar. The composition has a disordered rock salt crystal structure. The oxidation state of the Mg in MgO is +2 and the oxidation state of the Ni in NiO is +2. The oxidation states of Mg and Ni in the cathode composition Mg1.2Nio.sO2 are also +2. Figure 1 shows electric potential as a function of capacity for the cathode composition Mgi2Nio.a02, which demonstrates that the composition can be cycled effectively. EXAMPLE 2 Mg1.2Mno.sO2 A magnesium manganese oxide (MgMnO2) precursor was prepared having a molar ratio of 1.2 MgO to 0.8 MnO. This corresponded to 9.20g (46 wt%) MgO and 10.80g (54 wt%) MnO. The precursor was provided in a 20 ml ball mill jar made of tungsten carbide. 80 tungsten carbide milling bails each having a diameter of 5 mm were also provided in the ball mill jar. High-energy milling was used to mill the precursor at a milling speed of 800 rpm for a milling time period of at least 10 hours to form a cathode composition of the formula: Mg1.2Mno.3O2. This results in formation of 20g of Mg1.2Mno.3O2 powder inside the bail mill jar. The composition has a disordered rock salt crystal structure. The oxidation state of the Mg in MgO Is +2 and the oxidation state of the Mn in MnO is +2. The oxidation states of Mg and Mn in the cathode composition Mg1.2Mno.sO2 are also +2. Figure 2 shows electric potential as a function of capacity for the cathode composition Mg1.2Mno.8O2, which demonstrates that the composition can be cycled effectively. The X-ray diffraction pattern of the cathode composition Mg1.2Mno.8O2 is shown in Figure 3, demonstrating the crystalline structure of the composition. The XRD pattern is characteristic of a cation disordered rock salt structure. The pattern appears to show the broad major peaks consistent with a face centred cubic lattice with the Fm3(bar)m space group, as shown in Figure 3. Many modifications may be made to the specific embodiments described above without departing from the scope of the invention as defined in the accompanying claims. Features of one embodiment may also be used in other embodiments, either as an addition to such embodiment or as a replacement thereof. CLAUSES Clause 1. A cathode composition for a battery of the general formula: MgnxNivxO2 or MgnxMni.xO2 wherein the value of x is greater than 0. Clause 2. The cathode composition according to clause 1, wherein the composition has the form of a single phase having a rock salt crystal structure such that an x-ray diffraction pattern of the composition using a Cu Ka radiation source has an absence of peaks below a 29 value of 35. Clause 3. The cathode composition according to clause 1 or clause 2, wherein the value of x is equal to or less than approximately 0.3. Clause 4. The cathode composition according to any preceding clause, wherein the composition is Mg1.2Nio.sO2. Clause 5. The cathode composition according to any preceding clause, wherein the composition is Mg1.2Mno.sO2. Clause 6. The cathode composition according to any of clauses 1 to 3, wherein the value of x is equal to or less than approximately 0.15. Clause 7. A method of making the cathode composition according to any of clauses 1 to 6, the method comprising: providing a magnesium nickel oxide precursor or a magnesium manganese oxide precursor; high-energy milling the precursor with a plurality of milling balls at a milling speed for a milling time period to form the cathode composition; wherein the magnesium nickel oxide precursor or the magnesium manganese oxide precursor has oxidation states that are equal to the oxidation states of the respective elements in the cathode composition. Clause 8. The method according to clause 7, wherein the milling speed is at least approximately 400 rpm. Clause 9. The method according to clause 7 or clause 8, wherein the milling speed is between approximately 400 rpm and approximately 1000 rpm. Clause 10. The method according to any of clauses 7 to 9, wherein the milling speed is between approximately 400 rpm and approximately 800 rpm. Clause 11. The method according to any of clauses 7 to 10, wherein the milling speed is approximately 800 rpm. Clause 12. The method according to any of clauses 7 to 11, wherein the milling time period is between approximately 10 hours and approximately 180 hours. Clause 13. The method according to any of clauses 7 to 12, wherein the milling time period is between approximately 40 hours and approximately 100 hours. Clause 14. The method according to any of clauses 7 to 13, wherein the mining time period is between approximately 40 hours and approximately 80 hours. Clause 15. The method according to any of clauses 7 to 14, wherein the milling time period is between approximately 40 hours and approximately 60 hours. Clause 16. The method according to any of clauses 7 to 15, wherein the ratio of precursor powder to milling balls by weight is between 1:4 and 1:20. Clause 17. The method according to any of clauses 7 to 16, wherein the magnesium nickel oxide precursor comprises magnesium oxide and nickel oxide in a molar proportion of 1+x magnesium oxide to 1-x nickel oxide. Clause 18. The method according to any of clauses 7 to 16, wherein the magnesium manganese oxide precursor comprises magnesium oxide and manganese oxide in a molar proportion of 1+x magnesium oxide to 1-x manganese oxide. Clause 19. The method according to any of clauses 7 to 18, wherein the plurality of milling balls comprises tungsten carbide. Clause 20. The method according to clause 19, wherein the high-energy milling is performed within a ball mill jar comprising tungsten carbide. Clause 21. The method according to any of clauses 7 to 18, wherein the plurality of milling balls comprises zirconium oxide. Clause 22. The method according to clause 21, wherein the high-energy milling is performed within a ball mill jar comprising zirconium oxide. Clause 23. The method according to any of clauses 7 to 22, wherein each of the plurality of milling bails has a diameter of approximately 0.5 mm to approximately 1 cm. Clause 24. A cathode comprising the cathode composition according to any of clauses 1 to 6. Clause 25. An electrochemical cell comprising a cathode according to clause 24, an electrolyte and an anode.
Claims
1. A cathode composition for a battery of the general formula:Mg1+xMni.xO2wherein the value of x is greater than 0 and less than 1.
2. The cathode composition according to claim 1, wherein the composition has the form of a single phase having a rock, salt crystal structure that has an x-ray diffraction pattern when using a Cu Ka radiation source having an absence of peaks below a 29 value of 35.
3. The cathode composition according to claim 1 or claim 2, wherein the value of x is equal to or less than 0.3.
4. The cathode composition according to any preceding claim, wherein the composition is Mgi.2Mno.sO2.
5. The cathode composition according to any of claims 1 to 3, wherein the value of x is equal to or less than 0.15.
6. A method of making the cathode composition according to any of claims 1 to 5, the method comprising:providing a magnesium nickel oxide precursor or a magnesium manganese oxide precursor;high-energy milling the precursor with a plurality of milling balls at a milling speed for a milling time period to form the cathode composition;wherein the magnesium nickel oxide precursor or the magnesium manganese oxide precursor has oxidation states that are equal to the oxidation states of the respective elements in the cathode composition. / . The method according to claim 6, wherein the milling speed is at least 400 rpm.
8. The method according to claim 6 or claim 7, wherein the milling speed is between 400 rpm and 1000 rpm.
9. The method according to any of claims 6 to 8, wherein the milling speed is between 400 rpm and 800 rpm.
10. The method according to any of claims 6 to 9, wherein the milling speed is 800 rpm.
11. The method according to any of claims 6 to 10, wherein the milling time period is between 10 hours and 180 hours.
12. The method according to any of claims 6 to 11, wherein the milling time period is between 40 hours and 100 hours.
13. The method according to any of claims 6 to 12, wherein the milling time period is between 40 hours and 80 hours.
14. The method according to any of claims 6 to 13, wherein the milling time period is between 40 hours and 60 hours.
15. The method according to any of claims 6 to 14, wherein the ratio of precursor powder to milling balls by weight is between 1:4 and 1:20.
16. The method according to any of claims 6 to 15, wherein the magnesium manganese oxide precursor comprises magnesium oxide and manganese oxide in a molar proportion of 1+x magnesium oxide to 1-x manganese oxide.
17. The method according to any of claims 6 to 16, wherein the plurality of milling balls comprises tungsten carbide.
18. The method according to claim 17, wherein the high-energy milling is performed within a bail mill jar being made of a material comprising tungsten carbide.
19. The method according to any of claims 6 to 16, wherein the plurality of milling balls comprises zirconium oxide.
20. The method according to claim 19, wherein the high-energy milling is performed within a ball mill jar being made of a material comprising zirconium oxide.
21. The method according to any of claims 6 to 20, wherein each of the plurality of milling balls has a diameter of 0.5 mm to 1 cm.
22. A cathode comprising the cathode composition according to any of claims 1 to 5.
23. An electrochemical cell comprising a cathode according to claim 22, an electrolyte and an anode.16
Citation Information
Patent Citations
Cathode active material containing magnesium-transition metal composite oxide and magnesium secondary battery using the same
US20190296326A1