Semiconductor device and method for manufacturing semiconductor device

The semiconductor device addresses gate electrode defects by using a gate electrode with a thicker oxide layer at the lower end and controlled sacrificial layer impurities, ensuring complete filling and uniformity, thereby stabilizing transistor characteristics and improving manufacturing precision.

JP2024132564AInactive Publication Date: 2024-10-01KIOXIA CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023043382
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-17
Publication Date
2024-10-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Defects in gate electrode formation, such as residual sacrificial layers and incomplete filling of conductive layers, occur during the replacement process in semiconductor devices, leading to voids and inconsistent gate lengths.

Method used

The semiconductor device incorporates a gate electrode with a specific configuration, including an oxide layer and a nitride layer that cover the sidewalls, where the oxide layer is thicker at the lower end and has a wider upper end, and utilizes sacrificial layers with controlled impurity content and oxidation rates to ensure complete filling and uniformity.

Benefits of technology

This configuration suppresses formation defects, stabilizes transistor characteristics, and ensures precise gate length by preventing residual sacrificial layer remnants and voids, enhancing manufacturing controllability and transistor performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024132564000001_ABST
    Figure 2024132564000001_ABST
Patent Text Reader

Abstract

To prevent a failure in formation of a gate electrode.SOLUTION: A semiconductor device of an embodiment comprises a gate electrode, an oxidized layer covering a side wall of the gate electrode, and a nitrided layer covering a side wall of the gate electrode with the oxidized layer therebetween. The gate electrode is a single body of a conductive layer having a larger width at an upper end than at a lower end. The oxidized layer is thicker at a portion covering the lower end of the gate electrode than at a portion covering the upper end of the gate electrode.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE The present invention relates to a semiconductor device and a method for manufacturing the same. [Background technology]

[0002] In semiconductor devices including CMOS transistors, the gate electrode may be formed using a replacement technique. According to the replacement technique, a temporary electrode structure formed from a sacrificial layer such as a polysilicon layer is used for positioning, and impurities are diffused into the substrate. Then, a nitride layer or the like is formed to cover the electrode structure, and the sacrificial layer is removed, and the gap generated in the nitride layer is filled with a conductive layer such as a metal layer to form the gate electrode.

[0003] However, there are cases where defects in the formation of the gate electrode occur, such as the sacrificial layer remaining in the gap or the conductive layer not being completely filled into the gap, resulting in voids. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] US Patent Application Publication No. 2005 / 0214987 [Patent Document 2] US Patent Application Publication No. 2005 / 0269644 Summary of the Invention [Problem to be solved by the invention]

[0005] An object of one embodiment is to provide a semiconductor device and a method for manufacturing the semiconductor device that can suppress defective formation of a gate electrode. [Means for solving the problem]

[0006] A semiconductor device according to an embodiment includes a gate electrode, an oxide layer covering a sidewall of the gate electrode, and a nitride layer covering the sidewall of the gate electrode via the oxide layer, the gate electrode being a single conductive layer having an upper end wider than a lower end, and the oxide layer is thicker in a portion covering the lower end of the gate electrode than in a portion covering the upper end of the gate electrode. [Brief description of the drawings]

[0007] [Figure 1] 1 is a cross-sectional view showing an example of the configuration of a semiconductor device according to a first embodiment. [Diagram 2] 1A to 1C are cross-sectional views illustrating a part of a procedure of the method for manufacturing the semiconductor device according to the first embodiment in order. [Diagram 3] 1A to 1C are cross-sectional views illustrating a part of a procedure of the method for manufacturing the semiconductor device according to the first embodiment in order. [Figure 4] 1A to 1C are cross-sectional views illustrating a part of a procedure of a manufacturing method of a semiconductor device according to a comparative example. [Diagram 5] 4 is a graph showing the relationship between the thickness and the impurity concentration of a silicon oxide layer formed by an oxidation treatment used in the method for manufacturing a semiconductor device according to the first embodiment. [Figure 6] FIG. 2 is a cross-sectional view showing an example of the configuration of a semiconductor device according to Modification 1 of Embodiment 1. [Figure 7] 5A to 5C are cross-sectional views illustrating a part of a procedure of a method for manufacturing a semiconductor device according to a first modification of the first embodiment. [Figure 8] FIG. 11 is a cross-sectional view showing another example of the configuration of the semiconductor device according to Modification 1 of Embodiment 1. [Figure 9] FIG. 11 is a cross-sectional view showing still another example of the configuration of the semiconductor device according to Modification 1 of Embodiment 1. [Figure 10] FIG. 11 is a cross-sectional view showing an example of the configuration of a semiconductor device according to Modification 2 of Embodiment 1. [Figure 11] 10A to 10C are cross-sectional views illustrating a part of a procedure of a method for manufacturing a semiconductor device according to Modification 2 of Embodiment 1. [Figure 12] FIG. 11 is a cross-sectional view showing an example of the configuration of a semiconductor device according to a second embodiment. [Figure 13]10A to 10C are cross-sectional views illustrating a part of a procedure of a method for manufacturing a semiconductor device according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] The present invention will be described in detail below with reference to the drawings. Note that the present invention is not limited to the following embodiments. In addition, the components in the following embodiments include those that a person skilled in the art can easily imagine or that are substantially the same.

[0009] [Embodiment 1] Hereinafter, the first embodiment will be described in detail with reference to the drawings.

[0010] (Configuration of Semiconductor Device) 1 is a cross-sectional view showing an example of the configuration of a semiconductor device 100 according to embodiment 1. In this specification, the surface of a substrate 110 on which a transistor 10 (described later) and the like are formed is defined as the upper surface, and the connection end of a contact CG connected to a gate electrode 150 of the transistor 10 is defined as being on the lower side of the semiconductor device 1 in the extension direction of the contact CG.

[0011] In the drawings below, the X direction and the Y direction are both directions along the upper surface of the substrate 110 and are perpendicular to each other. In this specification, the extension direction of the gate electrode 150 described below may also be referred to as the first direction. The first direction is, for example, the direction along the Y direction. In this specification, the direction along the gate length L that intersects with the extension direction of the gate electrode 150 may also be referred to as the second direction. The second direction is, for example, the direction along the X direction.

[0012] As shown in FIG. 1, the semiconductor device 100 includes a transistor 10, an interlayer insulating layer 160, and contacts CG and CS, which are provided on a substrate 110.

[0013] The substrate 110 is a semiconductor substrate such as a silicon substrate. A predetermined conductive type of impurity is diffused into a region of the substrate 110 where the transistor 10 is formed to form a source / drain region 112. A halo region 113 having a higher impurity concentration than the source / drain region 112 may be formed on the outer edge of the source / drain region 112, including the region directly under the transistor 10.

[0014] The transistor 10 is provided on the substrate 110 so as to vertically overlap a portion of the source / drain region 112. The transistor 10 includes a gate electrode 150, a gate insulating layer 120, and spacer layers 131, 132, and 140. However, the source / drain region 112 and the halo region 113 may also be included in the configuration of the transistor 10.

[0015] The gate electrode 150 is a metal layer containing at least one of, for example, titanium (Ti), titanium nitride (TiN), tantalum (Ta), tantalum nitride (TaN), lanthanum (La), aluminum (Al), and titanium aluminum (AlTi).

[0016] The gate electrode 150 is configured in a line shape extending on the substrate 110 in a predetermined direction along the upper surface of the substrate 110. In a direction intersecting the extension direction of the gate electrode 150, the width of the upper end of the gate electrode 150 is wider than the width of the lower end of the gate electrode 150. The width of the lower end of the gate electrode 150 in the direction intersecting the extension direction of the gate electrode 150 is also referred to as the gate length L. The lower end of the gate electrode 150 overlaps with a partial region of the source / drain region 112 in the up-down direction at both ends.

[0017] More specifically, the gate electrode 150 includes a lower region 150a having a predetermined width as a first width in the direction along the gate length L and extending from the lower end to a predetermined height position, and an upper region 150b having a predetermined width as a second width generally wider than the width of the lower region 150a and extending from the upper end of the lower region 150a to the upper end of the gate electrode 150. At the boundary between the lower region 150a as the first region and the upper region 150b as the second region, the width of the gate electrode 150 changes discontinuously. As a result, the gate electrode 150 has a step on the sidewall of the boundary between the lower region 150a and the upper region 150b.

[0018] The gate insulating layer 120 is a high-k insulating layer containing at least one of hafnium oxide and zirconium oxide, for example. The gate insulating layer 120 covers the side walls and the lower end of the gate electrode 150. That is, the gate electrode 150 is provided on the substrate 110 via the gate insulating layer 120.

[0019] Thus, the transistor 10 has a metal gate structure with a gate insulating layer, for example a high-k insulating layer.

[0020] The spacer layers 131 and 132 as oxide layers are, for example, silicon oxide layers, and of the spacer layers 131 and 132, the spacer layer 131 contains impurities of a predetermined conductivity type. The impurities may be either P-type impurities such as boron or N-type impurities such as boron and arsenic, or at least one of these impurities.

[0021] The spacer layer 131 as a first oxide layer covers the sidewall of the lower region 150a of the gate electrode 150 with a predetermined thickness. The spacer layer 132 as a second oxide layer is thinner than the spacer layer 131 and covers the sidewall of the upper region 150b of the gate electrode 150. In the direction along the gate length L, the width of the spacer layer 131 including the gate electrode 150 is generally wider than the width of the spacer layer 132 including the gate electrode 150.

[0022] The spacer layer 140 as a nitride layer is a silicon nitride layer or the like, and covers the sidewall of the gate electrode 150 via the spacer layers 131 and 132. The spacer layer 140 may have a multi-layer structure including a different layer such as a silicon oxynitride layer in addition to the silicon nitride layer.

[0023] The interlayer insulating layer 160 is, for example, a silicon oxide layer, and covers the entire transistor 10 provided on the substrate 110. The interlayer insulating layer 160 has a flat upper surface by covering the transistor 10 with a sufficient thickness. After the interlayer insulating layer 160 is formed, the upper surface may be flattened.

[0024] The contacts CG and CS are each connected to each portion of the transistor 10. The contact CG penetrates the interlayer insulating layer 160 and is connected to an upper end of the gate electrode 150 of the transistor 10. The contacts CS penetrate the interlayer insulating layer 160 and are each connected to the source / drain regions 112 on the surface of the substrate 110. By providing a salicide layer (not shown) on the surface of the source / drain region 112, the contact CS may be connected to the source / drain region 112 via the salicide layer.

[0025] (Method of manufacturing a semiconductor device) Next, a method for manufacturing the semiconductor device 1 of the embodiment 1 will be described with reference to Fig. 2 and Fig. 3. Fig. 2 and Fig. 3 are cross-sectional views illustrating, in order, some of the steps of the method for manufacturing the semiconductor device 1 according to the embodiment.

[0026] As shown in Fig. 2(a), sacrificial layers 171, 172 and a cap layer 180 are formed in this order above a substrate 110 such as a silicon substrate. The sacrificial layer 171 as a first semiconductor layer is, for example, a polysilicon layer containing impurities of a predetermined conductivity type. The sacrificial layer 172 as a second semiconductor layer is, for example, a non-doped polysilicon layer to which no impurities are added except for unavoidable impurities. The cap layer 180 is, for example, a silicon nitride layer.

[0027] The impurity to be added to the sacrificial layer 171 may be either a P-type impurity such as boron or an N-type impurity such as boron or arsenic, or at least one of these impurities. By depositing a polysilicon layer or the like while adding such an impurity, the sacrificial layer 171 containing the impurity at a predetermined content is obtained. At this time, the concentration of the impurity in the sacrificial layer 171 is, for example, 1×10 19 atoms / cm 3 More preferably, it is equal to or greater than this.

[0028] These sacrificial layers 171, 172 and cap layer 180 are processed into lines extending on the substrate 110 in a predetermined direction along the upper surface of the substrate 110. Such sacrificial layers 171, 172 and cap layer 180 are obtained by forming these layers to cover the entire surface of the substrate 110, and then processing these layers through a resist pattern or the like by anisotropic etching such as RIE (Reactive Ion Etching).

[0029] By using anisotropic etching such as RIE, the sacrificial layers 171, 172 can be obtained in such a way that the width in a direction intersecting the extension direction of the sacrificial layers 171, 172 becomes a tapered shape in which the width increases from the upper end to the lower end, or a straight shape in which the width is approximately equal at the upper end and the lower end.

[0030] 2(b), annealing is performed in an oxidizing atmosphere such as oxygen to oxidize the sidewall portions of the sacrificial layers 171 and 172. At this time, the sacrificial layer 171 containing impurities of a predetermined conductivity type is oxidized at a higher oxidation rate than the sacrificial layer 172 which is a non-doped polysilicon layer or the like. On the other hand, the upper surface of the sacrificial layer 172 is covered with the cap layer 180 and is therefore not subjected to the above-mentioned oxidation process.

[0031] As a result, oxidation progresses from the sidewall surfaces of the sacrificial layers 171, 172 to a predetermined depth, and spacer layers 131, 132 such as silicon oxide layers are formed covering the sidewalls of the unoxidized sacrificial layers 171, 172. In other words, these spacer layers 131, 132 are layers formed by oxidizing the sidewalls of the sacrificial layers 171, 172.

[0032] As described above, since the oxidation rate of the sacrificial layer 171 is relatively high, the width of the sacrificial layer 171 remaining in an unoxidized state in the direction intersecting the extension direction of these sacrificial layers 171 and 172 is narrower than the width of the sacrificial layer 172 remaining in an unoxidized state. In addition, the spacer layer 131 covering the sidewall of the sacrificial layer 171 is thicker than the spacer layer 132 covering the sidewall of the sacrificial layer 172.

[0033] Furthermore, the spacer layers 131 and 132 are expanded in volume due to oxidation. Therefore, in a direction intersecting the extension direction of the sacrificial layers 171 and 172, the width of the spacer layer 131 including the unoxidized sacrificial layer 171 is wider than the width of the sacrificial layer 171 before the oxidation process. Similarly, the width of the spacer layer 132 including the unoxidized sacrificial layer 172 is wider than the width of the sacrificial layer 172 before the oxidation process.

[0034] Furthermore, the width of the spacer layer 131 including the unoxidized sacrificial layer 171 is wider than the width of the spacer layer 132 including the unoxidized sacrificial layer 172. These widths vary, for example, discontinuously at the height position of the interface between the spacer layer 131 and the spacer layer 132, and a step is generated at the height position of the interface between the spacer layer 131 and the spacer layer 132.

[0035] 2(c), impurities of a predetermined conductivity type are injected into the upper surface of the substrate 110 and diffused by heat. At this time, the sacrificial layers 171 and 172, the spacer layers 131 and 132, and the cap layer 180 prevent the impurities from diffusing into the substrate 110 directly below these structures. As a result, the diffusion position of the impurities is adjusted by a self-alignment method with respect to the formation positions of the sacrificial layers 171 and 172, and the source / drain regions 112 are formed on the surface of the substrate 110.

[0036] Halo regions 113 may then be formed in substrate 110 as described below.

[0037] 2(d), when forming the halo region 113, impurity ions are obliquely implanted into the substrate 110 at positions where the sacrificial layers 171 and 172, the spacer layers 131 and 132, and the cap layer 180 are to be formed, and are then thermally diffused. At this time, the source / drain region 112 itself may also extend slightly below the sacrificial layers 171 and 172. As a result, the halo region 113, which has a higher impurity concentration than the source / drain region 112, is formed at the outer edge of the source / drain region 112.

[0038] In this manner, when obliquely injecting impurity ions into substrate 110 to form halo region 113, spacer layers 131, 132 covering the sidewalls of sacrificial layers 171, 172 can function as offset spacers to inject impurities while avoiding the region that will later become directly below gate electrode 150.

[0039] 2E, a spacer layer 140 such as a silicon nitride layer is formed to cover the side walls of the sacrificial layers 171 and 172 via the spacer layers 131 and 132. The spacer layer 140 also covers the side wall of the cap layer 180 directly.

[0040] As shown in FIG. 2( f ), an interlayer insulating layer 160 that covers the entirety of the sacrificial layers 171 and 172, the spacer layers 131, 132, and 140, and the cap layer 180 is formed.

[0041] As shown in FIG. 2(g), the surface of the interlayer insulating layer 160 is polished by, for example, a CMP (Chemical Mechanical Polishing) method until the cap layer 180 is removed.

[0042] More specifically, the interlayer insulating layer 160 is polished using the cap layer 180 as a stopper layer until the upper surface of the cap layer 180 is reached. Then, an additional polishing process is performed until the cap layer 180 is removed. As a result, the sacrificial layer 172 sandwiched between the spacer layers 132 and 140 is exposed on the upper surface of the interlayer insulating layer 160.

[0043] In this manner, the cap layer 180 functions as an oxidation suppression layer that suppresses oxidation of the upper surface of the sacrificial layer 172 in the oxidation treatment of FIG. 2(b) described above, and functions as a stopper layer in the polishing treatment of FIG. 2(g).

[0044] As shown in FIG. 2(h), the sacrificial layer 172 exposed on the upper surface of the interlayer insulating layer 160 and the sacrificial layer 171 below the sacrificial layer 172 are sequentially removed. These sacrificial layers 171 and 172 can be removed by wet etching using a chemical solution that dissolves, for example, a polysilicon layer. As a result, a gap 150g is formed in the region sandwiched between the spacer layers 132 and 140. This gap 150g has a width on the upper end side wider than the lower end side in accordance with the shape of the sacrificial layers 171 and 172 of the removed unoxidized portions, and has a step between the upper end and the lower end.

[0045] 3(a), a gate insulating layer 120 such as a Hihg-k insulating layer is formed on the bottom surface and side walls of the gap 150g sandwiched between the spacer layers 132 and 140. Since the gate insulating layer 120 is formed to a substantially uniform thickness, even after the gate insulating layer 120 is formed, the shape of the gap 150g described above, in which the width on the upper end side is wider than the width on the lower end side and the step between the upper end and the lower end is maintained.

[0046] 3(b), a predetermined metal layer is filled in a gap 150g further inside the gate insulating layer 120 to form a gate electrode 150. The gate electrode 150 is formed in a shape corresponding to the shape of the gap 150g. That is, the gate electrode 150 includes a lower region 150a having a predetermined width and an upper region 150b wider than the lower region 150a, and has a step on the sidewall at the height position of the interface between the lower region 150a and the upper region 150b.

[0047] This also results in the formation of a transistor 10 comprising a gate electrode 150 and a gate insulating layer 120 .

[0048] 3(c), the interlayer insulating layer 160 is deposited to a sufficient thickness so as to cover the exposed gate electrode 150 etc. At this time, the upper surface of the interlayer insulating layer 160 may be planarized by a CMP method or the like.

[0049] As shown in FIG. 3(d), a plurality of contact holes CLg, CLs are formed which penetrate the interlayer insulating layer 160 and reach the gate electrode 150 and the source / drain region 112 of the transistor 10, respectively.

[0050] As shown in FIG. 3(e), a conductive layer is filled in the contact holes CLg and CLs to form contacts CG connected to the gate electrode 150 and contacts CS connected to the source / drain regions 112, respectively.

[0051] In this manner, the semiconductor device 100 of the first embodiment is manufactured.

[0052] (Comparative Example) There is known a semiconductor device having a transistor with a metal gate structure that uses a high-k insulating layer as a gate insulating layer. By using an insulating layer with a relatively high dielectric constant such as a high-k insulating layer, the gate insulating layer can be formed thick, and the leakage current of the transistor can be suppressed.

[0053] Since high-k insulating layers are easily altered by heat, when forming source / drain regions, a method is sometimes used in which impurities are injected into the substrate in a self-aligned manner using an electrode structure that uses a sacrificial layer, and then thermally diffused. However, when forming a gate electrode by replacing the sacrificial layer with a conductive layer such as a metal layer, defects in the formation of the gate electrode may occur. Figure 4 below shows an example of a gate electrode formation defect.

[0054] 4A to 4C are cross-sectional views illustrating a part of a procedure of a method for manufacturing a semiconductor device according to a comparative example.

[0055] 4A, a sacrificial layer 170x such as a polysilicon layer and a cap layer 180x such as a silicon nitride layer are formed in this order on a substrate 110x. The sacrificial layer 170x is a non-doped polysilicon layer to which no impurities are added.

[0056] The sacrificial layer 170x and the cap layer 180x are processed into a line shape. At this time, the sacrificial layer 170x is generally formed into a tapered shape that becomes wider from the upper end to the lower end, that is, a forward tapered shape or a straight shape.

[0057] As shown in FIG. 4B, impurities are implanted into the substrate 110x in a self-alignment manner using a sacrificial layer 170x and a cap layer 180x to form source / drain regions 112x and halo regions 113x.

[0058] 4(c), a spacer layer 140x such as a silicon nitride layer is formed to cover the side walls of the sacrificial layer 170x and the cap layer 180x, and an interlayer insulating layer 160x is formed to cover these structures.

[0059] 4(d), the interlayer insulating layer 160x is polished by CMP or the like using the cap layer 180x as a stopper layer, and the cap layer 180x is then removed by additional polishing, thereby exposing the upper end of the sacrificial layer 170x on the upper surface of the interlayer insulating layer 160x.

[0060] Thereafter, the sacrificial layer 170x is removed to form the gate electrode 150x. The following Figures 4(e) and 4(f) each show an example of a formation defect that may occur during the formation of the gate electrode 150x.

[0061] As shown in FIG. 4(e), the sacrificial layer 170x exposed on the upper surface of the interlayer insulating layer 160x is removed by wet etching or the like. However, the width of the upper end of the sacrificial layer 170x is equal to or smaller than the width of the lower end. For this reason, it is difficult for the chemical solution to reach both ends in the width direction of the lower end of the sacrificial layer 170x. In the example shown in FIG. 4(e), there is a remaining part of the sacrificial layer 170x at both ends of the bottom surface of the gap 150g generated by removing the sacrificial layer 170x.

[0062] As shown in Fig. 4(f), a gate insulating layer 120x is formed on the bottom and side walls of the gap 150gx after the sacrificial layer 170x is removed, and then a metal layer is filled to form a gate electrode 150x. However, due to the above-mentioned shape of the sacrificial layer 170x, it is difficult for the source gas of the metal layer or the like to reach both ends in the width direction of the lower end of the sacrificial layer 170x, and in the example shown in Fig. 4(f), the metal layer is not sufficiently filled in the gap 150gx, and voids 150v are generated at both ends in the width direction of the lower end of the gate electrode 150x.

[0063] Thus, if any part of the sacrificial layer 170x remains unremoved or if the gate electrode 150x contains voids 150v, the width of the bottom end of the gate electrode 150x becomes narrow, and there is a possibility that a desired gate length cannot be obtained.

[0064] Therefore, when processing the sacrificial layer 170x into a line shape, it is possible to form the sacrificial layer 170x into a tapered shape in which the width narrows from the upper end to the lower end, that is, an inverse tapered shape. However, in order to form the sacrificial layer 170x into an inverse tapered shape, for example, the reactivity in RIE is increased, and side etching is generated on the sidewall of the sacrificial layer 170x, which may deteriorate the controllability of the processing dimension of the sacrificial layer 170x.

[0065] In addition, when the source / drain regions 112x and the like are formed by injecting impurities into the substrate 110x, the thickness of the sacrificial layer 170x must be secured in order to suppress the permeation of the impurities. In processing a line-shaped shape with such a high aspect ratio, the sacrificial layer 170x is likely to have a tapered shape with an even wider lower end.

[0066] According to the manufacturing method of semiconductor device 100 of embodiment 1, the impurity content in sacrificial layer 171 is increased, and no impurities are added to sacrificial layer 172. The oxidation rate of sacrificial layer 171 is increased more than that of sacrificial layer 172, and the width of sacrificial layer 171 after oxidation in a direction intersecting the extension direction is made narrower than the width of sacrificial layer 172 after oxidation.

[0067] As described above, the sacrificial layers 171, 172, such as polysilicon layers, have a higher oxidation rate as the impurity content increases. Therefore, when the sacrificial layers 171, 172, which have different impurity contents and substantially the same width, are oxidized under the same conditions, the widths of the sacrificial layers 171, 172 that remain unoxidized can be made different. As an example, the relationship between the impurity content and the oxidation rate is shown in FIG. 5.

[0068] FIG. 5 is a graph showing the relationship between the thickness and the impurity concentration of a silicon oxide layer formed by the oxidation treatment used in the manufacturing method of the semiconductor device 100 according to the first embodiment.

[0069] Figure 5(a) is a graph showing the thickness of a silicon oxide layer formed by oxidation of a silicon layer doped with phosphorus (P) as an N-type impurity, and Figure 5(b) is a graph showing the thickness of a silicon oxide layer formed by oxidation of a silicon layer doped with molecular ions of boron fluoride (BF2) as a P-type impurity.

[0070] The horizontal axis of Fig. 5(a) and (b) is the concentration of each impurity when implanted into the silicon layer (atoms / cm 2 ) and the vertical axis represents the thickness (nm) of the silicon oxide layer formed by oxidizing each silicon layer.

[0071] As shown in Figures 5(a) and (b), for both N-type and P-type impurities, the higher the concentration of impurities implanted into the silicon layer, the faster the oxidation rate of the silicon layer increases, and the thickness of the silicon oxide layer formed from the silicon layer increases.

[0072] With the above-described configuration utilizing such characteristics of impurity doping, the upper sacrificial layer 172 has a width greater than the lower sacrificial layer 171, thereby preventing, for example, the occurrence of residual sacrificial layer 171 remaining at both ends of the bottom surface of gap 150g after sacrificial layers 171 and 172 are removed, and preventing voids from occurring at both ends of the width of the lower end of gate electrode 150.

[0073] Unlike the case where a single sacrificial layer is formed in an inverse tapered shape, each of the sacrificial layers 171 and 172 itself can be formed in a forward tapered shape or a straight shape, which makes it possible to improve the controllability of the processing dimensions.

[0074] Therefore, defects in the formation of the gate electrode 150 can be suppressed, and the gate electrode 150 can be formed to have the desired gate length L.

[0075] Furthermore, by oxidizing the sidewalls of the sacrificial layers 171, 172 as described above, for example, when processing the sacrificial layers 171, 172 into a line shape, it is expected that LER (Line Edge Roughness) that may occur on the sidewalls of the sacrificial layers 171, 172 is reduced on the sidewalls of the unoxidized portions of the sacrificial layers 171, 172. This is considered to enable the sidewalls of the gate electrode 150 formed using the unoxidized portions of the sacrificial layers 171, 172 as a template to be flattened.

[0076] Moreover, by making the oxidation depth of the sacrificial layers 171, 172 different, the width of the sacrificial layers 171, 172 that remain unoxidized can be controlled. Therefore, for example, the line width of the sacrificial layers 171, 172 can be initially formed wide, and the unoxidized sacrificial layers 171, 172 can be thinned by adjusting the oxidation depth of the sacrificial layers 171, 172. Therefore, it becomes easy to thin the gate electrode 150 without performing precise etching processing with a high aspect ratio.

[0077] According to the semiconductor device 100 of embodiment 1, the above manufacturing method results in a transistor 10 in which the width of the gate electrode 150 is wider at the upper end than at the lower end, and the spacer layer 131 is thicker in the portion covering the lower end of the gate electrode 150 than in the portion covering the upper end of the gate electrode 150.

[0078] According to the semiconductor device 100 of embodiment 1, the above-mentioned manufacturing method is used to provide a spacer layer 131 provided on the sidewall portion of the lower region 150a of the gate electrode 150, and a spacer layer 132 provided on the sidewall portion of the upper region 150b of the gate electrode 150 and containing at least more impurities of a predetermined conductivity type than the spacer layer 131.

[0079] For example, in the manufacturing method of the comparative example described above, when forming a halo region by implanting oblique ions of impurities, an offset spacer such as a silicon oxide layer is formed on the side wall of the sacrificial layer 170x to prevent the impurities from being implanted into the region directly below the gate electrode 150x. That is, in the manufacturing method of the comparative example, a process for forming an offset spacer is required, and unevenness may occur on the substrate 110x during the formation of the offset spacer. Such unevenness on the substrate 110x may cause an increase in the path resistance, etc., and may cause the transistor characteristics to become unstable.

[0080] As described above, the spacer layers 131 and 132 of the first embodiment are formed on the side walls of the sacrificial layers 171 and 172, for example, before the formation of the halo region 113 in the substrate 110. Therefore, it is possible to form the halo region 113 by using the spacer layers 131 and 132 as offset spacers without forming an offset spacer separately. This simplifies the manufacturing process of the semiconductor device 100, and also eliminates unevenness of the substrate 110 during the formation of the offset spacers, thereby suppressing an increase in the path resistance and the like, thereby further stabilizing the characteristics of the transistor 10.

[0081] In the above-mentioned first embodiment, the above-mentioned shape of the gate electrode 150 is obtained by using the sacrificial layer 171 containing an impurity of a predetermined conductivity type and the sacrificial layer 172 which is a non-doped polysilicon layer or the like. However, if the oxidation rate of the lower sacrificial layer 171 is higher than the oxidation rate of the upper sacrificial layer 172, the upper sacrificial layer 172 may also contain an impurity. For example, when the same type of impurity is added to the sacrificial layers 171 and 172, the oxidation rates of the sacrificial layers 171 and 172 can be adjusted as described above by increasing the impurity concentration of the sacrificial layer 171 to be higher than the impurity concentration of the sacrificial layer 172.

[0082] (Variation 1) Next, semiconductor devices 101-103 according to Modification 1 of Embodiment 1 will be described with reference to Figures 6-9. The semiconductor devices 101-103 according to Modification 1 differ from the above-described Embodiment 1 in that the gate electrodes 151-153 have at least a part that is tapered.

[0083] In the following drawings, the same components as those in the semiconductor device 100 of the above-described first embodiment are denoted by the same reference numerals, and the description thereof may be omitted.

[0084] FIG. 6 is a cross-sectional view showing an example of the configuration of a semiconductor device 101 according to Modification 1 of the first embodiment.

[0085] 6, a transistor 11 included in a semiconductor device 101 of the first modification has a gate electrode 151, a gate insulating layer 121, and spacer layers 131 to 133 and 140. However, the configuration of the transistor 11 may also include a source / drain region 112 and a halo region 113.

[0086] The gate electrode 151 is, for example, a metal layer containing the same material as the gate electrode 150 of the above-mentioned first embodiment, and is configured in a line shape extending in a predetermined direction on the upper surface of the substrate 110. In a direction along the gate length L intersecting with the extension direction of the gate electrode 151, the width of the upper end of the gate electrode 151 is wider than the width of the lower end of the gate electrode 151. The width between the upper end and the lower end of the gate electrode 151 is tapered downward.

[0087] More specifically, the gate electrode 151 includes a lower region 151a and an upper region 151b, similar to the gate electrode 150 of the above-mentioned embodiment 1. However, the upper region 151b is formed to be thinner than the upper region 150b of the above-mentioned embodiment 1. The thickness of the lower region 151a may be approximately equal to the thickness of the lower region 150a of the above-mentioned embodiment 1, for example.

[0088] Between the lower region 150a and the upper region 150b, an intermediate region 151c is inserted, the width of which increases from the lower region 150a side to the upper region 150b side in the direction along the gate length L. It is preferable that the width of the upper end of the intermediate region 151c is approximately equal to the width of the upper region 150b, and the width of the lower end of the intermediate region 151c is approximately equal to the width of the lower region 150a. As a result, the width of the gate electrode 151 changes continuously, for example, from the lower end to the upper end.

[0089] The gate insulating layer 121 is, for example, a High-k insulating layer similar to the gate insulating layer 120 in the above-described first embodiment, and covers the side walls and the lower end of the gate electrode 151 .

[0090] The spacer layer 131 contains impurities of a predetermined conductivity type, as in the above-described first embodiment, and covers the sidewall portion of the lower region 151a of the gate electrode 151 with a predetermined thickness. The spacer layer 132 is thinner than the spacer layer 131, as in the above-described first embodiment, and covers the sidewall portion of the upper region 151b of the gate electrode 151. The spacer layer 132 does not contain impurities except for unavoidable impurities. Alternatively, the spacer layer 132 may contain impurities at a lower content than the spacer layer 131.

[0091] The spacer layer 133, with its thickness decreasing from bottom to top, covers the sidewall portion of the intermediate region 151c of the gate electrode 151. It is preferable that the spacer layer 133 has a thickness approximately equal to that of the spacer layer 132 at the upper end portion and a thickness approximately equal to that of the spacer layer 131 at the lower end portion.

[0092] Moreover, the spacer layer 133 contains impurities of a predetermined conductivity type, the content of which decreases from bottom to top. The impurity content of the spacer layer 133 is preferably approximately equal to the impurity content of the spacer layer 132 at the upper end of the spacer layer 133. In other words, when the spacer layer 132 does not contain impurities, the content of impurities other than unavoidable impurities at the upper end of the spacer layer 133 is preferably approximately zero. Moreover, the impurity content at the lower end of the spacer layer 133 is preferably approximately equal to the impurity content of the spacer layer 131.

[0093] A method for manufacturing the semiconductor device 101 including such a transistor 11 will be described below.

[0094] 7A to 7C are cross-sectional views illustrating a part of a procedure of a method for manufacturing a semiconductor device 101 according to the first modification of the first embodiment.

[0095] 7A, sacrificial layers 171, 173, 172 and a cap layer 180 are formed in this order and processed into a line shape above a substrate 110 such as a silicon substrate. The cap layer 180 is, for example, a silicon nitride layer, as in the first embodiment.

[0096] The sacrificial layer 171 is, for example, a polysilicon layer containing impurities of a predetermined conductivity type, as in the above-described embodiment 1. The sacrificial layer 172 is, for example, a region to which no impurities are added, except for unavoidable impurities, as in the above-described embodiment 1. However, the sacrificial layer 172 may contain impurities in an amount less than that of the sacrificial layer 171.

[0097] The sacrificial layer 173 contains impurities in an amount equal to or less than the amount of impurities added in the sacrificial layer 171, and the amount of impurities added decreases from bottom to top. It is preferable that the amount of impurities added in the sacrificial layer 173 at the bottom end is approximately equal to the amount of impurities added in the sacrificial layer 171, and at the top end is approximately equal to the amount of impurities added in the sacrificial layer 172. In other words, when no impurities are added to the sacrificial layer 172, the amount of impurities added at the top end of the sacrificial layer 173 can be set to zero.

[0098] Such a sacrificial layer 173 can be formed as follows. First, a polysilicon layer is formed on the sacrificial layer 171 while doping impurities in an amount equal to or less than the amount of impurity added to the sacrificial layer 171. At this time, the amount of impurity added is decreased as the thickness of the polysilicon layer increases. If no impurity is added to the sacrificial layer 172, the doping of the impurity is stopped thereafter, and the formation of the polysilicon layer is completed.

[0099] 7(b), sidewall portions of the sacrificial layers 171-173 are oxidized by performing an annealing process in an oxidizing atmosphere such as oxygen. At this time, the oxidation rate of the sacrificial layer 171 is higher than that of the sacrificial layer 172. The oxidation rate of the sacrificial layer 173 is equal to or lower than that of the sacrificial layer 171. Moreover, the oxidation rate of the sacrificial layer 173 decreases from the lower end to the upper end.

[0100] This forms spacer layers 131 and 132 such as silicon oxide layers covering the side walls of the unoxidized sacrificial layers 171 and 172. The spacer layer 131 covers the side wall of the unoxidized sacrificial layer 171, and the spacer layer 132 covers the side wall of the unoxidized sacrificial layer 172. In addition, the spacer layer 133 covers the side wall of the unoxidized sacrificial layer 173.

[0101] In a direction intersecting the extension direction of these sacrificial layers 171 to 173, the width of sacrificial layer 171 remaining in an unoxidized state is narrower than the width of sacrificial layer 172 remaining in an unoxidized state. In addition, spacer layer 131 covering the side wall of sacrificial layer 171 is thicker than spacer layer 132 covering the side wall of sacrificial layer 172.

[0102] In addition, in a direction intersecting the extension direction of the sacrificial layers 171 to 173, the width of the sacrificial layer 173 remaining in an unoxidized state is equal to or greater than the width of the sacrificial layer 171 remaining in an unoxidized state, and the width further increases toward the top.

[0103] At this time, as described above, by adding an amount of impurity to the lower end of the sacrificial layer 173 that is approximately equal to the amount of impurity added to the sacrificial layer 171, the lower end of the unoxidized sacrificial layer 173 can have a width approximately equal to that of the unoxidized sacrificial layer 171. Also, by adding an amount of impurity to the upper end of the sacrificial layer 173 that is approximately equal to the amount of impurity added to the sacrificial layer 172, the upper end of the unoxidized sacrificial layer 173 can have a width approximately equal to that of the unoxidized sacrificial layer 172.

[0104] Corresponding to the state of the unoxidized sacrificial layer 173, the thickness of the spacer layer 133 covering the sidewall portion of the sacrificial layer 173 also decreases from the bottom end to the top end.

[0105] At this time, as described above, by adding an amount of impurity substantially equal to that of the sacrificial layer 171 at the lower end of the sacrificial layer 173, the lower end of the spacer layer 133 has a width substantially equal to that of the spacer layer 131 covering the side wall of the sacrificial layer 171. Also, as described above, by adding an amount of impurity substantially equal to that of the sacrificial layer 172 at the upper end of the sacrificial layer 173, the upper end of the spacer layer 133 has a width substantially equal to that of the spacer layer 132 covering the side wall of the sacrificial layer 172.

[0106] As a result, the width of the unoxidized sacrificial layers 171 to 173 in the direction intersecting the extension direction changes continuously, and the unoxidized sacrificial layers 171 to 173 having no steps on the side walls can be formed.

[0107] Also, in variant example 1, the width of spacer layer 131 including unoxidized sacrificial layer 171, the width of spacer layer 132 including unoxidized sacrificial layer 172, and the width of spacer layer 133 including unoxidized sacrificial layer 173 are wider than the width of sacrificial layer 171, the width of sacrificial layer 172, and the width of sacrificial layer 173 before the oxidation process, respectively, due to volume expansion during oxidation.

[0108] For the above reasons, the width of the spacer layer 131 including the unoxidized sacrificial layer 171 is wider than the width of the spacer layer 132 including the unoxidized sacrificial layer 172. Moreover, the width of the spacer layer 133 including the unoxidized sacrificial layer 173 decreases from the bottom end to the top end.

[0109] 7(c), similarly to the above-described first embodiment, the source / drain regions 112 are formed in the substrate 110 by a self-alignment method using the sacrificial layers 171-173, the spacer layers 131-133, and the cap layer 180. Thereafter, the halo regions 113 may be formed.

[0110] As shown in FIG. 7(d), similarly to the above-described embodiment 1, a spacer layer 140 such as a silicon nitride layer is formed to cover the side walls of the sacrificial layers 171-173 via the spacer layers 131-133, and further, an interlayer insulating layer 160 is formed to cover the entire configuration.

[0111] 7(e), similarly to the above-described first embodiment, the interlayer insulating layer 160 is polished by a CMP method or the like using the cap layer 180 as a stopper layer, and the cap layer 180 is then removed by additional polishing. As a result, the sacrificial layer 172 is exposed from the upper surface of the interlayer insulating layer 160.

[0112] 7(f), the sacrificial layers 172, 173, and 171 are successively removed by wet etching or the like, in the same manner as in the above-described embodiment 1. As a result, a gap 151g sandwiched between the spacer layers 131 to 133 and 140 is formed.

[0113] As shown in FIG. 7(g), similarly to the above-described first embodiment, a gate insulating layer 121 such as a High-k insulating layer is formed to cover the bottom and sidewalls of the gap 151g.

[0114] As shown in FIG. 7(h), similarly to the above-described first embodiment, the gap 151g is filled with a metal layer to form the gate electrode 151.

[0115] In this manner, the semiconductor device 101 of the first modification is manufactured.

[0116] 6 and 7, the sacrificial layer 172 is formed thinner than in the example of the above-mentioned embodiment 1, and the sacrificial layer 173 having the amount of impurity added differing in the layer thickness direction is inserted below the sacrificial layer 172. However, the layer thicknesses of the sacrificial layers 171 to 173 can be made different as appropriate. An example of this case is shown in FIG.

[0117] FIG. 8 is a cross-sectional view showing another example of the configuration of the semiconductor device 102 according to the first modification of the first embodiment.

[0118] 8, a transistor 12 included in a semiconductor device 102 of the first modification has a gate electrode 152, a gate insulating layer 122, and spacer layers 131 to 133 and 140. However, the configuration of the transistor 12 may include a source / drain region 112 and a halo region 113.

[0119] The gate electrode 152 is, for example, a metal layer containing the same material as the gate electrode 150 of the above-mentioned first embodiment, and is configured in a line shape extending on the substrate 110 in a predetermined direction along the upper surface of the substrate 110. Like the gate electrode 151 of the above-mentioned first modification, the gate electrode 152 includes an upper region 152b, a middle region 152c, and a lower region 152a, and has a shape similar to that of the gate electrode 151 of the first modification.

[0120] However, a lower region 152a of the gate electrode 152 is formed thinner than the lower region 152a of the gate electrode 151 of the above-mentioned modified example 1. On the other hand, an intermediate region 152c of the gate electrode 152 is formed thicker than the intermediate region 152c of the gate electrode 151 of the above-mentioned modified example 1. In other words, the gate electrode 152 has a higher proportion of the tapered portion than the gate electrode 151 of the above-mentioned modified example 1.

[0121] Such a gate electrode 152 can be formed, for example, by the same method as that shown in Fig. 7 of the above-mentioned modified example 1. In this case, the thickness of the bottom sacrificial layer 171 can be made thinner than that of the example of modified example 1, and the sacrificial layer 173 in the middle part can be made thicker accordingly.

[0122] 6 to 8, the sacrificial layers 171 and 172 are formed with the amount of impurity added kept constant. However, it is also possible to form only the sacrificial layer 173 with the amount of impurity added varying from the lower end to the upper end. An example of this case is shown in FIG.

[0123] FIG. 9 is a cross-sectional view showing still another example of the configuration of the semiconductor device 103 according to the first modification of the first embodiment.

[0124] 9, the transistor 13 included in the semiconductor device 103 of the first modification has a gate electrode 153, a gate insulating layer 123, and spacer layers 133 and 140. However, the configuration of the transistor 13 may include a source / drain region 112 and a halo region 113.

[0125] The gate electrode 153 is, for example, a metal layer containing the same material as the gate electrode 150 of the above-mentioned first embodiment, and is configured in a line shape extending in a predetermined direction on the upper surface of the substrate 110. Unlike the gate electrodes 151 and 152 of the above-mentioned first modification, the gate electrode 153 has a tapered shape over its entirety, the width of which increases in the direction along the gate length L from the lower end toward the upper end.

[0126] Such a gate electrode 153 can be obtained by, for example, forming the sacrificial layer 173 shown in FIG. 7 of the above-mentioned modified example 1 over the entire surface.

[0127] According to the manufacturing method of semiconductor devices 101-103 of Modification 1, in the thickness direction of sacrificial layer 173, the impurity content is made closer to the impurity content in sacrificial layer 172 toward sacrificial layer 172. Also, in the thickness direction of sacrificial layer 173, the impurity content is made different from the impurity content in sacrificial layer 171 as it moves away from sacrificial layer 171.

[0128] By carrying out at least one of these treatments, the unoxidized sacrificial layers 171 to 173 and the gaps after removing the sacrificial layers 171 to 173 have at least a partial tapered shape. This further suppresses, for example, the occurrence of residual sacrificial layer 171 at both ends of the bottom surface of the gap and the occurrence of voids at both ends of the lower end of gate electrode 151 in the width direction.

[0129] Therefore, defects in the formation of the gate electrodes 151 to 153 can be suppressed, and it becomes easier to form the gate electrodes 151 to 153 with the desired gate length L.

[0130] According to the semiconductor devices 101 to 103 of the first modification, the above manufacturing method provides the transistor 11 in which the side walls of the gate electrodes 151 to 153 at least partially have a tapered shape that widens upward.

[0131] The semiconductor devices 101 to 103 of the first modification and the manufacturing method thereof provide the same effects as the semiconductor device 100 of the first embodiment and the manufacturing method thereof.

[0132] (Variation 2) 10 and 11, a semiconductor device 104 according to a second modification of the first embodiment will be described. The semiconductor device 104 according to the third modification is different from the first embodiment in that the transistor 14 does not have the spacer layers 131, 132, etc.

[0133] In the following drawings, the same components as those in the semiconductor device 100 of the above-described first embodiment are denoted by the same reference numerals, and the description thereof may be omitted.

[0134] FIG. 10 is a cross-sectional view showing an example of the configuration of a semiconductor device 104 according to Modification 2 of Embodiment 1. As shown in FIG.

[0135] 10, the transistor 14 included in the semiconductor device 104 of the second modification does not have the spacer layers 131, 132 on the side walls of the gate electrode 150. That is, the spacer layer 140 of the transistor 14 covers the side walls of the gate electrode 150 via the gate insulating layer 120, without the spacer layers 131, 132. The rest of the configuration of the transistor 14 is the same as that of the transistor 10 of the first embodiment described above.

[0136] A method for manufacturing a semiconductor device 104 including such a transistor 14 will be described below.

[0137] 11 is a cross-sectional view illustrating a part of the procedure of the method for manufacturing a semiconductor device 104 according to Modification 2 of Embodiment 1. In the method for manufacturing a semiconductor device 104 of Modification 2, for example, the same processes as those shown in FIGS. 2(a) to 2(d) of the above-mentioned embodiment 1 are performed.

[0138] 11(a) shows a state after the process of FIG. 2(d) of the above-mentioned embodiment 1 is completed. That is, sacrificial layers 171, 172 and a cap layer 180 are formed in this order above the substrate 110, and parts of the sacrificial layers 171, 172 are oxidized to form spacer layers 131, 132 on their side walls, respectively. Also, the source / drain regions 112 and the halo regions 113 have already been formed in the substrate 110.

[0139] As shown in FIG. 11B, the spacer layers 131 and 132 covering the side walls of the sacrificial layers 171 and 172 are removed by, for example, wet etching.

[0140] As shown in FIG. 11C, a spacer layer 140 is formed so as to directly cover the side walls of the sacrificial layers 171 and 172 from which the spacer layers 131 and 132 have been removed, and further an interlayer insulating layer 160 is formed so as to cover the entire structure.

[0141] 11D, the interlayer insulating layer 160 is polished by CMP or the like using the cap layer 180 as a stopper layer, and then the cap layer 180 is removed by additional polishing. As a result, the sacrificial layer 172 is exposed on the upper surface of the interlayer insulating layer 160.

[0142] 11(e), the sacrificial layers 172, 171 are sequentially removed by wet etching or the like to form a gap 150g sandwiched by the spacer layers 140. The spacer layer 140 formed on the side walls of the sacrificial layers 171, 172 without the spacer layers 131, 132 has an inner shape corresponding to the shape of the sacrificial layers 171, 172. Therefore, in accordance with the shape of the sacrificial layers 171, 172, a gap 150g is obtained in which the open end of the upper surface of the interlayer insulating layer 160 has a width wider than the bottom surface.

[0143] As shown in FIG. 11(f), a gate insulating layer 120 such as a High-k insulating layer is formed to cover the bottom and sidewalls of the gap 150g.

[0144] As shown in FIG. 11(g), a metal layer is further filled into the gap 150g to form a gate electrode 150 whose upper end is wider than its lower end.

[0145] In this manner, the semiconductor device 104 of the second modification is manufactured.

[0146] According to the method for manufacturing the semiconductor device 104 of the second modification, the spacer layers 131 and 132 are removed before forming the spacer layer 140. This manufacturing method also provides the same effects as the semiconductor device 100 and the manufacturing method thereof of the first embodiment described above.

[0147] The manufacturing method of the second modification in which the spacer layers 131 and 132 are removed before the spacer layer 140 is formed can also be applied to the manufacturing method of the semiconductor devices 101 to 103 of the first modification described above.

[0148] [Embodiment 2] Hereinafter, the second embodiment will be described in detail with reference to the drawings. In the first embodiment and the first and second modifications described above, the gate electrodes 150-153 are formed to correspond to the shapes of the sacrificial layers 171, 172. The second embodiment differs from the first embodiment in that the gate electrodes are formed to correspond to the shapes of the spacer layers 131, 132 in addition to the sacrificial layers 171, 172.

[0149] In the following drawings, the same components as those in the semiconductor device 100 of the above-described first embodiment are denoted by the same reference numerals, and the description thereof may be omitted.

[0150] (Configuration of Semiconductor Device) FIG. 12 is a cross-sectional view showing an example of the configuration of a semiconductor device 200 according to the second embodiment.

[0151] 12, the transistor 20 included in the semiconductor device 200 of the second embodiment includes a gate electrode 250, a gate insulating layer 220, and a spacer layer 140. However, the configuration of the transistor 20 may include a source / drain region 112 and a halo region 113.

[0152] The gate electrode 250 is, for example, a metal layer containing the same material as the gate electrode 150 of the above-mentioned first embodiment, and is configured in a line shape extending in a predetermined direction on the upper surface of the substrate 110. In the direction along the gate length L intersecting with the extension direction of the gate electrode 250, the width of the upper end of the gate electrode 250 is wider than the width of the lower end of the gate electrode 250.

[0153] More specifically, the gate electrode 250 includes a lower region 250a having a predetermined width in the direction along the gate length L and extending from the lower end to a predetermined height position, and an upper region 250b having a width generally wider than the width of the lower region 250a and extending from the upper position of the lower region 250a to the upper end of the gate electrode 250. At the boundary between the lower region 250a and the upper region 250b, the width of the gate electrode 250 changes discontinuously. As a result, the gate electrode 250 has a step on the sidewall at the boundary between the lower region 250a and the upper region 250b.

[0154] In this way, the gate electrode 250 of the second embodiment has a shape similar to that of the gate electrode 150 of the first embodiment. In the example of Fig. 12, the gate electrode 250 has a width that is wider overall than that of the gate electrode 150 of the first embodiment. However, the gate electrode 250 may be formed to have the same width as that of the gate electrode 150 of the first embodiment.

[0155] The gate insulating layer 220 is, for example, a high-k insulating layer similar to the gate insulating layer 120 of the above-described first embodiment, and covers the sidewalls and the lower end of the gate electrode 250. In addition, the spacer layer 140 covers the sidewalls of the gate electrode 250 via the gate insulating layer 220.

[0156] As described above, the transistor 20 of the second embodiment has a similar overall configuration to the transistor 14 of the second modification of the first embodiment. However, the transistor 20 of the second embodiment is manufactured by a method different from that of the second modification of the first embodiment.

[0157] (Method of manufacturing a semiconductor device) 13A to 13C are cross-sectional views illustrating a part of the procedure of the method for manufacturing the semiconductor device 200 according to the second embodiment.

[0158] 13A, in the manufacturing method of the semiconductor device 200 of the second embodiment, the order of forming the sacrificial layers 171 and 172 is reversed. That is, the sacrificial layers 172 and 171 and the cap layer 180 are formed in this order above the substrate 110 such as a silicon substrate, and processed into a line shape.

[0159] The sacrificial layer 172 as the first semiconductor layer is, for example, a non-doped polysilicon layer, as in the above-described embodiment 1. The sacrificial layer 171 as the second semiconductor layer is, for example, a polysilicon layer doped with an impurity of a predetermined conductivity type, as in the above-described embodiment 1. The cap layer 180 is, for example, a silicon nitride layer, as in the above-described embodiment 1.

[0160] 13(b), the sidewalls of the sacrificial layers 171 and 172 are oxidized by performing an annealing process in an oxidizing atmosphere such as oxygen, thereby forming spacer layers 131 and 132 such as silicon oxide layers covering the sidewalls of the unoxidized sacrificial layers 171 and 172, respectively.

[0161] At this time, the oxidation rate of the sacrificial layer 171 is higher than the oxidation rate of the sacrificial layer 172. Therefore, in a direction intersecting with the extension direction of these sacrificial layers 171 and 172, the width of the sacrificial layer 171 remaining in an unoxidized state is narrower than the width of the sacrificial layer 172 remaining in an unoxidized state. In addition, the spacer layer 131 as the second oxidation layer covering the sidewall of the sacrificial layer 171 is thicker than the spacer layer 132 as the first oxidation layer covering the sidewall of the sacrificial layer 172.

[0162] Also in embodiment 2, the width of spacer layer 131 including unoxidized sacrificial layer 171 and the width of spacer layer 132 including unoxidized sacrificial layer 172 are wider than the width of sacrificial layer 171 and the width of sacrificial layer 172 before the oxidation process, respectively, due to the volume expansion during oxidation.

[0163] For the above reasons, the width of the spacer layer 131, which is formed on the upper side of the sacrificial layer 172 and includes the unoxidized sacrificial layer 171, is wider than the width of the spacer layer 132, which is formed on the side closer to the substrate 110 and includes the unoxidized sacrificial layer 172.

[0164] 13(c), similarly to the above-described first embodiment, the source / drain regions 112 are formed in the substrate 110 by a self-alignment method using the sacrificial layers 171 and 172, the spacer layers 131 and 132, and the cap layer 180. Thereafter, the halo regions 113 may be formed.

[0165] As shown in FIG. 13(d), similarly to the above-described embodiment 1, a spacer layer 140 such as a silicon nitride layer is formed to cover the side walls of the sacrificial layers 171, 172 via the spacer layers 131, 132, and further, an interlayer insulating layer 160 is formed to cover the entire structure.

[0166] 13(e), similarly to the above-described first embodiment, the interlayer insulating layer 160 is polished by a CMP method or the like using the cap layer 180 as a stopper layer, and the cap layer 180 is then removed by additional polishing. As a result, the sacrificial layer 171 and the spacer layer 131 are exposed from the upper surface of the interlayer insulating layer 160.

[0167] 13(f), the sacrificial layers 171, 172 are sequentially removed by wet etching or the like. Furthermore, the spacer layers 131, 132 are sequentially removed by wet etching or the like using a chemical liquid different from the chemical liquid used to remove the sacrificial layers 171, 172. As a result, a gap 250g sandwiched between the spacer layers 140 is formed.

[0168] The spacer layer 140 formed on the side walls of the sacrificial layers 171, 172 via the spacer layers 131, 132 has an inner shape corresponding to the shape of the spacer layers 131, 132 including the sacrificial layers 171, 172. Therefore, in accordance with the shape of the spacer layers 131, 132 including the sacrificial layers 171, 172, a gap 250g is obtained in which the open end of the upper surface of the interlayer insulating layer 160 has a width wider than the bottom surface.

[0169] As shown in FIG. 13(g), a gate insulating layer 220 such as a High-k insulating layer is formed to cover the bottom and sidewalls of the gap 250g.

[0170] As shown in FIG. 13(h), a metal layer is further filled into the gap 250g to form a gate electrode 250 whose upper end is wider than its lower end.

[0171] In this manner, the semiconductor device 200 of the second embodiment is manufactured.

[0172] According to the manufacturing method of the semiconductor device 200 of the second embodiment, impurities are not added to the sacrificial layer 172 closer to the substrate 110, the oxidation rate of the sacrificial layer 172 is made lower than that of the upper sacrificial layer 171, and the width of the oxidized sacrificial layer 172 in a direction intersecting the extension direction is made wider than the width of the oxidized sacrificial layer 171. In addition, a spacer layer 140 is formed to cover the side walls of the sacrificial layers 171 and 172 after the oxidation process, and the sacrificial layers 171 and 172 are removed, and the spacer layers 131 and 132 are also removed. This manufacturing method also provides the same effects as the semiconductor device 100 and its manufacturing method of the first embodiment described above.

[0173] In the above-described second embodiment, the sacrificial layer 172, which is a non-doped polysilicon layer or the like, is formed in the lower layer, and the sacrificial layer 171 containing an impurity of a predetermined conductivity type is formed in the upper layer, thereby obtaining the above-described shape of the gate electrode 250. However, also in the manufacturing method of the second embodiment, the lower sacrificial layer 172 may be doped with an impurity in an amount less than that of the upper sacrificial layer 171.

[0174] In addition, the manufacturing method of embodiment 2, in which sacrificial layer 171 with a high amount of impurity added is placed above sacrificial layer 172 that is non-doped or has a low amount of impurity added, and spacer layers 131, 132 are removed together with sacrificial layers 171, 172 after spacer layer 140 is formed, can also be applied to the manufacturing method of semiconductor devices 101 to 103 of variant example 1 described above.

[0175] In this case, a sacrificial layer is formed in which the amount of added impurity decreases from bottom to top, and a configuration can be formed in which the width, including a spacer layer such as a silicon oxide layer formed on the side wall portion of the sacrificial layer, has at least a portion of a tapered shape in which the width increases from bottom to top.

[0176] [Other embodiments] In the above-described first and second embodiments and first and second modifications, for example, polysilicon layers are used as the sacrificial layers 171 to 173. However, layers made of a material other than polysilicon layers, such as amorphous silicon layers, may be used as the sacrificial layers.

[0177] In the above-described first and second embodiments and first and second modifications, impurities are added when the sacrificial layers 171 to 173 are formed. However, the method of doping impurities into the sacrificial layers 171 to 173 is not limited to this. For example, impurities may be doped into the sacrificial layers by ion implantation or the like after a non-doped polysilicon layer or the like is formed.

[0178] At this time, by adjusting the acceleration energy of the ions and performing a subsequent annealing process, it is possible to control the impurity content in the depth direction of the sacrificial layer to be approximately uniform, or to control the impurity content so that it decreases from top to bottom.

[0179] [Note] Preferred aspects of the present invention will be described below.

[0180] (Appendix 1) According to one aspect of the present invention, A gate electrode; an oxide layer covering a sidewall of the gate electrode; a nitride layer covering a side wall of the gate electrode via the oxide layer; The gate electrode is A single conductive layer having an upper end wider than a lower end, The oxide layer is a portion covering a lower end of the gate electrode is thicker than a portion covering an upper end of the gate electrode; A semiconductor device is provided.

[0181] (Appendix 2) In the semiconductor device of Supplementary Note 1, The sidewall of the gate electrode is At least a portion of the surface has a tapered shape that widens upward.

[0182] (Appendix 3) In the semiconductor device of Supplementary Note 2, The oxide layer is The thickness of the tapered portion of the gate electrode becomes thinner from the portion covering the lower end to the portion covering the upper end.

[0183] (Appendix 4) In the semiconductor device of Supplementary Note 1, The semiconductor device further includes a gate insulating layer covering a lower end of the gate electrode and provided between a sidewall of the gate electrode and the oxide layer.

[0184] (Appendix 5) In the semiconductor device of Supplementary Note 4, the gate electrode is a metal layer; The gate insulating layer is a high-k insulating layer.

[0185] (Appendix 6) In the semiconductor device of Supplementary Note 5, The gate electrode is The material contains at least one of titanium, titanium nitride, tantalum, tantalum nitride, lanthanum, aluminum, and titanium aluminum.

[0186] (Appendix 7) In the semiconductor device of Supplementary Note 5, The gate insulating layer is The oxide contains at least one of hafnium oxide and zirconium oxide.

[0187] (Appendix 8) According to another aspect of the present invention, forming first and second semiconductor layers having different contents of a first conductivity type impurity on a substrate in this order; The first and second semiconductor layers are processed into lines extending in a first direction along a surface of the substrate; oxidizing sidewalls on both sides in a second direction intersecting with an extension direction of the first and second semiconductor layers processed into a line shape at an oxidation rate according to the content of the impurity to form a first oxide layer covering the sidewalls of the first semiconductor layer and a second oxide layer covering the sidewalls of the second semiconductor layer; forming a nitride layer covering sidewalls of the first and second semiconductor layers after the oxidation treatment; removing the first and second semiconductor layers to form a gap in a region sandwiched by the nitride layer; filling the gap with a conductive layer to form a gate electrode; A method for manufacturing a semiconductor device is provided.

[0188] (Appendix 9) In the method for manufacturing a semiconductor device according to claim 8, In a thickness direction of the first semiconductor layer, the content of the impurity is made closer to the content of the impurity in the second semiconductor layer toward the second semiconductor layer; and the content of the impurity in the second semiconductor layer varies from the content of the impurity in the first semiconductor layer as it goes away from the first semiconductor layer in the thickness direction of the second semiconductor layer.

[0189] (Appendix 10) In the method for manufacturing a semiconductor device according to claim 8, The content of the impurity in the first semiconductor layer is made higher than that of the second semiconductor layer, or alternatively, the second semiconductor layer is not doped with the impurity and the oxidation rate of the first semiconductor layer is made higher than that of the second semiconductor layer, so that the width of the first semiconductor layer in the second direction after oxidation is made narrower than the width of the second semiconductor layer in the second direction after oxidation.

[0190] (Appendix 11) In the method for manufacturing a semiconductor device according to claim 10, forming the voids in shapes corresponding to shapes of the first and second semiconductor layers after oxidation; The gate electrode is formed to have a first width at a bottom end and a second width at a top end in the second direction that is wider than the first width.

[0191] (Appendix 12) In the method for manufacturing a semiconductor device according to claim 10, The nitride layer is formed on sidewalls of the first and second semiconductor layers via the first and second oxide layers.

[0192] (Appendix 13) In the method for manufacturing a semiconductor device according to claim 10, The first and second oxide layers are removed before forming the nitride layer.

[0193] (Appendix 14) In the method for manufacturing a semiconductor device according to claim 8, The content of the impurity in the first semiconductor layer is made lower than that of the second semiconductor layer, or the impurity is not added to the first semiconductor layer and the oxidation rate of the first semiconductor layer is made lower than that of the second semiconductor layer, so that the width of the first semiconductor layer in the second direction after oxidation is made wider than the width of the second semiconductor layer in the second direction after oxidation.

[0194] (Appendix 15) In the method for manufacturing a semiconductor device according to claim 14, The width in the second direction of the first oxide layer including the first semiconductor layer after oxidation is made narrower than the width in the second direction of the second oxide layer including the second semiconductor layer after oxidation.

[0195] (Appendix 16) In the method for manufacturing a semiconductor device according to claim 15, The first and second semiconductor layers are removed, and the first and second oxide layers are removed.

[0196] (Appendix 17) In the method for manufacturing a semiconductor device according to claim 16, forming the void having a shape corresponding to a shape of the first and second oxide layers including the first and second semiconductor layers after oxidation; The gate electrode is formed to have a third width at a bottom end and a fourth width at a top end in the second direction that is wider than the third width.

[0197] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]

[0198] 10 to 14, 20... transistors, 120 to 123, 220... gate insulating layers, 131 to 133, 140... spacer layers, 150 to 153, 250... gate electrodes, 150a to 152a, 250a... lower regions, 150b to 152b, 250b... upper regions, 151c, 152c... middle regions, 160... interlayer insulating layer, 171 to 173... sacrificial layers, 180... cap layer, CG, CS... contacts.

Claims

1. A gate electrode; an oxide layer covering a sidewall of the gate electrode; a nitride layer covering a side wall of the gate electrode via the oxide layer; The gate electrode is A single conductive layer having an upper end wider than a lower end, The oxide layer is a portion covering a lower end of the gate electrode is thicker than a portion covering an upper end of the gate electrode; Semiconductor device.

2. The gate electrode is a first region having a first width; a second region located above the first region and having a second width greater than the first width; a step is provided on a sidewall portion extending from the first region to the second region; The semiconductor device according to claim 1 .

3. The oxide layer is a first oxide layer provided on a sidewall portion of the first region; a second oxide layer provided on a sidewall portion of the second region and containing a larger amount of impurities of the first conductivity type than at least the first oxide layer; The semiconductor device according to claim 2 .

4. The sidewall of the gate electrode is At least a part of the tapered shape widens upward. The semiconductor device according to claim 1 .

5. The oxide layer is a first conductivity type impurity whose content decreases from a portion covering a lower end of the tapered portion of the gate electrode to a portion covering an upper end of the tapered portion of the gate electrode; The semiconductor device according to claim 4.

6. forming first and second semiconductor layers having different contents of a first conductivity type impurity on a substrate in this order; The first and second semiconductor layers are processed into lines extending in a first direction along a surface of the substrate; oxidizing sidewalls on both sides in a second direction intersecting with an extension direction of the first and second semiconductor layers processed into a line shape at an oxidation rate according to the content of the impurity to form a first oxide layer covering the sidewalls of the first semiconductor layer and a second oxide layer covering the sidewalls of the second semiconductor layer; forming a nitride layer covering sidewalls of the first and second semiconductor layers after the oxidation treatment; removing the first and second semiconductor layers to form a gap in a region sandwiched by the nitride layer; filling the gap with a conductive layer to form a gate electrode; A method for manufacturing a semiconductor device.

7. a content of the impurity in the first semiconductor layer is made higher than that in the second semiconductor layer, or the second semiconductor layer is not doped with the impurity, and an oxidation rate of the first semiconductor layer is made higher than that of the second semiconductor layer, so that a width of the first semiconductor layer in the second direction after oxidation is made narrower than a width of the second semiconductor layer in the second direction after oxidation; The method for manufacturing a semiconductor device according to claim 6 .

8. a content of the impurity in the first semiconductor layer is made lower than that in the second semiconductor layer, or the first semiconductor layer is not doped with the impurity, and an oxidation rate of the first semiconductor layer is made lower than that of the second semiconductor layer, so that a width of the first semiconductor layer in the second direction after oxidation is made wider than a width of the second semiconductor layer in the second direction after oxidation; The method for manufacturing a semiconductor device according to claim 6 .

9. a width in the second direction of the first oxide layer including the first semiconductor layer after the oxidation is made narrower than a width in the second direction of the second oxide layer including the second semiconductor layer after the oxidation; The method for manufacturing a semiconductor device according to claim 8 .

10. removing the first and second semiconductor layers and removing the first and second oxide layers; The method for manufacturing a semiconductor device according to claim 9 .

Citation Information

Patent Citations

  • Replacement gate process for making a semiconductor device that includes a metal gate electrode

    US20050214987A1

  • Forming integrated circuits with replacement metal gate electrodes