Semiconductor device

By using oxide semiconductor transistors with low off-state current and capacitive elements, the issue of power consumption and operational delays in semiconductor integrated circuits is addressed, ensuring efficient data retention and reduced power consumption.

JP2024133666AActive Publication Date: 2024-10-02SEMICON ENERGY LAB CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2024109827
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2011-05-13
Filing Date
2024-07-08
Publication Date
2024-10-02
Estimated Expiration
2031-08-02

AI Technical Summary

Technical Problem

In semiconductor integrated circuits with a large number of elements, power consumption increases due to leakage current in memory circuits, leading to memory content erasure and operational delays when power gating is applied, which reduces the effectiveness of power gating in reducing overall power consumption.

Method used

Incorporating transistors with a channel formation region made of oxide semiconductor, which has a wider bandgap and lower intrinsic carrier density, to create transistors with extremely low off-state current, and using capacitive elements to maintain node potential during power gating, ensuring data retention without the need for recalculations.

Benefits of technology

This approach reduces power consumption and operational delays by maintaining data integrity in memory circuits during power gating, allowing seamless resumption of operations without additional calculations.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024133666000001_ABST
    Figure 2024133666000001_ABST
Patent Text Reader

Abstract

To reduce the consumption power and operation delay in a semiconductor integrated circuit.SOLUTION: Each 21_x of a plurality of sequential circuits 21_1 to 21_n included in a storage circuit 10 includes a transistor 31 whose channel formation region is formed of an oxide semiconductor, and a capacitor element 332 that makes a node in a floating state when the transistor is turned off, the node being electrically connected to one electrode. By the channel formation region of the transistor formed of the oxide semiconductor, the transistor whose off current (leak current) is extremely low can be realized. Therefore, by turning off the transistor in a period for which the power source voltage is not supplied to the storage circuit, the potential of the node electrically connected to the one electrode of the capacitor element in that period can be kept constant or substantially constant.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor integrated circuit. In particular, the semiconductor integrated circuit is configured using sequential circuits. A memory circuit is provided, and the supply of a power supply voltage to the memory circuit is controlled (power gating). The present invention relates to a semiconductor integrated circuit capable of [Background technology]

[0002] The scale of semiconductor integrated circuits that have logic circuits is expanding year by year. When the computer was created, it consisted of only a few elements. Now, it consists of a CPU (Central Processor). Processing Unit) and DSP (Digital Signal Processing Unit) Some devices, such as the MOS essor, are made up of tens of millions of elements. Although the power consumption per element has decreased due to the trend toward higher speed and lower voltage, The power consumption of the entire integrated circuit is increasing due to the increasing number of chips. As a method to lower the power consumption, clock gating is used to partially stop the clock, and the frequency of the clock is increased. Methods of reducing the number of power supplies and methods of partially reducing the power supply voltage have been developed.

[0003] Power consumption also includes the charging and dissipating current generated by switching elements such as transistors. Not only the operating power due to discharge, but also the leakage current when the element is off This static power is almost nonexistent in integrated circuits with a small number of elements. However, in integrated circuits with a huge number of elements, the magnitude of this can no longer be ignored. On the other hand, a method for controlling the supply of a power supply voltage to a circuit included in an integrated circuit (power gate This technology has been developed to reduce power consumption due to leakage current. It is possible.

[0004] For example, Patent Document 1 discloses a semiconductor integrated circuit capable of performing power gating. Specifically, a transistor is provided between a logic circuit and a power supply line, By controlling the switching of the transistor, the supply of power supply voltage to the logic circuit is A controllable semiconductor integrated circuit is disclosed. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2005-268694 A Summary of the Invention [Problem to be solved by the invention]

[0006] However, the logic circuit may include a memory circuit (such as a register) that is configured using multiple sequential circuits. If the power gating is performed, the contents stored in the memory circuit are erased. In fact, in the logic circuits included in current semiconductor integrated circuits, It is common sense to use many circuits, and power gating can be used to protect memory contents. In this case, when the supply of power voltage to the memory circuit is resumed, In other words, the same calculations must be performed twice. Therefore, the power consumption reduction effect obtained by power gating is diluted. In addition, the operation of the semiconductor integrated circuit cannot be resumed until the operation is completed. This causes a delay in the operation of the semiconductor integrated circuit.

[0007] In view of the above-described problems, one embodiment of the present invention provides a semiconductor integrated circuit that reduces power consumption. Another object of one embodiment of the present invention is to reduce a delay in operation of a semiconductor integrated circuit. It is an object of one embodiment of the present invention to achieve at least one of the above-described objects. The objective of the present invention is to solve the above problem. [Means for solving the problem]

[0008] At least one of the above-mentioned problems is that in each of a plurality of sequential circuits included in a memory circuit, a transistor in which a channel formation region is formed using an oxide semiconductor; When the node is turned off, the node to which one electrode is electrically connected is in a floating state. This problem can be solved by providing a capacitor. , it has a wider band gap than silicon and a lower intrinsic carrier density than silicon. The channel formation region of a transistor is formed of such an oxide semiconductor. This makes it possible to realize a transistor with extremely low off-state current (leakage current). Therefore, in a period in which the power supply voltage is not supplied to the memory circuit, the transistor By turning off the capacitor, one electrode of the capacitor is electrically connected during the period. The potential of the memory circuit can be kept constant or nearly constant. Therefore, when the supply of the power supply voltage is resumed, it is not necessary to perform calculations again. In the semiconductor integrated circuit of the embodiment, there is no power consumption or operational delay associated with the calculation, etc. , it is possible to solve the above-mentioned problems.

[0009] In addition, the oxide semiconductor has a low solubility in water and hydrogen, which can act as an electron donor. An i-type (intrinsic) semiconductor with reduced impurity concentration or an oxide semiconductor that is as close to i-type as possible (pu Specifically, the oxide semiconductor is preferably a secondary insulator. Secondary Ion Mass Spectrometry (SIMS) The hydrogen concentration measured by the 19 (atoms / cm 3 ) The following are preferred Or 5×10 18 (atoms / cm 3 ) or less, more preferably 5 × 10 17 (ato ms / cm 3 ) or less. In addition, the oxide semiconductor The carrier density is 1×10 14 / cm 3 Less than 1 x 10 12 / cm 3 Less than More preferably, 1×10 11 / cm 3 In addition, the band gap of the oxide semiconductor is is 2 eV or more, preferably 2.5 eV or more, and more preferably 3 eV or more.

[0010] Here, Secondary Ion Mass Spectrometry (SIMS) Here, we will discuss the analysis of hydrogen concentration using SIMS (Single Ink Spectroscopy). In principle, it is difficult to obtain accurate data near the sample surface or near the interface between layers of different materials. It is known that it is difficult to obtain a hydrogen concentration distribution in the thickness direction of the film. When analyzing by SIMS, there is no extreme fluctuation in the values ​​in the area where the target film exists. The average value in the region where a nearly constant value is obtained is adopted as the hydrogen concentration. When the thickness of the film to be measured is small, the hydrogen concentration in the adjacent film affects the thickness. In some cases, it may not be possible to find an area where a certain value can be obtained. In this case, The maximum or minimum value of the hydrogen concentration in the film is adopted as the hydrogen concentration in the film. In the region where the film exists, a mountain-shaped peak having a maximum value and a valley-shaped peak having a minimum value are If no peak exists, the value at the inflection point is taken as the hydrogen concentration.

[0011] The oxide semiconductor is an In-Sn-Ga-Zn-O oxide, which is a quaternary metal oxide. Semiconductors, ternary metal oxides, In-Ga-Zn-O oxide semiconductors, In-Sn-Z nO-based oxide semiconductor, In-Al-Zn-O-based oxide semiconductor, Sn-Ga-Zn-O-based Oxide semiconductors, Al-Ga-Zn-O oxide semiconductors, Sn-Al-Zn-O oxide semiconductors Conductors, binary metal oxides such as In-Zn-O oxide semiconductors and Sn-Zn-O oxides Semiconductors, Al-Zn-O oxide semiconductors, Zn-Mg-O oxide semiconductors, Sn-Mg- O-based oxide semiconductors, In-Mg-O-based oxide semiconductors, In-Ga-O-based oxide semiconductors, and In-O oxide semiconductors, Sn-O oxide semiconductors, Zn-O oxide semiconductors, etc. In the present specification, for example, an In-Sn-Ga-Zn-O system Oxide semiconductors are made of indium (In), tin (Sn), gallium (Ga), and zinc (Zn). The composition ratio is not particularly limited. The semiconductor may include silicon.

[0012] In this specification, the oxide semiconductor is, for example, a compound represented by the chemical formula InMO3(ZnO) m ( m>0), where M is selected from Ga, Al, Mn, and Co. It refers to one or more metallic elements. Effect of the Invention

[0013] In the semiconductor integrated circuit according to one embodiment of the present invention, In each of the plurality of sequential circuits included in the memory circuit, the potential of a specific node The potential held at the node is then stored in the sequential circuit. In other words, the semiconductor device according to one embodiment of the present invention can be In the integrated circuit, when the supply of the power supply voltage to the storage circuit is resumed, the operation is performed again. As a result, the semiconductor integrated circuit according to one embodiment of the present invention can reduce power consumption. It is possible to reduce the number of operations and delays in operation. [Brief description of the drawings]

[0014] [Figure 1] 1A to 1C are diagrams showing configuration examples of a semiconductor integrated circuit. [Diagram 2] 1A to 1H illustrate an example of a method for manufacturing a transistor. [Diagram 3] 1A to 1C are diagrams illustrating a method for measuring the off-state current of a transistor. [Figure 4] (A) and (B) Graph showing transistor characteristics. [Diagram 5] FIG. 13 shows characteristics of a transistor. [Figure 6] FIG. 13 shows characteristics of a transistor. [Figure 7] FIG. 13 shows characteristics of a transistor. [Figure 8] FIG. 13 shows characteristics of a transistor. [Figure 9] FIG. 1 is a diagram showing a specific example of a sequential circuit. [Figure 10] FIG. 13 is a diagram showing an example of the operation of a sequential circuit. [Figure 11] 1A to 1C are diagrams illustrating specific examples of transistors. [Figure 12] 1A to 1H illustrate an example of a specific manufacturing process for a transistor. [Figure 13] 1A to 1G illustrate an example of a specific manufacturing process for a transistor. [Figure 14] 1A to 1D illustrate an example of a specific manufacturing process for a transistor. [Figure 15] 13A to 13C are diagrams illustrating modified examples of a transistor. [Figure 16] 1A and 1B are diagrams showing modified examples of a transistor. [Figure 17] 1A and 1B are diagrams showing modified examples of a transistor. [Figure 18] 1A and 1B are diagrams showing modified examples of a transistor. [Figure 19] 13A to 13C are diagrams illustrating modified examples of a transistor. [Figure 20] 13A to 13C are diagrams illustrating modified examples of a transistor. [Figure 21] 1A to 1C are diagrams illustrating a modified example of the process for forming an oxide semiconductor layer. [Figure 22] FIG. 2 is a diagram showing a specific example of a CPU. [Figure 23] Illustrates the crystal structures of oxide materials. [Figure 24] Illustrates the crystal structures of oxide materials. [Diagram 25] Illustrates the crystal structures of oxide materials. [Figure 26] FIG. 13 is a diagram illustrating the gate voltage dependence of mobility obtained by calculation. [Figure 27] 1A to 1C are diagrams illustrating the gate voltage dependence of drain current and mobility obtained by calculation. [Figure 28] 1A to 1C are diagrams illustrating the gate voltage dependence of drain current and mobility obtained by calculation. [Figure 29] 1A to 1C are diagrams illustrating the gate voltage dependence of drain current and mobility obtained by calculation. [Diagram 30] 1A and 1B are diagrams illustrating a cross-sectional structure of a transistor used in calculation. [Diagram 31] 1A to 1C are graphs showing characteristics of a transistor including an oxide semiconductor. [Diagram 32] 1A and 1B show characteristics of a transistor including an oxide semiconductor. [Diagram 33] 1A and 1B show characteristics of a transistor including an oxide semiconductor. [Diagram 34] XRD spectrum of oxide semiconductor. [Diagram 35] 13A to 13C show characteristics of a transistor including an oxide semiconductor. [Diagram 36] 13A to 13C show characteristics of a transistor including an oxide semiconductor. [Figure 37] 1A and 1B show characteristics of a transistor including an oxide semiconductor. [Figure 38] 1A and 1B are a cross-sectional view and a plan view of a transistor including an oxide semiconductor. [Figure 39] 1A and 1B are a cross-sectional view and a plan view of a transistor including an oxide semiconductor. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. The present invention is not limited to the following description, and may be modified in any form without departing from the spirit and scope of the present invention. It will be readily understood by those skilled in the art that various modifications may be made to the details. The present invention should not be construed as being limited to the description of the following embodiments.

[0016] <Example of the configuration of a semiconductor integrated circuit> First, a configuration example of a semiconductor integrated circuit according to one embodiment of the present invention will be described with reference to FIGS. This will be explained in light of the above.

[0017] FIG. 1(A) is a block diagram showing a configuration example of a semiconductor integrated circuit. The semiconductor integrated circuit includes an arithmetic circuit 10 and data obtained by an arithmetic operation performed by the arithmetic circuit 10. A memory circuit 11 for storing the data, and a power gate for controlling the supply of a power supply voltage to the memory circuit 11. and a control circuit 12.

[0018] FIG. 1B is a specific example of the memory circuit 11 and the power gate control circuit 12 shown in FIG. FIG. 1B is a diagram showing an example of a configuration of a memory circuit 11. The memory circuit 11 shown in FIG. A clock signal (CKB), a high power supply potential (VDD), and a low power supply potential (VSS) are supplied. sequential circuits 21_1 to 21_n (n is a natural number of 3 or more) that can operate in a state where , and can operate when high power supply potential (VDD) and low power supply potential (VSS) are supplied. The circuit has combinational circuits 22_1 to 22_n.

[0019] The sequential circuit 21_1 has an input terminal electrically connected to the input terminal of the memory circuit 11. The output terminal is electrically connected to the input terminal of the combinational circuit 22_1. 1_a (a is a natural number between 2 and n) is an input terminal of the combinational circuit 22_a-1. The output terminal is electrically connected to the input terminal of the combinational circuit 22_a. The combinational circuit 22_n has an output terminal electrically connected to the output terminal of the storage circuit 11. are connected to the network.

[0020] The power gate control circuit 12 shown in FIG. The power gating control signal (PG) is output to the sequential circuits 21_1 to 21_n A set signal (SET), a reset signal (RES), and a first transfer signal ( It is possible to output a first transfer signal (TS1) and a second transfer signal (TS2). The drain of the gate transistor 20 is connected to the sequential circuits 21_1 to 21_n and the combinational circuit 2 Electrically connect to the wiring that supplies the low power supply potential (VSS) to each of 2_1 to 22_n. The source is electrically connected to the low power supply potential (VSS). By switching the power gate transistor 20, the sequential circuits 21_1 to 21_n and and supplying a low power supply potential (VSS) to each of the combinational circuits 22_1 to 22_n. The first transfer signal (TS1) can be controlled by the sequential circuits 21_1 to 21_2. The data stored in 1_n is stored in the channel formation region formed by an oxide semiconductor. A node that is in a floating state when a transistor that is configured as a transistor is turned off. The second transfer signal (TS2) is a signal for transferring the data from the node. This is a signal to

[0021] In FIG. 1B, sequential circuits 21_1 to 21_n and combinational circuit 22_ Regarding the configuration that controls the supply of low power supply potential (VSS) for each of 1 to 22_n However, the configuration for controlling the supply of the high power supply potential (VDD) or the low power supply potential (VSS) and It is also possible to configure the circuit to control the supply of the high power supply potential (VDD) and the low power supply potential (VDD). Each of the introductory circuits 21_1 to 21_n and the combinational circuits 22_1 to 22_n and a high power A power gate transistor is provided between the power supply and the wiring that supplies the potential (VDD). It is also possible.

[0022] FIG. 1C shows a sequential circuit 21_x (x is a natural number between 1 and n) shown in FIG. 1B. FIG. 1C is a diagram illustrating a configuration example of a sequential circuit 21_x having an input terminal The sequential circuit 21_x has an input terminal electrically connected thereto, and an output terminal electrically connected to the output terminal of the sequential circuit 21_x. A flip-flop 30 electrically connected to the input terminal of the flip-flop 30 and a gate of the flip-flop 30 receiving a first transfer signal (TS1). The flip-flop 30 has a source and a drain electrically connected to the wiring that supplies the The other of the source and drain is electrically connected to a first node, which is a node of the a transistor 31 electrically connected to a second node, the second node being a node within the flop 30; One electrode is electrically connected to the second node and the other to the source and drain of transistor 31. The other electrode is electrically connected to a wiring that supplies a fixed potential (Vcom). The transistor 31 has a channel formation region formed of an oxide semiconductor. The fixed potential (Vcom) is the power gate. It is sufficient if the potential always shows a constant value regardless of whether or not the switching is performed. Apply high power supply potential (VDD) or low power supply potential (VSS) as the power supply potential (Vcom). In this case, it is necessary to generate a new potential as a fixed potential (Vcom). It is preferable to use the low power supply potential (VSS) as the fixed potential (Vcom). In this case, the low power supply potential ( VSS) performs power gating on the logic gates included in the flip-flop 30. It is necessary to control so that the signal is supplied even during the period in which the sequential circuit 21_x The low power supply potential (VSS) is supplied as a fixed potential (Vcom) to the flip-flop. A separate supply path for the low power supply potential (VSS) supplied to the logic gates included in group 30 is provided. It would be sufficient to provide such a system.

[0023] In addition, here, one of the source and drain of the transistor 31 (the first node) is A high power supply voltage is applied through transistors constituting logic gates included in flip-flop 30. It is electrically connected to the wiring that supplies the power supply potential (VDD) or the wiring that supplies the low power supply potential (VSS). The other of the source and drain of the transistor 31 and the capacitance element 3 One electrode (second node) of the second transistor cannot be electrically connected to these wirings. For example, the former is a logic gate included in at least flip-flop 30. The transistors constituting the semiconductor device are electrically connected to the source or drain of one of the transistors. The latter is designed to electrically connect all of the sources and drains of the plurality of transistors. and electrically connected to at least one of the gates of the plurality of transistors. That is, in the sequential circuit 21_x shown in FIG. In this case, when the transistor 31 is turned off, the source and The other electrode of the drain and one electrode of the capacitance element 32 are electrically connected to a node (second node). It is possible to make the power supply (the power supply) floating.

[0024] That is, in the sequential circuit 21_x shown in FIG. 1C, the first transfer signal (TS1) When a high-level potential is supplied as The other of the source and drain of the transistor 31 and one of the electrodes of the capacitance element 32 are electrically connected to The data is then transferred to the connected node (second node) and stored in that node. It is possible to do so.

[0025] In this embodiment, each of the sequential circuits 21_1 to 21_n includes a transistor 31 and a capacitor Although the configuration in which the element 32 is provided has been shown, all of the sequential circuits 21_1 to 21_n are That is, the m sequential circuits 21_1 to 21_n need not have the same configuration. A transistor 31 and a capacitance element 32 are provided only in the circuit (m is a natural number equal to or greater than 1 and less than n). In this case, the transistor 31 and the capacitor 32 For a sequential circuit that is not provided with a first transfer signal (TS1) and a second transfer signal Note that (TS2) does not need to be provided.

[0026] <Off-state current of a transistor whose channel formation region is formed using an oxide semiconductor> Here, the off-state current of a transistor in which a channel formation region is formed using an oxide semiconductor is The results of measuring the leakage current are shown below.

[0027] First, a method for manufacturing the transistor used in the above measurement will be described with reference to FIGS.

[0028] First, a silicon nitride layer having a thickness of 100 nm and an oxide layer having a thickness of 150 nm are formed on a glass substrate 50. An underlayer 51 consisting of a stack of silicon nitride layers was formed by a CVD method (see FIG. 2(A)). ).

[0029] Next, a tungsten layer having a thickness of 100 nm is formed on the underlayer 51 by a sputtering method. Furthermore, the tungsten layer was selectively etched using a photolithography method. A gate layer 52 was formed by etching (see FIG. 2(B)).

[0030] Next, a silicon oxynitride layer having a thickness of 100 nm is deposited on the underlayer 51 and the gate layer 52. A gate insulating layer 53 made of SiO 2 was formed by the CVD method (see FIG. 2(C)).

[0031] Next, a 25 nm-thick oxide semiconductor layer is formed on the gate insulating layer 53 by a sputtering method. The oxide semiconductor layer was formed by the following method. A metal oxide target with a ratio of 1:1:2 [mol] was used. The composition was performed under the conditions of substrate temperature 200°C, chamber pressure 0.6 Pa, DC power supply 5 kW, oxygen and Argon mixed atmosphere (oxygen flow rate 50sccm, argon flow rate 50sccm) Further, the oxide semiconductor layer is selected by photolithography. Then, the oxide semiconductor layer 54 was formed by selectively etching the silicon substrate 51 (see FIG. 2D).

[0032] Then, the mixture was heated at 450°C for 1 hour in a mixed atmosphere of nitrogen and oxygen (80% nitrogen, 20% oxygen). The heat treatment was carried out.

[0033] Next, the gate insulating layer 53 was selectively etched using a photolithography method ( (Not shown). Note that this etching step is performed to remove the gate layer 52 and the conductive layer that will be formed later. This is a process for forming a contact hole.

[0034] Next, a titanium layer having a thickness of 100 nm is formed on the gate insulating layer 53 and the oxide semiconductor layer 54. A 200 nm thick aluminum layer and a 100 nm thick titanium layer are sputtered. The laminate was then selectively etched using a photolithography method. By this, a source layer 55a and a drain layer 55b were formed (see FIG. 2(E)).

[0035] Next, a heat treatment was carried out at 300° C. for 1 hour in a nitrogen atmosphere.

[0036] Next, the gate insulating layer 53, the oxide semiconductor layer 54, the source layer 55a, and the drain layer 5 A protective insulating layer 56 made of a silicon oxide layer having a thickness of 300 nm was formed on the insulating layer 5b. The protective insulating layer 56 was selectively etched using a photolithography method (see FIG. 2(F)). Note that the etching process is performed on the gate layer, the source layer, the drain layer, and the This is a step for forming contact holes to a conductive layer to be formed.

[0037] Next, an acrylic layer having a thickness of 1.5 μm is applied onto the protective insulating layer 56, and the acrylic layer is A planarization insulating layer 57 was formed by selectively exposing the resulting film to light (see FIG. 2(G)). Heat treatment at 250℃ for 1 hour in a nitrogen atmosphere creates a flat insulating layer made of an acrylic layer. Layer 57 was baked.

[0038] Next, a titanium layer having a thickness of 200 nm is formed on the planarizing insulating layer 57 by a sputtering method. Furthermore, the titanium layer was selectively etched using a photolithography method. Thus, a conductive layer (not shown) connected to the gate layer 52 and a conductive layer connected to the source layer 55a are formed. A conductive layer 58b connected to the drain layer 55b and the gate electrode 58a was formed (see FIG. 2H).

[0039] Next, a heat treatment was carried out at 250° C. for 1 hour in a nitrogen atmosphere.

[0040] Through the above steps, the transistor used in the above measurement was manufactured.

[0041] Furthermore, the method for calculating the off-state current value using the characteristic evaluation circuit used in the above measurement is as follows: will be explained.

[0042] The current measurement using the characteristic evaluation circuit will be explained with reference to Figure 3. FIG. 2 is a diagram for explaining a circuit.

[0043] First, the circuit configuration of the characteristic evaluation circuit will be described with reference to FIG. 3(A). FIG. 3(A) shows 1 is a circuit diagram showing a circuit configuration of a characteristic evaluation circuit.

[0044] The characteristic evaluation circuit shown in FIG. 3A includes a plurality of measurement systems 801. In this example, eight measurement systems 801 are connected in parallel. By using multiple measurement systems 801, multiple measurements can be performed simultaneously. .

[0045] The measurement system 801 includes a transistor 811, a transistor 812, a capacitance element 813, It includes a transistor 814 and a transistor 815.

[0046] Transistor 811, transistor 812, transistor 814, and transistor 8 15 is an N-channel field effect transistor.

[0047] A voltage V1 is input to one of the source and drain of the transistor 811. A voltage Vext_a is input to the gate of the transistor 811. The transistor 811 stores a charge This is an injection transistor.

[0048] One of the source and drain of the transistor 812 is connected to the source and drain of the transistor 811. The other of the source and drain of the transistor 812 is connected to a voltage The voltage V2 is input to the gate of the transistor 812, and the voltage Vext_b is input to the gate of the transistor 813. The transistor 812 is a transistor for evaluating leakage current. The current is a leakage current including an off-state current of a transistor.

[0049] One electrode of the capacitor 813 is connected to the other of the source and drain of the transistor 811. The other electrode of the capacitor 813 is connected to a ground potential V1, and a voltage V2 is input to the other electrode of the capacitor 813. The voltage V2 is 0V.

[0050] A voltage V3 is input to one of the source and drain of the transistor 814. The gate of the transistor 814 is connected to the other of the source and drain of the transistor 811 . Note that the gate of the transistor 814 and the other of the source and drain of the transistor 811 , one of the source and drain of the transistor 812, and one electrode of the capacitor 813 The connection point with is also referred to as node A. Here, voltage V3 is 5V.

[0051] One of the source and drain of the transistor 815 is connected to the source and drain of the transistor 814. The other of the source and drain of the transistor 815 is connected to a voltage V4 is input, and the voltage Vext_c is input to the gate of the transistor 815. Here, the voltage Vext_c is 0.5V.

[0052] Furthermore, the measurement system 801 is connected to the other of the source and drain of the transistor 814 and The voltage at the connection point between the source and drain of the resistor 815 is the output voltage Vout. Output.

[0053] Here, the transistor 811 is formed by the manufacturing method described with reference to FIG. A transistor having a channel length L=10 μm and a channel width W=10 μm is used.

[0054] The transistors 814 and 815 are the transistors fabricated as described with reference to FIG. A transistor having a channel length L=3 μm and a channel width W=100 μm formed by the method. Use Sta.

[0055] At least the transistor 812 has a gate layer 52 and a semiconductor layer 53 as shown in FIG. The source layer 55a does not overlap with the gate layer 52 and the drain layer 55b, and is offset by a width of 1 μm. By providing the offset region, it is possible to reduce parasitic capacitance. Furthermore, the transistor 812 can be formed of six transistors each having a different channel length L and channel width W. A sample of one transistor (also called SMP) is used (see Table 1).

[0056] [Table 1]

[0057] As shown in Figure 3(A), a transistor for charge injection and a transistor for leakage current evaluation are By providing the transistor for leak current evaluation separately from the transistor for charge injection, It can always be left off.

[0058] In addition, a transistor for charge injection and a transistor for leakage current evaluation are provided separately. This allows each transistor to be sized appropriately. The channel width W of the transistor for evaluating the current is set to the channel width W of the transistor for charge injection. By making it larger than the leakage current evaluation transistor, it is possible to evaluate characteristics other than the leakage current. This makes it possible to relatively reduce the leakage current component of the valence circuit. The leakage current of the transistor can be measured with high accuracy. In addition, since it is not necessary to turn on the transistor for leak current evaluation, the channel formation There is also no effect of voltage fluctuations at node A due to some of the charge in the region flowing into node A.

[0059] Next, the leakage current measurement method for the characteristic evaluation circuit shown in Figure 3(A) is explained using Figure 3(C). FIG. 3(C) shows a leakage current measurement method using the characteristic evaluation circuit shown in FIG. 3(A). 1 is a timing chart for explaining a method.

[0060] The leakage current measurement method using the characteristic evaluation circuit shown in FIG. 3(A) is performed during the write period and the hold period. The operation in each period is explained below.

[0061] In the writing period, the voltage Vext_b is set so that the transistor 812 is in an off state. Input the write voltage Vw as the voltage V1. Then, the voltage Vext_a is set to a voltage such that the transistor 811 is in an on state for a certain period of time. Input the voltage VH (5V). This causes charge to accumulate at node A, and the voltage at node A Then, the voltage Vext_a is set to the same value as the write voltage Vw. Then, the voltage V is input so that the transistor 811 is turned off. Input SS (0V).

[0062] During the hold period, the voltage at node A changes due to the change in the amount of charge held by node A. The amount of change in the voltage is measured. From the amount of change in the voltage, the source and drain of the transistor 812 are The current flowing between node A and node B can be calculated. It is possible to measure the amount of change in voltage at node A.

[0063] At this time, the charge of node A is stored and the amount of change in the voltage of node A is measured (storage and measurement operation). First, the first accumulation and measurement operation is repeated 15 times. In the accumulation and measurement operation of 1, a voltage of 5 V was input as the write voltage Vw during the write period. Then, the retention period is one hour. Next, the second accumulation and measurement operation is repeated twice. In the second accumulation and measurement operation, a voltage of 3.5 V is applied as the write voltage Vw during the write period. Then, input the value and hold for 50 hours in the hold period. Next, perform the third accumulation and measurement operation once. In the third accumulation and measurement operation, a voltage of 4.5 V is applied as the write voltage Vw during the write period. Input the value and hold for 10 hours. By repeating the accumulation and measurement operations, It can be confirmed that the measured current value is a value in a steady state. Then, the current I flowing through node A A Of these, the transient current (which decreases over time from the start of measurement) As a result, the leakage current can be measured with higher accuracy. It is possible.

[0064] In general, the voltage at node A, V A is expressed as a function of the output voltage Vout by equation (1). can be.

[0065]

number

[0066] Also, the charge Q at node A A is the voltage at node A, VA , capacitance C connected to node A A , Using a constant (const), it is expressed as in equation (2). Here, Capacity C A is the sum of the capacitance of the capacitance element 813 and the capacitance components other than the capacitance element 813.

[0067]

number

[0068] Current I at node A A is the charge flowing into (or out of) node A Since this is the time derivative of the current I A is expressed as equation (3).

[0069]

number

[0070] In this example, Δt is set to approximately 54,000 sec. Capacity C A The leakage current I A To ask for This makes it possible to obtain the leakage current of the characteristic evaluation circuit.

[0071] Next, the output voltage measurement results by the measurement method using the above-mentioned characteristic evaluation circuit and the The leakage current value of the characteristic evaluation circuit calculated using this method will be explained with reference to FIG.

[0072] FIG. 4(A) shows the above measurement results for transistors in SMP4, SMP5, and SMP6. The relationship between the elapsed time Time and the output voltage Vout in the first accumulation and measurement operation is shown. FIG. 4B shows the elapsed time Time for the above measurement and the current I calculated by the measurement. A The output voltage Vout fluctuates after the measurement starts, and it takes a while to reach a steady state. It is clear that more than 10 hours are required to achieve this.

[0073] FIG. 5 shows the estimated values ​​of SMP1 to SMP6 from the values ​​obtained by the above measurements. In Fig. 5, the relationship between the voltage and leakage current of node A in an SMP4 is shown. When the voltage of node A is 3.0V, the leakage current is 28yA / μm. Since the off-current of the transistor 812 is also included, the off-current of the transistor 812 is also 28 yA. / μm or less.

[0074] 6 to 8 show the results of the measurements at 85° C., 125° C., and 150° C. The relationship between the voltage and leakage current at node A in SMP1 to SMP6 is shown in FIG. As shown in FIG. 8, even at 150° C., the leakage current was less than 100 zA / μm. It turns out that it is below.

[0075] As described above, a transistor in which a channel formation region is formed using an oxide semiconductor is used. In the characteristic evaluation circuit, the leakage current is sufficiently low, so that the off-current of the transistor In addition, the off-state current of the transistor is However, it is clear that the

[0076] <Regarding the semiconductor integrated circuit disclosed in this specification> The semiconductor integrated circuit disclosed in this specification is configured to operate when a power supply voltage is not supplied to a memory circuit. In each of the plurality of sequential circuits included in the memory circuit, a specific node ( The other of the source and drain of the transistor 31 and one of the capacitors 32 shown in FIG. The potential of the node (the node to which the other electrode is electrically connected) can be maintained. The potential held at the node can correspond to the data held in the sequential circuit. That is, in the semiconductor integrated circuit disclosed in the present specification, the memory circuit When the supply of power voltage to the power supply is resumed, there is no need to perform calculations again. The semiconductor integrated circuit disclosed in the specification aims to reduce power consumption and operational delays. It is possible.

[0077] <Example> A specific example of the above-mentioned semiconductor integrated circuit will be described with reference to FIGS.

[0078] <Sequential circuit 21_x> FIG. 9 is a diagram showing a specific example of the sequential circuit 21_x shown in FIG. The first circuit 21_x includes a transistor 31, a capacitance element 32, and NAND gates 210a to 210c. 10f, AND gates 211a and 211b, and switches 212a to 212d. The connections between the various circuits are self-evident when referring to FIG. 9. A detailed description of the connection relationship of 1_x will be omitted. A node electrically connected to the other electrode of the input terminal and one electrode of the capacitance element 32 is referred to as a node N. The data holding operation in the node N will be described below.

[0079] FIG. 10 shows a data storage circuit in the node N of the sequential circuit 21_x shown in FIG. 10 is a diagram showing an example of an operation when the holding is performed. In the operation example shown in FIG. T1 and T3 are periods during which the power gating signal (PG) indicates a high-level potential (power supply Period T1 is a period during which the power gating signal (PG) indicates a low level potential. This is the period during which power is cut off.

[0080] In a period T1, the data held by the sequential circuit 21_x is read out prior to clock gating. In order to determine the data, a clock signal (CK) is supplied to the sequential circuit 21_x. Then, a high-level potential is supplied as the first transfer signal (TS1). As a result, the data held by the sequential circuit 21_x is transferred to the node N.

[0081] During a period T2, the power supply voltage is supplied to each logic gate of the sequential circuit 21_x. Therefore, the data of the sequential circuit 21_x is in an undefined state (Z). The data held in node N does not disappear.

[0082] In the period T3, a high-level potential is supplied as the second transfer signal (TS2). As a result, the data in the sequential circuit 21_x is restored. Next, the clock signal (CK) is supplied. By restarting the supply of the sequential circuit 21_x, the operation of the semiconductor integrated circuit having the sequential circuit 21_x is restarted early. It is possible.

[0083] <Transistor> The above-mentioned semiconductor integrated circuit is composed of a large number of transistors. The number of transistors required for each type of transistor is It is possible to appropriately select the appropriate value depending on the characteristics, etc. For example, in the above-mentioned semiconductor integrated circuit, The logic included in the sequential circuits 21_1 to 21_n and the combinational circuits 22_1 to 22_n The transistor that constitutes the gate is required to operate at high speed. Examples of the material include single crystal silicon, polycrystalline silicon, and gallium arsenide (GaAs). It is preferable to use a transistor in which a channel forming region is formed of a compound semiconductor. In addition, the power gate transistor 20 is required to have a low off-current (leak current). Therefore, the transistor has a channel formed of the above-mentioned oxide semiconductor. It is preferable to apply a transistor in which the formation region is configured.

[0084] In view of the above, an example of a transistor included in a semiconductor integrated circuit will be described. In general, transistors and and an example of a semiconductor integrated circuit including a transistor formed using an oxide semiconductor. show.

[0085] FIG. 11 is a diagram illustrating an example of a transistor included in a semiconductor integrated circuit. The transistor 160 includes a channel forming region 11 provided in a substrate 100 including a semiconductor material. A pair of impurity regions 114a and 116 are provided to sandwich a channel forming region 116 therebetween. 4b and a pair of high concentration impurity regions 120a, 120b (collectively referred to as impurity regions A gate insulating layer 108 is provided on the channel forming region 116. A gate layer 110 provided on the edge layer 108 and a solenoid electrically connected to the impurity region 114a. The semiconductor device has a source layer 130a and a drain layer 130b electrically connected to the impurity region 114b. do.

[0086] A sidewall insulating layer 118 is provided on the side surface of the gate layer 110. In the region of the substrate 100 including the semiconductor material that does not overlap with the sidewall insulating layer 118, There are a pair of high concentration impurity regions 120a and 120b. A pair of metal compound regions 124a and 124b are present on the substrate 100. An element isolation insulating layer 106 is provided on the transistor 160 so as to surround the transistor. An interlayer insulating layer 126 and an interlayer insulating layer 128 are provided to cover the transistor 160. The source layer 130a and the drain layer 130b are formed between the interlayer insulating layer 126 and the interlayer insulating layer 128. The metal compound regions 124a and 124b are electrically connected to one of the pair of metal compound regions 124a and 124b through an opening formed in the metal compound region 124a. That is, the source layer 130a is connected to the high concentration The drain layer 130b is electrically connected to the impurity region 120a and the impurity region 114a. The high concentration impurity region 120b and the impurity region 114 are connected to each other through the metal compound region 124b. b is electrically connected to

[0087] The transistor 164 shown in FIG. 11 includes a gate layer 136 provided on an interlayer insulating layer 128. d, a gate insulating layer 138 provided on the gate layer 136d, and an oxide semiconductor layer 140 provided on the oxide semiconductor layer 140; The source layer 142a and the drain layer 142b are electrically connected to the layer 140. .

[0088] Here, the gate layer 136d is embedded in the insulating layer 132 formed on the interlayer insulating layer 128. In addition, like the gate layer 136d, the transistor 160 is The electrode layer 136a contacts the source layer 130a and the electrode layer 136b contacts the drain layer 130b. 136b is formed.

[0089] In addition, a protective layer is provided on the transistor 164 so as to be in contact with part of the oxide semiconductor layer 140. A protective insulating layer 144 is provided, and an interlayer insulating layer 146 is provided on the protective insulating layer 144. Here, the protective insulating layer 144 and the interlayer insulating layer 146 are provided with the source layer 142a and An opening is provided that reaches the drain layer 142b, and the source layer 1 An electrode layer 150d in contact with the drain layer 42a and an electrode layer 150e in contact with the drain layer 142b are formed. In addition, the gate insulating layer 138, the protective insulating layer 140, and the electrode layer 150d and the electrode layer 150e are An electrode layer 136a is in contact with the electrode layer 136a through an opening provided in the edge layer 144 and the interlayer insulating layer 146. An electrode layer 150b is formed in contact with layer 150a and electrode layer 136b.

[0090] Here, impurities such as hydrogen are sufficiently removed from the oxide semiconductor layer 140, and the oxide semiconductor layer 140 is highly purified. Specifically, the hydrogen concentration in the oxide semiconductor layer 140 is 5×10 19 (atoms / cm 3 Note that the hydrogen concentration in the oxide semiconductor layer 140 is 5×10 18 (atoms / cm 3 ) or less, and 5×10 17 (atoms / cm 3 ) or less It is more preferable that the hydrogen concentration in the oxide semiconductor layer 140 is determined by the secondary ion mass. Secondary Ion Mass Spectroscop (SIMS) y).

[0091] An insulating layer 152 is provided on the interlayer insulating layer 146. Electrode layers 154a, 154b, and 154d are provided so as to be enclosed within the space. The electrode layer 154a is in contact with the electrode layer 150a, and the electrode layer 154b is in contact with the electrode layer 150b. and electrode layer 150d, and electrode layer 154d is in contact with electrode layer 150e.

[0092] As shown in FIG. 11, the drain layer 130b of the transistor 160 is Through the electrode layer 136b, the electrode layer 150b, the electrode layer 154b, and the electrode layer 150d, The source layer 142 a of the transistor 164 is electrically connected to the source layer 142 a.

[0093] <Production process example> Next, an example of a method for manufacturing the transistor 160 and the transistor 164 will be described. First, a method for fabricating the P-type transistor 160 will be described below with reference to FIG. Then, a method for manufacturing the transistor 164 will be described with reference to FIGS. 13 and 14. do.

[0094] First, a substrate 100 containing a semiconductor material is prepared (see FIG. 12(A)). The substrate 100 may be a single crystal semiconductor substrate or a multi-crystal substrate such as silicon or silicon carbide. A crystalline semiconductor substrate, a compound semiconductor substrate such as silicon germanium, or an SOI substrate is suitable. Here, a single crystal silicon substrate can be used as the substrate 100 containing a semiconductor material. In general, an "SOI substrate" is an insulating surface. A substrate having a silicon semiconductor layer on its surface. This also includes substrates having a semiconductor layer made of a material other than silicon on the surface. In other words, the semiconductor layer of the "SOI substrate" is not limited to a silicon semiconductor layer. In addition, in the SOI substrate, a semiconductor layer is provided on an insulating substrate such as a glass substrate via an insulating layer. This also includes configurations in which

[0095] A protective layer 102 is formed on the substrate 100 to serve as a mask for forming an element isolation insulating layer. (See FIG. 12(A)). The protective layer 102 is made of, for example, silicon oxide or silicon nitride. An insulating layer made of silicon oxide or silicon oxynitride can be used. Before and after, n-type conductivity is imparted to control the threshold voltage of the transistor. An impurity element or an impurity element that imparts p-type conductivity may be added to the substrate 100. In the case of silicon, impurities that give n-type conductivity include, for example, phosphorus and arsenic. In addition, impurities that impart p-type conductivity include, for example, boron, arsenic, and the like. Aluminum, gallium, etc. can be used.

[0096] Next, etching is performed using the protective layer 102 as a mask. The part of the substrate 100 in the uncovered area (exposed area) is removed. A semiconductor region 104 is formed (see FIG. 12(B)). It is preferable to use a gas such as zinc etchant, but wet etching may also be used. The etching solution can be appropriately selected depending on the material to be etched.

[0097] Next, an insulating layer is formed so as to cover the semiconductor region 104, and an insulating layer is formed in a region overlapping the semiconductor region 104. The insulating layer in the region is selectively removed to form an element isolation insulating layer 106 (FIG. 12(B) The insulating layer is made of silicon oxide, silicon nitride, silicon oxynitride, etc. The insulating layer is removed by chemical mechanical polishing (CMP). There are polishing processes such as polishing and etching, After the formation of the semiconductor region 104 or after the formation of the element isolation insulating layer 106, Afterwards, the protective layer 102 is removed.

[0098] Next, an insulating layer is formed on the semiconductor region 104, and a layer containing a conductive material is formed on the insulating layer. do.

[0099] The insulating layer will later become the gate insulating layer, and is deposited using CVD, sputtering, etc. Obtained silicon oxide, silicon nitride oxide, silicon nitride, hafnium oxide, aluminum oxide It is preferable to use a single layer or a multilayer structure of a film containing tungsten oxide, tantalum oxide, etc. The surface of the semiconductor region 104 is oxidized or nitrided by plasma treatment or thermal oxidation treatment. The insulating layer may be formed by the high density plasma treatment. This is done using a mixture of rare gases such as Xe and oxygen, nitrogen oxide, ammonia, nitrogen, etc. The thickness of the insulating layer is not particularly limited, but may be, for example, 1 nm or more and 100 nm or less. m or less.

[0100] The layer containing the conductive material is a metal material such as aluminum, copper, titanium, tantalum, or tungsten. The insulating layer can be formed of a semiconductor material such as polycrystalline silicon that contains a conductive material. The method for forming the layer containing the conductive material is not particularly limited, and examples thereof include a deposition method, Various film formation methods such as CVD, sputtering, and spin coating can be used. Here, an example of forming a layer containing a conductive material using a metal material will be described. This shall be shown.

[0101] Thereafter, the insulating layer and the layer containing the conductive material are selectively etched to form the gate insulating layer 10. 8. Form the gate layer 110 (see FIG. 12(C)).

[0102] Next, an insulating layer 112 is formed to cover the gate layer 110 (see FIG. 12(C)). Boron (B), phosphorus (P), arsenic (As), etc. are added to the semiconductor region 104 to form a shallow junction depth. In this case, a pair of impurity regions 114a and 114b having the same length are formed (see FIG. 12(C)). By forming the impurity regions 114a and 114b, the gate insulating layer 108 of the semiconductor region 104 A channel forming region 116 is formed in the lower part (see FIG. 12(C)). The concentration of impurities can be set appropriately, but when transistors are highly miniaturized, In this embodiment, after the insulating layer 112 is formed, the concentration of the insulating layer 112 is preferably high. The present invention employs a process for forming a pair of impurity regions 114a and 114b in the The step of forming the insulating layer 112 may be performed after the regions 114a and 114b are formed.

[0103] Next, the sidewall insulating layer 118 is formed (see FIG. 12(D)). The insulating layer 118 is formed by forming an insulating layer so as to cover the insulating layer 112 and then applying anisotropic By applying a highly efficient etching process, the structure can be formed in a self-aligned manner. During this process, the insulating layer 112 is partially etched to expose the upper surface of the gate layer 110 and a pair of impurities. Preferably, the top surfaces of the object regions 114a and 114b are exposed.

[0104] Next, the gate layer 110, the pair of impurity regions 114a and 114b, and the sidewall insulating layer An insulating layer is formed to cover the pair of impurity regions 114a and 114b. Adding boron (B), phosphorus (P), arsenic (As), etc. to a part of b creates a pair of high concentration Impurity regions 120a and 120b are formed (see FIG. 12(E)). Then, the insulating layer is The gate layer 110, the sidewall insulating layer 118, and the pair of high concentration impurity regions 120 are removed. A metal layer 122 is formed so as to cover the metal layers 120a, 120b, etc. (see FIG. 12(E)). 2 is formed using various film formation methods such as vacuum deposition, sputtering, and spin coating. The metal layer 122 can react with the semiconductor material that constitutes the semiconductor region 104 to form a It is preferable to form the insulating layer using a metal material that forms a low-resistance metal compound. Examples of materials include titanium, tantalum, tungsten, nickel, cobalt, and platinum. be.

[0105] Next, a heat treatment is performed to react the metal layer 122 with the semiconductor material. A pair of metal compound regions 124a, 124b are in contact with the high concentration impurity regions 120a, 120b. As the gate layer 110, polycrystalline silicon or the like is used. When using the metal compound region, the portion of the gate layer 110 in contact with the metal layer 122 is also provided with the metal compound region. will be formed.

[0106] As the heat treatment, for example, heat treatment by irradiation with a flash lamp can be used. Of course, other heat treatment methods may be used, but chemical reactions involving the formation of metal compounds are preferred. In order to improve the controllability of the reaction, it is necessary to use a method that allows for very short heat treatment times. The metal compound region is preferably formed by a reaction between a metal material and a semiconductor material. The metal compound region is formed in the region having a sufficiently high electrical conductivity. By doing so, the electrical resistance can be sufficiently reduced, and the element characteristics can be improved. After metal compound regions 124a, 124b are formed, metal layer 122 is removed.

[0107] Next, an interlayer insulating layer 126 and an interlayer insulating film 127 are formed to cover the respective components formed by the above-mentioned steps. The interlayer insulating layer 126 and the interlayer insulating layer 128 are formed by using an oxide film. Silicon oxide, silicon nitride, silicon oxide, hafnium oxide, aluminum oxide, The insulating layer 11 can be formed using a material containing an inorganic insulating material such as tantalum chloride. It is also possible to form the layer using an organic insulating material such as polycarbonate or acrylic. The structure has a two-layer structure of an interlayer insulating layer 126 and an interlayer insulating layer 128. After the interlayer insulating layer 128 is formed, the surface of the interlayer insulating layer 128 may be subjected to a process such as CMP or etching. It is desirable to flatten the surface by using a method such as flattening.

[0108] Thereafter, openings are formed in the interlayer insulating layer, the openings reaching the pair of metal compound regions 124a and 124b. In the opening, a source layer 130a and a drain layer 130b are formed (FIG. 12( The source layer 130a and the drain layer 130b are formed by, for example, forming a P After forming a conductive layer using the VD method or CVD method, the layer is then processed by etching or CMP. The insulating layer can be formed by removing a part of the conductive layer using a method.

[0109] When the source layer 130a and the drain layer 130b are formed, the surfaces of the layers are preferably flat. For example, a titanium film or a titanium nitride film is formed in the region including the opening. When a tungsten film is formed to fill the opening after a thin layer is formed, By using the CMP, unnecessary tungsten, titanium, titanium nitride, etc. are removed, and In this way, the flatness of the surface of the source layer 130a and the drain layer 130b can be improved. By planarizing the surface including the layer 130b, it is possible to form good electrodes, wiring, It becomes possible to form an insulating layer, a semiconductor layer, etc.

[0110] In this case, the source layer 130 in contact with the pair of metal compound regions 124a and 124b is Although only the a and drain layers 130b are shown, they function as wiring in this process. An electrode layer and the like may also be formed. There is no particular limitation on the material that can be used as the conductive material, and various conductive materials can be used. For example, molybdenum, titanium, chromium, tantalum, tungsten, aluminum, Conductive materials such as copper, neodymium, and scandium can be used.

[0111] In this manner, a transistor 160 is formed using the substrate 100 including a semiconductor material. After the above steps, electrodes, wiring, an insulating layer, etc. may be further formed. By adopting a multilayer wiring structure having a laminated structure of an interlayer insulating layer and a conductive layer, A highly integrated circuit can be provided.

[0112] Next, a transistor 164 is formed on the interlayer insulating layer 128 using FIG. 13 and FIG. 13 and 14 show the process of forming various electrodes on the interlayer insulating layer 128. Since the figure shows the manufacturing process of the electrode layer and the transistor 164, the transistor 164 The transistor 160 and other components present below are omitted.

[0113] First, an insulating layer 13 is formed on the interlayer insulating layer 128, the source layer 130a, and the drain layer 130b. The insulating layer 132 is formed by using a PVD method, a CVD method, or the like. In addition, silicon oxide, silicon nitride oxide, silicon nitride, and hafnium oxide can be used. The insulating layer is formed using a material containing an inorganic insulating material such as tungsten oxide, aluminum oxide, or tantalum oxide. It is possible.

[0114] Next, the insulating layer 132 is etched to reach the source layer 130a and the drain layer 130b. An opening is formed. At this time, an opening is also formed in a region where a gate layer 136d is to be formed later. Then, a conductive layer 134 is formed so as to fill the opening (see FIG. 13(B)). The opening can be formed by a method such as etching using a mask. The mask can be formed by a method such as exposure using a photomask. Either wet etching or dry etching may be used for the etching. From the viewpoint of process, it is preferable to use dry etching. The conductive layer 134 can be formed by a film formation method such as a PVD method or a CVD method. Materials that can be used include molybdenum, titanium, chromium, tantalum, tungsten, Conductive materials such as aluminum, copper, neodymium, and scandium, as well as their alloys and compounds (e.g. nitrides) and the like.

[0115] More specifically, for example, a thin titanium film is formed in the area including the opening by a PVD method, and C After forming a thin titanium nitride film by the VD method, a tungsten film is deposited to fill the opening. The titanium film formed by the PVD method is The oxide film at the interface is reduced, and the lower electrode layer (here, the source layer 130a and the drain layer 130b) is It also has the function of reducing the contact resistance with the titanium nitride film that is subsequently formed. It has a barrier function that suppresses the diffusion of conductive materials. After forming the barrier film, a copper film may be formed by plating.

[0116] After the conductive layer 134 is formed, the conductive layer 134 is removed by a method such as etching or CMP. 134 is removed to expose the insulating layer 132, and the electrode layers 136a, 136b, A gate layer 136d is formed (see FIG. 13C). When the electrode layer 136a, the electrode layer 136b, and the gate layer 136d are formed by removing the In this manner, the insulating layer 132, the electrode layer 136a, By planarizing the surfaces of the electrode layer 136b and the gate layer 136d, It becomes possible to form good electrodes, wiring, insulating layers, semiconductor layers, and the like.

[0117] Next, a layer is formed so as to cover the insulating layer 132, the electrode layer 136a, the electrode layer 136b, and the gate layer 136d. A gate insulating layer 138 is formed on the gate insulating layer 138 (see FIG. 13(D)). The gate insulating layer 138 can be formed by a deposition method, a sputtering method, or the like. , silicon oxide, silicon nitride, silicon oxynitride, silicon nitride oxide, aluminum oxide, hafnium oxide It is preferable to form the insulating film so as to contain aluminum, tantalum oxide, gallium oxide, etc. The insulating layer 138 may have a single layer structure or a multilayer structure. Silicon oxide nitride was produced by plasma CVD using silane (SiH4), oxygen, and nitrogen as the The gate insulating layer 138 can be formed from a material other than silicon. The thickness of the gate insulating layer 138 is preferably Although not limited thereto, the thickness can be, for example, 10 nm or more and 500 nm or less. In this case, for example, a first gate insulating layer having a film thickness of 50 nm to 200 nm and a first gate It is preferable to laminate a second gate insulating layer having a thickness of 5 nm to 300 nm on the gate insulating layer. be.

[0118] Next, an oxide semiconductor layer is formed over the gate insulating layer 138 and etched using a mask. The oxide semiconductor layer is processed by a method such as etching to form an island-shaped oxide semiconductor layer 140. (See FIG. 13(E)).

[0119] The oxide semiconductor used is one that contains at least indium (In) or zinc (Zn). It is preferable that the oxide semiconductor contains In and Zn. As a stabilizer to reduce the variation in the electrical characteristics of transistors In addition, it is preferable to have gallium (Ga). Also, tin (S n) as a stabilizer. It is preferable that the stabilizer is aluminum (Al). It is nice.

[0120] Other stabilizers include the lanthanides lanthanum (La) and cerium. (Ce), praseodymium (Pr), neodymium (Nd), samarium (Sm), europium Eu, Gadolinium (Gd), Terbium (Tb), Dysprosium (Dy), Luminium (Ho), Erbium (Er), Thulium (Tm), Ytterbium (Yb), It may contain one or more of lutetium (Lu).

[0121] For example, oxide semiconductors include indium oxide, tin oxide, zinc oxide, and oxides of binary metals. In-Zn oxides, Sn-Zn oxides, Al-Zn oxides, Zn-Mg oxides, oxides, Sn-Mg oxides, In-Mg oxides, In-Ga oxides, ternary metals In-Ga-Zn oxide (also written as IGZO), In-Al-Zn oxides, In-Sn-Zn oxides, Sn-Ga-Zn oxides, Al-Ga-Zn oxides Oxide, Sn-Al-Zn oxide, In-Hf-Zn oxide, In-La-Zn oxide oxides, In-Ce-Zn oxides, In-Pr-Zn oxides, In-Nd-Zn oxides In-Sm-Zn oxide, In-Eu-Zn oxide, In-Gd-Zn oxide , In-Tb-Zn oxide, In-Dy-Zn oxide, In-Ho-Zn oxide, In-Er-Zn oxide, In-Tm-Zn oxide, In-Yb-Zn oxide, I n-Lu-Zn ​​oxide, In-Sn-Ga-Zn oxide, which is an oxide of a quaternary metal, In-Hf-Ga-Zn oxide, In-Al-Ga-Zn oxide, In-Sn-Al -Zn oxide, In-Sn-Hf-Zn oxide, In-Hf-Al-Zn oxide It can be used.

[0122] In addition, for example, In-Ga-Zn oxide is a material containing In, Ga, and Zn as main components. The ratio of In, Ga, and Zn does not matter. Metal elements other than Ga and Zn may be included.

[0123] In addition, as an oxide semiconductor, InMO3(ZnO) m (m>0 and m is not an integer In addition, M is selected from Ga, Fe, Mn, and Co. In addition, the oxide semiconductor is In3SnO 5(ZnO) n A material expressed as (n>0, and n is an integer) may be used.

[0124] For example, In:Ga:Zn=1:1:1 (=1 / 3:1 / 3:1 / 3) or In: In-Ga-Zn system with an atomic ratio of Ga:Zn=2:2:1 (=2 / 5:2 / 5:1 / 5) The oxide or an oxide having a similar composition can be used. 1:1:1(=1 / 3:1 / 3:1 / 3), In:Sn:Zn=2:1:3(=1 / 3: 1 / 6:1 / 2) or In:Sn:Zn=2:1:5(=1 / 4:1 / 8:5 / 8) It is preferable to use an In-Sn-Zn oxide having an atomic ratio of 100% or an oxide having a composition close to that.

[0125] However, it is not limited to these, and the required semiconductor characteristics (mobility, threshold, variation, etc.) In order to obtain the required semiconductor characteristics, Carrier concentration, impurity concentration, defect density, atomic ratio of metal elements to oxygen, interatomic bond length, density It is preferable to set the degree, etc., appropriately.

[0126] For example, high mobility can be obtained relatively easily with In-Sn-Zn oxides. However, in the case of In-Ga-Zn oxides, the mobility can be improved by reducing the defect density in the bulk. It can be raised.

[0127] For example, the atomic ratio of In, Ga, and Zn is In:Ga:Zn=a:b:c(a+b +c=1), the atomic ratio of the oxide is In:Ga:Zn=A:B:C (A+B+ C=1) is close to the oxide composition when a, b, and c are (a-A) 2 +(b-B) 2 +(c-C) 2 ≦r 2 The above condition is satisfied, and r can be set to, for example, 0.05. The same is true for other oxides. .

[0128] The oxide semiconductor may be single-crystalline or non-single-crystalline. In the latter case, it may be amorphous or polycrystalline. In addition, the structure may include a portion having crystallinity in the amorphous state, or may be non-amorphous. It is also fine.

[0129] Amorphous oxide semiconductors can be used to obtain flat surfaces relatively easily. This can reduce interface scattering when a transistor is fabricated using this, and can be fabricated relatively easily and relatively High mobility can be obtained.

[0130] In addition, in a crystalline oxide semiconductor, defects in the bulk can be further reduced. By improving the flatness of the surface, it is possible to obtain a mobility higher than that of an amorphous oxide semiconductor. In order to improve the flatness of the surface, it is preferable to form an oxide semiconductor on a flat surface. Specifically, the average surface roughness (Ra) is 1 nm or less, preferably 0.3 nm or less, and more preferably It is preferable to form it on the surface with a thickness of 0.1 nm or less.

[0131] Note that Ra is the centerline average roughness defined in JIS B0601 applied to the surface. This is an extension to three dimensions, and is the "average of the absolute value of the deviation from the reference surface to the specified surface." This can be expressed as the "value obtained by dividing the total number of bits by the number of bits" and is defined by the following formula.

[0132]

number

[0133] In the above, S0 is the measurement surface (coordinates (x1, y1) (x1, y2) (x2, y 1) The area of ​​the rectangular region bounded by the four points (x2, y2), Z0 indicates the average height of the measurement surface. Ra is measured by an atomic force microscope (AFM). It can be evaluated using a microscope.

[0134] Here, an In-Ga-Zn-O metal oxide target is used as the oxide semiconductor layer. In this case, an amorphous oxide semiconductor layer is formed by a sputtering method.

[0135] Examples of targets for forming the oxide semiconductor layer 140 by a sputtering method include For example, a metal oxide target mainly composed of zinc oxide can be used. Metal oxide target containing In, Ga, and Zn (composition ratio: In2O3:Ga 2O3:ZnO=1:1:1[mol ratio], In:Ga:Zn=1:1:0.5[ato m ratio) can also be used. The target is In:Ga:Zn=1:1:1 [atom ratio] or In:Ga:Z A target having a composition ratio of n=1:1:2 [atom ratio] may be used. The filling rate of the oxide target is 90% or more and 100% or less, preferably 95% or more (for example, 99 By using a metal oxide target with a high filling rate, a dense oxide A semiconductor layer is formed.

[0136] In addition, when an In-Zn-O-based material is used for the oxide semiconductor layer 140, the substrate The composition ratio of the get is In:Zn=50:1 to 1:2 in atomic ratio (converted to molar ratio). In2O3:ZnO=25:1 to 1:4), preferably In:Zn=20:1 to 1:1 ( In terms of molar ratio, In2O3:ZnO=10:1 to 1:2), and more preferably In Zn = 15:1 to 1.5:1 (converted to molar ratio In2O3:ZnO = 15:2 to For example, the metal oxide ter used in the formation of In-Zn-O oxide semiconductors The get is that when the atomic ratio is In:Zn:O=X:Y:Z, Z>1.5X+Y.

[0137] In addition, In-Sn-Zn oxide can be called ITZO, and the target used is The composition ratio of In:Sn:Zn is 1:2:2, 2:1:3, 1:1:1, or For example, an oxide target with a ratio of 20:45:35 is used.

[0138] The oxide semiconductor layer is formed in a rare gas (typically, argon) atmosphere, an oxygen atmosphere, or Alternatively, it is preferable to use a mixed atmosphere of a rare gas (typically argon) and oxygen. Specifically, impurities such as hydrogen, water, hydroxyl groups, and hydrides are preferably present at a level of several ppm. It is preferable to use a high-purity gas in which the concentration of contaminants has been reduced to about a few ppb.

[0139] When the oxide semiconductor layer is formed, the substrate is held in a treatment chamber that is kept in a reduced pressure state. The temperature is set to 100°C or higher and 600°C or lower, preferably 200°C or higher and 400°C or lower. By forming the oxide semiconductor layer while heating, the impurity concentration in the oxide semiconductor layer Also, damage caused by sputtering is reduced. The residual moisture in the chamber is removed and a sputtering gas from which hydrogen and water have been removed is introduced to form a metal oxide. The oxide semiconductor layer is formed by using the target as a target. It is preferable to use an adsorption type vacuum pump. For example, a cryopump or an ion pump is used. A titanium sublimation pump or a titanium sublimation pump can be used as the exhaust means. A cryopump with a cold trap may be used. The deposition chamber is filled with, for example, hydrogen atoms and compounds containing hydrogen atoms such as water (H2O) (preferably Since the oxide semiconductor formed in the film formation chamber is exhausted, The concentration of impurities contained in the layer can be reduced.

[0140] The formation conditions are, for example, a distance of 100 mm between the substrate and the target and a pressure of 0. 6 Pa, DC power 0.5 kW, oxygen atmosphere (oxygen flow rate 100%) If a pulsed direct current (DC) power supply is used, The thickness of the oxide semiconductor layer is preferably 2 nm. The thickness is set to 200 nm or more, preferably 5 nm or more and 30 nm or less. The appropriate thickness varies depending on the semiconductor material, so the thickness should be selected appropriately depending on the material used. Good.

[0141] Before the oxide semiconductor layer is formed by a sputtering method, argon gas is introduced. The reverse sputtering is performed to generate plasma by sputtering the silicon dioxide particles 134. It is preferable to remove dust. Here, the reverse sputtering is the same as the normal sputtering. Instead of bombarding the sputtering target with ions, the treatment surface is bombarded with ions. This is a method of modifying the surface by bombarding the surface with ions. The method involves applying a high-frequency voltage to the processing surface in an argon atmosphere to generate plasma near the substrate. In addition, nitrogen, helium, oxygen, etc. can be used instead of argon atmosphere. You may use it.

[0142] The oxide semiconductor layer may be etched by either dry etching or wet etching. Of course, both can be used in combination. In order to etch the material, the etching conditions (etching gas, etching solution, etc.) are adjusted according to the material. Etching time, temperature, etc. are set appropriately.

[0143] The etching gas used in the dry etching is, for example, a gas containing chlorine (a chlorine-based gas). , e.g. chlorine (Cl2), boron trichloride (BCl3), silicon tetrachloride (SiCl4), tetrachloride Carbon (CCl4, etc.) and gases containing fluorine (fluorine-based gases, for example, tetrafluoroethylene). Carbon fluoride (CF4), sulfur hexafluoride (SF6), nitrogen trifluoride (NF3), trifluoromethan Hydrogen (CHF3), hydrogen bromide (HBr), oxygen (O2), and helium ( A gas containing a rare gas such as argon (Ar) or argon (He) may also be used.

[0144] As a dry etching method, parallel plate type RIE (Reactive Ion Etc. fing method and ICP (Inductively Coupled Plasma) Inductively coupled plasma etching can be used. It can be etched into the desired shape. As shown in the figure, the etching conditions (the amount of power applied to the coil-type electrode, the amount of power applied to the electrode on the substrate side) The power consumption, electrode temperature on the substrate side, etc. are set appropriately.

[0145] The etching solution used for wet etching is a mixture of phosphoric acid, acetic acid, and nitric acid. In addition, an etching solution such as ITO07N (manufactured by Kanto Chemical Co., Ltd.) can be used. It's fine.

[0146] Next, the oxide semiconductor layer is preferably subjected to a first heat treatment. The temperature of the first heat treatment can be set to 1000° C., so that the oxide semiconductor layer can be dehydrated or dehydrogenated. The temperature is set to 300° C. or higher and 750° C. or lower, preferably 400° C. or higher and lower than the distortion point of the substrate. For example, The substrate is placed in an electric furnace using a resistance heating element or the like, and the oxide semiconductor layer 140 is heated in a nitrogen atmosphere. A heat treatment is performed at 450° C. for 1 hour in an atmosphere. During this time, the oxide semiconductor layer 140 is Ensure that there is no contact with the gas and that no water or hydrogen is re-mixed.

[0147] The heat treatment device is not limited to an electric furnace, and may be any device that utilizes heat conduction from a medium such as a heated gas, or The heating device may be a device that heats the object to be treated by thermal radiation. For example, a GRTA (Gas Rapid Thermal Anneal) equipment, LRTA (Lamp Rapid Thermal Annealing equipment such as RTA (Rapid Thermal Annealing) The LRTA device can be used with halogen lamps, metal halide lamps, etc. lamp, xenon arc lamp, carbon arc lamp, high pressure sodium lamp, high pressure A device that heats the workpiece by radiating light (electromagnetic waves) emitted from a lamp such as a mercury lamp. The GRTA device is a device that performs heat treatment using high-temperature gas. An inert gas that does not react with the workpiece during heat treatment, such as a rare gas such as argon or nitrogen. Sexual gas is used.

[0148] For example, the first heat treatment is performed by subjecting the substrate to a base in an inert gas heated to a high temperature of 650° C. to 700° C. The plate is put in and heated for a few minutes, after which the GRTA process is carried out, in which the plate is removed from the inert gas. GRTA treatment allows high-temperature heat treatment in a short time. Since this is a heat treatment, it can be applied even under temperature conditions that exceed the distortion point of the substrate.

[0149] The first heat treatment is performed in a vacuum chamber mainly composed of nitrogen or a rare gas (helium, neon, argon, etc.). It is preferable to carry out the process in an atmosphere that does not contain water, hydrogen, etc. For example, the purity of nitrogen or rare gases such as helium, neon, and argon introduced into the heat treatment device may be , 6N (99.9999%) or more, preferably 7N (99.99999%) or more (i.e. That is, the impurity concentration is 1 ppm or less, preferably 0.1 ppm or less.

[0150] Depending on the conditions of the first heat treatment or the material of the oxide semiconductor layer, the oxide semiconductor layer may become crystalline. For example, the crystallinity is 90% or more, or 80% or more. In some cases, the oxide semiconductor layer may be a microcrystalline oxide semiconductor layer having a crystallinity of 0% or more. Depending on the material of the oxide semiconductor layer, the oxide semiconductor layer may be an amorphous oxide semiconductor layer that does not contain crystalline components. There are cases like this.

[0151] In addition, microcrystals (grain size 1 nm) are formed in the amorphous oxide semiconductor (for example, the surface of the oxide semiconductor layer). and 20 nm or less (typically 2 nm or more and 4 nm or less) are mixed. In some cases.

[0152] In addition, the electrical characteristics of the oxide semiconductor layer can be changed by arranging microcrystals in the amorphous state. For example, it is possible to use an In-Ga-Zn-O metal oxide target. When forming an oxide semiconductor layer, the crystal of In2Ga2ZnO7, which has electrical anisotropy, is used. By forming a microcrystal part in which grains are oriented, the electrical characteristics of an oxide semiconductor layer are changed. can be done.

[0153] More specifically, for example, the c-axis of In2Ga2ZnO7 is perpendicular to the surface of the oxide semiconductor layer. By orienting the oxide semiconductor layer in a specific direction, the electrical conductivity in the direction parallel to the surface of the oxide semiconductor layer is improved. As a result, the insulating property in a direction perpendicular to the surface of the oxide semiconductor layer can be improved. Such a microcrystal portion has a function of suppressing the intrusion of impurities such as water and hydrogen into the oxide semiconductor layer. Possesses the ability.

[0154] Note that the oxide semiconductor layer having the above-described microcrystal portion is an oxide semiconductor layer formed by GRTA treatment. The Zn content can be reduced by heating the surface of the Zn alloy. By using a sputtering target smaller than the amount of .

[0155] Here, the c-axis is oriented and has a triangular or hexagonal shape as viewed from the ab plane, surface, or interface direction. The metal atoms are arranged in layers or metal atoms and oxygen atoms are arranged in layers along the c-axis. The layers are arranged in a layered fashion, and the orientation of the a-axis or b-axis is different on the ab plane (rotating around the c-axis). CAAC: C-Axis Aligned Crystal An oxide containing the compound will be described.

[0156] In a broad sense, oxides containing CAAC are non-single crystals that are perpendicular to the ab plane. When viewed from the outside, the atomic arrangement is a triangle, a hexagon, an equilateral triangle, or an equilateral hexagon, and the c-axis direction is perpendicular to the When viewed from any direction, it contains a phase in which metal atoms are arranged in layers, or metal atoms and oxygen atoms are arranged in layers. This refers to oxides.

[0157] CAAC is not a single crystal, but it is not composed of only amorphous matter. AAC contains crystallized parts (crystalline parts), but the boundary between one crystalline part and another crystalline part is Sometimes it is not possible to clearly distinguish

[0158] When oxygen is contained in CAAC, a part of the oxygen may be replaced by nitrogen. The c-axes of the individual crystals that make up C are aligned in a certain direction (e.g., the substrate surface supporting the CAAC, The CAAC may be aligned in a direction perpendicular to the surface of the CAAC. The normal of the ab plane of each crystal part is in a certain direction (e.g., the substrate plane supporting the CAAC, C) may be oriented in a direction perpendicular to the surface.

[0159] CAAC can be a conductor, a semiconductor, or an insulator depending on its composition. Also, depending on the composition, it may be transparent or opaque to visible light. Or something like that.

[0160] An example of such a CAAC is a film-like CAAC that is perpendicular to the film surface or the supporting substrate surface. When observed from a certain direction, a triangular or hexagonal atomic arrangement is observed, and when the cross section of the film is observed, Then, a layered arrangement of metal atoms or metal atoms and oxygen atoms (or nitrogen atoms) is observed. Examples of such crystals include

[0161] An example of a crystal structure contained in CAAC will be described in detail with reference to FIGS. 23 to 25. 23 to 25, the upward direction is the c-axis direction, and the direction perpendicular to the c-axis direction is the The intersecting plane is the ab plane. Note that when simply referring to the upper half and the lower half, the ab plane is the boundary. The upper and lower halves of the

[0162] In Figure 23(A), one hexacoordinate In atom and six tetracoordinate oxygen atoms (hereafter The structure shown has four-coordinated oxygen atoms. Here, one metal atom has one adjacent oxygen atom. The structure showing only the atoms is called a small group. The structure in Figure 23(A) has an octahedral structure, For simplicity, the structure is shown in a plane. The small group shown in Figure 23(A) has a charge of 0.

[0163] In Figure 23(B), one pentagonal Ga atom and three trigonal oxygen atoms (hereafter The structure has a tricoordinated O and two tetracoordinated O adjacent to Ga. , both of which exist on the ab plane. There is one each in the upper and lower halves of Figure 23(B). There is a 4-coordinate O. In also has 5-coordinate In, so the structure shown in Figure 23(B) can be formed. The small group shown in Figure 23(B) has a charge of 0.

[0164] FIG. 23(C) shows a structure having one tetracoordinate Zn and four tetracoordinate O atoms adjacent to the Zn. The structure of Fig. 23(C) shows one tetracoordinate O in the upper half and three tetracoordinate O in the lower half. Or, in the upper half of Figure 23(C), there are three 4-coordinate O atoms, and in the lower half, one There may be four-coordinated O. The small group shown in Figure 23(C) has a charge of 0.

[0165] FIG. 23(D) shows a structure having one hexacoordinate Sn atom and six tetracoordinate O atoms adjacent to the Sn atom. The structure of Figure 23(D) shows three tetracoordinate Os in the upper half and three tetracoordinate Os in the lower half. The small group shown in Figure 23(D) has a charge of +1.

[0166] Figure 23(E) shows a small group containing two Zn atoms. The upper half of Figure 23(E) shows one Zn atom. The small group shown in Figure 23(E) has four tetrahedral O atoms, and the lower half has one tetrahedral O atom. The charge of the atom is -1.

[0167] Here, a collection of multiple small groups is called a medium group, and a collection of multiple medium groups is called a is called a large group (also called a unit cell).

[0168] Here, we will explain the rules for combining these small groups. The upper three O atoms of the 6-coordinate In have three adjacent In atoms downward, Each of the three O atoms has three neighboring In atoms in the upward direction. Each O has one adjacent Ga in the downward direction, and each O in the lower half has one adjacent Ga in the upward direction. One O atom in the upper half of the 4-coordinated Zn has one neighboring Zn atom downward, and the three O atoms in the lower half Each O has three neighboring Zn atoms in the upward direction. Thus, the four-coordinated structure of the metal atom in the upward direction The number of O atoms is equal to the number of adjacent metal atoms below the O atoms. The number of 4-coordinated O atoms is equal to the number of adjacent metal atoms above the O atoms. Therefore, the sum of the number of adjacent metal atoms below and the number of adjacent metal atoms above is 4. Therefore, the number of 4-coordinated O atoms above a metal atom and the number of 4-coordinated O atoms below another metal atom are When the sum of the number of O and metal atoms is 4, the two small groups containing metal atoms can bond together. For example, a hexacoordinated metal atom (In or Sn) can be bonded to the lower half of the tetracoordinated O atom. In this case, since there are three tetracoordinated O atoms, the five-coordinated metal atom (Ga or In) or the four-coordinated It will bond to one of the coordinated metal atoms (Zn).

[0169] Metal atoms with these coordination numbers are bonded via tetracoordinated oxygen in the c-axis direction. In addition, multiple small groups are bonded together so that the total charge of the layer structure is zero. The medium group is composed of these.

[0170] Figure 24(A) shows a model diagram of the middle group that constitutes the In-Sn-Zn-O system layer structure. FIG. 24(B) shows a large group consisting of three medium groups. FIG. 24C shows the atomic arrangement when the layer structure of FIG. 24B is observed from the c-axis direction.

[0171] In FIG. 24(A), for simplicity, the tricoordinate O is omitted, and only the number of the tetracoordinate O is shown. For example, the upper and lower halves of Sn each contain three tetrahedral O atoms. Similarly, in FIG. 24(A), the upper and lower halves of In are Each of the has one 4-coordinate O atom, which is shown as 1 in a circle. Similarly, in Figure 2 In 4(A), there is one tetracoordinate O in the lower half and three tetracoordinate O in the upper half. A Zn atom with one tetracoordinate O atom in the upper half and three tetracoordinate O atoms in the lower half is n.

[0172] In FIG. 24(A), the middle group, which is made up of an In-Sn-Zn-O-based layer structure, is Sn has three tetrahedral O atoms in the upper half and one tetrahedral O atom in the lower half. It bonds to In in the upper and lower halves, and the In has three tetracoordinate O in the upper half. It bonds to Zn, and three tetracoordinate O atoms are bonded to the upper half of the Zn via one tetracoordinate O atom in the lower half of the Zn. The In is bonded to a Zn atom with one tetracoordinated O in the upper half. It bonds to a small group of two via a tetracoordinate O in the lower half of this small group. The structure is such that three tetracoordinate O atoms are bonded to the Sn atoms in the upper and lower halves. Multiple groups combine to form larger groups.

[0173] Here, for the three-coordinate O and four-coordinate O, the charge per bond is -0. 667, -0.5. For example, In (6 or 5 coordinate), Zn ( The charges of Sn (four-coordinated), Sn (five-coordinated or six-coordinated) are +3, +2, and +4, respectively. Therefore, the small group containing Sn has a charge of +1. Therefore, the layer structure containing Sn To achieve this, a charge of -1 is required to cancel out the charge of +1. As shown in Fig. 23(E), there is a small group containing two Zn atoms. For example, If there is one small group containing Zn and one small group containing 2 Zn, the charges are cancelled out. Therefore, the total charge of the layer structure can be set to zero.

[0174] Specifically, the large group shown in FIG. 24(B) is repeated to form the In-Sn-Z The resulting In-SnO crystal (In2SnZn3O8) can be obtained. The layer structure of the n-Zn-O system is In2SnZn2O7(ZnO). m (m is 0 or a natural number. ) can be expressed by the formula:

[0175] In addition, there are also oxides of four-element metals, such as In-Sn-Ga-Zn oxides, In-Ga-Zn oxide (also written as IGZO), which is an oxide of a ternary metal, In -Al-Zn oxide, Sn-Ga-Zn oxide, Al-Ga-Zn oxide, Sn- Al-Zn oxide, In-Hf-Zn oxide, In-La-Zn oxide, In- Ce-Zn oxide, In-Pr-Zn oxide, In-Nd-Zn oxide, In-S m-Zn oxide, In-Eu-Zn oxide, In-Gd-Zn oxide, In-Tb -Zn-based oxide, In-Dy-Zn-based oxide, In-Ho-Zn-based oxide, In-Er- Zn-based oxide, In-Tm-Zn-based oxide, In-Yb-Zn-based oxide, In-Lu-Z n-based oxides, binary metal oxides such as In-Zn-based oxides, Sn-Zn-based oxides, and A l-Zn oxide, Zn-Mg oxide, Sn-Mg oxide, In-Mg oxide, The same applies when In-Ga oxides are used.

[0176] For example, in Figure 25(A), a middle group model with an In-Ga-Zn-O layer structure is shown. A diagram of the data is shown.

[0177] In FIG. 25(A), the middle group, which is made up of an In-Ga-Zn-O-based layer structure, is In the upper half and lower half have three tetracoordinate O atoms, and in the lower half have one tetracoordinate O atom. It bonds to the Zn in the molecule, and the tetracoordinate O atom is connected to the Zn via the three tetracoordinate O atoms in the lower half of the Zn. Each of them bonds to Ga in the upper and lower halves, and one 4-coordinate O in the lower half of the Ga is The structure is such that three tetracoordinate O atoms are bonded to the In atoms in the upper and lower halves via the Several of these medium groups combine to form large groups.

[0178] Figure 25(B) shows a large group consisting of three medium groups. 25(B) shows the atomic arrangement when the layer structure of FIG. 25(B) is observed from the c-axis direction.

[0179] Here, the charges of In (6 or 5 coordinates), Zn (4 coordinates), and Ga (5 coordinates) are Since they are +3, +2, and +3, respectively, they are in a small group that contains either In, Zn, or Ga. The charge is 0. Therefore, if these small groups are combined, The total charge is always zero.

[0180] The middle group, which is composed of the In-Ga-Zn-O layer structure, is shown in FIG. The combination of middle groups with different arrangements of In, Ga, and Zn is not limited to the same middle group. Large groups are also possible.

[0181] The first heat treatment for the oxide semiconductor layer 140 is performed to process the oxide semiconductor layer 140 into an island-shaped oxide semiconductor layer 140. In that case, the first heat treatment may be performed on the oxide semiconductor layer before the first heat treatment. The substrate is then removed from the mold and a photolithography process is performed.

[0182] The heat treatment may have a dehydration or dehydrogenation effect on the oxide semiconductor layer 140. Such dehydration treatment, dehydrogenation treatment, etc. The oxidation treatment is performed by forming a source layer and a drain layer on the oxide semiconductor layer 140 after the oxide semiconductor layer is formed. After laminating the layers, or after forming a protective insulating layer on the source and drain layers, etc. In addition, such dehydration and dehydrogenation treatments can be carried out in the following steps: The process may be performed not only once but also multiple times.

[0183] Next, the source layer 142a and the drain layer 142b are formed in contact with the oxide semiconductor layer 140. b is formed (see FIG. 13(F)). The source layer 142a and the drain layer 142b are oxidized. A conductive layer is formed to cover the compound semiconductor layer 140, and then the conductive layer is selectively etched. It can be formed by

[0184] The conductive layer is formed by PVD methods such as sputtering and plasma CVD methods. The conductive layer can be formed by using a CVD method. The conductive layer can be formed of aluminum, An element selected from the group consisting of chromium, copper, tantalum, titanium, molybdenum, and tungsten, or any of the above. The alloys containing the elements manganese, magnesium, zirconium, etc. can be used. Alternatively, a material selected from one or more of aluminum, beryllium, and thorium may be used. In addition, aluminum, titanium, tantalum, tungsten, molybdenum, chromium, neodymium A material containing a single or multiple combinations of elements selected from the group consisting of ruthenium, zinc, and scandium may also be used. The conductive layer may have a single layer structure or a laminated structure of two or more layers. Single layer structure of aluminum film containing silicon, two-layer structure of titanium film laminated on aluminum film and a three-layer structure in which a titanium film, an aluminum film and a titanium film are laminated.

[0185] In addition, when etching the conductive layer, the oxide semiconductor layer 140 is not removed. The materials and etching conditions are adjusted as appropriate. Therefore, in this step, a part of the oxide semiconductor layer 140 is etched, and a groove (a recess In some cases, the oxide semiconductor layer may have a gate insulating film.

[0186] In addition, between the oxide semiconductor layer 140 and the source layer 142a or between the oxide semiconductor layer 140 and the drain layer 142b, An oxide conductive layer may be formed between the drain layer 142b and the source layer 142b. The metal layer for forming the drain layer 142a and the drain layer 142b is formed continuously (continuously). The oxide conductive layer can function as a source or drain region. By providing such an oxide conductive layer, the resistance of the source region or the drain region can be reduced. This allows high speed operation of the transistor.

[0187] In order to reduce the number of masks used and the number of processes, the exposure method is used in which the transmitted light has multiple intensities. A resist mask is formed using a multi-tone optical mask, and this is used for etching. The resist mask formed using the multi-tone mask has a plurality of thicknesses. The shape becomes stepped, and the shape can be further deformed by ashing. It can be used in multiple etching processes to process different patterns. By using the multi-tone mask, resist patterns corresponding to at least two different patterns can be produced. Therefore, the number of exposure masks can be reduced, and the corresponding The photolithography process can also be eliminated, simplifying the process.

[0188] After the above process, plasma treatment using gas such as N2O, N2, or Ar may be performed. It is preferable that the exposed surface of the oxide semiconductor layer is treated by the plasma treatment. Water and other substances adhering to the surface are removed. In addition, plasma treatment is performed using a mixture of oxygen and argon gas. may be carried out.

[0189] Next, the protective insulating layer 1 in contact with a part of the oxide semiconductor layer 140 is removed without exposing it to the air. 44 is formed (see FIG. 13(G)).

[0190] The protective insulating layer 144 is formed by removing impurities such as water and hydrogen from the protective insulating layer 144 using a method such as sputtering. The thickness of the insulating layer is at least 10 mm. The thickness is set to 1 nm or more. Examples of materials that can be used for the protective insulating layer 144 include silicon oxide, nitride, and the like. Silicon nitride, silicon oxynitride, silicon nitride oxide, etc. Also, the structure can be a single layer structure. The substrate temperature when forming the protective insulating layer 144 is room temperature or higher. The temperature is preferably 300°C or less, and the atmosphere is a rare gas (typically argon) atmosphere, an oxygen atmosphere, or the like. It is preferable to use a nitrogen atmosphere or a mixed atmosphere of a rare gas (typically argon) and oxygen. do.

[0191] If hydrogen is contained in the protective insulating layer 144, the hydrogen may penetrate into the oxide semiconductor layer 140 or The hydrogen extracts oxygen from the oxide semiconductor layer 140, and the oxide semiconductor layer 14 The back channel side of MOSFET 0 becomes low-resistance, which may result in the formation of a parasitic channel. Therefore, in order to prevent the protective insulating layer 144 from containing hydrogen as much as possible, the formation method is It is important not to use

[0192] In addition, it is preferable to form the protective insulating layer 144 while removing residual moisture in the processing chamber. This is because the oxide semiconductor layer 140 and the protective insulating layer 144 contain hydrogen, hydroxyl groups, or moisture. This is to prevent this from happening.

[0193] To remove residual moisture in the processing chamber, it is preferable to use an adsorption type vacuum pump. For example, cryopumps, ion pumps, and titanium sublimation pumps can be used. The exhaust means is preferably a turbo pump with a cold trap. The deposition chamber evacuated using a cryopump may contain hydrogen atoms, water (H 2O), etc., which contain hydrogen atoms, are removed, so the protective insulation formed in the film formation chamber The concentration of impurities contained in the edge layer 144 can be reduced.

[0194] The sputtering gas used in forming the protective insulating layer 144 may be hydrogen, water, a hydroxyl group, or Impurities such as hydrides are removed to a few ppm (preferably a few ppb). It is preferable to use a high purity gas.

[0195] Then, a second heat treatment (preferably 2 It is preferable to carry out the heating at a temperature between 00°C and 400°C, for example between 250°C and 350°C. For example, a second heat treatment is performed at 250° C. for 1 hour in a nitrogen atmosphere. The variation in the electrical characteristics of the transistors can be reduced.

[0196] In addition, heat treatment is performed in air at 100°C to 200°C for 1 hour to 30 hours. This heat treatment may be performed by holding the temperature constant or by heating from room temperature to 100°C. Repeat heating to a temperature of 200°C or more and cooling from the heating temperature to room temperature several times. This heat treatment may be carried out under reduced pressure before the formation of the protective insulating layer. If the heat treatment is performed under reduced pressure, the heating time can be shortened. This may be carried out instead of the second heat treatment, or may be carried out before or after the second heat treatment.

[0197] Next, an interlayer insulating layer 146 is formed on the protective insulating layer 144 (see FIG. 14(A)). The interlayer insulating layer 146 can be formed by using a PVD method, a CVD method, or the like. Silicon, silicon oxide nitride, silicon nitride, hafnium oxide, aluminum oxide, tantalum oxide The interlayer insulating layer 146 can be formed using a material containing an inorganic insulating material such as tantalum. After formation, the surface can be flattened by methods such as CMP or etching. desirable.

[0198] Next, electrodes are formed on the interlayer insulating layer 146, the protective insulating layer 144, and the gate insulating layer 138. Openings reaching the layer 136a, the electrode layer 136b, the source layer 142a, and the drain layer 142b Then, a conductive layer 148 is formed so as to fill the opening (see FIG. 14B). The openings can be formed by a method such as etching using a mask. It can be formed by a method such as exposure using a photomask. Either wet etching or dry etching may be used for the etching. From this viewpoint, it is preferable to use dry etching. The conductive layer 148 can be formed by a deposition method such as a deposition method or a CVD method. Materials that can be used include molybdenum, titanium, chromium, tantalum, tungsten, and aluminum. Conductive materials such as tungsten, copper, neodymium, and scandium, as well as their alloys and compounds (e.g. (e.g. nitrides) and the like.

[0199] Specifically, for example, a thin titanium film is formed in the area including the opening by the PVD method, and then CVD After forming a thin titanium nitride film by the method, a tungsten film is formed to fill the opening. Here, the titanium film formed by the PVD method has an interface The oxide film of the lower electrode (here, the electrode layer 136a, the electrode layer 136b, and the source layer 136a) is reduced. 42a, and the drain layer 142b). The titanium nitride film thus formed has a barrier function that suppresses the diffusion of conductive materials. Even if a copper film is formed by plating after forming a barrier film using tungsten or titanium nitride, good.

[0200] After the conductive layer 148 is formed, the conductive layer 14 is removed by a method such as etching or CMP. 8 is removed to expose the interlayer insulating layer 146, and the electrode layers 150a, 150b, The electrode layer 150d and the electrode layer 150e are formed (see FIG. 14(C)). 48 is removed to form electrode layer 150a, electrode layer 150b, electrode layer 150d, and electrode layer 150 When forming the layer e, it is desirable to process it so that the surface is flat. The interlayer insulating layer 146, the electrode layer 150a, the electrode layer 150b, the electrode layer 150d, and the electrode layer 150e By flattening the surface, it is possible to form good electrodes, wiring, insulating layers, and semiconductor layers in the subsequent processes. It is possible to form the following:

[0201] Further, an insulating layer 152 is formed, and the electrode layers 150a, 150b, Openings are formed so as to reach the electrode layers 150d and 150e, and the electrode layers 150c are embedded in the openings. After the conductive layer is formed, a part of the conductive layer is removed by a method such as etching or CMP to form an insulating layer. The edge layer 152 is exposed to form the electrode layers 154a, 154b, and 154d. (See FIG. 14(D)). This process is the same as that for forming the electrode layer 150a, etc. , details will be omitted.

[0202] <Modifications of Transistor> 15 to 18 are diagrams showing modified examples of the transistor 164. In FIG.

[0203] In FIG. 15, a gate layer 136d is provided under an oxide semiconductor layer 140, and a source layer 142a is provided under the oxide semiconductor layer 140. and the drain layer 142b is in contact with the lower surface of the oxide semiconductor layer 140. 1 shows resistor 164.

[0204] A major difference between the configuration shown in FIG. 15 and the configuration shown in FIG. 11 is that the source layer 142a and the drain The position of the connection between the drain layer 142b and the oxide semiconductor layer 140 is one example. In the configuration shown in FIG. 1, the source layer 142a and the drain layer 142b are formed on the upper surface of the oxide semiconductor layer 140. 15, the oxide semiconductor layer 140 is in contact with the drain layer 142b. The lower surface of the semiconductor layer 142 contacts the source layer 142a and the drain layer 142b. Due to the difference in contact, the arrangement of other electrode layers, insulating layers, etc. is also different. The details of each component are the same as those in FIG.

[0205] Specifically, the transistor 164 shown in FIG. 15 has a gate insulating layer 128 formed on the interlayer insulating layer 128. a gate insulating layer 138 provided on the gate layer 136d; A source layer 142a and a drain layer 142b are provided on the layer 138, and the source layer 142 and an oxide semiconductor layer 140 in contact with the upper surfaces of the drain layer 142b. A protective insulating layer 144 is provided on the transistor 164 so as to cover the oxide semiconductor layer 140. is provided.

[0206] FIG. 16 shows a transistor 16 having a gate layer 136d on an oxide semiconductor layer 140. FIG. 16A shows a state in which the source layer 142a and the drain layer 142b are oxidized. FIG. 13 is a diagram showing an example of a configuration in which the lower surface of the organic semiconductor layer 140 is in contact with the oxide semiconductor layer 140. 16B, the source layer 142a and the drain layer 142b are formed on the oxide semiconductor layer 1. 4 is a diagram showing an example of a configuration in which the upper surface of the oxide semiconductor layer 140 is in contact with the oxide semiconductor layer 140.

[0207] A major difference between the configuration shown in FIG. 11 or FIG. 15 and the configuration shown in FIG. 16 is that the oxide semiconductor layer 1 16(A) and 16(B) are different in that the gate layer 136d is provided on the semiconductor device 40. The main difference in the configuration shown in FIG. 1B is that the source layer 142a and the drain layer 142b are oxidized. The point is whether the contact is at the lower surface or the upper surface of the compound semiconductor layer 140. Due to these differences, the arrangement of other electrode layers, insulating layers, etc. may differ. The details of each component are the same as those in FIG. 11 etc.

[0208] Specifically, the transistor 164 shown in FIG. 16A is provided over the interlayer insulating layer 128. The source layer 142a and the drain layer 142b are formed by the above-mentioned method. The oxide semiconductor layer 140 is in contact with the upper surface of the second insulating film 2b. The gate insulating layer 138 and the oxide semiconductor layer 140 on the gate insulating layer 138 and a gate layer 136d.

[0209] In addition, a transistor 164 shown in FIG. 16B includes an oxide film provided over the interlayer insulating layer 128. The oxide semiconductor layer 140 and a solenoid provided in contact with the upper surface of the oxide semiconductor layer 140. The oxide semiconductor layer 140, the source layer 142a, and the drain layer 142b are A gate insulating layer 138 is provided on the drain layer 142b. and a gate layer 136 d provided in a region overlapping with the oxide semiconductor layer 140 .

[0210] In addition, in the configuration shown in FIG. 16, compared with the configuration shown in FIG. 11, components are omitted. In this case, the electrode layer 150a, the electrode layer 154a, etc. may be formed. Of course, in the configuration shown in FIG. It goes without saying that non-essential components can be omitted.

[0211] FIG. 17 shows a case where the size of the element is relatively large, and a The transistor 164 has a gate layer 136d. Since the requirements for coverage are relatively low, wiring and electrodes can be placed in the insulating layer. It is not necessary to form the conductive layer so as to be embedded. For example, the conductive layer may be patterned after it is formed. Thus, the gate layer 136d and the like can be formed.

[0212] The major difference between the configuration shown in FIG. 17(A) and the configuration shown in FIG. 17(B) is that the source layer 142 a and the drain layer 142b are formed on either the lower surface or the upper surface of the oxide semiconductor layer 140. Due to these differences, the other electrode layers The layout of the insulating layers is different. For details of each component, see Figure 11. is the same as:

[0213] Specifically, the transistor 164 shown in FIG. 17A is provided over the interlayer insulating layer 128. a gate insulating layer 138 provided on the gate layer 136d; A source layer 142a and a drain layer 142b are provided on the insulating layer 138. and an oxide semiconductor layer 140 in contact with the upper surfaces of the drain layer 142a and the drain layer 142b. .

[0214] In addition, the transistor 164 shown in FIG. 17B has a gate insulating layer 128 over which the a gate insulating layer 138 provided on the gate layer 136d; an oxide semiconductor layer 140 provided in a region overlapping with the gate layer 136d over the layer 138; The source layer 142a and the drain layer 142b are provided in contact with the upper surface of the compound semiconductor layer 140. layer 142b.

[0215] In addition, the configuration shown in FIG. 17 also has fewer components than the configuration shown in FIG. In this case, too, the effect of simplifying the manufacturing process can be obtained.

[0216] FIG. 18 shows a case where the size of the element is relatively large, and a Transistor 164 is shown configured with gate layer 136d. Again, the surface planarity Since the requirements for performance and coverage are relatively low, wiring and electrodes can be placed on the insulating layer. It is not necessary to form the conductive layer so as to be embedded in the conductive layer. For example, the conductive layer may be patterned after it is formed. In this way, the gate layer 136d and the like can be formed.

[0217] The major difference between the configuration shown in FIG. 18(A) and the configuration shown in FIG. 18(B) is that the source layer 142 a and the drain layer 142b are formed on either the lower surface or the upper surface of the oxide semiconductor layer 140. Due to these differences, the other electrode layers The layout of the insulating layers is different. For details of each component, see Figure 11. is the same as:

[0218] Specifically, the transistor 164 shown in FIG. 18A is provided over the interlayer insulating layer 128. The source layer 142a and the drain layer 142b are formed by the above-mentioned method. The oxide semiconductor layer 140 in contact with the upper surface of the second insulating layer 2b, the source layer 142a, and the drain layer 142 b, and a gate insulating layer 138 provided on the oxide semiconductor layer 140, and a gate insulating layer 13 and a gate layer 136d provided in a region overlapping with the oxide semiconductor layer 140 on the gate electrode 136. .

[0219] In addition, the transistor 164 shown in FIG. 18B has an oxide film formed over the interlayer insulating layer 128. The oxide semiconductor layer 140 and a solenoid provided in contact with the upper surface of the oxide semiconductor layer 140. The source layer 142a, the drain layer 142b, and the A gate insulating layer 138 is provided on the oxide semiconductor layer 140. The gate layer 136d is formed by insulating the gate insulating layer 13. The insulating film 114 is provided in a region overlapping with the oxide semiconductor layer 140 via the insulating film 114 .

[0220] In addition, the configuration shown in FIG. 18 also has fewer components than the configuration shown in FIG. In this case, too, the effect of simplifying the manufacturing process can be obtained.

[0221] In addition, the oxide semiconductor layer 140, the source layer 142a, and the drain layer 142b shown in FIG. An oxide conductive layer functioning as a source region and a drain region is provided between the 19 and 20 show a transistor in which an oxide conductive layer is provided in the transistor 164 of FIG. FIG.

[0222] The transistor 164 in FIGS. 19 and 20 includes an oxide semiconductor layer 140, a source layer 142a, Between the drain layer 142b, an oxide conductive layer functioning as a source region and a drain region is provided. The difference between the transistor 164 in FIGS. The shape of the oxide conductive layers 162a and 162b differs depending on the manufacturing process.

[0223] In the transistor 164 in FIG. 19, a stack of an oxide semiconductor layer and an oxide conductive layer is formed. The stack of the oxide semiconductor layer and the oxide conductive layer is processed into a shape by the same photolithography process. The oxide semiconductor layer 140 and the oxide conductive layer are formed in an island shape. After forming a source layer 142a and a drain layer 142b on the conductive layer, The island-shaped oxide conductive layer is etched using the drain layer 142b as a mask to form a source region and Then, oxide conductive layers 162a and 162b which are to become the gate and drain regions are formed.

[0224] In the transistor 164 in FIG. 20, an oxide conductive layer is formed over the oxide semiconductor layer 140. A metal conductive layer is formed thereon, and the oxide conductive layer and the metal conductive layer are formed by the same photolithography. The oxide conductive layers 162a and 162b are processed to become the source and drain regions. 62b, a source layer 142a, and a drain layer 142b are formed.

[0225] Note that during etching treatment for processing the shape of the oxide conductive layer, the oxide semiconductor layer may be overcoated. In order to prevent excessive etching, the etching conditions (type, concentration, etc. of etching material) Adjust the time, etc., for testing as appropriate.

[0226] The oxide conductive layers 162a and 162b are formed by a sputtering method or a vacuum deposition method (electron The method is to use the arc discharge ion plating method, the spray method, etc. The material of the conductive layer is zinc oxide, zinc aluminum oxide, or zinc aluminum oxynitride. , zinc gallium oxide, indium tin oxide, etc. can be used. Silicon oxide may be contained.

[0227] The oxide conductive layer is formed as a source region and a drain region by forming an oxide semiconductor layer 140 and a source layer By providing the insulating layer 142a between the drain layer 142b, the low This allows the transistor 164 to operate at high speed.

[0228] In addition, by adopting such a configuration, the withstand voltage of the transistor 164 can be improved. This can be done.

[0229] 19 and 20, the oxide semiconductor layer 140 of the transistor 164 shown in FIG. Regarding a structure in which an oxide conductive layer is provided between the source layer 142a and the drain layer 142b, 15, 16, 17, and 18. However, the oxide semiconductor layer 1 of the transistor 164 shown in FIG. 40, and an oxide conductive layer is provided between the source layer 142a and the drain layer 142b. It is also possible to do so.

[0230] Note that in this example, the transistor 164 is stacked over the transistor 160. However, the configuration of the transistor 160 and the transistor 164 is not limited to this. For example, the transistor 160 and the transistor 164 are formed on the same plane. Furthermore, the transistor 160 and the transistor 164 can be overlapped. It's okay to do that.

[0231] <Modification of the Process for Forming Oxide Semiconductor Layer> A manufacturing process of an oxide semiconductor layer, which is different from the manufacturing process of the above-described transistor, is shown in FIG. I will use this to explain.

[0232] The oxide semiconductor layer includes a first crystalline oxide semiconductor layer and a second crystalline oxide semiconductor layer. The second crystalline oxide semiconductor layer is thicker than the first crystalline oxide semiconductor layer.

[0233] An insulating layer 437 is formed on the insulating layer 400. In this embodiment, the insulating layer 437 is made of PECV. Using the D method or sputtering method, oxide insulation with a thickness of 50 nm to 600 nm is For example, the oxide insulating layer may be a silicon oxide layer, a gallium oxide layer, or an oxide an aluminum nitride layer, a silicon oxynitride layer, an aluminum oxynitride layer, or a silicon nitride oxide layer; A layer selected from the silicon layers or a laminate of these layers can be used.

[0234] Next, a first oxide semiconductor layer is formed to a thickness of 1 nm to 10 nm over the insulating layer 437. The first oxide semiconductor layer is formed by a sputtering method. The substrate temperature during the film formation is set to 200° C. or higher and 400° C. or lower.

[0235] Here, a metal oxide target (In-Ga-Zn-O metal oxide target (I The substrate and target were prepared using a ZnO / GaO / ZnO ratio of 1:1:2 (molar ratio). The distance between the substrate and the board was 170 mm, the substrate temperature was 250°C, the pressure was 0.4 Pa, and the DC power supply was 0 .5kW, oxygen only, argon only, or argon and oxygen atmosphere, 5 nm thick, An oxide semiconductor layer is formed.

[0236] Next, the atmosphere in the chamber in which the substrate is placed is changed to nitrogen or dry air, and a first heating process is performed. The temperature of the first heat treatment is 400° C. or more and 750° C. or less. In this manner, a first crystalline oxide semiconductor layer 450a is formed (see FIG. 21A).

[0237] Although it depends on the substrate temperature during film formation and the temperature of the first heat treatment, Therefore, crystallization occurs from the film surface, and crystals grow from the surface to the inside of the film, forming a c-axis orientation. The first heat treatment causes zinc and oxygen to gather on the surface of the film, resulting in a flat crystal. A graphene-type two-dimensional crystal consisting of zinc and oxygen with hexagonal faces is formed on the outermost surface. The film is formed in multiple layers, which grow in the film thickness direction and overlap to form a laminate. When this occurs, crystal growth progresses from the surface to the inside, and then from the inside to the bottom.

[0238] By the first heat treatment, oxygen in the insulating layer 437, which is an oxide insulating layer, is converted into a first crystalline oxide. Diffusion at the interface with the nitride semiconductor layer 450a or in the vicinity thereof (within ±5 nm from the interface). As a result, oxygen vacancies in the first crystalline oxide semiconductor layer are reduced. The insulating layer 437 used is a layer having a thickness of 100 nm and a thickness of 100 nm. At least an amount of oxygen exceeding the stoichiometric ratio is present at any one of the interfaces of the insulating layer 437. It is preferable.

[0239] Next, a second oxide semiconductor layer having a thickness of more than 10 nm is formed on the first crystalline oxide semiconductor layer 450a. The conductive layer is formed. The second oxide semiconductor layer is formed by a sputtering method. The substrate temperature during film formation is set to 200° C. or higher and 400° C. or lower. By setting the temperature to 0° C. or higher and 400° C. or lower, The precursors are aligned in the oxide semiconductor layer to be formed, and so-called orderliness can be imparted to the oxide semiconductor layer. do.

[0240] Here, a metal oxide target (In-Ga-Zn-O metal oxide target (I The substrate and target were prepared using a ZnO / GaO / ZnO ratio of 1:1:2 (molar ratio). The distance between the substrate and the substrate was 170 mm, the substrate temperature was 400°C, the pressure was 0.4 Pa, and the DC power supply was 0 The first experiment was performed at 25 nm thickness under an atmosphere of oxygen only, argon only, or argon and oxygen. An oxide semiconductor layer 2 is formed.

[0241] Next, the atmosphere in the chamber in which the substrate is placed is changed to nitrogen or dry air, and a second heating process is performed. The temperature of the second heat treatment is 400° C. or more and 750° C. or less. Thus, a second crystalline oxide semiconductor layer 450b is formed (see FIG. 21B). Heat treatment should be carried out in a nitrogen atmosphere, an oxygen atmosphere, or a mixture of nitrogen and oxygen. This increases the density of the second crystalline oxide semiconductor layer and reduces the number of defects. According to this theory, the first crystalline oxide semiconductor layer 450a is the core and the first crystalline oxide semiconductor layer 450a is the nucleus. Crystal growth proceeds in the portion, forming a second crystalline oxide semiconductor layer 450b.

[0242] In addition, the steps from the formation of the insulating layer 437 to the second heat treatment are performed continuously without exposure to the air. The steps from the formation of the insulating layer 437 to the second heat treatment are preferably performed without using hydrogen or and in an atmosphere containing almost no moisture (inert atmosphere, reduced pressure atmosphere, dry air atmosphere, etc.). For example, the moisture content is preferably below a dew point of -40°C, more preferably below a dew point of -5 The atmosphere should be dry nitrogen at 0℃ or below.

[0243] Next, the first crystalline oxide semiconductor layer 450a and the second crystalline oxide semiconductor layer 450b The oxide semiconductor layer 4 is formed by processing the oxide semiconductor layer 4. In FIG. 21C, the first crystalline oxide semiconductor layer 450a and the second crystalline oxide semiconductor layer 53 are formed. The interface of the second crystalline oxide semiconductor layer 450b is indicated by a dotted line, and the oxide semiconductor stack is described as a stack of oxide semiconductor layers. However, there is no clear interface, and the diagram is only for the purpose of easy understanding. It shows.

[0244] The oxide semiconductor stack is processed as follows: a mask having a desired shape is formed on the oxide semiconductor stack; The above-described mask can be used for etching the oxide semiconductor stack. The insulating layer 11 can be formed by a method such as photolithography. The mask may be formed using a method such as a photolithography method.

[0245] Note that the etching of the oxide semiconductor stack can be performed by either dry etching or wet etching. Of course, these may be used in combination.

[0246] The first crystalline oxide semiconductor layer and the second crystalline oxide semiconductor layer obtained by the above manufacturing method are One of the features of the nitride semiconductor layer is that it has a c-axis orientation. The crystalline oxide semiconductor layer and the second crystalline oxide semiconductor layer do not have a single crystal structure but have an amorphous structure. The structure is not a c-axis aligned crystal. The first crystalline oxide semiconductor has an oxide containing stal (also called CAAC). The oxide semiconductor layer and the second crystalline oxide semiconductor layer partially have crystal grain boundaries.

[0247] The first and second crystalline oxide semiconductor layers are made of an oxide material containing at least Zn. There are four-element metal oxide materials, In-Al-Ga-Zn-O and In-Sn-G a-Zn-O based materials, In-Ga-Zn-O based materials, which are ternary metal oxides, In -Al-Zn-O based materials, In-Sn-Zn-O based materials, Sn-Ga-Zn-O based materials Materials, Al-Ga-Zn-O materials, Sn-Al-Zn-O materials, and binary metal oxides In-Zn-O based materials, Sn-Zn-O based materials, and Al-Zn-O based materials are oxides. , Zn-Mg-O-based materials, Zn-O-based materials, etc. In-Si-Ga- Zn-O based materials, In-Ga-B-Zn-O based materials, In-B-Zn-O based materials Alternatively, the above materials may contain SiO2. The n-Ga-Zn-O system material is made up of indium (In), gallium (Ga), and zinc (Zn The composition ratio is not particularly important. It may contain elements other than Zn.

[0248] Also, a two-layer structure in which a second crystalline oxide semiconductor layer is formed on a first crystalline oxide semiconductor layer is formed. The present invention is not limited to the above structure, and may be modified so as to form a third crystalline oxide semiconductor layer after forming a second crystalline oxide semiconductor layer. The process of film formation and heat treatment is repeated to form a laminated structure of three or more layers. Good too.

[0249] The first crystalline oxide semiconductor layer such as the oxide semiconductor layer 453 and the second crystalline oxide semiconductor layer By using stacked layers in transistors, it is possible to achieve stable electrical characteristics and high reliability. High-performance transistors can be realized.

[0250] <cpu> A specific example of a CPU having the above-mentioned semiconductor integrated circuit will be described with reference to FIG. .

[0251] FIG. 22 is a block diagram showing a specific configuration of a CPU. The CPU shown in FIG. Arithmetic logic unit (ALU) 90 on board 900 1, ALU Controller902, Instruction Decoder9 03, Interrupt Controller904, Timing Control ller905, Register906, Register Controller9 07, bus interface (Bus I / F) 908, rewritable ROM 909, The ROM 909 and the ROM interface (ROM I / F) 920 are mainly included. The ROM I / F 920 may be provided on a separate chip. This is just a simplified example of the configuration of the CPU. Actual CPUs have a wide variety of configurations depending on their applications. It has a composition.

[0252] The instructions input to the CPU via the Bus I / F 908 are The signal is input to the Decoder 903, decoded, and then passed to the ALU Controller 9 02, Interrupt Controller904, Register Cont. The signal is input to roller907 and Timing Controller905.

[0253] ALU Controller902, Interrupt Controller9 04, Register Controller907, Timing Control The ler905 performs various controls based on the decoded instructions. The controller 902 generates signals to control the operation of the ALU 901. The interrupt controller 904 is also Interrupt requests from external I / O devices and peripheral circuits are judged based on their priority and mask status. The Register Controller 907 determines whether the Generates the address of 906 and reads or writes the register 906 depending on the CPU state. Do the writing.

[0254] In addition, the Timing Controller 905 is a troller902, Instruction Decoder903, Interr upt Controller904, Register Controller907 It generates signals that control the timing of the operation of er905 generates an internal clock signal CLK2 based on a reference clock signal CLK1. It has an internal clock generating section, which supplies a clock signal CLK2 to the various circuits mentioned above.

[0255] In the CPU shown in FIG. 22, the memory circuit 11 shown in FIG. The Register Controller 907 also includes the registers shown in FIG. In the CPU shown in FIG. The star controller 907 follows the instructions from the ALU 901 and In other words, the register 906 has In the memory circuit 11, sequential circuits 21_1 to 21_n are used to hold data or to store data. A node electrically connected to one electrode of the capacitance element 32 is selected to hold data. When the sequential circuits 21_1 to 21_n are selected to hold data, the Reg A power supply voltage is supplied to the memory circuit 11 in the transistor 906. If data retention is selected for the node electrically connected to one electrode, Re The supply of power supply voltage to the memory circuit 11 in the memory 906 can be stopped.

[0256] In this way, when the CPU operation is temporarily stopped and the supply of power voltage is stopped, It is possible to retain data even if the power is turned off, and power consumption can be reduced. For example, a user of a personal computer inputs information into an input device such as a keyboard. The CPU can be stopped even while input is stopped, thereby reducing power consumption. It is possible.

[0257] Although the CPU has been described as an example here, the semiconductor integrated circuit of the present invention is not limited to a CPU. DSP, custom LSI, FPGA (Field Programmable Gate Array) It can also be applied to LSIs such as LSIs (Low-Speed ​​Arrays). EXAMPLES

[0258] The field effect mobility of insulated gate transistors that are actually measured, not limited to oxide semiconductors, The mobility of the electrons is lower than the original mobility due to various reasons. There are defects inside the semiconductor and defects at the interface between the semiconductor and the insulating film. Using this method, it is possible to theoretically derive the field effect mobility assuming that there are no defects inside the semiconductor. I can.

[0259] The inherent mobility of the semiconductor is μ0, and the measured field-effect mobility is μ. Assuming the existence of potential barriers (grain boundaries, etc.),

[0260]

number

[0261] Here, E is the height of the potential barrier, k is the Boltzmann constant, and T is the absolute temperature. Also, if we assume that the potential barrier originates from defects, Levin In the son model,

[0262]

number

[0263] Here, e is the elementary charge, and N is the average defect density per unit area in the channel. , ε is the dielectric constant of the semiconductor, n is the number of carriers contained in the channel per unit area, C ox teeth Capacitance per unit area, V g is the gate voltage, and t is the channel thickness. For semiconductor layers of less than 100 nm, the channel thickness can be considered to be the same as the semiconductor layer thickness. The drain current in the linear region I d teeth,

[0264]

number

[0265] Here, L is the channel length and W is the channel width, where L=W=10μ. m. Also, V d is the drain voltage. g Divide by and then take the logarithm of both sides If you take

[0266]

number

[0267] The right hand side of number 8 is V g As can be seen from this equation, the vertical axis is a function of ln(I d / V g ), the horizontal axis is 1 / V g From the slope of the line on the graph obtained by plotting the measured values ​​as The defect density N is calculated. That is, the I d -V g From the characteristics, the defect density is evaluated. The oxide semiconductors are indium (In), tin (Sn), and zinc (Zn). When the ratio is In:Sn:Zn=1:1:1, the defect density N is 1×10 12 / cm 2 Process degrees.

[0268] Based on the defect density thus obtained, equations 5 and 6 are used to calculate μ0 = 120 cm 2 / V The mobility measured in the defective In-Sn-Zn oxide is 40 cm 2 / However, the oxide film without defects in the semiconductor and at the interface between the semiconductor and the insulating film The semiconductor mobility μ0 is 120 cm 2 It can be expected that / Vs.

[0269] However, even if there are no defects inside the semiconductor, the electrons may be scattered at the interface between the channel and the gate insulating layer. The transport properties of the transistor are affected by the distance x from the gate-insulator interface. The mobility μ1 at the location is

[0270]

number

[0271] Here, D is the electric field in the gate direction, and B and l are constants. From the above measurement results, B = 4.75 × 10 7 cm / s, l = 10 nm (depth of interface scattering). D increases (i.e., gate voltage It can be seen that as the pressure increases, the second term of equation 9 increases, and therefore the mobility μ1 decreases.

[0272] Development of a transistor with an ideal oxide semiconductor channel that is free of internal defects The results of calculating the degree μ2 are shown in Figure 26. The calculation was performed using a Synopsys device simulator. Sentaurus Device is a software that can be used to measure the bandgap of oxide semiconductors. The gap, electron affinity, dielectric constant, and thickness are 2.8 eV and 4.7 eV, respectively. These values ​​were measured for thin films formed by sputtering. This was obtained by

[0273] In addition, the work functions of the gate layer, source, and drain are set to 5.5 eV and 4. The gate insulating layer was 100 nm thick and the specific dielectric constant was 1.6 eV and 4.6 eV. The dielectric constant was set to 4.1. The channel length and width were both 10 μm, and the drain voltage V d is 0.1V.

[0274] As shown in Figure 26, the mobility is 100 cm at a gate voltage of just over 1 V. 2 Peaks above / Vs However, if the gate voltage is increased further, the interface scattering increases and the mobility decreases. In order to reduce interface scattering, the surface of the semiconductor layer must be flattened at the atomic level (A 100% saturation layer flatness is preferred.

[0275] When a miniaturized transistor is manufactured using an oxide semiconductor having such mobility, The results of calculating the characteristics are shown in Figures 27 to 29. The structure is shown in FIG. 30. The transistor shown in FIG. + Conductivity type The semiconductor region 503a and the semiconductor region 503c are The resistivity of the conductor region 503c is 2×10 -3 Let it be Ωcm.

[0276] The transistor shown in FIG. 30A includes a base insulating layer 501 and a semiconductor layer embedded in the base insulating layer 501. A buried insulator 502 made of aluminum oxide is formed so as to be embedded in the insulating layer 502. The transistor is made up of a semiconductor region 503a and a semiconductor region 503c. The gate layer 505 is an intrinsic semiconductor region 503b that serves as a panel forming region. The width of 05 is 33 nm.

[0277] Between the gate layer 505 and the semiconductor region 503b, there is a gate insulating layer 504. The gate layer 505 is provided on both sides with sidewall insulators 506a and 506b. On the top of the gate layer 505, there is an insulator 507 to prevent short circuits between the gate layer 505 and other wiring. The width of the sidewall insulator is set to 5 nm. In contact with the transistor c, a source layer 508a and a drain layer 508b are provided. The channel width in the sta is set to 40 nm.

[0278] The transistor shown in FIG. 30B is made of a base insulating layer 501 and aluminum oxide. A semiconductor region 503a, a semiconductor region 503c, and the like are formed on the buried insulator 502. Sandwiched between these are an intrinsic semiconductor region 503b, a gate layer 505 having a width of 33 nm, and a gate insulating layer 506. The layer 504, the sidewall insulator 506a, the sidewall insulator 506b, the insulator 507, and the source layer 50 30(A) in that it has a drain layer 508a and a drain layer 508b. do.

[0279] The difference between the transistor shown in FIG. 30(A) and the transistor shown in FIG. 30(B) is that The conductivity type of the semiconductor region under the insulator 506a and the sidewall insulator 506b. In the transistor shown in FIG. 1, the semiconductor under the sidewall insulator 506a and the sidewall insulator 506b The area is n + The semiconductor regions 503a and 503c have the same conductivity type. In the transistor shown in FIG. 30(B), the intrinsic semiconductor region is 503b. In the semiconductor layer shown in FIG. 1B, the semiconductor region 503a (semiconductor region 503c) and the gate There is an area where the layers 505 do not overlap by Loff. This area is called the offset area. The width Loff is called the offset length. As is clear from the figure, the offset length is It is the same as the width of the insulator 506a (sidewall insulator 506b).

[0280] The other parameters used in the calculation are as described above. We used the chair simulation software Sentaurus Device. , the drain current (I d , solid line) and movement (μ, dotted line) of gate voltage (V g , the gate-source potential difference) dependence. current I d The drain voltage (potential difference between the drain and source) is +1V, and the mobility μ is The input voltage was calculated at +0.1V.

[0281] FIG. 27(A) shows a gate insulating layer with a thickness of 15 nm, and FIG. 27(B) shows a gate insulating layer with a thickness of 10 nm, and FIG. 27(C) is 5 nm. Especially, the drain current I d On the other hand, the off-state current (OFF current) is significantly decreased. The peak value of the on-state drain current I d There is no noticeable change in (on-state current). It was shown that the drain current exceeded 10 μA at a gate voltage of around 1 V.

[0282] FIG. 28 shows a transistor having the structure shown in FIG. 30(B) with an offset length Loff of 5 nm, the drain current I d (solid line) and mobility μ (dotted line) vs. gate voltage V g Depends The drain current I d The drain voltage is +1V, and the mobility μ is the drain voltage The calculation was performed with the gate insulating layer thickness set to 15 nm. FIG. 28(B) is for 10 nm, and FIG. 28(C) is for 5 nm. This is what was done.

[0283] FIG. 29 shows the offset length Lof The drain current I d (solid line) and mobility μ (dotted line) The drain current I d The drain voltage is +1V, and the mobility μ is the drain The voltage was calculated at +0.1 V. Figure 29(A) shows the gate insulating layer thickness of 15 nm, FIG. 29(B) is for 10 nm, and FIG. 29(C) is for 5n The value is m.

[0284] In both cases, the thinner the gate insulating layer, the more significantly the off-state current decreases, while the peak of the mobility μ decreases. There is no noticeable change in the peak value or on-state current.

[0285] In addition, the peak of the mobility μ is 80 cm in FIG. 2 / Vs, but in Figure 28, 0cm 2 / Vs, 40 cm in Figure 29 2 / Vs, the offset length Loff increases The off-current also shows a similar trend. On the other hand, the on-current also decreases with increasing offset length. It decreases with increasing Loff, but the decrease is much slower than the decrease in the off-state current. In addition, it was shown that the drain current exceeds 10 μA at a gate voltage of about 1 V in both cases. It was.

[0286] A transistor with a channel formation region made of an oxide semiconductor mainly composed of In, Sn, and Zn The oxide semiconductor film is formed by heating the substrate or by By forming the layer and then performing heat treatment, good characteristics can be obtained. An element that is contained in a mixture at a concentration of 5 atomic % or more.

[0287] After the formation of an oxide semiconductor film mainly composed of In, Sn, and Zn, the substrate is intentionally heated. This makes it possible to improve the field effect mobility of the transistor. This makes it possible to positively shift the threshold voltage of the transistor and make it normally off.

[0288] For example, FIG. 31(A) to FIG. 31(C) show a semiconductor device having In, Sn, and Zn as main components and a channel The length L is 3 μm, the channel width W is 10 μm, and the gate electrode is 100 nm thick. These are the characteristics of a transistor using a thin insulating layer. d was set to 10V.

[0289] Figure 31(A) shows a sputtering method in which the substrate was not intentionally heated and In, Sn, and Zn were the main components. The field-effect transition (field-effect transition) of the transistor is shown in FIG. Mobility is 18.8cm 2 On the other hand, by intentionally heating the substrate, In, By forming an oxide semiconductor film mainly composed of Sn and Zn, the field effect mobility can be improved. FIG. 31(B) shows the structure of the substrate heated to 200°C and the structure of the substrate mainly composed of In, Sn, and Zn. The transistor characteristics when an oxide semiconductor film is formed are shown in Fig. 1. The field effect mobility is 32. 2cm 2 / Vsec is obtained.

[0290] The field effect mobility was measured by forming an oxide semiconductor film mainly composed of In, Sn, and Zn and then thermally The effect can be further improved by further treatment. The oxide semiconductor film mainly composed of n was formed by sputtering at 200°C, and then heated at 650°C. The transistor characteristics after the treatment are shown below. The field effect mobility is 34.5 cm 2 / Vsec is obtained.

[0291] By intentionally heating the substrate, moisture is absorbed into the oxide semiconductor film during sputtering. In addition, by performing heat treatment after film formation, Hydrogen, a hydroxyl group, or moisture can be released and removed from the oxide semiconductor film. Such an improvement in field effect mobility can be achieved by Not only do they remove impurities through hydration and dehydrogenation, but they also shorten the interatomic distances through densification. It is also estimated that the crystallization of oxide semiconductors can be achieved by removing impurities from the oxide semiconductors and purifying them. Such a highly purified non-single-crystal oxide semiconductor can be ideally 00cm 2 It is estimated that it will be possible to achieve a field effect mobility of more than 1000 times the current / Vsec. .

[0292] Oxygen ions are implanted into an oxide semiconductor whose main components are In, Sn, and Zn, and then the oxide semiconductor is heated to Hydrogen, hydroxyl groups, or moisture contained in the oxide semiconductor is released, and the heat treatment is performed simultaneously or simultaneously. The oxide semiconductor may be crystallized by subsequent heat treatment. By the crystallization treatment, a non-single-crystal oxide semiconductor with good crystallinity can be obtained.

[0293] The effect of intentionally heating the substrate during film formation and / or heat treatment after film formation is This not only improves the field effect mobility but also contributes to making the transistor normally off. The oxides, mainly composed of In, Sn, and Zn, were formed without intentionally heating the substrate. The threshold voltage of a transistor that uses a semiconductor film as a channel formation region is shifted negatively. However, the oxide semiconductor film formed by intentionally heating the substrate is In this case, the negative shift of the threshold voltage is eliminated. This tendency is shown in Figure 31(A) and Figure 31(B). This can also be confirmed by comparing with B).

[0294] The threshold voltage can also be controlled by changing the ratio of In, Sn, and Zn. By setting the composition ratio to In:Sn:Zn=2:1:3, Normally-off can be expected. In addition, the composition ratio of the target is In:Sn:Z When n=2:1:3, an oxide semiconductor film with high crystallinity can be obtained.

[0295] The intentional substrate heating temperature or heat treatment temperature is 150° C. or higher, preferably 200° C. or higher. The temperature is preferably 400° C. or higher. This makes it possible to make the resistor normally off.

[0296] In addition, the gate barrier can be reduced by intentionally heating the substrate during film formation and / or by carrying out heat treatment after film formation. It can improve the stability against bias stress. For example, 2MV / cm, 150 ℃, 1 hour application conditions, the drift is less than ±1.5V, preferably 1.0 Less than V can be obtained.

[0297] In fact, Sample 1 was not subjected to heat treatment after the oxide semiconductor film was formed, and Sample 2 was subjected to heat treatment at 650° C. The transistor of sample 2 that had been subjected to the treatment was subjected to a BT test.

[0298] First, the substrate temperature is set to 25°C, and V ds is set to 10V, and the V of the transistor g -I d Measurement of characteristics The V ds indicates the drain voltage (potential difference between the drain and source). Next, The substrate temperature was set to 150°C, and V ds Next, the voltage applied to the gate insulating layer was set to 0.1 V. V so that the field strength is 2MV / cm g A voltage of 20 V was applied to the sample and the sample was held there for 1 hour. To, V g Next, the substrate temperature was set to 25°C, and V ds is set to 10V, and the transistor V g -I d This measurement was called the Plus BT test.

[0299] Similarly, first set the substrate temperature to 25°C and V ds is set to 10V, and the V of the transistor g -I d Next, the substrate temperature was set to 150°C, and V ds was set to 0.1 V. Next, V is set so that the electric field strength applied to the gate insulating layer is -2MV / cm. g Apply -20V to Then, the V g Next, the substrate temperature was set to 25°C, and V ds is set to 10V, and the V of the transistor g -I d This is called the negative BT test. Call.

[0300] The results of the positive BT test for sample 1 are shown in Figure 32(A), and the results of the negative BT test are shown in Figure 32(B). The results of the positive BT test for sample 2 are shown in FIG. 33(A), and the results of the negative BT test for sample 2 are shown in FIG. The results are shown in Figure 33(B).

[0301] The threshold voltage shifts of sample 1 due to the positive BT test and the negative BT test are The positive and negative BT tests of sample 2 were 1.80V and -0.42V. The threshold voltage shift due to the BT test was 0.79 V and 0.76 V, respectively. In both Sample 1 and Sample 2, the change in threshold voltage before and after the BT test was small. It is clear that it is highly reliable.

[0302] Heat treatment can be carried out in an oxygen atmosphere, but it should first be replaced with nitrogen or an inert gas, or with a reducing gas. Alternatively, heat treatment may be performed under pressure and then in an oxygen-containing atmosphere. By adding oxygen to the oxide semiconductor after dehydrogenation, the effect of the heat treatment can be further improved. To add oxygen later, oxygen ions can be accelerated by an electric field to form a A method of injecting the film may also be applied.

[0303] Defects due to oxygen vacancies occur in the oxide semiconductor and at the interface between the oxide semiconductor and a film in contact with the oxide semiconductor. However, when excess oxygen is contained in the oxide semiconductor by such heat treatment, In this way, the oxygen deficiency that is constantly generated can be compensated for by excess oxygen. The oxygen atoms are mainly present between the lattices, and the oxygen concentration is 1×10 16 / cm 3 2×1 or more 0 20 / cm 3 If the above conditions are met, the oxide semiconductor can be made to contain the fluorine atom without causing distortion or the like to the crystal. It is possible.

[0304] In addition, the oxide semiconductor is at least partially crystallized by the heat treatment. For example, a more stable oxide semiconductor film can be obtained with a composition ratio of In:Sn:Zn= The acid film was sputtered using a 1:1:1 target without intentionally heating the substrate. The compound semiconductor film was found to be halo- The oxide semiconductor film thus formed is crystallized by heat treatment. The heat treatment temperature can be selected as desired. For example, heat treatment at 650°C can be performed to obtain the X Clear diffraction peaks can be observed by X-ray diffraction.

[0305] In fact, we performed XRD analysis of the In-Sn-Zn-O film. r Using the AXS X-ray diffraction device D8 ADVANCE, the out-of-plane method was measured.

[0306] Samples A and B were prepared for XRD analysis. A method for producing sample B will be described.

[0307] A 100 nm thick In-Sn-Zn-O film was formed on a dehydrogenated quartz substrate. Ta.

[0308] The In-Sn-Zn-O film was formed using a sputtering device in an oxygen atmosphere at a power of 100 W. The target was In:Sn:Zn=1:1:1 [atomic ratio]. An In-Sn-Zn-O target was used. The substrate heating temperature during film formation was 200°C. The sample thus prepared was designated as sample A.

[0309] Next, a sample prepared in the same manner as sample A was subjected to a heat treatment at a temperature of 650°C. The heat treatment is first performed in a nitrogen atmosphere for one hour, and then in an oxygen atmosphere without lowering the temperature. The sample was then heated for another hour at 40° C. The sample thus prepared was designated as sample B.

[0310] Figure 34 shows the XRD spectra of sample A and sample B. In sample A, the peaks derived from crystals No cracks were observed in sample B, but the 2θ values ​​were around 35 deg and 37 deg to 38 deg. In eg, a peak derived from crystals was observed.

[0311] In this way, oxide semiconductors that are mainly composed of In, Sn, and Zn are formed on a substrate intentionally. Improve the transistor characteristics by heating and / or heat treatment after film formation It is possible.

[0312] This substrate heating and heat treatment removes hydrogen and hydroxyl groups, which are harmful impurities in oxide semiconductors, from the film. In other words, it has the effect of preventing oxides from being included in the film or removing them from the film. By removing hydrogen, which acts as a donor impurity in semiconductors, high purification can be achieved. This allows the transistor to be normally off, and the oxide semiconductor is highly purified. By this, the off-current can be reduced to 1 aA / μm or less. The unit indicates the current value per 1 μm of channel width.

[0313] Figure 35 shows the relationship between the off-state current of a transistor and the inverse of the substrate temperature (absolute temperature) at the time of measurement. For simplicity, the reciprocal of the substrate temperature during measurement is multiplied by 1000 (1000 Specifically, as shown in FIG. 35, when the substrate temperature is 125° C., has a resistance of 1aA / μm (1×10 -18 A / μm) or less, 100zA / μm at 85℃ (1×10 -19 A / μm), and at room temperature (27°C), 1zA / μm (1×10 - 21 Preferably, the resistance can be 0.1 aA / μm at 125° C. m(1×10 -19 A / μm) or less at 85°C, 10zA / μm (1×10 -20 A / μm) or less at room temperature, -22 A / μm) or less It is possible.

[0314] However, in order to prevent hydrogen or moisture from being mixed into the oxide semiconductor film during the formation of the film, The sputtering gas is highly purified by sufficiently suppressing leaks from the inside of the chamber and degassing from the inner walls of the deposition chamber. For example, the sputtering gas is preferably kept at a dew point of -70°C so that moisture is not included in the film. It is preferable to use a gas that is equal to or less than 1000 nm. In addition, the target itself does not contain hydrogen, moisture, etc. It is preferable to use a highly purified target so that it does not contain impurities. Oxide semiconductors that are mainly composed of In, Sn, and Zn can be made to remove moisture from the film by heat treatment. However, the moisture release temperature is higher than that of oxide semiconductors mainly composed of In, Ga, and Zn. Therefore, it is preferable to form a film that does not contain moisture from the beginning.

[0315] In addition, a transistor using sample B which was subjected to heat treatment at 650° C. after the oxide semiconductor film was formed The relationship between the substrate temperature and the electrical characteristics was evaluated for the device.

[0316] The transistor used for the measurement has a channel length L of 3 μm, a channel width W of 10 μm, and Lo v is 0 μm and dW is 0 μm. ds The voltage was set to 10 V. The substrate temperature was -4 The experiments were carried out at 0°C, -25°C, 25°C, 75°C, 125°C and 150°C. In the gate electrode, the width of overlap between the gate layer and a pair of electrodes is called Lov, and the width of overlap between the gate layer and a pair of electrodes is called Lov. The protrusion of the pair of electrodes is called dW.

[0317] In Figure 36, I d (solid line) and field-effect mobility (dotted line) g The dependency is shown in Fig. Figure 37(A) shows the relationship between the substrate temperature and the threshold voltage, and Figure 37(B) shows the relationship between the substrate temperature and the field effect transfer This shows the relationship of degrees.

[0318] From FIG. 37(A), it can be seen that the higher the substrate temperature, the lower the threshold voltage. The range was 1.09V to -0.23V at -40℃ to 150℃.

[0319] Also, from FIG. 37(B), it can be seen that the higher the substrate temperature, the lower the field effect mobility. The temperature range is -40℃ to 150℃ and is 36cm 2 / Vs~32cm 2 / Vs. Therefore, it is understood that the variation in electrical characteristics is small within the above-mentioned temperature range.

[0320] The above-mentioned oxide semiconductor containing In, Sn, and Zn as main components is used for the channel formation region. According to the transistor, the field effect mobility is increased to 30 while keeping the off-current below 1aA / μm. cm 2 / Vsec or more, preferably 40cm 2 / Vsec or more, preferably 60cm 2 / Vsec or more, and the on-current value required by the LSI can be satisfied. For example, FET with L / W=33nm / 40nm, gate voltage 2.7V, drain voltage 1.0V When the transistor is turned on, an on-current of 12 μA or more can flow. Even in the temperature range, sufficient electrical characteristics can be ensured. In this case, a transistor made of oxide semiconductor can be mixed into an integrated circuit made of silicon semiconductor. It is possible to realize an integrated circuit with new functions without sacrificing the operating speed even if the chip is mounted on a can. EXAMPLES

[0321] In this example, an example of a transistor using an In-Sn-Zn-O film as an oxide semiconductor film will be described. This will be described with reference to FIG.

[0322] Figure 38 shows a coplanar type top-gate top-contact transistor. FIG. 38A shows a top view of a transistor. FIG. FIG. 38B shows a cross section AB corresponding to the dashed line AB in FIG.

[0323] The transistor shown in FIG. 38B includes a substrate 600 and a base insulating film provided on the substrate 600. The insulating film 602, the protective insulating film 604 provided around the insulating base film 602, and the insulating base film 603 are 02 and a high resistance region 606a and a low resistance region 606 provided on the protective insulating film 604. an oxide semiconductor film 606 having b and a gate insulating layer provided over the oxide semiconductor film 606; 608, a gate insulating layer 608 provided to overlap with the oxide semiconductor film 606, and a sidewall insulating film 612 provided in contact with a side surface of the gate layer 610; A pair of electrodes 614 provided in contact with the low resistance region 606b and at least an oxide semiconductor An interlayer insulating film 616 is provided to cover the film 606, the gate layer 610, and the pair of electrodes 614. and at least one of a pair of electrodes 614 through an opening provided in the interlayer insulating film 616. and a wiring 618 provided in connection therewith.

[0324] Although not shown, a protective film is provided to cover the interlayer insulating film 616 and the wiring 618. By providing the protective film, the surface conduction of the interlayer insulating film 616 can be prevented. The minute leakage current caused by the semiconductor device can be reduced, and the off-current of the transistor can be reduced. can be done. EXAMPLES

[0325] In this embodiment, a transistor using an In-Sn-Zn-O film as an oxide semiconductor film, which is different from the above, was used. Another example of the transistor will be described.

[0326] FIG. 39 is a top view and a cross-sectional view showing the structure of a transistor fabricated in this example. FIG. 39(A) is a top view of a transistor. FIG. 39(B) is a cross-sectional view of a portion of FIG. FIG. 2 is a cross-sectional view corresponding to the dashed line AB.

[0327] The transistor shown in FIG. 39B includes a substrate 700 and a base insulating film provided over the substrate 700. An insulating film 702, an oxide semiconductor film 706 provided on the base insulating film 702, and an oxide semiconductor A pair of electrodes 714 in contact with the oxide semiconductor film 706 and a pair of electrodes 714 a gate insulating layer 708 provided on the oxide semiconductor film 706 A gate layer 710 is provided so as to overlap the gate insulating layer 708 and the gate layer 710. The insulating interlayer 716 is provided with an opening between the insulating interlayer 716 and the insulating film 716. A wiring 718 connected to the electrode 714 and a layer insulating film 716 and a wiring 718 are provided to cover the layer insulating film 716 and the wiring 718. and a protective film 720 formed thereon.

[0328] The substrate 700 is a glass substrate, the insulating base film 702 is a silicon oxide film, and The semiconductor film 706 is an In-Sn-Zn-O film, and the pair of electrodes 714 is a tongue. The gate insulating layer 708 is a silicon oxide film, and the gate layer 710 is a nitride film. The interlayer insulating film 716 is a silicon oxynitride film. The laminated structure is made of a composite film and a polyimide film. The wiring 718 is made of a titanium film, an aluminum film, The laminated structure in which the titanium film is formed in this order is a polyimide film as a protective film 720, Each was used.

[0329] In the transistor having the structure shown in FIG. The width of the overlap with the oxide semiconductor film 706 is referred to as Lov. The protrusion of pole 714 is called dW. [Explanation of symbols]

[0330] 10 Arithmetic circuit 11 Memory circuit 12 Power gate control circuit 20 Power Gate Transistor 21_1~21_n Sequential circuit 21_x sequential circuit 22_1~22_n Combinational circuits 30. Flip-Flop 31 Transistor 32 Capacitive element 50 Substrates 51 Base layer 52 Gate Layer 53 Gate insulating layer 54 Oxide semiconductor layer 55a Source Layer 55b Drain layer 56 Protective insulation layer 57 Planarizing Insulating Layer 58a conductive layer 58b Conductive layer 100 Substrates 102 Protective layer 104 Semiconductor area 106 Element isolation insulating layer 108 Gate Insulation Layer 110 Gate Layer 112 Insulating layer 114a Impurity region 114b Impurity region 116 Channel formation region 118 Sidewall insulating layer 120a High concentration impurity region 120b High concentration impurity region 122 Metal layer 124a Metal compound area 124b Metal compound area 126 Interlayer Insulation Layer 128 Interlayer Insulation Layer 130a Source Layer 130b Drain layer 132 Insulating Layer 134 Conductive Layer 136a Electrode layer 136b Electrode layer 136d Gate layer 138 Gate Insulation Layer 140 Oxide semiconductor layer 142a Source Layer 142b Drain layer 144 Protective Insulation Layer 146 Interlayer Insulation Layer 148 Conductive Layer 150a electrode layer 150b electrode layer 150d electrode layer 150e electrode layer 152 Insulating layer 154a Electrode layer 154b Electrode layer 154d electrode layer 160 Transistors 162a Oxide conductive layer 162b Oxide conductive layer 164 Transistors 210a NAND gate 210b NAND gate 210c NAND gate 210d NAND gate 210e NAND gate 210f NAND gate 211a AND Gate 211b AND gate 212a Switch 212b Switch 212c Switch 212d Switch 400 Insulation Layer 437 Insulating Layer 450a Crystalline oxide semiconductor layer 450b Crystalline oxide semiconductor layer 453 Oxide Semiconductor Layer 501 Undercoat insulation layer 502 Embedded insulation 503a Semiconductor area 503b Semiconductor area 503c Semiconductors 504 Gate insulation layer 505 Gate Layer 506a Sidewall Insulation 506b Sidewall insulation 507 Insulation 508a Source Layer 508b Drain layer 600 Substrates 602 Undercoat insulating film 604 Protective insulating film 606 Oxide Semiconductor Film 606a High resistance area 606b Low resistance region 608 Gate Insulation Layer 610 Gate Layer 612 Sidewall insulating film 614 Electrode 616 Interlayer insulating film 618 Interlayer insulating film 700 Substrates 702 Undercoat insulating film 706 Oxide Semiconductor Film 708 Gate Insulation Layer 710 Gate Layer 714 Electrode 716 Interlayer insulating film 718 Wiring 720 Protective film 801 Measurement System 811 Transistor 812 Transistor 813 Capacitive element 814 Transistor 815 Transistor 900 Substrate 901 ALU 902 ALU Controller 903 Instruction Decoder 904 Interrupt Controller 905 Timing Controller 906 Register 907 Register Controller 908 Bus I / F 909 ROM 920 ROM interface< / cpu>

Claims

1. a first transistor including a channel formation region made of silicon and a second transistor including a channel formation region made of an oxide semiconductor; A semiconductor device in which one of a source or a drain of the first transistor is always electrically connected to one of a source or a drain of the second transistor, a first conductive film having a region located above a channel formation region of the first transistor and functioning as a gate electrode of the first transistor; a first insulating film having a region disposed above the first conductive film; a second conductive film having a region disposed above the first insulating film and functioning as a gate electrode of the second transistor; a third conductive film having a region disposed above the first insulating film; a second insulating film having a region disposed above the second conductive film and a region disposed above the third conductive film; a semiconductor film having a region disposed above the second insulating film and having a channel formation region of the second transistor; a third insulating film having a region disposed above the semiconductor film; a fourth conductive film having a region disposed above the third insulating film; a fifth conductive film having a region disposed above the third insulating film and always electrically connected to the third conductive film; having the fourth conductive film is always electrically connected to one of a source or a drain of the first transistor, and is always electrically connected to one of a source or a drain of the second transistor; when the third conductive film is electrically connected to the fourth conductive film at least through a channel formation region of the first transistor, the fifth conductive film is electrically connected to the fourth conductive film; Semiconductor device.

2. a first transistor including a channel formation region made of silicon and a second transistor including a channel formation region made of an oxide semiconductor; A semiconductor device in which one of a source or a drain of the first transistor is always electrically connected to one of a source or a drain of the second transistor, a first conductive film having a region located above a channel formation region of the first transistor and functioning as a gate electrode of the first transistor; a first insulating film having a region disposed above the first conductive film; a second conductive film having a region disposed above the first insulating film and functioning as a gate electrode of the second transistor; a third conductive film having a region disposed above the first insulating film; a second insulating film having a region disposed above the second conductive film and a region disposed above the third conductive film; a semiconductor film having a region disposed above the second insulating film and having a channel formation region of the second transistor; a third insulating film having a region disposed above the semiconductor film; a fourth conductive film having a region disposed above the third insulating film; a fifth conductive film having a region disposed above the third insulating film and always electrically connected to the third conductive film; having the third conductive film overlaps with the fifth conductive film; the fourth conductive film is always electrically connected to one of a source or a drain of the first transistor, and is always electrically connected to one of a source or a drain of the second transistor; when the third conductive film is electrically connected to the fourth conductive film at least through a channel formation region of the first transistor, the fifth conductive film is electrically connected to the fourth conductive film; Semiconductor device.

3. a first transistor including a channel formation region made of silicon and a second transistor including a channel formation region made of an oxide semiconductor; A semiconductor device in which one of a source or a drain of the first transistor is always electrically connected to one of a source or a drain of the second transistor, a first conductive film having a region located above a channel formation region of the first transistor and functioning as a gate electrode of the first transistor; a first insulating film having a region disposed above the first conductive film; a second conductive film having a region disposed above the first insulating film and functioning as a gate electrode of the second transistor; a third conductive film having a region disposed above the first insulating film; a second insulating film having a region disposed above the second conductive film and a region disposed above the third conductive film; a semiconductor film having a region disposed above the second insulating film and having a channel formation region of the second transistor; a third insulating film having a region disposed above the semiconductor film; a fourth conductive film having a region disposed above the third insulating film; a fifth conductive film having a region disposed above the third insulating film and always electrically connected to the third conductive film; having the fourth conductive film has a region in contact with an upper surface of the third insulating film, the fifth conductive film has a region in contact with an upper surface of the third insulating film, the fourth conductive film is always electrically connected to one of a source or a drain of the first transistor, and is always electrically connected to one of a source or a drain of the second transistor; when the third conductive film is electrically connected to the fourth conductive film at least through a channel formation region of the first transistor, the fifth conductive film is electrically connected to the fourth conductive film; Semiconductor device.

4. a first transistor including a channel formation region made of silicon and a second transistor including a channel formation region made of an oxide semiconductor; A semiconductor device in which one of a source or a drain of the first transistor is always electrically connected to one of a source or a drain of the second transistor, a first conductive film having a region located above a channel formation region of the first transistor and functioning as a gate electrode of the first transistor; a first insulating film having a region disposed above the first conductive film; a second conductive film having a region disposed above the first insulating film and functioning as a gate electrode of the second transistor; a third conductive film having a region disposed above the first insulating film; a second insulating film having a region disposed above the second conductive film and a region disposed above the third conductive film; a semiconductor film having a region disposed above the second insulating film and having a channel formation region of the second transistor; a third insulating film having a region disposed above the semiconductor film; a fourth conductive film having a region disposed above the third insulating film; a fifth conductive film having a region disposed above the third insulating film and always electrically connected to the third conductive film; having the second conductive film has a region in contact with an upper surface of the first insulating film, the third conductive film has a region in contact with an upper surface of the first insulating film, the fourth conductive film is always electrically connected to one of a source or a drain of the first transistor, and is always electrically connected to one of a source or a drain of the second transistor; when the third conductive film is electrically connected to the fourth conductive film at least through a channel formation region of the first transistor, the fifth conductive film is electrically connected to the fourth conductive film; Semiconductor device.

5. a first transistor including a channel formation region made of silicon and a second transistor including a channel formation region made of an oxide semiconductor; A semiconductor device in which one of a source or a drain of the first transistor is always electrically connected to one of a source or a drain of the second transistor, a first conductive film having a region located above a channel formation region of the first transistor and functioning as a gate electrode of the first transistor; a first insulating film having a region disposed above the first conductive film; a second conductive film having a region disposed above the first insulating film and functioning as a gate electrode of the second transistor; a third conductive film having a region disposed above the first insulating film; a second insulating film having a region disposed above the second conductive film and a region disposed above the third conductive film; a semiconductor film having a region disposed above the second insulating film and having a channel formation region of the second transistor; a third insulating film having a region disposed above the semiconductor film; a fourth conductive film having a region disposed above the third insulating film; a fifth conductive film having a region disposed above the third insulating film and always electrically connected to the third conductive film; having the third conductive film overlaps with the fifth conductive film; the fourth conductive film has a region in contact with an upper surface of the third insulating film, the fifth conductive film has a region in contact with an upper surface of the third insulating film, the fourth conductive film is always electrically connected to one of a source or a drain of the first transistor, and is always electrically connected to one of a source or a drain of the second transistor; when the third conductive film is electrically connected to the fourth conductive film at least through a channel formation region of the first transistor, the fifth conductive film is electrically connected to the fourth conductive film; Semiconductor device.

6. a first transistor including a channel formation region made of silicon and a second transistor including a channel formation region made of an oxide semiconductor; A semiconductor device in which one of a source or a drain of the first transistor is always electrically connected to one of a source or a drain of the second transistor, a first conductive film having a region located above a channel formation region of the first transistor and functioning as a gate electrode of the first transistor; a first insulating film having a region disposed above the first conductive film; a second conductive film having a region disposed above the first insulating film and functioning as a gate electrode of the second transistor; a third conductive film having a region disposed above the first insulating film; a second insulating film having a region disposed above the second conductive film and a region disposed above the third conductive film; a semiconductor film having a region disposed above the second insulating film and having a channel formation region of the second transistor; a third insulating film having a region disposed above the semiconductor film; a fourth conductive film having a region disposed above the third insulating film; a fifth conductive film having a region disposed above the third insulating film and always electrically connected to the third conductive film; having the third conductive film overlaps with the fifth conductive film; the second conductive film has a region in contact with an upper surface of the first insulating film, the third conductive film has a region in contact with an upper surface of the first insulating film, the fourth conductive film is always electrically connected to one of a source or a drain of the first transistor, and is always electrically connected to one of a source or a drain of the second transistor; when the third conductive film is electrically connected to the fourth conductive film at least through a channel formation region of the first transistor, the fifth conductive film is electrically connected to the fourth conductive film; Semiconductor device.

7. a first transistor including a channel formation region made of silicon and a second transistor including a channel formation region made of an oxide semiconductor; A semiconductor device in which one of a source or a drain of the first transistor is always electrically connected to one of a source or a drain of the second transistor, a first conductive film having a region located above a channel formation region of the first transistor and functioning as a gate electrode of the first transistor; a first insulating film having a region disposed above the first conductive film; a second conductive film having a region disposed above the first insulating film and functioning as a gate electrode of the second transistor; a third conductive film having a region disposed above the first insulating film; a second insulating film having a region disposed above the second conductive film and a region disposed above the third conductive film; a semiconductor film having a region disposed above the second insulating film and having a channel formation region of the second transistor; a third insulating film having a region disposed above the semiconductor film; a fourth conductive film having a region disposed above the third insulating film; a fifth conductive film having a region disposed above the third insulating film and always electrically connected to the third conductive film; having the third conductive film overlaps with the fifth conductive film; the second conductive film has a region in contact with an upper surface of the first insulating film, the third conductive film has a region in contact with an upper surface of the first insulating film, the fourth conductive film has a region in contact with an upper surface of the third insulating film, the fifth conductive film has a region in contact with an upper surface of the third insulating film, the fourth conductive film is always electrically connected to one of a source or a drain of the first transistor, and is always electrically connected to one of a source or a drain of the second transistor; when the third conductive film is electrically connected to the fourth conductive film at least through a channel formation region of the first transistor, the fifth conductive film is electrically connected to the fourth conductive film; Semiconductor device.

8. a first transistor including a channel formation region made of silicon and a second transistor including a channel formation region made of an oxide semiconductor; A semiconductor device in which one of a source or a drain of the first transistor is always electrically connected to one of a source or a drain of the second transistor, a first conductive film having a region located above a channel formation region of the first transistor and functioning as a gate electrode of the first transistor; a first insulating film having a region disposed above the first conductive film; a second conductive film having a region disposed above the first insulating film and functioning as a gate electrode of the second transistor; a third conductive film having a region disposed above the first insulating film; a second insulating film having a region disposed above the second conductive film and a region disposed above the third conductive film; a semiconductor film having a region disposed above the second insulating film and having a channel formation region of the second transistor; a third insulating film having a region disposed above the semiconductor film; a fourth conductive film having a region disposed above the third insulating film; a fifth conductive film having a region disposed above the third insulating film and always electrically connected to the third conductive film; having the second conductive film has a region in contact with an upper surface of the first insulating film, the third conductive film has a region in contact with an upper surface of the first insulating film, the fourth conductive film has a region in contact with an upper surface of the third insulating film, the fifth conductive film has a region in contact with an upper surface of the third insulating film, the fourth conductive film is always electrically connected to one of a source or a drain of the first transistor, and is always electrically connected to one of a source or a drain of the second transistor; when the third conductive film is electrically connected to the fourth conductive film at least through a channel formation region of the first transistor, the fifth conductive film is electrically connected to the fourth conductive film; Semiconductor device.

9. In any one of claims 1 to 8, a channel formation region of the first transistor is disposed in a silicon semiconductor film on an insulating surface; Semiconductor device.

Citation Information

Patent Citations

  • Electro-optical device, electronic apparatus, and semiconductor device

    JP2007251100A

  • Semiconductor device

    JP2009094494A

  • Fabricating method of semiconductor device

    JP2009135350A

  • Semiconductor device, and method of manufacturing semiconductor device

    JP2010141230A

  • Method of making a semiconductor device having an arched structure strained semiconductor layer

    US20060228872A1