Wiring board and method for manufacturing wiring board
Patent Information
- Application Number
- JP2022017380
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-07-06
- Filing Date
- 2022-02-07
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2042-02-07
AI Technical Summary
【0008】 本願が開示する配線基板及び配線基板の製造方法の1つの態様によれば、内蔵されるインダクタの電気特性を向上することができるという効果を奏する。
Abstract
Description
[Technical Field]
[0001] The present invention relates to a wiring board and a method for manufacturing a wiring board. [Background technology]
[0002] Conventionally, some wiring boards have built-in inductors formed using a magnetic material. Such inductors are formed, for example, by placing the magnetic material in a through hole in an insulating resin layer of the wiring board, drilling a through hole in the magnetic material, and providing a plating film on the inner wall of the through hole. The process of providing a plating film on the inner wall of the through hole in the magnetic material is generally performed simultaneously with providing a plating film on the surface of the wiring board, for example, by electrolytic copper plating. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Publication No. 1-162281 [Patent Document 2] Japanese Patent Application Laid-Open No. 2007-12746 [Patent Document 3] Japanese Patent Application Publication No. 2019-220504 Summary of the Invention [Problem to be solved by the invention]
[0004] However, the above-mentioned wiring board has a problem in that the inductor formation process is complicated, and errors that occur in each process affect the inductor's electrical characteristics, limiting its improvement. Specifically, for example, through holes are formed in the magnetic material by drilling, but depending on the precision of the drilling, it is difficult to form the through holes at the center of the magnetic material. As a result, the position of the plating film formed on the inner wall of the through hole in the magnetic material is also biased, worsening the inductance variation.
[0005] Furthermore, through holes formed inside the plating film that penetrate the magnetic material are typically filled with insulating resin. Because both ends of this insulating resin are exposed on the surface of the wiring board, a plating film is laminated on the surface of the wiring board to cover both ends of the insulating resin. Furthermore, when through holes are formed in the wiring board, a plating film is further laminated on the surface of the wiring board to cover the inner walls of these through holes. Because multiple plating films are laminated on the surface of the wiring board in this way, the plating thickness can become uneven even around the inductor, degrading the electrical characteristics of the inductor.
[0006] The disclosed technology has been made in view of the above points, and aims to provide a wiring board and a method for manufacturing the wiring board that can improve the electrical characteristics of the built-in inductor. [Means for solving the problem]
[0007] In one aspect, the wiring board disclosed in the present application comprises a base material, a through hole formed in the base material, a magnetic member embedded in the through hole, and a plating film covering an end face of the magnetic member exposed from the through hole, wherein the magnetic member comprises a conductor wire covered with a magnetic material. [Effects of the Invention]
[0008] According to one aspect of the wiring board and the method for manufacturing the wiring board disclosed in the present application, it is possible to obtain an effect that the electrical characteristics of the built-in inductor can be improved. [Brief explanation of the drawings]
[0009] [Figure 1] FIG. 1 is a partial cross-sectional view showing the configuration of a core substrate according to the first embodiment. [Figure 2] FIG. 2 is a diagram showing a specific example of a method for forming the magnetic member. [Figure 3] FIG. 3 is a diagram showing another specific example of a method for forming the magnetic member. [Figure 4] FIG. 4 is a diagram showing a specific example of the structure of the magnetic member. [Figure 5] FIG. 5 is a flowchart showing a method for manufacturing a wiring board according to the first embodiment. [Figure 6] FIG. 6 is a diagram showing the structure of the substrate. [Figure 7] FIG. 7 is a diagram showing a specific example of the through-hole forming step. [Figure 8] FIG. 8 is a diagram showing a specific example of the magnetic material embedding step. [Figure 9] FIG. 9 is a diagram showing a specific example of the surface polishing step. [Figure 10] FIG. 10 is a diagram showing a specific example of the first electroless copper plating step. [Figure 11] FIG. 11 is a diagram showing a specific example of the first electrolytic copper plating step. [Figure 12] FIG. 12 is a diagram showing a specific example of the insulating resin filling step. [Figure 13] FIG. 13 is a diagram showing a specific example of the surface polishing step. [Figure 14] FIG. 14 is a diagram showing a specific example of the second electroless copper plating step. [Figure 15] FIG. 15 is a diagram showing a specific example of the second electrolytic copper plating step. [Figure 16] FIG. 16 is a diagram showing a specific example of the etching mask formation step. [Figure 17] FIG. 17 is a diagram showing a specific example of the etching process. [Figure 18] FIG. 18 is a diagram illustrating an example of the configuration of a wiring board. [Figure 19] FIG. 19 is a diagram illustrating a configuration example of a semiconductor device. [Figure 20] FIG. 20 is a flowchart showing a method for manufacturing a wiring board according to the second embodiment. [Figure 21] FIG. 21 is a diagram showing a specific example of the through-hole forming step. [Figure 22] FIG. 22 is a diagram showing a specific example of the first electrolytic copper plating step. [Figure 23] FIG. 23 is a diagram showing a specific example of the insulating resin filling step. [Figure 24]FIG. 24 is a diagram showing a specific example of the through-hole forming step. [Figure 25] FIG. 25 is a diagram showing a specific example of the magnetic member embedding step. [Figure 26] FIG. 26 is a diagram showing a specific example of the second electrolytic copper plating step. [Figure 27] FIG. 27 is a diagram showing a specific example of the etching process. [Figure 28] FIG. 28 is a flowchart showing a method for manufacturing a wiring board according to the third embodiment. [Figure 29] FIG. 29 is a diagram showing a specific example of the through-hole forming step. [Figure 30] FIG. 30 is a diagram showing a specific example of the magnetic member embedding step. [Figure 31] FIG. 31 is a diagram showing a specific example of the surface polishing step. [Figure 32] FIG. 32 is a diagram showing a specific example of the through-hole forming step. [Figure 33] FIG. 33 is a diagram showing a modified example of the core substrate according to the first embodiment. [Figure 34] FIG. 34 is a diagram showing a modified example of the core substrate according to the second embodiment. DETAILED DESCRIPTION OF THE INVENTION
[0010] Hereinafter, embodiments of a wiring board and a method of manufacturing a wiring board disclosed in the present application will be described in detail with reference to the drawings. However, the present invention is not limited to these embodiments.
[0011] (Embodiment 1) 1 is a partial cross-sectional view showing the configuration of a core substrate 100 included in a multilayer wiring board according to embodiment 1. As shown in FIG. 1, core substrate 100 is a wiring board having a base material 110, a through-hole portion 120, and an inductor portion 130.
[0012] The base material 110 is an insulating plate-like member and is the base material of the core substrate 100. The base material 110 is, for example, a glass cloth with an epoxy resin or a polyimide resin. A glass epoxy substrate impregnated with insulating resin can be used. Alternatively, a substrate made of woven or nonwoven fabric such as glass fiber, carbon fiber, or aramid fiber impregnated with epoxy resin can also be used as the base material 110. The thickness of the base material 110 can be, for example, about 700 to 2000 μm.
[0013] The through-hole portion 120 is provided at the position of the through-hole 112 that penetrates the base material 110, and ensures electrical continuity between the surfaces 110a on both sides of the base material 110. The through-hole portion 120 has a conductor layer 140a formed on the surface 110a of the base material 110, and an insulating resin 125 that penetrates the through-hole 112.
[0014] Conductive layer 140a has metal foil 111, first electroless plated film 141a, first electrolytic plated film 141b, second electroless plated film 142a, and second electrolytic plated film 142b, and forms the pads of through-hole portion 120. The pads formed from conductive layer 140a are included in a wiring layer provided on the surface of base material 110. Metal foil 111 is a metal foil that is provided in advance on surface 110a of base material 110 and can be removed by etching. For example, copper foil or copper alloy foil can be used as metal foil 111, and the thickness of metal foil 111 is, for example, 4 to 12 μm.
[0015] First electroless plated film 141a and second electroless plated film 142a are electroless plated films formed by, for example, copper electroless plating. Meanwhile, first electroless plated film 141b and second electroless plated film 142b are electroless plated films formed by, for example, copper electrolytic plating. First electroless plated film 141a is laminated on metal foil 111 and coats the inner walls of through-holes 112. First electroless plated film 141b is laminated on first electroless plated film 141a. Second electroless plated film 142a is laminated on first electroless plated film 141b and coats the end faces of insulating resin 125. Second electroless plated film 142b is laminated on second electroless plated film 142a.
[0016] Insulating resin 125 is an insulating resin that fills the through hole inside first electroless plated film 141a and first electrolytic plated film 141b that coat the inner wall of through hole 112. For example, an epoxy resin containing a filler such as silica can be used as insulating resin 125. Both end faces of insulating resin 125 are covered with second electroless plated film 142a and second electrolytic plated film 142b.
[0017] Inductor section 130 is provided at the position of through-hole 113 that penetrates substrate 110, and functions as an inductor. Inductor section 130 has conductor layer 140b formed on surface 110a of substrate 110, and magnetic member 135 that penetrates through-hole 113.
[0018] Similar to conductor layer 140a, conductor layer 140b has metal foil 111, first electroless plated film 141a, first electrolytic plated film 141b, second electroless plated film 142a, and second electrolytic plated film 142b, and forms the pads of inductor section 130. The pads formed from conductor layer 140b are included in a wiring layer provided on the surface of substrate 110.
[0019] In inductor portion 130, first electroless plated film 141a, first electroless plated film 141b, second electroless plated film 142a, and second electroless plated film 142b are laminated on metal foil 111 and cover the end faces of magnetic member 135. That is, first electroless plated film 141a is formed so as to cover the end faces of metal foil 111 and magnetic member 135, and first electroless plated film 141b, second electroless plated film 142a, and second electroless plated film 142b are laminated in this order on first electroless plated film 141a.
[0020] First electroless plated film 141a, first electrolytic plated film 141b, second electroless plated film 142a, and second electrolytic plated film 142b of conductor layers 140a, 140b are all electroless plated films or electrolytic plated films formed simultaneously.
[0021] Magnetic member 135 is a member including a magnetic body and a conductor, and is embedded in through-hole 113 formed in substrate 110. Specifically, magnetic member 135 is a member formed by, for example, covering conductor wire 132 with magnetic body 131, and is shaped to a size that fits through-hole 113. Both end faces of magnetic member 135 are covered with first electroless plated film 141a, first electrolytic plated film 141b, second electroless plated film 142a, and second electrolytic plated film 142b.
[0022] Here, a specific example will be given to explain the structure of the magnetic member 135. Fig. 2 is a diagram showing a specific example of a method for forming the magnetic member 135. The magnetic member 135 shown in Fig. 2 is formed by covering a conductor wire with a magnetic material.
[0023] That is, for example, a magnetic-material-coated conductor wire is formed by covering a conductor wire 201 shown in Fig. 2(a) with a magnetic material 202 as shown in Fig. 2(b). The conductor wire 201 may be a wire made of metal such as a copper wire.
[0024] For example, an insulating resin such as an epoxy resin containing magnetic particles can be used as the magnetic substance 202. Examples of magnetic particles include fillers such as iron, iron oxide, cobalt iron oxide, silicon iron, nickel, nickel oxide, magnetic alloys, and ferrite. When such a resin containing magnetic filler is used as the magnetic substance 202, the periphery of the conductor wire 201 having a diameter of, for example, about 100 to 200 μm is coated with the magnetic substance 202 having a thickness of about 75 to 175 μm. This allows the formation of a magnetic-coated conductor wire having a diameter of, for example, 250 to 550 μm.
[0025] Furthermore, a magnetic metal such as iron, nickel, or chromium can be used as the magnetic body 202. When such a magnetic metal is used as the magnetic body 202, a plating film of the magnetic body 202 having a thickness of about 50 to 200 μm is formed by electrolytic plating around the conductor wire 201 having a diameter of, for example, 50 to 300 μm. This makes it possible to form a magnetic-coated conductor wire having a diameter of, for example, 150 to 700 μm.
[0026] The diameter of these magnetic coated conductor wires is approximately equal to the diameter of the through-hole 113 of the substrate 110 in which the magnetic member 135 is embedded, but is preferably slightly larger than the diameter of the through-hole 113 .
[0027] After the magnetic-substance coated conductor wire is formed, it is cut to a predetermined length, as shown in Fig. 2(c) for example. Specifically, the magnetic-substance coated conductor wire is cut to a length of, for example, 700 to 2000 µm, which is approximately the same as the thickness of the substrate 110, to obtain the magnetic member 135. At this time, it is preferable that the length of the magnetic member 135 is slightly longer than the thickness of the substrate 110 so that both ends of the magnetic member 135 protrude from the surface of the substrate 110 when the magnetic member 135 is embedded in the through-hole 113.
[0028] Fig. 3 is a diagram showing another specific example of a method for forming the magnetic member 135. The magnetic member 135 shown in Fig. 3 is formed by twisting together a plurality of magnetic-coated conductor wires to form a stranded wire, and then covering the stranded wire with an insulating resin.
[0029] That is, for example, a conductor wire 201 shown in Fig. 3(a) is covered with a magnetic material 202 as shown in Fig. 3(b) to form a magnetic-material-coated conductor wire. For example, a copper wire can be used as the conductor wire 201. For example, a magnetic filler-containing resin or a magnetic metal can be used as the magnetic material 202, as described above.
[0030] When a plurality of such magnetic-substance-coated conductor wires are formed, the plurality of magnetic-substance-coated conductor wires are twisted together to form a stranded wire, as shown in FIG. 3(c). Then, as shown in FIG. 3(d), the stranded wire is coated with insulating resin 203. The stranded wire coated with insulating resin 203 is cut to a predetermined length, as shown in FIG. 3(e), for example. Specifically, the stranded wire coated with insulating resin 203 is cut to a length of, for example, 700 to 2000 μm, which is approximately the same as the thickness of the substrate 110, to obtain the magnetic member 135. At this time, it is preferable that the length of the magnetic member 135 is slightly longer than the thickness of the substrate 110 so that both ends of the magnetic member 135 protrude from the surface of the substrate 110 when the magnetic member 135 is embedded in the through-hole 113.
[0031] When the magnetic member 135 is formed using a twisted wire, any number of magnetic-substance coated conductor wires may be twisted together. For example, as shown in Fig. 4(a), the magnetic member 135 may be formed from a twisted wire with a double helix structure in which two magnetic-substance coated conductor wires are twisted together, or as shown in Fig. 4(b), the magnetic member 135 may be formed from a twisted wire with a triple helix structure in which three magnetic-substance coated conductor wires are twisted together.
[0032] The magnetic member 135 described above is formed using a magnetic-coated conductor wire in which the conductor wire 201 is arranged at the center of the magnetic body 202, and the conductor wire 201 and the magnetic body 202 are uniformly arranged. As a result, in the core substrate 100 in which the magnetic member 135 is embedded in the base material 110, it is possible to reduce variations in the inductance of the inductor section 130. Furthermore, since the conductor wire 201 is included in the center of the magnetic member 135, the volume of the conductor in the magnetic member 135 increases, and the electrical resistance can be reduced. In this way, by using the magnetic member 135, it is possible to improve the electrical characteristics of the inductor built into the core substrate 100.
[0033] Furthermore, since magnetic member 135 already includes conductor wire 201, there is no need for a plating step to electrically connect both ends of magnetic member 135 after embedding magnetic member 135 in base material 110. This makes it possible to simplify the process of manufacturing core substrate 100, reduce the number of plating steps, and make the plating thickness uniform.
[0034] Next, the electroless plated film and the electrolytic plated film will be described.
[0035] First electroless plated film 141a is formed on the surface of metal foil 111, the inner wall surfaces of through holes 112, and the end faces of magnetic member 135. That is, in through-hole portion 120, first electroless plated film 141a is formed continuously on the surface of metal foil 111 and the inner wall surfaces of through holes 112. On the other hand, in inductor portion 130, first electroless plated film 141a is laminated on the surface of metal foil 111 and the end faces of magnetic member 135. The thickness of first electroless plated film 141a is, for example, approximately 0.1 to 2.0 μm.
[0036] First electrolytic plated film 141b is laminated on first electroless plated film 141a. That is, in through-hole portion 120, first electrolytic plated film 141b is laminated continuously on first electroless plated film 141a above and below metal foil 111 and within through-hole 112. On the other hand, in inductor portion 130, first electrolytic plated film 141b is laminated in a planar manner on first electroless plated film 141a. The thickness of first electrolytic plated film 141b is, for example, approximately 2 to 18 μm.
[0037] Second electroless plated film 142a is formed on the surface of first electroless plated film 141b and on the end face of insulating resin 125. That is, in through-hole portion 120, second electroless plated film 142a is laminated on first electroless plated film 141b and the end face of insulating resin 125. On the other hand, in inductor portion 130, second electroless plated film 142a is laminated in a planar manner on first electroless plated film 141b. The thickness of second electroless plated film 142a is, like that of first electroless plated film 141a, approximately 0.1 to 2.0 μm, for example.
[0038] Second electrolytic plated film 142b is laminated on second electroless plated film 142a. That is, second electrolytic plated film 142b is laminated in a planar manner on second electroless plated film 142a in through-hole portion 120 and inductor portion 130. The thickness of second electrolytic plated film 142b is, like first electrolytic plated film 141b, approximately 2 to 18 μm, for example.
[0039] Next, a method for manufacturing a multilayer wiring board including the core substrate 100 configured as described above will be described by way of a specific example with reference to the flow chart shown in FIG.
[0040] First, through holes 112 and 113 for forming the through-hole portion 120 and the inductor portion 130 are formed in a substrate 110 composed of an insulating plate-like member (step S101). The substrate 110 is, for example, as shown in FIG. 6, in which a metal foil 111 is formed on a surface 110a of an insulating plate-like member. The thickness of the substrate 110 is, for example, about 700 to 2000 μm. In the substrate 110, for example, as shown in FIG. 7, a cylindrical through hole 112 having an opening diameter of about 100 to 200 μm and a cylindrical through hole 113 having an opening diameter of about 250 to 550 μm are formed. The through holes 112 and 113 are formed by, for example, laser processing or drilling. After the through holes 112 and 113 are formed, a desmear treatment is performed to remove resin residue from the inner wall surfaces. For example, a potassium permanganate solution can be used for the desmear treatment.
[0041] Then, the magnetic member 135 is embedded in the through hole 113 (step S102). That is, for example, as shown in FIG. 8, the magnetic member 135 having, for example, a magnetic body 131 and a conductor wire 132 is inserted into the through hole 113 formed in the base material 110. At this time, the magnetic member 135 is embedded in the through hole 113 so that the conductor wire 132 provided at the center of the magnetic member 135 is positioned on the central axis of the through hole 113. Because the diameter of the magnetic member 135 is approximately equal to or slightly larger than the diameter of the through hole 113, the elasticity of the magnetic body 131 allows the magnetic member 135 to be inserted into the through hole 113 without any gaps. Note that even when the magnetic member 135 has the structure shown in FIG. 3, the elasticity of the insulating resin 203 that covers the stranded wire allows the magnetic member 135 to be inserted into the through hole 113 without any gaps.
[0042] Alternatively, an insulating resin such as an epoxy resin may be injected along the inner wall surface of through hole 113 to adjust the diameter of through hole 113 to the diameter of magnetic body 135. In this way, the injected insulating resin is interposed between the inner wall surface of through hole 113 and magnetic member 135, and even if magnetic body 131 forming magnetic member 135 does not have elasticity, it is possible to prevent a gap from being generated between the inner wall surface of through hole 113 and magnetic member 135.
[0043] When magnetic member 135 is inserted through through-hole 113 , both ends of magnetic member 135 protrude above and below metal foil 111 of substrate 110 because the length of magnetic member 135 is slightly longer than the thickness of substrate 110 .
[0044] Therefore, the protruding portion is polished to a flat surface (step S103) so that both end portions of magnetic member 135 are flush with the surface of metal foil 111. That is, for example, as shown in Fig. 9, both end portions of magnetic member 135 are polished so that the surface of metal foil 111 and both end faces of magnetic member 135 are flush with each other.
[0045] When the surface of metal foil 111 and both end faces of magnetic member 135 are flush with each other, first electroless plated film 141a is formed to cover the exposed portions of the surface (step S104). Specifically, as shown in Fig. 10, for example, first electroless plated film 141a is formed by applying electroless copper plating to the surface of metal foil 111, the end faces of magnetic member 135, and the inner wall surfaces of through-hole 112. The thickness of first electroless plated film 141a is, for example, about 0.1 to 2.0 µm.
[0046] Then, first electrolytic plated film 141b is laminated on first electroless plated film 141a (step S105). That is, as shown in Fig. 11, for example, first electrolytic plated film 141b is formed by applying electrolytic copper plating to the surface on which first electroless plated film 141a is formed. The thickness of first electrolytic plated film 141b is, for example, approximately 2 to 18 µm.
[0047] By forming first electroless plated film 141a and first electrolytic plated film 141b, a through hole is formed inside first electrolytic plated film 141b within through hole 112. This through hole is filled with insulating resin 125 (step S106). That is, as shown in FIG. 12 , for example, insulating resin 125 is filled inside first electrolytic plated film 141b within through hole 112. For example, epoxy resin containing a filler such as silica can be used as insulating resin 125. Insulating resin 125 is filled without any gaps inside first electrolytic plated film 141b, and both ends of insulating resin 125 protrude above and below first electroless plated film 141a and first electrolytic plated film 141b that are laminated on metal foil 111.
[0048] Therefore, the protruding portions are polished to a flat surface so that both end portions of insulating resin 125 are flush with the surface of first electrolytic plated film 141b (step S107). That is, as shown in FIG. 13, for example, both ends of insulating resin 125 are polished so that the top and bottom surfaces of first electrolytic plated film 141b and both end faces of insulating resin 125 are flush with each other. Furthermore, resin residue remaining on the surface of first electrolytic plated film 141b due to the polishing of insulating resin 125 is removed by desmearing. At this time, both end faces of magnetic member 135 are polished to a flat surface so that the top and bottom surfaces of first electrolytic plated film 141b and Since the magnetic material 131 is covered with 141b, it is protected from the solution used for desmearing.
[0049] When the top and bottom surfaces of first electrolytic plated film 141b and both end faces of insulating resin 125 are flush with each other, second electroless plated film 142a is formed to cover the exposed surface (step S108). Specifically, as shown in Fig. 14, for example, electroless copper plating is applied to the surface of first electrolytic plated film 141b and the end faces of insulating resin 125 to form second electroless plated film 142a. The thickness of second electroless plated film 142a is, for example, approximately 0.1 to 2.0 µm, similar to that of first electroless plated film 141a.
[0050] Then, second electrolytic plated film 142b is laminated on second electroless plated film 142a (step S109). That is, as shown in Fig. 15, for example, second electrolytic plated film 142b is laminated in a planar shape by applying, for example, electrolytic copper plating to the surface on which second electroless plated film 142a is formed. The thickness of second electrolytic plated film 142b is, like first electrolytic plated film 141b, for example, approximately 2 to 18 µm.
[0051] Since all electroless plated films and electrolytic plated films have been formed by the electroless plating and electrolytic plating up to this point, etching is performed to form conductor layers 140a and 140b of through-hole portion 120 and inductor portion 130 (step S110). That is, as shown in FIG. 16, for example, etching resists 210 are formed in the portions where the plated films will remain as conductor layers 140a and 140b. FIG. 16 illustrates etching resists 210 for forming conductor layers 140a and 140b as pads at the positions of insulating resin 125 and magnetic member 135, respectively. These etching resists 210 are formed on the surface of second electrolytic plated film 142b so as to cover areas wider than through-holes 112 and 113, respectively. The etching resists 210 have the desired resolution and are formed from a material that is resistant to etching.
[0052] Then, using etching resist 210 as a mask, metal foil 111, first electroless plated film 141a, first electrolytic plated film 141b, second electroless plated film 142a, and second electrolytic plated film 142b are removed by wet etching. As a result, as shown in Fig. 17, for example, through-hole portion 120 having conductor layer 140a as a pad and inductor portion 130 having conductor layer 140b as a pad are formed. By removing etching resist 210 from these conductor layers 140a and 140b, core substrate 100 is completed.
[0053] 18, insulating layers 230 and wiring layers 220 are laminated on the upper and lower surfaces of core substrate 100, and the vertically laminated wiring layers 220 are electrically connected by via wiring 225 provided in insulating layer 230. Furthermore, the wiring layer 220 closest to core substrate 100 is electrically connected to conductor layers 140a and 140b of core substrate 100 by via wiring 225 provided in insulating layer 230.
[0054] The uppermost wiring layer 220 is covered with a solder resist layer 240. Through holes are formed in the solder resist layer 240, and connection terminals 250 made of solder or the like are formed in these through holes to electrically connect electronic components such as semiconductor chips to the wiring layer 220. Meanwhile, the lowermost wiring layer 220 is covered with a solder resist layer 260. Openings are formed in the solder resist layer 260, and external connection pads 270 formed on the lowermost wiring layer 220 are exposed through the openings. The external connection pads 270 can be electrically connected to external components or devices.
[0055] In this way, a multilayer wiring board having a plurality of wiring layers 220 can be formed from core substrate 100 incorporating inductor section 130 using magnetic member 135. This multilayer wiring board can be used in a semiconductor device on which components such as semiconductor chips are mounted. Specifically, as shown in FIG. 19 , a semiconductor chip 310 is mounted on the upper surface of the multilayer wiring board. For example, connection terminals 250 of the multilayer wiring board are joined to electrodes 315 made of solder or the like of semiconductor chip 310. The joints between connection terminals 250 and electrodes 315 are then sealed with underfill resin 320, resulting in a semiconductor device on which semiconductor chip 310 is mounted.
[0056] As described above, according to this embodiment, an inductor is formed in which a magnetic member formed using a magnetic-coated conductor wire is embedded in a through hole in a substrate, and the end face of the magnetic member exposed from the opening of the through hole is coated with an electroless plating film and an electrolytic plating film. This results in a uniform arrangement of the conductor wire and magnetic material in the inductor, reducing inductance variation. Furthermore, the volume of the conductor in the inductor is increased, reducing electrical resistance. In other words, the electrical characteristics of the inductor built into the core substrate can be improved.
[0057] (Embodiment 2) In the above-described first embodiment, magnetic member 135 is embedded in through hole 113 of substrate 110, and then insulating resin 125 is filled into through hole 112, but it is also possible to first fill through hole 112 with insulating resin 125, and then embed magnetic member 135 into through hole 113. Therefore, in the second embodiment, a method for manufacturing a multilayer wiring board in the case where magnetic member 135 is embedded later will be described.
[0058] Fig. 20 is a flow diagram showing a method for manufacturing a multilayer wiring board according to embodiment 2. In Fig. 20, the same parts as in Fig. 5 are denoted by the same reference numerals. In the method for manufacturing a multilayer wiring board shown in Fig. 20, after insulating resin 125 is filled in step S106, magnetic member 135 is embedded in step S102.
[0059] First, a through hole 112 for forming a through-hole portion 120 is formed in a substrate 110 composed of an insulating plate-like member (step S201). That is, as shown in FIG. 21, for example, a cylindrical through hole 112 having an opening diameter of about 100 to 200 μm is formed in the substrate 110. The through hole 112 is formed by, for example, laser processing or drilling, and after the through hole 112 is formed, a desmear treatment is performed to remove resin residue from the inner wall surface. For example, a potassium permanganate solution can be used for the desmear treatment.
[0060] After through-hole 112 is formed, first electroless plated film 141a is formed to cover the exposed surface (step S104), and then first electroless plated film 141b is laminated on first electroless plated film 141a (step S105). Specifically, as shown in FIG. 22, first electroless plated film 141a is formed by, for example, electroless copper plating on the surface of metal foil 111 and the inner wall surface of through-hole 112. Then, first electroless plated film 141b is formed by, for example, electrolytic copper plating on the surface on which first electroless plated film 141a is formed. First electroless plated film 141a has a thickness of, for example, approximately 0.1 to 2.0 μm. First electroless plated film 141b has a thickness of, for example, approximately 2 to 18 μm.
[0061] By forming first electroless plated film 141a and first electrolytic plated film 141b, a through hole is formed inside first electrolytic plated film 141b within through hole 112. This through hole is filled with insulating resin 125 (step S106). That is, as shown in FIG. 23 , for example, insulating resin 125 is filled inside first electrolytic plated film 141b within through hole 112. For example, epoxy-based resin containing a filler such as silica can be used as insulating resin 125. Insulating resin 125 is filled tightly inside first electrolytic plated film 141b, and both ends of insulating resin 125 protrude above and below first electroless plated film 141a and first electrolytic plated film 141b that are laminated on metal foil 111.
[0062] Both protruding ends of insulating resin 125 are polished to a flat surface (step S107), and when the top and bottom surfaces of first electrolytic plated film 141b and both end surfaces of insulating resin 125 are flush with each other, through hole 113 for forming inductor portion 130 is formed (step S202). That is, cylindrical through hole 113 with an opening diameter of approximately 250 to 550 μm is formed in base material 110 on which first electroless plated film 141a and first electrolytic plated film 141b are formed, as shown in FIG. 24, for example. Through hole 113 is formed by laser processing or drilling, for example, and after through hole 113 is formed, a desmear process is performed to remove resin residue from the inner wall surface.
[0063] Then, magnetic member 135 is embedded in through hole 113 (step S102). That is, for example, as shown in FIG. 25 , magnetic member 135 having magnetic body 131 and conductor wire 132 is inserted into through hole 113. Because the diameter of magnetic member 135 is approximately equal to or slightly larger than the diameter of through hole 113, the elasticity of magnetic body 131 allows magnetic member 135 to be inserted into through hole 113 without any gaps. In addition, because the length of magnetic member 135 is slightly longer than the thickness of base material 110, both ends of magnetic member 135 protrude above and below first electroless plated film 141a and first electrolytic plated film 141b laminated on metal foil 111.
[0064] Both protruding ends of magnetic member 135 are polished to a flat surface (step S103). Once the top and bottom surfaces of first electrolytic plated film 141b are flush with both end surfaces of magnetic member 135, second electroless plated films 142a and 142b are formed on the exposed surface (steps S108 and S109). Specifically, as shown in FIG. 26, for example, electroless copper plating is applied to the surface of first electrolytic plated film 141b, the end surfaces of insulating resin 125, and the end surfaces of magnetic member 135, thereby forming second electroless plated film 142a. Then, electrolytic copper plating is applied to the surface on which second electroless plated film 142a is formed, thereby forming second electroless plated film 142b in a flat configuration. The thickness of second electroless plated film 142a is, for example, approximately 0.1 to 2.0 μm. The thickness of second electroless plated film 142b is, for example, approximately 2 to 18 μm.
[0065] Since all electroless plated films and electrolytic plated films have been formed by the electroless plating and electrolytic plating up to this point, etching is performed to form conductor layers 140a and 140b of through-hole portion 120 and inductor portion 130 (step S110). That is, an etching resist is formed on the portions where the plated films are to remain as conductor layers 140a and 140b, and metal foil 111, first electroless plated film 141a, first electrolytic plated film 141b, second electroless plated film 142a, and second electrolytic plated film 142b are removed by wet etching. As a result, through-hole portion 120 having conductor layer 140a as a pad and inductor portion 130 having conductor layer 140b as a pad are formed, as shown in FIG. 27, for example.
[0066] Insulating layers and wiring layers are built up in this order on the upper and lower surfaces of core substrate 100 thus formed, thereby forming a multilayer wiring substrate (step S111). A semiconductor chip may also be mounted on the multilayer wiring substrate to form a semiconductor device. Core substrate 100 according to the present embodiment differs from core substrate 100 according to embodiment 1 in that both end faces of magnetic member 135 are covered with second electroless plated film 142a. That is, core substrate 100 according to embodiment 1 is formed by embedding magnetic member 135 before insulating resin 125 is filled, and therefore both end faces of magnetic member 135 are covered with first electroless plated film 141a. In contrast, core substrate 100 according to the present embodiment is formed by embedding magnetic member 135 after insulating resin 125 is filled, and therefore both end faces of magnetic member 135 are covered with second electroless plated film 142a. In other respects, the structures of core substrates 100 according to the first and second embodiments are similar, and the structures of the multilayer wiring board and semiconductor device formed using core substrate 100 are also common between the first and second embodiments.
[0067] As described above, according to this embodiment, after the through-holes are filled with insulating resin, a magnetic member formed using a magnetic-coated conductor wire is embedded in the through-holes of the substrate to form an inductor. Therefore, even when a core substrate is manufactured by forming an inductor using a magnetic member after forming through-holes filled with insulating resin, the electrical characteristics of the inductor built into the core substrate can be improved.
[0068] (Embodiment 3) In the above-described first and second embodiments, through hole 112 is already formed when magnetic member 135 is embedded in through hole 113 of substrate 110, but it is also possible to form through hole 112 after embedding magnetic member 135 in through hole 113. Therefore, in the third embodiment, a method for manufacturing a multilayer wiring board in which through hole 112 is formed later will be described.
[0069] Fig. 28 is a flow diagram showing a method for manufacturing a multilayer wiring board according to embodiment 3. In Fig. 28, the same parts as in Fig. 5 are denoted by the same reference numerals. In the method for manufacturing a multilayer wiring board shown in Fig. 28, after the magnetic member 135 is flattened in step S103, through holes 112 for filling with insulating resin 125 are formed.
[0070] First, through-hole 113 for forming inductor section 130 is formed in substrate 110, which is configured to have an insulating plate-like member (step S301). That is, cylindrical through-hole 113 with an opening diameter of approximately 250 to 550 μm is formed in substrate 110, for example, as shown in FIG. 29. Through-hole 113 is formed by, for example, laser processing or drilling, and after through-hole 113 is formed, a desmear treatment is performed to remove resin residue from the inner wall surface. For example, a potassium permanganate solution can be used for the desmear treatment.
[0071] Then, a magnetic member 135 is embedded in the through hole 113 (step S102). That is, for example, as shown in FIG. 30 , a magnetic member 135 having a magnetic body 131 and a conductor wire 132 is inserted into the through hole 113. Because the diameter of the magnetic member 135 is approximately equal to or slightly larger than the diameter of the through hole 113, the elasticity of the magnetic body 131 allows the magnetic member 135 to be inserted into the through hole 113 without any gaps. In addition, because the length of the magnetic member 135 is slightly longer than the thickness of the base material 110, both ends of the magnetic member 135 protrude above and below the metal foil 111 of the base material 110.
[0072] Therefore, the protruding portion is polished to a flat surface so that both end portions of the magnetic member 135 are flush with the surface of the metal foil 111 (step S103). That is, as shown in FIG. 31 for example, both ends of the magnetic member 135 are polished so that the surface of the metal foil 111 and both end faces of the magnetic member 135 are flush with each other. In this embodiment, when both ends of the magnetic member 135 are polished, the through holes 112 for forming the through-hole portions 120 have not yet been formed. Therefore, residues generated by polishing the magnetic member 135 do not enter the through holes 112 and remain there.
[0073] Once the surface of the metal foil 111 and both end faces of the magnetic member 135 are flush with each other, through holes 112 for forming the through-hole portions 120 are formed (step S302). That is, as shown in FIG. 32, for example, a cylindrical through hole 112 having an opening diameter of about 100 to 200 μm is formed in the base material 110. The through hole 112 is formed by, for example, laser processing or drilling, and after the through hole 112 is formed, a desmear process is performed to remove resin residue from the inner wall surface. At this time, in order to reduce the effect of the solution used for desmearing on both end faces of the magnetic member 135 that are exposed to the surface, the magnetic body 131 constituting the magnetic member 135 may be made of a magnetic metal.
[0074] After through-hole 112 is formed, first electroless plated film 141a is formed to cover the exposed surface (step S104), and then first electrolytic plated film 141b is laminated on first electroless plated film 141a (step S105). That is, similar to the first embodiment, first electroless plated film 141a and first electrolytic plated film 141b are formed by applying, for example, electroless copper plating and electrolytic copper plating to the surface of metal foil 111, the end face of magnetic member 135, and the inner wall surface of through-hole 112.
[0075] By forming first electroless plated film 141a and first electrolytic plated film 141b, a through hole is formed inside first electrolytic plated film 141b within through hole 112. This through hole is filled with insulating resin 125 (step S106). For example, an epoxy-based resin containing a filler such as silica can be used as insulating resin 125. Insulating resin 125 fills the inside of first electrolytic plated film 141b without leaving any gaps, and both ends of insulating resin 125 protrude above and below first electroless plated film 141a and first electrolytic plated film 141b that are laminated on metal foil 111.
[0076] Both protruding ends of insulating resin 125 are polished to a flat surface (step S107), and when the top and bottom surfaces of first electrolytic plated film 141b are flush with both end surfaces of insulating resin 125, second electroless plated films 142a and 142b are formed on the exposed surface (steps S108 and S109). That is, similar to the first embodiment, the surface of first electrolytic plated film 141b and the end surfaces of insulating resin 125 are subjected to, for example, electroless copper plating and electrolytic copper plating, thereby forming second electroless plated films 142a and 142b.
[0077] Since all electroless plated films and electrolytic plated films have been formed by the electroless plating and electrolytic plating up to this point, etching is performed to form conductor layers 140a and 140b of through-hole portion 120 and inductor portion 130 (step S110). That is, an etching resist is formed on the portions where the plated films are to remain as conductor layers 140a and 140b, and metal foil 111, first electroless plated film 141a, first electrolytic plated film 141b, second electroless plated film 142a, and second electrolytic plated film 142b are removed by wet etching. As a result, through-hole portion 120 having conductor layer 140a as a pad and inductor portion 130 having conductor layer 140b as a pad are formed, as in the first embodiment (FIG. 17).
[0078] An insulating layer and a wiring layer are sequentially built up on the upper and lower surfaces of the thus formed core substrate 100 to form a multilayer wiring substrate (step S111). Also, a semiconductor chip may be mounted on the multilayer wiring substrate to form a semiconductor device.
[0079] As described above, according to this embodiment, a magnetic member formed using a magnetic-coated conductor wire is embedded in a through hole in a substrate, and then the through hole is formed in the substrate to form a through hole. This prevents residue generated during polishing of the magnetic member from entering and remaining in the through hole, while improving the electrical characteristics of the inductor built into the core substrate.
[0080] In the above-described embodiments, conductor layer 140b covers the entire end face of magnetic member 135. However, conductor layer 140b does not necessarily have to cover the entire end face of magnetic member 135. Specifically, as shown in FIG. 33, for example, a portion of the end face of magnetic member 135 of core substrate 100 according to embodiments 1 and 3 may not be covered by conductor layer 140b. That is, in FIG. 33, conductor wire 132 of magnetic member 135 is covered by conductor layer 140b, while a portion of magnetic body 131 is exposed and not covered by conductor layer 140b. In this case, conductor layer 140b includes first electroless plated film 141a, first electrolytic plated film 141b, second electroless plated film 142a, and second electrolytic plated film 142b.
[0081] Similarly, as shown in Fig. 34, for example, a portion of the end face of magnetic member 135 of core substrate 100 according to embodiment 2 may not be covered by conductor layer 140b. That is, in Fig. 34, conductor wire 132 of magnetic member 135 is covered by conductor layer 140b, while a portion of magnetic body 131 is exposed and not covered by conductor layer 140b. In this case, conductor layer 140b has second electroless plated film 142a and second electrolytic plated film 142b.
[0082] In this way, the core substrate 100 in which a portion of the magnetic member 135 is not covered by the conductor layer 140b can be formed by adjusting the size of the etching resist 210. That is, after all the electroless plated films and electrolytic plated films are formed, the etching resist 210 is formed only on the portion corresponding to the center of the end face of the magnetic member 135, and etching is performed using the etching resist 210 as a mask. As a result, the electroless plated films and electrolytic plated films around the etching resist 210 and the metal foil 111 are removed, exposing the peripheral portion of the end face of the magnetic member 135.
[0083] As described above, the conductor layer 140b covering the end face of the magnetic member 135 can be formed in various structures. [Explanation of symbols]
[0084] 100 core board 110 Base material 111 Metal foil 112, 113 through holes 120 through hole section 125 insulating resin 130 Inductor section 135 Magnetic Components 141a First electroless plating film 141b First electrolytic plating film 142a Second electroless plating film 142b Second electrolytic plating film 201 Conductor wire 202 Magnetic material 203 Insulating resin 220 wiring layer 225 via wiring 230 Insulating layer
Claims
1. A substrate; A through hole formed in the substrate; A magnetic member embedded in the through hole; a plating film that covers an end surface of the magnetic member exposed from the through hole, The magnetic member is The conductor wire is covered with a magnetic material. A wiring board comprising:
2. At the end surface of the magnetic member, the end of the conductor wire is exposed from the magnetic body.
2. The wiring board according to claim 1.
3. The magnetic member is The conductive wire is covered with an insulating resin containing magnetic particles.
2. The wiring board according to claim 1.
4. The magnetic member is The conductor wire is covered with a magnetic metal plating film.
2. The wiring board according to claim 1.
5. The magnetic member is a stranded wire formed by stranding together a plurality of conductor wires covered with a magnetic material; An insulating resin that covers the stranded wire; 2. The wiring board according to claim 1, further comprising:
6. The plating film is an electroless plating film covering an end surface of the magnetic member; an electrolytic plating film laminated on the electroless plating film; 2. The wiring board according to claim 1, further comprising:
7. The plating film is a first electroless plating film covering a surface of the base material; a first electrolytic plating film laminated on the first electroless plating film; a second electroless plating film covering a surface of the first electrolytic plating film and an end face of the magnetic member; a second electrolytic plating film laminated on the second electroless plating film; 2. The wiring board according to claim 1, further comprising:
8. The plating film is A part of the end face of the magnetic member is covered and the other part is exposed.
2. The wiring board according to claim 1.
9. Another through hole formed in the substrate; and an insulating resin filled in the other through hole, The plating film is a first plating film interposed between an inner wall surface of the other through hole and the insulating resin; a second plating film that covers an end surface of the insulating resin exposed from the other through hole; 2. The wiring board according to claim 1.
10. An insulating resin interposed between the inner wall surface of the through hole and the magnetic member.
2. The wiring board according to claim 1, further comprising:
11. An insulating layer provided on a surface of the base material; a wiring layer provided on a surface of the insulating layer; and a via wiring provided in the insulating layer, The wiring layer is The via wiring is connected to the plating film.
2. The wiring board according to claim 1.
12. forming a through hole in a substrate; A step of covering the conductor wire with a magnetic material to form a magnetic member; embedding the magnetic member in the through hole; forming a plating film to cover an end surface of the magnetic member exposed from the through hole; 2. A method for manufacturing a wiring board comprising the steps of:
13. The step of forming the through hole includes: forming the through hole and another through hole in the base material; The step of forming the plating film includes: A plating film is formed to cover the end surface of the magnetic member exposed from the through hole and the inner wall surface of the other through hole.
13. The method for manufacturing a wiring board according to claim 12.
14. The method further includes a step of forming another through hole in the base material after the magnetic member is embedded in the through hole, The step of forming the plating film includes: A plating film is formed to cover the end surface of the magnetic member exposed from the through hole and the inner wall surface of the other through hole.
13. The method for manufacturing a wiring board according to claim 12.
15. A step of filling the other through hole on which the plating film is formed with an insulating resin.
15. The method for manufacturing a wiring board according to claim 13, further comprising: