Method for pressing stamped sheet metal parts into a laminate stack
Patent Information
- Application Number
- JP2021566459
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2019-05-08
- Filing Date
- 2020-05-08
- Publication Date
- 2024-12-09
- Estimated Expiration
- 2040-05-08
AI Technical Summary
Existing methods for laminating sheet metal parts require precise positioning of release elements, which can damage press dies and are costly, and lack efficient separation mechanisms.
A method involving a second profile stamping step to create recesses in an electromagnetic steel strip for receiving release elements, allowing them to be integrated with the strip and positioned accurately, eliminating the need for additional release elements and reducing die damage.
Ensures high stability and reproducibility in lamination, extends press die life, and improves process efficiency by reducing waste and maintaining throughput.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method of laminating a plurality of press-worked sheet metal parts to form a plurality of laminated stacks, the method comprising: first, blanking a first sheet metal part from an electromagnetic steel strip having a curable adhesive layer, particularly a hot melt adhesive coating layer, on at least one of its planar sides; and subsequently laminating the plurality of first sheet metal parts and joining the plurality of first sheet metal parts by bonding, particularly bonding between materials. The method includes means for facilitating the separation of the joined first sheet metal parts into laminated stacks, the means comprising laminating at least one release element together with the plurality of sheet metal parts.
Background Art
[0002] Providing a release element between a plurality of first sheet metal parts laminated in a vertical hole adjacent to the final press stage of a progressive press die is known from the prior art (International Publication No. 2017 / 060483). This release element, for example, a surface provided with a non-stick coating, reduces the adhesiveness of the curable polymer adhesive layer of the adjacent first sheet metal part and facilitates the separation of the plurality of laminated stacks of the plurality of sheet metal parts joined by material bonding. Such a release element is inserted under the electromagnetic steel strip for blanking in the final press process, enters the vertical hole by blanking the first sheet metal part, and forms a laminated stack with other blanked first sheet metal parts. The drawback is that when inserting this release element under the electromagnetic steel strip, relatively high-precision positioning is required so that the release element is not similarly blanked, and if the release element is similarly blanked, it may cause damage to the press die, especially.
Prior Art Documents
Patent Documents
[0003]
Patent Document 1
Summary of the Invention
Problems to be Solved by the Invention
[0004] The object of the present invention is to improve the above-described method so that high stability is guaranteed even when the release element is used in lamination together with multiple first sheet metal parts. [Means for solving the problem]
[0005] The problems of the present invention are solved by the function of claim 1.
[0006] If the means for facilitating the separation of a plurality of joined first sheet metal parts into a laminated stack includes a second outline punching step that punches out at least one second sheet metal part preceding the first outline punching step, then the electrical steel strip may already be included in the steps for facilitating the separation of a plurality of joined first sheet metal parts into a laminated stack. The electrical steel strip has recesses from the second outline punching step that can function as receivers on the electrical steel strip side.
[0007] By pushing the release element back onto the portion of the electromagnetic steel strip from which the second sheet metal part has been punched, the release element can bond with the electromagnetic steel strip and be supplied together to the first outer shape punching process.
[0008] In other words, the release elements are supplied to the lamination process in the same manner as the first sheet metal parts. Therefore, expensive means of inserting the release elements between multiple sheet metal parts at the final press stage can be avoided, and this can be achieved by punching the release elements from the electrical steel strip using the first outer shape punching process. Furthermore, the positioning of the electrical steel strip at the first press stage ensures reproducible alignment of the release elements using the press stage, thus reliably preventing damage to the press stage. Thus, in contrast to the prior art, the method of the present invention can achieve a particularly long service life.
[0009] For example, the curable adhesive layer may be polyvinyl butyral, polyamide, polyester, modified polyamide, or epoxy resin. Preferably, the adhesive layer is a baked varnish, and especially a thermosetting varnish. Coating with a curable polymer adhesive has been found to be advantageous.
[0010] If this method includes a step of deactivating, curing, and / or removing the adhesive layer of the second sheet metal part, this second sheet metal part can be used as a release element. This not only eliminates the need for additional release elements, but also ensures that the pushed-back release element always corresponds to the dimensions of the punched area of the electrical steel strip. Thus, the release element can be bonded to the electrical steel strip with high repeatability, further extending the service life of the press die.
[0011] The second sheet metal part can be provided as a release element for the electrical steel strip, provided that it is at least partially removed during the pushback process. Lengthening can be achieved, for example, by tension, pressing, etc.
[0012] When a second sheet metal part is joined to a first sheet metal part to form a laminated stack, the second sheet metal part can also be used as part of the laminated stack, further improving the efficiency of use when forming a laminated stack from electrical steel strips, thereby reducing waste.
[0013] Even if measures are taken to facilitate the separation of the joined first sheet metal parts into a laminated stack, the process throughput can be maintained without change if the second outer shape punching process and the push-back process are performed in different stages in the press die.
[0014] The second outer shape punching process could also be performed using a progressive die, similar to the first outer shape punching process performed on a second press stage. In other words, there would be no need to modify the design of the progressive die to bond the release element to the electrical steel strip.
[0015] Alternatively, the second outer shape punching process could be performed on a third press stage downstream of the press die used for the first outer shape punching process on the second press stage. This would require a design change to a progressive press die known in the prior art, but it would further improve the reproducibility of the process by synchronizing each stage.
[0016] If a pushback is applied in the stage immediately preceding the first outer shape punching process, the release element will not be punched out in the preceding stage of the progressive press die, thereby improving process reliability.
[0017] By performing the second outer shape punching process on the stage immediately following the pushback, idle operation of the preceding stage of the progressive press die can be avoided. This, in particular, reduces the risk of damage to the press die or cooperating dies.
[0018] If at least one guide hole is punched before or during the second outer shape punching process, the release element and the electrical steel strip can be relatively positioned on this guide hole during the pushback process, further improving the reliability of the process.
[0019] If the outer dimensions of the second sheet metal part are punched out to be smaller than those of the first sheet metal part, the electrical steel strip can be prepared in a particularly advantageous manner for pushback.
[0020] Preferably, the second sheet metal part is punched out so that its outer diameter is reduced by up to 2 mm.
[0021] When an interference fit is formed between the release element and the electrical steel strip, the release element can be firmly held in place by the electrical steel strip. If there are protrusions on the release element and / or electrical steel strip that form an interference fit, this interference fit can be formed with particularly good reproducibility.
[0022] Advantageously, the release element is configured to reduce the adhesive force with an adjacent first sheet metal part in order to facilitate separation of the joined plurality of first sheet metal parts into a plurality of stacked stacks.
[0023] Advantageously, it can be seen that using at least one release element pushed back onto a part of an electromagnetic steel strip having a curable adhesive layer facilitates separation of the joined plurality of first sheet metal parts into a plurality of stacked stacks during press lamination.
[0024] In the figures, for example, the objects of the present invention are shown in detail based on several embodiments.
Brief Description of the Drawings
[0025] [Figure 1] FIG. 1 is a side view, with a break, of a part of an apparatus for implementing the method according to the first embodiment. <http: / / www.google.com / patents / US0000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000000L [Figure 2a] FIG. 2a is a top view of the electromagnetic steel strip in the apparatus shown in FIG. [Figure 2b] FIG. 2b is a detailed view of FIG. 2a. [Figure 3] FIG. 3 is a side view of an apparatus for implementing the method according to the second embodiment.
Embodiments for Carrying Out the Invention
[0026] In the first embodiment shown in FIG. 1, an apparatus 1 for implementing the method of the present invention is schematically shown. This apparatus 1 is used to stack a plurality of punched sheet metal parts 2 into a plurality of stacked stacks 3. For this purpose, the electromagnetic steel strip 5 is unwound from the coil 4, and one or both of its functional surfaces 6, 7 have a completely flat, curable polymer adhesive layer 8, 9, that is, a hot melt adhesive layer, for example, a thermosetting sintering varnish. These adhesive layers 8, ʘ are, for example, shown in the enlarged part of FIG. 1.
[0027] Such thermosetting or thermosetting hot-melt adhesives or hot-melt adhesive layers are known as baking varnishes. For example, the hot-melt adhesive varnish may be epoxy resin-based. Preferably, the hot-melt adhesive varnish is a bisphenol epoxy resin system using, for example, a dicyandiamide-based curing agent. In particular, the hot-melt adhesive varnish mentioned may be a bisphenol A epichlorohydrin resin system using dicyandiamide as a curing agent. This two-step curing epoxy resin system is in state B on electrical steel strip. Therefore, the partially cross-crosslinked hot-melt varnish is still reactive. Heating allows the reaction of the hot-melt varnish in state B to proceed, and thus transition to a fully cross-crosslinked state C, also referred to as bonded. Typically, the thickness of this partially cross-crosslinked hot-melt coating is several microns.
[0028] Multiple first sheet metal parts 2 are punched out or separated from a baking lacquer-coated electrical steel strip 5 using a progressive die press 10.1. Such punching out processes generally include cutting, cutting, detaching, trimming, and press separation.
[0029] As shown in Figure 1, the press die 10 is, for example, a progressive punch die 10.1 in this case, which performs cutting with multiple strokes 11 of the upper die 12 cooperating with the lower die 13. For this reason, the punch die 10 is equipped with multiple press stages 14, 15, and 16.
[0030] The first punch 14.1 of the pre-processing press stage 14 of the upper die 11 is used to pre-process the electrical steel strip 5 for outer shape punching, and then the second punch 15.1 of the second and final press stage 15 of the upper die 11 is used for outer shape punching or separation of the first metal part 2 from the electrical steel strip 5. For this reason, the punches 14.1, 15.1, and 16.1 operate together with the respective dies 14.2, 15.2, and 16.2 of the press stages 14, 15, and 16 of the lower die 13.
[0031] Figure 1 shows such a progressive press die. In particular, it can be seen that part 17 is punched out in a pre-treatment press process in order to prepare the electromagnetic steel strip 5 for punching out the outer shape of the first sheet metal part 2.
[0032] The multiple first sheet metal parts 2, punched out by the press stage 15, are fed into the laminating device 18 by the pressure of the upper die 11 or punch 14.1 and stacked. For this purpose, the laminating device 18 is equipped with a vertical hole 18.1 and a counter plate 18.2 in the lower die 13. The counter plate 18.2 of the lower die 13 brakes the multiple first sheet metal parts 2, thereby physically and / or chemically bonding them together under the pressure of the upper die 11, utilizing the adhesive layers 8, 9 present between the multiple sheet metal parts 2. It is generally mentioned that the laminating device 18 may be actively heated to stack the multiple first sheet metal parts 2 in the vertical hole 18.1. In addition, the first stacked stack 3 may be subject to a curing process (not shown) to form material bonds between the multiple first sheet metal parts 2. Furthermore, although not shown in the diagram, it is also possible to remove the divided stacks of the stacked stack 3 from the stacking device 18 and rotate the stacking device 18 so that multiple first sheet metal parts 2 are arranged adjacently to each other and stacked on top of each other.
[0033] To facilitate the separation of multiple stacked sheets 3 as they exit the lamination apparatus 18, at least one release element 19 is laminated together with the multiple first sheet metal parts 2. For this purpose, the release element 19 is designed to reduce the adhesion force between at least one adjacent first sheet metal part 2 and the adhesive layers 8, 9. This reduces the bonding strength between the multiple first sheet metal parts 2 in adjacent stacked sheets 3, facilitating the separation of the bonded multiple first sheet metal parts 2 into the multiple stacked sheets 3.
[0034] According to the present invention, the release element 19 is inserted into the lamination apparatus 18 using the electric steel strip 5. Therefore, a second outer shape punching process is first performed on the press stage 16 by the cooperation of the punch 16.1 and the die 16.2, thereby separating the second sheet metal part 20 from the electric steel strip 5. In this process, a recess 21 is formed in the electric steel strip 5.
[0035] The recess 21 is used to receive the release element 19 into the electrical steel strip 5, which is done by a press die 10 equipped with a stage 22 having means for pushing back into the electrical steel strip 5. This means is designed as a movable press device 22.1 in the lower die and a fixed opposing plate 22.2 in the upper die. The stage 22 pushes the release element 19 back from there into the region 21 of the electrical steel strip 5 from which the second sheet metal part 20 has been punched out. That is, the release element 19 moves together with the electrical steel strip 5 within the press die 10. Other means for pushing back are also known, for example in German European Patent Translation No. 11207002887T2, which also discloses a pushing back process.
[0036] In the final press stage 15, the release element 19 is punched out from the electrical steel strip 5. Thus, the release element 19 is positioned between multiple first sheet metal parts 2 in the lamination device 18, facilitating the separation of the lamination stack 3 when it leaves the lamination device 18.
[0037] As shown in Figure 1, the polymer adhesive layer 8 on one side of the second sheet metal part 20 is deactivated by the heat source 23. That is, the second sheet metal part 20 can also be used as a release element 19 and is pushed back onto the electric steel strip 5. Other methods for deactivating the polymer adhesive layer 8 include, for example, curing and / or removal.
[0038] Since only one side of the second sheet metal part 20, i.e., the adhesive layer 8, is deactivated, the second sheet metal part 20 not only acts as a release element 19, but can also be bonded to the laminated stack 3 based on its undeactivated adhesive layer 9, and as a result, can be reused. This ensures a high utilization rate of the electrical steel strip 5.
[0039] As shown in Figure 2a, the second outer shape punching and back-punching are performed at different stages 16 and 22, respectively, during press lamination. Specifically, back-punching is performed at stage 22 immediately after the first outer shape punching, and the second outer shape punching is performed at stage 22 immediately after back-punching. Furthermore, all stages 14, 15, 16, and 22 are part of the press die 10.
[0040] Furthermore, during the second outer punching process, two guide holes 24 are punched into the electrical steel strip using a third stage 16. These multiple guide holes 24 are used to position the release element 19 and the electrical steel strip 5 relative to each other. For this purpose, the press device 22.1 is equipped with two pins 25, each protruding into the guide holes 24 of the electrical steel strip 5. This ensures accurate positioning of the release element 19 into the recesses 21 of the electrical steel strip 5, greatly improving the repeatability of the process.
[0041] Figure 2b shows that the outer shape punching of the second sheet metal part 20 is performed to an outer shape that is smaller by a normal distance s than that of the first sheet metal part 2. Therefore, the recess 21 is smaller than the outer shape contour of the second press stage 15. Preferably, the normal distance s corresponds to 2 millimeters (mm).
[0042] Furthermore, Figure 2b shows that the release element 19 has protruding portions V. These multiple rectangular protruding portions V form an interference fit P on the electromagnetic steel strip 5, thereby firmly holding the release element 19 on the electromagnetic steel strip 5. For this reason, for example, the second sheet metal part 20 used as the release element 19 is placed across the multiple protruding portions V. However, interference fits P can also be formed on other parts of the release element 19, although these are not shown in the figure.
[0043] Figure 3 schematically shows an alternative apparatus 101 for carrying out the method of the present invention. This second apparatus 101 differs from the first apparatus 1 shown in Figure 1 in that an additional die 26 is present prior to the second progressive die 10.2 for press lamination. This die 26, separated from the second progressive die 10.2, performs the same process as the progressive die 10 shown in Figure 1, namely the second outer shape punching and pushback. Therefore, the second outer shape punching and pushback are performed in the progressive die 10.2 that performs the first outer shape punching with the second press 16, in addition to preparatory press work. In Figure 1, the stage 14 of the progressive die 10.2 is used.
[0044] Therefore, a known progressive press die 10.2 can be replicated by the die 26 to perform the process of the present invention. [Explanation of Symbols]
[0045] 1 device 101 Equipment 2 Sheet metal parts 3 stacked 4 coils 5 Electrical steel strip 6, 7 Functional aspects 8, 9 Adhesive layer 10 Press molds 10.1 Progressive die press 10.2 Progressive die press 11 strokes 12 Upper mold 13 Lower mold 14, 15, 16 Press Stage Stages 14, 15, and 16 14 Pre-processing press stage 14.1, 15.1, 16.1 punches 14.2, 15.2, 16.2 Die 17 parts 18. Stacking apparatus 18.1 Vertical hole 18.2 Opposing plate 19 Release elements 20 Sheet metal parts 21 Recess 22 stages 22.1 Movable press machine 22.1 Pressing device 22.2 Fixed opposing plate 23 Heat source 24 guide holes 25 pins P Interlocking fit V protrusion
Claims
1. A method for stacking stamped sheet metal parts (2) to form a plurality of stacked stacks (3), comprising the steps of: a first outline punching step of pressing a first sheet metal part (2) from an electromagnetic steel strip (5) having a curable adhesive layer (8, 9) on at least one of its flat sides (6, 7); Then, the plurality of first sheet metal parts are stacked and joined together by joining the plurality of first sheet metal parts (2). The method comprises a means for facilitating separation of the joined first sheet metal parts (2) into a stack (3), the means comprising stacking at least one release element (19) together with the plurality of first sheet metal parts (2). The means is Prior to the first outline punching step, at least one second sheet metal part (20) is outline punched. A second outer shape punching process. a pushing-back step of pushing the release element (19) back onto the portion of the electromagnetic steel strip (5) from which the second sheet metal part (20) has been punched; a third outline punching step of punching the release element (19) from the electromagnetic steel strip (5) in the first outline punching step; A method comprising:
2. 2. The method according to claim 1, further comprising the step of passivating, hardening and / or removing the adhesive layer (8, 9) of the second sheet metal part (20) and using it as a release element (19).
3. 3. The method of claim 2, wherein the second sheet metal part (20) is elongated in a plurality of areas prior to the pushing back step.
4. 4. The method according to claim 2 or 3, characterized in that the second sheet metal part (20) is joined with the first sheet metal part (2) to form a laminate stack (3).
5. 5. The method according to claim 1, wherein the second profile punching step and the pushing back step in the press lamination process are performed in different press stages (16, 22).
6. 6. The method according to claim 1, wherein a second profile punching step is performed before the first profile punching step, which is performed by a progressive press die (10.2) using a second press stage (15).
7. 6. The method according to claim 1, wherein the second profile punching step is performed by a third press stage (16) of a progressive press die (10.1) which performs the first profile punching step using a second press stage (15).
8. 8. The method according to claim 7, characterized in that the pushing back step is performed in a stage (22) immediately prior to the first pressing step.
9. 9. The method according to claim 8, characterized in that the second profile punching step is performed in a stage (16) immediately prior to the pushing back step.
10. 10. The method according to claim 1, further comprising punching at least one guide hole (24) in the magnetic strip (5) before or during the second profile punching step, and the release element (19) and the magnetic strip (5) are positioned relative to each other with the aid of the guide hole (24).
11. 11. The method according to claim 1, wherein the outer diameter of the second sheet metal part (20) is smaller than that of the first sheet metal part (2).
12. 12. The method according to claim 11, characterized in that the second sheet metal part (20) is stamped out to be max. 2 mm undersized.
13. 13. The method according to any one of claims 1 to 12, characterized in that an interference fit (P) is formed between the demolding element (19) and the electromagnetic steel strip (5).
14. 14. The method according to claim 13, characterized in that the demolding element (19) and / or the electromagnetic steel strip (5) have a protruding portion (V) through which the interference fit (P) is formed.
15. 15. The method according to any one of claims 1 to 14, characterized in that the release element (19) is designed to weaken the adhesive forces of the joined first sheet metal parts (2) in order to facilitate separation of the joined first sheet metal parts (2) into a plurality of laminate stacks (3).