Method of patterning surface of substrate body and substrate body

JP2022044033A5Active Publication Date: 2024-11-06SCHOTT AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2021144037
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-02-26
Filing Date
2021-09-03
Publication Date
2024-11-06

AI Technical Summary

Technical Problem

Existing methods for patterning substrate surfaces, such as thermal separation using lasers, often fail to achieve the desired target surface due to uncontrollable mechanical or thermal damage, leading to inefficiencies and potential substrate destruction.

Method used

A method involving exposure of substrate material to an electromagnetic field in curved regions to induce nonlinear interactions, allowing precise control over the substrate material's alteration, including volume changes, cracks, and cavities, without mechanical stress, enabling flexible and efficient patterning.

Benefits of technology

This approach allows for the creation of predetermined, accurately formed surfaces on substrates, including thin and fragile materials, without mechanical stress, and enhances durability by avoiding micro-cracks, enabling efficient patterning of complex shapes and structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

To provide a method of preparing and / or executing patterning of a surface of a substrate body, capable of surely forming the substrate body on a scheduled surface, and a substrate body.SOLUTION: A method for preparing and executing patterning of a surface of a substrate body having a substrate material, in which the substrate material in at least one curved active region 7a-7c is exposed to an electromagnetic field causing non-linear interaction between the electromagnetic field and the substrate material in the working region to at least partially influence on the substrate material arranged in the active region; after patterning a characterized surface, the characterized surface has at least one first curved profile partially determined and / or influenced by the curved shape in at least one curved active region at least partial regionally, the nonlinear interaction causes at least one non-linear absorption of an electromagnetic field in the substrate material.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates to a method for preparing and / or performing patterning on the surface of a substrate body. The present invention further relates to the substrate body.

[0002] prior art Prior art has shown that separation processes for processing a starting substrate to form a predetermined surface such as a separation surface include scratching and breaking, wheel cutting, laser-assisted thermal separation (i.e., infusing the substrate with mechanical pre-damage and inducing cracks through a thermal stress field in the material), and laser-assisted perforation separation (i.e., filamentizing along the contour and then separating mechanically or thermally along the perforations).

[0003] However, these methods have the drawback that the desired target surface is often not achieved. This drawback is sometimes due to pre-damage intentionally introduced into the substrate material, but such damage cannot be adequately controlled.

[0004] Therefore, the objective of the present invention is to ensure that a predetermined surface is reliably formed on the substrate body.

[0005] Description of the present invention The problem is a method for preparing and / or performing a predetermined or predetermined characterized surface patterning of a substrate body having a substrate material, according to a first aspect of the present invention, The method involves exposing a substrate material in at least one curved operating region to an electromagnetic field that causes a nonlinear interaction between the electromagnetic field and the substrate material in each of the at least one curved operating region, thereby affecting the substrate material placed in the curved operating region at least partially. After patterning the characterized surface, the characterized surface has at least one first curved profile which is at least partially determined and / or influenced by the curved shape of at least one curved working region, This nonlinear interaction is resolved by proposing that it causes at least one nonlinear absorption of the electromagnetic field in the substrate material.

[0006] This method is based on the remarkable fact that the spatial extent of the electromagnetic field, and therefore the shape of individual curved regions of action, can be used to pre-define a planned surface, at least in its basic profile.

[0007] In other words, the substrate material is exposed to an electromagnetic field. In at least one region of the electromagnetic field, and this curved region, a nonlinear interaction occurs between the electromagnetic field and the substrate material. As a result, in this curved region, called the curved region of action, the substrate material placed in this region is at least partially affected.

[0008] Here, the affected areas of the substrate material can be understood to mean, for example, areas of volume change in the substrate material. The types of changes may include cracks, cavities, and / or structural changes in the substrate material, which will be etched away more quickly (compared to unaffected substrate material).

[0009] In this case, for example, an interface may exist between the affected substrate material and the unaffected substrate material. This corresponds to the surface of the curved region of action. This interface may extend entirely or partially into the substrate material. If a cavity is created by the nonlinear interaction, the interface may correspond to the surface of the cavity.

[0010] Therefore, the unaffected substrate material has a complementary shape to the curved region of action. In other words, the unaffected substrate material has a surface that locally interacts with the surface of the affected region in a shape-coupled manner.

[0011] By exposing and / or further processing this unaffected surface of the substrate material, a characterized surface can be provided while maintaining the imparted profile.

[0012] The formation of a curved area of ​​action is highly flexible because the region where the electromagnetic field can interact nonlinearly with the substrate material has a corresponding shape. Therefore, the curved area of ​​action can be defined and controlled by controlling the region through nonlinear interaction via the electromagnetic field. As a result, it is possible to pattern a surface characterized not only on the outside of the substrate body but also entirely or partially within the substrate body.

[0013] In one embodiment, the nonlinear interaction is achieved by the electromagnetic field having an intensity that results in a nonlinear interaction with the substrate material, at least in a partial region. In this case, the curved region of action is in a volume region where the corresponding high intensity exists.

[0014] For example, the curved working region may be entirely formed within the substrate, or it may extend from at least one surface of the substrate into the interior of the substrate body. In this case, the curved working region may extend to the other surface of the substrate body. Alternatively or additionally, the curved working region may intersect with another surface of the (unpatterned) substrate body, such as a side. The latter is particularly useful when it is desired to pattern the side of the substrate body. In this case, the curved working region may be formed within the substrate material so as to intersect with, for example, three sides of the unpatterned substrate body.

[0015] Thus, in this method, it is possible to prepare and / or carry out the patterning of a planned surface as the characterized surface of the substrate body particularly easily and efficiently. In so doing, the form of the affected substrate material can be selected almost arbitrarily. It is only necessary that a corresponding-shaped electromagnetic field be provided, by which the substrate material is (locally) exposed and can interact non-linearly.

[0016] The term "patterning of the characterized surface" is generally understood to mean forming a surface of the substrate body that did not exist prior to the change. Patterning can be carried out, for example, by operating on an existing surface, ultimately removing the substrate material in the surface area of the existing surface, so that as a result, a new surface is formed as the characterized surface. Patterning can also be carried out, for example, by separating a part of the substrate material from the substrate body along a planned surface, and thus exposing a new surface as the characterized surface. Of course, it is possible to transition smoothly between the case where an existing surface is still being operated on and the case where a part of the substrate material has already been separated.

[0017] However, this difference is not necessarily important in the following respect. Because in either case, the form of the curved action area is intended to (partially) determine or influence the profile of the interface between the affected and the non-affected substrate material, and thus the profile of the planned or characterized surface, and thus an impact is exerted on the substrate material of the substrate body.

[0018] Therefore, the material to be removed to pattern the characterized surface is preferably able to be removed from the original substrate body in a form different from powder form. This method is also applicable to rooms that require a high degree of cleanliness, such as clean rooms. For example, there are powders with a particle size of less than 10 nm.

[0019] In one embodiment, material is removed from the original substrate body in order to pattern the characterized surface.

[0020] In one embodiment, the material removed from the original substrate body to pattern the characterized surface is removed from the original substrate body in whole or in part as a continuous piece of material.

[0021] In this process, various types of characterized surfaces can be patterned. This makes it possible to provide substrate bodies that can be used for a variety of purposes.

[0022] For example, a nonlinear interaction can be induced in only one curved region of action. In this case, the substrate material is affected only in that region. For example, the affected substrate material can then be completely confined within the substrate material and not appear on the surface of the substrate body. Alternatively, the affected substrate material may appear on one or more surfaces of the substrate body, particularly two opposing surfaces. In this case, the affected substrate material extends from one surface to at least the other.

[0023] For example, nonlinear interactions can be induced in multiple curved action regions, and in each of those regions, the substrate material can be affected. In this case, the individual curved action regions may be, for example, continuous. In this case, the curved action regions may be offset from each other and / or rotated around the principal axis of each action region.

[0024] When a substrate material is affected in a curved region of action, the shape of the curved region of action (partially) determines or influences the first profile of the characterized surface. This is evident from the fact that the substrate material is affected in a curved volume region. The curved volume region has a surface that is simultaneously the interface with the unaffected substrate material. The surface region of the unaffected substrate material and the surface region of the volume region are exactly complementary (negative) to each other. Therefore, the shape of the curved region of action can co-determine or influence the surface region of the unaffected substrate material. As a result, the characterized surface is (partially) determined or influenced by the curved shape of the region of action.

[0025] This method can be carried out with optional additional measures, and as a result, microscopic cracks may not occur, or only occur slightly, in the characterized surface area from an overall perspective. Consequently, the strength of the characterized surface is high from the outset, and therefore the patterned substrate itself has excellent durability.

[0026] This method does not require the application of mechanical stress when separating a portion of the substrate material. Therefore, for example, it is possible to separate the substrate into two parts or remove a recess from the substrate without applying mechanical stress. As a result, the substrate itself is not subjected to stress and does not suffer any damage or special damage.

[0027] Therefore, the proposed method allows the starting substrate to be processed so that it is formed as a surface characterized by a predetermined or pre-defined surface, such as a separation surface.

[0028] Therefore, the present invention provides a substrate body in which its surface, particularly its circumferential side surface, has a predetermined target surface at least partially, and the surface may be advantageously etched as a whole. In this case, there is no need to apply a stress-inducing separation process.

[0029] As a result, the characterized surface can be formed with great precision.

[0030] In particular, this proposed method does not require the application of a polishing process to the patterned surface. Especially when the patterned surface is the entire or partial side of the substrate body, and especially in the case of thin substrate bodies, the polishing process cannot be performed, or if it can be performed, it is only possible under difficult conditions.

[0031] This is because the polishing process for substrate surfaces, especially the sides, requires high dimensional stability of the substrate and, correspondingly, sufficient thickness to mechanically fix the substrate to the polishing machine. Since this method does not require a polishing process, it can pattern even very thin substrates.

[0032] In one embodiment, a nonlinear interaction between the electromagnetic field and the substrate material exists if nonlinear absorption of the substrate material occurs in the region of the curved action area based on the electromagnetic field.

[0033] For example, nonlinear interactions between an electromagnetic field and a substrate material can result in nonlinear absorption of the substrate material.

[0034] In one embodiment, the substrate body is made of glass, glass ceramic, silicon, or sapphire, or has these materials.

[0035] In one embodiment, mechanical separation can be performed in a humid atmosphere and / or by CO2 cleavage (CO2-Cleaven). This can be advantageously used to ensure that the substrate body has bent or curved edges immediately after interaction with the electromagnetic field.

[0036] The electromagnetic field is tuned so that a nonlinear interaction occurs between the electromagnetic field and the substrate material within the curved region of action, particularly within the entire curved region of action.

[0037] In one embodiment, a substrate material in at least one curved operating region is exposed to an electromagnetic field such that a nonlinear interaction occurs between the electromagnetic field and the substrate material in the curved operating region, and as a result, the substrate material placed in the curved operating region is at least partially affected.

[0038] In one embodiment, the nonlinear absorption of an electromagnetic field in a substrate material includes causing nonlinear absorption of a laser beam in the substrate material.

[0039] Alternatively or additionally, the substrate material may be intended to be exposed to an electromagnetic field in multiple curved operating regions. Here, to have an advantage (i) The characterized surface has the same first curved profile in multiple regions, in particular determined by or influenced by the curved shape of multiple curved working regions and / or has the first curved profile overall. and / or (ii) The curved working regions are selected to be spaced apart from one another, particularly in the cross-sectional plane of the substrate body, such that the centers or centroids of the parts of the curved working regions that intersect with the cross-sectional plane are at a distance from one another such that the distance between the working regions and the intersecting parts of the curved working regions is 30% to 100% or 100% to 200% of the maximum extent of the curved working regions in the cross-sectional plane.

[0040] Using multiple curved working regions makes it particularly easy to provide extended, characterized surfaces. For example, extended sides of a substrate body can be reliably patterned. In this case, the individual curved working regions may be, for example, continuous. The curved working regions may also be offset from one another in each case, and / or rotated around the principal axis of each working region. As a result, multiple continuous regions with the affected substrate material can be created, and a characterized surface can be formed by exposing and / or further processing the respective interfaces between the affected and unaffected substrate materials.

[0041] In one embodiment, the substrate material is exposed to an electromagnetic field in at least two curved operating regions. Advantageously, the characterized surface is determined or influenced by both curved operating regions, particularly at various locations. Thus, in one embodiment, a first curved profile can be achieved in multiple regions of the characterized surface by multiple curved operating regions.

[0042] In this process, the first curved profile may be determined by or influenced by a portion of the curved working region, particularly a portion of its outer surface. The degree to which the curved working region co-determines the first curved profile may depend on how closely the individual working regions are continuous and how the affected substrate material is further processed.

[0043] In this case, in the cross-sectional plane of the substrate body, individual curved working regions may extend along straight lines or arbitrary curves, particularly arcs or perfect circles. For example, a certain distance may exist between the centers or centroids of consecutive common portions of curved working regions located in the cross-sectional plane. This distance can be approximately 100% to 200%, preferably 110% to 150% or 140% to 180%, of the maximum extent of the curved working regions in the cross-sectional plane. In this case, the curved working regions extend apart from each other by so-called web regions. This distance can also be 30% to 100%, preferably 50% to 70% or 60% to 80%, of the maximum extent of the curved working regions in the cross-sectional plane. In this case, the curved working regions are nested, so to speak, or in other words, the web regions have a negative width.

[0044] For example, existing sides of the substrate body, such as flat or otherwise shaped sides, can be newly patterned. To this end, the substrate material can be affected in a curved area of ​​action continuous with the existing side. Then, if not already done, the affected material can be removed by further measures as needed, thereby completely forming the characterized surface.

[0045] In cases like this, where a surface is patterned using multiple (same) curved action regions, the characterized surface is determined or influenced in the same way by the curved action regions in multiple areas. Therefore, the characterized surface also has the same first curved profile overall.

[0046] In one embodiment, the first curved profile can be found repeatedly or continuously on the characterized surface. For example, multiple curved working regions can be used for patterning the characterized surface, spaced apart from each other so as not to overlap. In this case, advantageously, the first curved profile can be found on the characterized surface over the entire area where the curved working regions acted.

[0047] For example, for patterning a characterized surface, multiple curved action regions can be used, spaced apart from each other and overlapping. In particular, the overlapping portion can be selected to be very large, that is, for example, 0.1% to 80%, preferably 0.1% to 20%, preferably 0.1% to 5%, or preferably 0.1% to 1% of the maximum extent of the curved action region in a plane perpendicular to the main extension direction of the curved action region. In this case, preferably, a continuous first curved profile can be found on the characterized surface, because as the overlapping portion increases, at each point on the characterized surface, only the outermost portion of the curved action region determines the shape of the characterized surface.

[0048] In one embodiment, the first curved profiles extend perpendicularly to the curved working region profiles, spaced apart from each other.

[0049] For example, a rectangular or circular recess can be cut out from a cubic substrate body. Then, two parts will exist: one from the substrate body with the recess, and the other from the cut-out portion. For this reason, the substrate material can influence a continuous, curved region of action along a curve (definable in the cross-sectional plane of the substrate body), such as a rectangular or circular curve. The affected material can then be removed by further measures, if necessary, if not already done. Each time the affected material is removed, the characterized surface can be completely formed, and the cut-out portion can be separated from the substrate body because there is no longer anything connecting the two.

[0050] According to one definition, the portion from which the recess has been cut out can be considered the patterned substrate body. According to another definition, the portion cut out from the substrate body to be patterned can also be considered the patterned substrate body.

[0051] Similarly, by influencing the substrate material in a continuous curved region of action along a straight line or a curve of any shape (definable in the cross-sectional plane of the substrate body), the substrate body can be separated along a intended surface, thereby forming a characterized surface. This further enables strategies to flexibly control and adjust the profile of the separation surface along its main extension direction.

[0052] In this process, the entire characterized surface does not need to be determined by or influenced by the shape of one or more curved action regions. For example, the substrate material affected within two adjacent curved action regions can be ultimately removed, thereby introducing two cavities into the substrate body. By connecting the two cavities, that is, by removing the wall material between the cavities, the exposed surface can also become part of the characterized surface.

[0053] Alternatively or additionally, affecting the substrate material involves changing, at least partially, one or more material properties of the substrate material, such as refractive index, etching rate, and / or density, particularly increasing or decreasing them. and / or The effect on the substrate material may be intended to involve at least partially removing and / or eliminating the substrate material from the curved area of ​​action, in particular by compressing the substrate material into the surrounding substrate material.

[0054] By altering the substrate material's material properties during the influence process, it becomes possible to selectively remove specific substrate materials to form a characterized surface or a portion thereof, for example. Furthermore, advantageously, the material properties allow for the removal of the affected material at different rates by applying further measures, depending on the degree of influence. As a result, it is even possible to spatially adjust the selectivity of the affected material in response to further measures.

[0055] In any case, the characterized surfaces can be correctly identified by the different material properties and then exposed by appropriate measures. In this process, measures that affect different regions with different material properties are advantageous. That is, if the measures act only on the affected substrate material, then after the effect, this material can be processed, for example, by removal. If the affected substrate material is removed, the substrate itself will have a new surface at the removed location, which will be at least part of the characterized surface. This new surface is determined by or influenced by the curved shape of the area of ​​action.

[0056] By immediately removing or eliminating the substrate material during the influence process, the patterning of the characterized surface can be performed very efficiently. In this case, further action may no longer be necessary. In this case, the new surface created after the influence will be equivalent to the characterized surface or a part of it. On the other hand, of course, it is also possible to take further action so that the new surface created after the influence becomes the characterized surface or a part of it at the stage after the further action is applied.

[0057] By compressing the removed material within the substrate body, the strength of the characterized surface can be improved. This is because compressing the surface area to be patterned within the substrate material increases its density and, consequently, its durability.

[0058] Alternatively or additionally, the characterized surface may be formed by at least partially removing the substrate material by affecting and / or by at least partially removing the affected substrate material with an acid and / or alkaline solution by at least a subsequent etching process, particularly a wet chemical process, where, advantageously, a potassium hydroxide solution may be used as the etching medium.

[0059] The affected substrate material can be advantageously removed by an etching process performed after the impact. This makes it possible to provide a characterized surface particularly efficiently and purposefully. In this way, by selecting the etching technique and / or etching medium, the affected substrate material can be purposefully removed. For example, the affected substrate material can be etched away entirely or partially, while the unaffected substrate remains. Alternatively, a portion of the unaffected substrate material can also be etched away in a partial area.

[0060] In one embodiment, the etching process involves isotropic etching of the substrate body, particularly the affected substrate material and / or the unaffected substrate material.

[0061] In one embodiment, the etching process involves wet etching and / or dry etching of the substrate body, particularly the affected substrate material and / or the unaffected substrate material.

[0062] In this process, it is particularly effective to combine the etching process with the use of multiple curved working regions and, consequently, the affected areas of the substrate material. In this way, the substrate material can be affected in multiple curved working regions. The individual curved working regions may be separated from each other, that is, they may not be connected to each other initially. For example, the individual working regions may be arranged in one direction, parallel to each other and at a distance from each other. The etching process can then remove the regions containing the affected substrate material. By continuing the etching, the substrate material in the region between two working regions, i.e., the unaffected substrate material, can also be removed by the etching process. As a result, connections can be made between the individual (etched) working regions.

[0063] When multiple areas of action, or in other words, areas of influence, extend from one surface to another, for example, the substrate itself may be separated into two parts simultaneously.

[0064] When multiple operating regions, or in other words, influence areas, extend from one surface to another, for example, when an operating region extends near the original substrate edge or extends further and terminates at that edge, only the outer surface of the substrate body is formed.

[0065] In other words, since at least the affected substrate material is removed by the etching process, there is also a possibility that unaffected substrate material may be removed by the etching process.

[0066] If the affected area penetrates at least one substrate surface of the substrate body (i.e., the affected area reaches at least one substrate surface), the affected substrate material can be etched away from the substrate body by, for example, so-called laser-selective etching (so-called anisotropic etching). This utilizes the fact that, especially during etching such as wet chemical etching, the affected area of ​​the substrate material is etched away from the substrate material more quickly than the unaffected area. If it penetrates one side, in addition to uniformly removing the substrate material from all substrate surfaces, the laser-modified area is etched more quickly than the surrounding substrate material, thus creating a cavity (i.e., a single-sided opening) in the area of ​​the affected substrate material. If the affected area extends further and penetrates two, particularly opposing, surfaces, a curved through-hole ("via") can be created in this way. Advantageously, such a curved through-hole can be used as the basis for the fabrication of an interposer by a subsequent metallization process.

[0067] In one embodiment, the curved working region penetrates at least one of the surfaces of the substrate body, such as the first and / or second upper surface.

[0068] Therefore, in a preferred embodiment, the subsequent etching process involves laser-activated etching of at least the affected substrate material.

[0069] For laser-selective etching, examples of etching media that can be used include hydrofluoric acid (HF), sodium hydroxide (NaOH), and / or aqueous potassium hydroxide solution (KOH).

[0070] Advantageously, the etching process is carried out in an acidic and / or alkaline etching medium.

[0071] Advantageously, the etching process is carried out until the areas where the affected substrate material has been removed are connected.

[0072] Advantageously, the etching process is carried out until the affected regions are connected.

[0073] As the average process output and consequently pulse energy of the electromagnetic field (e.g., the laser used) increases, the affected area (e.g., created by the laser or its line focus) extends, either entirely or partially, not only to changes in the density and refractive index of the substrate material, but also, for example, to voids introduced into the substrate material that appear outward, advantageously on one or more faces. A void appearing outward here means a void that is accessible from the outside. If a void appears outward on one face, it is accessible through one opening. If it appears outward on two faces, it is accessible through two openings.

[0074] If, as a result of the effect, a cavity appears that extends outward, the etching medium penetrates the cavity, and in an isotropic etching process, the substrate material can be simultaneously removed from all surfaces of the substrate body, especially from the surface of the created cavity, thereby increasing the diameter of the cavity. For example, a potassium hydroxide (KOH)-based etching process is applied for this purpose. For example, an alkali-etched substrate surface, such as a glass surface, is characterized by the formation of a dome-shaped depression.

[0075] The cavities may be introduced, for example, in the form of curved holes in the substrate material, in which case the holes appear outward, for example, on two opposing surfaces. Advantageously, the curved holes are widened by an etching process, which may be the same etching process used to pre-remove the affected material and then seamlessly remove the unaffected material as part of a continuous etching process. Advantageously, the etching process is then carried out until adjacent cavities are connected to each other.

[0076] In one embodiment, the affected substrate material is anisotropically etched at least partially and / or temporarily.

[0077] In one embodiment, the affected substrate material is isotropically etched at least partially and / or temporarily.

[0078] In one embodiment, the substrate material is affected, and then at least the affected substrate material is anisotropically etched away, thereby forming cavities, particularly through-holes, in the substrate body. Optionally, further etching can remove at least partially the unaffected substrate material between the through-holes, thereby connecting the through-holes to each other at least partially. In this case, these connecting surfaces can also be part of a similarly characterized surface.

[0079] In this process, it is particularly preferable to achieve that the characterized surface is height-adjusted at least in a partial region. For example, this surface may be configured in a dome shape at least in a partial region. This is achieved by exposing the characterized surface by both removing the affected substrate material (e.g., by etching) and removing the unaffected substrate material (e.g., by etching).

[0080] This height adjustment has proven advantageous because it contributes to increasing the strength of the characterized surface. Therefore, in one embodiment, it is preferable that the characterized surface has a dome-shaped structure, such as a dome-shaped depression, at least in a partial area.

[0081] If there are multiple consecutive regions having the affected substrate material, in one embodiment, the etching process is carried out until the affected regions are not only released (i.e., the affected material is etched away in those regions) but also connected. In this case, the two substrate portions can be separated, for example, as an inner portion and an outer portion, without relying on force.

[0082] Alternatively or additionally, the electromagnetic field may be provided in the form of a curved line focus, particularly a laser beam, and / or the curved region of action may be determined by the form of the line focus.

[0083] Providing an electromagnetic field in the form of a curved line focus is a particularly efficient strategy, because line focuses can be formed very easily in many different forms, especially using lasers.

[0084] A laser beam using a line focus can be guided and controlled along its optical path by known means. The line focus can be adjusted and adapted by various measures such as optical elements. Therefore, an electromagnetic field can be created within the substrate body that can take any spatial shape achievable by beam shaping or beam steering means. Accordingly, a nonlinear interaction with the substrate material can be generated in the corresponding shaped region of the substrate body.

[0085] Therefore, a laser beam with a linear focus achieves a nonlinear interaction between the electromagnetic field and the substrate body in a curved operating region, and in particular, becomes an extremely flexible means of achieving nonlinear absorption.

[0086] When processing a substrate using a laser, generally, it is necessary to distinguish between a linear absorption process and a non-linear absorption process. Linear absorption means that the material to be processed is partially or completely absorptive with respect to the wavelength of the laser used (e.g., absorption of CO2 laser light in glass), and the intensity of the interaction can be appropriately adjusted by factors such as the laser wavelength, laser energy, pulse width, etc. Separately from this, there is a non-linear absorption process. In this process, the material to be processed initially does not show absorption in the region of the laser beam used, that is, it is transparent with respect to the laser wavelength. However, when creating a so-called ultra-short laser pulse (where the typical pulse length here varies in the range of 10 ps to 100 fs, especially in the range of 1 ps to 100 fs), a sufficiently high electromagnetic field is created in the substrate material by the laser, and this electromagnetic field causes non-linear changes in the material properties of the substrate body or its material, such as the refractive index, and thus the absorption properties of the material. When the threshold value characterizing the material is exceeded, the laser beam has a continuous effect on the material. The resulting local changes in the material range from continuous changes in the refractive index, changes in etching behavior (selective laser etching) to the occurrence of cracks and channels in the substrate, but in each case, they depend on the interaction between the laser parameters and the material parameters and are limited to the region of the laser focus formed in the material.

[0087] For example, for a glass substrate, the critical intensity that causes non-linear changes in its material properties is at least 10 13 W / cm 2 or more.

[0088] In one embodiment, the substrate material has glass, and the electromagnetic field has a field strength of at least 10 13 W / cm 2 , preferably at least 5×10 13 W / cm 2 , preferably at least 10 14 W / cm 2 , most preferably at least 5×10 14 W / cm 2 Optionally, the electromagnetic field has a maximum of 10 16W / cm 2 It possesses the strength of the field.

[0089] In one embodiment, the curved operating region corresponds to the region where the laser line focus causes a nonlinear interaction with the substrate material, where the nonlinear interaction favorably exhibits and / or is nonlinear absorption, and consequently affects the substrate material.

[0090] Based on the existence of a line focus, an electromagnetic field that causes nonlinear interactions also exists in the associated curved region of action.

[0091] In one embodiment, the nonlinear interaction between the electromagnetic field and the substrate material occurs within the entire curved region of action.

[0092] In one embodiment, the electromagnetic field corresponds to a line focus.

[0093] Alternatively or additionally, the laser beam can be provided by an ultrashort pulse laser. The phase of the laser beam is adjusted and / or adapted, in particular, using a spatial light modulator, a diffractive optical element and / or a combination of multiple cylindrical lenses. The laser beam is focused onto the substrate body, preferably using a microscope objective lens or Fourier lens, and the focusing is preferably performed after adjusting or matching the phase of the laser beam and / or forming a line focus. Line focus is for accelerated laser beams, especially Airy beams. The laser beam has a wavelength of 1064 nm, the microscope lens or Fourier lens has a focal length of 10-20 mm, and the phase coefficient of the cube (laser parameter β) is 0.5 × 10⁻⁶. 3 / m~5×10 3 The value is / m, the raw beam diameter (laser parameter ω0) is 1mm to 10mm, preferably 2.5mm to 5mm, the pulse width (laser parameter τ) is 0.1 to 10ps, and the pulse energy (laser parameter E) is pThe pulse strength (laser parameter N) has a value of 1 to 1500 μJ, preferably 30 to 500 μJ, and especially 474 μJ, and / or the number of pulses during the burst (laser parameter N) has a value of 1 to 200, preferably 1 to 100, and especially 1 to 8. The spatial extent of the curved working region, advantageously one of its length and / or diameter, is adjusted and / or changed over time by changing the average output range of the laser and / or by changing its phase, in particular by adjusting different extents for at least some of the multiple curved working regions. and / or The spatial orientation of the curved working region may be adjusted and / or changed over time by changing the inclination of the optical axis of the laser beam with respect to the normal to the substrate surface, particularly the substrate surface into which the laser beam enters the substrate body, and in particular, different orientations may be adjusted for at least some of the multiple curved working regions.

[0094] The phase of a laser beam affects the spatial shape of the electromagnetic field at the line focus, and consequently, the curved region of action can be adjusted and adapted. Therefore, a spatial light modulator (SLM), a diffractive optical element, and / or a combination of multiple cylindrical lenses that can collectively adapt the phase of the laser beam are suitable means for controlling the spatial shape of the electromagnetic field.

[0095] A possible setup for creating a curved area of ​​effect according to the present invention, and the correspondingly spatially formed electromagnetic field, can be designed in principle as follows: The laser beam of an ultrashort pulse laser strikes a spatial light modulator (SLM), which changes the phase of the incident laser pulse by applying a phase such as the phase of a cube. The beam is then focused onto the substrate body to be patterned by passing it through a microscope objective lens and / or onto a Fourier lens. Depending on the phase distribution that occurs behind the spatial light modulator, the imaging objective lens creates a curved focal line rather than a straight line, and this focal line leaves a spatially curved area of ​​influence on the substrate material on the substrate body. In one embodiment, the secondary peak value of the Airy beam can also be suppressed. In this case, the intensity ratio of the primary focus to the other beams can be optimized (1.2~10). This can be achieved, for example, by non-radiatively symmetric apodization on the Fourier plane using an aperture.

[0096] In preferred embodiments, instead of a spatial light modulator to change the phase distribution as desired, a diffractive optical element (DOE) is used to create a curved working region. For example, the element has a diameter of 5–15 mm, preferably 9 mm, and the DOE is located at the “front focal plane” of the microscope objective lens or Fourier lens. Advantageously, the SLM or DOE (i.e., generally speaking, the phase mask) has a working distance from the target lens that is equal to and / or 2–15 mm, preferably 5 mm, of the lens's focal length. In cases where the “front focal plane” of the microscope objective lens is on the objective lens itself, in these cases, the minimum (structural) distance is preferably selected. Similar setups, such as a 2f setup, may also be intended for the SLM. In further embodiments, instead of a spatial light modulator or diffractive optical element, a combination of multiple cylindrical lenses is used to create the phase of the laser beam, particularly the phase of a cube.

[0097] For example, an Airy beam is used here. Airy beams are particularly well suited for asymmetric / lateral beam supply.

[0098] Pulse energy (laser parameter E) p For example, a value of 300 μJ can be selected as the pulse strength (laser parameter N), for example, a value of 2 can be selected as the number of pulses during the burst (laser parameter τ), and / or a value of 5 ps can be selected as the pulse width (laser parameter τ). Optionally, the focal length of the optical system may be set to f=10 mm, and / or a beam expander with a magnification of 2.0 (especially for a 10 mm diameter input Gaussian beam) may be provided.

[0099] Furthermore, Airy beams can be produced particularly easily and efficiently. For example, an Airy beam can be obtained as an image of a beam with a cubic phase directly produced by a setup using a phase mask (DOE or SLM) or a cylindrical lens.

[0100] With the appropriate selection of the optical apparatus (particularly the definition of the vertical distance between the focal optical system and the substrate material to be processed, i.e., the focal position and focal length), this method can create a curved working area that penetrates the substrate material, either internally or on one of two large surfaces (bottom and / or top), or even on both large surfaces.

[0101] Advantageously, to create a linear focus, particularly an accelerated beam, SLM, DOE, and / or lens optics can be used as a single component or as an array of lenses such as cylindrical lenses, allowing for the application of an appropriate phase function to the laser beam.

[0102] In one embodiment, the curved working regions are positioned along a closed contour at predetermined distances from one another (i.e., with a so-called pitch) on the substrate material, for example, at distances of 1 μm to 50 μm, preferably 1 μm to 10 μm, 10 μm to 30 μm, 20 μm to 40 μm, or 30 μm to 50 μm. Distances of 1 μm, 20 μm, or 50 μm may be advantageous. In this case, the alignment of the modified portion can be controlled by optical tracking (mechanical tracking of the DOE or changes in the phase distribution by software) so that the inscribed structure is not tilted, or at least a surface characterized by convexity at a certain angle. Such curved working regions make it possible to define a new outer contour on the substrate body, for example, a raw glass substrate. At that time, it is also possible to optionally use auxiliary cuts as needed to remove excess material along the intended contour.

[0103] In one embodiment, beam alignment is advantageously tracked at a constant angle relative to the target contour, mechanically in the DOE and by software in the SLM.

[0104] In one embodiment, the surface patterning sequence is controlled to prevent undesirable interactions, particularly shadowing. Favorable interactions between consecutive influencing areas are possible, and favorable directions can be adjusted along the target contour.

[0105] Airy beams offer advantageous properties for supplying electromagnetic fields.

[0106] The spatial extent and / or intensity of the nonlinear interaction can be adjusted to suit the purpose by selecting appropriate laser parameters.

[0107] Generally, when patterning outward or inward surfaces (inner and / or outer surfaces), it is preferable to align the laser optical system to enable the formation of a convex first curved profile toward the inward side (when patterning the inner surface) or toward the outward side (when patterning the outer surface). This method also allows for combinations of inner and outer surfaces, and can even be performed in a single run.

[0108] In the embodiment, the specific shape of the curved area of ​​action or the affected substrate material is determined or can be determined by the phase applied by SLM and / or DOE.

[0109] It was found that adjusting the spatial extent of the curved area of ​​action, and consequently the area affected by the substrate material, by controlling the average output range of the laser was particularly effective.

[0110] By varying, and especially increasing, the pulse energy of the laser pulse, the laser output in this case exceeds the threshold of the substrate material over a wider area of ​​the curved focal line. Therefore, the length of the curved area of ​​action or influence can be adjusted.

[0111] For example, by varying a 10 ps laser pulse across the average output range of the laser (e.g., using output levels of 1W to 500W, preferably 1W to 40W, especially 2W to 10W, 10W to 20W, 20W to 30W, or 30W to 40W, and / or pulse energies of 1 μJ to 500 μJ, preferably 30 μJ to 300 μJ), and / or by phase changes using a spatial light modulator, various lengths of curved action regions and thus influence areas can be achieved on substrate materials such as glass.

[0112] For example, a curved region of action or influence having a length from more than 0.1 mm to more than 3 mm, preferably 0.1 mm to 5 mm, particularly 0.5 mm to 3 mm, and / or a maximum deviation from a linear focal line of 200 μm, preferably 10 μm to 80 μm, particularly 20 μm to 80 μm, can be formed, particularly by the means described above. The curved profile of the influence, and consequently the first curved profile of the characterized surface, is determined or influenced by a shape that can be theoretically predetermined by the phase function used.

[0113] Therefore, in one embodiment, the length of the curved working region is adapted and / or changed over time by changing the pulse energy of the laser pulse.

[0114] By adjusting the average output of the pulses, it is possible to influence the spread of the electromagnetic field, and consequently the spatial extent of the curved region of action, in a way that is particularly tailored to the purpose. The same can be said for phase changes.

[0115] For example, a higher output results in a longer curved focal length. Therefore, this output can be used and / or controlled to suit the purpose, thereby aligning the focal point and, consequently, the curved area of ​​action within its spatial extent.

[0116] For example, if the phase of the cube is stronger, the focal length will be longer and the curve will be greater. Therefore, this phase can be used and / or controlled as needed to fit the focal point and, consequently, the curved region of action within its spatial extent.

[0117] In particular, when the substrate material is affected by the laser without being removed, the subsequent etching process is advantageous in the embodiment. In this case, the amount of etching removed and / or the etching rate can be increased by performing the etching on individual affected areas in the curved treatment region not with individual pulses, but with multiple pulses within a pulse group, i.e., using so-called burst pulses. Therefore, in the embodiment, it is preferable that the ultrashort pulse laser executes multiple pulses within a single pulse group as burst pulses.

[0118] Therefore, the proposed method makes it possible to provide a substrate having a predetermined (lateral) shape (thickness) and a predetermined surface, particularly the sides, from a starting substrate such as a glass substrate or a glass-ceramic substrate. To achieve this, the substrate material of the starting substrate can be influenced along the intended surface using, for example, an ultrashort pulse (UKP) laser within a curved area of ​​action of a predetermined shape, and then the influenced area of ​​the substrate material can be selectively etched and removed. In particular, etching can be performed until the thus defined areas are joined, and then the two parts, for example, an inner and an outer part, can be separated from each other without relying on force.

[0119] Alternatively or additionally, during at least the nonlinear interaction, at least one auxiliary substrate body is positioned on the substrate body, with each curved operating region and / or line focus extending at least partially within the auxiliary substrate body, where, advantageously, two or more auxiliary substrate bodies are positioned on the substrate body, particularly on opposing surfaces of the substrate body, with each curved operating region and / or line focus extending at least partially within the two or more auxiliary substrate bodies.

[0120] Advantageously, the auxiliary circuit board itself is made from the same material as the main circuit board.

[0121] By using such an auxiliary substrate body, when a curved working area penetrates, it is possible to avoid or at least significantly reduce ablation components or ablation effects on the exposed surface of the substrate.

[0122] For example, in one embodiment, the substrate body to be patterned can be processed together with an auxiliary substrate body that has been linzing, bonding, and / or ultrashort pulse welding, during which initially only the internal influence areas are created, and in a further processing step (e.g., debonding) by removing the auxiliary substrate body, these influence areas are exposed, so to speak.

[0123] Therefore, by providing an auxiliary substrate body, it is possible to influence the substrate material even in the area near the surface of the substrate body, in accordance with the specified surface specifications, especially for the purpose. This is because, based on the auxiliary substrate body, the curved working area can extend beyond the substrate body without the profile of the curved working area being damaged or significantly damaged. Therefore, even in the area near the surface of the substrate body, it is guaranteed that the curved working area does not deviate from the desired shape and that it spatially influences the substrate material according to the specifications.

[0124] In particular, if the auxiliary substrate body and the substrate body are made of the same material, it is guaranteed that the curved working region will transition seamlessly, and especially without displacement, at the interface between the two bodies.

[0125] After the nonlinear interaction, the auxiliary substrate can be removed from the main substrate. Thus, the actual main substrate, containing the affected substrate material, is exposed again.

[0126] In other words, if the auxiliary substrate body is removed again after the nonlinear interaction, a clean influence area can be achieved on the substrate body, extending all the way to the outer surface of the substrate body.

[0127] One or more auxiliary circuit board bodies can be provided.

[0128] The auxiliary circuit board can be positioned around the main circuit board so as to surround it with one or more surfaces.

[0129] The auxiliary substrate body ensures that the accumulation of substrate material in the characteristic surface edge regions due to the ablation effect is reliably prevented.

[0130] Alternatively or additionally, at least one of the at least one curved region of action, advantageously multiple and / or all of the region of action, is completely confined within the substrate body, particularly during at least nonlinear interactions. Herein, it may be advantageously intended that the method further includes removing material from the substrate body at least partially, particularly along the main stretching direction of the curved working region within the substrate body, thereby making the affected substrate material in the confined curved working region accessible from the outside at least partially and / or partially, in particular by etching the removal of material from the substrate body.

[0131] In other words, by ensuring that the curved working area is completely within the substrate body, it is possible to reliably avoid ablation components or ablation effects on both the original surface of the substrate body and the resulting surface.

[0132] In other words, in this proposed feature, the nonlinear interaction occurs only between the electromagnetic field and the substrate material within the substrate body. That is, it is inaccessible from the outside. As a result, the profile of the curved region of action is not damaged or significantly damaged. Therefore, it is guaranteed that the curved region of action does not deviate from the desired shape and that it has a spatial influence on the substrate material according to the specifications.

[0133] After the nonlinear interaction, the substrate material can be removed from the substrate body until it reaches (or beyond) the affected substrate material. For example, the corresponding etching process has been found to be advantageous for this purpose because it can be performed accurately and efficiently. In this way, a new surface, particularly distinct from the characterized surface, can be formed, for example, at least a new, at least temporary, top surface of the substrate body. By removing the substrate material, the affected material region becomes accessible from the outside. As a result, for example, the affected substrate material can then be removed to form the characterized surface, as described elsewhere.

[0134] In this way, the affected material regions on the substrate, extending to the final processed surface of the substrate itself, can be defined with great certainty. As a result, a clean and well-defined surface can also be achieved.

[0135] For example, by removing material from the substrate body, at least one, preferably both, upper surfaces of the substrate body are altered. In other words, a shift of the upper surface can occur, for example, along the main stretching direction of the curved working region.

[0136] In this case, the main stretching direction of the curved working region can be, for example, perpendicular to the original and / or modified upper surface of the substrate body.

[0137] Alternatively or additionally, the substrate material may be exposed to an electromagnetic field continuously, or entirely, or partially in parallel, in individual regions of multiple curved operating regions. The entire substrate material within the curved area of ​​action is simultaneously exposed to the electromagnetic field. In each case, the curved region of action has a maximum deviation from the linear profile of more than 20 μm, more than 40 μm, more than 60 μm, more than 80 μm, or more than 100 μm. and / or The length of the curved area of ​​action may be intended to be greater than 0.1 mm, 0.3 mm, 0.5 mm, 0.7 mm, 1 mm, 3 mm, or 5 mm in each case.

[0138] By continuously exposing the substrate material to an electromagnetic field in individual curved action regions, and thus sequentially influencing the substrate material in each region, patterning can be prepared or executed with minimal technical effort. In this case, if the electromagnetic field is provided using, for example, a laser line focus, only one laser is needed. In this case, by relatively moving the substrate body and the line focus, line focuses can be easily and continuously formed in different curved action regions, thereby influencing the substrate material.

[0139] By simultaneously exposing the substrate material to an electromagnetic field across multiple curved action regions (or all of them), the influence on the substrate material can be performed very efficiently in terms of time, thereby shortening the preparation or execution of patterning. In this way, multiple lasers can form parallel line foci at different locations on the substrate material, in each case, thereby influencing the substrate material in parallel across multiple curved action regions.

[0140] In this case, additionally, once the substrate material in the corresponding curved working region has been affected, the substrate itself can be moved relative to multiple focal points. In this way, the substrate material can be sequentially affected in parallel at multiple locations in each case. This enables a particularly efficient patterning strategy. In particular, this procedure is scalable to larger substrates or larger-scale patterning processes. This is because, for larger-scale work, for example, additional lasers can be added to form multiple curved working regions in parallel, with the lasers creating additional linear focal points in the substrate material in each case.

[0141] In the case of lasers, a linear focus is formed in the substrate material, and as a result, a curved region of action is determined. That is, the region in the substrate material where an electromagnetic field is generated by the linear focus becomes the curved region of action. In particular, this region is the part of the electromagnetic field that causes a nonlinear interaction with the substrate material.

[0142] Of course, the linear focus exists outside the main substrate body, for example, in a medium that at least partially surrounds the main substrate body, such as a fluid, such as air or liquid, and / or partially in the auxiliary substrate body as well. However, in this case, since the electromagnetic field is still present within the main substrate body, a curved region of action can be defined on the main substrate body, even if the curved region of action continues in the other medium.

[0143] Because this method is flexible, it is possible to create a curved working area with a curved portion and / or length adapted to each case. In this way, the curved portion or length can be made smaller or larger depending on the intended surface patterning.

[0144] The curved working region is preferably formed three-dimensionally on the substrate body. The curved working region preferably has a main stretching direction within the substrate body. A central axis can be positioned through the curved working region, which itself may have a curved profile. The length of this central axis corresponds to the length of the curved working region. This central axis has a start point and an end point on the substrate material. Advantageously, the start and end points are on the surface of the substrate body in each case, for example, at the intersection of the substrate body and the curved working region. The maximum displacement of the curved working region is the maximum distance a point on the central axis can have from a point on the straight line connecting the start and end points of the central axis.

[0145] The spatial shape of the curved area of ​​action, that is, the spatial shape of the affected substrate material, i.e., the shape of the characterized surface, depends on or is co-determined by this maximum displacement, which is sometimes called the profile stroke.

[0146] To adjust the maximum displacement or profile stroke, the numerical aperture A=n of the focusing optical system. * sin(ALPHA) can be adjusted and / or adapted. In this case, generally speaking, the larger the numerical aperture of the focusing optical system, the shorter the length of the formed focal point, and in the typical case of an Airy beam, the curvature of the Airy beam near the focal point becomes higher.

[0147] This means that, in the case of a curved area of ​​action or a characterized surface, in order to create a profile stroke worthy of evaluation on the characterized surface, the local curvature needs to increase as the thickness of the substrate body decreases.

[0148] Therefore, this method can be used for processing / patterning thin circuit boards. This is especially true for patterning the sides of the circuit board.

[0149] The thin substrate body is preferably 500 μm or less, 300 μm or less, or 100 μm or less in thickness, and preferably in the range of 30 μm to 100 μm. Any thin substrate is 0.1 μm or more, 1 μm or more, 10 μm or more, 50 μm or more, or 100 μm or more in thickness.

[0150] While it is possible to mechanically fix a substrate body with a thickness exceeding 1 mm and polish its sides using conventional methods, this was previously not possible for thin substrate bodies because the substrate body is (mechanically) unstable, and there is a risk that the thin substrate body will be destroyed by cracks forming from the sides due to the mechanical stress caused during polishing.

[0151] This method makes it possible for the first time to pattern the surface of a thin substrate, particularly one with a thickness of 500 μm or less, without using any force and therefore without the risk of damaging or adversely affecting the substrate. In particular, this surface is the side surface of the substrate, and more advantageously, the circumferential side surface.

[0152] In one embodiment, the numerical aperture of the optical system used to focus the laser is adjusted as a function of the thickness of the substrate material, which is advantageous as it allows the sides of the substrate body having a thickness of 500 μm or less and / or 0.1 μm or more to be patterned as a characterized surface.

[0153] In one embodiment, the characterized surface may have an adjustable inclination. Optionally, this is achieved using a shifted and / or inclined, particularly vertically shifted or inclined, Airy beam.

[0154] In this case, it is advantageous to use an Airy beam, where the beam centroid moves parallel to the optical axis / perpendicular to the substrate surface such as a glass surface (angle 0 degrees), and is distributed symmetrically through the middle of the substrate (along the propagation direction / substrate thickness). That is, the beam reaches its maximum deviation (focal position) precisely at that point. In the case of a shifted (un-tilted) Airy beam, the focal point (and point of maximum deviation) is located off-center from the substrate (along the substrate thickness). In the case of a tilted Airy beam, the optical axis (as the trajectory of the beam centroid) is not parallel to the normal of the substrate surface.

[0155] In one embodiment, the existing surface of the substrate body, particularly the sides, is chamfered, especially in multiple passes.

[0156] In one embodiment, the laser beam is an Airy beam.

[0157] In one embodiment, the combination of inner and outer surfaces is patterned and, advantageously, used as a glass hinge for use in flexible mobile devices. This is understood to mean a patterned, usually strip-shaped, glass substrate with a maximum thickness of 200 μm, preferably 100 μm or less, and particularly preferably 20 μm, comprising an intermediate patterned region extending between two opposing edges of the substrate and two adjacent unpatterned regions. The recesses in the patterned region created according to this method enable reproducible bending around a bending axis perpendicular to the orientation of the glass strip.

[0158] Alternatively or additionally, (i) the substrate body is transparent and made of glass, and has a first upper surface and / or preferably a second upper surface extending parallel to and / or facing the first upper surface, (ii) Preferably the thickness of the substrate body measured between the first upper surface and the second upper surface is 500 μm or less, preferably 400 μm or less, more preferably 300 μm or less, more preferably 200 μm or less, more preferably 100 μm or less, more preferably 70 μm or less, more preferably 50 μm or less, more preferably 30 μm or less, and most preferably 10 μm or less. and / or (iii) After patterning the characterized surface, 1. The characterized surface extends between the first upper surface and the second upper surface. 2. The characterized surface is connected at least partially to the first upper surface and / or the second upper surface, 3. At least one side of the substrate body, preferably at least a portion of the circumferential side, has a characterized surface. 4. Advantageously, at least a portion of the surface of the through-hole extending from the first upper surface to the second upper surface has a characterized surface, and advantageously, the through-hole is formed by affecting and / or etching the substrate material. 5. At least one surface region of a cavity in the substrate body has a characterized surface, the cavity is advantageously accessible from the outside or completely enclosed within the substrate material, and advantageously the cavity is formed by affecting and / or etching the substrate material. 6. The characterized surface is at least partially an inward-facing surface of the substrate body, and / or 7. The characterized surface may be intended to be, at least partially, an outward-facing surface of the substrate body.

[0159] Previous methods, especially for transparent substrates, have not yielded satisfactory results in terms of efficiency and the strength of the formed surface. This method allows for reliable patterning of the surface of transparent substrates.

[0160] The first and second upper surfaces clearly separate the upper surface from the main body of the substrate, thus enabling a reliable influence on the substrate material.

[0161] In one embodiment, the first and / or second upper surfaces are planar.

[0162] In one embodiment, the substrate body is cubic.

[0163] In one embodiment, the substrate body is transparent and has a first upper surface, a second upper surface, and circumferential side surfaces that are curved in at least a partial area along the thickness direction of the substrate body.

[0164] This method is particularly well suited for patterning the surface of thin substrates, i.e., substrates with a small thickness. In particular, it is used to pattern surfaces having a stretch direction along the thickness of the substrate, for example, the advantageously circumferential side surfaces of the substrate.

[0165] For example, a cubic substrate body may have a small thickness. In this case, the substrate body may only have small dimensions in one direction corresponding to the small thickness, but this method also allows for patterning of its sides or regions. Optionally, the sides are circumferential sides.

[0166] In this application, advantageously, the substrate body is considered to have a thin or small thickness when the thickness of the substrate material is 500 μm or less and / or 10 μm or more.

[0167] If the characterized surface is connected to at least one upper surface, a particularly seamless transition can be created between the existing surface and the patterned surface. This results in a very stable substrate body.

[0168] For example, the side surface of the substrate body, such as the circumferential side surface, can be patterned, or shaped, by this method. In this case, the characterized surface is a part of this circumferential side surface.

[0169] This method can be used with particularly high versatility. For example, if a curved area of ​​action extends from one surface region (e.g., one upper surface) to another surface region (e.g., the other upper surface), and the affected substrate material extends accordingly, a through-hole can be created from one upper surface to the other upper surface (generally: surface region) by patterning the characterized surface. For example, if the curved area of ​​action does not extend to the other surface of the substrate body (e.g., the other upper surface of the substrate body), but extends from one surface region of the upper surface (e.g., one surface region) into the substrate, and the affected material extends accordingly from one surface region into the substrate, a cavity can be formed on one surface (generally: top surface) by patterning the characterized surface. If the affected substrate material does not extend to the outside, a completely enclosed cavity can also be created in the substrate body by patterning the characterized surface.

[0170] Apart from the case of confined cavities, affected material can be selectively removed directly by the effect and / or, for example, by a subsequent etching process.

[0171] This method allows for the cutting of a circular opening from a thin, cubic substrate body by patterning a characterized surface having a circular contour in at least one cross-sectional plane within the thickness range of the substrate body.

[0172] This method allows, for example, the outer side surface of a thin, cubic substrate to be shaped into a convex or concave form.

[0173] In one embodiment, the characterized surface patterning involves shaping the outer sides of the substrate body, particularly thin cubic substrate bodies, into a convex shape.

[0174] Alternatively or additionally, after patterning the characterized surface, the first curved profile of the characterized surface extends perpendicular to the principal elongation direction of the characterized surface. and / or It may be intended that the characterized surface has a second curved profile, at least partially, in the main stretching direction of the characterized surface, particularly in the circumferential direction of the substrate body.

[0175] When the sides of a circular or cubic substrate body are patterned and thus represent a characterized surface, the sides may have a curved portion along the thickness of the substrate body, where the curved portion is co-determined or determined, at least partially, by the curved portion of the curved working region. This is the first curved profile. This profile also extends perpendicular to the principal stretching direction of the side of the substrate body, where the side represents, for example, a circumferential side.

[0176] In the case of a circular circuit board, the sides also curve and extend around the circuit board accordingly, and these sides represent a second curved profile.

[0177] In one embodiment, the first curved profile, which is at least partially concave or convex, can be adjusted by rotating the line focus by 180°, preferably around at least one axis parallel to the principal extension direction of the line focus.

[0178] Alternatively or additionally, after patterning a characterized surface in at least one cross-sectional plane of the substrate body, the characterized surface has a contour along a first curved profile, the contour being (i) curved in a convex or concave manner, at least partially (ii) It corresponds at least partially to the curved contour of the area of ​​action, and / or (iii) It may be intended that the profile has, at least in part, a parabolic profile, a quarter-circular profile, a logarithmic profile, a profile following a polynomial function of degree n, favorably an even n, in particular n=6, n=8, n=10 or n=12, and / or a C-shaped profile.

[0179] By adjusting the corresponding phase, the line focus can take on a wide range of shapes, thereby forming a wide range of three-dimensional action regions and influencing the substrate material within those regions. For example, it can influence the substrate material in multiple adjacent action regions, thereby giving the patterned substrate body a surface characterized as a new side. In this case, the curved action region can be selected so that the curved portion protrudes from the substrate material of the desired substrate body after patterning in order to obtain a concave-shaped characteristic surface. Alternatively, the curved action region can be rotated, so to speak, 180 degrees to obtain a convex-shaped characteristic surface.

[0180] Therefore, this method can be used particularly easily to pattern surfaces characterized by various shapes.

[0181] The various properties of convexly curved surfaces / sides can be advantageous depending on the subsequent application. For example, the parabolic / cubic phase can realize top / side surfaces that are close to the C-cut top / side surfaces commonly used in the glass industry, whereas the quadrant phase function corresponds more to top / side surfaces with phases on the upper and lower sides (rather than continuously curved top / side surfaces). Various asymmetrical top / side shapes can be similarly realized by tilting the beam axis and / or shifting the focus relative to the substrate body. Such top / side surfaces are used, for example, when self-alignment effects are relevant when applying them to the substrate body.

[0182] Similarly, it is possible to partially process the top / side surfaces of thick glass in several stages.

[0183] This problem is solved by proposing the following substrate body according to the second aspect of the present invention, which is: It has at least a first upper surface and at least one characterized surface, which is manufactured or can be manufactured in accordance with a method according to a first aspect of the present invention, The characterized surface has at least one first curved profile, at least partially. The first curved profile is located in a cross-sectional plane of the substrate body fixed to a plane having at least one normal vector of the characterized surface and the normal vector of the top surface, The first curved profile can be described, at least partially, by parabolic, quadrant, logarithmic, and / or polynomial phase functions. The thickness of the substrate itself is 500 μm or less.

[0184] A substrate body having a surface with a curved contour patterned in the cross-sectional plane, despite its small thickness, is provided for the first time.

[0185] In particular, it was previously impossible to represent the surface in the lateral direction of the circuit board itself.

[0186] This is because substrates with a thickness of 500 μm or less exhibit the property of bending under their own weight when fixed in place. This behavior is very similar to that of a single sheet of paper. Therefore, such substrates are also called microsheets.

[0187] Based on this behavior, it was previously impossible to mechanically fix such thin substrates and perform polishing measures on the processed surface, which were conventionally required. The method according to the present invention already provides a high-quality, characterized surface, so polishing is not necessary.

[0188] An electromagnetic field is formed even within the extremely thin substrate body, allowing it to appropriately influence the substrate material. As a result, even with a thin substrate, it is possible to reliably provide a substrate body with a highly sensitive, patterned, and characterized surface. This is ideal for microsheets.

[0189] The substrate itself is advantageous if its thickness is 400 μm or less, 300 μm or less, 200 μm or less, 100 μm or less, 50 μm or less, 20 μm or less, or 10 μm or less.

[0190] The substrate itself is advantageously characterized by a thickness of 1 μm or more, 10 μm or more, 50 μm or more, or 100 μm or more.

[0191] In one embodiment, the narrow side of the substrate body has a spherical shape with a C-cut design.

[0192] In one embodiment, the curved portion on the narrow side of the substrate extends along at least one direction and / or partially in a parabolic, polynomial, or logarithmic form and / or is predetermined by the intensity profile of the quadrant beam.

[0193] In one embodiment, the substrate body has at least one modification inside, which is advantageously a spatially limited modification of the density and / or refractive index of the substrate material, having cavities, cracks and / or through-holes in the substrate material, and advantageously comprising formed outer / inner contours and / or taper angles. Optionally, the modification may be internally separated by different types of contours, for example, straight or curved. Furthermore, the modification may penetrate at least one or both of the upper surfaces of the substrate body, or neither.

[0194] In one embodiment, the characterized surface roughness Ra is 5 μm or less, preferably 2 μm or less, and more preferably 1 μm or less. For example, the roughness is the average roughness and is preferably measured according to ISO 25178:2016.

[0195] In one embodiment, the characterized surface has a grooved structure.

[0196] In one embodiment, the substrate body has two or more layers and curved sides. Optionally, the substrate body with functional components may be processed as is.

[0197] In one embodiment, the substrate body is made of glass, glass ceramic, silicon, or sapphire, or has one of these materials.

[0198] In one embodiment, the substrate body does not have an accumulation of substrate material in the edge region of the characterized surface.

[0199] Alternatively or additionally, the characterized surface has a strength of at least 100 MPa, preferably at least 150 MPa, more preferably at least 200 MPa. Advantageously, the characterized surface may be intended to be etched whole or in part, in particular, with hydrofluoric acid, sodium hydroxide, alkaline solutions, such as potassium hydroxide solution, and / or acids.

[0200] The high strength of the characterized surface gives the substrate body durability against external influences such as mechanical stress acting on the characterized surface. This stabilization is a significant advantage, especially for thin substrate bodies.

[0201] The method according to the present invention provides such a characterized surface, because damage such as fine cracks that occurred with conventional methods does not occur with the proposed method, and in particular these known methods cannot be applied to the substrate body of the thickness in question here.

[0202] Etching the characterized surface, either entirely or partially, can further increase its strength.

[0203] Alternatively or additionally, the characterized surface may be height-adjusted at least partially, and in particular may be intended to have wavy and / or dome-shaped structures, advantageously along and / or perpendicular to the principal stretching direction of the characterized surface.

[0204] By adjusting the height, the strength of the characterized surface can be increased. As a result, the substrate becomes more resistant to external influences such as mechanical stress acting on the characterized surface. This has the significant advantage of providing additional stabilization, especially in the case of thin substrates.

[0205] Until now, it has not been possible to safely and reliably perform such height adjustments, especially on the sides of thin circuit boards. Because thin circuit boards are mechanically unstable, the necessary processes, particularly grinding, could not be performed on such boards in the past. The proposed method makes it possible to pattern even very thin circuit boards, especially their sides, and to incorporate height adjustments during the process.

[0206] In this way, for example, by affecting the substrate material of multiple curved working regions, a height profile can be achieved particularly easily and reliably. If the substrate material of the curved working regions is removed, for example, by the effect itself or by a subsequent etching process, then, for example, individual cavities in the substrate body can be connected to each other by subsequent etching by etching away the unaffected substrate material between the individual cavities. As a result, a characteristic wavy structure can be achieved along the main stretching direction of the characterized surface.

[0207] Advantageously, the principal elongation direction of the characterized surface extends perpendicular to the principal elongation direction of the curved area of ​​action.

[0208] Alternatively or additionally, (i) the substrate body is transparent and made of glass, and has a first upper surface and / or preferably a second upper surface extending parallel to and / or facing the first upper surface, (ii) Preferably the thickness of the substrate body measured between the first upper surface and the second upper surface is 500 μm or less, preferably 400 μm or less, more preferably 300 μm or less, more preferably 200 μm or less, more preferably 100 μm or less, more preferably 70 μm or less, more preferably 50 μm or less, more preferably 30 μm or less, and most preferably 10 μm or less. and / or (iii) 1. The characterized surface extends between the first upper surface and the second upper surface. 2. The characterized surface is connected at least partially to the first upper surface and / or the second upper surface, 3. At least one side of the substrate body, preferably at least a portion of the circumferential side, has a characterized surface. 4. Advantageously, at least a portion of the surface of the through-hole extending from the first upper surface to the second upper surface has a characterized surface, and advantageously, the through-hole is formed by affecting and / or etching the substrate material. 5. At least one surface region of a cavity in the substrate body has a characterized surface, the cavity is advantageously accessible from the outside or completely enclosed within the substrate material, and advantageously the cavity is formed by affecting and / or etching the substrate material. 6. The characterized surface is at least partially an inward-facing surface of the substrate body, and / or 7. The characterized surface is, at least partially, an outward-facing surface of the substrate body.

[0209] Alternatively or additionally, after patterning the characterized surface, the first curved profile of the characterized surface extends perpendicular to the principal elongation direction of the characterized surface. and / or It may be intended that the characterized surface has a second curved profile, at least partially, in the main stretching direction of the characterized surface, particularly in the circumferential direction of the substrate body.

[0210] Alternatively or additionally, in at least one cross-sectional plane of the substrate body, the characterized surface has a contour along a first curved profile, and the contour is (i) curved in a convex or concave manner, at least partially (ii) It corresponds at least partially to the curved contour of the area of ​​action, and / or (iii) It may be intended that the profile has, at least in part, a parabolic profile, a quarter-circular profile, a logarithmic profile, a profile following a polynomial function of degree n, favorably an even n, in particular n=6, n=8, n=10 or n=12, and / or a C-shaped profile.

[0211] These features have already been described in the section on the corresponding features of the first aspect of the present invention. That description will be applied mutatis mutandis here. Therefore, you can refer to that description.

[0212] This problem is advantageously solved by proposing a substrate body according to the second aspect of the present invention, according to the third aspect of the invention. The substrate body has at least one spatial modification of the substrate material, such as a change in refractive index, a change in density, and / or a cavity, at least in a partial region. The modified portion has a curved contour in at least a partial region of the cross-sectional plane of the substrate body. Advantageously, the modified portion extends from the first upper surface of the substrate body into the substrate material, particularly toward and to the second upper surface of the substrate body, and / or to the second upper surface of the substrate body, the second upper surface being advantageously opposite to and / or parallel to the first upper surface. Advantageously, the substrate body has a thickness of 500 μm or less, particularly measured between the first upper surface and the second upper surface of the substrate body.

[0213] A substrate body is provided for the first time that, despite its small thickness, can have corresponding modified sections with curved contours patterned in the cross-sectional plane.

[0214] In particular, this has not been possible with respect to such thin substrate bodies until now. In this case, the conventional method will result in the same problems as described above with respect to the second aspect of the present invention.

[0215] An electromagnetic field can be formed even within the extremely thin substrate body, allowing it to appropriately influence the substrate material. As a result, even a thin substrate body can be equipped with such a modification function, making it ideal for microsheets.

[0216] The modified portion may be, for example, a change in the refractive index and / or density of the substrate material. The modified portion may also be a cavity in the substrate material.

[0217] The substrate itself is advantageous if its thickness is 400 μm or less, 300 μm or less, 200 μm or less, 100 μm or less, 50 μm or less, or 10 μm or less.

[0218] The substrate itself is advantageously characterized by a thickness of 0.1 μm or more, 1 μm or more, 10 μm or more, 50 μm or more, or 100 μm or more.

[0219] In one embodiment, the substrate body is made of glass, glass ceramic, silicon, or sapphire, or has one of these materials.

[0220] Alternatively or additionally, the modified portion has a maximum deviation from the linear profile of over 20 μm, over 40 μm, over 60 μm, over 80 μm, or over 100 μm. and / or The length of the modified portion may be intended to be greater than 0.1 mm, 0.3 mm, 0.5 mm, 0.7 mm, 1 mm, 3 mm, or 5 mm in each case.

[0221] These features have already been described in the section on the corresponding features of the first aspect of the present invention. That description will be applied mutatis mutandis here. Therefore, you can refer to that description.

[0222] Further features and advantages of the present invention will become apparent from the following description, in which preferred embodiments of the invention are described with reference to schematic drawings. [Brief explanation of the drawing]

[0223] [Figure 1] This is a top view of the first circuit board body. [Figure 2] This figure shows the first substrate body in a first cross-sectional view. [Figure 3] This figure shows the first substrate body in the second cross-sectional view. [Figure 4a] This is a top view of the first substrate body having the affected substrate material. [Figure 4b] This is a side view of the first substrate body having the affected substrate material. [Figure 5] This figure shows different profiles of the side surfaces of the first substrate body after the etching process, as depicted in the cross-sectional plane of the first cross-sectional view. [Figure 6a] This figure shows the first substrate body after the etching process in the cross-sectional plane of the first cross-sectional view. [Figure 6b] This figure shows the first substrate body after the etching process in the cross-sectional plane of the second cross-sectional view. [Figure 7a] This is a top view of the second circuit board. [Figure 7b] This figure shows the second substrate body in a cross-sectional view. [Figure 8a] This is a top view of the third circuit board. [Figure 8b] This figure shows the third substrate body in a cross-sectional view. [Figure 9] This figure shows the effect of the focal length of a focusing optical system on a laser beam. [Figure 10] This diagram shows the line focus when the laser output is changed. [Figure 11] This diagram shows various line focus points on the main body of the circuit board. [Figure 12a] This figure shows line foci for different phase functions. [Figure 12b] This figure shows line foci for different phase functions. [Figure 12c] This figure shows line foci for different phase functions. [Figure 13]This diagram shows the optical setup for a 2f configuration. [Figure 14] This diagram shows the phase shift represented by Gray value coding. [Figure 15] This is a top view of the processed circuit board. [Figure 16] This is a top view of the processed circuit board. [Figure 17] This is a diagram showing the circuit board body modified from Figure 16. [Figure 18a] This is a cross-sectional view of the substrate body in which the curved working region is confined. [Figure 18b] This is a cross-sectional view of a substrate body having a material change section that can be accessed from the outside. [Figure 18c] This is a cross-sectional view of the patterned circuit board.

[0224] Examples Figure 1 shows a top view of a cubic, transparent substrate body 1. The substrate body 1 is made of glass; that is, its substrate material is glass.

[0225] The side surface 3 of the main board 1 on the right side of Figure 1 is patterned. In other words, a new shape is given to side surface 3.

[0226] Figure 2 shows a cross-sectional view of the substrate body 1, and this cross-sectional plane extends parallel to the first upper surface 5 of the substrate body 1.

[0227] To pattern a new surface on side 3 that had not been patterned before, the substrate material of the substrate body 1 is uniformly exposed to an electromagnetic field in multiple curved action regions 7a to 7c. The electromagnetic field causes a nonlinear interaction with the substrate material in each of the action regions. As a result of this nonlinear interaction, the substrate material is affected in the curved action regions 7a to 7c. This effect is accompanied by a change in the refractive index of the substrate material.

[0228] This electromagnetic field is the laser line focus formed within the substrate material. By moving the line focus relative to the substrate body 1, the laser line focus is continuously formed in different regions of the substrate material. That is, the substrate material is first affected in the curved action region 7a, then in the curved action region 7b, and then in the curved action region 7c.

[0229] The electromagnetic field at the line focus corresponds in particular to individual curved regions of action. Each of these curved regions of action also corresponds in each case to a region containing the affected substrate material.

[0230] The laser beam can be propagated by a spatial light modulator, and depending on the applied phase, the line focus will also be curved, thereby forming each curved region of action.

[0231] The individual curved action regions are spaced apart from each other. In the cross-sectional plane of Figure 2, the centroid (not shown) of the intersection of the curved action regions 7a-7c and the cross-sectional plane extends along a straight line parallel to the edge 9 of side surface 3.

[0232] Figure 3 shows the substrate body 1 in a different cross-sectional view. This cross-sectional plane extends perpendicularly to the first upper surface 5 of the substrate body 1 and intersects with the cross-sectional view of Figure 2 at the intersection line S shown by the dashed line. The crescent shape of the curved working region 7b can be seen in Figure 3. Other curved working regions that are not visible in Figure 3 have the same shape in their corresponding parallel cross-sectional planes.

[0233] If the cross-sectional planes in Figures 2 and 3 are moved parallel to each other, the shape of the common area with the curved region of action will also change. The specific way in which it changes depends on the three-dimensional shape of the curved region of action. The spatial shape of the curved region of action can be adjusted and adapted by the phase of the line focus.

[0234] As can be seen further in Figure 3, the curved working regions 7a to 7c intersect the first upper surface 5, the second upper surface 11, and the side surface 3 to be patterned of the substrate body 1 in each case. Therefore, the affected substrate material can be accessed from the outside at the corresponding common areas between the substrate body 1 and the curved working regions 7a to 7c.

[0235] Figure 4a shows a top view of the substrate body 1. In this figure, it can be seen that the curved working regions 7a to 7c have common parts with the first top surface 5. Figure 4b shows the substrate body 1 viewed from one side, and thus the side surface 3 to be patterned. In this figure as well, it can be seen that the curved working regions 7a to 7c have common parts with the side surface 3.

[0236] Subsequently, the affected substrate material is removed by applying selective laser etching. For this purpose, the substrate body 1 is exposed to the etching medium at least locally.

[0237] Laser selective etching removes both the affected and unaffected substrate materials from the substrate body 1. However, the affected substrate material is etched away more quickly than the unaffected substrate material.

[0238] Figure 5 shows the substrate body 1 in the same cross-sectional plane as already shown in Figure 2, but this is after the etching process. When only the affected substrate material is removed by the etching process, the patterned contour of the substrate body in the cross-sectional plane of Figure 5 extends along the solid line. The curved working regions 7a to 7c emboss a circular contour 13 onto the substrate material in the cross-sectional plane of Figure 5.

[0239] However, since this etching process also removes unaffected material, the substrate material 15 between and at the edges of the individual curved working regions is also partially etched away. As a result, the web between the regions containing the affected material is removed in particular. Furthermore, for the same reason, the circular contours 13 are also shifted entirely within the substrate material, as indicated by the slightly shifted dashed profile.

[0240] Therefore, the unpatterned side surface 3 of the substrate body 1 will have a contour following the dashed line after being patterned in the cross-sectional plane of Figure 5.

[0241] Figure 6a shows the profile of the patterned surface 17 in the cross-sectional plane of Figure 2, and Figure 6b shows the profile of the original unpatterned surface 3, indicated by dashed lines, in the cross-sectional plane of Figure 3. The patterned surface 17 has a height adjustment and partially has a dome-shaped structure corresponding to a dome-shaped recess.

[0242] As a result, the affected substrate material, as well as the unaffected substrate material, is removed by etching, forming a patterned surface 17. This patterned surface 17 is a characterized surface in the sense of the present invention.

[0243] The patterned surface 17 is connected to the first and second upper surfaces 5 and 11, at least partially. The patterned surface 17 is the outer surface.

[0244] The curved profile of the patterned side surface 17 shown in FIG. 6b is convex and corresponds to the first curved profile. The first curved profile was affected by the shape of the curved working area 7b. That is, although a part of the substrate material that was not affected was also removed by the etching process here, the basic profile of the patterned right side surface 17 of the substrate body 1 is partially co-determined in each case by the curved shape of the curved working area (in this case the curved working area 7b) applied thereto. Since the curved working areas 7a to 7c are involved in the surface patterning at a plurality of locations, the patterned surface 17 has the same first curved profile in a plurality of regions. This is because the curved shape of the curved working areas 7a to 7c may determine or affect the profile of the patterned surface 17 in a plurality of regions. In other words, the first curved profile is achieved by a plurality of curved working areas in a plurality of regions of the patterned or characterized surface 17.

[0245] The first and second upper surfaces 5, 11 of the substrate body 1 are parallel to each other in FIGS. 3 and 6b and have a distance of 500 μm from each other.

[0246] If the curved working areas 7a to 7c were rotated 180° about an axis perpendicular to the first upper surface 5, the first curved profile would be concave in the cross-sectional plane of FIG. 6b.

[0247] If the curved working areas 7a to 7c are positioned from the surface 3 to be patterned towards the middle of the substrate body 1, the substrate body 1 can be divided into two parts. In this case, at the separation surface, the remaining substrate body has a patterned surface such as the patterned surface 17 in the corresponding procedure as described above.

[0248] Figure 7a shows the substrate body 1' in a top view, and Figure 7b shows the substrate body 1' in a cross-sectional view. Here, the cross-sectional plane extends in a direction perpendicular to the first upper surface 5' of the substrate body 1', and intersects the cross-sectional view of Figure 7a indicated by the dotted line S' in the same figure. In the substrate body 1', the substrate material is affected only in a single curved working area 7'. The curved working area 7' extends from the first upper surface 5' towards the second upper surface 11'. When the affected material is etched away, a cavity can be created in the substrate body 1'. The surface of this cavity is a patterned surface and thus a characterized surface. In this case, the said surface becomes the inner surface.

[0249] Figure 8a shows the substrate body 1'' in a top view, and Figure 8b shows the substrate body 1'' in a cross-sectional view. Here, the cross-sectional plane extends in a direction perpendicular to the first upper surface 5'' of the substrate body 1'', and intersects the cross-sectional view of Figure 8a indicated by the dotted line S'' in the same figure. In the substrate body 1'', the substrate material is affected only in a single curved working area 7''. The curved working area 7'' extends from the first upper surface 5'' to the second upper surface 11''. When the affected material is etched away, a through-hole, that is, a via, can be created in the substrate body 1''. The surface of this through-hole is a patterned surface and thus a characterized surface. In this case, the said surface becomes the inner surface.

[0250] Effect of focal length in a focusing optical system Figure 9 shows the influence of the focal length of the focusing optical system in an airy laser beam. The following constants: - Cubic phase (β = 3 1 / 3 × 10 3 / m); - Laser wavelength (λ = 1.030 × 10 -6 m); and - Beam diameter (diameter of the raw beam w0 = 5 × 10 -3 m) in which, as the focal length increases, the length of the focal region (relative definition: 1 / e of the maximum value 2The decrease in (the value) becomes larger (solid curve in Figure 9), and the angle that the upper and lower focal points have with respect to the optical axis in each case becomes smaller (dashed curve in Figure 9). Therefore, the left vertical axis relates to the solid line, and the right vertical axis relates to the dashed line.

[0251] Effect of laser power on line focus Figure 10 shows the material regions of a glass substrate affected by line focal points with different laser power outputs. As the laser power increases from top to bottom, the curved area of ​​effect expands, and consequently, the affected area of ​​material also increases.

[0252] Effects of tilt and displacement of the line focus "Misalignment" refers to the distance between the vertices of the focal region from the center of the substrate. "Slope" refers to the angle between the surface normal and the tangent to the vertex.

[0253] When an un-tilted Airy beam is placed at the center, the vertex of the focal region along the normal to the substrate surface is in the middle of the substrate itself, that is, in the middle of the extension in the thickness direction, and the tangent to the surface normal and the vertex are parallel.

[0254] Figure 11 shows various line focal points 23a to 23e of the laser beam formed at least partially on the substrate body 21. The cross-sectional plane in Figure 11 shows the thickness region of the substrate body 21.

[0255] The linear focus 23a specifically represents the linear focus of an Airy beam, is centrally located, and has no inclination. The linear focus 23a has the vertex 25 of the focal region 23a of the parabola.

[0256] Line focus 23b specifically indicates the line focus of the Airy beam and is shifted.

[0257] Line focus 23c specifically represents the line focus of an Airy beam, which is tilted and shifted.

[0258] The line focus 23d represents a line focus with a variable curvature, particularly for functions other than Airy beams. For example, the curvature can represent a C-profile.

[0259] The line focus 23e represents the line focus of a function, particularly an Airy beam, and modifies the upper part of the substrate material 1 in the first region 27a and the lower part of the substrate 1 in the second region 27b.

[0260] In Figure 11, the lengths of the individual line foci 23a to 23e can also be defined as the lengths of the curved profiles shown inside the substrate body 1. Furthermore, a connecting line 29 is shown at line foci 23a, passing through the end of line foci 23a inside the substrate body 21. This can be understood as representing a straight focal line, and the maximum deviation from the straight focal line corresponds in particular to the distance between the connecting line 29 and the vertex 25.

[0261] Phase function The following table shows various exemplary phase functions that can be applied to a laser beam, and how these can be used to form a curved working region on the substrate material. [Table 1]

[0262] This parameter is described in the publication Froehly, L., Courvoisier, F., Mathis, A., Jacquot, M., Furfaro, L., Giust, R., ... & Dudley, JM (2011). Arbitrary accelerating micron-scale caustic beams in two and three dimensions. Optics express, 19(17), 16455–16465.

[0263] Figures 12a to 12c show examples of line foci for different phase functions. The unit of the horizontal axis is millimeters (mm) in all cases. The unit of the vertical axis is millimeters (mm) in all cases. Figure 12a shows a laser beam of a line focus having a parabolic acceleration profile. Figure 12b shows a laser beam of a line focus having a quarter-circle acceleration profile. Figure 12c shows a laser beam of a line focus having a logarithmic acceleration profile. By the corresponding line foci, different curved action regions can be realized, and thus the substrate material can be affected in the corresponding spatial region.

[0264] The overall theoretical profile of the line focus according to the phase function is shown by a dashed line in each case. The line focus itself is formed only along one section (slightly shifted partially to enable recognition of the theoretical profile). Nonlinear interactions can occur only where the line focus is formed. Thus, it is basically possible to understand how an externally accessible cavity or a completely confined cavity can be obtained using the line focus.

[0265] Further characteristics Figure 13 shows an optical setup of a 2f configuration that can be advantageously used in the method according to the present invention. In this case, a phase distribution is applied to an incident laser beam 35 having a beam diameter 36 by a phase mask 33, and the incident laser beam is imaged from the phase mask at a distance corresponding to its output focal length 39 by a subsequent focusing optical system 31 located at a distance of its input focal length 37, so that a curved line focus 23 is formed inside the substrate 1.

[0266] Figure 14 shows an exemplary phase shift applied to a laser beam 35 by a phase mask 33 that can be advantageously realized in the form of an SLM (spatial light modulator) or a DOE (diffractive optical element), represented by gray value coding, whereby a curved contour 23 of the laser focus is obtained. In this case, the phase values from 0 to 2Pi are represented by gray values from 0 to 255. The phase distribution exists in a cross-section perpendicular to the main propagation direction of the laser beam.

[0267] Figure 15 shows a top view of a substrate body patterned by the method according to the present invention. In particular, the normal vector of the characterized surface extends within the diagrammatic plane of Figure 15. Thus, in Figure 15, the first curved profile of the characterized surface can be recognized particularly advantageously.

[0268] The laser beam used for patterning extended parallel to the plane in Figure 15, as indicated by the arrow.

[0269] - For patterning the characterized surface, the following general and laser parameters were set: - Microscope objective lens and Fourier lens (focal length f=10mm); - Wavelength 1030nm; - Beam diameter 5.3 mm; - Topology of a cube φ = exp(i*(x 3 +y 3 )) and φ = exp(iβ / 3*(x 3 +y 3 )) is equivalent to, and in the formula, β=3 1 / 3 mm -1 x and y are in millimeters; - Pulse width τ = 5 ps; - Number of pulses in a burst of N=2; - Energy per burst: 228 μJ; and - Pitch: 10 μm.

[0270] Figure 16 shows a top view of a substrate body patterned by the method according to the present invention. In particular, the normal vector of the characterized surface extends within the figure plane of Figure 16. Therefore, in Figure 16, the first curved profile of the characterized surface can be recognized particularly advantageously.

[0271] The laser beam used for patterning extended parallel to the plane in Figure 16, as indicated by the arrow.

[0272] For patterning the characterized surface, the following general and laser parameters were set: - Substrate material having a thickness selected from the range of 900 to 1000 μm, e.g., BF33; - Pitch: 40 μm; - Microscope objective lens and Fourier lens (focal length f=10mm); - Beam expander with a magnification of 2.0 (especially for a 10mm diameter Gaussian input beam); - Pulse width τ = 5 ps; - Number of pulses in a burst of N=2; - Energy per burst: 300 μJ; and - Wavelength 1030nm; - Topology of a cube φ = exp(i*(x 3 +y 3 )) and φ = exp(iβ / 3*(x 3 +y 3 )) is equivalent to, and in the formula, β=3 1 / 3 mm -1 x and y are in millimeters.

[0273] As in this case, by selecting a sufficiently large pitch, interaction between adjacent regions within the substrate having the modified portion is avoided or at least significantly reduced.

[0274] Figure 17 shows a transmitted light microscope image of the substrate after the laser process but before etching (viewed parallel to the laser propagation direction) on the left. Lateral application of the modified area is shown, with the modified area indicated at three selected different depths of the substrate. Each depth is indicated on the right side of Figure 17.

[0275] When introducing the modifications, a sufficiently large pitch was selected so that the spread of the laterally angled / arrow-shaped modifications overlapped minimally. This ensured that propagation within the material was not obstructed, or only slightly obstructed, by the aforementioned modifications.

[0276] The "zigzag" pattern is due to a modification that extends laterally near the focal point, while the modification remains on a straight line. Furthermore, the apex of the curved working region is held midway between the two upper surfaces, and the curved working region was fully formed within the substrate material.

[0277] Further Embodiments Figure 18a shows a cross-sectional view of the rectangular substrate body 41. Inside the substrate body 41, the substrate material is exposed to an electromagnetic field in a curved working region 43, and in the corresponding region, the substrate material is modified by a nonlinear interaction between the electromagnetic field and the substrate material due to nonlinear absorption.

[0278] The curved working region 43, and consequently the modified portion after the introduction of said region 43, are completely enclosed within the main body of the substrate 41.

[0279] Therefore, according to embodiments of the present invention, for example, material is intended to be removed from the substrate body by etching. This can be done along the main stretching direction H of the curved working region 43, which in this case extends perpendicular to the two upper surfaces 45. In other words, material is removed from the two upper surfaces 45 of the substrate body 41. As a result, the new upper surface 45 of the substrate body is shifted, so to speak, along the main stretching direction H. This can be seen in Figure 18b. Furthermore, in the same figure, it can be seen that since a portion of the affected substrate material is now located on the surface of the upper surface 45, the substrate material 43 affected in the confined curved working region 43 becomes accessible from the outside by the removal of the substrate material.

[0280] The curved action region 43 or the substrate material 43 affected thereby has a profile that is not affected by surface effects (e.g., the top surface 45) because the interaction takes place entirely within the substrate body 41 (Figure 18a).

[0281] Since the modified substrate material 43 (Figure 18b) is accessible, the substrate body 41 can then be further processed as described above to pattern the characterized surface 47 as shown in Figure 18c. For example, the affected material 43 can be removed by etching.

[0282] The features disclosed in the above description, claims, and drawings may be important to the present invention, either individually or in any combination, in various embodiments thereof. [Explanation of Symbols]

[0283] 1,1',1'' Main board 3 Sides 5,5',5'' top surface 7a-7c Curved area of ​​action 7',7'' Curved area of ​​action 9 Edge 11,11',11'' top surface 13 Outline 15 Substrate materials 17 Surface 21 Main board 23a~23e Line focus 25 vertices 27a,27b area 29 Connecting Line 31 Imaging Optical System 33 Phase Mask 35 Laser beams 36 Laser beam diameter 37. Focal length of the input side 39. Output focal length 41 Main board 43. Curved area of ​​action 45 Top 47 Surface H Main stretching direction S,S',S'' intersection line

Claims

1. 1. A method for preparing and / or carrying out patterning of a defined or predeterminable characterized surface of a substrate body having a substrate material, comprising: The method includes exposing the substrate material in at least one curved region of action to an electromagnetic field that causes a nonlinear interaction between the electromagnetic field and the substrate material in each of the at least one curved region of action, thereby at least partially affecting the substrate material disposed in the curved region of action; after patterning the characterized surface, the characterized surface has, at least in part areas, at least one first curved profile that is at least partially determined and / or influenced by the curved shape of the at least one curved active area, The method, wherein the nonlinear interaction causes at least one nonlinear absorption of the electromagnetic field in the substrate material.

2. exposing the substrate material to an electromagnetic field at a plurality of curved regions of effect; Here, advantageously (i) the characterized surface has the same first curved profile in multiple regions, in particular determined or influenced by the curved shapes of the multiple curved active regions and / or has the first curved profile throughout; and / or (ii) The method according to claim 1, wherein the curved active areas are selected to be arranged at a distance from one another, in particular in a cross-sectional plane of the substrate body, such that the centers or centroids of the intersections of the curved active areas with the cross-sectional plane extend along a straight line or along any, in particular circular, curve, and / or successive active areas have a distance from one another that is 30% to 100% or 100% to 200% of the maximum extent of the curved active areas in the cross-sectional plane.

3. Influencing the substrate material comprises at least partially changing, in particular increasing or decreasing, one or more material properties, such as in particular the refractive index, etching rate and / or density of the substrate material, and / or 3. The method according to claim 1 or 2, wherein influencing the substrate material comprises at least partially removing and / or excluding the substrate material from the curved area of ​​action, in particular compressing the substrate material into the surrounding substrate material.

4. 4. The method according to claim 1, wherein the characterized surface is formed by at least partially removing the substrate material by the impacting and / or by at least partially removing the affected substrate material by at least a subsequent etching process, in particular a wet chemical process, using an acid and / or alkaline liquid, preferably using a potassium hydroxide solution as etching medium.

5. 5. The method according to claim 1, wherein the electromagnetic field is provided in the form of and / or by a curved line focus, in particular a laser beam, and / or the curved area of ​​action is determined by the shape of the line focus.

6. the laser beam is provided by an ultrashort pulse laser; adjusting and / or adapting the phase of the laser beam, in particular using a combination of a spatial light modulator, a diffractive optical element and / or a plurality of cylindrical lenses; the laser beam is focused onto the substrate body, preferably by means of a microscope objective or a Fourier lens, wherein the focusing is preferably carried out after adjusting or adapting the phase of the laser beam and / or forming the line focus, said line focus being that of an accelerated laser beam, in particular an Airy beam; The wavelength of the laser beam is 1064 nm, the microscope objective lens or Fourier lens has a focal length of 10-20 mm, and the cubic phase coefficient (laser parameter β) is 0.5×10 3 / m ~ 5 x 10 3 / m and the raw beam diameter (laser parameter ω 0 ) has a value of 1 mm to 10 mm, preferably 2.5 mm to 5 mm, the pulse duration (laser parameter τ) has a value of 0.1 to 10 ps, ​​and the pulse energy (laser parameter E p ) has a value of 1 to 1500 μJ, preferably 30 to 500 μJ, in particular 474 μJ, and / or the number of pulses in the burst (laser parameter N) has a value of 1 to 200, preferably 1 to 100, in particular 1 to 8, The spatial extent of the curved active areas, advantageously one of its length and / or its diameter, is adjusted and / or varied over time by varying the average power range of the laser and / or by varying the phase, in particular adjusting different extents for at least some of the curved active areas, and / or 6. The method of claim 5, wherein the spatial orientation of the curved active areas is adjusted and / or varied over time by changing the tilt of the optical axis of the laser beam relative to the normal of the substrate surface, in particular the substrate surface at which the laser beam is incident on the substrate body, in particular adjusting different orientations for at least some of the plurality of curved active areas.

7. 7. The method according to claim 1, wherein at least one auxiliary substrate body is arranged on the substrate body, at least during the nonlinear interaction, and each of the curved areas of action and / or the line foci extends at least partially within the auxiliary substrate body, and preferably, two or more auxiliary substrate bodies are arranged on the substrate body, in particular on opposite sides of the substrate body, and each of the curved areas of action and / or the line foci extends at least partially within two or more auxiliary substrate bodies.

8. at least one, preferably a plurality and / or all of the at least one curved active area are completely confined within the substrate body, in particular at least during the nonlinear interaction, 8. The method according to claim 1, further comprising removing material from the substrate body at least in a partial area, in particular along the main direction of extension of the curved active area in the substrate body, so that the substrate material affected in the confined curved active area is at least partially and / or partially accessible from the outside, in particular by carrying out the removal of material from the substrate body by etching.

9. exposing the substrate material to the electromagnetic field in individual areas of the plurality of curved active areas sequentially, totally or partially in parallel; (i) simultaneously exposing the entire substrate material within a curved area of ​​effect to the electromagnetic field; (ii) the curved active area has in each case a maximum deviation from a straight profile of more than 20 μm, more than 40 μm, more than 60 μm, more than 80 μm or more than 100 μm; and / or 9. The method of any one of claims 1 to 8, wherein (iii) the length of the curved area of ​​action is in each case greater than 0.1 mm, greater than 0.3 mm, greater than 0.5 mm, greater than 0.7 mm, greater than 1 mm, greater than 3 mm or greater than 5 mm.

10. (i) the substrate body is transparent, made of glass, and has a first top surface and / or a second top surface, preferably extending parallel to and / or opposite to the first top surface; (ii) the thickness of said substrate body, advantageously measured between said first top surface and said second top surface, is 500 μm or less, advantageously 400 μm or less, more preferably 300 μm or less, more preferably 200 μm or less, more preferably 100 μm or less, more preferably 70 μm or less, more preferably 50 μm or less, more preferably 30 μm or less, and most preferably 10 μm or less; and / or (iii) after patterning the characterized surface, 1. The characterized surface extends between the first upper surface and the second upper surface; 2. The characterized surface is at least partially connected to the first upper surface and / or the second upper surface; 3. At least one side surface of the substrate body, preferably at least a portion of a circumferential side surface, has the characterized surface; 4. At least a portion of the surface of the through hole, which preferably extends from the first upper surface to the second upper surface, has a characterized surface, and preferably the through hole has been formed by affecting and / or etching the substrate material; 5. At least one surface area of ​​a cavity in the substrate body has the characterized surface, the cavity being advantageously accessible from the outside or completely enclosed in the substrate material, advantageously formed by affecting and / or etching the substrate material; 6. The characterized surface is at least partially an inwardly facing surface of the substrate body; and / or 7. Method according to any one of claims 1 to 9, wherein the characterized surface is at least in part-area an outwardly facing surface of the substrate body.

11. after patterning the characterized surface, the first curved profile of the characterized surface extends perpendicular to a main extension direction of the characterized surface; and / or 11. The method according to claim 1, wherein the characterized surface has a second curved profile at least in part areas in the main direction of extension of the characterized surface, in particular in the circumferential direction of the substrate body.

12. After the patterning of the characterized surface in at least one cross-sectional plane of the substrate body, the characterized surface has a contour along the first curved profile, the contour comprising: (i) at least partially convexly or concavely curved; (ii) corresponds, at least in part, to the contour of the curved working area; and / or 12. The method according to claim 1, wherein the coating has at least partially a parabolic profile, a quadrant profile, a logarithmic profile, a profile according to a polynomial function of degree n, preferably an even number n, in particular n=6, n=8, n=10 or n=12, and / or a C-shaped profile.

13. A substrate body, It has at least a first upper surface and at least one characterized surface, in particular produced or producible according to the method of any one of claims 1 to 12, the characterized surface has, at least in part, at least one first curved profile; the first curved profile is located in a cross-sectional plane of the substrate body fixed in a plane having at least one normal vector of the characterized surface and a normal vector of the top surface; the first curved profile can be described, at least in part, by a parabolic, quadratic, logarithmic and / or polynomial phase function; The substrate body has a thickness of 500 μm or less.

14. the characterized surface has a strength of at least 100 MPa, advantageously at least 150 MPa, more preferably at least 200 MPa; Advantageously, the characterized surface has been etched, in whole or in part, in particular with hydrofluoric acid, sodium hydroxide, an alkaline solution, for example potassium hydroxide solution, and / or an acid.

15. 15. The substrate body according to claim 13 or 14, wherein the characterized surface is height-adjusted at least in part of its area, in particular having a wave-like and / or domed structure, advantageously along and / or perpendicular to the main direction of extension of the characterized surface.

16. (i) the substrate body is transparent, made of glass, and has a first top surface and / or a second top surface, preferably extending parallel to and / or opposite to the first top surface; (ii) the thickness of said substrate body, advantageously measured between said first top surface and said second top surface, is 500 μm or less, advantageously 400 μm or less, more preferably 300 μm or less, more preferably 200 μm or less, more preferably 100 μm or less, more preferably 70 μm or less, more preferably 50 μm or less, more preferably 30 μm or less, and most preferably 10 μm or less; and / or (iii) 1. The characterized surface extends between the first upper surface and the second upper surface; 2. The characterized surface is at least partially connected to the first upper surface and / or the second upper surface; 3. At least one side surface of the substrate body, preferably at least a portion of a circumferential side surface, has the characterized surface; 4. At least a portion of the surface of the through hole, which preferably extends from the first upper surface to the second upper surface, has a characterized surface, and preferably the through hole has been formed by affecting and / or etching the substrate material; 5. At least one surface area of ​​a cavity in the substrate body has the characterized surface, the cavity being advantageously accessible from the outside or completely enclosed in the substrate material, advantageously formed by affecting and / or etching the substrate material; 6. The characterized surface is at least partially an inwardly facing surface of the substrate body; and / or 7. The characterized surface is the outward facing surface of the substrate body at least in part of the area; The substrate body according to any one of claims 13 to 15.

17. the first curved profile of the characterized surface extends perpendicular to a main direction of extension of the characterized surface; and / or 17. The substrate body according to claim 13, wherein the characterized surface has a second curved profile at least in a partial area in the main direction of extension of the characterized surface, in particular in the circumferential direction of the substrate body.

18. In at least one cross-sectional plane of the substrate body, the characterized surface has a contour along the first curved profile, the contour comprising: (i) at least partially convexly or concavely curved; (ii) corresponds, at least in part, to the contour of the curved working area; and / or (iii) The substrate body according to any one of claims 13 to 17, which at least partially has a parabolic profile, a quadrant profile, a logarithmic profile, a profile according to a polynomial function of degree n, preferably an even number n, in particular n=6, n=8, n=10 or n=12, and / or a C-shaped profile.

19. the substrate body has at least one spatial modification of the substrate material, such as a refractive index change, a density change and / or a cavity, at least in a partial area thereof, The modified portion has a contour that is curved at least in a partial area in a cross-sectional plane of the substrate body, Advantageously, the modification extends from a first upper surface of the substrate body into the substrate material, in particular in the direction of and / or up to a second upper surface of the substrate body, which second upper surface is advantageously opposite to and / or extends parallel to the first upper surface, Advantageously, the substrate body has a thickness of 500 μm or less, measured in particular between the first upper surface and the second upper surface of the substrate body.

20. the alteration has a maximum deviation from a straight profile of more than 20 μm, more than 40 μm, more than 60 μm, more than 80 μm or more than 100 μm; and / or 20. The substrate body according to claim 19, wherein the length of the alteration is in each case greater than 0.1 mm, greater than 0.3 mm, greater than 0.5 mm, greater than 0.7 mm, greater than 1 mm, greater than 3 mm or greater than 5 mm.