AI Technical Summary
Existing light-emitting devices face challenges in achieving high-resolution displays with fast operation speeds and reliable thin film transistors that require different circuit configurations on the same substrate, particularly in forming pixel and drive circuits with varying characteristics.
The invention employs a light-emitting device with a pixel portion and a driver circuit on the same substrate, utilizing a bottom contact type thin film transistor with a compound semiconductor layer for the pixel section and a channel-etched type thin film transistor for the drive circuit, along with specific electrode and electrode layer configurations to enhance electrical characteristics and reliability.
This configuration allows for high-definition, high-brightness displays with reduced manufacturing costs and improved aperture ratios, enabling fast operation and reliable performance by optimizing thin film transistors for their respective functions.
Abstract
Description
[Technical field]
[0001] The present invention relates to a light-emitting device having a layer containing an organic compound as a light-emitting layer, and a method for manufacturing the same. The present invention relates to electronic equipment incorporating a light-emitting display device having light-emitting elements as a component. [Background technology]
[0002] The organic compound used as the light emitter has characteristics such as being thin and lightweight, having high-speed response, and being driven by a low direct current voltage. The light-emitting element is being considered for use in next-generation flat panel displays and lighting. In particular, display devices in which light-emitting elements are arranged in a matrix are more difficult to manufacture than conventional liquid crystal display devices. Compared to LCDs, it is believed to have an advantage in that it has a wider viewing angle and better visibility.
[0003] The mechanism of light emission of a light-emitting element is to sandwich an EL layer between a pair of electrodes and apply a voltage to the cathode. The electrons injected from the anode and the holes injected from the anode recombine at the luminescence centers of the EL layer to form molecules. When an exciton is formed, and the molecular exciton relaxes to the ground state, it releases energy and emits light. There are two types of excited states: singlet and triplet. It is believed that this is possible even after going through a state of
[0004] The EL layer constituting the light-emitting element has at least a light-emitting layer. The layer structure may include a hole injection layer, a hole transport layer, an electron transport layer, an electron injection layer, etc. It is also possible.
[0005] Metal oxides are also attracting attention as materials that exhibit semiconducting properties. Examples of oxides include tungsten oxide, tin oxide, indium oxide, and zinc oxide. There are thin-film transistors in which metal oxides that exhibit such semiconducting properties are used as channel formation regions. The thin film transistor (TFT) is already known (Patent Document 1 and Patent Document 2).
[0006] In addition, the TFT using an oxide semiconductor has a high field effect mobility. It is also possible to configure a driving circuit for a display device or the like using the above. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] JP 2007-123861 A [Patent Document 2] JP 2007-96055 A Summary of the Invention [Problem to be solved by the invention]
[0008] When forming a plurality of different circuits on an insulating surface, for example, a pixel section and a driver circuit are formed on the same substrate. In the case where the thin film transistor used in the pixel portion is formed in the same manner as the pixel portion, the thin film transistor has excellent switching characteristics, e.g. For example, a large on-off ratio is required, and the thin-film transistors used in the drive circuits have high operating speeds. In particular, the higher the resolution of the display device, the faster the display image quality. Since the image writing time is shortened, the thin film transistors used in the driver circuits can operate at high speed and It is preferable to do so.
[0009] Multiple types of circuits are formed on the same substrate, and multiple types of thin films are used to match the characteristics of each type of circuit. An object of the present invention is to provide a light-emitting device including a film transistor.
[0010] According to one embodiment of the present invention, a thin film transistor having favorable electrical characteristics and high reliability is used as a switching element. It is an object of the present invention to manufacture a highly reliable light-emitting device by using the organic EL element as a semiconductor material. [Means for solving the problem]
[0011] One embodiment of the present invention is a light-emitting device having a display portion (also referred to as a pixel portion) and a driver circuit over the same substrate. The pixel thin film transistor has a structure different from that of the driver circuit thin film transistor. The first thin film transistor in the pixel portion is an oxide film overlapping the source electrode layer and the drain electrode layer. Inverted coplanar type (also called bottom contact type) thin film transistor with a nitride semiconductor layer The second transistor in the driver circuit has a source electrode layer over the oxide semiconductor layer. and a drain electrode layer are overlapped at an end of the thin film transistor.
[0012] In addition, the upper surface and side surface of the oxide semiconductor layer of the first thin film transistor and the second thin film transistor Part of a top surface of the oxide semiconductor layer in the transistor is in contact with the oxide insulating film. The source electrode layer and the drain electrode layer of the first thin film transistor are formed using an oxide conductive film. The source electrode layer and the drain electrode layer of the second thin film transistor are formed using a metal conductive film. and a metal conductive film is used to form wiring for the drive circuit.
[0013] In addition, the thin film transistor for the driver circuit is exposed between the source electrode layer and the drain electrode layer. A bottom-gate thin-film transistor having an oxide insulating layer in contact with an oxide semiconductor layer. do.
[0014] The thin film transistor for the driver circuit has a drain electrode layer made of a metal conductive film such as Ti. The drain electrode layer is in contact with a part of a top surface of the oxide semiconductor layer and overlaps with an oxygen vacancy. The high resistance drain region (HRD) is a depleted type. Specifically, the carrier concentration in the high-resistance drain region is 1 ×10 18 / cm 3 The carrier concentration in the channel formation region is within the above range. 1×10 18 / cm 3 In this specification, the carrier concentration is This refers to the carrier concentration value obtained from Hall effect measurements at room temperature.
[0015] The source electrode layer is in contact with a part of a top surface of the oxide semiconductor layer and overlaps with an oxygen-deficient region. The high resistance source region (HRS) is a depleted type. ) region) is formed.
[0016] In addition, a first pixel electrode electrically connected to the first thin film transistor is formed in a plurality of layers in the pixel portion. A light-emitting device such as a display device can be manufactured by forming a light-emitting element on each of the first pixel electrodes. Furthermore, if light-emitting elements with multiple types of luminescent colors are provided in the pixel portion, a full-color display can be achieved. In addition, a plurality of light emitting elements that emit white light can be provided, An optical film, specifically a color filter, is provided so as to overlap the light-emitting region of each light-emitting element. It is also possible to provide a full-color light-emitting display device.
[0017] A color filter is provided between the white light emitting element and the pixel thin film transistor. In the case where light emitted from a light-emitting element is passed through a color filter to display an image, a thin film transistor for a pixel is used. The gate electrode layer, the source electrode layer, and the drain electrode layer of the transistor are made of a light-transmitting material. The use of a conductive film can improve the aperture ratio. Three color filter layers including black matrix and overcoat (red color filter This refers to the entire film that includes a color filter, blue color filter, green color filter, etc. The term does not refer to a single color filter, but rather to a color filter of one color.
[0018] That is, one embodiment of the present invention is a display portion (pixel a second thin film transistor having a structure different from that of the first thin film transistor, The first thin film transistor has a gate electrode on a substrate. a gate insulating layer on the gate electrode layer; a first electrode layer and a second electrode layer on the gate insulating layer; an electrode layer; an oxide semiconductor layer that is on a gate insulating layer and overlaps with the first electrode layer and the second electrode layer; An oxide insulating layer in contact with the oxide semiconductor layer and electrically connected to a second electrode layer on the gate insulating layer. A gate electrode layer of the first thin film transistor and a connection electrode layer of the second thin film transistor are also provided. The insulating layer, the oxide semiconductor layer, the first electrode layer, the second electrode layer, and the oxide insulating layer have a light-transmitting property. The pixel portion is provided with a color filter layer on the oxide insulating layer, and a pixel electrode on the color filter layer. a first pixel electrode electrically connected to the connection electrode layer; and a light-emitting layer and a and a second pixel electrode on the light-emitting layer.
[0019] In addition, one embodiment of the present invention is a thin film transistor having the above structure, The source electrode layer and the drain electrode layer of the first thin film transistor are the gate electrode layer and the first electrode layer and the material of the second electrode layer is different from that of the first electrode layer of the first thin film transistor. The light-emitting device is characterized in that the conductive material has a lower resistance than the electrode layer.
[0020] In addition, in one aspect of the present invention, in the above structure, the connection electrode layer is made of Al, Cr, Cu, Ta, Ti , Mo, W as the main component, or an alloy film of these. The light emitting device is characterized by being composed of a laminated film.
[0021] In addition, one embodiment of the present invention is a thin film transistor having the above structure, The drain electrode layer is made of the same material as the connection electrode layer of the first thin film transistor. It is a light emitting device.
[0022] Further, one embodiment of the present invention is a semiconductor device having the above structure, The second electrode layer is made of indium oxide, an alloy of indium oxide and tin oxide, or an alloy of indium oxide and zinc oxide. The light emitting device is characterized in that the material is a lead alloy or zinc oxide.
[0023] In addition, one embodiment of the present invention is a semiconductor device having the above structure, The transistor includes an oxide semiconductor layer and an oxide insulating layer over the oxide semiconductor layer. The channel forming region of the oxide semiconductor layer is in contact with the oxide insulating layer.
[0024] In addition, one embodiment of the present invention is a semiconductor device having the above-described structure, wherein the first thin film transistor and the second thin film transistor The oxide insulating layer in contact with the channel formation region of the oxide semiconductor layer of the thin film transistor is An inorganic insulating film formed by a sputtering method is used. Representative examples include silicon oxide film, silicon nitride oxide film, and oxide The light emitting device is made of an aluminum film, an aluminum oxynitride film, or the like.
[0025] The above configuration solves at least one of the above problems.
[0026] The oxide semiconductor layer is InMO3(ZnO) m A thin film expressed as (m>0) A thin film transistor is fabricated using the thin film as an oxide semiconductor layer. contains one or more metal elements selected from Ga, Fe, Ni, Mn and Co. For example, M can be Ga, Ga and Ni, or Ga and Fe, etc. In some cases, the above-mentioned metal elements other than Ga are contained. In addition to the metallic elements contained as impurities, there are also Fe, Ni and other transition metal elements, In the present specification, InMO3(Z nO) m Among oxide semiconductor layers having a structure represented by (m>0), a structure containing Ga as M The oxide semiconductor is called the In-Ga-Zn-O oxide semiconductor, and the thin film of the In-Ga- It is also called a Zn-O based non-single crystal film.
[0027] In addition to the above, metal oxides that can be used for the oxide semiconductor layer include In-Sn-O, I n-Sn-Zn-O system, In-Al-Zn-O system, Sn-Ga-Zn-O system, Al-Ga -Zn-O series, Sn-Al-Zn-O series, In-Zn-O series, Sn-Zn-O series, Al- Zn-O, In-O, Sn-O, and Zn-O metal oxides can be used. Further, the oxide semiconductor layer made of the above metal oxide may contain silicon oxide.
[0028] In addition, one embodiment of the present invention for realizing the above structure is to form a first gate electrode on a substrate having an insulating surface. forming a gate electrode layer and a second gate electrode layer; forming a gate insulating layer on the layer; and forming a first electrode layer on the gate insulating layer so as to overlap the first gate electrode layer. A first gate electrode layer and a second electrode layer are formed on the gate insulating layer. a first oxide semiconductor layer overlapping a portion of the first oxide semiconductor layer and a portion of the second electrode layer; and a second gate electrode layer overlapping the first oxide semiconductor layer. A second oxide semiconductor layer is formed, and a source electrode layer and a drain electrode layer are formed on the second oxide semiconductor layer. a connection electrode layer electrically connected to the second electrode layer on the gate insulating layer; The oxide semiconductor layer 1 is formed on a first oxide semiconductor layer 2 and a second oxide semiconductor layer 3. A color filter layer is formed on the oxide insulating layer overlapping the first oxide semiconductor layer. forming a first pixel electrode on the color filter layer, the first pixel electrode being electrically connected to the connection electrode layer; A light-emitting device is fabricated by forming a light-emitting layer on a first pixel electrode and forming a second pixel electrode on the light-emitting layer. This is the manufacturing method.
[0029] In the above-described manufacturing method, The oxide insulating layer is formed by dehydrating or dehydrogenating the oxide semiconductor layer and then exposing it to the air. In this case, the oxide semiconductor layer is formed while preventing water or hydrogen from re-entering the oxide semiconductor layer.
[0030] Dehydration or dehydrogenation is performed using inert gases such as nitrogen or noble gases (argon, helium, etc.). At 400°C or higher and lower than 750°C, preferably 425°C or higher and 700°C or lower, in an atmosphere This heat treatment reduces impurities such as moisture contained in the oxide semiconductor layer.
[0031] Heat treatment is performed under an inert gas atmosphere of nitrogen or rare gas (argon, helium, etc.). In this case, the oxide semiconductor layer becomes oxygen-deficient and has low resistance, that is, becomes N-type ( N - Then, an oxide insulating film is formed in contact with the oxide semiconductor layer. In other words, the oxide semiconductor layer is made high-resistance, i.e., i-type, by making the oxide semiconductor layer oxygen-excessive. This makes it possible to provide a semiconductor device having thin film transistors with good electrical characteristics and high reliability. It is possible to produce and provide
[0032] The oxide semiconductor layer that has been dehydrated or dehydrogenated is Thermal Desorption Spectroscopy (TDS) was performed on the layer. Even when measurements were taken up to 450°C using the ectroscopy method, two peaks of water were observed. The heat treatment conditions are set so that one peak that appears around 300°C is not detected. TDS for thin-film transistors using hydrated or dehydrogenated oxide semiconductor layers Even when measurements were taken up to 450°C, the water peak that appears at around 300°C was not detected. stomach.
[0033] Then, the temperature is lowered from the heating temperature T at which the oxide semiconductor layer is dehydrated or dehydrogenated. When dehydrating or dehydrogenating, the water or hydrogen is removed without exposing it to the air in the same furnace where the dehydration or dehydrogenation was performed. It is important not to re-contaminate the oxide semiconductor layer by dehydration or dehydrogenation. Low resistance, i.e. N-type (N - , N + After that, the oxide semiconductor is made high-resistance and made I-type. When a thin-film transistor is fabricated using a conductor layer, the threshold voltage value of the thin-film transistor can be programmed. A so-called normally-off switching element can be realized. The transistor gate voltage forms a channel at a positive threshold voltage as close as possible to 0V. It is desirable for the display device to have a negative threshold voltage value. When the gate voltage is 0V, current flows between the source and drain electrodes. In an active matrix display device, the circuit The electrical characteristics of the thin film transistor are important and determine the performance of the display device. Of the electrical characteristics of thin film transistors, the threshold voltage (Vth) is particularly important. Even if the effective mobility is high, the threshold voltage is high, or the threshold voltage is negative. It is difficult to control the threshold voltage as a circuit. In the case of a thin-film transistor with a large capacitance, when the driving voltage is low, the transistor functions as a switch. The transistor may not be able to perform its function and may become a load. In the case of a transistor, a channel is formed only when a positive voltage is applied to the gate voltage, and the drain voltage A transistor in which current flows out is desirable. A channel does not form unless the driving voltage is high. Transistors in which a channel is formed and drain current flows even under negative voltage conditions However, such a thin film transistor is not suitable for use in circuits.
[0034] In addition, the gas atmosphere used to lower the temperature from T is different from the gas atmosphere used to raise the temperature to T. A gas atmosphere may be switched to, for example, air in the same furnace where dehydration or dehydrogenation was performed. The inside of the furnace is filled with high-purity oxygen gas or N2O gas, ultra-dry air (dew point Cooling is performed by filling the container with water at a temperature of -40°C or less, preferably -60°C or less.
[0035] The moisture content in the film is reduced by a heat treatment for dehydration or dehydrogenation, and then the film is Cool slowly (or cool) in an atmosphere that is not prone to dew (dew point is -40°C or less, preferably -60°C or less). The oxide semiconductor film is used to improve the electrical characteristics of thin film transistors and to facilitate mass production. This will realize thin-film transistors that are both reliable and high performance.
[0036] In this specification, the method is carried out under an inert gas atmosphere of nitrogen or a rare gas (argon, helium, etc.). This heat treatment is called a heat treatment for dehydration or dehydrogenation. Dehydrogenation does not only mean that hydrogen is released as H2 by the hydrogenation process, but also means that H For convenience, this process is referred to as dehydration or dehydrogenation, which also includes the elimination of OH and other groups.
[0037] In a light-emitting display device using a light-emitting element, a pixel portion has a plurality of thin film transistors. In the elemental portion, the gate electrode of a thin film transistor and the source wiring of another transistor, The light emitting device has a portion for connecting a drain wiring. In the driving circuit, the gate electrode of the thin film transistor and the source The semiconductor device has a portion for connecting a wiring or a drain wiring.
[0038] In addition, since thin-film transistors are easily damaged by static electricity, etc., For the line, a protection circuit for protecting the thin film transistor in the pixel area can be provided on the same substrate. The protection circuit is preferably formed using a nonlinear element using an oxide semiconductor layer. It is nice.
[0039] The ordinal numbers such as 1st and 2nd are used for convenience and do not indicate the order of steps or stacking. In addition, the specific names used in this specification are not intended to identify the invention. This does not indicate the
[0040] The semiconductor device according to one embodiment of the present invention includes a driver circuit having a TFT for a driver circuit on the same substrate. A display section having a path section and a pixel TFT is manufactured. can be reduced.
[0041] In addition, a white light emitting element can be formed on the substrate to manufacture a light emitting device such as a lighting device. The lighting device is particularly an electroluminescent device. The present invention relates to a lighting device using a light-emitting element having a layer containing a light-emitting material that can obtain an EL (electroluminescence) light-emitting diode. It is a bright device. Effect of the Invention
[0042] A gate electrode layer, a gate insulating layer, and an oxide semiconductor layer of a first thin film transistor in a pixel portion The first electrode layer, the second electrode layer, the oxide insulating layer, and the first electrode have a light-transmitting property, and the aperture ratio and In both cases, the channel width can be kept large. As a result, even in high resolution, the light-emitting element Therefore, it is possible to provide a light emitting device with high luminance.
[0043] A gate electrode layer including a gate electrode of a second thin film transistor included in the driver circuit, and The source electrode layer including the source electrode and the drain electrode layer including the drain electrode have electrical resistance As a result, the wiring resistance of the display device according to one embodiment of the present invention is suppressed. This allows the delay time to be shortened, and the writing time for the displayed image to be shortened. can be provided.
[0044] In this way, multiple types of circuits are formed on the same substrate, and the characteristics of each type of circuit are adjusted accordingly. A light emitting device including a plurality of types of thin film transistors can be provided.
[0045] According to one embodiment of the present invention, a thin film transistor having favorable electrical characteristics and high reliability is used as a switching element. By using the above-mentioned light emitting device as a light emitting diode, a highly reliable light emitting device can be provided.
[0046] By using an oxide semiconductor layer that has been subjected to heat treatment for dehydration or dehydrogenation, Thin-film transistors with excellent electrical characteristics and high reliability are used as switching elements, It is also possible to fabricate a high-performance light-emitting device by forming a TFT for pixels and a TFT for driving circuits on the same substrate. Light-emitting devices can be fabricated by combining FT and each circuit in a different structure. . [Brief description of the drawings]
[0047] [Figure 1] 1A to 1C are cross-sectional process views illustrating one embodiment of the present invention. [Diagram 2] FIG. 2 is a diagram showing an example of a pixel configuration. [Diagram 3] FIG. 1 is a cross-sectional view illustrating one embodiment of the present invention. [Figure 4] FIG. 1 is a cross-sectional view illustrating one embodiment of the present invention. [Diagram 5] 1A and 1B are a cross-sectional view and a plan view illustrating one embodiment of the present invention. [Figure 6] FIG. 1 is a cross-sectional view illustrating one embodiment of the present invention. [Figure 7] 1A and 1B are a cross-sectional view and a plan view illustrating one embodiment of the present invention. [Figure 8] FIG. 1 is a block diagram illustrating an active matrix display device. [Figure 9] 1A and 1B are a diagram illustrating a configuration of a signal line driver circuit and a timing chart illustrating the operation of the signal line driver circuit. [Figure 10] FIG. 1 is a circuit diagram showing a configuration of a shift register. [Figure 11]1A and 1B are a diagram illustrating a configuration of a shift register and a timing chart illustrating the operation of the shift register; [Figure 12] FIG. [Figure 13] FIG. [Figure 14] FIG. [Figure 15] FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0048] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. The present invention is not limited to the following description, and those skilled in the art will recognize that the present invention may be modified in various ways in form and detail. The present invention is not limited to the description of the following embodiments. In the drawings in this specification, parts having the same parts or similar functions are The same reference numerals will be used to denote the same parts, and their explanations may be omitted.
[0049] (Embodiment 1) In this embodiment mode, a light-emitting device and a manufacturing method thereof will be described with reference to FIGS. Figure 1(E) shows the cross-sectional structure of two thin-film transistors with different structures fabricated on the same substrate. An example is shown below.
[0050] The thin film transistor 450 shown in FIG. 1E is one of the bottom gate structures. The Transistor 460 is a bottom-gate transistor called a bottom-contact type (also called an inverted coplanar type). It is one of the structures.
[0051] The thin film transistor 460 disposed in the pixel is a bottom contact type thin film transistor. A gate electrode layer 111a, a gate insulating layer 402, a gate insulating film 403, and a gate insulating film 404 are formed on a substrate 400 having an insulating surface. The oxide semiconductor layer 123 including the channel formation region, the first electrode layer 115a, and the second electrode layer In addition, the insulating film 115b covers the thin film transistor 460 and the upper surface of the oxide semiconductor layer 123 and the An oxide insulating layer 407 is provided in contact with the side surfaces of the first and second electrodes.
[0052] In addition, the thin film transistor 460 disposed in the pixel is a thin film transistor having a single gate structure. However, if necessary, a multi-gate structure having a plurality of channel forming regions may be used. A thin film transistor having the above structure can also be formed.
[0053] Note that the oxide semiconductor layer 123 is formed on the first electrode layer 115a and the second electrode layer 115b. The first electrode layer 115a and the second electrode layer 115b are formed in the same direction. The oxide semiconductor layer 123 overlaps the gate electrode layer 111a with the gate insulating layer 402 interposed therebetween. The channel formation region of the thin film transistor 460 arranged in the pixel is formed of an oxide semiconductor layer. 123, the side surface of the first electrode layer 115a and the second electrode layer 115 b, that is, the region that is in contact with the gate insulating layer 402 and is sandwiched between the side surface of the gate electrode layer 111 This is the area that overlaps with a.
[0054] In addition, the thin film transistor 460 is a light-transmitting thin film transistor having a high aperture ratio. In order to realize a light-emitting device having such a structure, the first electrode layer 115a and the second electrode layer 115b are made of a light-transmitting material. A conductive film having a high conductivity is used.
[0055] The gate electrode layer 111a of the thin film transistor 460 also transmits visible light. In this specification, a film that is transparent to visible light is a film that is transparent to visible light. If the film has electrical conductivity, it is also called a transparent conductive film. Also, a conductive film that is semi-transparent to visible light may be used. This refers to a visual light transmittance of 50-75%.
[0056] The thin film transistor 450 disposed in the driver circuit is formed on the substrate 400 having an insulating surface. The gate electrode layer 211a, the gate insulating layer 402, the oxide semiconductor layer, and the source electrode layer 215a The oxide semiconductor layer includes at least a channel forming region 223, high-resistance source region 213a, and high-resistance drain region 213b. The oxide semiconductor layer includes an oxide insulating layer 407 in contact with the channel formation region 223. In addition, a protective insulating layer 408 is provided over the oxide insulating layer 407, forming a stacked structure. This is also fine.
[0057] In FIG. 1E, an oxide insulating layer 407 and a gate insulating layer 404 are formed on the gate electrode layer. A region of the oxide semiconductor layer sandwiched between the first and second electrodes is referred to as a channel formation region. The channel length L of the thin film transistor 450 is The length is a length sandwiched between ends of a pair of the source electrode layer 215a and the drain electrode layer 215b.
[0058] In the following, Figs. 1(A), 1(B), 1(C), 1(D), and 1(E) will be used to The process of manufacturing the thin film transistor 450 and the thin film transistor 460 on a substrate will be described. .
[0059] First, a conductive film is formed on a substrate 400 having an insulating surface, and then a first photolithography process is performed. Through the process, gate electrode layers 211a and 211c are formed.
[0060] The resist mask may be formed by an ink-jet method. When the film is formed by the jet method, a photomask is not used, and therefore the manufacturing cost can be reduced.
[0061] The conductive film forming the gate electrode layers 211a and 211c may be Al, Cr, Ta, Ti, An element selected from Mo, W, or an alloy containing the above elements, or a combination of the above elements. Examples of such films include alloy films in which a metal oxide is combined with another metal oxide.
[0062] In addition, for glass substrates, if the temperature of the subsequent heat treatment is high, the distortion point is 730°C or higher. For the glass substrate, for example, aluminosilicate glass, alumina Glass materials such as lumino borosilicate glass and barium borosilicate glass are used. In addition, by containing more barium oxide (BaO) than boric acid, it is more practical. Heat-resistant glass can be obtained. For this reason, it is recommended to use a glass substrate containing more BaO than B2O3. is preferred.
[0063] Instead of the above glass substrate, an insulating substrate such as a ceramic substrate, a quartz substrate, or a sapphire substrate may be used. A substrate made of an insulating material may be used. Alternatively, crystallized glass or the like may be used.
[0064] In addition, an insulating film serving as a base film is provided between the substrate 400 and the gate electrode layers 211a and 211c. The undercoat film has a function of preventing diffusion of impurity elements from the substrate 400. A silicon oxide film, a silicon nitride oxide film, or a silicon oxynitride film is used. The insulating film can be formed by a laminate structure.
[0065] Next, a light-transmitting conductive film is formed to cover the gate electrode layers 211a and 211c, and then The gate electrode layers 111a and 111c are formed by a second photolithography process. In the embodiment, in order to reduce the wiring resistance, the gate wiring arranged in the pixel portion is formed on the gate electrode layer. The gate insulating layer 40 is formed from the same metal conductive film as the gate insulating layer 211c. The gate electrode layer 111a overlapping with the gate electrode 111a via the gate electrode 111b is formed using a light-transmitting conductive film.
[0066] Next, a gate insulating layer 402 is formed on the gate electrode layers 211a, 211c, 111a, and 111c. Form.
[0067] The gate insulating layer 402 is a silicon oxide layer formed by using a plasma CVD method, a sputtering method, or the like. A silicon nitride layer, a silicon oxynitride layer, or a silicon nitride oxide layer may be formed as a single layer or a stacked layer. The film may be doped with phosphorus (P) or boron (B).
[0068] For example, the deposition gas is SiH4, oxygen, and nitrogen, and the deposition gas is oxidized by plasma CVD. A silicon nitride layer may be formed. The thickness of the gate insulating layer 402 is 100 nm to 500 nm. In the case of a stacked layer, for example, the first gate insulating film has a thickness of 50 nm to 200 nm. and a second gate insulating layer having a thickness of 5 nm to 300 nm on the first gate insulating layer. The layer is called a layer.
[0069] In this embodiment, silicon oxynitride (SiON (composition ratio N <O)) A film is formed as the gate insulating layer 402 with a thickness of 100 nm.
[0070] Next, a light-transmitting conductive film is formed over the gate insulating layer 402, and then a third photolithography A first electrode layer 115a and a second electrode layer 115b are formed by a lithography process (FIG. The light-transmitting conductive film is made of a conductive material that transmits visible light, For example, In-Sn-O, In-Sn-Zn-O, In-Al-Zn-O, Sn-G a-Zn-O, Al-Ga-Zn-O, Sn-Al-Zn-O, In-Zn-O , Sn-Zn-O, Al-Zn-O, In-O, Sn-O, Zn-O metal oxides The thickness of the film can be appropriately selected within the range of 50 nm to 300 nm. In addition, when using a sputtering method, a target containing SiO2 in an amount of 2% by weight or more and 10% by weight or less is used. The transparent conductive film is coated with SiOx (X>0) which inhibits crystallization. This causes crystallization during the heat treatment for dehydration or dehydrogenation in the subsequent process. It is preferable to suppress the above.
[0071] Next, the gate insulating layer 402 is selectively etched by a fourth photolithography process. A contact hole reaching the gate electrode layer 211c is then formed.
[0072] Next, a film having a thickness of 5 nm to 200 nm, preferably 10 nm, is formed on the gate insulating layer 402. An oxide semiconductor film having a thickness of 20 nm or less is formed. After the oxide semiconductor film is formed, dehydration or Since the oxide semiconductor film is made amorphous even after heat treatment for dehydrogenation, the thickness It is preferable to make the oxide semiconductor film thin, ie, 50 nm or less. When a heat treatment is performed after the formation of the semiconductor layer, crystallization can be suppressed.
[0073] The oxide semiconductor film is an In-Ga-Zn-O non-single crystal film, an In-Sn-Zn-O film, or an In -Al-Zn-O system, Sn-Ga-Zn-O system, Al-Ga-Zn-O system, Sn-Al- Zn-O series, In-Zn-O series, Sn-Zn-O series, Al-Zn-O series, In-O series, S The oxide semiconductor film is made of a rare gas (typically Zn-O or Zn-O). In an atmosphere of noble gas (typically argon), in an atmosphere of oxygen, or in an atmosphere of noble gas (typically argon) and oxygen The film can be formed by sputtering in a sintered atmosphere. In this case, a target containing SiO2 in an amount of 2% by weight or more and 10% by weight or less is used for deposition, and the oxide The semiconductor film contains SiOx (X>0), which inhibits crystallization, and is dehydrated or It is preferable to suppress crystallization during the heat treatment for dehydrogenation.
[0074] Here, an oxide semiconductor target containing In, Ga, and Zn (composition ratio: In2 O3:Ga2O3:ZnO=1:1:1[mol%], In:Ga:Zn=1:1:0. 5[at.%]), the distance between the substrate and the target was 100 mm, and the pressure was 0.6P a) The film is formed in an oxygen atmosphere (oxygen flow rate ratio 100%) with a direct current (DC) power supply of 0.5 kW. In addition, if a pulsed direct current (DC) power supply is used, dust can be reduced and the film thickness distribution becomes uniform. In this embodiment, the oxide semiconductor film is preferably an In—Ga—Zn—O-based oxide. A 15 nm thick In-Ga-Zn-O system non-monocrystalline substrate was fabricated by sputtering using a semiconductor target. A crystalline film is formed.
[0075] There are two types of sputtering: RF sputtering, which uses a high-frequency power source for the sputtering power supply, and DC sputtering. There is also the pulsed DC sputtering method, which applies a pulsed bias. The DC sputtering method is mainly used to deposit insulating films, while the DC sputtering method is mainly used to deposit metal conductive films. It is used in such cases.
[0076] There are also multi-target sputtering devices that can accommodate multiple targets of different materials. The equipment can deposit layers of different materials in the same chamber, or multiple types of films in the same chamber. It is also possible to form a film by discharging two or more materials at the same time.
[0077] Also, a sputtering apparatus using a magnetron sputtering method equipped with a magnet mechanism inside the chamber and ECR sputtering using plasma generated by microwaves without glow discharge. There is a sputtering apparatus that uses this method.
[0078] In addition, in a film formation method using a sputtering method, a target material and a sputtering gas component are mixed during film formation. Reactive sputtering is a method of forming thin films of compounds by chemically reacting them with each other, and There is also a bias sputtering method in which a voltage is also applied to the substrate.
[0079] Note that before the oxide semiconductor film is formed by a sputtering method, argon gas is introduced to the plasma Reverse sputtering is performed to generate ions, and dust adhering to the surface of the gate insulating layer 402 is removed. In the reverse sputtering, an electric current is applied to the substrate side using an RF power source in an argon atmosphere. This method modifies the surface by applying pressure to generate plasma near the substrate. Instead of the atmosphere, nitrogen, helium, oxygen, etc. may be used.
[0080] In this embodiment, the gate insulating layer is selectively etched by the fourth photolithography process. A contact hole reaching the gate electrode layer 211c is formed by etching, but this is not particularly limited. After etching the oxide semiconductor film, a resist mask is formed over the oxide semiconductor layer. A contact hole reaching the base electrode layer 211c may be formed. In that case, The oxide semiconductor layer and the gate insulating layer 402 are removed by etching. It is preferable to remove the above.
[0081] In addition, after an oxide semiconductor film is formed over the gate insulating layer, a resist mask is formed on the oxide semiconductor film. A contact hole reaching the gate electrode layer 211c is formed, and then a resist mask is formed. Then, a resist mask is formed again on the oxide semiconductor film. A step of processing a film into an island-shaped oxide semiconductor layer by selectively etching the film may be performed.
[0082] In addition, before the formation of the oxide semiconductor film, an inert gas atmosphere (nitrogen, helium, neon, Heat treatment (400°C or higher but below the distortion point of the substrate) under argon gas or other gases is then performed. Impurities such as hydrogen and water contained in the gate insulating layer may be removed.
[0083] In this embodiment, the gate insulating layer is selectively etched by the fourth photolithography process. In order to form a contact hole reaching the gate electrode layer 211c by etching, After the formation of the hole, the mixture is heated under an inert gas atmosphere (nitrogen, helium, neon, argon, etc.). The layer is heated (400°C or higher but less than 750°C) to remove the hydrogen and water contained in the layer. After impurities such as these are removed, an oxide semiconductor film is formed.
[0084] Next, the oxide semiconductor film is formed into an island-shaped oxide semiconductor layer by a fifth photolithography process. Note that the etching conditions for the oxide semiconductor film are If the selection ratio between the first electrode layer 115a and the second electrode layer 115b is not sufficient, The first electrode layer 115a and the second electrode layer 115b that are not covered by the mask are then formed into an oxide semiconductor. It may be removed partially or completely together with the membrane. If it is completely removed, it is removed as shown in FIG. 1(B). As shown in the figure, the top surface of the conductive layer including the first electrode layer 115a and the second electrode layer 115b is made of an acid. An oxide semiconductor layer is formed, and the end of the conductive layer coincides with the end of the oxide semiconductor layer. In addition, when a portion of the oxide semiconductor layer is removed, the island-shaped oxide semiconductor layer is more likely to be removed than the region overlapping with the island-shaped oxide semiconductor layer. The first electrode layer 115a and the second electrode layer 115b are formed in a region extending outward from the edge of the semiconductor layer 113. The thickness of 115b is reduced.
[0085] In addition, a resist mask for forming an island-shaped oxide semiconductor layer is formed by an ink-jet method. If the resist mask is formed by the inkjet method, no photomask is required. This reduces manufacturing costs.
[0086] Next, the oxide semiconductor layer is dehydrated or dehydrogenated. The temperature of the heat treatment in step 1 is 400° C. or higher and lower than 750° C., preferably 425° C. or higher. If the temperature is 425°C or higher, the heat treatment time may be 1 hour or less. In this case, the heat treatment time is set to be longer than one hour. The substrate is placed in an electric furnace, and the oxide semiconductor layer is subjected to heat treatment in a nitrogen atmosphere. After this, the oxide semiconductor layer is prevented from being exposed to the air, and water and hydrogen are prevented from re-mixing into the oxide semiconductor layer. In this embodiment, a process for dehydrating or dehydrogenating an oxide semiconductor layer is performed. From the heating temperature T, use the same furnace until it reaches a temperature that is high enough to prevent water from entering again. The temperature is gradually cooled in a nitrogen atmosphere until it drops by 100°C below the temperature T. Dehydration or dehydrogenation can be performed under a rare gas atmosphere such as helium, neon, or argon. conduct.
[0087] The heat treatment device is not limited to an electric furnace, and may be a heat treatment device using heat conduction or heat from a heating element such as a resistance heating element. A device that heats the object to be treated by radiation may be used. For example, a GRTA (Gas Rapid Thermal Anneal) equipment, LRTA (Lamp Rapid RTA (Rapid Thermal Anneal) equipment etc. The LRTA device can be equipped with halogen lamps, metal halide lamps, etc. Lamps, xenon arc lamps, carbon arc lamps, high pressure sodium lamps, high pressure water A device that heats the workpiece by radiating light (electromagnetic waves) emitted from a lamp such as a silver lamp. The GRTA device heats the workpiece by thermal conduction from a heated gas. The gas can be a rare gas such as argon or nitrogen, which is used to heat the material to be treated. An inert gas that does not react with is used.
[0088] In the first heat treatment, nitrogen or a rare gas such as helium, neon, or argon is used. It is preferable that the nitrogen introduced into the heat treatment device does not contain water, hydrogen, etc. Or the purity of rare gases such as helium, neon, and argon must be 6N (99.9999%) or higher. Preferably, the concentration of impurities is 7N (99.99999%) or more (i.e., the impurity concentration is 1 ppm or less, It is preferable to keep the concentration of the ion exchange resin at 0.1 ppm or less.
[0089] Depending on the conditions of the first heat treatment or the material of the oxide semiconductor layer, the oxide semiconductor layer may be crystallized and microcrystalline. For example, the crystallinity may be 90% or more, or 80% or more. In addition, depending on the conditions of the first heat treatment or the amount of the acid, the oxide semiconductor film may become a microcrystalline oxide semiconductor film. Depending on the material of the oxide semiconductor layer, it may become an amorphous oxide semiconductor film that does not contain crystalline components. There are also.
[0090] After the first heat treatment, the oxide semiconductor layer 213, 1 After the first heat treatment, the oxide semiconductor film is The carrier concentration is increased to 1×10 18 / cm 3 having a carrier concentration of The oxide semiconductor layers 213 and 113 are formed. Depending on the material of the layers 111a and 111c, the gate electrode layer 111a and the gate electrode layer 11 In some cases, the gate electrode layer 11c is crystallized to become a microcrystalline film or a polycrystalline film. When an indium oxide tin oxide alloy film is used as 1a or 111c, the film is heated at 450° C. for 1 hour. The gate electrode layers 111a and 111c are crystallized by a first heat treatment. When an indium tin oxide alloy film is used, crystallization does not occur.
[0091] In addition, the first heat treatment of the oxide semiconductor layer is performed on the oxide semiconductor layer before it is processed into the island-shaped oxide semiconductor layer. In this case, the substrate is removed from the heating device after the first heat treatment. It is then taken out and subjected to a fifth photolithography step.
[0092] Next, the gate electrode layer 211c, the gate insulating layer 402, and the first After forming a conductive film over the electrode layer 115a, the second electrode layer 115b, and the oxide semiconductor layer, A resist mask is formed by a sixth photolithography process, and selective etching is performed. Then, a source electrode layer 215a and a drain electrode layer 215b are formed (see FIG. 1C). As shown in FIG. 1C, a connection electrode electrically connected to the gate electrode layer 211c is provided. The electrode layer 215c is electrically connected to the second electrode layer 115b via the oxygen-deficient oxide semiconductor layer. A connection electrode layer 215d for connection is also formed. The conductive film is formed by a sputtering method or a vacuum deposition method. (Electron beam deposition method, etc.), arc discharge ion plating method, spray method, etc. The conductive film is made of an element selected from Ti, Mo, W, Al, Cr, Cu, Ta, or Alternatively, an alloy containing the above elements or a combination of the above elements may be used. The conductive film is not limited to a single layer containing the above-mentioned elements, but may be a laminate of two or more layers. In this embodiment, a titanium film (thickness 100 nm) and an aluminum film (thickness 200 nm) are A three-layer conductive film is formed with a titanium film (thickness 100 nm). A titanium dioxide film may also be used.
[0093] In the sixth photolithography step, only the conductive film in contact with the oxide semiconductor layer is Therefore, only the conductive film in contact with the oxide semiconductor layer is selectively removed. In order to remove the fluorine, an alkaline etchant was used, which was ammonia hydrogen peroxide (composition: weight ratio: 31% hydrogen peroxide: 28% ammonia: water = 5:2:2) The metal conductive film is selectively removed to leave an oxide semiconductor made of an In-Ga-Zn-O oxide semiconductor. The layer can be left.
[0094] In addition, depending on the etching conditions, the oxide semiconductor layer The exposed areas of (113, 213) may be etched. In that case, the source electrode layer The oxide semiconductor layer in the region sandwiched between the source electrode layer 215a and the drain electrode layer 215b is The oxide semiconductor layer in the region overlapping with the drain electrode layer 215b or the oxide semiconductor layer in the region overlapping with the drain electrode layer 215b The thickness of the film is thinner than that of the solid semiconductor layer.
[0095] The source electrode layer 215a, the drain electrode layer 215b, the connection electrode layers (215c, 215 The resist mask for forming d) may be formed by an inkjet method. When the inkjet method is used to form the mask, no photomask is required, reducing manufacturing costs. can.
[0096] Next, a thin film is formed on the gate insulating layer 402 and the oxide semiconductor layer (213, 113) by a sputtering method. An oxide insulating layer 407 is formed by depositing an oxide insulating film using a method such as the steps of: The oxide insulating layer 407 is formed in a region that overlaps with the gate electrode layer. The region of the oxide semiconductor layer sandwiched between the oxide insulating layer 407 and the gate insulating layer 402 is the channel region. This is the region where the holes are formed.
[0097] The oxide insulating film is at least 1 nm thick and is formed by an oxide insulating method such as a sputtering method. The film can be formed by using an appropriate method that does not allow impurities such as water and hydrogen to be mixed into the film. In the embodiment, a silicon oxide film is formed as the oxide insulating film by a sputtering method. The substrate temperature during the process may be set to room temperature or higher and 300° C. or lower. In this embodiment, the substrate temperature is set to 100° C. The deposition of silicon oxide films by sputtering is carried out under a rare gas (typically argon) atmosphere. The reaction can be carried out in an oxygen atmosphere or in an atmosphere of rare gas (typically argon) and oxygen. In addition, a silicon oxide target or a silicon target is used as the target. For example, a silicon target can be used for sputtering in an oxygen and rare gas atmosphere. A silicon oxide film can be formed by a ring method. The oxide insulating film formed by this process is resistant to moisture, hydrogen ions, and OH - It does not contain impurities such as The inorganic insulating film used is a material that blocks the intrusion of these elements from the outside. A silicon oxide film, an aluminum oxide film, an aluminum oxynitride film, or the like is used. However, the oxide insulating film formed by the sputtering method is particularly dense, and impurities tend to diffuse into the adjacent layer. It can be used as a single layer as a protective film to suppress the phenomenon. Using a target doped with boron (B), phosphorus (P) or boron (B) is added to the oxide insulating film. It is also possible.
[0098] In this embodiment, a columnar polycrystalline B-doped silicon target (resistivity 0 The distance between the substrate and the target (TS distance) was 89 mm, and the pressure was 1.01 Ωcm. Pulse was measured under an oxygen atmosphere (oxygen flow rate 100%) with a pressure of 0.4 Pa and a direct current (DC) power of 6 kW. The film is formed by DC sputtering. The film thickness is 300 nm.
[0099] Next, a second heat treatment (preferably a second heat treatment) is performed under an inert gas atmosphere or a nitrogen gas atmosphere. The heating is performed at a temperature of 00° C. or higher and 400° C. or lower, for example, 250° C. or higher and 350° C. or lower (see FIG. 1(D)). For example, the second heat treatment is performed at 250° C. for 1 hour in a nitrogen atmosphere. When the above-mentioned process is performed, part of the oxide semiconductor layer 213 is heated in a state of being in contact with the oxide insulating layer 407. Note that when the second heat treatment is performed, the oxide semiconductor layer whose resistance is reduced by the first heat treatment is converted into an oxide semiconductor layer. In this case, the oxide semiconductor becomes an oxide-excessive state, resulting in high resistance (I-type). When the body layer is 15 nm or less, the source electrode layer 215a and the drain electrode In the oxide semiconductor layer overlapping the layer 215b, oxygen is easily transferred to the metal conductive film side. In addition, when the oxide semiconductor layer is 30 nm to 50 nm, The area near the interface with the metal conductive film becomes N-type, but the area below becomes I-type or N-type. - A stylized state and The oxide insulating layer 407 is in contact with a region that is to be a channel formation region of the oxide semiconductor layer. It functions as a channel protection layer.
[0100] The second heat treatment is performed immediately after the sixth photolithography process. There is no particular limitation as long as it is a process subsequent to the sixth photolithography process.
[0101] Next, a protective insulating layer 408 is formed over the oxide insulating layer 407 (see FIG. 1E). The protective insulating layer 408 may be a silicon nitride film, a silicon nitride oxide film, an aluminum nitride film, or the like. In this embodiment, the protective insulating layer 408 of a silicon nitride film is formed by RF sputtering. Form.
[0102] After the protective insulating layer 408 is formed, a resist mask is formed by a seventh photolithography process. A contact hole is formed by selectively etching the contact hole so as to reach the connection electrode layer 215d. The formation of the pores is also performed.
[0103] Through the above process, two types of thin-film transistors, a channel-etch type thin-film transistor, and a A bottom-contact type thin film transistor 460 can be fabricated. do.
[0104] A gate electrode including a gate electrode of a channel-etched thin film transistor 450 in the driving circuit An electrode layer, a source electrode layer including a source electrode, and a drain electrode layer including a drain electrode. uses metal with low electrical resistance for wiring. This reduces the wiring resistance of the light-emitting device. It is possible to provide a light-emitting device that can be driven in a short writing time. The transistor 460 is made of a light-transmitting material except for the connection electrode layer 215d. Therefore, the channel width can be increased while maintaining a high aperture ratio. Even if the luminance is low, a large current can be supplied to the light emitting element, and a light emitting device with high luminance can be provided.
[0105] In addition, in a light-emitting device, thin film transistors having a plurality of configurations may be arranged in one pixel. For example, the driving TFT electrically connected to the light emitting element is configured to obtain a large on-current. It is preferable that the switching TFT be electrically connected to the gate electrode layer of the driving TFT. Therefore, a bottom transistor having the same structure as the thin film transistor 460 is used. By using a contact-type TFT as the driving TFT for the pixel section, the aperture ratio is kept high while By increasing the channel width, a large on-current can be obtained. A channel-etched TFT with the same structure as the 450 is used as the switching TFT for the pixel area. Since the switching TFT does not require a large current, it can be used It can be made smaller than the conventional liquid crystal display, and the aperture ratio is less likely to decrease.
[0106] In addition, when manufacturing a light-emitting device, a power supply that is electrically connected to the source electrode layer of the driving TFT is A power supply line is provided, the power supply line intersecting the gate wiring and a connection line made of a metal conductive film. The power supply line is formed of the same material and in the same process as the polar layer 215c. The gate electrode layer 211c is formed of the same material and in the same process as the gate electrode layer 211c.
[0107] In addition, when a light emitting device is manufactured, one electrode of the light emitting element is the drain electrode layer of the driving TFT. and a common potential line electrically connected to the other electrode of the light emitting element. The common potential line is made of the same material and in the same process as the connection electrode layer 215c made of a metal conductive film. Alternatively, the common potential line is formed in the same process using the same material as the gate electrode layer 211c. Complete.
[0108] In addition, when a light-emitting device is manufactured, one pixel has a plurality of thin film transistors. A connection portion is provided to connect the gate electrode layer of the film transistor to the other drain electrode layer. This connection portion is the same as the connection electrode layer 215c electrically connected to the gate electrode layer 211c. It is formed in the same process.
[0109] In this embodiment mode, a driver circuit and a pixel portion are formed, and the driver circuit and the pixel portion or the driver in the pixel portion are Considering the characteristics suitable for the driving TFT and the selection TFT, a channel-etched thin-film transistor 45 0 or bottom-contact thin-film transistor 460 for optimization. It is possible to plan this.
[0110] This embodiment mode can be freely combined with other embodiment modes.
[0111] (Embodiment 2) In this embodiment, a plurality of thin film transistors shown in Embodiment 1 and an electroluminescent An active matrix type light emitting display device is manufactured by using a light emitting element that utilizes a light emitting diode. Here is an example.
[0112] Light-emitting elements that utilize electroluminescence are characterized by the fact that the light-emitting material is either an organic compound or an inorganic compound. Generally, the former are organic EL elements and the latter are inorganic EL elements. It is called.
[0113] In an organic EL element, electrons and holes are released from a pair of electrodes by applying a voltage to the light-emitting element. are injected into layers containing light-emitting organic compounds, causing a current to flow. The rears (electrons and holes) recombine to form an excited state in the light-emitting organic compound. When the excited state returns to the ground state, light is emitted. Such a light-emitting element is called a current-excitation type light-emitting element.
[0114] Inorganic EL elements are divided into dispersion-type inorganic EL elements and thin-film-type inorganic EL elements according to their element structure. Dispersion-type inorganic EL elements have a light-emitting layer in which particles of a light-emitting material are dispersed in a binder. The emission mechanism is a donor-acceptor reaction that utilizes the donor and acceptor levels. Thin-film inorganic EL elements are made by sandwiching a light-emitting layer between dielectric layers. The structure is sandwiched between electrodes, and the light emission mechanism utilizes the inner shell electron transition of metal ions. In this example, the light-emitting element is an organic EL element. do.
[0115] FIG. 2 shows an example of a pixel configuration to which digital time gray scale driving can be applied as an example of a semiconductor device. FIG.
[0116] The configuration of a pixel to which digital time gray scale driving can be applied and the operation of the pixel will be described. The figure shows an n-channel transistor that uses an oxide semiconductor layer as a channel formation region in one pixel. Here is an example of using two of them.
[0117] The pixel 6400 includes a switching transistor 6401, a driving transistor 6402, The light emitting element 6404 and the capacitor element 6403 are included. 01 has a gate connected to a scanning line 6406 and a first electrode (one of the source and drain electrodes) The first electrode (the other of the source electrode and the drain electrode) is connected to a signal line 6405, and the second electrode (the other of the source electrode and the drain electrode) is connected to a drive The driving transistor 6402 is connected to the gate of the driving transistor 6402. The gate is connected to a power supply line 6407 via a capacitor element 6403, and the first electrode is connected to a power supply line 640 7, and the second electrode is connected to the first electrode (pixel electrode) of the light emitting element 6404. The second electrode of the light emitting element 6404 corresponds to a common electrode 6408. It is electrically connected to a common potential line formed on the substrate.
[0118] A low power supply potential is set to the second electrode (common electrode 6408) of the light emitting element 6404. Note that the low power supply potential is a low power supply potential with respect to the high power supply potential set to the power supply line 6407. Potential < High power supply potential. For example, GND, 0V, etc. are set as low power supply potential. The potential difference between the high power supply potential and the low power supply potential is applied to the light emitting element 6404. In order to make the light emitting element 6404 emit light by passing a current through the light emitting element 6404, a high power supply potential and the low power supply potential is set to be equal to or higher than the forward threshold voltage of the light emitting element 6404. Each potential is set.
[0119] The capacitor 6403 is omitted by substituting the gate capacitance of the driving transistor 6402. It is also possible to set the gate capacitance of the driving transistor 6402 as follows: A capacitance may be formed between the gate electrode and the second electrode.
[0120] In the case of a voltage input voltage driving method, the gate of the driving transistor 6402 is The driving transistor 6402 is in two states, either fully on or fully off. A video signal is inputted, that is, the driving transistor 6402 is operated in a linear region. In order to operate the driving transistor 6402 in a linear region, the voltage of the power supply line 6407 must be higher than that of the driving transistor 6402. A high voltage is applied to the gate of the driving transistor 6402. A voltage equal to or higher than (power supply line voltage + Vth of the driving transistor 6402) is applied.
[0121] In addition, when analog gray scale driving is performed instead of digital time gray scale driving, the input of the signal is different. By doing so, the same pixel configuration as in FIG. 2 can be used.
[0122] In the case of performing analog gradation driving, a light emitting element 6404 is connected to the gate of a driving transistor 6402. A voltage equal to or higher than the forward voltage of the light emitting element 6401 and the Vth of the driving transistor 6402 is applied. The forward voltage in 04 refers to the voltage required to achieve the desired brightness, and should be at least 100% forward voltage. In addition, the video transistor 6402 is designed to operate in the saturation region. By inputting an optical signal, a current can be passed through the light emitting element 6404. In order to operate the transistor 6402 in the saturation region, the potential of the power supply line 6407 is The gate potential of the light emitting element 6402 is set higher than that of the gate of the transistor 6403. Analog gradation drive can be performed by passing a current corresponding to a video signal through 6404.
[0123] Note that the pixel configuration shown in FIG. 2 is not limited to this. For example, if a new switch is added to the pixel shown in FIG. A switch, a resistive element, a capacitive element, a transistor, a logic circuit, or the like may be added.
[0124] Next, the configuration of the light-emitting element will be described with reference to FIG. 3. Here, the driving TFT is an n-channel The cross-sectional structure of a pixel will be described using a channel type as an example. ), and TFTs 7001 and 7002 which are driving TFTs used in the semiconductor device of FIG. The thin film transistors 11 and 7021 can be manufactured in the same manner as in the embodiment 1, and are oxide semiconductors. The thin film transistor is highly reliable and includes a dielectric layer.
[0125] The light emitting element only needs to have at least one of the anode and cathode transparent in order to extract light. Then, a thin film transistor and a light emitting element are formed on the substrate, and light is taken from the surface opposite to the substrate. The structure has a top emission structure that emits light from the top surface of the substrate, a bottom emission structure that emits light from the bottom surface of the substrate, and a structure that emits light from the bottom surface of the substrate and the bottom surface of the substrate. There are also light-emitting elements with a double-sided emission structure that emit light from the opposite side of the pixel. The present invention can also be applied to a light emitting device having a structure.
[0126] A light emitting element having a bottom emission structure will be described with reference to FIG.
[0127] In FIG. 3A, a driving TFT 7011 is an n-channel type, and light emitted from a light-emitting element 7012 FIG. 3A is a cross-sectional view of a pixel in the case where light emitted from the pixel is emitted to the first electrode 7013 side. A light-transmitting layer electrically connected to the driving TFT 7011 via a connection electrode layer 7030 A first electrode 7013 of the light-emitting element 7012 is formed over the conductive film 7017. An EL layer 7014 and a second electrode 7015 are laminated in this order on the electrode 7013. The connecting electrode layer 7030 is electrically connected to the drain electrode layer of the driving TFT 7011 .
[0128] The light-transmitting conductive film 7017 can be formed of indium oxide containing tungsten oxide, oxide Indium zinc oxide with tungsten oxide, indium oxide with titanium oxide, Indium tin oxide containing titanium, indium tin oxide, indium zinc oxide, oxide carbide A light-transmitting conductive film such as indium tin oxide to which indium is added can be used.
[0129] In addition, various materials can be used for the first electrode 7013 of the light-emitting element. When the electrode 7013 is used as a cathode, a material having a small work function, specifically, For example, alkali metals such as Li and Cs, and alkaline earth metals such as Mg, Ca, and Sr, and alloys containing these (Mg:Ag, Al:Li, etc.), as well as rare earth metals such as Yb and Er. In FIG. 3A, the film thickness of the first electrode 7013 is set to a thickness that allows light to pass therethrough (preferably For example, an aluminum film having a thickness of 20 nm is , is used as the first electrode 7013 .
[0130] After a light-transmitting conductive film and an aluminum film are laminated, the film is selectively etched. In this case, the light-transmitting conductive film 7017 and the first electrode 7013 may be formed. This is preferable because the same mask can be used for etching.
[0131] The periphery of the first electrode 7013 is covered with a partition wall 7019. The partition wall 7019 is made of polyimide. Organic resin films such as acrylic, polyamide, and epoxy, inorganic insulating films, and organic polysiloxanes. The partition wall 7019 is formed by using a photosensitive resin material. 13, and an opening is formed on the surface of the substrate 13, and the side wall of the opening is an inclined surface having a continuous curvature. In the case where a photosensitive resin material is used as the partition wall 7019, In this case, the step of forming a resist mask can be omitted.
[0132] The EL layer 7014 formed on the first electrode 7013 and the partition wall 7019 is at least It is sufficient to include a light-emitting layer, and the light-emitting device may be composed of a single layer or may be composed of multiple layers stacked together. When the EL layer 7014 is composed of a plurality of layers, An electron injection layer, an electron transport layer, a light emitting layer, a hole transport layer, a hole transport layer, and a hole transport layer are formed on a first electrode 7013 that functions as a light emitting layer. It is not necessary to provide all of these layers.
[0133] In addition, the stacking order is not limited to the above, and the first electrode 7013 may function as an anode. A hole injection layer, a hole transport layer, a light emitting layer, an electron transport layer, and an electron injection layer are laminated on top of 7013 in this order. However, when comparing power consumption, the first electrode 7013 may function as a cathode. On the first electrode 7013, an electron injection layer, an electron transport layer, a light emitting layer, a hole transport layer, a hole injection layer, and a By stacking the layers in the order of insertion, it is possible to suppress the voltage rise in the drive circuit section and reduce power consumption. Therefore, it is preferable.
[0134] In addition, the second electrode 7015 formed on the EL layer 7014 can be made of various materials. For example, when the second electrode 7015 is used as an anode, a material with a large work function can be used. Materials such as ZrN, Ti, W, Ni, Pt, Cr, ITO, IZO, ZnO, etc. A transparent conductive material is preferable. In addition, a shielding film 7016, for example, a film for blocking light, is provided on the second electrode 7015. A light-shielding metal, a light-reflecting metal, or the like is used. In this embodiment mode, the second electrode 7015 and An ITO film is used as the shielding film 7016, and a Ti film is used as the shielding film 7017.
[0135] An EL layer 7014 including a light-emitting layer is sandwiched between a first electrode 7013 and a second electrode 7015. In the case of the element structure shown in FIG. Light emitted from 012 is emitted to the first electrode 7013 side as shown by the arrow.
[0136] Note that FIG. 3A shows an example in which a light-transmitting conductive film is used as a gate electrode layer. The light emitted from the light emitting element 7012 passes through the color filter layer 7033 and is The light is emitted through the gate electrode layer and source electrode layer of the FT7011. A conductive film having light-transmitting properties is used as the gate electrode layer and the source electrode layer of 1 to improve the aperture ratio. It is possible.
[0137] The color filter layer 7033 is formed by a droplet discharge method such as an inkjet method, a printing method, a photolithography method, or the like. Each is formed by an etching method using graphic technology.
[0138] The color filter layer 7033 is covered with an overcoat layer 7034, which is a protective insulating layer. In FIG. 3A, the overcoat layer 7034 is thin. As shown in the figure, the overcoat layer 7034 covers the unevenness caused by the color filter layer 7033. It has a flattening function.
[0139] In addition, a protective insulating layer 7035, an overcoat layer 7034, a color filter layer 7033, and A contact hole is formed in the oxide insulating layer 7031 and reaches the connection electrode layer 7030. The connection electrode layer 7030 is disposed at a position overlapping with the partition wall 7019. In FIG. Since this is an example using a metal conductive film, a contact hole reaching the connection electrode layer 7030 and a partition wall The aperture ratio is improved by overlapping the connection electrode layer 7019 and the connection electrode layer 7030. It is possible.
[0140] Next, a light emitting element having a dual emission structure will be described with reference to FIG.
[0141] In FIG. 3B, the driving TFT 7021 is electrically connected to the connection electrode layer 7040. A first electrode 7023 of a light-emitting element 7022 is formed over the light-transmitting conductive film 7027. An EL layer 7024 and a second electrode 7025 are laminated in this order on a first electrode 7023. The connection electrode layer 7040 is electrically connected to the drain electrode layer of the driving TFT 7021. Connected.
[0142] The light-transmitting conductive film 7027 can be formed using indium oxide containing tungsten oxide, Indium zinc oxide with tungsten oxide, indium oxide with titanium oxide, Indium tin oxide containing titanium, indium tin oxide, indium zinc oxide, oxide carbide A light-transmitting conductive film such as indium tin oxide to which indium is added can be used.
[0143] In addition, various materials can be used for the first electrode 7023. For example, When using 23 as a cathode, a material with a small work function, specifically, for example, Li or Cs Alkaline metals such as Mg, Ca, Sr, and alkaline earth metals including these In addition to alloys (Mg:Ag, Al:Li, etc.), rare earth metals such as Yb and Er are preferred. In the embodiment, the first electrode 7023 is used as a cathode, and its film thickness is set to a level that allows light to pass through. (Preferably, about 5 nm to 30 nm). For example, an aluminum film having a thickness of 20 nm is A ZnO film is used as the cathode.
[0144] After a light-transmitting conductive film and an aluminum film are laminated, the film is selectively etched. In this case, the light-transmitting conductive film 7027 and the first electrode 7023 may be formed by the same method. It is preferable that the same mask be used for etching.
[0145] The periphery of the first electrode 7023 is covered with a partition wall 7029. The partition wall 7029 is made of polyimide. Organic resin films such as acrylic, polyamide, and epoxy, inorganic insulating films, and organic polysiloxanes. The partition wall 7029 is formed by using a photosensitive resin material. 23, and an opening is formed on the surface of the substrate 23, and the side wall of the opening is an inclined surface having a continuous curvature. In the case where a photosensitive resin material is used as the partition wall 7029, In this case, the step of forming a resist mask can be omitted.
[0146] In addition, the EL layer 7024 formed over the first electrode 7023 and the partition wall 7029 includes a light-emitting layer. It is sufficient if the material is made up of a single layer or multiple layers are laminated. Either is acceptable. When the EL layer 7024 is composed of multiple layers, it functions as a cathode. On the first electrode 7023, an electron injection layer, an electron transport layer, a light emitting layer, a hole transport layer, a hole injection layer It is not necessary to provide all of these layers.
[0147] In addition, the stacking order is not limited to the above. The first electrode 7023 may be used as an anode, and a hole may be formed on the anode. The injection layer, the hole transport layer, the light emitting layer, the electron transport layer, and the electron injection layer may be laminated in this order. When comparing power consumption, the first electrode 7023 is used as a cathode, and an electron injection layer 7024 is provided on the cathode. In this case, power consumption is reduced by stacking the electron transport layer, light emitting layer, hole transport layer, and hole injection layer in this order. This is preferable because
[0148] In addition, the second electrode 7025 formed on the EL layer 7024 can be made of various materials. For example, when the second electrode 7025 is used as an anode, a material with a large work function can be used. A transparent conductive material such as ITO, IZO, or ZnO can be preferably used. In this embodiment, the second electrode 7025 is used as an anode, and an ITO film containing silicon oxide is used as the anode. Form.
[0149] An EL layer 7024 including a light-emitting layer is sandwiched between a first electrode 7023 and a second electrode 7025. In the case of the element structure shown in FIG. 3B, the light-emitting element 7022 corresponds to the light-emitting element 7022. The light emitted from the first electrode 7022 is incident on the second electrode 7025 side and the first electrode 702 as shown by the arrows. It fires on both sides.
[0150] In FIG. 3B, a light-transmitting conductive film is used as the gate electrode layer and the source electrode layer. In this example, the light emitted from the light emitting element 7022 to the first electrode 7023 is The light passes through the filter layer 7043 and the gate electrode layer and source electrode layer of the driving TFT 7021. The gate electrode layer and source electrode layer of the driving TFT7021 are made of transparent material. By using a conductive film having the above structure, the aperture ratio of the second electrode 7025 side and the aperture ratio of the first electrode 7023 side can be reduced. The aperture ratio can be made almost the same.
[0151] The color filter layer 7043 is formed by a droplet discharge method such as an inkjet method, a printing method, a photolithography method, or the like. Each is formed by an etching method using graphic technology.
[0152] The color filter layer 7043 is covered with an overcoat layer 7044, which is a protective insulating layer. Covered by layer 7045 .
[0153] In addition, a protective insulating layer 7045, an overcoat layer 7044, a color filter layer 7043, and A contact hole is formed in the oxide insulating layer 7041 and reaches the connection electrode layer 7040. The connection electrode layer 7040 is disposed at a position overlapping with the partition wall 7029. In FIG. Since this is an example using a metal conductive film, a contact hole reaching the connection electrode layer 7040 and a partition wall The second electrode 7025 is formed by overlapping the connection electrode layer 7040 with the second electrode 7029. The aperture ratio on the side of the first electrode 7023 can be made substantially the same as the aperture ratio on the side of the first electrode 7023.
[0154] However, when using a light-emitting element with a dual-side emission structure and making both display surfaces full color display, Since the light from the second electrode 7025 side does not pass through the color filter layer 7043, a separate color filter is used. It is preferable that a sealing substrate having a -filter layer is provided above the second electrode 7025.
[0155] Next, a light emitting element having a top emission structure will be described with reference to FIG.
[0156] In FIG. 3C, a driving TFT 7001 is an n-channel type, and a light-emitting element 7002 FIG. 3 shows a cross-sectional view of a pixel in the case where light emitted from the first electrode 7001 exits to the second electrode 7005 side. In C), a light-emitting element 7001 is electrically connected to a TFT 7001 via a connection electrode layer 7050. A first electrode 7003 of the semiconductor device 002 is formed, and an EL layer 7004 is formed on the first electrode 7003. , and a second electrode 7005 are laminated in this order.
[0157] In addition, various materials can be used for the first electrode 7003. For example, When using 03 as a cathode, a material with a small work function, specifically, for example, Li or Cs Alkaline metals such as Mg, Ca, Sr, and alkaline earth metals including these In addition to alloys (Mg:Ag, Al:Li, etc.), rare earth metals such as Yb and Er are preferable.
[0158] The periphery of the first electrode 7003 is covered with a partition wall 7009. The partition wall 7009 is made of polyimide. Organic resin films such as acrylic, polyamide, and epoxy, inorganic insulating films, and organic polysiloxanes. The partition wall 7009 is formed by using a photosensitive resin material. 03, an opening is formed on the surface, and the side wall of the opening is an inclined surface formed with a continuous curvature. In the case where a photosensitive resin material is used as the partition wall 7009, In this case, the step of forming a resist mask can be omitted.
[0159] The EL layer 7004 formed on the first electrode 7003 and the partition wall 7009 is at least It is sufficient to include a light-emitting layer, and the light-emitting device may be composed of a single layer or may be composed of multiple layers stacked together. When the EL layer 7004 is composed of a plurality of layers, An electron injection layer, an electron transport layer, a light emitting layer, a hole transport layer, a hole transport layer, and a hole transport layer are formed on the first electrode 7003 used for the purpose. It is not necessary to provide all of these layers.
[0160] The stacking order is not limited to the above, and the hole injection layer 7002 may be formed on the first electrode 7003 used as an anode. Alternatively, the layer may be laminated in the following order: a hole transport layer, a light emitting layer, an electron transport layer, and an electron injection layer.
[0161] In Figure 3(C), holes are injected onto a laminated film consisting of a Ti film, an aluminum film, and a Ti film. A hole transport layer, a light emitting layer, an electron transport layer, and an electron injection layer are laminated in that order, and then a Mg:Ag A laminate of an alloy thin film and ITO is formed.
[0162] However, when the TFT 7001 is an n-channel type, an electron injection layer and an electrode The order of lamination of the electron transport layer, light emitting layer, hole transport layer, and hole injection layer is advantageous in terms of the efficiency of the driving circuit. This is preferable because it can suppress the voltage rise caused by the voltage rise and reduce power consumption.
[0163] The second electrode 7005 is formed using a light-transmitting conductive material, for example, tungsten oxide. Indium oxide containing tungsten oxide, indium zinc oxide containing tungsten oxide, titanium oxide indium oxide containing titanium oxide, indium tin oxide containing titanium oxide, Translucent materials such as indium zinc oxide and indium tin oxide doped with silicon oxide A conductive film may also be used.
[0164] An EL layer 7004 including a light-emitting layer is sandwiched between a first electrode 7003 and a second electrode 7005. The region corresponds to the light-emitting element 7002. In the case of the pixel shown in FIG. Light emitted from the second electrode 7002 exits toward the second electrode 7005 as indicated by the arrow.
[0165] In FIG. 3C, a TFT 7001 is an example in which a thin film transistor 460 is used. However, there is no particular limitation, and a thin film transistor 450 can be used. When the thin film transistor 450 is used as the first electrode 7003, the drain electrode layer and electrically connect them so that they are in contact with each other.
[0166] In FIG. 3C, the drain electrode layer of the TFT 7001 is connected to the connection electrode layer 7050. The connection electrode layer 7050 is electrically connected to the planarization insulating layer 7053, the protective insulating layer 7055, and The first electrode 7003 and the second electrode 7004 are electrically connected through a contact hole formed in the oxide insulating layer 7051. The planarization insulating layer 7053 is made of polyimide, acrylic, benzocyclobutene, Resin materials such as polyamide and epoxy can be used. Low dielectric constant materials (low-k materials), siloxane resins, PSG (phosphorus glass), BPSG (phosphorus boron glass) and the like can be used. Note that insulating films formed from these materials can be used. The planarization insulating layer 7053 may be formed by stacking a plurality of the planarization insulating layers 705. The method for forming the layer 3 is not particularly limited, and may be a sputtering method, a SOG method, a spin coating method, or the like, depending on the material. Dipping, spray coating, droplet ejection method (inkjet method, screen printing, offset printing Printing, etc.), doctor knife, roll coater, curtain coater, knife coater, etc. can be used.
[0167] In the structure of FIG. 3C, when a full-color display is performed, for example, the light-emitting element 700 2 is a green light-emitting element, one of the adjacent light-emitting elements is a red light-emitting element, and the other The optical element is a blue light-emitting element. In addition to the three types of light-emitting elements, a white light-emitting element is also added. A light-emitting display device capable of full-color display using four types of light-emitting elements may be manufactured.
[0168] In the structure of FIG. 3C, all the light emitting elements are white light emitting elements. A sealing substrate having a color filter or the like is disposed above the light emitting element 7002. A light-emitting display device capable of displaying multiple colors may be manufactured. By forming a color filter and combining it with a color conversion layer, a full color display can be achieved. This can be done.
[0169] Of course, a single-color display may be used. For example, a lighting device may be formed using white light. Alternatively, monochromatic light may be used to form an area color type light emitting device.
[0170] If necessary, an optical film such as a polarizing film, eg, a circular polarizing plate, may be provided.
[0171] Although the organic EL element has been described as the light-emitting element here, inorganic EL elements can also be used as the light-emitting element. It is also possible to provide an L element.
[0172] In addition, the thin film transistor (driving TFT) that controls the driving of the light-emitting element and the light-emitting element are electrically However, a current control TFT is connected between the driving TFT and the light emitting element. The configuration may be such that the input / output terminals are connected to each other.
[0173] This embodiment mode can be freely combined with other embodiment modes.
[0174] (Embodiment 3) In this embodiment mode, a plurality of thin film transistors shown in Embodiment Mode 1 are used to form a single semiconductor device on the same substrate. An example of forming a pixel portion and a driver circuit in an active matrix type light emitting display device is shown below. show.
[0175] In the first embodiment, two thin film transistors and a cross section of a connection portion are illustrated. In the embodiment, a wiring intersection and a capacitance portion are also illustrated and described.
[0176] FIG. 4 is a cross-sectional view showing the state of the substrate before an EL layer is formed on a first electrode (pixel electrode). In addition, the same reference numerals are used for the same parts as in FIG.
[0177] In FIG. 4, the driving TFT electrically connected to the first electrode 414 is a bottom contact type. The thin film transistor 460 is manufactured according to the method of the first embodiment. This can be done.
[0178] After forming the oxide insulating layer 407 according to the first embodiment, a green color filter layer 411 A blue color filter layer and a red color filter layer are formed in this order. The oxide insulating film formed in is particularly dense and suppresses the phenomenon of impurities diffusing into adjacent layers. A single layer can be used as a protective film. Also, each color filter layer can be printed. method, inkjet method, and etching method using photolithography technology, respectively. A color filter layer is provided on the substrate on which the TFT is formed, forming a sealing substrate. The color filter layer and the light-emitting area of the light-emitting element can be precisely aligned without relying on the accuracy of lamination. You can easily align the position.
[0179] Next, a green color filter layer 411, a blue color filter layer, and a red color filter layer are An overcoat layer 412 is formed to cover the filter layer. The overcoat layer 412 has a light-transmitting property. A resin having such properties is used.
[0180] Here, an example of full color display using three colors of RGB is shown, but there is no particular limitation. A full color display may be performed using the four colors of BW.
[0181] Next, a protective insulating layer 408 is formed to cover the overcoat layer 412 and the oxide insulating layer 407. The protective insulating layer 408 is made of an inorganic insulating film, such as a silicon nitride film, an aluminum nitride film, or a nitride film. A silicon oxide film, an aluminum oxynitride film, or the like is used.
[0182] Next, the protective insulating layer 408 and the oxide insulating layer 407 are selected by a photolithography process. A contact hole reaching the connection electrode layer 215d is formed by selectively etching the The protective insulating layer 408 and the oxide insulating layer 407 of the terminal portion are selected by the photolithography process. A portion of the terminal electrode is exposed by selective etching. In order to connect the two electrodes to a common potential line, a contact hole reaching the common potential line is also formed. .
[0183] Next, a conductive film having light transmitting properties is formed, and a connection electrode layer 21 is formed by a photolithography process. A first electrode 414 is formed to be electrically connected to 5d.
[0184] Next, a partition wall 459 is formed so as to cover the periphery of the first electrode 414. organic resin films such as polyimide, acrylic, polyamide, and epoxy; inorganic insulating films or organic poly The partition wall 459 is formed by using a photosensitive resin material. 14, and an opening is formed on the surface of the substrate 14, and the side wall of the opening is an inclined surface having a continuous curvature. When a photosensitive resin material is used for the partition wall 459, a resist mask is formed. The step of forming the insulating film can be omitted.
[0185] Through the above steps, the substrate state shown in FIG. 4 can be obtained. The following steps are the same as those in the second embodiment. As shown in FIG. 1, an EL layer is formed on the first electrode 414, and a second electrode is formed on the EL layer. The second electrode is electrically connected to a common potential line.
[0186] In addition, a capacitance section is formed in the pixel section as shown in FIG. The gate insulating layer 402 is used as a dielectric, and the capacitor wiring layer 111b and the capacitor electrode layer 115c are formed. In the light emitting device, the capacitance wiring layer 111b is a part of the gate electrode layer of the pixel TFT. and the capacitive electrode layer 115c is a part of the power supply line.
[0187] In addition, in FIG. 4, an example in which the gate wiring layer 211b is a metal conductive film is shown. Alternatively, the gate electrode layer 111a of the gate electrode 460 may be formed using a conductive film having a light-transmitting property. In addition, the wiring layer 215e is formed of the same conductive layer as the connection electrode layers (215c, 215d). It intersects with the gate wiring layer 211b via a gate insulating film.
[0188] In addition, in FIG. 4, at least one TFT arranged in the driving circuit is a channel etch type. The thin film transistor 450 is manufactured according to the method of the first embodiment. This can be done.
[0189] In addition, a conductive layer 216 is provided above the oxide semiconductor layer of the thin film transistor 450 of the driver circuit. The conductive layer 216 may be formed of the same material and in the same process as the first electrode 414. do.
[0190] The conductive layer 216 is provided so as to overlap with the channel formation region 223 of the oxide semiconductor layer. The bias-thermal stress test (BT) is used to check the reliability of thin-film transistors. In the test, the threshold voltage of the thin film transistor 450 before and after the BT test was In addition, the conductive layer 216 has a potential different from that of the gate electrode layer 211a. It may be the same or different and may function as a second gate electrode layer. The potential of the conductive layer 216 may be GND, 0 V, or may be in a floating state. In addition, the thin film transistor 450 provided with the conductive layer 216 is a four-terminal transistor. It works.
[0191] In addition, thin film transistors are easily damaged by static electricity, etc. The protection circuit is preferably provided over the same substrate as the semiconductor device. It is preferable to use a nonlinear element. For example, the protection circuit is In this embodiment, a plurality of protection circuits are provided between the terminal and the signal line input terminal. A surge voltage is applied to the scanning lines, signal lines and capacitance bus lines due to static electricity or the like, and the pixel transistors are The protection circuit is designed to prevent the transistors from being destroyed. When a voltage is applied, the protection circuit is configured to release the electric charge to the common wiring. It is composed of nonlinear elements arranged in parallel with a scanning line between them. It is composed of a two-terminal element such as a diode or a three-terminal element such as a transistor. For example, It is possible to form the thin film transistor 460 in the pixel portion in the same process. By connecting the inlet and drain terminals together, it can have the same characteristics as a diode. Cut.
[0192] This embodiment mode can be freely combined with embodiment mode 1 or 2.
[0193] (Embodiment 4) In this embodiment, one of the configurations of the terminal portion provided on the same substrate as the thin film transistor is An example is shown in Fig. 5. In Fig. 5, the same parts as in Fig. 4 are described using the same reference numerals.
[0194] FIG. 5(A1) and FIG. 5(A2) are a cross-sectional view and a top view, respectively, of a gate line terminal portion. FIG. 5(A1) corresponds to a cross-sectional view taken along line C1-C2 in FIG. 5(A2). In (A1), a conductive layer is formed on a stack of an oxide insulating layer 407 and a protective insulating layer 408. 415 is a terminal electrode for connection that functions as an input terminal. In the terminal portion, a first terminal 417 formed of the same material as the gate wiring layer 211b and a A connection electrode layer 215f is formed of the same material as the source wiring layer including the source electrode layer 215a. The gate insulating layer 402 is interposed between the gate insulating layer 402 and the conductive layer 415 is used for electrical connection. The second electrode 5 can be formed in the same process using the same light-transmitting material as the first electrode 414. Cut.
[0195] FIG. 5(B1) and FIG. 5(B2) are a cross-sectional view and a top view of a source wiring terminal portion, respectively. FIG. 5(B1) is a cross-sectional view taken along line C3-C4 in FIG. 5(B2). In FIG. 5B1, a stack of the oxide insulating layer 407 and the protective insulating layer 408 is The conductive layer 418 is a terminal electrode for connection that functions as an input terminal. 5(B1), in the terminal portion, an electrode layer formed of the same material as the gate wiring layer 211b 416 is a gate insulating layer 4 below the second terminal 215g that is electrically connected to the source line. The electrode layer 416 is not electrically connected to the second terminal 215g. The electrode layer 416 is set to a potential different from that of the second terminal 215g, for example, floating, GND, or 0V. By setting the value to 0, it is possible to form a capacitance for noise countermeasures or a capacitance for static electricity countermeasures. The second terminal 215g can be formed by insulating the oxide insulating layer 407 and the protective insulating layer 408. Through the contact hole, the conductive layer 418 is electrically connected. The conductive layer 418 is formed in the same process as the first electrode 414 using a material having the same light-transmitting properties. It is possible.
[0196] A plurality of gate lines, source lines, common potential lines, and power supply lines are provided according to the pixel density. In addition, in the terminal section, a first terminal having the same potential as the gate wiring, a source wiring a second terminal at the same potential as the line; a third terminal at the same potential as the power supply line; and a fourth terminal at the same potential as the common potential line. The number of each terminal can be set to any number. This is acceptable, and the implementer can make the appropriate decision.
[0197] This embodiment can be freely combined with embodiment 1, embodiment 2, or embodiment 3. It is possible.
[0198] (Embodiment 5) In this embodiment mode, the light-emitting element used in FIGS. 3(A) and 3(C) shown in Embodiment 2 is An example of the element structure will be described.
[0199] The element structure shown in FIG. 6A includes a pair of electrodes (a first electrode 1001 and a second electrode 1002). The EL layer 1003 including the light-emitting region is sandwiched between the first and second electrodes. In the description, the first electrode 1001 is used as an anode, and the second electrode 100 2 shall be used as the cathode.
[0200] The EL layer 1003 is sufficient as long as it includes at least a light-emitting layer. The functional layer other than the light-emitting layer may be a layer structure including a functional layer having a high hole injection property. materials with high hole transport properties, materials with high electron transport properties, materials with high electron injection properties, A layer containing a material having a high electron and hole transporting property can be used. Specifically, functional layers such as a hole injection layer, a hole transport layer, an electron transport layer, and an electron injection layer are appropriately combined. It can be used in combination.
[0201] The light-emitting element shown in FIG. 6A has a first electrode 1001 and a second electrode 1002. The potential difference causes a current to flow, and holes and electrons recombine in the EL layer 1003, emitting light. In other words, the EL layer 1003 is configured to form a light-emitting region.
[0202] Light is emitted through either the first electrode 1001 or the second electrode 1002, or both. Therefore, the electric current is taken out to the outside through either the first electrode 1001 or the second electrode 1002. Either or both of the first and second electrodes are made of a material having optical transparency.
[0203] As shown in FIG. 6B, the EL layer is formed between the first electrode 1001 and the second electrode 1002. In the case of a laminated structure of n layers (n is a natural number of 2 or more), (m is a natural number, 1≦m≦n-1)th EL layer and (m+1)th EL layer It is preferable to provide a charge generating layer 1004 between the two layers.
[0204] The charge generating layer 1004 may be a composite material of an organic compound and a metal oxide, a metal oxide, an organic compound, Alkali metals, alkaline earth metals, or composite materials with these compounds, as well as Examples of composite materials of organic compounds and metal oxides include Examples include organic compounds and metal oxides such as V2O5, MoO3, and WO3. The following compounds are considered to be suitable for use: aromatic amine compounds, carbazole derivatives, aromatic hydrocarbons, polymer compounds (oligosaccharides, etc.) Various compounds such as carboxymers, dendrimers, polymers, etc. can be used. As an organic compound, a hole-transporting organic compound with a hole mobility of 10 -6 cm 2 / Vs or later However, it is preferable that the material has a higher hole transporting property than the electron transporting property. If necessary, materials other than these may be used. The material has excellent carrier injection and carrier transport properties, and is therefore suitable for low-current driving of light-emitting devices and It is possible to realize low-voltage driving.
[0205] The charge generating layer 1004 is made of a composite material of an organic compound and a metal oxide, and other materials. For example, a layer including a composite material of an organic compound and a metal oxide and a layer including an electron transport layer may be formed. A compound selected from among the electroconductive materials and a layer containing a compound having high electron transport properties are combined. Alternatively, a layer containing a composite material of an organic compound and a metal oxide and a transparent conductive film may be combined. may be formed in combination.
[0206] A light-emitting element having such a configuration is less susceptible to problems such as energy transfer and quenching. By expanding the range of materials to be selected, it will be possible to develop light-emitting devices that have both high luminous efficiency and a long lifespan. It is also easy to obtain phosphorescence in one EL layer and fluorescence in the other. .
[0207] The charge generating layer 1004 is a layer that generates a charge when a voltage is applied between the first electrode 1001 and the second electrode 1002. When the charge generating layer 1004 is turned on, holes are generated in the EL layer 1003 formed in contact with the charge generating layer 1004. The EL layer 1002 has a function of injecting electrons into the other EL layer 1003 .
[0208] The light-emitting element shown in FIG. 6B can be used in various ways by changing the type of light-emitting material used in the light-emitting layer. In addition, it is possible to obtain a variety of luminescent colors by using multiple luminescent materials with different luminescent colors. This makes it possible to obtain light emission with a broad spectrum or white light emission.
[0209] When white light is obtained using the light-emitting element shown in FIG. 6B, a combination of a plurality of light-emitting layers is used. The light source may be configured to emit white light containing red, blue, and green light. For example, The first EL layer contains fluorescent materials as emissive materials, and the second EL layer contains green and red phosphorescent materials as emissive materials. In addition, a first EL layer that emits red light and a second EL layer that contains The device has a second EL layer that emits green light and a third EL layer that emits blue light. Alternatively, a white light may be produced by using a configuration having light-emitting layers that emit light of complementary colors. In a stacked element in which two EL layers are stacked, light is emitted from the first EL layer. When the color of the light emitted from the first EL layer and the color of the light emitted from the second EL layer are in a complementary color relationship, Examples of the relationship include blue and yellow, or blue-green and red.
[0210] In the above-mentioned laminated element configuration, a charge generating layer is disposed between the laminated EL layers. This makes it possible to realize a long-life element in the high-luminance region while keeping the current density low. In addition, the voltage drop due to the resistance of the electrode material can be reduced, allowing for uniform light emission over a large area. This becomes possible.
[0211] This embodiment mode can be combined with any one of the first to fourth embodiments.
[0212] (Embodiment 6) In this embodiment mode, the appearance and cross section of a light-emitting display panel (also called a light-emitting panel) will be described with reference to FIG. FIG. 7(A) shows a thin film transistor and a light emitting device formed on a first substrate. FIG. 7 is a plan view of a panel in which an optical element is sealed between a second substrate and the panel by a sealant. (B) corresponds to a cross-sectional view taken along line HI in FIG. 7(A).
[0213] A pixel portion 4502, a signal line driver circuit 4503a, and a signal line driver circuit 4504 are provided on a first substrate 4501. A sealant 4505 is formed to surround the gate driver circuits 4504a and 4504b. In addition, a pixel portion 4502, signal line driver circuits 4503a and 4503b, and A second substrate 4506 is provided on the scanning line driver circuits 4504a and 4504b. The pixel portion 4502, the signal line driver circuits 4503a and 4503b, and the scanning line driver circuit 45 4504a and 4504b are a first substrate 4501, a sealant 4505, and a second substrate 4506. The filling material 4507 is sealed with the sealing material 4507. Highly sealed protective film with little outgassing (lamination film, UV curable resin film) It is preferable to package (enclose) the package in a material such as a film or a cover material.
[0214] A pixel portion 4502, a signal line driver circuit 4503a, and a fourth 503b and the scanning line driver circuits 4504a and 4504b each have a plurality of thin film transistors. In FIG. 7B, a thin film transistor 4510 included in a pixel portion 4502 and a signal A thin film transistor 4509 included in the line driver circuit 4503a is illustrated.
[0215] The thin film transistors 4509 and 4510 are the signal transistors including the oxide semiconductor layer described in Embodiment 1. Thin film transistors with high reliability can be used. Thin film transistors for driving circuits 4 As the transistor 509, the thin film transistor 450 shown in the embodiment mode 1, the thin film transistor for a pixel A thin film transistor 460 can be used as the transistor 4510. In this embodiment, the thin film transistors 4509 and 4510 are n-channel thin film transistors.
[0216] The oxide semiconductor layer of the thin film transistor 4509 for the driver circuit is formed over the insulating layer 4544. A conductive layer 4540 is provided in a position overlapping with the channel forming region. By providing the MOSFET in a position overlapping the channel formation region of the semiconductor layer, It is possible to reduce the amount of change in the threshold voltage of the thin film transistor 4509. The potential of the gate electrode layer 4540 may be the same as that of the gate electrode layer of the thin film transistor 4509 or may be different. The conductive layer 4 may be formed of a conductive material and may function as a second gate electrode layer. The potential of 540 may be GND, 0V, or may be in a floating state.
[0217] The thin film transistor 4510 is electrically connected to the first pixel electrode 4517 through a connection electrode layer 4548. In addition, the oxide semiconductor layer of the thin film transistor 4510 is electrically connected to the oxide An insulating layer 4542 is formed.
[0218] The oxide insulating layer 4542 was formed using a material and a method similar to those of the oxide insulating layer 407 described in Embodiment 1. An insulating layer 4544 is formed to cover the oxide insulating layer 4542. The insulating layer 4544 is formed using a material and a method similar to those of the protective insulating layer 408 described in the first embodiment. That's good.
[0219] A color filter layer 4545 is formed on the thin film transistor 4511 so as to overlap the light emitting region of the light emitting element 4511. It is formed on the star 4510.
[0220] In addition, it functions as a planarizing insulating film to reduce the surface unevenness of the color filter layer 4545. It is covered with an overcoat layer 4543 .
[0221] In addition, an insulating layer 4544 is formed on the overcoat layer 4543. The protective insulating layer 408 may be formed using a material and a method similar to those of the protective insulating layer 408 described in Embodiment 1.
[0222] In addition, 4511 corresponds to a light-emitting element, and a first pixel electrode which is a pixel electrode of the light-emitting element 4511 is a pixel electrode. The electrode 4517 is electrically connected to the source electrode layer or the drain electrode layer of the thin film transistor 4510. The light emitting element 4511 is configured with a first pixel electrode 4517, an electric field generating The optical layer 4512 and the second pixel electrode 4513 are laminated together, but are not limited to the illustrated configuration. The configuration of the light emitting element 4511 is appropriately determined according to the direction of the light to be extracted from the light emitting element 4511. It can be changed as needed.
[0223] The partition 4520 is formed using an organic resin film, an inorganic insulating film, or an organic polysiloxane. In particular, a photosensitive material is used to form an opening on the first pixel electrode 4517, and the side of the opening It is preferable that the wall is formed to have an inclined surface having a continuous curvature.
[0224] The electroluminescent layer 4512 may be composed of a single layer or a plurality of layers may be laminated. It doesn't matter whether it is done or not.
[0225] In order to prevent oxygen, hydrogen, moisture, carbon dioxide, etc. from entering the light emitting element 4511, the second pixel electrode A protective film may be formed on the electrode 4513 and the partition wall 4520. The protective film may be a silicon nitride film. A silicon oxynitride film, a DLC film, or the like can be formed.
[0226] In addition, signal line driver circuits 4503a and 4503b, scanning line driver circuits 4504a and 4504b Various signals and potentials applied to the pixel portion 4502 are It is supplied by b.
[0227] The connection terminal electrode 4515 has the same conductive property as the first pixel electrode 4517 of the light-emitting element 4511. The terminal electrode 4516 is formed from a source electrode layer and a drain electrode layer of the thin film transistor 4509. It is formed from the same conductive film as the rain electrode layer.
[0228] The connection terminal electrode 4515 is connected to the terminal of the FPC 4518a via the anisotropic conductive film 4519. The electrodes are electrically connected to each other.
[0229] The substrate located in the direction in which light is extracted from the light emitting element 4511 has transparency to visible light. In that case, glass plates, plastic plates, polyester films, etc. A light-transmitting material such as film or acrylic film is used.
[0230] In addition, filler 4507 can be inert gas such as nitrogen or argon, or ultraviolet-curing resin. It can be made of oil or thermosetting resin, and can be made of PVC (polyvinyl chloride), acrylic, Polyimide, epoxy resin, silicone resin, PVB (polyvinyl butyral) or EV A (ethylene vinyl acetate) can be used. For example, nitrogen can be used as a filler. That's good.
[0231] If necessary, a polarizing plate or a circular polarizing plate (including an elliptical polarizing plate) may be provided on the light-emitting surface of the light-emitting element. Optical films such as retardation plates (λ / 4 plates, λ / 2 plates) and color filters may be provided as appropriate. In addition, the polarizing plate or the circular polarizing plate may be provided with an anti-reflection film. Anti-glare treatment can be applied to diffuse reflected light and reduce glare.
[0232] The signal line driver circuits 4503a and 4503b and the scanning line driver circuits 4504a and 4504b are A driving circuit formed of a single crystal semiconductor film or a polycrystalline semiconductor film on a separately prepared substrate is Also, only the signal line driver circuit, or a part of the signal line driver circuit, or the scanning line driver circuit may be mounted. Only the path or only a part of the path may be separately formed and mounted, and the configuration is not limited to that of FIG.
[0233] Through the above steps, a highly reliable light-emitting display device (display panel) can be manufactured as a semiconductor device. It is possible.
[0234] (Embodiment 7) In this embodiment, at least a part of the driver circuit and a thin film transistor to be disposed in the pixel portion are formed on the same substrate. An example of fabricating a transistor will be described below.
[0235] The thin film transistors arranged in the pixel portion are formed according to the first embodiment. The thin film transistor shown in the embodiment 1 is an n-channel TFT, so the n-channel A part of the driving circuit that can be configured with a panel-type TFT is the same as the thin-film transistor of the pixel part. It is formed on a substrate.
[0236] An example of a block diagram of an active matrix display device is shown in FIG. On the plate 5300, a pixel section 5301, a first scanning line driver circuit 5302, a second scanning line driver The pixel portion 5301 includes a signal line driver circuit 5303 and a signal line driver circuit 5304. A signal line driver circuit 5304 is extended from the first scanning line driver circuit 5305. 302 and the second scanning line driver circuit 5303. At the intersections with the signal lines, pixels each having a display element are arranged in a matrix. In addition, the display device substrate 5300 is a flexible printed circuit board (FPC). Through the connection part such as the timing control circuit 5305 (controller, control IC (also called the
[0237] In FIG. 8A, a first scanning line driver circuit 5302, a second scanning line driver circuit 5303, a signal The line driver circuit 5304 is formed on the same substrate 5300 as the pixel portion 5301. The number of externally provided components such as drive circuits is reduced, which contributes to cost reduction. In the case where a driving circuit is provided outside the substrate 5300, the wiring is extended to connect the driving circuit at the connection portion. The number of connections can be reduced, and the reliability or yield can be improved.
[0238] The timing control circuit 5305 is, for example, A first scanning line driving circuit start signal (GSP1), a scanning line driving circuit clock signal The timing control circuit 5305 also supplies the second scanning line driving circuit (GCLK1). For example, a start signal for the second scanning line driving circuit (GSP2) (S It supplies a clock signal (GCLK2) for the scanning line driver circuit. The timing control circuit 5305 controls the signal line driver circuit 5304 to receive a start signal for the signal line driver circuit. signal (SSP), clock signal for signal line driver circuit (SCLK), data for video signal ( The CLKIN signal (CLKIN) is supplied to the CLKIN terminal. ... Each clock signal may be a plurality of clock signals with different periods, or may be a clock signal that is inverted. The first scanning line driver may be supplied together with a signal (CKB) that is inverted by the first scanning line driver. It is possible to omit one of the second scanning line driver circuit 5302 and the second scanning line driver circuit 5303.
[0239] In FIG. 8B, circuits with low driving frequencies (for example, the first scanning line driving circuit 5302, the second The scanning line driver circuit 5303) is formed on the same substrate 5300 as the pixel portion 5301, and the signal line driver The circuit 5304 is formed on a substrate different from that of the pixel portion 5301. The thin film transistor has a smaller field effect mobility than a transistor using a single crystal semiconductor. A driver circuit formed on the substrate 5300 can be formed by using transistors. Therefore, it is possible to increase the size of the display device, reduce the cost, and improve the yield. .
[0240] The thin film transistor shown in Embodiment 1 is an n-channel TFT. FIG. 9B shows the configuration and operation of a signal line driver circuit made up of an n-channel TFT. An example will be given to explain.
[0241] The signal line driver circuit includes a shift register 5601 and a switching circuit 5602 . The switching circuit 5602 includes switching circuits 5602_1 to 5602_N (N is a natural number). The switching circuits 5602_1 to 5602_N each have a A plurality of thin film transistors 5603_1 to 5603_k (k is a natural number) are provided. The thin film transistors 5603_1 to 5603_k are n-channel TFTs. An example will be explained.
[0242] The connection relationship of the signal line driver circuit will be described using the switching circuit 5602_1 as an example. The first terminals of the thin film transistors 5603_1 to 5603_k are respectively connected to the wiring 5604_1 The second terminals of the thin film transistors 5603_1 to 5603_k are connected to are connected to the signal lines S1 to Sk, respectively. The gate of k is connected to the wiring 5605_1.
[0243] The shift register 5601 sequentially outputs H level (H signal) to the wirings 5605_1 to 5605_N. , or high power supply potential level), and the switching circuits 5602_1 to 56 It has the function of selecting 02_N in sequence.
[0244] The switching circuit 5602_1 includes wirings 5604_1 to 5604_k and signal lines S1 to Sk. The function of controlling the conduction state (conduction between the first terminal and the second terminal) with the wiring 5604_ The switches have a function of controlling whether or not potentials of 1 to 5604_k are supplied to the signal lines S1 to Sk. In this way, the switching circuit 5602_1 has a function as a selector. The film transistors 5603_1 to 5603_k are connected to the wirings 5604_1 to 5604_k, respectively. and the signal lines S1 to Sk, that is, the wirings 5604_1 to 5604_k The thin film transistor 56 has a function of supplying the potential to the signal lines S1 to Sk. Each of 03_1 to 5603_k has a function as a switch.
[0245] In addition, the wirings 5604_1 to 5604_k each carry video signal data (DATA). The video signal data (DATA) is an analog signal corresponding to the image information or image signal. This is often a signal that
[0246] Next, the operation of the signal line driver circuit in FIG. 9(A) will be described with reference to the timing chart in FIG. 9(B). 9B shows signals Sout_1 to Sout_N and a signal Vda The signals Sout_1 to Sout_N are each an example of 5601. The signals Vdata_1 to Vdata_k are an example of an output signal of the soft register 5601. , are examples of signals input to the wirings 5604_1 to 5604_k. One operation period of the drive circuit corresponds to one gate selection period in the display device. As an example, the period is divided into periods T1 to TN. This is a period for writing video signal data (DATA) to pixels belonging to a selected row.
[0247] In the drawings of the present embodiment, the signal waveforms of the components are not rounded for clarity. Therefore, the scale may not necessarily be limited to the actual scale. It should be noted that
[0248] During the period T1 to the period TN, the shift register 5601 outputs an H-level signal to the wiring 560 For example, in the period T1, the shift registers 5 601 outputs a high-level signal to the wiring 5605_1. Since 5603_1 to 5603_k are turned on, wiring 5604_1 to 5604_k and signal At this time, the wirings 5604_1 to 5604_k are in a conductive state. Data(S1)~Data(Sk) are input. Data(S1)~Data(Sk ) belong to a selected row via thin film transistors 5603_1 to 5603_k. In this way, during the periods T1 to TN, Then, the video signal data (DATA) is sent to the pixels in the selected row in order of k columns. It will be written.
[0249] As described above, video signal data (DATA) is written to the pixels in multiple columns. This makes it possible to reduce the number of video signal data (DATA) or the number of wirings. This reduces the number of connections to external circuits. By writing directly to the memory, the writing time can be increased, and the video signal can be written more quickly. This can prevent under-crowding.
[0250] The shift register 5601 and the switching circuit 5602 are the same as those in the first embodiment. It is possible to use a circuit composed of thin film transistors shown in 3 and 6. In this case, The polarity of all the transistors in the shift register 5601 is n-channel or p-channel. The filter can be constructed with only one polarity of the two panel types.
[0251] Regarding one form of a shift register used as a part of a scanning line driver circuit and / or a signal line driver circuit, This will be explained with reference to FIG. 10 and FIG. 11.
[0252] The scanning line driving circuit has a shift register. In some cases, it may also have a level shifter or a buffer. In the scanning line driver circuit, a clock signal is input to the shift register. The selection signal is generated by inputting the clock (CLK) and start pulse signal (SP). The generated selection signal is buffered and amplified in a buffer and then supplied to the corresponding scan line. The gate electrodes of the transistors of the pixels for one line are connected to the scanning line. Since the transistors of the pixels in one line must be turned on simultaneously, The capacitor used is capable of carrying a large current.
[0253] The shift register includes a first pulse output circuit 10_1 to an N-th pulse output circuit 10_N ( N is a natural number equal to or greater than 3 (see FIG. 10(A)). The first pulse output circuit 10_1 to the N-th pulse output circuit 10_N of the register are A first clock signal CK1 is transmitted from a wiring 11, and a second clock signal CK2 is transmitted from a second wiring 12. , a third clock signal CK3 is output from a third wiring 13, and a fourth clock signal CK4 is output from a fourth wiring 14. In the first pulse output circuit 10_1, a signal CK4 is supplied from the fifth wiring 15. A start pulse SP1 (first start pulse) is input. In the pulse output circuit 10_n (n is a natural number between 2 and N), A signal from the previous stage (called the previous stage signal OUT(n-1)) (n is a natural number greater than or equal to 2) is input. In addition, in the first pulse output circuit 10_1, the third pulse output circuit 10_3, which is two stages behind, Similarly, in the second or subsequent n-th pulse output circuit 10_n, a signal from the second or subsequent stage is input. The signal from the (n+2)th pulse output circuit 10_(n+2) in the latter stage (the latter stage signal OUT(n +2) is input. Therefore, the pulse output circuit of each stage outputs the following stage and / or The first output signal (OUT(1)(SR) to be input to the two preceding pulse output circuits UT(N)(SR)), the second output signal (OUT(1) to OUT As shown in FIG. 10(A), the 2nd stage of the shift register is Since the next stage signal OUT(n+2) is not input to one stage, for example, The start pulse SP2 and the third start pulse SP3 may be input. stomach.
[0254] The clock signal (CK) goes between H and L levels (L signal, low power supply potential) at regular intervals. Here, the first clock signal (CK1) to the second clock signal (CK2) are The fourth clock signal (CK4) is delayed by 1 / 4 cycle in sequence. The first clock signal (CK1) to the fourth clock signal (CK4) are used to generate a pulse output circuit. The clock signal is GCK depending on the input drive circuit. It is sometimes called SCK, but here we will use the term CK for explanation.
[0255] The first input terminal 21, the second input terminal 22, and the third input terminal 23 are connected to the first wiring 11 to The fourth wiring 14 is electrically connected to the fourth wiring 14. For example, in FIG. The first pulse output circuit 10_1 has a first input terminal 21 electrically connected to the first wiring 11. The second input terminal 22 is electrically connected to the second wiring 12, and the third input terminal 23 is The second pulse output circuit 10_2 is electrically connected to the third wiring 13. The first input terminal 21 is electrically connected to the second wiring 12, and the second input terminal 22 is electrically connected to the third wiring 13. The third input terminal 23 is electrically connected to the fourth wiring 14. There are.
[0256] Each of the first pulse output circuit 10_1 to the N-th pulse output circuit 10_N has a first input terminal a first input terminal 21, a second input terminal 22, a third input terminal 23, a fourth input terminal 24, a fifth input terminal The input terminal 25, the first output terminal 26, and the second output terminal 27 (see FIG. 10(B)). In the first pulse output circuit 10_1, a first clock signal is input to a first input terminal 21. A first clock signal CK1 is input to the first input terminal 22, a second clock signal CK2 is input to the third input terminal 23, and a third clock signal CK3 is input to the second input terminal 24. A third clock signal CK3 is input to the input terminal 23 of the second clock CLK1, and a start signal CK4 is input to the fourth input terminal 24 of the third clock CLK2. A pulse is input, the next stage signal OUT(3) is input to the fifth input terminal 25, and the first output A first output signal OUT(1)(SR) is output from a terminal 26, and a second output signal OUT(1)(SR) is output from a second output terminal 27. The second output signal OUT(1) is output.
[0257] The first pulse output circuit 10_1 to the N-th pulse output circuit 10_N are each a three-terminal thin-film transistor. In addition to TFTs (also called Thin Film Transistors), The four-terminal thin film transistor described in the above embodiment can be used. 1 shows a symbol of the four-terminal thin film transistor 28 described in the above embodiment. The symbol of the thin film transistor 28 shown in FIG. 10(C) corresponds to either the third or sixth embodiment. This refers to the four-terminal thin film transistor described in the above paragraph 1, and will be used hereinafter in the drawings, etc. In this specification, when a thin film transistor has two gate electrodes via a semiconductor layer, In this case, the gate electrode below the semiconductor layer is called the lower gate electrode, and the gate electrode above the semiconductor layer is called the upper gate electrode. The electrode is also called the upper gate electrode. The thin film transistor 28 is connected to the lower gate electrode. A first control signal G1 is input to the gate electrode of the upper gate electrode and a second control signal G2 is input to the gate electrode of the upper gate electrode. It is an element that can perform electrical control between the In terminal and the Out terminal.
[0258] When an oxide semiconductor is used for a semiconductor layer including a channel formation region of a thin film transistor, The threshold voltage may shift to the negative or positive side depending on the process. Therefore, in a thin film transistor in which an oxide semiconductor is used for a semiconductor layer including a channel formation region, A structure capable of controlling the threshold voltage is preferable. The threshold voltage of the thin film transistor 28 is determined by gate electrodes above and below the channel forming region of the thin film transistor 28. A gate electrode is provided through a gate insulating film, and the potential of the upper and / or lower gate electrodes is controlled. By doing so, it is possible to control the value to a desired value.
[0259] Next, an example of a specific circuit configuration of the pulse output circuit will be described with reference to FIG.
[0260] The first pulse output circuit 10_1 includes a first transistor 31 to a thirteenth transistor 43. (See FIG. 10(D)). In addition, the first input terminal 21 to the fifth input terminal a first output terminal 25, a first output terminal 26, a second output terminal 27, and a first high power supply potential VDD a power supply line 51 to which a second high power supply potential VCC is supplied, a power supply line 52 to which a low power supply potential The first transistor 31 to the thirteenth transistor 4 are connected to the power supply line 53 through which VSS is supplied. A signal or a power supply potential is supplied to 3. Here, the magnitude of the power supply potential of each power supply line in FIG. The minor relationship is that the first power supply potential VDD is equal to or higher than the second power supply potential VCC, and The potential VCC is set to a potential higher than the third power supply potential VSS. K1) to the fourth clock signal (CK4) alternate between H and L levels at regular intervals. When it is a signal, its H level is VDD and when it is a L level it is VSS. By making the potential VDD of 51 higher than the potential VCC of the power supply line 52, the operation is not affected. The potential applied to the gate electrode of the transistor can be kept low without causing a problem. This reduces the threshold shift of the transistor and suppresses degradation. As shown in FIG. 1, among the first transistor 31 to the thirteenth transistor 43, the first The first transistor 31 and the sixth to ninth transistors 36 to 39 are shown in FIG. It is preferable to use a four-terminal thin film transistor 28 shown in FIG. The operation of the sixth transistor 31, the sixth transistor 36 to the ninth transistor 39 is The potential of the node to which one of the drain electrodes is connected is controlled by the gate electrode control signal. A transistor that is required to switch in response to a control signal input to its gate electrode. The fast response (the rise of the on-current is steep) reduces malfunction of the pulse output circuit. Therefore, the four-terminal thin film transistor shown in FIG. By using the transistor 28, the threshold voltage can be controlled, and malfunctions are reduced. In FIG. 10(D), the first control signal G The first and second control signals G1 and G2 are the same control signal, but different control signals are input. You may do so.
[0261] In FIG. 10D, the first transistor 31 has a first terminal electrically connected to a power supply line 51. The second terminal is electrically connected to the first terminal of the ninth transistor 39, and the gate electrode ( The lower gate electrode and the upper gate electrode are electrically connected to a fourth input terminal 24. The second transistor 32 has a first terminal electrically connected to the power supply line 53 and a second terminal A gate electrode of the ninth transistor 39 is electrically connected to the first terminal of the fourth transistor The third transistor 33 has a first terminal electrically connected to a gate electrode of the second transistor 34. A first terminal is electrically connected to the input terminal 21, and a second terminal is electrically connected to the first output terminal 26. The fourth transistor 34 has a first terminal electrically connected to the power supply line 53 and a second terminal electrically connected to the power supply line 53. The second terminal is electrically connected to the first output terminal 26. The fifth transistor 35 is One terminal is electrically connected to the power supply line 53, and the second terminal is a gate voltage of the second transistor 32. and a gate electrode of a fourth transistor 34, the gate electrode of which is electrically connected to the fourth input The sixth transistor 36 has a first terminal electrically connected to the power supply line 5. 2, and the second terminal is electrically connected to the gate electrode of the second transistor 32 and the gate electrode of the fourth transistor The gate electrode of the transistor 34 is electrically connected to the gate electrode of the gate electrode (the lower gate electrode and the upper The gate electrode of the seventh transistor 3 is electrically connected to the fifth input terminal 25. The seventh transistor has a first terminal electrically connected to the power supply line 52 and a second terminal electrically connected to the eighth transistor 38. The gate electrodes (lower gate electrode and upper gate electrode) are electrically connected to the second terminal. The eighth transistor 38 has a first terminal electrically connected to the third input terminal 23. The gate electrode of the second transistor 32 and the gate electrode of the fourth transistor 34 are electrically connected to , and the gate electrodes (the lower gate electrode and the upper gate electrode) are connected to the second input terminal 2 The ninth transistor 39 has a first terminal electrically connected to the first transistor 2. a second terminal of the second transistor 31 and a second terminal of the second transistor 32; The gate electrode of the third transistor 33 and the gate electrode of the tenth transistor 40 are supplied with a current. The gate electrodes (lower gate electrode and upper gate electrode) are electrically connected to the power supply line 52. The tenth transistor 40 has a first terminal electrically connected to the first input terminal 21. the second terminal is electrically connected to the second output terminal 27, and the gate electrode is The second terminal of the ninth transistor 39 is electrically connected to the second terminal of the eleventh transistor 4 1 has a first terminal electrically connected to the power supply line 53 and a second terminal electrically connected to the second output terminal 27. The gate electrodes of the second transistor 32 and the fourth transistor The twelfth transistor 42 is electrically connected to the gate electrode of the first terminal is electrically connected to the power supply line 53, the second terminal is electrically connected to the second output terminal 27, The gate electrode of the seventh transistor 37 (the lower gate electrode and the upper gate electrode) The thirteenth transistor 43 has a first terminal electrically connected to the power supply line 53. the second terminal is electrically connected to the first output terminal 26, and the gate electrode is The gate electrodes (lower gate electrode and upper gate electrode) of the seventh transistor 37 are electrically connected to are actively connected.
[0262] In FIG. 10D, the gate electrode of the third transistor 33 and the gate electrode of the tenth transistor 4 The connection point of the gate electrode of transistor 0 and the second terminal of transistor 939 is referred to as node A. In addition, the gate electrode of the second transistor 32, the gate electrode of the fourth transistor 34, the second terminal of the fifth transistor 35, the second terminal of the sixth transistor 36, the second terminal of the eighth transistor The connection point of the first terminal of the transistor 38 and the gate electrode of the eleventh transistor 41 is node B. (See FIG. 11(A)).
[0263] FIG. 11A shows the pulse output circuit described in FIG. 10D as a first pulse output circuit 10_ 1, the first input terminal 21 to the fifth input terminal 25 and the first output terminal 26 and a signal input to or output from a second output terminal 27.
[0264] Specifically, a first clock signal CK1 is input to the first input terminal 21, and A second clock signal CK2 is input to the third input terminal 22, and a third clock signal CK3 is input to the third input terminal 23. A start pulse is input to the fourth input terminal 24, and a clock signal CK3 is input to the fifth input terminal The next stage signal OUT(3) is input to the first output terminal 25, and the first output signal OUT (1)(SR) is output, and the second output signal OUT(1) is output from the second output terminal 27. will be done.
[0265] A thin film transistor is defined as a transistor having at least three elements including a gate, a drain, and a source. A semiconductor device has a terminal and a channel region formed in a region overlapping with the gate. By controlling the gate potential, the drain and source are connected via the channel region. The current flowing between the source and drain can be controlled by the thin film transistor. Which is the source and which is the drain depends on the transistor structure and operating conditions, etc. Therefore, the regions that function as the source and drain are In some cases, the term "source" or "drain" is not used. In such cases, for example, They may be referred to as terminal or second terminal.
[0266] In FIG. 10(D) and FIG. 11(A), the node A is put into a floating state, and the boot A capacitor may be provided separately to perform a strap operation. To achieve this, a capacitor having one electrode electrically connected to the node B may be provided separately.
[0267] Here, the timing of the shift register having a plurality of pulse output circuits shown in FIG. A shift register is a scanning line driver circuit. In this case, the period 61 in FIG. 11B corresponds to a vertical blanking period, and the period 62 corresponds to a gate selection period. do.
[0268] As shown in FIG. 11A, the ninth transistor has a gate to which the second power supply potential VCC is applied. By providing the transistor 39, the following can be achieved before and after the bootstrap operation: There are such advantages.
[0269] In the absence of the ninth transistor 39, the gate electrode of which is applied with the second power supply potential VCC, When the potential of the node A rises due to the base strap operation, the second transistor 31 The potential of the source terminal rises and becomes higher than the first power supply potential VDD. Then, the source of the first transistor 31 is switched to the first terminal side, that is, the power supply line 51 side. Therefore, in the first transistor 31, between the gate and the source, between the gate and the drain In both cases, a large bias voltage is applied, which places a large stress on the transistor. Therefore, the ninth power supply potential VCC is applied to the gate electrode. By providing the transistor 39, the voltage of the node A is increased by the bootstrap operation. The potential of the second terminal of the first transistor 31 is increased, but the potential of the second terminal of the first transistor 31 is not increased. That is, by providing the ninth transistor 39, It is possible to reduce the value of the negative bias voltage applied between the gate and source of the transistor 31. Therefore, by using the circuit configuration of this embodiment, the first transistor 31 The negative bias voltage applied between the gate and source can also be reduced, reducing the stress-induced Deterioration of the first transistor 31 can be suppressed.
[0270] The ninth transistor 39 is provided at a position corresponding to the second gate of the first transistor 31. A terminal is connected between the terminal and the gate of the third transistor 33 via a first terminal and a second terminal. In addition, in the present embodiment, a system having a plurality of pulse output circuits may be provided. In the case of a soft register, the signal line driver circuit has more stages than the scan line driver circuit. The resistor 39 may be omitted, which has the advantage of reducing the number of transistors.
[0271] Note that the semiconductor layers of the first to thirteenth transistors 31 to 43 are made of oxide semiconductor. By using a conductor, the off-current of the thin film transistor is reduced, and the on-current and Because it is possible to increase the field effect mobility and reduce the degree of degradation. In addition, a transistor using an oxide semiconductor can be used. Compared to transistors using amorphous silicon, a higher potential is applied to the gate electrode. Therefore, the degree of deterioration of the transistor due to the second power supply potential VCC is small. The same operation can be obtained by supplying the first power supply potential VDD to the power supply line, and the wiring between the circuits is Since the number of power supply lines can be reduced, the circuit can be made more compact.
[0272] The gate electrodes (lower gate electrode and upper gate electrode) of the seventh transistor 37 a clock signal provided by the third input terminal 23 to the gate of the eighth transistor 38; The input electrodes (lower gate electrode and upper gate electrode) are supplied with a second input terminal 22. The clock signal is applied to the gate electrode of the seventh transistor 37 (the lower gate electrode and the upper gate electrode). A clock signal is supplied to the gate electrode of the eighth transistor by the second input terminal 22. The gate electrodes of the gate electrodes of the first input terminal 23 are connected to the gate electrodes of the second input terminal 23. Therefore, the same effect can be obtained by switching the wiring so that the clock signal is supplied. In the shift register shown in FIG. The seventh transistor 37 is turned off, and the eighth transistor 38 is turned on. The seventh transistor 37 is turned off, and the eighth transistor 38 is turned on. When the power supply 38 is turned off, the second input terminal 22 and the third input terminal 23 are turned on. The voltage drop at node B is applied to the gate of the seventh transistor 37. 2 due to a drop in the potential of the gate electrode of the eighth transistor 38 and a drop in the potential of the gate electrode of the eighth transistor 39. On the other hand, in the shift register shown in FIG. The seventh transistor 37 and the eighth transistor 38 are both in an on state. is on, the eighth transistor 38 is off, and then the seventh transistor 37 is off. By turning off the eighth transistor 38, the second input terminal 22 and The voltage drop at the node B caused by the voltage drop at the input terminal 23 of the third transistor is The potential of the gate electrode of the transistor 38 can be reduced to one time. The gate electrodes (lower gate electrode and upper gate electrode) of the seventh transistor 37 are connected to the third A clock signal CK3 is supplied from the input terminal 23, and the gate electrode of the eighth transistor 38 A clock signal CK is input from the second input terminal 22 to the lower gate electrode and the upper gate electrode. It is preferable to have a wiring relationship in which 2 is input. This is because the number of times the potential of node B changes This is because the difference in the signal strength between the input and output signals is reduced, thereby reducing noise.
[0273] In this manner, the potentials of the first output terminal 26 and the second output terminal 27 are maintained at the L level. By configuring the node B to periodically receive a high-level signal during the period, the pulse output This makes it possible to suppress malfunction of the power circuit.
[0274] (Embodiment 8) The light emitting device disclosed in this specification can be applied to various electronic devices (including gaming machines). The electronic device can be, for example, a television device (a television or a television receiver). (also called "transmitting devices"), computer monitors, digital cameras, digital video cameras Cameras, digital photo frames, mobile phones (also called mobile phones or mobile phone devices) , portable game machines, personal digital assistants, audio playback devices, pachinko machines and other large game machines. Some examples include:
[0275] FIG. 12A shows an example of a mobile phone. The mobile phone 1100 has a housing 1101. In addition to the display unit 1102, the operation buttons 1103, the external connection port 1104, It is equipped with a speaker 1105, a microphone 1106, etc.
[0276] In the mobile phone 1100 shown in FIG. 12A, information is displayed by touching a display unit 1102 with a finger or the like. You can also make calls, write emails, and perform other operations from the display. This can be done by touching the display unit 1102 with a finger or the like.
[0277] The screen of the display unit 1102 has three main modes. The first is a display mode that mainly displays images. The first mode is a display mode, the second is an input mode for inputting information such as characters, and the third mode is a display mode. This is a display + input mode that combines the display mode and the input mode.
[0278] For example, when making a call or composing an e-mail, the display unit 1102 is used to input characters. The main character input mode is to input characters displayed on the screen. It is preferable to display a keyboard or number buttons on most of the screen of the display unit 1102. I wish.
[0279] In addition, the mobile phone 1100 may include a sensor for detecting tilt, such as a gyro or an acceleration sensor. By providing a detection device having the above configuration, the orientation of the mobile phone 1100 (portrait or landscape) can be determined and the display The screen display of the display unit 1102 can be automatically switched.
[0280] The screen mode can be changed by touching the display unit 1102 or by operating the housing 1101. This is done by operating the button 1103. Also, depending on the type of image displayed on the display unit 1102, For example, the image signal to be displayed on the display unit is a moving image. If it is data, the mode is switched to display mode, and if it is text data, the mode is switched to input mode.
[0281] In the input mode, the optical sensor of the display unit 1102 detects a signal and displays If there is no input by touch operation of the unit 1102 for a certain period of time, the screen mode is changed to the input mode. Alternatively, the display mode may be switched from the normal mode to the display mode.
[0282] The display unit 1102 can also function as an image sensor. By touching the palm or fingers to the sensor 02, the palm print, fingerprint, etc. can be captured and identity authentication can be performed. In addition, the display unit may be equipped with a backlight that emits near-infrared light or a sensor that emits near-infrared light. By using a scanning light source, it is also possible to image finger veins, palm veins, etc.
[0283] The display portion 1102 includes a plurality of thin film transistors 460 described in Embodiment 1. Since the film transistor 460 has a light-transmitting property, when a photosensor is provided in the display portion 1102, In this case, the thin film transistor 460 does not block the incident light. When using a backlight that emits external light or a sensing light source that emits near-infrared light This is preferable because the thin film transistor 460 does not block light.
[0284] FIG. 12(B) is also an example of a mobile phone. The portable information terminal shown in FIG. 12(B) is It can have multiple functions. For example, in addition to the telephone function, it can have a built-in computer and perform various functions. It can also be equipped with various data processing functions.
[0285] The portable information terminal shown in FIG. 12B includes two housings, a housing 1800 and a housing 1801. The housing 1801 includes a display panel 1802, a speaker 1803, a microphone, and a 1804, a pointing device 1806, a camera lens 1807, an external connection terminal The housing 1800 includes a keyboard 1810, an external memory slot 1812, and the like. 811, etc. Also, an antenna is built into the housing 1801.
[0286] The display panel 1802 is equipped with a touch panel, and the image displayed on the display panel 1802 is shown in FIG. A plurality of operation keys 1805 are indicated by dotted lines.
[0287] In addition to the above configuration, a non-contact IC chip, a small recording device, etc. may be built in.
[0288] The light emitting device can be used in a display panel 1802, and the display direction can be appropriately adjusted according to the usage mode. In addition, a camera lens 1807 is provided on the same surface as the display panel 1802. A speaker 1803 and a microphone 1804 are used for voice communication. Not only can it be used for phone calls, but also for video calls, recording, playback, etc. 1801 slides and changes from the unfolded state shown in Figure 12(B) to the overlapped state. This allows for miniaturization suitable for portability.
[0289] The external connection terminal 1808 can be connected to various cables such as AC adapters and USB cables. It is possible to charge the battery and to communicate data with a personal computer, etc. By inserting a recording medium into the memory slot 1811, it is possible to store and transfer a larger amount of data. do.
[0290] In addition to the above functions, even if the device has infrared communication function, TV reception function, etc. good.
[0291] FIG. 13A shows an example of a television device. The television device 9600 includes: A display unit 9603 is incorporated in a housing 9601. The display unit 9603 displays images. In this embodiment, the housing 9601 is supported by a stand 9605. The figure shows a configuration in which
[0292] The television device 9600 can be operated using an operation switch on the housing 9601 or a separate remote control. This can be done by the remote control operation device 9610. The channel and volume can be controlled by the 9609, and the display 9603 shows In addition, the remote control unit 9610 can control the video. A display portion 9607 for displaying information output from 9610 may be provided.
[0293] The television device 9600 includes a receiver and a modem. It can receive more general television broadcasts, and can also be connected to a modem via wired or wireless connection. By connecting to a network, communication can be one-way (sender to receiver) or two-way. It is also possible to communicate information (between a sender and a receiver, or between receivers).
[0294] In order to provide a plurality of thin film transistors 460 described in Embodiment 1 in the display portion 9603, The aperture ratio can be increased, particularly when the light emitting device is of a bottom emission type.
[0295] FIG. 13B shows an example of a digital photo frame. In the frame 9700, a display unit 9703 is incorporated in a housing 9701. 3 is capable of displaying various images, for example images taken with a digital camera. By displaying data, it can function just like a normal photo frame.
[0296] In order to provide a plurality of thin film transistors 460 described in Embodiment 1 in the display portion 9703, The aperture ratio can be increased, particularly when the light emitting device is of a bottom emission type.
[0297] The Digital Photo Frame 9700 is equipped with an operation unit, external connection terminals (USB terminal, US A terminal that can be connected to various cables such as B cable, etc., and a recording medium insertion section, etc. These components may be installed on the same surface as the display unit, but they may be installed on the side or back. It is preferable to have a digital photo frame with a built-in memory card because it improves the design. A memory that stores image data taken with a digital camera is inserted into the body insertion section. The captured image data can be displayed on the display portion 9703 .
[0298] The digital photo frame 9700 may also be configured to transmit and receive information wirelessly. It is also possible to wirelessly import and display desired image data.
[0299] FIG. 14 shows a portable gaming machine, which is composed of two cabinets, a cabinet 9881 and a cabinet 9891. The housing 9881 includes a display unit 988 and a connector 9893 for connecting the display unit 988 to the housing 9881 in an openable and closable manner. 2 is incorporated in the housing 9891, and a display unit 9883 is incorporated in the housing 9891.
[0300] The display portion 9882 and the display portion 9883 include the thin film transistor 460 described in Embodiment 1. Since a plurality of light emitting devices are arranged, the aperture ratio can be increased, particularly when the light emitting device is of a bottom emission type.
[0301] In addition, the portable game machine shown in FIG. 14 also includes a speaker unit 9884 and a recording medium insertion unit 98 86, LED lamp 9890, input means (operation keys 9885, connection terminal 9887, sensor 9888 (force, displacement, position, velocity, acceleration, angular velocity, rotation speed, distance, light, liquid, magnetism, temperature , chemicals, voice, time, hardness, electric field, current, voltage, power, radiation, flow rate, humidity, gradient, Equipped with a microphone 9889) and other equipment, including a function to measure vibration, odor, or infrared rays Of course, the configuration of the portable gaming machine is not limited to the above, and at least It is sufficient that the device has the thin film transistor disclosed in the document, and other auxiliary equipment is provided as appropriate. The portable game machine shown in FIG. 14 can be configured as follows. The function of reading out programs or data and displaying them on the display unit, as well as wireless communication with other portable gaming machines, The portable gaming machine shown in FIG. 14 has the following functions: is not limited thereto and can have various functions.
[0302] FIG. 15 shows a light emitting device formed by applying the above embodiment as an indoor lighting device 3001. The light emitting device shown in the second embodiment can be enlarged. The light-emitting device described in the above embodiment 2 can be used as a lighting device. It can also be used as a tabletop lighting fixture 3000. In addition to lighting fixtures and tabletop lighting fixtures, this also includes wall-mounted lighting fixtures, in-car lighting, and emergency exit lights. can be.
[0303] As described above, the light emitting devices shown in the second and third embodiments can be used in various The thin film transistor 450 can be disposed in a display panel of various electronic devices. and the thin film transistor 460 is used as a switching element of the display panel. Therefore, the light emitting device has a display section with a high aperture ratio, particularly in the case of a bottom emission type, and is highly reliable. It is possible to provide a new electronic device. [Explanation of symbols]
[0304] 10 Pulse output circuit 11 Wiring 12 Wiring 13 Wiring 14 Wiring 15 Wiring 21 Input terminal 22 Input terminal 23 Input terminal 24 Input terminals 25 Input terminal 26 Output terminal 27 Output terminal 28 Thin-film transistor 31 Transistor 32 Transistor 33 Transistor 34 Transistor 35 Transistor 36 Transistor 37 Transistor 38 Transistor 39 Transistor 40 Transistor 41 Transistor 42 Transistor 43 Transistor 51 Power line 52 Power line 53 Power line 61 period 62 period 111a Gate electrode layer 111b Capacitor wiring layer 111c Gate electrode layer 113 Oxide semiconductor layer 115a Electrode layer 115b Electrode layer 115c capacitive electrode layer 123 Oxide semiconductor layer 211a Gate electrode layer 211b Gate wiring layer 211c Gate electrode layer 213 Oxide semiconductor layer 213a High resistance source region 213b High-resistance drain region 215a Source electrode layer 215b Drain electrode layer 215c Connection electrode layer 215d Connection electrode layer 215e wiring layer 215f Connection electrode layer 215g Terminal 216 Conductive Layer 223 Channel formation region 400 Substrates 402 Gate insulating layer 407 Oxide insulating layer 408 Protective insulation layer 411 Color filter layer 412 Overcoat layer 414 Electrode 415 Conductive Layer 416 Electrode layer 417 Terminal 418 Conductive Layer 450 Thin Film Transistor 459 Bulkhead 460 Thin Film Transistor 1001 Electrode 1002 Electrode 1003 EL layer 1004 Charge generating layer 1100 Mobile Phone 1101 Case 1102 Display section 1103 Operation button 1104 External connection port 1105 Speaker 1106 Mike 1800 Case 1801 Case 1802 Display Panel 1803 Speaker 1804 Microphone 1805 Operation key 1806 Pointing Device 1807 Camera Lenses 1808 External connection terminal 1810 Keyboard 1811 External memory slot 3000 Table Lamp 3001 Lighting equipment 4501 Board 4502 Pixel section 4503a Signal line driver circuit 4504a Scanning line driver circuit 4505 Sealing material 4506 Board 4507 Filling material 4509 Thin-film transistor 4510 Thin-film transistor 4511 Light emitting element 4512 Electroluminescent layer 4513 Pixel electrode 4515 Connection terminal electrode 4516 Terminal electrode 4517 Pixel electrode 4518a FPC 4519 Anisotropic conductive film 4520 Bulkhead 4540 Conductive layer 4542 Oxide insulating layer 4543 Overcoat layer 4544 Insulation layer 4545 Color filter layer 4548 Connection electrode layer 5300 Board 5301 Pixel unit 5302 Scanning line driver circuit 5303 Scanning line driver circuit 5304 Signal line driver circuit 5305 Timing Control Circuit 5601 Shift Register 5602 Switching Circuit 5603 Thin Film Transistor 5604 Wiring 5605 Wiring 6400 pixels 6401 Switching transistor 6402 Driving transistor 6403 Capacitor 6404 Light emitting element 6405 Signal Line 6406 scan lines 6407 Power line 6408 Common electrode 7001 TFT 7002 Light emitting element 7003 Electrode 7004 EL layer 7005 Electrode 7009 Bulkhead 7011 Driving TFT 7012 Light emitting element 7013 Electrode 7014 EL layer 7015 Electrode 7016 Shielding membrane 7017 Conductive film 7019 Bulkhead 7021 Driving TFT 7022 Light emitting element 7023 Electrode 7024 EL layer 7025 Electrode 7027 Conductive film 7029 Bulkhead 7030 Connection electrode layer 7031 Oxide insulating layer 7033 Color filter layer 7034 Overcoat layer 7035 Protective insulation layer 7040 Connection electrode layer 7041 Oxide insulating layer 7043 Color filter layer 7044 Overcoat layer 7045 Protective insulation layer 7050 Connection electrode layer 7051 Oxide insulating layer 7053 Planarizing insulating layer 7055 Protective insulation layer 9600 Television Equipment 9601 Case 9603 Display section 9605 Stand 9607 Display section 9609 Operation key 9610 Remote control device 9700 Digital Photo Frame 9701 Case 9703 Display section 9881 Case 9882 Display section 9883 Display section 9884 Speaker section 9885 Operation key 9886 Recording medium insertion section 9887 Connection terminal 9888 Sensor 9889 Microphone 9890 LED Lamp 9891 Case 9893 Connection section
Claims
1. A semiconductor device including a first transistor having a first channel formation region and a second transistor having a second channel formation region, a first conductive layer and a second conductive layer; a first insulating layer in contact with a lower surface of the oxide semiconductor layer including the first channel formation region and a lower surface of the oxide semiconductor layer including the second channel formation region, the lower surface being above the first conductive layer and the second conductive layer; a third conductive layer electrically connected to the oxide semiconductor layer including the first channel formation region; and a fourth conductive layer electrically connected to the oxide semiconductor layer including the second channel formation region; and a second insulating layer on and in contact with the third conductive layer and the fourth conductive layer; A semiconductor device, wherein a fifth conductive layer formed in the same process as the first conductive layer is located below a sixth conductive layer formed in the same process as the second conductive layer and has a region overlapping with the sixth conductive layer.
2. In claim 1, The second insulating layer comprises silicon oxide.
3. In claim 1 or 2, The third conductive layer and the fourth conductive layer comprise the same material.
4. In any one of claims 1 to 3, The first conductive layer comprises Mo.