Scalable corrosion-conversion method for three-dimensional structuring and chemical passivation of metal current collectors

IN606936BActive Publication Date: 2026-10-23INDIAN INSTITUTE OF TECHNOLOGY BOMBAY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202621015473
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2026-02-12
Publication Date
2026-10-23
Estimated Expiration
2046-02-12

AI Technical Summary

Technical Problem

Existing rechargeable battery technologies face challenges with non-uniform metal nucleation, dendritic growth, parasitic reactions, electrolyte degradation, and corrosion issues at the anode interface, particularly in lithium-ion, sodium-ion, and zinc-ion batteries, which are not adequately addressed by current vacuum-deposited coatings and alloy interlayers.

Method used

A controlled corrosion-conversion process transforms the surface of metal current collectors into a three-dimensional porous layer that undergoes electrochemical conversion during cycling, forming a chemically bonded, ion-conductive passivation interphase that stabilizes metal deposition and suppresses parasitic reactions.

Benefits of technology

The method enables uniform metal deposition, improved Coulombic efficiency, and enhanced cycling stability across multiple battery chemistries without requiring vacuum deposition or electrolyte additives, while maintaining mechanical integrity and ionic transport.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to electrochemical energy storage systems, and more particularly to surface engineering of metal foil current collectors through controlled corrosion-conversion processes. The present invention provides a scalable, solution-phase corrosion-conversion methodology for modifying metal current collectors. Copper and aluminum current collectors are engineered for use in lithium- and sodium-based batteries, while zinc current collectors are specifically engineered for aqueous zinc-ion batteries. The corrosion process creates a porous surface layer of controlled thickness and speciation, which undergoes electrochemical conversion during cycling to form a chemically passivating, ion-conductive interphase that stabilizes metal deposition and improves Coulombic efficiency. Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

FIELD OF THE INVENTION:The present invention relates to electrochemical energy storage systems, and moreparticularly to surface engineering of metal foil current collectors throughcontrolled corrosion-conversion processes. Specific fields of application includelithium-ion batteries, sodium-ion batteries, anodeless and anode-free batteryarchitectures, zinc-ion batteries, solid-state batteries employing ceramic or polymerelectrolytes, and liquid-electrolyte-based rechargeable battery systems. Theinvention further relates to scalable manufacturing methods for current collectormodification compatible with industrial roll-to-roll processing.BACKGROUND OF THE INVENTION:Rechargeable batteries based on lithium, sodium, and zinc chemistries are centralto modern energy storage technologies. In anodeless / anode-free / "excess-Li / Na / Znfree" and metal-plating battery architectures, metal current collectors serve assubstrates for in situ metal deposition during charging. However, freshly depositedmetals often exhibit non-uniform nucleation, dendritic growth, and parasitic sidereactions with the electrolyte. In solid-state batteries, these reactions can lead torapid degradation of solid electrolytes such as NASICON-type, argyrodite, halide,or polymer electrolytes. In liquid electrolyte systems, uncontrolled metal depositioncompromises safety and cycling efficiency. Existing mitigation strategies rely onvacuum-deposited coatings, alloy interlayers, polymer films, or electrolyteadditives, which add cost, complexity, and are often chemistry-specific. In aqueouszinc-ion batteries, zinc current collectors and electrodes additionally suffer fromcorrosion, hydrogen evolution, and shape change during cycling. Accordingly,there is a need for a simple, scalable, and chemistry-agnostic surface engineeringapproach that enables controlled morphology and chemical passivation of metalcurrent collectors.Problem Addressed by the InventionDespite significant advances in rechargeable battery technologies, the performanceand reliability of "beyond lithium-ion" technologies such as sodium-ion, solid-statelithium / sodium or aqueous zinc-based batteries remain limited by interfacialinstabilities at the anode. In metal-plating and anodeless battery architectures,freshly deposited metal often nucleates non-uniformly on the current collectorsurface, leading to dendritic growth, parasitic side reactions, and continuous loss ofactive metal. These issues result in low Coulombic efficiency, rapid capacity fade,and safety concerns.In solid-state battery systems, direct contact between plated metal and solidelectrolytes lead to chemical reduction of the electrolyte, interphase thickening,increased impedance, and mechanical degradation. In liquid electrolyte systems,uncontrolled metal deposition and electrolyte decomposition further compromisecycling stability. In aqueous zinc-ion batteries, zinc current collectors andelectrodes additionally suffer from corrosion, hydrogen evolution, and shapechange during repeated plating and stripping.Existing approaches to address these challenges typically rely on vacuum-depositedcoatings, metallic alloy interlayers, polymer films, or electrolyte additives. Suchmethods are often material-specific, cost-prohibitive, difficult to scale, andincompatible with multiple battery chemistries. Accordingly, there exists a need fora simple, scalable, and chemistry-agnostic strategy that enables simultaneouscontrol over the surface morphology and surface chemistry of metal currentcollectors to achieve stable, reversible metal deposition across diverse batterysystems.CN118645637A discloses AgF / Ag-C composite coatings on copper currentcollectors with prelithiation. The approach requires external coating layers,composite binders, and pre-lithiation, resulting in a thick artificial interphase.WO2024 / 101510A1 describes Zr-based amorphous alloy interlayers deposited bysputtering. This method relies on vacuum-based deposition and produces a staticalloy layer that is chemistry-specific.US2022 / 223868A1 involves sputtered two-dimensional material coatings withoptional metal interlayers. The process requires sputtering or chemical vapordeposition, yielding laminated layers without intrinsic surface transformation.CN118231670A provides lithiophilic metal nanoparticle layers to guide lithiumnucleation. This technique depends on foreign nanoparticles and alloying, withinterlayer consumption occurring during cycling.US2020 / 0144599A1 discloses polymer-bound composite coatings incorporatingconductive fillers. These binder-based laminated coatings involve multistepfabrication and present risks of delamination.US2023 / 0231143A1 describes graphene / graphene oxide slurry coatings withlithiophilic metal additives. The slurry-casting approach is additive-dependent andresults in a static layered architecture.CN115275212B describes CNT-Cu composite current collectors. This methodinvolves bulk composite metallurgy and complex fabrication processes.CN112259743A provides sol-gel derived polymer coatings on current collectors.The coatings require heat treatment and introduce foreign polymer phases.CN117117199A discloses chemical silver soaking and post-treatment forlithiophilicity. This approach relies on deposited silver layers and subsequent heattreatment.Prior approaches rely on additive coatings, alloy layers, or external pressure,externally deposited metallic, polymeric, or composite coatings on currentcollectors. These include sputtered metallic layers, slurry-cast composite films, andpolymer-bound conductive coatings. Such approaches introduce laminated layersthat require vacuum processing, binders, or multistep fabrication, and are prone todelamination and scalability challenges.Other prior art strategies employ alloy-forming or lithiophilic metals to reducenucleation overpotential. These methods depend on alloy formation and gradualconsumption of the interlayer, limiting long-term stability and cross-chemistryapplicability.Several disclosures rely on high external stack pressure to maintain interfacialcontact and suppress degradation in solid-state batteries. Such approaches increasesystem complexity and are unsuitable for practical large-format cells.Existing aqueous zinc-ion battery literature emphasizes electrolyte additives,polymer coatings, or artificial SEI layers. These methods are chemistry-specific anddo not involve intrinsic transformation of the zinc current collector surface.Prior art does not involve controlled chemical corrosion of the current collectoritself to generate a three-dimensional porous surface layer that subsequentlyconverts during battery operation into a chemically passivating, ion-conductiveinterphase.Solution provided by the InventionThe present inventors have found that the above-mentioned problems may beaddressed by a controlled corrosion-conversion methodology for engineering metalfoil current collectors. In this approach, the surface of a metal current collector issubjected to a controlled chemical corrosion process that generates a threedimensional porous surface layer with tailored chemical speciation. The corrosion-derived layer is chemically bonded and, therefore, well adhered to the underlyingmetal and serves as a precursor interphase.During subsequent electrochemical cycling in a battery cell, the corrosion-derivedsurface species undergo conversion reactions with plated metal ions, resulting inthe formation of a stable, ion conductive, and chemically passivating interphase.This passivation layer regulates metal nucleation and growth, suppresses parasiticinterfacial reactions, and accommodates volume changes during repeated metalplating and stripping.The methodology is applicable to copper and aluminum current collectors used inlithium-ion and sodium-ion batteries, and to zinc current collectors used in aqueouszinc-ion batteries. The approach is compatible with both solid-state and liquidelectrolyte systems and does not require vacuum deposition, external coatings, orelectrolyte-specific additives. As a result, the invention enables uniform metaldeposition, improved Coulombic efficiency, enhanced cycling stability, andscalable manufacturing across multiple battery chemistries.The present invention is characterized by the implementation of a controlledcorrosion-conversion process that enables the simultaneous engineering of threedimensional surface morphology and tailored surface chemistry directly on metalcurrent collectors. Unlike prior approaches that deposit external coatings orinterlayers, the invention generates an in situ, chemically bonded porous layer thatsubsequently converts during battery operation into a stable, ion-conductivepassivation interphase. The method is adaptable across multiple metals and batterychemistries while maintaining a single underlying process principle.The present invention is fundamentally differentiated from prior art approaches thatrely on externally deposited coatings, interlayers, or films. Instead of addingmaterial onto the current collector surface, the present invention deliberatelyconverts the surface of the metal current collector itself through a controlledcorrosion process, followed by electrochemical conversion during batteryoperation. This intrinsic surface transformation results in a chemically bondedinterphase intrinsically integrated with the underlying metal. This approach ensuresrobust adhesion, and mechanical integrity that cannot be replicated by physicaldeposition techniques.Unlike patterned, templated, or fabricated three dimensional current collectors, thepresent invention through the corrosion process generates three-dimensionalporosity in situ through chemical corrosion directly on the current collector surface.The resulting porous architecture is inherently conformal, continuous, and welladhered to the underlying metal, eliminating the need for lithography, templating,sintering, or additive manufacturing.The interfacial layer in the present invention is not static. The corrosion-derivedsurface species are intentionally designed to undergo electrochemical conversionduring initial and subsequent cycling, evolving into a stable, ion-conductivepassivation layer. This dynamic evolution distinguishes the invention from staticartificial interlayers that do not adapt to electrochemical operating conditions.Prior art interlayers often prioritize chemical stability at the expense of ionictransport, or vice versa. The present invention uniquely achieves chemicalpassivation while retaining ion conductivity by forming conversion-derived phases(such as metal oxides and metal fluorides) that suppress parasitic reactions whilemaintaining efficient ion transport (i.e. without blocking metal-ion transport).Many solid-state battery interface solutions depend on elevated stack pressure tomaintain contact, suppress void formation, or prevent interfacial degradation. Incontrast, the present invention achieves interfacial stabilization through intrinsicsurface chemistry and morphology, enabling effective operation under ambientpressure conditions.Although the resulting interphase exhibits complex three-dimensional morphologyand multi-component chemical speciation, the fabrication method itself isintentionally simple, relying on solution-phase chemical processing. Thiscombination of high functional sophistication with low manufacturing complexityis a defining differentiator.The present invention does not rely on specific electrolyte formulations, additives,or decomposition products to form the passivation layer. Instead, interfacialstabilization originates from the engineered current collector surface itself. Thisdecouples interfacial stability from electrolyte chemistry and enables broadcompatibility with solid-state and liquid electrolyte systems.Finally, the corrosion-conversion principle is applicable to copper and aluminiumcurrent collectors for lithium- and sodium-based, batteries, and to zinc currentcollectors for aqueous zinc-ion batteries. This unified strategy contrasts with priorart solutions that are narrowly tailored to a single metal or battery chemistry.The corrosion-conversion derived interphase intrinsically limits continuouselectrolyte reduction and metal corrosion by forming a chemically stable barrier atthe current collector interface.Because the passivation interphase is derived from the underlying metal currentcollector, it exhibits superior adhesion and mechanical integrity compared tolayered or laminated coatings. This reduces the risk of delamination, cracking, orloss of contact during repeated metal plating and stripping.The present invention does not rely on alloy formation between deposited metal andlithiophilic or sodiophilic elements to reduce nucleation overpotential. Instead,stabilization is achieved through controlled surface chemistry and morphology,providing a fundamentally different mechanism from alloy-based interlayers.By intrinsically suppressing parasitic reactions and avoiding alloy-basedinterlayers, the present invention provides a unified, scalable, and robust strategyfor enhancing battery interfaces with robust adhesion, superior mechanical integrityand electrochemical performance. The ability to stabilize metal deposition withoutvacuum deposition, alloy layers, electrolyte additives, or external pressurerepresents a significant technical advancement.OBJECTS OF THE INVENTION:It is an object of the present invention to provide a current collector modificationmethodology that enables simultaneous control of surface morphology and surfacechemistry through a single corrosion-conversion process, thereby generating athree-dimensional porous structure and a chemically passivating surface interphase.It is another object of the present invention to provide an in-situ formed passivationlayer derived from corrosion-generated surface species during electrochemicalcycling, wherein the passivation layer is chemically bonded to the underlyingcurrent collector and exhibits improved mechanical robustness and adhesion.It is another object of the present invention to provide a solution-phase corrosion-conversion methodology that is scalable and compatible with existing metal foilprocessing infrastructure, enabling uniform treatment over large surface areassuitable for industrial-scale battery manufacturing.It is another object of the present invention to provide a modified current collectorthat promotes uniform metal nucleation and deposition and suppresses parasiticinterfacial reactions, thereby improving Coulombic efficiency during metal platingand stripping, particularly under metal-limited or anodeless battery configurations.It is another object of the present invention to provide an ion-conductive passivationinterphase formed by electrochemical conversion of corrosion-derived surfacespecies, wherein the interphase provides chemical stability without substantiallyimpeding ionic transport.It is another object of the present invention to provide a current collectormodification strategy that is compatible with a broad range of electrolytechemistries, including solid-state electrolytes and liquid electrolytes.It is yet another object of the present invention to provide enhanced interfacialstability in anodeless, anode-free, or metal-plating battery configurations bysuppressing irreversible metal consumption and interfacial degradation.SUMMARY OF THE INVENTION:According to an aspect of the present invention there is provided a method formodifying metal foil current collectors for rechargeable electrochemical cells, themethod comprising:i. subjecting the surface of the metal foil current collector to a controlledchemical corrosion using a reactive solution comprising a hydrolyticallyunstable salt selected from lithium hexafluorophosphate (LiPF6) or sodiumhexafluorophosphate (NaPF6) in an organic solvent;ii. heating said salt with water under stirring to generate a hydrofluoric acid(HF)-containing corrosion solution, the solution further comprising lithiumfluoride (LiF) or sodium fluoride (NaF);iii. converting the surface of the metal current collector into a porous layer byexposure to the corrosion solution, thereby generating three-dimensionalporosity in situ through chemical corrosion, wherein the pore comprisescorrosion-derived surface species chemically bonded to the underlying metal;andiv. during subsequent electrochemical cycling of the cell, transforming thecorrosion-derived surface species through reactions with plated metal speciespresent in the electrochemical cell to form an ion-conductive passivationinterphase chemically bonded to the current collector, wherein the passivationinterphase suppresses parasitic interfacial reactions and promotes uniformmetal deposition.According to another aspect of the present invention there is provided a currentcollector for a rechargeable electrochemical cell, comprising a corrosion-derivedporous surface layer that is configured to undergo chemical and / or electrochemicalconversion during electrochemical cycling of the cell to form a chemically bonded,ion-conductive passivation interphase.BRIEF DESCRIPTION OF FIGURES:Figure 1 illustrates Schematic illustration of electrochemical passivation ofcorroded Cu in an anodeless solid-state half-cell.Figure 2 illustrates Top-view FE-SEM image of corroded Cu foil.Figure 3 illustrates FIB-SEM cross-section image of corroded Cu foil.Figure 4 illustrates Relative distribution of Cu-species obtained from XPSquantification.Figure 5A illustrates Galvanostatic charge-discharge (GCD) profile of theanodeless solid-state half-cell with corroded Cu electrode at a current density of 60μA cm-2 and constant lithium plating capacity of 1.2 mAh cm-2.Figure 5B illustrates GCD profile for control experiment with bare Cu foil underidentical conditions.Figure 6A illustrates Coulombic efficiency versus cycle number plot for corrodedCu electrode.Figure 6B illustrates Coulombic efficiency versus cycle number plot for bare Cuelectrode.DETAILED DESCRIPTION OF THE INVENTIONThe following description with reference to the accompanying drawings is providedto assist in a comprehensive understanding of exemplary embodiments of theinvention. It includes various specific details to assist in that understanding butthese are to be regarded as merely exemplary.Accordingly, those of ordinary skill in the art will recognize that various changesand modifications of the embodiments described herein can be made withoutdeparting from the scope of the invention. In addition, descriptions of well-knownfunctions and constructions are omitted for clarity and conciseness.The terms and words used in the following description and claims are not limitedto the bibliographical meanings, but, are merely used by the inventor to enable aclear and consistent understanding of the invention. Accordingly, it should beapparent to those skilled in the art that the following description of exemplaryembodiments of the present invention are provided for illustration purpose only andnot for the purpose of limiting the scope of the invention as defined by the appendedclaims and their equivalents.It is to be understood that the singular forms "a," "an," and "the" include pluralreferents unless the context clearly dictates otherwise.Features that are described and / or illustrated with respect to one embodiment maybe used in the same way or in a similar way in one or more other embodimentsand / or in combination with or instead of the features of the other embodiments.It should be emphasized that the term "comprises / comprising" when used in thisspecification is taken to specify the presence of stated features, steps or componentsbut does not preclude the presence or addition of one or more other features, steps,components or groups thereof.The present invention relates to electrochemical energy storage systems, and moreparticularly to surface engineering of metal foil current collectors throughcontrolled corrosion-conversion processes. Specific fields of application includelithium-ion batteries, sodium-ion batteries, anodeless and anode-free batteryarchitectures, zinc-ion batteries, solid-state batteries employing ceramic or polymerelectrolytes, and liquid-electrolyte-based rechargeable battery systems. Theinvention further relates to scalable manufacturing methods for current collectormodification compatible with industrial roll-to-roll processing.The present invention provides a scalable, solution-phase corrosion-conversionmethodology for modifying metal current collectors. Copper and aluminum currentcollectors are engineered for use in lithium- and sodium-based batteries, while zinccurrent collectors are specifically engineered for aqueous zinc-based batteries. Thecorrosion process creates a porous surface layer of controlled thickness andspeciation, which undergoes electrochemical conversion during cycling to form achemically passivating, ion-conductive interphase that stabilizes metal depositionand improves Coulombic efficiency.The method comprises controlled chemical corrosion of a metal current collectorusing a reactive solution comprising of a hydrolytically unstable salt, viz. LiPF6 orNaPF6, which is heated with an optimal amount of water to create an Hydrofluoricacid (HF)-containing corrosion solution that also contains LiF or NaF, to partiallyconvert the surface of the metal current collector into a porous layer. Processparameters such as water content (0.0025 M to 0.2 M), overall solution compositioncomprising LiPF6 or NaPF6, exposure time (0.2 to 12 hours), temperature (45°C to80°C) and stirring rate (200-1000 rpm) are adjusted to tune porosity, surfacecomposition, and reaction depth. During subsequent electrochemical cycling, thecorrosion-derived surface species undergo conversion reactions with plated metalspecies, forming a stable passivation interphase that suppresses parasitic reactionsand promotes uniform metal deposition.In an embodiment of the present invention there is provided a method for modifyingmetal foil current collectors for rechargeable electrochemical cells, the methodcomprising:i. subjecting the surface of the metal foil current collector to a controlledchemical corrosion using a reactive solution comprising a hydrolyticallyunstable salt selected from lithium hexafluorophosphate (LiPF6) or sodiumhexafluorophosphate (NaPF6) in an organic solvent;ii. heating said salt with water under stirring to generate a hydrofluoric acid(HF)-containing corrosion solution, the solution further comprising lithiumfluoride (LiF) or sodium fluoride (NaF);iii. converting the surface of the metal current collector into a porous layer byexposure to the corrosion solution, thereby generating three-dimensionalporosity in situ through chemical corrosion, wherein the pore comprisescorrosion-derived surface species chemically bonded to the underlying metal;andiv. during subsequent electrochemical cycling of the cell, transforming thecorrosion-derived surface species through reactions with plated metal speciespresent in the electrochemical cell to form an ion-conductive passivationinterphase chemically bonded to the current collector, wherein the passivationinterphase suppresses parasitic interfacial reactions and promotes uniformmetal deposition.In another embodiment of the present invention, Lithium hexafluorophosphate(LiPF6) or sodium hexafluorophosphate (NaPF6) in a carbonate-based organicsolvent with specific amount of water is employed, wherein the carbonate-basedorganic solvent is selected from ethylene carbonate, dimethyl carbonate, diethylcarbonate, or propylene carbonate.In another embodiment of the present invention, the metal current collectorcomprises copper or aluminum foil. The surface of the foil is subjected to controlledchemical corrosion to produce a porous layer. The corrosion-derived layercomprises metal oxides, fluorides, hydroxides, and mixed alkali-containing species.During electrochemical cycling, these species undergo further conversion to forma chemically bonded, ion-conductive passivation interphase. Such modified copperand aluminum current collectors are suitable for use in lithium and sodium-basedbatteries, providing enhanced interfacial stability and suppression of parasiticreactions.In another embodiment of the present invention, the metal current collectorcomprises zinc foil. Controlled corrosion of the zinc surface produces a porous layercomprising zinc oxides, zinc hydroxides, and zinc fluorides. Duringelectrochemical cycling in an aqueous zinc-ion battery, this porous layer regulateszinc deposition, suppresses uncontrolled corrosion, and evolves into a stable,ion-conductive passivation interphase. The resulting interface improves cyclingefficiency and mechanical integrity compared to untreated zinc foils. Such modifiedzinc current collectors are suitable for use in aqueous zinc-ion batteries, providingenhanced interfacial stability and suppression of parasitic reactions.In another embodiment of the present invention, the corrosion process is conductedat a temperature between 45°C to 80°C.In another embodiment of the present invention, the the exposure time to thecorrosion solution is between 0.2 to 12 hours, preferably 4 hours, to obtain a threedimensionally porous surface layer of thickness in the range of 0.05 to 20 μm,preferably 10 μm.In yet another embodiment of the present invention, the corrosion-derived surfacespecies comprise metal oxides, hydroxides, halides of the metal foil current+collector and mixed alkali-metal-containing surface species formed duringoperation of the electrochemical cell.In another embodiment of the present invention, the metal ions are selected fromLi+, Na+, or Zn2+.In another embodiment of the present invention, the passivation interphasecomprises at least one ion-conductive inorganic compound selected from Li2O, LiF,Na2O, NaF, or ZnO.In another embodiment of the present invention, the metal is plated inside the poresof the current collector during the first electrochemical charge.In another embodiment of the present invention, the passivation interphase ischemically bonded to the underlying metal of the current collector and suppressesparasitic interfacial reactions while allowing ionic transport.In another embodiment of the present invention, the porous layer has a depth or sizein the range of 0.05 to 20 μm such that it accommodates reversible metal platingand stripping without blocking ion transport.In an embodiment of the present invention, the corrosion step is carried out atambient temperature and pressure.In an embodiment of the present invention, there is provided a current collector fora rechargeable electrochemical cell, comprising a corrosion-derived porous surfacelayer that is configured to undergo chemical and / or electrochemical conversionduring electrochemical cycling of the cell to form a chemically bonded,ion-conductive passivation interphase.In further embodiment of the present invention, there is provided a batterycomprising:i. a counter electrode, which is either metal foil or cathode-active material;ii. a separator;iii. an electrolyte; andiv. current collector as claimed in claim 13;wherein the said current collector possesses a modified surface morphology thatsuppresses interfacial degradation between the electrolyte and the current collector.In an embodiment of the present invention, the counter electrode comprises eitherlithium foil or sodium foil or zinc foil, or a cathode-active material selected fromlithium iron phosphate or lithium nickel manganese cobalt oxide for lithium-ionbatteries, and sodium nickel iron oxide, sodium vanadium phosphate or sodiumvanadium fluorophosphate for sodium-ion batteries, and bromine, manganesedioxide, vanadium dioxide etc. for zinc-ion batteries,The separator comprises a glass fiber (GF) or polymer based separator suchas polypropylene, andThe electrolyte comprises a solid electrolyte selected from lithiumaluminum titanium phosphate, argyrodite, lithium phosphosulfides, lithiumtransition metal halides for lithium-ion batteries, and sodium phosphosulfides,sodium antimony sulfide, sodium tantalum oxychlorides for sodium-ion batteriesor a liquid electrolyte selected from Lithium hexafluorophosphate (LiPF6) orLithium bis(trifluoromethanesulfonyl)imide (LiTFSI), Lithiumbis(fluorosulfonyl)imide (LiFSI) in a mixture of organic carbonate solvents such asethylene carbonate, propylene carbonate, diethyl carbonate, dimethyl carbonate forlithium-ion batteries, and Sodium hexafluorophosphate (NaPF6) or Sodiumbis(trifluoromethanesulfonyl)imide (NaTFSI), Sodium bis(fluorosulfonyl)imide(NaFSI) in a mixture of organic carbonate solvents such as ethylene carbonate,propylene carbonate, diethyl carbonate, dimethyl carbonate, diglyme, tetraglymeand zinc triflate, zinc sulfate, zinc acetate etc. in de-ionized water for zinc-ionbatteries.EXAMPLES:The following examples are meant to illustrate the present invention. The examplesare presented to exemplify the invention and are not to be considered as limitingthe scope of the invention.EXAMPLE 1:METHODOLOGYCorrosion composition details:Lithium hexafluorophosphate (LiPF6) or sodium hexafluorophosphate (NaPF6) in acarbonate-based organic solvent (ethylene carbonate (EC), dimethyl carbonate(DMC), diethyl carbonate, propylene carbonate etc) with specific amount of water(0.0025 to 0.2 M) is employed.Example 1:A corrosion solution is prepared by dissolving lithium hexafluorophosphate (LiPF6)at a concentration of 1.0 M in a solvent comprising a mixture of ethylene carbonate(EC) and diethyl carbonate in a 1:1 mixture. Water is introduced into the solutionat a concentration ranging from 0.0025 M to 0.2 M, preferably 0.1 M and themixture was heated between 45°C and 80°C, preferably 60°C under continuousstirring at 200-1000 rpm, preferably 450 rpm. Under these conditions, the PF6-anion undergoes hydrolysis, generating hydrogen fluoride (HF) and phosphorylfluoride (POF3), which act as corrosive agents toward metallic substrates such asLithium, aluminum or zinc current collectors.Example 2:A corrosion solution is prepared by dissolving sodium hexafluorophosphate(NaPF6) is dissolved at a concentration of 1.0 M in a mixed solvent comprisingpropylene carbonate (PC). Water is introduced into the solution at a concentrationof 0.2 M and the mixture was heated at 60°C under continuous stirring at 600 rpm.Hydrolysis of the PF6- anion under these conditions produces HF and relatedspecies, which induce corrosion of metallic surfaces and accelerate electrolytedegradation.Corrosion method details:Example 3:A corrosion solution was prepared according to example 1 or example 2. A metalcurrent collector, copper or aluminium or zinc foil, was exposed to this solution fora controlled duration of 4 hours. Upon exposure, the surface of the current collectorunderwent chemical corrosion, resulting in the in situ formation of a porous layer.The porous structure comprised corrosion-derived surface species that werechemically bonded to the underlying metal, thereby generating three-dimensionalporous surface layer of 10 μm thickness. During subsequent electrochemicalcycling of the cell, these corrosion-derived surface species reacted with plated metalions present in the electrolyte. This transformation produced an ion-conductivepassivation interphase that was chemically bonded to the current collector. Thepassivation interphase suppressed parasitic interfacial reactions and facilitateduniform deposition of the plated metal, thereby improving the stability andperformance of the electrochemical cell.RESULTS AND DISCUSSIONFigure 1 illustrates Schematic illustration of electrochemical passivation ofcorroded Cu in an anodeless solid-state half-cell. The diagram explains theproposed mechanism by which the corroded surface stabilizes lithium plating.Figure 2 illustrates Top-view FE-SEM image of the corroded Cu foil. Themicrostructural features and surface roughness are revealed, offering insight intothe morphology resulting from the corrosion process.Figure 3 illustrates FIB-SEM cross-section image of the corroded Cu foil. Thisfigure shows subsurface structural modifications, including depth of corrosion andlayered changes within the foil.Figure 4 illustrates Relative distribution of Cu-species obtained from XPSquantification. The plot identifies chemical states and oxidation levels of copper,confirming the transformation of surface species during corrosion.Figure 5A illustrates Galvanostatic charge-discharge (GCD) profile of theanodeless solid-state half-cell with corroded Cu electrode at 60 μA cm-2 currentdensity and 1.2 mA cm-2 lithium plating capacity. This figure demonstrates theelectrochemical behavior and stability of the modified electrode.Figure 5B illustrates GCD profile for the control experiment with bare Cu foil underidentical conditions.The comparison of Figure 5A and Figure 5B highlights the differences inperformance between untreated and corroded electrodes.The galvanostatic charge-discharge comparison shows that the corroded Cuelectrode with a corrosion-derived passivation interphase exhibits significantlyimproved lithium plating / stripping stability, lower overpotential, and consistentcapacity retention over 20 cycles, whereas the bare Cu foil shows poor nucleation,increased polarization, and rapid capacity fading. This confirms that the corrosionmodified current collector effectively suppresses parasitic interfacial reactions andpromotes uniform metal deposition, in line with the objectives of the presentinvention.Figure 6A illustrates Coulombic efficiency versus cycle number plot for thecorroded Cu electrode. The data shows improved cycling stability and efficiency,supporting the role of corrosion-induced passivation.Figure 6B illustrates Coulombic efficiency versus cycle number plot for the bareCu electrode. This serves as a baseline, illustrating the lower efficiency and stabilityof untreated copper compared to the corroded sample.The Coulombic efficiency comparison demonstrates that the corroded Cu electrodewith corrosion-derived passivation interphase achieves high and stable efficiency(~90-95%) over 35 cycles, whereas the bare Cu foil exhibits extremely low andunstable efficiency, dropping near zero after a 18 cycles. This confirms that thecorrosion-modified current collector significantly suppresses parasitic interfacialreactions and enables reversible metal plating / stripping, in line with the objectivesof the present invention.Advantages of the Invention:The present invention offers several technical, manufacturing, and performanceadvantages over existing current collector modification and interfacial engineeringstrategies for rechargeable batteries.1. Simultaneous Control of Surface Morphology and Surface Chemistry:Unlike prior approaches that focus solely on either morphological structuring orchemical passivation, the present invention enables simultaneous control overthree-dimensional surface porosity and surface chemical speciation through asingle corrosion-conversion process. The corrosion step generates a porousarchitecture that accommodates metal deposition, while subsequentelectrochemical conversion produces a chemically passivating interphase.2. In Situ Formation of a Chemically Bonded Passivation Layer: Thepassivation interphase is not externally deposited but is formed in situ fromcorrosion-derived surface species during electrochemical cycling. This results ina chemically bonded, mechanically robust interphase that exhibits superioradhesion to the underlying current collector compared to physically depositedcoatings or laminated interlayers.3. Elimination of Vacuum-Based and Gas-Phase Deposition Techniques: Theinvention avoids the use of sputtering, atomic layer deposition, chemical vapordeposition, or other vacuum-based coating techniques commonly employed inprior art. This significantly reduces capital cost, process complexity, andmanufacturing constraints, enabling direct compatibility with large-area androll-to-roll processing.4. Scalability and Manufacturing Compatibility: The solution-phase corrosionconversion methodology is inherently scalable and compatible with existingmetal foil processing infrastructure. The process can be applied uniformly overlarge areas without requiring specialized equipment, making it suitable forindustrial-scale battery manufacturing.5. Improved Metal Deposition Uniformity and Coulombic Efficiency: Thecorrosion-induced three dimensional porous structure promotes homogeneousmetal nucleation and deposition, while the conversion-derived passivation layersuppresses continuous parasitic reactions. As a result, the invention enablessignificantly improved Coulombic efficiency during metal plating and stripping,particularly under metal-limited conditions such as anodeless / anode-free or'excess Li / Na / Znfree' and zinc-based battery configurations.6. Formation of Ion-Conductive Passivation Interphases: The electrochemicalconversion of corrosion-derived surface species results in passivation layers richin ion-conductive components (for example, lithium oxide and lithium fluoridein lithium-based systems). These interphases provide chemical stability withoutseverely impeding ionic transport, unlike many dense or electronically insulatingartificial coatings.7. Operation under Ambient Temperature and Pressure: The invention enablesstable battery operation under ambient temperature and pressure conditions.Unlike many prior art systems that require elevated stack pressure or temperatureto maintain interfacial contact and suppress degradation, the present approachachieves improved cycling stability without external mechanical constraints.8. Broad Electrolyte Compatibility: The methodology is agnostic to electrolytechemistry and is compatible with solid-state electrolytes (including NASICONtype, argyrodite, halide, polymer, and composite electrolytes) as well asconventional liquid electrolytes. This flexibility allows the same currentcollector engineering strategy to be deployed across diverse batteryarchitectures.9. Applicability Across Multiple Battery Chemistries: The invention isapplicable to copper and aluminium current collectors used in lithium-ion,sodium-ion, and zinc-ion batteries, and to zinc current collectors used in zincion batteries. This broad applicability distinguishes the invention fromchemistry-specific interlayers or coatings and enables platform-leveldeployment.10. Reduced Dependence on Electrolyte Additives and Interlayers: Byengineering the current collector interface directly, the invention reduces oreliminates reliance on electrolyte additives, polymer binders, or multilayerinterfacial stacks to achieve interfacial stability. This simplifies cell design andimproves reproducibility.11. Enhanced Interfacial Stability in Anodeless and Metal-PlatingArchitectures: The invention is particularly advantageous for theanodeless / anode-free or 'excess Li / Na / Zn-free' and metal plating batteryconfigurations, where limited metal inventory amplifies the consequences ofinterfacial inefficiency. The corrosion-conversion derived interphasesignificantly suppresses irreversible metal consumption and interfacialdegradation.12. Generalizable Process Principle: Although specific embodiments may employparticular metals or corrosion chemistries, the underlying principle: controlledcorrosion to generate a porous, reactive surface followed by electrochemicalconversion to a stable passivation layer, is general and adaptable. This allowsfuture extensions of the invention to additional metals, electrolytes, and batterysystems without departing from the core inventive concept.It is to be understood that the present invention is susceptible to modifications,changes and adaptations by those skilled in the art. Such modifications, changes,adaptations are intended to be within the scope of the present invention.

Claims

1. A method for modifying metal foil current collectors for rechargeable electrochemical cells, the method comprising: i. subjecting the surface of the metal foil current collector to a controlled chemical corrosion using a reactive solution comprising a hydrolytically unstable salt selected from lithium hexafluorophosphate (LiPF6) or sodium hexafluorophosphate (NaPF6) in an organic solvent; ii. heating said salt with water under stirring to generate a hydrofluoric acid (HF)-containing corrosion solution, the solution further comprising lithium fluoride (LiF) or sodium fluoride (NaF); iii. converting the surface of the metal current collector into a porous layer by exposure to the corrosion solution, thereby generating three-dimensional porosity in situ through chemical corrosion, wherein the pore comprises corrosion-derived surface species chemically bonded to the underlying metal; and iv. during subsequent electrochemical cycling of the cell, transforming the corrosion-derived surface species through reactions with plated metal species present in the electrochemical cell to form an ion-conductive passivation interphase chemically bonded to the current collector, wherein the passivation interphase suppresses parasitic interfacial reactions and promotes uniform metal deposition.

2. The method as claimed in claim 1, wherein the organic solvent is carbonatebased organic solvent selected from ethylene carbonate, dimethyl carbonate, diethyl carbonate, or propylene carbonate.

3. The method as claimed in claim 1, wherein the metal current collector comprises copper or aluminum and is used in lithium-ion or sodium-ion batteries.

4. The method as claimed in claim 1, wherein the metal current collector comprises zinc and is used in zinc-ion batteries.

5. The method as claimed in claim 1, wherein the corrosion process is conducted at a temperature between 45°C to 80°C.

6. The method as claimed in claim 1, wherein the exposure time to the corrosion solution is between 0.2 to 12 hours to obtain a three-dimensionally porous surface layer of thickness in the range of 0.05 to 20 μm.

7. The method as claimed in claim 1, wherein the corrosion-derived surface species comprise metal oxides, hydroxides, halides of the metal foil current collector and mixed alkali-metal-containing surface species formed during operation of the electrochemical cell.

8. The method as claimed in claim 1, wherein metal ions are selected from Li+, Na+, or Zn2+.

9. The method as claimed in claim 1, wherein the passivation interphase comprises at least one ion-conductive inorganic compound selected from Li2O, LiF, Na2O, NaF, or ZnO.

10. The method as claimed in claim 1, wherein metal is plated inside the pores of the current collector during the first electrochemical charge.

11. The method as claimed in claim 1, wherein the passivation interphase is chemically bonded to the underlying metal of the current collector and suppresses parasitic interfacial reactions while allowing ionic transport.

12. A current collector for a rechargeable electrochemical cell, comprising a corrosion-derived porous surface layer that is configured to undergo chemical and / or electrochemical conversion during electrochemical cycling of the cell to form a chemically bonded, ion-conductive passivation interphase.

13. A battery comprising: i. a counter electrode, which is selected from metal foil or cathode-active material; ii. a separator; iii. an electrolyte; and iv. current collector as claimed in claim 12; wherein the said current collector possesses a modified surface morphology that suppresses interfacial degradation between the electrolyte and the current collector.

14. The battery as claimed in claim 13, wherein the the counter electrode comprises either lithium foil or sodium foil or zinc foil, or a cathode-active material, the separator comprises a glass fiber (GF) separator or polymer based separator, and the electrolyte comprises a solid electrolyte or liquid electrolyte.

15. The battery as claimed in claim 14, wherein: i. cathode-active material is selected from: - lithium iron phosphate or lithium nickel manganese cobalt oxide for lithium-ion batteries; - sodium nickel iron oxide, sodium vanadium phosphate, or sodium vanadium fluorophosphate for sodium-ion batteries, and - bromine, manganese dioxide, vanadium dioxide for zinc-ion batteries, ii. polymer based separator is polypropylene, and iii. the electrolyte comprises: - a solid electrolyte selected from lithium aluminum titanium phosphate, argyrodite, lithium phosphosulfides, lithium transition metal halides for lithium-ion batteries, and sodium phosphosulfides, sodium antimony sulfide, sodium tantalum oxychlorides for sodiumion batteries or - a liquid electrolyte selected from: - Lithium hexafluorophosphate (LiPF6) or Lithium bis(trifluoromethanesulfonyl)imide (LiTFSI), Lithium bis(fluorosulfonyl)imide (LiFSI) in a mixture of organic carbonate solvents selected from ethylene carbonate, propylene carbonate, diethyl carbonate, dimethyl carbonate for lithium-ion batteries; - Sodium hexafluorophosphate (NaPF6) or Sodium bis(trifluoromethanesulfonyl)imide (NaTFSI), Sodium bis(fluorosulfonyl)imide (NaFSI) in a mixture of organic carbonate solvents selected from ethylene carbonate, propylene carbonate, diethyl carbonate, dimethyl carbonate, diglyme, and tetraglyme for sodium-ion batteries. and - Zinc triflate, zinc sulfate, zinc acetate in de-ionized water for zinc-ion batteries.