Semiconductor manufacturing apparatus and manufacturing method for semiconductor device

The semiconductor manufacturing apparatus addresses substrate warpage by measuring and adjusting the gap and pressing force during bonding, enhancing the reliability and quality of semiconductor device production.

JP2024132449AActive Publication Date: 2024-10-01KIOXIA CORP
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2023043213
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-17
Publication Date
2024-10-01
Estimated Expiration
2043-03-17

AI Technical Summary

Technical Problem

When bonding substrates together in semiconductor manufacturing, warped substrates can lead to improper bonding due to misalignment and defects such as high resistance or disconnection.

Method used

A semiconductor manufacturing apparatus with a warpage amount measuring section, gap determining section, and bonding control unit that adjusts the gap and pressing force based on substrate warpage to ensure proper alignment and bonding.

Benefits of technology

The solution effectively corrects substrate warpage and misalignment, ensuring reliable bonding of semiconductor devices with improved yield and reduced defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024132449000001_ABST
    Figure 2024132449000001_ABST
Patent Text Reader

Abstract

To provide a semiconductor manufacturing apparatus and a manufacturing method for a semiconductor device capable of suitably bonding substrates to each other.SOLUTION: In one embodiment, a semiconductor manufacturing apparatus includes a warpage measurement unit that measures the value of warpage of a first substrate or a second substrate. The apparatus further includes a gap determination unit that determines the value of a gap between the first substrate and the second substrate, based on the value of the warpage. The apparatus moreover includes a bonding control unit that controls the gap to be the determined value before the first substrate and the second substrate are bonded together.SELECTED DRAWING: Figure 18
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] An embodiment of the present invention relates to a semiconductor manufacturing apparatus and a method for manufacturing a semiconductor device. [Background technology]

[0002] When substrates are bonded together, if at least one of the substrates is warped, the substrates may not be bonded together properly. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] International Patent Application Publication No. WO2020 / 045148 [Patent Document 2] Patent No. 6407803 [Patent Document 3] Patent No. 6640546 [Patent Document 4] Special Publication No. 2016-526299 Summary of the Invention [Problem to be solved by the invention]

[0004] A semiconductor manufacturing apparatus and a method for manufacturing a semiconductor device that are capable of suitably bonding substrates together are provided. [Means for solving the problem]

[0005] According to one embodiment, a semiconductor manufacturing apparatus includes a warpage measurement unit that measures a value of a warpage of a first substrate or a second substrate. The apparatus further includes a gap determination unit that determines a value of a gap between the first substrate and the second substrate based on the value of the warpage. The apparatus further includes a bonding control unit that controls the gap to the determined value before bonding the first substrate and the second substrate. [Brief description of the drawings]

[0006] [Figure 1] 2A to 2C are cross-sectional views illustrating a method for manufacturing the semiconductor device of the first embodiment. [Diagram 2] FIG. 1 is a plan view showing a configuration of a bonding apparatus according to a first embodiment. [Diagram 3] 2 is a cross-sectional view showing the configuration of a processing block 25 according to the first embodiment. [Figure 4] 2 is a cross-sectional view showing a configuration of an upper chuck 51 and the like in the first embodiment. FIG. [Diagram 5] 2 is a cross-sectional view showing the configuration of a lower chuck 52 and the like in the first embodiment. FIG. [Figure 6] 5A to 5C are cross-sectional views showing the operation of the bonding apparatus of the first embodiment. [Figure 7] 3A to 3C are cross-sectional views showing a processing method for the upper wafer 1 according to the first embodiment. [Figure 8] 1 is a perspective view showing a configuration of an exposure apparatus in a first embodiment. [Figure 9] FIG. 2 is a plan view for explaining exposure correction in the first embodiment. [Figure 10] FIG. 4 is a cross-sectional view for explaining exposure correction in the first embodiment. [Figure 11] FIG. 2 is a plan view for explaining exposure correction in the first embodiment. [Figure 12] 5A to 5C are schematic diagrams showing a flow of exposure and lamination in a comparative example. [Figure 13] FIG. 11 is a cross-sectional view for explaining details of lamination in a comparative example. [Figure 14] 5A to 5C are schematic diagrams showing a flow of exposure and lamination in a comparative example. [Figure 15] FIG. 3 is a cross-sectional view for explaining details of bonding in the first embodiment. [Figure 16] 4 is a graph for explaining bonding correction according to the first embodiment. [Figure 17] 4 is a graph for explaining bonding correction according to the first embodiment. [Figure 18] 3A to 3C are schematic diagrams illustrating a flow of exposure and lamination in the first embodiment. [Figure 19]11 is a table for explaining bonding correction according to the first embodiment. [Figure 20] 4 is a flowchart showing a method for manufacturing the semiconductor device according to the first embodiment. [Figure 21] 2 is a block diagram showing a functional configuration of a control unit 30 according to the first embodiment. FIG. [Figure 22] 5A to 5C are cross-sectional views showing a method for manufacturing a semiconductor device according to a modified example of the first embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In Fig. 1 to Fig. 22, the same components are denoted by the same reference numerals, and duplicated descriptions will be omitted.

[0008] (First embodiment) (1) Lamination 1A to 1C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to a first embodiment.

[0009] The semiconductor device of this embodiment is manufactured by bonding an upper wafer 1 shown in FIG. 1(a) and a lower wafer 2 shown in FIG. 1(b). One of the upper wafer 1 and the lower wafer 2 is an example of a first substrate, and the other of the upper wafer 1 and the lower wafer 2 is an example of a second substrate. For example, the upper wafer 1 is an example of the first substrate, and the lower wafer 2 is an example of the second substrate. FIG. 1(c) shows a bonded wafer 3 including the upper wafer 1 and the lower wafer 2 bonded together. The bonded wafer 3 is then diced into a plurality of chips (semiconductor devices).

[0010] 1(a) to 1(c) show mutually perpendicular X, Y, and Z directions. In this specification, the +Z direction is treated as the upward direction, and the -Z direction is treated as the downward direction. The -Z direction may or may not coincide with the direction of gravity.

[0011] As shown in FIG. 1(a), the upper wafer 1 includes a wafer 1a, an interlayer insulating film 1b formed on the wafer 1a, and a plurality of metal pads 1c formed in the interlayer insulating film 1b. The wafer 1a is, for example, a semiconductor wafer such as a Si (silicon) wafer. The interlayer insulating film 1b is, for example, a laminated insulating film including a SiO2 film (silicon oxide film) and a SiN film (silicon nitride film). The interlayer insulating film 1b may include various devices such as a memory cell array and a transistor, and may include various conductive layers such as a wiring layer and a plug layer. The metal pads 1c are, for example, a metal layer including a Cu (copper) layer.

[0012] As shown in Fig. 1(b), the lower wafer 2 includes a wafer 2a, an interlayer insulating film 2b formed on the wafer 2a, and a plurality of metal pads 2c formed in the interlayer insulating film 2b. The materials and structures of the wafer 2a, the interlayer insulating film 2b, and the metal pads 2c are similar to those of the wafer 1a, the interlayer insulating film 1b, and the metal pads 1c, respectively. For example, the upper wafer 1 includes a memory cell array, and the lower wafer 2 includes transistors that control the memory cell array.

[0013] As shown in Fig. 1(c), the bonded wafer 3 includes a lower wafer 2 and an upper wafer 1 disposed on the lower wafer 2. The orientation of the upper wafer 1 shown in Fig. 1(c) is opposite to that of the upper wafer 1 shown in Fig. 1(a). In Fig. 1(c), the lower surface of the interlayer insulating film 1b is bonded to the upper surface of the interlayer insulating film 2b, and the lower surface of each metal pad 1c is bonded to the upper surface of the corresponding metal pad 2c.

[0014] When manufacturing the semiconductor device of this embodiment, the magnification of the pattern formed on the wafer 1a may not be the same as the magnification of the pattern formed on the wafer 2a. For example, the magnification of the metal pad 1c may not be the same as the magnification of the metal pad 2c. In this case, each metal pad 1c may not be properly bonded to the corresponding metal pad 2c, and bonding failure such as high resistance at the bonding point or disconnection may occur.

[0015] Therefore, when manufacturing the semiconductor device of this embodiment, the chuck holding the upper wafer 1 or the lower wafer 2 may be deformed to correct the magnification difference between the upper wafer 1 and the lower wafer 2. In this case, the upper wafer 1 and the lower wafer 2 are bonded together with the chuck in a deformed state. This makes it possible to properly bond each metal pad 1c to the corresponding metal pad 2c. For example, it becomes possible to correct a misalignment of about 0 to 10 ppm. Further details of the correction of the magnification difference will be described later.

[0016] 2 is a plan view showing the configuration of a bonding apparatus according to the first embodiment. In this embodiment, this bonding apparatus bonds an upper wafer 1 and a lower wafer 2. This bonding apparatus is an example of a semiconductor manufacturing apparatus.

[0017] As shown in Fig. 2, the bonding apparatus of this embodiment includes a wafer transport unit 10, a wafer processing unit 20, and a control unit 30. The wafer transport unit 10 transports the upper wafer 1 and the lower wafer 2 from the outside of the housing of the bonding apparatus to the inside, and transports the bonded wafer 3 from the inside of the housing of the bonding apparatus to the outside. The wafer processing unit 20 processes the upper wafer 1, the lower wafer 2, and the bonded wafer 3, for example, bonding the upper wafer 1 and the lower wafer 2 together. The control unit 30 controls various operations of the bonding apparatus, for example, controlling the transport of each wafer by the wafer transport unit 10 and the processing of each wafer by the wafer processing unit 20.

[0018] The wafer transfer section 10 includes a placement section 11 on which each wafer is placed, and a transfer section 12 that transfers each wafer. The placement section 11 includes a plurality of placement tables 11a. The transfer section 12 includes a transfer path 12a and a transfer robot 12b.

[0019] The mounting table 11a is used for mounting the cassette 4 in which the upper wafer 1 is accommodated, the cassette 5 in which the lower wafer 2 is accommodated, and the cassette 6 for accommodating the bonded wafer 6. The two cassettes 6 shown in FIG. 2 are the cassette 6 for accommodating a normal bonded wafer 3 and the cassette 6 for accommodating an abnormal bonded wafer 3.

[0020] The transport path 12a extends in the X direction. The transport robot 12b can move on the transport path 12a in the ±X directions and rotate on the transport path 12a in the ±θ directions around the Z direction. The transport robot 12b can transport each wafer between the mounting table 11a located in the -Y direction and the wafer processing unit 20 located in the +Y direction. This allows each wafer to be carried into the housing and carried out to the outside of the housing.

[0021] The wafer processing section 20 includes a transfer block 21 for transferring each wafer, and processing blocks 22, 23, 24, and 25 for processing each wafer. The transfer block 21 includes a transfer robot 21a.

[0022] The transport robot 21a in the transport block 21 can transport each wafer between the wafer transport section 10 and the processing blocks 22 to 25. The processing block 22 moves the upper wafer 1, the lower wafer 2, and the bonded wafer 3 in the ±Z directions. The processing block 23 modifies the surfaces of the upper wafer 1 and the lower wafer 2. The processing block 24 makes the surfaces of the upper wafer 1 and the lower wafer 2 hydrophilic. The processing block 25 bonds the upper wafer 1 and the lower wafer 2 together.

[0023] FIG. 3 is a cross-sectional view showing the configuration of the processing block 25 of the first embodiment.

[0024] The processing block 25 includes a transport area 40 and a bonding area 50, which are separated by an inner wall 25a of the processing block 25. The transport area 40 and the bonding area 50 are connected to each other through an entrance 25b provided in the inner wall 25a. The transport area 40 is an area for transporting each wafer between the inside and outside of the processing block 25. The bonding area 50 is an area for bonding the upper wafer 1 and the lower wafer 2. The bonding area 50 is an example of a bonding section.

[0025] The transport area 40 includes a transport module 41, a position adjustment module 42, and an inversion module 43. The position adjustment module 42 includes a base 42a and a detection unit 42b. The inversion module 43 includes a holding arm 43a, a plurality of holding members 43b, a drive unit 43c, and a support 43d.

[0026] The transport module 41 transports each wafer in the X direction, Y direction, Z direction, etc. Specifically, the transport module 41 transports the upper wafer 1 and the lower wafer 2 from the outside of the bonding area 50 to the inside, and transports the bonded wafer 3 from the inside of the bonding area 50 to the outside.

[0027] The position adjustment module 42 adjusts the orientation of the notch of each wafer. Specifically, the position adjustment module 42 supports the wafer on a base 42a, detects the position of the notch of the wafer on the base 42a with a detector 42b, and rotates the wafer by the base 42a according to the detected position of the notch. This adjusts the orientation of the notch.

[0028] The inversion module 43 inverts the orientation of the upper wafer 1. Specifically, the inversion module 43 holds the upper wafer 1 with a holding member 43b on a holding arm 43a, and inverts the orientation of the upper wafer 1 with the holding arm 43a. The holding arm 43a is supported by a support 43d via a driving unit 43c, and is driven by the driving unit 43c. This inverts the orientation of the upper wafer 1. For example, if the metal pad 1c of the upper wafer 1 before inversion faces the +Z direction, the metal pad 1c of the upper wafer 1 after inversion faces the -Z direction.

[0029] The bonding area 50 includes an upper chuck 51, a lower chuck 52, an upper chuck support part 53, a lower chuck moving part 54, two rails 55 extending in the Y direction, a lower chuck moving part 56, two rails 57 extending in the X direction, and a mounting table 58. The upper chuck support part 53 includes an upper imaging part 53a, a support member 53b, a plurality of supports 53c, and a striker 53d. The lower chuck moving part 54 includes a lower imaging part 54a. The upper chuck support part 53 is an example of a first support part. The lower chuck moving part 54, the rail 55, the lower chuck moving part 56, the rail 57, and the mounting table 58 are examples of a second support part. The striker 53d is an example of a pressing part.

[0030] The upper chuck 51 is supported by an upper chuck support part 53 and holds the upper wafer 1 from above. The upper chuck support part 53 is provided on the ceiling surface of the container of the processing block 25 and supports the upper chuck 51 from above. Specifically, the upper chuck support part 53 supports the upper chuck 51 by a support member 53b, and the support member 53b is supported by a support column 53c. The upper imaging part 53a is provided on the support member 53b and captures an image of the lower wafer 2. This makes it possible to detect the state of the lower wafer 2. The striker 53d is provided on the support member 53b and presses the upper wafer 1. This makes it possible to bond the upper wafer 1 and the lower wafer 2 together.

[0031] The lower chuck 52 is supported by the lower chuck moving part 54, the rail 55, the lower chuck moving part 56, the rail 57, and the mounting table 58, and holds the lower wafer 2 from below. The lower chuck moving part 54, the rail 55, the lower chuck moving part 56, the rail 57, and the mounting table 58 are provided on the floor surface of the container of the processing block 25, and support the lower chuck 52 from below. The lower chuck moving part 54 can move the lower chuck 52 in the ±Y direction by moving on the rail 55 provided on the lower chuck moving part 56. The lower chuck moving part 56 can move the lower chuck 52 in the ±X direction by moving on the rail 57 provided on the mounting table 58. Furthermore, the lower chuck moving part 54 can raise and lower or rotate the lower chuck 52 by moving in the ±Z direction or rotating around an axis parallel to the Z direction. This can increase and decrease the gap between the upper wafer 1 and the lower wafer 2. The lower imaging unit 54a is provided in the lower chuck moving unit 54, and captures an image of the upper wafer 1. This makes it possible to detect the state of the upper wafer 1.

[0032] FIG. 4 is a cross-sectional view showing the configuration of the upper chuck 51 and the like in the first embodiment.

[0033] As shown in FIG. 4, the bonding area 50 of this embodiment further includes a through hole 61, a plurality of suction pipes 62, a plurality of suction pipes 63, an actuator 64, a cylinder 65, a vacuum pump 66, and a vacuum pump 67.

[0034] The through hole 61 penetrates the upper chuck 51 and the support member 53b. The actuator 64 and the cylinder 65 constitute a striker 53d that presses the upper wafer 1. Specifically, the cylinder 65 is provided on the support member 53b. The actuator 64 includes an upper part provided in the cylinder 65 and a lower part provided in the through hole 61. When the upper part of the actuator 64 moves up and down in the cylinder 65, the lower part of the actuator 64 also moves up and down in the through hole 61. As a result, the lower part of the actuator 64 presses the upper wafer 1 held by the upper chuck 51. The striker 53d of this embodiment is driven by air supplied from a regulator (not shown).

[0035] The suction pipes 62, 63 pass through the upper chuck 51 and are used to suck the upper wafer 1. The upper chuck 51 of this embodiment holds the upper wafer 1 by sucking the upper wafer 1 through the suction pipes 62, 63. The vacuum pumps 66, 67 are connected to the suction pipes 62, 63, respectively, and draw the upper wafer 1 by vacuum through the suction pipes 62, 63. The upper wafer 1 is held by this vacuum drawing action. In the bonding area 50 of this embodiment, the vacuum pumps 66 and 67 can be driven independently of each other. The suction pipes 62, 63 and the vacuum pumps 66, 67 are examples of suction units.

[0036] In the bonding area 50 of this embodiment, an upward force can be applied from the suction pipes 62 and 63 to the upper wafer 1, and a downward force can be applied from the actuator 64 (striker 53d) to the upper wafer 1. Further details of these forces will be described later.

[0037] FIG. 5 is a cross-sectional view showing the configuration of the lower chuck 52 and the like in the first embodiment.

[0038] 5(a) and 5(b) show different states of the same lower chuck 52. Details of the lower chuck 52 will be described below with reference to Fig. 5(a). In this description, Fig. 5(b) will also be referred to as appropriate.

[0039] 5(a), the lower chuck 52 of this embodiment includes a base 71, a placement portion 72, a measurement portion 73, a plurality of suction tubes 74, and an air hole 75. The bonding area 50 of this embodiment further includes a vacuum pump 76 and a deformation portion 77 as components for the lower chuck 52. The deformation portion 77 includes a switching valve 77a, a regulator 77b, and a vacuum pump 77c.

[0040] The base 71 supports from below a mounting portion 72 on which the lower wafer 2 is placed. A space S exists between the substrate 71 and the mounting portion 72. The mounting portion 72 has a diameter equal to or greater than the diameter of the lower wafer 2 in a plan view. As shown in FIG. 5(a), the thickness of the mounting portion 72 becomes thicker toward the center of the mounting portion 72 and becomes thinner away from the center of the mounting portion 72. The mounting portion 72 is formed, for example, from a ceramic material.

[0041] The placement portion 72 can be deformed as shown in FIG. 5(a) and FIG. 5(b). The bonding area 50 of this embodiment can deform the lower wafer 2 placed on the placement portion 72 by deforming the placement portion 72. This makes it possible to correct the magnification difference between the upper wafer 1 and the lower wafer 2. The bonding area 50 of this embodiment can correct the misalignment between the metal pads 1c and the metal pads 2c by bonding the upper wafer 1 and the lower wafer 2 together in a state in which the lower wafer 2 is deformed by the placement portion 72. The placement portion 72 shown in FIG. 5(a) has a flat upper surface, and as a result, the shape of the lower wafer 2 is also flat. The placement portion 72 shown in FIG. 5(b) has a curved upper surface that is convex upward, and as a result, the shape of the lower wafer 2 is also curved upward.

[0042] The measuring unit 73 is provided at the center of the base 71, and measures the displacement (deformation) of the mounting unit 72. The suction pipe 74 penetrates the base 71 and the mounting unit 72, and is used to suck the lower wafer 2. The lower chuck 52 of this embodiment holds the lower wafer 2 by sucking the lower wafer 2 through the suction pipe 74. The vacuum pump 76 is connected to the suction pipe 74, and draws the lower wafer 2 by vacuum from the suction pipe 74. The lower wafer 2 is held by this vacuum action.

[0043] The ventilation hole 75 penetrates the base 71 and is used to supply air to the space S and exhaust air from the space S. The deformation portion 77 deforms the placement portion 72 by supplying air to the space S and exhausting air from the space S. Specifically, the deformation portion 77 supplies air to the space S by a regulator 77b and exhausts air from the space S by a vacuum pump 77c. Switching between supplying air and exhausting air is performed by a switching valve 77a.

[0044] 6A to 6D are cross-sectional views showing the operation of the bonding apparatus of the first embodiment. 6A to 6D show how the upper wafer 1 held by the upper chuck 51 and the lower wafer 2 held by the lower chuck 52 are bonded together.

[0045] Fig. 6(a) shows the upper wafer 1 and the lower wafer 2 before the start of bonding. Fig. 6(a) shows a suction force Fa acting on the upper wafer 1 from the suction pipe 62 (Fig. 4) and a suction force Fb acting on the upper wafer 1 from the suction pipe 63 (Fig. 4). At this point, the striker 53d is not in contact with the upper wafer 1, and no pressing force is acting on the upper wafer 1 from the striker 53d.

[0046] FIG. 6(a) further shows the gap G between the upper wafer 1 and the lower wafer 2 before the start of bonding. In this embodiment, the gap G corresponds to the distance between the lower surface of the upper wafer 1 and the upper surface of the lower wafer 2. The gap G shown in FIG. 6(a) is the distance between the center of the upper wafer 1 and the center of the lower wafer 2. The center of the upper wafer 1 is located on the central axis of the upper wafer 1, and the center of the lower wafer 2 is located on the central axis of the lower wafer 2.

[0047] 6(a) may be deformed by the mounting part 72. By bonding the lower wafer 2 in a deformed state, it is possible to correct the magnification difference between the upper wafer 1 and the lower wafer 2.

[0048] When the upper wafer 1 and the lower wafer 2 are bonded together, the vacuum pump 66 (FIG. 4) is stopped to stop the vacuum pumping from the suction pipe 62. After that, the striker 53d presses the upper wafer 1 while the suction pipe 63 sucks the upper wafer 1 (FIG. 6(b)). In this embodiment, the striker 53d presses the center of the upper wafer 1 against the center of the lower wafer 2, and the suction pipe 63 sucks the portions of the upper wafer 1 other than the center. Therefore, the bonding of the upper wafer 1 and the lower wafer 2 progresses from the center of the upper wafer 1 and the lower wafer 2 to the outer periphery. That is, the contact area between the upper wafer 1 and the lower wafer 2 expands from the center of the upper wafer 1 and the lower wafer 2 to the outer periphery.

[0049] The progress of bonding stops after that. This is called the wait state. Figure 6(b) shows the upper wafer 1 and the lower wafer 2 in the wait state.

[0050] When the bonding apparatus of this embodiment reaches a waiting state, the vacuum pump 67 (FIG. 4) is stopped while the striker 53d is pressing the upper wafer 1, and the vacuum pump 67 stops drawing the vacuum from the suction pipe 63. As a result, the upper wafer 1 falls onto the lower wafer 2, and the bonding between the upper wafer 1 and the lower wafer 2 progresses further (FIG. 6(c)).

[0051] In this way, the bonding of the upper wafer 1 and the lower wafer 2 progresses to the ends of the upper wafer 1 and the lower wafer 2, and the bonding is completed (FIG. 6(d)). FIG. 6(d) shows a bonded wafer 3 obtained by bonding the upper wafer 1 and the lower wafer 2 together.

[0052] Here, the operation of the control unit 30 (FIG. 2) of this embodiment will be described.

[0053] Before starting bonding, the control unit 30 measures the value of the amount of warpage of the upper wafer 1. Then, the control unit 30 determines the value of the gap G between the upper wafer 1 and the lower wafer 2 based on the value of the amount of warpage, and determines the value of the pressing force of the striker 53d based on the value of the gap G.

[0054] Before starting the bonding, the control unit 30 controls the gap G between the upper wafer 1 and the lower wafer 2 to the determined value. Then, the control unit 30 controls the operation of the bonding region 50 to bond the upper wafer 1 and the lower wafer 2 together as shown in Figs. 6(a) to 6(d). During this bonding, the control unit 30 controls the pressing force of the striker 53d to the determined value. Also, the gap G between the upper wafer 1 and the lower wafer 2 is set to the determined value at the time when the bonding starts (the time shown in Fig. 6(a)).

[0055] According to this embodiment, by controlling the gap G and the pressing force to these values, it is possible to suitably bond the upper wafer 1 and the lower wafer 2. Further details of such effects will be described later.

[0056] (2) Exposure and lamination (exposure correction) FIG. 7 is a cross-sectional view showing a method of processing the upper wafer 1 in the first embodiment.

[0057] First, an interlayer insulating film 1b is formed on a wafer 1a, and a resist layer 7 is formed on the interlayer insulating film 1b (FIG. 7(a)). Next, the resist layer 7 is patterned by lithography and etching (FIG. 7(b)). As a result, a plurality of recesses H1 are formed in the resist layer 7.

[0058] Next, the pattern of the resist layer 7 is transferred to the interlayer insulating film 1b by etching using the resist layer 7 as a mask (FIG. 7(c)). As a result, a plurality of recesses H2 are formed in the resist layer 7.

[0059] Next, after removing the resist layer 7, a plurality of metal pads 1c are formed in the recesses H2 (FIG. 7(d)). These metal pads 1c are formed, for example, by forming a metal layer, which is the material of these metal pads 1c, on the interlayer insulating film 1b and planarizing the surface of the metal layer by CMP (Chemical Mechanical Polishing).

[0060] In this manner, the upper wafer 1 shown in Fig. 1(a) is manufactured. The lower wafer 2 shown in Fig. 1(b) can also be manufactured by the steps shown in Fig. 7(a) to Fig. 7(d).

[0061] Fig. 8 is a perspective view showing the configuration of an exposure apparatus according to the first embodiment. In this embodiment, exposure for processing the upper wafer 1 and the lower wafer 2 is performed by this exposure apparatus. For example, lithography in the step shown in Fig. 7(b) is performed by this exposure apparatus.

[0062] As shown in Fig. 8, the exposure apparatus of this embodiment includes an illumination optical system 81, a table 82, a projection lens 83, a stage 84, an X-axis interferometer 85, a Y-axis interferometer 86, an off-axis microscope 87, and a control unit 88. Fig. 8 further shows a reticle 8 placed on the table 82, and an upper wafer 1 placed on the stage 84. Instead of the upper wafer 1, a lower wafer 2 may be placed on the stage 84.

[0063] The illumination optical system 81 generates light for exposing the upper wafer 1. The light from the illumination optical system 81 is irradiated onto the reticle 8 on the table 82. The table 82 can scan the reticle 8 with light by moving the reticle 8. The light transmitted through the reticle 8 is incident on the upper wafer 2 on the stage 84 via the projection lens 83. In this manner, the upper wafer 2 is exposed. The X-axis interferometer 85, the Y-axis interferometer 86, and the off-axis microscope 87 are used to observe the state of exposure. The operation of the exposure apparatus of this embodiment is controlled by a control unit 88.

[0064] FIG. 9 is a plan view for explaining exposure correction in the first embodiment.

[0065] FIG. 9(a) shows a plurality of shot areas 9 of the upper wafer 1. When the upper wafer 1 is exposed, exposure is performed for each individual shot area 9. When exposing the shot area 9, the exposure apparatus of this embodiment can perform exposure correction to change the shot area 9 to a shot area 9' as shown in FIG. 9(b) to FIG. 9(d). The exposure correction shown in FIG. 9(b) shifts the shot area 9 to the shot area 9'. The exposure correction shown in FIG. 9(c) enlarges (or reduces) the shot area 9 to the shot area 9'. The exposure correction shown in FIG. 9(d) rotates the shot area 9 to the shot area 9'. According to this embodiment, for example, it is possible to reduce the positional deviation when bonding the upper wafer 1 and the lower wafer 2 by such exposure correction.

[0066] FIG. 10 is a cross-sectional view for explaining exposure correction in the first embodiment.

[0067] FIG. 10(a) shows an upper wafer 1 and a lower wafer 2 bonded together. The upper wafer 1 includes a wafer 1a, an interlayer insulating film 1b, a metal pad 1c, and a wiring layer 1d. The metal pad 1c is formed on the lower surface of the wiring layer 1d. The lower wafer 2 includes a wafer 2a, an interlayer insulating film 2b, a metal pad 2c, and a wiring layer 2d. The metal pad 2c is formed on the upper surface of the wiring layer 2d. This is similar to FIG. 10(b).

[0068] Fig. 10(a) shows the upper wafer 1 and the lower wafer 2 when no exposure correction is performed. In Fig. 10(a), the metal pad 1c is not bonded to the metal pad 2c, even though it should be bonded to the metal pad 2c. In other words, there is a positional deviation between the metal pad 1c and the metal pad 2c.

[0069] FIG. 10(b) shows the upper wafer 1 and the lower wafer 2 when exposure correction is performed. The metal pad 1c in FIG. 10(b) is formed by performing exposure correction during lithography in the process shown in FIG. 7(b). Therefore, the position of the metal pad 1c in FIG. 10(b) is different from the position of the metal pad 1c in FIG. 10(a). As a result, in FIG. 10(b), the metal pad 1c is bonded to the metal pad 2c. Thus, according to this embodiment, the positional deviation between the metal pad 1c and the metal pad 2c can be reduced by exposure correction.

[0070] FIG. 11 is a plan view for explaining exposure correction in the first embodiment.

[0071] FIG. 11 shows a plurality of shot areas 9 of the upper wafer 1, similarly to FIG. 9(a). The arrows shown in FIG. 11 indicate the positional deviation between the ideal shot area 9 and the actual shot area 9 of the upper wafer 1. The ideal shot area 9 corresponds to, for example, a shot area located below the actual shot area 9. The size of the arrow indicates the magnitude of the positional deviation. FIG. 11 is also called an exposure OL (overlay) map. On the other hand, a map relating to the positional deviation when bonding the upper wafer 1 and the lower wafer 2 is called a bonding OL map. In each OL map, a state in which the positional deviation amount is relatively small can be called "good", and a state in which the positional deviation amount is relatively large can be called "deteriorated".

[0072] A general exposure correction is performed so as to reduce the positional deviation between the ideal shot area 9 and the actual shot area 9 of the upper wafer 1. That is, a general exposure correction is performed so that the arrow shown in FIG. 11 becomes smaller on average. On the other hand, the exposure correction of this embodiment is performed so as to reduce the amount of positional deviation when bonding the upper wafer 1 and the lower wafer 2. Therefore, the exposure correction of this embodiment does not need to be performed so that the arrow becomes smaller on average, but may be performed so that the arrow becomes larger on average. This makes it possible to reduce the amount of positional deviation when bonding the upper wafer 1 and the lower wafer 2 even if the amount of positional deviation between the ideal shot area 9 and the actual shot area 9 of the upper wafer 1 increases. In other words, even if the exposure OL map deteriorates, the bonding OL map can be improved. The above-mentioned FIG. 10 shows an example in which the amount of positional deviation when bonding the upper wafer 1 and the lower wafer 2 is reduced.

[0073] (3) Comparative Example FIG. 12 is a schematic diagram showing a flow of exposure and lamination in a comparative example.

[0074] In this comparative example, multiple semiconductor devices are manufactured from a pair of an upper wafer 1 and a lower wafer 2. Hereinafter, such a pair is referred to as a "wafer pair." Fig. 12 shows a flow in which multiple semiconductor devices are manufactured from a wafer pair of a preceding lot, and then multiple semiconductor devices are manufactured from a wafer pair of a succeeding lot.

[0075] First, the upper wafer 1 and the lower wafer 2 of the preceding lot are manufactured. At this time, the upper wafer 1 and the lower wafer 2 are exposed using the exposure apparatus of Fig. 8. For example, exposure when forming the metal pad 1c of the upper wafer 1 and the metal pad 2c of the lower wafer 2 is performed using this exposure apparatus. This exposure is performed so that both the exposure OL map of the upper wafer 1 and the exposure OL map of the lower wafer 2 are good.

[0076] Next, the upper wafer 1 and the lower wafer 2 of the preceding lot are bonded together. At this time, the upper wafer 1 and the lower wafer 2 are bonded together using the bonding device of FIG. 2. As described above, the exposure of the preceding lot is performed so that both the exposure OL map of the upper wafer 1 and the exposure OL map of the lower wafer 2 are good, but this may deteriorate the bonding OL map of the preceding lot. For example, as shown in FIG. 10(a), a positional deviation may occur between the metal pad 1c and the metal pad 2c.

[0077] Therefore, when manufacturing the upper wafer 1 and the lower wafer 2 of the following lot, the exposure correction of the following lot is performed based on the bonding OL map of the preceding lot. For example, the exposure correction of the upper wafer 1 of the following lot is performed so that the bonding OL map of the following lot becomes good. In this case, the exposure of the following lot is performed so that the exposure OL map of the upper wafer 1 becomes worse and the exposure OL map of the lower wafer 2 becomes good. This makes it possible to improve the bonding OL map of the following lot. For example, as shown in FIG. 10(b), it is possible to reduce the positional deviation between the metal pad 1c and the metal pad 2c.

[0078] When manufacturing the upper wafer 1 and the lower wafer 2 of the following lot, the upper wafer 1 and the lower wafer 2 are exposed using the exposure device of FIG. 8. At this time, as described above, the exposure correction of the following lot is performed based on the bonding OL map of the preceding lot. Also, when bonding the upper wafer 1 and the lower wafer 2 of the following lot, the bonding of the upper wafer 1 and the lower wafer 2 is performed using the bonding device of FIG. 2. According to this comparative example, the exposure correction of the following lot makes it possible to improve the bonding OL map of the following lot.

[0079] FIG. 13 is a cross-sectional view for explaining the details of lamination in the comparative example.

[0080] Figures 13(a) to 13(e) show five pairs of upper wafers 1 and lower wafers 2. The upper wafer 1 in Figure 13(a) is significantly warped so as to have an upward convex shape. The upper wafer 1 in Figure 13(b) is slightly warped so as to have an upward convex shape. The upper wafer 1 in Figure 13(c) is not warped. The upper wafer 1 in Figure 13(d) is slightly warped so as to have a downward convex shape. The upper wafer 1 in Figure 13(e) is significantly warped so as to have a downward convex shape. It should be noted that the lower wafer 2 is not warped in any of Figures 13(a) to 13(e).

[0081] Each of Fig. 13(a), Fig. 13(b), Fig. 13(d), and Fig. 13(e) shows the amount of warpage W of the upper wafer 1. Here, the magnitude of the amount of warpage W is the maximum protrusion amount of the upper wafer 1 relative to the edge of the upper wafer 1. For example, in Fig. 13(a), the center of the upper wafer 1 protrudes the most in the +Z direction relative to the edge of the upper wafer 1, and the amount of warpage W is the difference between the Z coordinate of the center of the upper wafer 1 and the Z coordinate of the edge of the upper wafer 1. This is similar to Fig. 13(b), Fig. 13(d), and Fig. 13(e). The value of the amount of warpage W is defined to be negative in Fig. 13(a) and Fig. 13(b), zero in Fig. 13(c), and positive in Fig. 13(d) and Fig. 13(e). 13(a) to 13(e), the amount of warping W in Fig. 13(a) is the smallest, and the amount of warping W in Fig. 13(e) is the largest. The magnitude (absolute value) of the amount of warping W is large in Fig. 13(a) and Fig. 13(e), and small in Fig. 13(b) and Fig. 13(d).

[0082] The bonding OL map of the upper wafer 1 and the lower wafer 2 changes depending on the warpage W of the upper wafer 1. The reason is that in the bonding process shown in FIG. 6(b), the stress acting on the upper wafer 1 from the upper chuck 51 changes depending on the warpage W of the upper wafer 1.

[0083] FIG. 14 is a schematic diagram showing a flow of exposure and lamination in a comparative example.

[0084] FIG. 14, like FIG. 12, shows a flow in which a plurality of semiconductor devices are manufactured from a wafer pair of a preceding lot, and then a plurality of semiconductor devices are manufactured from a wafer pair of a succeeding lot.

[0085] First, the upper wafer 1 and the lower wafer 2 of the preceding lot are manufactured. At this time, the upper wafer 1 and the lower wafer 2 are exposed so that the exposure OL maps of both the upper wafer 1 and the lower wafer 2 are good.

[0086] Next, the upper wafer 1 and the lower wafer 2 of the preceding lot are bonded together. As described above, the exposure of the preceding lot is performed so that the exposure OL map of the upper wafer 1 and the exposure OL map of the lower wafer 2 are both good, but this may deteriorate the bonding OL map of the preceding lot.

[0087] Therefore, when manufacturing the upper wafer 1 and the lower wafer 2 of the following lot, the exposure correction of the upper wafer 1 of the following lot is performed based on the bonding OL map of the preceding lot. In this case, the exposure of the following lot is performed so that the exposure OL map of the upper wafer 1 deteriorates and the exposure OL map of the lower wafer 2 improves. This makes it possible to improve the bonding OL map of the following lot.

[0088] In this case, the warpage amount W of the upper wafer 1 of the preceding lot becomes an issue. FIG. 14 shows upper wafers 1 with negative, zero, and positive warpage amounts W as examples of the upper wafer 1 of the preceding lot. For example, when the warpage amount W of the upper wafer 1 of the preceding lot is zero, the exposure correction of the upper wafer 1 of the following lot is suitable for the upper wafer 1 with zero warpage amount W. Therefore, when the warpage amount W of the upper wafer 1 of the following lot is zero, the exposure correction of the upper wafer 1 of the following lot makes the bonding OL map of the following lot good. However, when the warpage amount W of the upper wafer 1 of the following lot is not zero, the exposure correction of the upper wafer 1 of the following lot may not make the bonding OL map of the following lot good.

[0089] Therefore, in this embodiment, not only exposure correction but also bonding correction is performed on the following wafer. This makes it possible to address the problem of the warpage amount W of the upper wafer 1. The bonding correction in this embodiment is performed by controlling the value of the gap G between the upper wafer 1 and the lower wafer 2, as described in the description of FIG. 6. Further details of the bonding correction will be described later.

[0090] (4) Pasting correction FIG. 15 is a cross-sectional view for explaining details of bonding in the first embodiment.

[0091] 15(a) to 15(e) show five pairs of upper wafers 1 and lower wafers 2, similar to FIGS. 13(a) to 13(e). The upper wafer 1 in FIG. 15(a) is significantly warped to form an upward convex shape. The upper wafer 1 in FIG. 15(b) is slightly warped to form an upward convex shape. The upper wafer 1 in FIG. 15(c) is not warped. The upper wafer 1 in FIG. 15(d) is slightly warped to form a downward convex shape. The upper wafer 1 in FIG. 15(e) is significantly warped to form a downward convex shape. The lower wafer 2 is not warped in any of FIGS. 15(a) to 15(e).

[0092] 15(a) to 15(e) further show a gap G between the upper wafer 1 and the lower wafer 2. The gap G in this embodiment is the distance between the center of the upper wafer 1 and the center of the lower wafer 2. The bonding correction in this embodiment is performed by controlling the value of this gap G.

[0093] FIG. 16 is a graph for explaining the bonding correction according to the first embodiment.

[0094] In FIG. 16(a), the horizontal axis indicates the warpage W of the upper wafer 1, and the vertical axis indicates the 3σ value of the bonding OL map of the upper wafer 1 and the lower wafer 2. Here, σ represents the standard deviation of the X component (or Y component) of the arrow in the bonding OL map. Also, the 3σ value represents the variation of the X component (or Y component) with respect to the arrow in the bonding OL map. In this embodiment, the larger the warpage W, the larger the 3σ value of the bonding OL map. Therefore, as the warpage W increases, the bonding OL map deteriorates, and as the warpage W decreases, the bonding OL map improves.

[0095] In FIG. 16(b), the horizontal axis indicates the gap G between the upper wafer 1 and the lower wafer 2 before bonding begins (see FIG. 6(a)), and the vertical axis indicates the 3σ value of the bonding OL map of the upper wafer 1 and the lower wafer 2. In this embodiment, the larger the gap G, the larger the 3σ value of the bonding OL map. Therefore, as the gap G increases, the bonding OL map deteriorates, and as the gap G decreases, the bonding OL map improves.

[0096] FIG. 17 is a graph for explaining the bonding correction according to the first embodiment.

[0097] In Fig. 17(a), the horizontal axis indicates the amount of warpage W of the upper wafer 1, and the vertical axis indicates the gap G between the upper wafer 1 and the lower wafer 2 before bonding begins. Bonding correction in this embodiment is performed as shown in Fig. 17(a). That is, bonding correction in this embodiment is performed such that the gap G becomes smaller as the amount of warpage W increases. In Fig. 17(a), the gap G decreases as the amount of warpage W increases.

[0098] FIG. 17(b) shows the relationship between the warpage amount W and the 3σ value when the bonding correction shown in FIG. 17(a) is performed. In this case, even if the warpage amount W of the upper wafer 1 varies, the 3σ value of the bonding OL map of the upper wafer 1 and the lower wafer 2 is constant. Therefore, according to this embodiment, by performing the bonding correction shown in FIG. 17(a), it is possible to suppress the influence of the warpage amount W on the bonding OL map. As a result, it is possible to improve the bonding OL map even when the upper wafer 1 is warped.

[0099] FIG. 18 is a schematic diagram showing a flow of exposure and lamination in the first embodiment.

[0100] 18, like FIGS. 12 and 14, shows a flow in which a plurality of semiconductor devices are manufactured from a wafer pair of a preceding lot, and then a plurality of semiconductor devices are manufactured from a wafer pair of a succeeding lot.

[0101] First, the upper wafer 1 and the lower wafer 2 of the preceding lot are manufactured. At this time, the upper wafer 1 and the lower wafer 2 are exposed using the exposure apparatus of Fig. 8. For example, exposure when forming the metal pad 1c of the upper wafer 1 and the metal pad 2c of the lower wafer 2 is performed using this exposure apparatus. This exposure is performed so that both the exposure OL map of the upper wafer 1 and the exposure OL map of the lower wafer 2 are good.

[0102] Next, the upper wafer 1 and the lower wafer 2 of the preceding lot are bonded together. At this time, the upper wafer 1 and the lower wafer 2 are bonded together using the bonding device of FIG. 2. As described above, the exposure of the preceding lot is performed so that both the exposure OL map of the upper wafer 1 and the exposure OL map of the lower wafer 2 are good, but this may deteriorate the bonding OL map of the preceding lot. For example, as shown in FIG. 10(a), a positional deviation may occur between the metal pad 1c and the metal pad 2c.

[0103] Therefore, when manufacturing the upper wafer 1 and the lower wafer 2 of the following lot, the exposure correction of the following lot is performed based on the bonding OL map of the preceding lot. For example, the exposure correction of the upper wafer 1 of the following lot is performed so that the bonding OL map of the following lot becomes good. In this case, the exposure of the following lot is performed so that the exposure OL map of the upper wafer 1 becomes worse and the exposure OL map of the lower wafer 2 becomes good. This makes it possible to improve the bonding OL map of the following lot. For example, as shown in FIG. 10(b), it is possible to reduce the positional deviation between the metal pad 1c and the metal pad 2c.

[0104] In this case, the warpage amount W of the upper wafer 1 of the preceding lot becomes an issue. FIG. 18 shows upper wafers 1 with negative, zero, and positive warpage amounts W as examples of the upper wafer 1 of the preceding lot. For example, when the warpage amount W of the upper wafer 1 of the preceding lot is zero, the exposure correction of the upper wafer 1 of the following lot is suitable for the upper wafer 1 with zero warpage amount W. Therefore, when the warpage amount W of the upper wafer 1 of the following lot is zero, the exposure correction of the upper wafer 1 of the following lot makes the bonding OL map of the following lot good. However, when the warpage amount W of the upper wafer 1 of the following lot is not zero, the exposure correction of the upper wafer 1 of the following lot may not make the bonding OL map of the following lot good.

[0105] Therefore, when bonding the upper wafer 1 and the lower wafer 2 of the following lot, bonding correction of the following lot is performed based on the warpage W of the upper wafer 1 of the following lot. For example, bonding correction of the following lot is performed so that the above-mentioned gap G becomes smaller as the warpage W increases. This makes it possible to improve the bonding OL map of the following lot even when the upper wafer 1 of the following lot is warped.

[0106] When manufacturing the upper wafer 1 and the lower wafer 2 of the following lot, the exposure of the upper wafer 1 and the lower wafer 2 is performed using the exposure device of FIG. 8. At this time, as described above, the exposure correction of the following lot is performed based on the bonding OL map of the preceding lot. Also, when bonding the upper wafer 1 and the lower wafer 2 of the following lot, the bonding of the upper wafer 1 and the lower wafer 2 is performed using the bonding device of FIG. 2. At this time, as described above, the bonding correction of the following lot is performed based on the warpage amount W of the upper wafer 1 of the following lot. According to this embodiment, even if the upper wafer 1 of the following lot is warped, the exposure correction and bonding correction of the following lot make it possible to improve the bonding OL map of the following lot.

[0107] In addition, the exposure correction in this embodiment is performed with common contents for all wafer pairs of the following lot. The reason is that the bonding OL map of the preceding lot used for the exposure correction is common to all wafer pairs of the following lot. On the other hand, the bonding correction in this embodiment is performed with individual contents for these wafer pairs of the following lot. The reason is that the warpage W of the upper wafer 1 of the following lot is different for each wafer pair of the following lot. However, the relational expression between the warpage W and the gap G in this embodiment is common to all wafer pairs of the following lot. This relational expression is given in the form of, for example, FIG. 17(a). Details of this relational expression will be described later.

[0108] FIG. 19 is a table for explaining the bonding correction according to the first embodiment.

[0109] 19 shows the 3σ value of the bonding OL map when the warpage W of the upper wafer 1 is a predetermined value and the gap G between the upper wafer 1 and the lower wafer 2 is set to a predetermined value when bonding the upper wafer 1 and the lower wafer 2. For example, when the warpage W is −40 μm and the gap G is set to 60 μm, the 3σ value is 70 nm.

[0110] The 3σ value shown in Fig. 19 is 100 nm under the center condition. Specifically, the 3σ value shown in Fig. 19 is 100 nm when the warpage W is -20 μm and the gap G is set to 100 μm.

[0111] The bonding correction in this embodiment is performed so that the 3σ value is 100 nm. For example, when the warpage amount W is −40 μm, the gap G is set to 120 μm. In FIG. 19, the columns where the 3σ value is 100 nm are indicated by thick lines. These columns correspond to the straight lines shown in FIG. 17(a).

[0112] FIG. 20 is a flowchart showing a method for manufacturing the semiconductor device of the first embodiment.

[0113] 20(a) shows a flow of exposure and lamination of the preceding lot. This exposure and lamination is performed using the exposure device in FIG. 8 and the lamination device in FIG.

[0114] First, a plurality of upper wafers 1 are manufactured from a plurality of wafers 1a. At this time, when forming a plurality of metal pads 1c above each wafer 1a, exposure is performed using an exposure device (step S11). In this embodiment, these upper wafers 1 are manufactured to have different warpage amounts W from each other. Each upper wafer 1 may be warped due to the warpage of the original wafer 1a, or may be warped due to the influence of the metal pads 1c. The same applies to each lower wafer 2.

[0115] Next, a plurality of lower wafers 2 are manufactured from the plurality of wafers 2a. At this time, when forming a plurality of metal pads 2c above each wafer 2a, exposure is performed using an exposure device (step S12). In this embodiment, these lower wafers 2 are manufactured to have the same amount of warpage.

[0116] Next, the upper wafer 1 and the lower wafer 2 are bonded together for each wafer pair by a bonding device to manufacture a plurality of bonded wafers 3 (step S13). In this case, the gap G between the upper wafer 1 and the lower wafer 2 before bonding is started is set to the same value for all wafer pairs.

[0117] Next, the bonding OL of these bonded wafers 3 is measured (step S14). Next, from the measurement data of the bonding OL of these bonded wafers 3, the value of a predetermined coefficient of polynomial regression (K value) is extracted (step S15). For example, the values ​​of two coefficients K17 and K18 of the polynomial regression are extracted. Next, using the warpage W of the upper wafer 1 in these bonded wafers 3 and the K value extracted from these bonded wafers 3, a relational expression between the K value and the warpage W is created (step S16). The processing of steps S14 to S16 may be automatically performed by a device such as a sensor or a computer. In this way, the relational expression between the K value and the warpage W in this embodiment is created by actually performing exposure and bonding.

[0118] In the flow of the subsequent lot (FIG. 20(d)) described later, before the upper wafer 1 is exposed, a value of a position correction amount that is an amount by which the exposure position of the upper wafer 1 can be corrected is determined. An example of the position correction amount is a polynomial regression coefficient (e.g., K17, K18). In this embodiment, it is possible to correct the exposure position of the upper wafer 1 by correcting the value of the polynomial regression coefficient for the upper wafer 1. Then, when the upper wafer 1 is exposed, the position correction amount is controlled to the determined value. In this manner, the exposure correction of the upper wafer 1 is performed.

[0119] The number of coefficients of the polynomial regression used as the position correction amount may be any number equal to or greater than one. The position correction amount may be something other than the coefficients of the polynomial regression, for example, it may be one or more coefficients of a Zernike polynomial. The coefficients of the polynomial regression or Zernike polynomial can be used not only to correct the exposure position of the upper wafer 1, but also to correct the bonding position of the upper wafer 1 relative to the lower wafer 2.

[0120] 20(b) shows another flow of exposure and lamination of the preceding lot, which is performed using the exposure apparatus of FIG. 8 and the lamination apparatus of FIG.

[0121] First, a plurality of upper wafers 1 and a plurality of lower wafers 2 are manufactured, and these upper wafers 1 and lower wafers 2 are bonded together for each wafer pair by a bonding device to manufacture a plurality of bonded wafers 3 (step S21). In this case, the gap G between the upper wafer 1 and the lower wafer 2 before the start of bonding is set to a different value for each wafer pair. In addition, these upper wafers 1 are manufactured to have the same amount of warpage W. Similarly, these lower wafers 2 are manufactured to have the same amount of warpage.

[0122] Next, the bonding OL of these bonded wafers 3 is measured (step S21). Next, from the measurement data of the bonding OL of these bonded wafers 3, the value of a predetermined coefficient of polynomial regression (K value) is extracted (step S22). For example, the values ​​of two coefficients K17 and K18 of the polynomial regression are extracted. Next, using the above-mentioned gap G for these bonded wafers 3 and the K value extracted from these bonded wafers 3, a relational expression between the K value and the gap G is created (step S23). The processes of steps S22 to S24 may be automatically performed by a device such as a sensor or a computer. In this way, the relational expression between the K value and the gap G in this embodiment is created by actually performing exposure and bonding.

[0123] FIG. 20(c) shows a flow for setting a recipe for a subsequent lot based on a preceding lot.

[0124] First, a relationship table between the amount of warpage W and the gap G is created (step S31) using the relational expression between the K value and the amount of warpage W created in step S16 and the relational expression between the K value and the gap G created in step S24. As a result, a table such as that shown in FIG. 19 is created.

[0125] Next, the center conditions in the relationship table are set in the recipe (step S32). The center conditions are as described with reference to FIG.

[0126] Next, a relational expression between the warpage amount W and the gap G is created based on the relational table and the center conditions (step S33). For example, as shown by the thick line in FIG. 19, this relational expression is created so that when the warpage amount W and the gap G satisfy this relational expression, the 3σ value becomes 100 nm. According to this embodiment, by using this relational expression determined in advance, it becomes possible to perform bonding correction. The processes of steps S31 to S33 may be performed manually by a person or automatically by a device such as a computer.

[0127] 20(d) shows a flow of exposure and lamination of the subsequent lot. This exposure and lamination is performed using the exposure device of FIG. 8 and the lamination device of FIG.

[0128] First, the upper wafer 1 is manufactured from the wafer 1a. At this time, when forming a plurality of metal pads 1c above the wafer 1a, exposure is performed using an exposure device (step S41). During this exposure, exposure correction is performed based on the bonding OL map of the preceding lot. This exposure correction is performed, for example, in the manner described with reference to FIG. 18. Also, this exposure correction is controlled, for example, by the control unit 88 in the exposure device.

[0129] Next, the lower wafer 2 is manufactured from the wafer 2a. At this time, when forming a plurality of metal pads 2c above the wafer 2a, exposure is performed using an exposure device (step S42).

[0130] Next, the value of the amount of warpage W of the upper wafer 1 is measured (step S43). The value of the amount of warpage W is measured by, for example, a bonding device under the control of the control unit 30.

[0131] Next, based on the relational expression created in step S33, the value of the gap G is calculated from the value of the amount of warpage W measured in step S43 (step S44). The calculation of the value of the gap G is performed, for example, by the control unit 30. In this case, the above relational expression may be stored in advance in the storage of the bonding device, or may be stored in advance in the storage of a device with which the bonding device can communicate.

[0132] Next, the upper wafer 1 and the lower wafer 2 are bonded together by a bonding device to produce a bonded wafer 3 (step S45). At this time, the gap G between the upper wafer 1 and the lower wafer 2 before the start of bonding is set to the value calculated in step S44. In this manner, bonding correction is performed based on the warpage amount W of the upper wafer 1. This bonding correction is controlled by, for example, the control unit 30.

[0133] FIG. 21 is a block diagram showing the functional configuration of the control unit 30 in the first embodiment.

[0134] 21, the control unit 30 includes a relational equation management unit 91, a warpage amount measurement unit 92, a gap determination unit 93, a pressing force determination unit 94, and a bonding control unit 95. Each of these functional blocks (91 to 95) may be realized by hardware or software.

[0135] The relational equation management unit 91 manages the relational equation between the warpage amount W and the gap G. Before step S44 is performed, the relational equation management unit 91 obtains this relational equation from a storage. This storage may be provided in the bonding device, or may be provided in a device with which the bonding device can communicate.

[0136] In step S43, the warpage measurement unit 92 measures the value of the warpage W of the upper wafer 1. For example, the warpage measurement unit 92 measures the value of the warpage W of the upper wafer 1 by controlling a measuring device provided in the bonding device.

[0137] In step S44, the gap determination unit 93 determines the value of the gap G based on the value of the amount of warpage W. For example, the gap determination unit 93 calculates the value of the gap G from the value of the amount of warpage W measured by the amount of warpage measurement unit 92 based on the relational equation managed by the relational equation management unit 91.

[0138] Before step S45 is performed, the pressing force determination unit 94 determines the value of the pressing force with which the striker 53d presses the upper wafer 1, based on the value of the gap G. For example, the value of the pressing force is determined so that the pressing force increases as the gap G increases. In this case, when the value of the gap G determined by the gap determination unit 93 is small, the value of the pressing force is determined to be small. On the other hand, when the value of the gap G determined by the gap determination unit 93 is large, the value of the pressing force is determined to be large. According to the present embodiment, by determining the value of the pressing force in this manner, it is possible to press the upper wafer 1 with an appropriate pressing force.

[0139] The bonding control unit 95 controls bonding and bonding correction in step S45. For example, before the start of bonding, the bonding control unit 95 controls the gap G between the upper wafer 1 and the lower wafer 2 to a value determined by the gap determination unit 93. In addition, the bonding control unit 95 controls the pressing force with which the striker 53d presses the upper wafer 1 during bonding to a value determined by the pressing force determination unit 94. This makes it possible to perform bonding and bonding correction in an optimal manner.

[0140] These functional blocks are realized, for example, by a computer program that causes a processor in the control unit 30 to execute these processes. In this case, the control unit 30 is provided with a computer-readable recording medium on which this program is installed. The whole or part of this program may be downloaded to the recording medium from a network.

[0141] 22A to 22C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to a modification of the first embodiment.

[0142] 22 shows gap G1 and gap G2 as examples of gap G. Gap G1 is a gap between the center of upper wafer 1 and the center of lower wafer 2. Gap G2 is a gap between a portion other than the center of upper wafer 1 and a portion other than the center of lower wafer 2. In this way, gap G in this embodiment may be defined at the centers of upper wafer 1 and lower wafer 2, or may be defined at a portion other than the centers of upper wafer 1 and lower wafer 2.

[0143] As described above, the control unit 30 of this embodiment determines the value of the gap G between the upper wafer 1 and the lower wafer 2 based on the value of the warpage W of the upper wafer 1, and controls the gap G to the determined value before bonding the upper wafer 1 and the lower wafer 2 together. Therefore, according to this embodiment, even if the upper wafer 1 has warpage, the upper wafer 1 and the lower wafer 2 can be bonded together appropriately. For example, even if the upper wafer 1 has warpage when performing exposure correction of the upper wafer 1, it is possible to achieve appropriate bonding by correcting the bonding of the upper wafer 1 and the lower wafer 2.

[0144] Although several embodiments have been described above, these embodiments are presented only as examples and are not intended to limit the scope of the invention. The novel device and method described in this specification can be implemented in various other forms. In addition, various omissions, substitutions, and modifications can be made to the forms of the device and method described in this specification without departing from the spirit of the invention. The appended claims and their equivalents are intended to include such forms and modifications that fall within the scope and spirit of the invention. [Explanation of symbols]

[0145] 1: upper wafer, 1a: wafer, 1b: interlayer insulating film, 1c: metal pad, 1d: wiring layer, 2: lower wafer, 2a: wafer, 2b: interlayer insulating film, 2c: metal pad, 2d: wiring layer, 3: bonded wafer, 4: cassette, 5: cassette, 6: cassette, 7: resist layer, 8: reticle, 9: shot area, 9': shot area, 10: wafer transport section, 11: placement section, 11a: placement table, 12: conveying section, 12a: conveying path, 12b: conveying robot, 20: wafer processing section, 21: transport block, 21a: transport robot, 22: processing block, 23: processing block, 24: processing block, 25: processing block, 25a: inner wall, 25b: entrance / exit, 30: control unit, 40: conveying area, 41: conveying module, 42: position adjustment module, 42a: base, 42b: detector, 43: inversion module, 43a: holding arm, 43b: holding member, 43c: driving part, 43d: support, 50: bonding area, 51: upper chuck, 52: lower chuck, 53: upper chuck support portion, 53a: upper imaging unit, 53b: support member, 53c: support column, 53d: striker, 54: lower chuck moving part, 54a: lower imaging part, 55: rail, 56: Lower chuck moving part, 57: Rail, 58: Placement table, 61: through hole, 62: suction tube, 63: suction tube, 64: actuator, 65: cylinder, 66: vacuum pump, 67: vacuum pump, 71: base, 72: placement part, 73: measurement part, 74: suction tube, 75: vent hole, 76: vacuum pump, 77: deformation portion, 77a: switching valve, 77b: regulator, 77c: vacuum pump, 81: illumination optical system, 82: table, 83: projection lens, 84: stage, 85: X-axis interferometer, 86: Y-axis interferometer, 87: off-axis microscope, 88: control unit, 91: relational expression management unit, 92: warpage amount measurement unit, 93: gap determination unit, 94: pressing force determination unit, 95: bonding control unit

Claims

1. a warpage measurement unit that measures the value of the warpage of the first substrate or the second substrate; a gap determination unit that determines a value of a gap between the first substrate and the second substrate based on the value of the amount of warping; a bonding control unit that controls the gap to the determined value before bonding the first substrate and the second substrate; A semiconductor manufacturing apparatus comprising:

2. 2 . The semiconductor manufacturing apparatus according to claim 1 , wherein the gap determination unit determines the value of the gap based on the value of the amount of warpage by using a relational expression between the amount of warpage and the gap that is determined in advance.

3. The semiconductor manufacturing apparatus according to claim 1 , wherein the gap determination unit determines a value of the gap such that the gap decreases as the amount of warpage increases.

4. The semiconductor manufacturing apparatus according to claim 1 , wherein the gap determination unit determines a value of the gap between a center portion of the first substrate and a center portion of the second substrate.

5. a pressing force determination unit that determines a value of a pressing force for pressing the first substrate or the second substrate based on the value of the gap, The semiconductor manufacturing apparatus according to claim 1 , wherein the bonding control unit controls the pressing force to the determined value when bonding the first substrate and the second substrate together.

6. The semiconductor manufacturing apparatus according to claim 5 , wherein the pressing force determination unit determines a value of the pressing force used to press the center portion of the first substrate or the second substrate.

7. 6. The semiconductor manufacturing apparatus according to claim 5, wherein the pressing force determination unit determines a value of the pressing force used to press the first substrate, and the warpage measurement unit measures a value of the warpage of the first substrate.

8. The semiconductor manufacturing apparatus according to claim 1 , further comprising a bonding unit that is controlled by the bonding control unit and bonds the first substrate and the second substrate together.

9. 9. The semiconductor manufacturing apparatus according to claim 8, wherein the bonding section comprises a suction section that sucks the first substrate, and a pressing section that presses the first substrate with the pressing force.

10. the bonding unit includes a first support unit that supports a chuck that holds the first substrate, and a second support unit that supports a chuck that holds the second substrate, The semiconductor manufacturing apparatus according to claim 8 , wherein the gap is controlled to the determined value by the bonding control section controlling the first support section or the second support section.

11. measuring the amount of warping of the first substrate or the second substrate; determining a gap value between the first substrate and the second substrate based on the warpage value; controlling the gap to the determined value before bonding the first substrate and the second substrate together; A method for manufacturing a semiconductor device comprising the steps of:

12. The method for manufacturing a semiconductor device according to claim 11 , wherein the value of the gap is determined based on the value of the amount of warpage by using a relational expression between the amount of warpage and the gap that is determined in advance.

13. The method for manufacturing a semiconductor device according to claim 11 , wherein a value of the gap is determined such that the gap decreases as the amount of warpage increases.

14. determining a value of a pressing force for pressing the first substrate or the second substrate based on the value of the gap; The method for manufacturing a semiconductor device according to claim 11 , wherein the pressing force is controlled to the determined value when the first substrate and the second substrate are bonded together.

15. The method for manufacturing a semiconductor device according to claim 11 , further comprising bonding the first substrate and the second substrate together while controlling the gap to the determined value.

16. determining a position correction amount value that is an amount by which an exposure position of the first substrate or the second substrate can be corrected before exposing the first substrate or the second substrate; controlling the amount of position correction to the determined value when exposing the first substrate or the second substrate; Further including: The method for manufacturing a semiconductor device according to claim 11 , wherein the first substrate and the second substrate are bonded together after the first substrate or the second substrate is exposed to light.

17. the value of the gap is determined based on the value of the amount of warpage by using a relational expression between the amount of warpage and the gap that is determined in advance; the relational expression between the warp amount and the gap is created based on a relational expression between the warp amount and the position correction amount and a relational expression between the gap and the position correction amount; The method for manufacturing a semiconductor device according to claim 16.

18. 18. The method for manufacturing a semiconductor device according to claim 17, wherein the relational expressions between the amount of warpage and the amount of positional correction and the relational expressions between the gap and the amount of positional correction are created by actually performing exposure and lamination.

19. The method of manufacturing a semiconductor device according to claim 16 , wherein the position correction amount is a coefficient of a polynomial regression.

20. The method for manufacturing a semiconductor device according to claim 16, wherein the position correction amount is a coefficient of a Zernike polynomial.

Citation Information

Patent Citations

  • Semiconductor device manufacturing apparatus and semiconductor device manufacturing method

    JP2013258377A

  • Bonding device and bonded substrate manufacturing method

    JP2014209571A

  • Distortion detection method, exposure equipment, exposure method, and device manufacturing method

    JP2017049456A

  • Lamination apparatus, activation apparatus, control apparatus, laminate manufacturing apparatus, and laminate manufacturing method

    JP2019129286A

  • Substrate bonding apparatus

    US20190189593A1