Optical System

JP2023552658A5Active Publication Date: 2024-11-223M INNOVATIVE PROPERTIES CO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023535797
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2020-12-14
Filing Date
2021-11-16
Publication Date
2024-11-22
Estimated Expiration
2041-11-16

AI Technical Summary

Technical Problem

Existing optical systems face challenges in maintaining shape accuracy and reliability due to thermal expansion mismatches and unbalanced mechanical properties in layered composite polymer optical lenses, leading to changes in curvature over time and failure in reliability tests.

Method used

The integration of multilayer polymer optical films with balanced elastic properties and thermal strains, aligned with the principal directions of stress development, to ensure symmetrical material distribution and mechanical balance, preventing changes in lens curvature.

Benefits of technology

The solution maintains shape accuracy and enhances reliability by balancing mechanical properties in both orthogonal axes, ensuring consistent performance over time and under varying temperatures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The optical assembly includes an integrated lens assembly having one or more lenses bonded together with spaced-apart first and second lens major surfaces. First and second optical films are bonded to the first and second lens major surfaces, respectively. The first and second optical films include multiple polymer layers. Each of the polymer layers has an average thickness of less than about 500 nm. For substantially normally incident light and in the visible wavelength range, the multiple polymer layers in the first optical film have an average optical transmittance and average optical reflectance greater than about 70% for a first polarization state and an orthogonal second polarization state, respectively. The multiple polymer layers in the second optical film have an average optical transmittance greater than about 70% for at least one of the first and second polarization states.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] FIELD OF THE DISCLOSURE The present disclosure relates generally to the field of optics, and more particularly to optical systems for forming images. [Background technology]

[0002] Optical systems capable of forming images from illuminated objects find numerous and important applications in areas such as advertising, marketing, and product display. Optical systems may also be included in head-mounted displays to provide images to a viewer. The optical system may include a display panel and various optical components between the display panel and the viewer's eyes. Such systems are advantageously small in size, have a wide viewing angle and high contrast, and be viewable in all ambient lighting conditions. Summary of the Invention

[0003] Some aspects of the present disclosure relate to an optical assembly including an integrated lens assembly having one or more lenses bonded together, the lenses having first and second spaced-apart lens major surfaces. First and second optical films are bonded to the first and second lens major surfaces, respectively. Each of the first and second optical films includes a plurality of polymer layers, totaling at least 10 layers, each having an average thickness of less than about 500 nm. For substantially normally incident light and in the visible wavelength range spanning from about 420 nm to about 680 nm, the plurality of polymer layers in the first optical film have an average optical transmittance of greater than about 70% for a first polarization state in the visible wavelength range and an average optical reflectance of greater than about 70% for an orthogonal second polarization state. The plurality of polymer layers in the second optical film have an average optical transmittance of greater than about 70% for at least one of the first and second polarization states in the visible wavelength range.

[0004] Some other aspects of the present disclosure relate to optical assemblies including a polymer optical lens having oppositely facing first and second lens major surfaces, at least one of which is curved. First and second polymer optical films are bonded to the first and second lens major surfaces, respectively. The first and second polymer optical films have respective average thicknesses T1 and T2, respective elastic shear moduli Q1 and Q2 in the same first direction, and respective thermal strains E1 and E2 in the same second direction, and the products Q1T1E1 and Q2T2E2 are within 20% of each other.

[0005] Some other aspects of the present disclosure relate to optical assemblies that include a polymer optical lens having first and second opposing lens major surfaces, at least one of which is curved. First and second polymer optical films are bonded to the first and second lens major surfaces, respectively. The first and second polymer optical films have respective average thicknesses T1 and T2, respective elastic shear moduli Q1 and Q2 in the same first direction, and respective thermal expansion coefficients A1 and A2 in the same second direction, and the products Q1T1A1 and Q2T2A2 are within 20% of each other.

[0006] Some aspects of the present disclosure relate to an optical assembly including an integrated lens assembly having one or more lenses bonded together with spaced-apart first and second lens major surfaces. A polymeric reflective polarizer is bonded to the first lens major surface, and an optical film is bonded to the second lens major surface. The optical film includes a first optical layer having refractive indices nx1 and ny1 along mutually orthogonal in-plane x and y directions, respectively, and nz1 along a thickness direction of the optical layer, which is orthogonal to the x and y directions. For at least one wavelength in the visible wavelength range spanning from about 420 nm to about 650 nm, the magnitude of the difference between nx1 and ny1 is greater than about 0.02, and the magnitude of the difference between nz1 and one of nx1 and ny1 is less than about 0.02. For substantially normally incident light and in the visible wavelength range, the reflective polarizer has an average light transmittance of greater than about 70% for incident light polarized along one of the x and y directions, and an average light reflectance of greater than about 70% for incident light polarized along the other of the x and y directions. Polymeric reflective polarizers exhibit transmittance variation depending on the azimuthal orientation, with maximum reflectance corresponding to one orientation that defines the major optical axis. This may alternatively be referred to as the block state. At an orientation perpendicular to the block state, transmittance reaches a maximum, which is commonly referred to as the pass state of the polarizer. These pass and block states define the major optical axis of the reflective polarizer. The first optical layer of the optical film has an average light transmittance of greater than about 70% for incident light polarized along each of the x and y directions.

[0007] Some aspects of the present disclosure relate to an optical assembly including an integrated lens assembly having one or more lenses bonded together, the lenses having first and second spaced-apart lens major surfaces. A polymeric reflective polarizer is bonded to the first lens major surface, and an optical film is bonded to the second lens major surface. The optical film includes a first optical layer having refractive indices nx1 and ny1 along mutually orthogonal in-plane x and y directions, respectively, and nz1 along a thickness direction of the optical layer, which is orthogonal to the x and y directions. For at least one wavelength in the visible wavelength range spanning from about 420 nm to about 650 nm, nx1 > ny1 > nz1, and each of nx1 - ny1 and ny1 - nz1 is greater than about 0.02. For substantially normally incident light and in the visible wavelength range, the reflective polarizer has an average optical transmittance of greater than about 70% for incident light polarized along one of the x and y directions and an average optical reflectance of greater than about 70% for incident light polarized along the other of the x and y directions. The first optical layers of the optical film have an average optical transmittance of greater than about 70% for incident light polarized along each of the x and y directions.

[0008] Some other aspects of the present disclosure relate to optical assemblies including a polymeric optical lens having first and second opposing lens major surfaces, at least one of which is curved. First and second polymeric optical films are bonded to the first and second lens major surfaces, respectively. Each of the first and second polymeric optical films has an average thickness T, an elastic shear modulus Q along the same first direction, and a thermal distortion E along the first direction, and the product QTE of the first polymeric optical film is within 20% of the product QTE of the second polymeric optical film.

[0009] In some cases, the thermal strain may be dominated by reversible thermal expansion behavior. In these cases, the thermal strain may be fully defined as the product of the thermal expansion coefficients A1 and A2 defined in the same second direction and the temperature change. In other embodiments, the thermal strain may be dominated by irreversible or contraction behavior. In other embodiments, the thermal strain may result from a combination of both reversible thermal expansion and irreversible effects.

[0010] Some other aspects of the present disclosure relate to optical assemblies including a polymeric optical lens having first and second opposing lens major surfaces, at least one of which is curved. First and second polymeric optical films are bonded to the first and second lens major surfaces, respectively. Each of the first and second polymeric optical films has an average thickness T, a modulus of elasticity Q along the same first direction, and a coefficient of thermal expansion A along the first direction, and the product QTA of the first polymeric optical film is within 20% of the product QTA of the second polymeric optical film.

[0011] Another embodiment of the present disclosure relates to an optical system for displaying an image to a viewer, the optical system including a display adapted to emit an image and an optical assembly according to one or more of the embodiments described in the present disclosure. A first retarder layer is disposed between the optical assembly and the display. A display lens is disposed between the first retarder layer and the display. A partial reflector is disposed on and conforms to a major surface of the first optical lens, and has an average light reflectance of at least 30% in the visible wavelength range. [Brief explanation of the drawings]

[0012] Various aspects of the present disclosure will be discussed in more detail with reference to the accompanying drawings.

[0013] [Figure 1A] 1A and 1B are schematic diagrams illustrating optical assemblies according to some embodiments. [Figure 1B] 1A-1C are schematic diagrams illustrating an integrated lens assembly according to some embodiments. [Figure 2] 1A-1C are schematic diagrams illustrating the structure of optical films according to some embodiments. [Figure 3A] 1A-1C show schematic diagrams of lens assemblies with one or more lenses having concave and / or convex lens surfaces according to different embodiments. [Figure 3B]1A-1C show schematic diagrams of lens assemblies with one or more lenses having concave and / or convex lens surfaces according to different embodiments. [Figure 3C] 1A-1C show schematic diagrams of lens assemblies with one or more lenses having concave and / or convex lens surfaces according to different embodiments. [Figure 4] FIG. 1 illustrates a schematic diagram of an optical system for displaying an image to a viewer, according to some embodiments. [Figure 5] 1A-1C are schematic diagrams illustrating optical assemblies with polymer optical lenses according to some embodiments.

[0014] The drawings are not necessarily to scale. Like numbers used in the drawings refer to like components. However, it will be understood that the use of a number to refer to a component in a particular drawing is not intended to limit the component in another drawing bearing the same number. DETAILED DESCRIPTION OF THE INVENTION

[0015] In the following description, reference is made to the accompanying drawings, which form a part hereof, and in which are shown by way of illustration various embodiments. It is to be understood that other embodiments are contemplated and may be made without departing from the scope or spirit of the present disclosure. Accordingly, the following detailed description is not to be taken in a limiting sense.

[0016] Without considering the balance of the mechanical system, especially with regard to thermal expansion mismatch in layered composites, insert molding a lens with an optical film can result in changes in optical shape that may no longer meet the optical specifications of the lens. If the in-plane mechanical properties are not balanced, changes in curvature with temperature or time can occur. Mechanically unbalanced composite polymer optical lenses that include optically functional films (uniaxially / biaxially stretched optical films, whose material is similar or dissimilar to the polymer resin) on the lens surface(s) may be unable to maintain shape accuracy and may fail reliability tests. In layered composites, mechanical balance is achieved by ensuring symmetric distribution of material properties from a central "plane."

[0017] While it may be possible to reduce the bending effect by making one layer thicker than the other, it cannot eliminate the effect. The initial curvature can be altered so that the structure bends to the desired shape at the end of the process, but the desired shape may only occur at one temperature and may be prone to change over time due to creep. It may be advantageous to balance both elastic (reversible) properties and residual stresses within the structure. Also, while balancing mechanical properties in one direction can reduce bending in that direction, in practice, this balancing must generally be performed simultaneously along two separate, orthogonal axes, preferably aligned with the axes of maximum and minimum stress development within the film, also referred to herein as the principal directions of stress development.

[0018] The embodiments disclosed herein provide a solution for producing insert molded optical lenses with reliable morphology. Other embodiments disclosed herein describe compound optical lenses with balanced uniaxial / biaxially stretched optical films on the lens surface(s) to maintain and improve shape accuracy.

[0019] An optical system (600) for displaying an image (111) to a viewer (113) is shown schematically in Figure 4. The optical system includes an optical assembly (400) and a display (110) adapted to emit an image (112). A first retarder layer (120) may be disposed between the optical assembly (400) and the display (110), and a display lens (130) may be disposed between the first retarder layer (120) and the display (110). A partial reflector (140) may be disposed on the display lens (130) and, in some embodiments, may be fabricated to conform to a major surface (131) of the display lens (130). The partial reflector (140) may have an average light reflectance of at least 30% in the visible wavelength range.

[0020] 1A and 1B schematically illustrate an optical assembly (400) including an integrated lens assembly (100). In some embodiments, the integrated lens assembly may include a single lens (10, 20). In other embodiments, the lens assembly (100) may include one or more lenses (10, 20) bonded together, having spaced-apart first and second lens major surfaces (11, 21), as best seen in FIG. 1B. A first optical film (30) may be bonded to the first lens major surface (11), and a second optical film (40) may be bonded to the second lens major surface (21).

[0021] In some embodiments, as shown in FIG. 3A, one or more lenses (10, 20) of an integrated lens assembly (100′) may be bonded to one another via an adhesive layer (60). As shown in FIGS. 3A-3C, both the first lens major surface (11) and the second lens major surface (21) of the lenses (10, 20) may be convex, or both the first lens major surface (11′) and the second lens major surface (21′) may be concave. In other embodiments, one of the first and second lens major surfaces (11″) may be concave, and the other of the first and second lens major surfaces (21″) may be convex.

[0022] In some embodiments, each of the first optical film (30) and the second optical film (40) may be a multilayer optical film (MOF) including multiple polymer layers (31, 32), as shown in FIG. 2 . In some examples, the multiple polymer layers (31, 32) may have a total number of at least 10 layers. In some examples, the multiple polymer layers (31, 32) may have a total number of at least 50, at least 100, at least 200, at least 300, at least 400, or at least 500 layers. Each of the polymer layers (31, 32) may have an average thickness of less than about 500 nm, less than about 400 nm, or less than about 200 nm. In some embodiments, the number of layers in the optical film (30) may be selected to achieve desired optical properties using a minimum number of layers for reasons of film thickness, flexibility, and economy. For example, at least one of the first optical film (30) and the second optical film (40) may include fewer than 10 polymer layers. At least one of the first optical film (30) and the second optical film (40) may include at least one skin layer (33). The average thickness of the at least one skin layer (33) may be greater than about 500 nm, and in some instances, greater than 700 nm, or even greater than 1 micron. For the first and second optical films including multiple polymer layers described herein, the major directions are selected so that the x- and y-axes are in the plane of the layers and the z-axis corresponds to the thickness of the layers. The major axes of elasticity of the film are the directions along which the elastic modulus, thermal expansion coefficient, and refractive index reach their extreme values ​​(maximum or minimum). These should also be aligned with the light-transmitting and light-blocking directions within the film. When thermal strain is dominated by reversible thermal expansion behavior, the major direction of stress development will be aligned with the major direction of elasticity of the film. However, when irreversible effects such as shrinkage dominate the thermal strain, the major direction of stress development may differ significantly from the major direction of elasticity.

[0023] Multilayer polymer films can exhibit a wide range of optical and physical properties and may be utilized in a variety of optical and non-optical applications. The optical and physical properties of a multilayer film can depend on many variables, including the type of polymer material used in the individual layers, the overall number of individual layers in the film, and / or the layer thickness profile of the film. As a result, the properties of a multilayer film can be tailored by precisely controlling one or more of these variables during the film manufacturing process. A multilayer polymer film may include multiple individual layers, each formed from one or more types of polymer material. For example, a particular multilayer optical film may include hundreds of individual polymer layers, alternating between high and low refractive index polymer materials. The formation of such polymer layers can be achieved via a feedblock device that receives suitable polymeric materials, typically in the form of a polymer melt stream, and directs the polymeric materials into a multilayer polymer flowstream containing a stack of individual layers. After exiting the feedblock, the multilayer flowstream can be further processed in a film line to produce a multilayer optical film. Examples of feedblocks and film lines configured to produce multilayer optical films are described, for example, in U.S. Patent No. 6,783,349 to Neavin et al.

[0024] Various MOFs are commonly known. MOFs generally comprise alternating first and second polymer layers (31, 32) comprising at least one birefringent polymer (e.g., an oriented semi-crystalline polymer) and one second polymer. In some aspects, the optical film (30) may be a multilayer stack having alternating first and second optical layers (31, 32) of at least two materials. In one embodiment, the materials of the first and second layers (31, 32) may be composed of a polymer such as polyester. For example, an exemplary polymer useful as the first birefringent layer (31) in the multilayer optical film (30) may be polyethylene naphthalate (PEN). Other semi-crystalline polyesters suitable as birefringent polymers for the first birefringent layer (31) in the multilayer optical film (30) may include, for example, polybutylene 2,6-naphthalate (PBN), polyethylene terephthalate (PET), and the like. The second layer (32) of the multilayer optical film (30) can be made from a variety of polymers having a glass transition temperature compatible with that of the first birefringent polymer layer (31) and a refractive index similar to the isotropic refractive index of the first birefringent polymer layer (31). Examples of other polymers suitable for use in optical films, particularly the second polymer layer (32), can include vinyl polymers and copolymers made from monomers such as vinyl naphthalene, styrene, maleic anhydride, acrylates, and methacrylates. Examples of such polymers include polyacrylates, polymethacrylates such as poly(methyl methacrylate) (PMMA), and isotactic or syndiotactic polystyrenes. Other polymers include condensation polymers such as polysulfones, polyamides, polyurethanes, polyamic acids, and polyimides. Additionally, the second polymer layer (32) can be formed from homopolymers and copolymers of polyester, polycarbonate, fluoropolymer, and polydimethylsiloxane, as well as mixtures thereof. The layers are selected to achieve reflection of a specific bandwidth of electromagnetic radiation. In one embodiment, the materials of the layers (31, 32) can have different refractive indices.In some embodiments, one of the first optical film (30) and the second optical film (40) may include PET as the first optical layer (31) and a copolymer of PMMA (coPMMA) or any other polymer with a low refractive index, including copolyesters, fluorinated polymers, or combinations thereof, as the second optical layer (32). The transmission and reflection properties of the optical films (30, 40) are based on the coherent interference of light caused by the refractive index difference between layers (31) and (32) and the thickness of layers (31, 32).

[0025] In some embodiments, for substantially normally incident light (50) and in the visible wavelength range spanning from about 420 nm to about 680 nm, the multiple polymer layers (31, 32) in the first optical film (30) may have an average light transmittance for a first polarization state (x-axis) of greater than about 70% and an average light reflectance for an orthogonal second polarization state (y-axis) of greater than about 70% in the visible wavelength range. In some examples, the average light transmittance of the first optical film (30) for the first polarization state (x-axis) may be greater than about 80%, greater than about 85%, greater than about 90%, greater than about 95%, or greater than about 99%; and the light reflectance of the first optical film (30) for the orthogonal second polarization state (y-axis) in the visible wavelength range may be greater than about 80%, greater than about 85%, greater than about 90%, greater than about 95%, or greater than about 99%. The multiple polymer layers in the second optical film (40) may have an average light transmittance in the visible wavelength range for at least one or each of the first and second polarization states of greater than about 70%, and in some examples, greater than about 80%, greater than about 85%, greater than about 90%, greater than about 95%, or greater than about 99%.

[0026] In some embodiments, in the ultraviolet wavelength range, for example, for at least one wavelength less than about 400 nm, the multiple polymer layers (31, 32) in the second optical film (40) may have an average light transmittance for a first polarization state (x-axis) of greater than about 60%, greater than about 70%, or greater than about 80% and an average light reflectance for a second polarization state (y-axis) of greater than about 60%, greater than about 70%, or greater than about 80%.

[0027] According to some embodiments, in the infrared wavelength range, for example, for at least one wavelength greater than about 750 nm, the multiple polymer layers (31, 32) in the second optical film (40) may have an average light transmittance for a first polarization state (x-axis) of greater than about 60%, greater than about 70%, or greater than about 80% and an average light reflectance for a second polarization state (y-axis) of greater than about 60%, greater than about 70%, or greater than about 80%.

[0028] In another embodiment, the second optical film (40) may be made to be substantially transparent to at least one wavelength greater than about 750 nm in the infrared wavelength range. For example, the polymer layers within the second optical film (40) may have an average light transmittance of greater than about 60%, greater than about 70%, or greater than about 80% for each of the first (x-axis) and second (y-axis) polarization states.

[0029] In another embodiment, the second optical film (40) may be made to be substantially reflective for at least one wavelength greater than about 750 nm in the infrared wavelength range. For example, the multiple polymer layers within the second optical film (40) may have an average light reflectivity greater than about 60%, greater than about 70%, or greater than about 80% for each of the first (x-axis) and second (y-axis) polarization states.

[0030] In another embodiment, at least one of the first optical film (30) and the second optical film (40) may be fabricated to be substantially non-absorbing in the visible wavelength range spanning from about 420 nm to about 680 nm. For example, for at least one of the first (x-axis) and second (y-axis) polarization states, the multiple polymer layers of at least one of the first optical film (30) and the second optical film (40) may have an average optical absorptance of less than about 20%, less than about 15%, less than about 10%, or less than about 5% in the visible wavelength range.

[0031] In other embodiments, an optical assembly may include multiple layers of orthotropic materials that may flex to a small extent due to either external loads or internal loads (e.g., thermal mismatch). Each layer may have an average thickness, a set of orthotropic elastic stiffness properties, and a set of orthotropic thermal strains. For example, as best seen in FIG. 5 , a multiple-layer optical assembly (500) may include a polymer optical lens (70) having a first lens major surface (71) and an opposing second lens major surface (72), a first polymer optical film (80) bonded to the first lens major surface (71), and a second polymer optical film (90) bonded to the second lens major surface (72). At least one of the first lens surface (71) and the second lens surface (72) may be curved. Each of the first polymeric optical film (80) and the second polymeric optical film (90) may have an average thickness T, an elastic modulus Q along the same first direction (101), and a thermal strain E along the first direction. In some embodiments, the product QTE of the first polymeric optical film (80) may be within 20%, 15%, 10%, 5%, 2%, or 1% of the product QTE of the second polymeric optical film (90). When the thickness of the polymeric optical lens (70) is greater than the average thickness of the first polymeric optical film (80) and the second polymeric optical film (90), the thermal strain along the midplane located halfway through the total thickness of the optical assembly may be dominated by the lens material. In some examples, to prevent thermal bending of the optical lens, both the layer stiffness modulus of the first polymer optical film (80) and the second polymer optical film (90) and the product of the layer stiffness modulus and the thermal distortion of the first polymer optical film (80) and the second polymer optical film (90) may be offset.

[0032] In other embodiments, the first polymeric optical film (80) bonded to the first lens major surface (71) may have an average thickness T1, and the second polymeric optical film (90) bonded to the second lens major surface (72) may have an average thickness T2. At least one of the first lens surface (71) and the second lens surface (72) may be curved. In some examples, the first polymeric optical film (80) may be a mechanically balanced film (MBF), and the second polymeric optical film (90) may be a reflective polarizing film (RPF). The thickness profiles of the first polymeric optical film (80) and the second polymeric optical film (90) can generally be selectively obtained, as described, for example, in U.S. Patent Nos. 5,882,774 (Jonza et al.), 6,179,948 (Merrill et al.), 6,783,349 (Neavin et al.), 6,967,778 (Wheatley et al.), and 9,162,406 (Neavin et al.). In some examples, at least one of the first polymeric optical film (80) and the second polymeric optical film (90) can include a plurality of polymer layers totaling at least 10 layers. In other examples, at least one of the first polymeric optical film (80) and the second polymeric optical film (90) can include fewer than 10 polymer layers.

[0033] For example, as shown in Figure 5, a first polymer optical film (80) may have an elastic shear modulus Q1 in a first direction (101), and a second polymer optical film (90) may have an elastic shear modulus Q2 in the same first direction (101). The first polymer optical film (80) may have a thermal strain E1 in a second direction (102), and the second polymer optical film (90) may have a thermal strain E2 in the same second direction (102). The first direction (101) and the second direction (102) may be within 20 degrees of each other, and in some examples may be within 15 degrees, 10 degrees, 5 degrees, or 2 degrees of each other.

[0034] In some embodiments, the products Q1T1E1 and Q2T2E2 may be within 20% of each other. In some other embodiments, the products Q1T1E1 and Q2T2E2 may be within 15%, 10%, 5%, 2%, or 1% of each other. By canceling the product of the elastic shear modulus, thickness, and thermal strain of the first polymeric optical film (80) and the second polymeric optical film (90), changes in lens curvature can be prevented.

[0035] Changes in lens curvature can also occur in optical lenses as a result of simple thermal expansion of the lens material. In some embodiments, the first polymer optical film (80) and the second polymer optical film (90) can each have an average thickness T, an elastic modulus Q along the same first direction (101), and a thermal expansion coefficient A along the same first direction. The product QTA of the first polymer optical film (80) can be within 20% of the product QTA of the second polymer optical film (90). In some examples, the product QTA of the first polymer optical film (80) can be within 15%, 10%, 5%, 2%, or 1% of the product QTA of the second polymer optical film (90).

[0036] In most cases, the major axis of A will coincide with the major axis of Q within 5 degrees. In contrast, the major axis of E can be completely independent of the major axes of Q and A. In some instances, the difference between the major axes of A and Q and E may be greater than 20 degrees. In other cases, the difference between the major axes of A and Q and E may be greater than 30 degrees. In other cases, the difference between the major axes of A and Q and E may be greater than 40 degrees. In such cases, the major axis or direction of thermal stress development will be defined as the direction in which the product of the elastic modulus Q and the thermal strain E achieves their extreme value (maximum or minimum), as opposed to the major direction of the individual properties. In such cases, the major direction of thermal stress may not be aligned with the light transmission and light blocking directions within the film. Also, while balancing mechanical properties in one direction can reduce bending in that direction, in practice this balancing must generally be done simultaneously along two separate orthogonal axes, preferably aligned with the axes of maximum and minimum stress development within the film.

[0037] When the lens thickness is much greater than the film thickness and the lens curvature is small, the above design criteria can be applied very strictly, especially when the film expansion is governed by reversible behavior. However, for thinner lenses and / or higher lens curvatures, the mechanisms governing both the magnitude and direction of mechanical balancing become more complex and may require some corrections. For example, for thinner lenses, the lens's elastic and bending stiffness moduli may also need to be considered. The mathematical equations covering the precise balancing become more complex, but have been well-studied over time in the composites industry and are well documented in composites textbooks such as Vinson and Sierakowski (The Behavior of Structures Composed of Composite Materials, Martinus Nijhoff Publishers, Dordrecht, 1987). High lens curvatures can further complicate these relationships. However, while the mathematical equations describing the exact balancing can be more complex, in many cases of interest within this application, the results of the exact calculations will still fall within the aforementioned conditions of the products of Q, T, and E, and / or Q, T, and A for each film, and be in the same direction and within 20% of each other.

[0038] Also, if one of the lens surfaces has a very high curvature relative to the other side, forming an orthotropic film on the curved surface may cause the film's principal directions, and even the projection of those principal directions onto the low-curvature (or flat) side, to vary with position and relative to a substantially uniform film on the low-curvature side. In such cases, it may only be possible to achieve perfect balance at a single point or along a pair of horizontal axes. In such cases, balancing becomes an optimization problem, and the selection of the best balancing region is determined by whichever results in the least amount of deviation from the desired lens shape. However, in many cases of interest within this application, the directional difference between the principal directions of the two films at any point projected onto the low-curvature surface remains within 20 degrees of each other.

[0039] In some embodiments, the first polymer optical film (80) and the second polymer optical film (90) may have the same thermal expansion coefficients A1 and A2, respectively, in the third direction (103), as shown in FIG. 5 . In some examples, canceling the products of the elastic modulus, thickness, and thermal expansion of the first polymer optical film (80) and the second polymer optical film (90) can prevent changes in lens curvature. For example, in some aspects, the products Q1T1A1 and Q2T2A2 can be within 20% of each other. In other examples, the products Q1T1A1 and Q2T2A2 can be within 15%, 10%, 5%, 2%, or 1% of each other. The first direction (101) and the third direction (103) can be within 20 degrees of each other, and in some examples, can be within 15, 10, 5, or 2 degrees of each other.

[0040] In some other embodiments, along the same second direction (102) perpendicular to the first direction, the first polymer optical film (80) and the second polymer optical film (90) may each have an average thickness T, an elastic shear modulus Q', and a thermal distortion E'. The product Q'TE' of the first polymer optical film (80) may be within 20% of the product Q'TE' of the second polymer optical film (90). In some examples, the product Q'TE' of the first polymer optical film (80) may be within 15%, 10%, 5%, 2%, or 1% of the product Q'TE' of the second polymer optical film (90). In other aspects, along the second direction (102), the first polymer optical film (80) and the second polymer optical film (90) may each have a coefficient of thermal expansion A'. The product Q'TA' of the first polymeric optical film (80) may be within 20%, within 15%, within 10%, within 5%, within 2%, or within 1% of the product Q'TA' of the second polymeric optical film (90).

[0041] In some embodiments, the first direction may be substantially in-plane of each of the first polymeric optical film (80) and the second polymeric optical film (90). The second direction may be substantially in-plane of each of the first polymeric optical film (80) and the second polymeric optical film (90). For first and second polymeric optical films comprising multiple polymer layers described herein, the major directions are selected such that the x- and y-axes are in the plane of the layers and the z-axis corresponds to the thickness or height of the layers. In some embodiments, the first and second directions may be selected to be within 10 degrees, or within 5 degrees, of the major in-plane directions (x, y) of the films.

[0042] In some embodiments, for substantially normally incident light (51, 52), the first polymeric optical film (80) and the second polymeric optical film (90) each may have an average light transmittance of greater than about 70%, greater than 80%, or greater than 90% for at least a first polarization state (x-axis) in the visible wavelength range from about 420 nm to about 650 nm. For substantially normally incident light (51, 52), at least one of the first polymeric optical film (80) and the second polymeric optical film (90) may have an average light transmittance of greater than about 70%, greater than 80%, or greater than 90% for a second polarization state (y-axis) orthogonal to the first polarization state in the visible wavelength range from about 420 nm to 650 nm.

[0043] Referring back to FIGS. 1A and 1B, in some embodiments, the first optical film (30) may be a polymeric reflective polarizer (30) bonded to the first lens major surface (11), and the second optical film (40) may be a uniaxially oriented optical film (40) bonded to the second lens major surface (21). In some aspects, the optical film may comprise a birefringent material. The term "birefringence" means that the refractive indices in the orthogonal x, y, and z directions are not all the same. For the optical films described herein, the principal directions may be selected such that the x and y axes are in the plane of the film and the z axis corresponds to the thickness or height of the film. The principal directions of the film are the directions in which the modulus of elasticity, coefficient of thermal expansion, and refractive index achieve their extreme values ​​(maximum or minimum). These should also be aligned with the light-passing and light-blocking directions within the reflective polarizer film.

[0044] In some examples, the optical film (40) may include a first optical layer having refractive indices nx1 and ny1 along the mutually perpendicular in-plane x- and y-directions, respectively, and a refractive index nz1 along a thickness direction of the optical layer perpendicular to the x- and y-directions. For at least one wavelength in the visible wavelength range spanning from about 420 nm to about 650 nm, the in-plane birefringence, which is the magnitude of the difference between the maximum in-plane refractive index nx1 and the minimum in-plane refractive index ny1 of the first optical layer, may be greater than about 0.02. In some examples, the magnitude of the difference between nx1 and ny1 may be greater than about 0.05, greater than about 0.10, greater than about 0.15, greater than about 0.20, or greater than about 0.22. The out-of-plane birefringence, which is the magnitude of the difference between one of the in-plane refractive indices (e.g., nx1 or ny1) and the out-of-plane refractive index nz1 of the first optical layer, may be less than about 0.02. In some examples, the magnitude of the difference between nz1 and one of nx1 and ny1 may be less than about 0.015, less than about 0.01, less than about 0.007, or less than about 0.005. The optical film (40) may also include a second optical layer, which may be an isotropic layer. The second optical layer includes refractive indices nx2, ny2, and nz2 along the x-, y-, and z-directions, respectively. In some examples, the in-plane birefringence, which is the magnitude of the maximum difference between the refractive indices nx2, ny2, and nz2 of the second optical layer, may be less than about 0.02 for at least one wavelength in the visible wavelength range spanning from about 420 nm to about 650 nm. In some examples, the out-of-plane birefringence, which is the magnitude of the difference between the refractive indices nx2, ny2, and nz2 of the second optical layer, may be less than about 0.015, less than about 0.01, less than about 0.007, or less than about 0.005.

[0045] In some other embodiments, nx1 > ny1 > nz1 for at least one wavelength in the visible wavelength range spanning from about 420 nm to about 650 nm. In other embodiments, the magnitude of the difference between each of nx1 - ny1 and ny1 - nz1 may be greater than about 0.02. In some examples, the magnitude of each of nx1 - ny1 and ny1 - nz1 may be greater than about 0.03, greater than about 0.04, or greater than about 0.05.

[0046] For substantially normally incident light and in the visible wavelength range, the reflective polarizer (30) may have an average light transmittance of greater than about 70% for incident light polarized along one of the x and y directions. In some examples, the average light transmittance may be greater than about 80% or greater than about 90% for incident light polarized along one of the x and y directions. For substantially normally incident light and in the visible wavelength range, the average light reflectance of the reflective polarizer (30) may be greater than about 70% for incident light polarized along the other of the x and y directions. In some examples, the average light reflectance may be greater than about 80% or greater than about 90% for incident light polarized along the other of the x and y directions. The first optical layer of the optical film (40) may have an average light transmittance of greater than about 70% for incident light polarized along each of the x and y directions. In some examples, the average light transmittance may be greater than about 80% or greater than about 90% for incident light polarized along each of the x and y directions.

Claims

1. an integral lens assembly including one or more lenses cemented together, the one or more lenses having spaced apart first and second lens major surfaces; first and second optical films bonded to the first and second lens major surfaces, respectively, each of the first and second optical films comprising a plurality of polymer layers totaling at least 10 layers, each of the polymer layers having an average thickness of less than about 500 nm, thereby providing substantially normal incident light and a visible wavelength range spanning from about 420 nm to about 680 nm; the plurality of polymer layers in the first optical film have an average light transmittance of greater than about 70% for a first polarization state and an average light reflectance of greater than about 70% for an orthogonal second polarization state in the visible wavelength range; the plurality of polymer layers in the second optical film have an average light transmittance of greater than about 70% for at least one of the first and second polarization states in the visible wavelength range; first and second optical films; An optical assembly comprising:

2. 2. The optical assembly of claim 1, wherein the plurality of polymer layers in the second optical film have an average light transmittance of greater than about 70% for each of the first and second polarization states in the visible wavelength range.

3. 2. The optical assembly of claim 1, wherein for at least one wavelength less than about 400 nm, the plurality of polymer layers in the second optical film have an average light transmittance for the first polarization state greater than about 60% and an average light reflectance for the second polarization state greater than about 60%, and for at least one wavelength greater than about 750 nm, the plurality of polymer layers in the second optical film have an average light transmittance for the first polarization state greater than about 60% and an average light reflectance for the second polarization state greater than about 60%.

4. 10. The optical assembly of claim 1, wherein for at least one of the first and second polarization states, the plurality of polymer layers of at least one of the first and second optical films has an average light absorption of less than about 20% in the visible wavelength range.

5. 1. An optical system for displaying an image to a viewer, comprising: a display adapted to emit an image; The optical assembly of claim 1 ; a first retarder layer disposed between the optical assembly and the display; a display lens disposed between the first retarder layer and the display; a partial reflector disposed on and conforming to a major surface of the display lens, the partial reflector having an average light reflectance of at least 30% in the visible wavelength range; An optical system comprising:

6. a polymer optical lens including first and second opposing lens major surfaces, at least one of the first and second lens surfaces being curved; first and second polymeric optical films bonded to the first and second lens major surfaces, respectively, having respective average thicknesses T1 and T2, respective elastic shear moduli Q1 and Q2 in the same first direction, and respective thermal strains E1 and E2 in the same second direction, the products Q1T1E1 and Q2T2E2 being within 20% of each other; An optical assembly comprising:

7. 7. The optical assembly of claim 6, wherein the first and second polymeric optical films have respective thermal expansion coefficients A1 and A2 in the same third direction, the products Q1T1A1 and Q2T2A2 are within 20% of each other, and the first direction and the third direction are within 20 degrees of each other.

8. a polymer optical lens including first and second opposing lens major surfaces, at least one of the first and second lens surfaces being curved; first and second polymeric optical films bonded to the first and second lens major surfaces, respectively, having respective average thicknesses T1 and T2, respective elastic shear moduli Q1 and Q2 in the same first direction, and respective thermal expansion coefficients A1 and A2 in the same second direction, the products Q1T1A1 and Q2T2A2 being within 20% of each other; An optical assembly comprising:

9. 9. The optical assembly of claim 8, wherein for substantially normally incident light, the first and second polymeric optical films each have an average light transmission of greater than about 70% for at least a first polarization state in the visible wavelength range spanning from about 420 nm to about 650 nm.

10. 9. The optical assembly of claim 8, wherein the first and second polymeric optical films have respective thermal strains E1 and E2 in the same third direction, the products Q1T1E1 and Q2T2E2 are within 20% of each other, and the first direction and the third direction are within 20 degrees of each other.