Silicon carbide semiconductor device
The silicon carbide semiconductor device addresses leakage defects by using 3C-SiC source contact regions and 4H-SiC structures to achieve low resistance ohmic contact without a silicide layer, reducing damage and enhancing performance.
Patent Information
- Application Number
- JP2023044020
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-20
- Publication Date
- 2024-10-03
AI Technical Summary
Trench gate type silicon carbide semiconductor devices face issues with leakage defects due to damage in the source region caused by ion implantation, which inverts the conductivity type and forms silicide layers, leading to potential peeling and increased resistance.
The device employs a 3C-SiC structure for source contact regions to enable ohmic contact without a silicide layer, using 4H-SiC for source extension and base contact regions, and a 4H-SiC structure for the drift layer, reducing damage and leakage by interposing 4H-SiC between these regions.
This configuration suppresses leakage defects and reduces resistance by eliminating the need for a silicide layer, maintaining low resistance ohmic contact and minimizing damage from ion implantation, thereby enhancing the device's performance.
Smart Images

Figure 2024133974000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to silicon carbide semiconductor devices. [Background technology]
[0002] Patent Document 1 discloses a semiconductor device in which an amorphous layer is formed by ion-implanting phosphorus into a hexagonal single crystal silicon carbide substrate, the amorphous layer is recrystallized into cubic single crystal n-type silicon carbide by heat treatment, and an electrode is formed by vapor-depositing nickel on the upper surface of the n-type silicon carbide.
[0003] Patent Document 2 describes a n-type 4H-SiC + The n-type SiC was formed on the first main surface. - In the epitaxial growth layer, + A type source region, + n-type source region + Type 3C-SiC region and p + and a n-type potential clamping region. + Type 3C-SiC region and p + A semiconductor device is disclosed in which a barrier metal film is formed in contact with a type potential fixing region, and a source wiring electrode is formed on the barrier metal film. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2009-49198 A [Patent Document 2] International Publication No. 2017 / 042963 Summary of the Invention [Problem to be solved by the invention]
[0005] In a trench-gate silicon carbide semiconductor device, it has been considered to form the source region (main region) from 3C-SiC in order to make ohmic contact with the source electrode (main electrode). In this case, n-type impurity ions are implanted to form n + After forming a p-type source region on the entire surface, a mask is used to implant p-type impurities into the source region, reversing the conductivity type of a portion of the source region to p + From a manufacturing perspective, it is reasonable to form a base contact region on the source region. However, a lot of damage occurs in the part of the source region where the source region is pushed back, which may cause leakage defects.
[0006] In view of the above problems, an object of the present disclosure is to provide a trench-gate type silicon carbide semiconductor device in which a main region can make ohmic contact with a main electrode without a silicide layer and in which leakage defects can be suppressed. [Means for solving the problem]
[0007] In order to achieve the above object, one aspect of the present disclosure is a silicon carbide semiconductor device including: a drift layer of a first conductivity type made of silicon carbide; a base region of a second conductivity type made of silicon carbide and provided on an upper surface side of the drift layer; a source contact region of the first conductivity type made of silicon carbide and including a 3C structure and provided on an upper surface side of the base region; a gate insulating film provided inside a trench penetrating the source contact region and the base region; a gate electrode provided inside the trench via the gate insulating film; a base contact region of the second conductivity type made of silicon carbide with a 4H structure and having a higher impurity concentration than the base region and provided on the upper surface side of the drift layer; Effect of the Invention
[0008] According to the present disclosure, it is possible to provide a trench-gate silicon carbide semiconductor device in which a main region can be in ohmic contact with a main electrode without a silicide layer therebetween and leakage defects can be suppressed. [Brief description of the drawings]
[0009] [Figure 1] 1 is a schematic cross-sectional view showing an example of a silicon carbide semiconductor device in accordance with a first embodiment. [Diagram 2] 1 is a schematic perspective view showing an example of a silicon carbide semiconductor device in accordance with a first embodiment. [Diagram 3] 2 is a schematic cross-sectional view showing an enlarged area A of FIG. 1. [Figure 4] 5A to 5C are schematic cross-sectional views illustrating an example of a method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. [Diagram 5] 5 is a schematic cross-sectional view continuing from FIG. 4 for illustrating the example of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. FIG. [Figure 6] 6 is a schematic cross-sectional view continuing from FIG. 5 for illustrating the example of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. FIG. [Figure 7] 7 is a schematic cross-sectional view continuing from FIG. 6 for illustrating the example of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. FIG. [Figure 8] 8 is a schematic cross-sectional view continuing from FIG. 7 for illustrating the example of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. FIG. [Figure 9] 9 is a schematic cross-sectional view continuing from FIG. 8 for illustrating the example of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. [Figure 10] 10 is a schematic cross-sectional view continuing from FIG. 9 for illustrating the example of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. FIG. [Figure 11] 11 is a schematic cross-sectional view continuing from FIG. 10 for illustrating the example of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. FIG. [Figure 12]12 is a schematic cross-sectional view continuing from FIG. 11 for illustrating the example of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment. FIG. [Figure 13] 10A to 10C are schematic cross-sectional views for illustrating a method for manufacturing a silicon carbide semiconductor device according to a comparative example. [Figure 14] 14 is a schematic cross-sectional view continuing from FIG. 13 for illustrating a method for manufacturing a silicon carbide semiconductor device according to a comparative example. FIG. [Figure 15] 1 is a schematic cross-sectional view showing an example of a silicon carbide semiconductor device according to a second embodiment. [Figure 16] 16 is a schematic cross-sectional view showing an enlarged area A of FIG. 15. [Figure 17] 10 is a schematic cross-sectional view illustrating an example of a method for manufacturing a silicon carbide semiconductor device in accordance with a second embodiment. FIG. [Figure 18] 10 is a schematic cross-sectional view showing an example of a silicon carbide semiconductor device according to a third embodiment. [Figure 19] FIG. 19 is a schematic cross-sectional view showing an enlarged area A of FIG. [Figure 20] 10 is a schematic cross-sectional view showing an example of a silicon carbide semiconductor device in accordance with a fourth embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, the first to fourth embodiments of the present disclosure will be described with reference to the drawings. In the description of the drawings, the same or similar parts are denoted with the same or similar reference numerals, and duplicated explanations will be omitted. However, the drawings are schematic, and the relationship between thickness and planar dimensions, the ratio of thickness of each layer, etc. may differ from the actual ones. In addition, the drawings may include parts with different dimensional relationships and ratios. In addition, the first to fourth embodiments shown below are examples of devices and methods for embodying the technical idea of the present disclosure, and the technical idea of the present disclosure does not specify the materials, shapes, structures, arrangements, etc. of the components as described below.
[0011] In this specification, the source region of a metal-oxide semiconductor field-effect transistor (MOSFET) is "one main region (first main region)" that can be selected as the emitter region of an insulated gate bipolar transistor (IGBT). In addition, in a thyristor such as a MOS-controlled static induction thyristor (SI thyristor), the "one main region" can be selected as the cathode region. The drain region of a MOSFET is the "other main region (second main region)" of the semiconductor device that can be selected as the collector region in an IGBT and as the anode region in a thyristor. In this specification, when the term "main region" is used simply, it means either the first main region or the second main region that is appropriate from the technical common sense of a person skilled in the art.
[0012] In addition, the definitions of directions such as up and down in the following description are merely for the convenience of explanation and do not limit the technical idea of the present disclosure. For example, if an object is rotated 90 degrees and observed, up and down are converted to left and right and read as such, and if it is rotated 180 degrees and observed, up and down are of course read as reversed. In addition, "upper surface" may be read as "front surface" and "lower surface" may be read as "reverse surface."
[0013] In the following description, the first conductivity type is n-type and the second conductivity type is p-type. However, the conductivity types may be selected in the opposite relationship, with the first conductivity type being p-type and the second conductivity type being n-type. The + or - attached to n or p means that the semiconductor region has a relatively high or low impurity concentration, respectively, compared to a semiconductor region without + or -. However, even if the semiconductor regions have the same n and n attached, it does not mean that the impurity concentrations of the respective semiconductor regions are strictly the same.
[0014] Silicon carbide (SiC) crystals also have crystal polymorphism, the main ones being cubic 3C, and hexagonal 4H and 6H. The band gap at room temperature has been reported to be 2.23 eV for SiC with a 3C structure (3C-SiC), 3.26 eV for SiC with a 4H structure (4H-SiC), and 3.02 eV for SiC with a 6H structure (6H-SiC). The following explanation will be given as an example in which 4H-SiC and 3C-SiC are mainly used.
[0015] (First embodiment) <Structure of Silicon Carbide Semiconductor Device> The silicon carbide semiconductor device according to the first embodiment includes a trench-gate vertical MOSFET as an active element, as shown in Fig. 1. Note that Fig. 1 illustrates a unit cell including an insulated gate electrode structure (11, 12) embedded in one trench 10, but in reality, a large number of such unit cells are periodically arranged.
[0016] The silicon carbide semiconductor device according to the first embodiment is a first conductivity type (n - The drift layer 2 is formed of an epitaxially grown layer of SiC such as 4H-SiC. The impurity concentration of the drift layer 2 is, for example, 1×10 15 cm -3 That's it, 5 x 10 16 cm -3 The thickness of the drift layer 2 is, for example, about 1 μm or more and 100 μm or less. The impurity concentration and thickness of the drift layer 2 can be appropriately adjusted according to the withstand voltage specifications and the like.
[0017] Base regions 6a, 6b of a second conductivity type (p-type) are provided on the upper surface side of the drift layer 2. The lower surfaces of the base regions 6a, 6b are in contact with the upper surface of the drift layer 2. The base regions 6a, 6b are, for example, regions made of SiC such as 4H-SiC formed by ion implantation of p-type impurities into the drift layer 2. The base regions 6a, 6b may be regions made of SiC such as 4H-SiC epitaxially grown on the upper surface of the drift layer 2. The impurity concentration of the base regions 6a, 6b is, for example, 1×10 16 cm -3 That's it, 1×10 18 cm -3 It is about the following.
[0018] A current spreading layer (CSL) of a first conductivity type (n-type) having a higher impurity concentration than the drift layer 2 may be provided between the drift layer 2 and the base regions 6a and 6b. When the current spreading layer is provided, the upper surface of the drift layer 2 contacts the lower surface of the current spreading layer, and the upper surface of the current spreading layer contacts the lower surfaces of the base regions 6a and 6b.
[0019] The upper surface side of the base regions 6a and 6b is provided with a first conductivity type (n + First main regions (source regions) 7a, 7b of n-type (type) are selectively provided in the drift layer 2. The source regions 7a, 7b are regions made of SiC formed by ion-implanting n-type impurities into the drift layer 2, for example.
[0020] The source region 7a is an n-type semiconductor layer having a bottom surface in contact with the top surface of the base region 6a. + A source extension region (first region) 71a and a n-type MOSFET provided in a part of the upper portion (upper surface side) of the source extension region 71a. + The source region 7b includes an n-type source contact region (second region) 72a. The source region 7b is provided with its lower surface in contact with the upper surface of the base region 6b. + A source extension region (first region) 71b and a n-type MOSFET provided in a part of the upper portion (upper surface side) of the source extension region 71b. + The source regions 7a and 7b include a source contact region (second region) 72b. The source regions 7a and 7b will be described in detail later.
[0021] A trench 10 is provided penetrating the source regions 7a, 7b and the base regions 6a, 6b from the upper surfaces of the source regions 7a, 7b toward the normal direction (depth direction) of the upper surfaces of the source regions 7a, 7b. The lower surface of the trench 10 reaches the drift layer 2. If a current diffusion layer is provided, the lower surface of the trench 10 reaches the current diffusion layer. The width of the trench 10 is, for example, about 1 μm or less. The source region 7a and the base region 6a are in contact with the left side surface of the trench 10. The source region 7b and the base region 6b are in contact with the right side surface of the trench 10. The cross section of FIG. 1 illustrates a case where the lower surface and the side surface of the trench 10 form a corner, but the lower surface of the trench 10 may be a curved surface.
[0022] A gate insulating film 11 is provided along the bottom surface and both side surfaces of the trench 10. A gate electrode 12 is buried inside the trench 10 via the gate insulating film 11. The gate insulating film 11 and the gate electrode 12 form a trench-gate type insulated gate electrode structure (11, 12).
[0023] The gate insulating film 11 may be a single layer film of any one of silicon oxide film (SiO2 film), silicon oxynitride (SiON) film, strontium oxide (SrO) film, silicon nitride (Si3N4) film, aluminum oxide (Al2O3) film, magnesium oxide (MgO) film, yttrium oxide (Y2O3) film, hafnium oxide (HfO2) film, zirconium oxide (ZrO2) film, tantalum oxide (Ta2O5) film, and bismuth oxide (Bi2O3) film, or a composite film formed by stacking a plurality of these films. The gate electrode 12 may be made of a material such as a polysilicon layer (doped polysilicon layer) doped with a high concentration of p-type or n-type impurities, or a high-melting point metal such as titanium (Ti), tungsten (W), or nickel (Ni).
[0024] Inside the drift layer 2 and at the bottom (lower part) of the trench 10, a second conductivity type (p + The upper surface of the gate protection region 4b is in contact with the lower surface of the trench 10. The upper surface of the gate protection region 4b does not have to be in contact with the lower surface of the trench 10. The gate protection region 4b is, for example, a region made of SiC such as 4H-SiC formed by ion implantation of p-type impurities into the drift layer 2. The impurity concentration of the gate protection region 4b is, for example, 1×10 17 cm -3 That's it, 1×10 19 cm -3 It is about the following.
[0025] Within the drift layer 2, a second conductivity type (p +The buried regions 4a, 4c are formed at approximately the same depth as the gate protection region 4b. The buried regions 4a, 4c are formed of SiC such as 4H-SiC by ion implantation of p-type impurities into the drift layer 2. The impurity concentration of the buried regions 4a, 4c is, for example, 1×10 17 cm -3 That's it, 1×10 19 cm -3 In addition, in the front side or the back side of the paper surface of FIG. 1, the p + A semiconductor region of the type may be selectively provided.
[0026] The upper portion of the drift layer 2 and on the upper surface side of the buried regions 4a and 4c are provided with a second conductivity type (p + The base contact regions 5a and 5b are formed of, for example, SiC such as 4H-SiC in which p-type impurities are ion-implanted into the drift layer 2. The impurity concentration of the base contact regions 5a and 5b is, for example, 1×10 18 cm -3 That's it, 1×10 21 cm -3 The lower surfaces of the base contact regions 5a and 5b have a depth approximately equal to that of the lower surfaces of the base regions 6a and 6b, but may be shallower or deeper than the lower surfaces of the base regions 6a and 6b.
[0027] The lower surface of the base contact region 5a is in contact with the upper surface of the buried region 4a. When the lower surface of the base contact region 5a is shallower than the lower surface of the base region 6a, the base region 6 is provided between the lower surface of the base contact region 5a and the buried region 4a. The side surface of the base contact region 5a is in contact with the base region 6a and the source extension region 71a of the source region 7a. A part of the source extension region 71a, which is a semiconductor region of 4H-SiC, is interposed between the side surface of the base contact region 5a and the side surface of the source contact region 72a of the source region 7a. The source extension region 71a has an L-shaped cross section.
[0028] The lower surface of the base contact region 5b contacts the upper surface of the buried region 4c. When the lower surface of the base contact region 5b is shallower than the lower surface of the base region 6b, the base region 6 is provided between the lower surface of the base contact region 5b and the buried region 4c. The side surface of the base contact region 5b contacts the base region 6b and the source extension region 71b of the source region 7b. A part of the source extension region 71b, which is a semiconductor region of 4H-SiC, is interposed between the side surface of the base contact region 5b and the side surface of the source contact region 72b of the source region 7b. The source extension region 71b has an L-shaped cross section.
[0029] An interlayer insulating film 13 is provided on the upper surface side of the gate electrode 12. The interlayer insulating film 13 is composed of a single layer film such as a silicon oxide film (BPSG film) doped with boron (B) and phosphorus (P), a silicon oxide film (PSG film) doped with phosphorus (P), a non-doped silicon oxide film called "NSG" that does not contain phosphorus (P) or boron (B), a silicon oxide film (BSG film) doped with boron (B), a silicon nitride film (Si3N4 film), or a laminated film thereof. The interlayer insulating film 13 is provided with contact holes 13a and 13b so as to expose at least a part of the upper surfaces of the source extension regions 71a and 71b, the source contact regions 72a and 72b, and the base contact regions 5a and 5b.
[0030] First main electrodes (source electrodes) (14, 15, 16) are provided so as to cover the interlayer insulating film 13 and the source extension regions 71a, 71b, source contact regions 72a, 72b, and base contact regions 5a, 5b exposed in the contact holes 13a, 13b of the interlayer insulating film 13. The source electrodes (14, 15, 16) include a barrier metal layer 14, a source wiring layer 15, and a silicide layer 16.
[0031] The silicide layer 16 is selectively provided on the upper surfaces of the base contact regions 5a and 5b, and is in ohmic contact with the base contact regions 5a and 5b with low resistance. The silicide layer 16 is made of nickel silicide (NiSi xThe source electrodes (14, 15, 16) may be composed of only the barrier metal layer 14 and the source wiring layer 15 without including the silicide layer 16.
[0032] The barrier metal layer 14 is provided to cover the interlayer insulating film 13, the source extension regions 71a, 71b, the source contact regions 72a, 72b, and the silicide layer 16 exposed in the contact holes 13a, 13b of the interlayer insulating film 13. The barrier metal layer 14 is in direct contact with the source extension regions 71a, 71b and the source contact regions 72a, 72b. The barrier metal layer 14 is in ohmic contact with the source contact regions 72a, 72b having a 3C structure at low resistance, but is not in ohmic contact with the source extension regions 71a, 71b having a 4H structure. The barrier metal layer 14 is made of a metal such as titanium nitride (TiN), titanium (Ti), or a TiN / Ti laminated structure with Ti as the lower layer.
[0033] The source wiring layer 15 is provided so as to cover the barrier metal layer 14. The source wiring layer 15 is electrically connected to the source contact regions 72a, 72b and the base contact regions 5a, 5b. The source wiring layer 15 is made of a metal or an alloy such as aluminum (Al), aluminum-silicon (Al-Si), aluminum-copper (Al-Cu), copper (Cu), etc. The source wiring layer 15 is provided separately from a gate wiring electrode (not shown) electrically connected to the gate electrode 12.
[0034] The lower surface side of the drift layer 2 is provided with a first conductivity type (n + A second main region (drain region) 1 of a GaN type is provided. The drain region 1 is made of a semiconductor substrate (SiC substrate) made of SiC such as 4H-SiC. The impurity concentration of the drain region 1 is, for example, 1×10 19 cm -3 That's it, 3 x 10 20 cm -3The thickness of the drain region 1 is, for example, about 30 μm or more and 500 μm or less. Note that, between the drift layer 2 and the drain region 1, a dislocation conversion layer or a recombination promotion layer, which is an n-type buffer layer having a higher impurity concentration than the drift layer 2 and a lower impurity concentration than the drain region 1, may be provided.
[0035] A second main electrode (drain electrode) 17 is provided on the lower surface side of the drain region 1. The drain electrode 17 may be, for example, a single layer film made of gold (Au) or a metal film laminated in the order of titanium (Ti), nickel (Ni) and Au from the drain region 1 side, and further a metal film of molybdenum (Mo), tungsten (W) or the like may be laminated on the bottom layer. Nickel silicide (NiSi x A drain contact layer such as a SiO 2 film may be provided.
[0036] Fig. 2 is a schematic perspective view of a part of the semiconductor device according to the first embodiment shown in Fig. 1. As shown in Fig. 2, the trench 10 has a planar pattern extending in a stripe shape. The trench 10 is not particularly limited to a planar pattern extending in a stripe shape, and may have, for example, a dot-shaped planar pattern. The source extension regions 71a, 71b, the source contact regions 72a, 72b, and the base contact regions 5a, 5b have planar patterns extending in a stripe shape parallel to the trench 10.
[0037] Fig. 3 is a schematic cross-sectional view of an enlarged region A of the semiconductor device according to the first embodiment shown in Fig. 1. With reference to Fig. 3, the configurations of the source extension region 71a and the source contact region 72a, and the positional relationship between the source extension region 71a, the source contact region 72a, the base contact region 5a, and the insulated gate electrode structure (11, 12) will be described.
[0038] The depth d1 from the top surface to the bottom surface of the source extension region 71a (the thickness of the source extension region 71a) is, for example, about 150 nm or more and 450 nm or less. The width (w1+w2) of the source extension region 71a is, for example, about 400 nm or more and 1000 nm or less. The right side surface of the source extension region 71a directly contacts the gate insulating film 11 and faces the gate electrode 12 with the gate insulating film 11 interposed therebetween.
[0039] The source extension region 71a has fewer crystal defects than the source contact region 72a and does not inherit the crystal defects of the source contact region 72a. The source extension region 71a is mainly composed of 4H-SiC (4H structure). The proportion of 4H-SiC contained in the source extension region 71a is, for example, about 90% or more and 100% or less. In addition to 4H-SiC, the source extension region 71a may also contain small amounts of amorphous structure, 3C-SiC, etc. The impurity concentration of the source extension region 71a is, for example, 1×10 16 cm -3 That's it, 1×10 20 cm -3 The source extension region 71a contains, for example, nitrogen (N) or phosphorus (P) as an n-type impurity. The source extension region 71a may contain arsenic (As) as an n-type impurity.
[0040] The depth d2 from the upper surface to the lower surface of the source contact region 72a (thickness of the source contact region 72a) is, for example, about 30 nm or more and 100 nm or less. The width w1 of the source contact region 72a is narrower than the width (w1+w2) of the source extension region 71a and is, for example, about 400 nm or more and 1000 nm or less.
[0041] The right side surface of the source contact region 72a is in direct contact with the gate insulating film 11 and faces the interlayer insulating film 13 via the gate insulating film 11. The left side surface of the source contact region 72a is spaced apart from the right side surface of the base contact region 5a. A part of the source extension region 71a is interposed between the left side surface of the source contact region 72a and the right side surface of the base contact region 5a. The width w2 of the source extension region 71a sandwiched between the left side surface of the source contact region 72a and the right side surface of the base contact region 5a is, for example, about 10 nm or more and 500 nm or less.
[0042] The source contact region 72a is a region including 3C-SiC (3C structure). The ratio of 3C-SiC included in the source contact region 72a is higher than the ratio of 3C-SiC included in the source extension region 71a, and is, for example, about 10% or more and 100% or less. The source contact region 72a may be a mixed crystal of 3C-SiC and 4H-SiC. The source contact region 72a may include an amorphous structure, 4H-SiC, etc., in addition to 3C-SiC. Since 3C-SiC has a narrower band gap than 4H-SiC, the source contact region 72a including 3C-SiC can make ohmic contact with the source electrode (14, 15, 16) with low resistance without the silicide layer 16. To achieve good ohmic contact, the ratio of 3C-SiC included in the source contact region 72a is preferably 10% or more.
[0043] The impurity concentration of the source contact region 72a is higher than or equal to the impurity concentration of the source extension region 71a. The impurity concentration of the source contact region 72a is, for example, 1×10 20 cm -3 That's it, 1×10 22 cm -3or less. The source contact region 72a contains, for example, phosphorus (P) or arsenic (As) as an n-type impurity. The source contact region 72a may contain, for example, nitrogen (N) as an n-type impurity. The source contact region 72a may contain, for example, a plurality of types of P, As, and N as an n-type impurity. The source contact region 72a may contain an inert element such as argon (Ar) or helium (He).
[0044] The crystal structures of the source extension region 71a and the source contact region 72a can be made different by changing the element to be ion-implanted, the temperature during ion implantation, the dose (impurity concentration), the activation temperature, etc., for each of the source extension region 71a and the source contact region 72a. The source contact region 72a containing 3C-SiC can be formed, for example, by ion-implanting a high concentration (high dose) of n-type impurities or inert elements into 4H-SiC at room temperature, thereby breaking down the 4H-SiC and forming an amorphous structure by utilizing the damage caused by the ion implantation. Thereafter, activation annealing is performed, and the amorphous structure is recrystallized to become 3C-SiC, thereby forming the source contact region 72a containing 3C-SiC.
[0045] On the other hand, the source extension region 71a of 4H-SiC can be formed by ion implanting n-type impurities into 4H-SiC at room temperature or high temperature (e.g., 200° C. or higher and 600° C. or lower) at a concentration (dose) that does not destroy the structure of the 4H-SiC, thereby maintaining the 4H-SiC and forming the source extension region 71a. The source extension region 71a contains, for example, aluminum (Al) or boron (B) as a p-type impurity.
[0046] As a method for measuring (observing) the crystal structure of the source extension region 71a and the source contact region 72a, for example, a field emission scanning electron microscope (FE-SEM) and electron backscatter diffraction (EBSD) can be used to measure the area ratio of the crystal structure of the surface. As an example, samples were fabricated by changing the temperature during ion implantation between 500°C and room temperature (25°C) under the same conditions of the ion implantation element, dose (impurity concentration), and activation temperature, and the samples were observed by FE-SEM and EBSD. As a result, the ratio of 4H-SiC on the surface of the 500°C sample was 100%. On the other hand, the ratio of 4H-SiC on the surface of the room temperature sample was 86% and the ratio of 3C-SiC was 14%.
[0047] The method for forming the base contact region 5a of 4H-SiC is the same as the method for forming the source extension region 71a of 4H-SiC. The method for forming the base contact region 5a of 4H-SiC is to perform ion implantation of p-type impurities into 4H-SiC at room temperature or a high temperature (e.g., about 200° C. or higher and 600° C. or lower) at a concentration (dose) that does not destroy the structure of 4H-SiC, thereby forming the base contact region 5a while maintaining the 4H-SiC.
[0048] 3, the upper surface (upper end) of the gate electrode 12 at the end where it contacts the gate insulating film 11 is deeper than the lower surface (lower end) of the source contact region 72a at the end where it contacts the gate insulating film 11, and is shallower than the lower surface (lower end) of the source extension region 71a at the end where it contacts the gate insulating film 11. The upper surface of the gate electrode 12 at the end where it contacts the gate insulating film 11 may be the uppermost surface of the gate electrode 12. For example, if the upper surface of the gate electrode 12 as a whole is a curved surface that is convex downward, the upper surface of the center part of the gate electrode 12 may be deeper than the upper surfaces of the ends of the gate electrode 12.
[0049] The gate electrode 12 and the source extension region 71a face each other via the gate insulating film 11. The gate electrode 12 and the source contact region 72a do not face each other via the gate insulating film 11. The source contact region 72a faces the interlayer insulating film 13 via the gate insulating film 11. A depression amount d0 of the gate electrode 12 from an upper surface of the source contact region 72a is, for example, about 100 nm or more and 300 nm or less. The depression amount d0 of the gate electrode 12 and the position of the upper surface of the gate electrode 12 at the position where the gate electrode 12 contacts the gate insulating film 11 can be controlled by, for example, adjusting the etching conditions of the gate electrode 12.
[0050] The upper surface (upper end) of the gate electrode 12 at the position of the end where it contacts the gate insulating film 11 may be shallower than the lower surface (lower end) of the source contact region 72a at the position where it contacts the gate insulating film 11.
[0051] The source extension region 71b and the source contact region 72b of the source region 7b shown in Fig. 1 have the same configuration as the source extension region 71a and the source contact region 72a of the source region 7a, respectively, and therefore a duplicated description will be omitted. Also, the positional relationship between the source extension region 71b, the source contact region 72b, the base contact region 5b, and the insulated gate electrode structure (11, 12) is the same as the positional relationship between the source extension region 71a, the source contact region 72a, the base contact region 5a, and the insulated gate electrode structure (11, 12) of the source region 7a shown in Fig. 3, and therefore a duplicated description will be omitted.
[0052] During operation of the silicon carbide semiconductor device according to the first embodiment, when the source electrodes (14, 15, 16) are at earth potential, a positive voltage is applied to the drain electrode 17, and a positive voltage equal to or greater than a threshold is applied to the gate electrode 12, an inversion layer (channel) is formed on the side surface of the trench 10 in the base regions 6a, 6b, resulting in an ON state. In the ON state, a current flows from the drain electrode 17 to the source electrode (14, 15, 16) via the drain region 1, the drift layer 2, the inversion layer in the base regions 6a, 6b, and the source regions 7a, 7b. On the other hand, when the voltage applied to the gate electrode 12 is less than the threshold, an inversion layer is not formed in the base regions 6a, 6b, resulting in an OFF state, and no current flows from the drain electrode 17 to the source electrode (14, 15, 16).
[0053] In the silicon carbide semiconductor device according to the first embodiment, source contact regions 72a, 72b containing 3C-SiC of source regions 7a, 7b contact the source electrodes (14, 15, 16), thereby achieving ohmic contact with low resistance without the silicide layer 16. Therefore, the silicide layer 16 is not required on the contact junction surfaces of the source contact regions 72a, 72b, and peeling of the silicide layer 16 can be suppressed.
[0054] Furthermore, in the silicon carbide semiconductor device according to the first embodiment, the source extension regions 71a, 71b of 4H-SiC are interposed between the source contact regions 72a, 72b containing 3C-SiC and the base contact regions 5a, 5b of 4H-SiC. Therefore, compared to the case where the source contact regions 72a, 72b and the base contact regions 5a, 5b are in contact with each other, there is no damage caused by ion implantation for forming the source extension regions 71a, 71b in the base contact regions 5a, 5b, and leakage defects can be suppressed.
[0055] Furthermore, in the silicon carbide semiconductor device of the first embodiment, the pn junction formed by the 4H—SiC source extension regions 71a, 71b and the 4H—SiC base contact regions 5a, 5b is made of 4H—SiC, and therefore leakage current at the pn junction can be prevented compared to a case in which the pn junction is formed by source contact regions 72a, 72b containing 3C—SiC, which has many remaining crystal defects, and base contact regions 5a, 5b of 4H—SiC.
[0056] Furthermore, in the silicon carbide semiconductor device according to the first embodiment, the upper surface of the gate electrode 12 is made deeper than the lower surface of the source contact region 72a and shallower than the lower surface of the source extension region 71a. As a result, the source extension region 71a, which has relatively few crystal defects and little surface irregularity, of the source region 7a faces the gate electrode 12 via the gate insulating film 11, while the source contact region 72a, which has relatively many crystal defects and much surface irregularity, of the source region 7a, does not face the gate electrode 12 via the gate insulating film 11. This makes it possible to suppress the generation of leakage current between the source region 7a and the gate electrode 12.
[0057] <Method for manufacturing silicon carbide semiconductor device> Next, an example of a method for manufacturing the silicon carbide semiconductor device according to the first embodiment will be described. Note that the method for manufacturing the silicon carbide semiconductor device described below is just one example, and it goes without saying that various other manufacturing methods, including modifications thereof, can be implemented within the spirit and scope of the claims.
[0058] First, n-type impurities such as nitrogen (N) are added. + A semiconductor substrate (SiC substrate) 1 (see FIG. 4) made of SiC such as 4H-SiC is prepared. The top surface of the SiC substrate 1 has an off angle of, for example, 3 degrees to 8 degrees from the {0001} plane. Next, as shown in FIG. 4, n-type impurities such as N are added to the top surface of the SiC substrate 1 to form an n-type substrate with a lower impurity concentration than the SiC substrate 1. - A drift layer 2 made of SiC such as 4H-SiC of the type is epitaxially grown.
[0059] Next, an oxide film is deposited on the upper surface of the drift layer 2 by chemical vapor deposition (CVD) technology or the like. A photoresist film is applied to the upper surface of the oxide film, and the oxide film is patterned by photolithography technology, dry etching technology or the like. Using the patterned oxide film as an ion implantation mask, p-type impurities such as aluminum (Al) are selectively ion-implanted. Note that a photoresist film may be used as the ion implantation mask instead of the oxide film. Thereafter, the oxide film used as the ion implantation mask is removed. As a result, p-type impurities are formed inside the drift layer 2, as shown in FIG. 5. + The buried regions 4a, 4c and p + In the case of forming a charge storage layer (current diffusion layer), an n-type impurity is selectively injected at this stage to form the charge storage layer inside the drift layer 2.
[0060] In addition, the drift layer 2 shown in FIG. 4 is epitaxially grown up to the middle (lower) portion, and p + The buried regions 4a, 4c and p + Alternatively, the structure shown in FIG. 5 may be obtained by forming the gate protection region 4b of the transistor and epitaxially growing the remaining portion (upper portion) of the drift layer 2.
[0061] Next, the buried regions 4a, 4c and p + P-type impurities such as aluminum (Al) are ion-implanted into the entire surface at an acceleration voltage lower than that used for the ion-implantation when forming the gate protection region 4b. In addition, n-type impurities such as nitrogen (N) are ion-implanted into the entire surface at an acceleration voltage lower than that used for the ion-implantation when forming the base region 6. As a result, as shown in FIG. 6, a p-type base region 6 made of SiC such as 4H-SiC is formed on the upper surface side of the buried regions 4a, 4c and the gate protection region 4b. In addition, an n-type impurity such as nitrogen (N) is ion-implanted into the entire surface at an acceleration voltage lower than that used for the ion-implantation when forming the base region 6. + A source extension region 71 of the mold is formed.
[0062] In order to cause less damage during ion implantation of the source extension region 71 compared to ion implantation of source contact regions 72a and 72b described later, phosphorus (P) (atomic number 15) having a relatively small atomic number is preferable as the n-type impurity, and nitrogen (N) (atomic number 7) having a relatively small atomic number is more preferable. Note that, in addition to P or N, arsenic (As) (atomic number 33) having a relatively large atomic number may also be implanted. The temperature during ion implantation is set to be higher than that for ion implantation of the source contact regions 72a and 72b described later, for example, at a temperature of 200° C. or higher and 600° C. or lower. The dose during ion implantation is set so that the impurity concentration in the source extension region 71 is, for example, 1×10 16 cm -3 That's it, 1×10 20 cm -3 The dose during ion implantation is set to about 2×10 15 cm -2 It is set to less than this.
[0063] Next, an oxide film 20 (see FIG. 7) is deposited on the upper surface of the source extension region 71 by CVD technology or the like. A photoresist film is applied to the upper surface of the oxide film 20, and the oxide film 20 is patterned by photolithography technology, dry etching technology, or the like. Using the patterned oxide film 20 as an ion implantation mask, n-type impurities such as nitrogen (N) are selectively ion-implanted as shown in FIG. 7. Note that a photoresist film may be used as the ion implantation mask instead of the oxide film 20. As a result, n-type impurities such as nitrogen (N) are implanted into a portion of the upper surface (upper portion) of the source extension region 71. + A source contact region 72 of the type is selectively formed.
[0064] During ion implantation of the source contact region 72, the structure of 4H-SiC on the upper surface side of the source extension region 71 is broken to form an amorphous structure. FIG. 7 illustrates an example of ion implantation of N, but in order to cause higher damage than the ion implantation of the source extension region 71 described above, as the n-type impurity, P (atomic number 15) having a relatively larger number of atoms is preferable, and arsenic (As) (atomic number 33) having a relatively larger number of atoms is more preferable. During ion implantation of the source contact region 72, the same impurity as that used in the ion implantation of the source extension region 71 described above may be implanted, or a different impurity may be implanted. The temperature during ion implantation is set lower than the temperature during ion implantation of the source extension region 71 described above, for example, at 20° C. or higher and 150° C. or lower. The dose during ion implantation is set so that the impurity concentration of the source contact region 72 is, for example, 1×10 20 cm -3 That's it, 1×10 22 cm -3 The dose of ions to be implanted into the source extension region 71 is set to, for example, 2×10 15 cm -2 It is set to the above level.
[0065] When ion implanting the source contact region 72, an inert element such as argon (Ar) or helium (He) may be ion implanted instead of the n-type impurity. The total dose of the inert element ion implantation, including the dose of the ion implantation of the source extension region 71 described above, is, for example, 2×10 15 cm -2 or more. When an inert element is ion-implanted, the n-type impurity ion-implantation is performed only in the source extension region 71, so that the impurity concentrations in the source extension region 71 and the source contact region 72 are approximately the same. After the ion-implantation in the source contact region 72, the oxide film 20 used as the ion-implantation mask is removed.
[0066] Next, an oxide film 21 (see FIG. 8) is deposited on the upper surface of the base region 6 by CVD technology or the like. A photoresist film is applied to the upper surface of the oxide film 21, and the oxide film 21 is patterned by photolithography technology, dry etching technology or the like. The width w11 of the source contact region 72 is narrower than the width w12 of the mask pattern of the oxide film 21 covering the upper surface of the source contact region 72 (see FIG. 8). Using the patterned oxide film 21 as an ion implantation mask, as shown in FIG. 8, p-type impurities such as aluminum (Al) and boron (B) are selectively ion-implanted, thereby inverting (reversing) the conductivity type of a portion of the source extension region 71 from n-type to p-type. As a result, p-type impurities of 4H-SiC are formed on the upper surface sides of the buried regions 4a and 4c. + The base contact regions 5a, 5b are selectively formed. The base contact regions 5a, 5b are spaced apart from the source contact region 72 and are in contact with the source extension region 71 and the base region 6. Note that a photoresist film may be used as an ion implantation mask instead of the oxide film 21. Thereafter, the oxide film 21 used as the ion implantation mask is removed.
[0067] The order of the ion implantation for forming the base region 6, the ion implantation for forming the source extension region 71, the ion implantation for forming the source contact region 72, and the ion implantation for forming the base contact regions 5a and 5b is not limited to this, and may be changed. For example, the ion implantation for forming the source contact region 72 may be performed after the ion implantation for forming the base contact regions 5a and 5b.
[0068] Next, activation annealing (heat treatment) is performed at a temperature of, for example, about 1600° C. or higher and 1900° C. or lower using an annealing furnace or the like to simultaneously activate the p-type impurities or n-type impurities ion-implanted into the buried regions 4a, 4c, the gate protection region 4b, the source extension region 71, the source contact region 72, the base contact regions 5a, 5b, etc. At this time, the amorphous structure of the source contact region 72 is recrystallized to become 3C-SiC, and the source contact region 72 containing 3C-SiC is formed.
[0069] Although the case where one activation anneal is performed after all the ion implantation steps is exemplified here, activation anneal may be performed multiple times individually after each ion implantation step. Also, before activation anneal, a cap film made of carbon (C) may be formed, activation anneal is performed in a state where the substrate is covered with the cap film, and the cap film may be removed after activation anneal.
[0070] Next, an oxide film 22 (see FIG. 9) is deposited on the upper surfaces of the source extension region 71, the source contact region 72, and the base contact regions 5a, 5b by CVD or the like. A photoresist film is applied to the upper surface of the oxide film 22, and the oxide film 22 is patterned by photolithography, dry etching, or the like. Using the patterned oxide film 22 as an etching mask, a trench 10 is selectively formed in the depth direction from the upper surface of the source contact region 72 by dry etching such as reactive ion etching (RIE), as shown in FIG. 9. Note that a photoresist film may be used as the etching mask instead of the oxide film 22.
[0071] The trench 10 penetrates the source extension region 71, the source contact region 72, and the base region 6, and further excavates a part of the gate protection region 4b. The source extension region 71 is divided into two source extension regions 71a and 71b, the source contact region 72 is divided into two source contact regions 72a and 72b, and the base region 6 is divided into two base regions 6a and 6b. The source extension region 71a and the source contact region 72a form the source region 7a, and the source extension region 71b and the source contact region 72b form the source region 7b. Thereafter, the oxide film 22 used as the etching mask is removed.
[0072] Next, a gate insulating film 11 (see FIG. 10) is formed on the bottom and side surfaces of the trench 10, and on the top surfaces of the source extension regions 71a, 71b, the source contact regions 72a, 72b, and the base contact regions 5a, 5b by CVD technology, high temperature oxidation (HTO) method, thermal oxidation method, etc. When forming the gate insulating film 11, a heat treatment (PDA: Post Deposition Annealing) is performed at, for example, about 900° C. or higher and 1350° C. or lower.
[0073] Next, a polysilicon layer (doped polysilicon layer) doped with a high concentration of impurities such as phosphorus (P) or boron (B) is deposited by CVD technology or the like so as to fill the inside of the trench 10. After that, a part of the polysilicon layer and a part of the gate insulating film 11 are selectively removed by photolithography technology and dry etching. As a result, as shown in Fig. 10, an insulated gate electrode structure (11, 12) consisting of the gate insulating film 11 and the gate electrode 12 is formed. At this time, the amount of depression of the gate electrode 12 may be adjusted so that the upper surface of the gate electrode 12 at the position where it contacts the gate insulating film 11 is deeper than the lower surfaces of the source contact regions 72a, 72b.
[0074] Next, an interlayer insulating film 13 (see FIG. 11) is deposited on the upper surface of the insulated gate electrode structure (11, 12) by CVD technology or the like. Part of the interlayer insulating film 13 is selectively removed by photolithography technology, dry etching technology or the like, and contact holes 13a, 13b are opened in the interlayer insulating film 13, exposing at least part of the upper surfaces of the source extension regions 71a, 71b, the source contact regions 72a, 72b, and the base contact regions 5a, 5b, as shown in FIG. 11. Thereafter, a heat treatment (reflow) may be performed to planarize the interlayer insulating film 13.
[0075] Next, a silicide layer 16 (see FIG. 12) is deposited by sputtering or deposition, and a part of the silicide layer 16 is selectively removed by photolithography and etching. As a result, the silicide layer 16 is selectively formed on the upper surface of the base contact regions 5a and 5b. The silicide layer 16 makes ohmic contact with the base contact regions 5a and 5b with low resistance. Furthermore, a barrier metal layer 14 and a source wiring layer 15 are sequentially formed by sputtering or deposition so as to cover the interlayer insulating film 13, the source extension regions 71a and 71b, the source contact regions 72a and 72b, and the silicide layer 16 exposed in the contact holes 13a and 13b of the interlayer insulating film 13, as shown in FIG. 12, to form source electrodes (14, 15, 16). The barrier metal layer 14 makes ohmic contact with the source contact regions 72a and 72b of the source regions 7a and 7b with low resistance.
[0076] Although the source contact regions 72a, 72b and the base contact regions 5a, 5b are connected to the source electrodes (14, 15, 16) through the contact holes 13a, 13b, the source contact regions 72a, 72b and the base contact regions 5a, 5b may be connected to the source electrodes (14, 15, 16) through individual contact holes.
[0077] Next, as necessary, the SiC substrate 1 is thinned from the lower surface side by grinding, chemical mechanical polishing (CMP), or the like to adjust the thickness to form the drain region 1. Next, a drain electrode 17 (see FIG. 1) made of gold (Au) or the like is formed on the entire lower surface of the drain region 1 by a sputtering method, a vapor deposition method, or the like. In this manner, the silicon carbide semiconductor device shown in FIG. 1 is completed.
[0078] Here, a method for manufacturing a semiconductor device according to a comparative example will be described. In the method for manufacturing a semiconductor device according to the comparative example, a difference between an impurity concentration for satisfying a contact resistance required for source contact regions 72a, 72b and an impurity concentration for satisfying a contact resistance required for base contact regions 5a, 5b is utilized, which is rational from the viewpoint of manufacturing, and after forming n-type regions for forming source contact regions 72a, 72b on the entire surface, the conductivity type of a part of the n-type region is inverted (returned) to p-type to form base contact regions 5a, 5b.
[0079] Specifically, in the method for manufacturing a semiconductor device according to the comparative example, after the procedure for forming the base region 6 and the source extension region 71 shown in Fig. 6, n-type impurities such as nitrogen (N) are ion-implanted into the entire surface as shown in Fig. 13. As a result, the entire surface on the upper surface side of the source extension region 71 is doped with n + A source contact region 72 is formed.
[0080] Next, an oxide film 21 (see FIG. 14) is deposited on the upper surface of the base region 6, and the oxide film 21 is patterned. As shown in FIG. 14, the patterned oxide film 21 is used as an ion implantation mask to selectively implant ions of p-type impurities such as aluminum (Al), thereby inverting (reversing) the conductivity type of a portion of the source extension region 71 and the source contact region 72 to p-type. As a result, p-type impurities are formed on the upper surface sides of the buried regions 4a and 4c. + Mold base contact regions 5a, 5b are selectively formed.
[0081] However, in the manufacturing method of the semiconductor device according to the comparative example, leakage defects may occur in the bumped-back portions of the source contact region 72, which are the regions A1 and A2 shown by the dashed lines in Fig. 14. This is presumably because the ion implantation for forming the source contact region 72 and the ion implantation for forming the base contact regions 5a and 5b cause a lot of damage, causing the base contact regions 5a and 5b to become 3C-SiC, which becomes a leakage source.
[0082] In contrast, according to the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment, as shown in Fig. 8, during ion implantation for forming the base contact regions 5a, 5b, the base contact regions 5a, 5b can be formed by implanting a part of the source extension region 71 at a portion spaced apart from the source contact region 72 without implanting the source contact region 72. Therefore, the crystal structure of the base contact regions 5a, 5b remains unchanged and becomes 4H-SiC, thereby suppressing leakage defects.
[0083] Second embodiment As shown in FIG. 15, the silicon carbide semiconductor device in accordance with the second embodiment has n + 1 in that source contact regions 72a, 72b are spaced apart from the gate insulating film 11 inside the trench 10.
[0084] FIG. 16 is a schematic cross-sectional view of an enlarged broken-line region A shown in FIG. 15. The source contact region 72a is spaced from the gate insulating film 11 inside the trench 10. The width w3 of the source contact region 72a spaced from the gate insulating film 11 inside the trench 10 (in other words, the width of the source extension region 71a sandwiched between the source contact region 72a and the gate insulating film 11) is, for example, 100 nm or more and 500 nm or less. By setting the width w3 to 100 nm or more, it is possible to effectively prevent a gate leakage current, which will be described later. The width w1 of the source contact region 72a is, for example, 300 nm or more and 500 nm or less. The depth d2 from the upper surface to the lower surface of the source contact region 72a (the thickness of the source contact region 72a) is, for example, 30 nm or more and 100 nm or less.
[0085] In FIG. 16, the right end (side) of the source contact region 72a is located closer to the gate electrode 12 than the end of the contact hole 13a in the interlayer insulating film 13 (in other words, the ends of the gate insulating film 11 and the interlayer insulating film 13), but it may also coincide with the position of the end of the contact hole 13a.
[0086] The upper surface (upper end) of the gate electrode 12 at the position of the end in contact with the gate insulating film 11 is coincident with the lower surface of the source contact region 72a or is located at a position shallower than the lower surface of the source contact region 72a. The amount of depression d0 of the gate electrode 12 from the upper surface of the source extension region 71a is, for example, about 10 nm or more and 300 nm or less. By reducing the amount of depression d0 of the gate electrode 12 and making the upper surface of the gate electrode 12 shallower than the lower surface of the source contact region 72a, it is possible to reduce variations in the gate threshold voltage. Note that the upper surface of the end of the gate electrode 12 at the position of the end in contact with the gate insulating film 11 may be located at a position deeper than the lower surface of the source contact region 72a.
[0087] The source extension region 71b and the source contact region 72b of the source region 7b shown in Fig. 15 have the same configuration as the source extension region 71a and the source contact region 72a of the source region 7a, respectively, and therefore a duplicated description will be omitted. The positional relationship between the source extension region 71b and the source contact region 72b of the source region 7b and the base contact region 5b, the gate insulating film 11, and the gate electrode 12 is similar to the positional relationship between the source extension region 71a and the source contact region 72a of the source region 7a and the base contact region 5a, the gate insulating film 11, and the gate electrode 12 shown in Fig. 16, and therefore a duplicated description will be omitted. The other configurations of the silicon carbide semiconductor device according to the second embodiment are substantially similar to those of the silicon carbide semiconductor device according to the first embodiment, and therefore a duplicated description will be omitted.
[0088] The method for manufacturing a silicon carbide semiconductor device according to the second embodiment differs from the method for manufacturing a silicon carbide semiconductor device according to the first embodiment shown in FIG. 7 in that after the procedure for forming the base region 6 and source extension region 71 shown in FIG. 6, the oxide film 20 (see FIG. 17) is patterned using photolithography techniques, dry etching techniques, etc. so as to cover the region in which the trench 10 is formed.
[0089] 17, the patterned oxide film 20 is used as an ion implantation mask to selectively implant ions of n-type impurities such as nitrogen (N). Note that a photoresist film may be used as the ion implantation mask instead of the oxide film 20. As a result, n-type impurities such as nitrogen (N) are selectively implanted on the upper surface side of the source extension region 71. + In addition, source contact regions 72a, 72b of the silicon carbide semiconductor device according to the second embodiment are formed in the silicon carbide semiconductor device according to the first embodiment. Since other steps of the method for manufacturing the silicon carbide semiconductor device according to the second embodiment are substantially similar to those of the method for manufacturing the silicon carbide semiconductor device according to the first embodiment, a duplicated description will be omitted.
[0090] According to the second embodiment, the source contact regions 72a, 72b containing 3C-SiC of the source regions 7a, 7b contact the source electrodes (14, 15, 16), thereby achieving ohmic contact with low resistance without the silicide layer 16. Therefore, the silicide layer 16 is not required on the contact junction surfaces of the source contact regions 72a, 72b, and peeling of the silicide layer 16 can be suppressed.
[0091] Furthermore, according to the second embodiment, the source extension regions 71a, 71b of 4H-SiC are interposed between the source contact regions 72a, 72b containing 3C-SiC and the base contact regions 5a, 5b of 4H-SiC. Therefore, compared to the case where the source contact regions 72a, 72b and the base contact regions 5a, 5b are in contact with each other, there is no damage caused by ion implantation for forming the source extension regions 71a, 71b in the base contact regions 5a, 5b, and leakage defects can be suppressed.
[0092] Furthermore, according to the second embodiment, the pn junction formed by the 4H-SiC source extension regions 71a, 71b and the 4H-SiC base contact regions 5a, 5b is made of 4H-SiC, so that leakage current at the pn junction can be prevented more effectively than when the pn junction is formed by the source contact regions 72a, 72b containing 3C-SiC and the base contact regions 5a, 5b of 4H-SiC.
[0093] Furthermore, according to the second embodiment, the source contact regions 72a, 72b containing 3C-SiC with relatively many crystal defects in the source regions 7a, 7b are separated from the gate insulating film 11 and the gate electrode 12 inside the trench 10 so as not to directly contact the gate insulating film 11 inside the trench 10. On the other hand, the source extension regions 71a, 71b made of 4H-SiC with relatively few crystal defects in the source regions 7a, 7b are in direct contact with the gate insulating film 11 inside the trench 10 and face the gate electrode 12 via the gate insulating film 11. This makes it possible to suppress the generation of leakage current between the source regions 7a, 7b and the gate electrode 12.
[0094] Third embodiment As shown in FIG. 18, the silicon carbide semiconductor device in accordance with the third embodiment has n + 1 in that the 4H—SiC semiconductor regions interposed between the source contact regions 72a, 72b and the base contact regions 5a, 5b are part of the base regions 6a, 6b. The base regions 6a, 6b have an L-shaped cross section.
[0095] Fig. 19 is a schematic cross-sectional view of an enlarged region A shown in Fig. 18. The position of the left side surface of the source extension region 71a and the position of the left side surface of the source contact region 72a are approximately the same. The left side surfaces of the source extension region 71a and the source contact region 72a are spaced apart from the right side surface of the base contact region 5a. A part of the base region 6a is interposed between the left side surfaces of the source extension region 71a and the source contact region 72a and the right side surface of the base contact region 5a.
[0096] The source extension region 71b and the source contact region 72b of the source region 7b shown in Fig. 18 have the same configuration as the source extension region 71a and the source contact region 72a of the source region 7a, respectively, and therefore a duplicated description will be omitted. The positional relationship between the source extension region 71b and the source contact region 72b of the source region 7b and the base contact region 5b, the gate insulating film 11, and the gate electrode 12 is similar to the positional relationship between the source extension region 71a and the source contact region 72a of the source region 7a and the base contact region 5a, the gate insulating film 11, and the gate electrode 12 shown in Fig. 19, and therefore a duplicated description will be omitted. The other configurations of the silicon carbide semiconductor device according to the third embodiment are substantially similar to those of the silicon carbide semiconductor device according to the first embodiment, and therefore a duplicated description will be omitted.
[0097] In the method for manufacturing a silicon carbide semiconductor device in accordance with the third embodiment, in the procedure shown in FIG. 6, ion implantation for forming source extension region 71 is not performed, and source extension region 71 is not formed over the entire surface. Then, as shown in FIG. + When ion implantation is performed to form the n-type source contact region 72, the common oxide film 20 is used as an ion implantation mask to perform ion implantation. + A source extension region 71 of the type is formed to have the same width as the source contact region 72. The other procedures of the method for manufacturing the silicon carbide semiconductor device in accordance with the third embodiment are substantially similar to those of the method for manufacturing the silicon carbide semiconductor device in accordance with the first embodiment, and therefore repeated explanations will be omitted.
[0098] According to the third embodiment, the source contact regions 72a, 72b containing 3C-SiC of the source regions 7a, 7b contact the source electrodes (14, 15, 16), thereby making ohmic contact with low resistance without the silicide layer 16. Therefore, the silicide layer 16 is not required on the contact junction surfaces of the source contact regions 72a, 72b, and peeling of the silicide layer 16 can be suppressed.
[0099] Furthermore, according to the third embodiment, the base regions 6a, 6b made of 4H-SiC are interposed between the source contact regions 72a, 72b containing 3C-SiC and the base contact regions 5a, 5b made of 4H-SiC. Therefore, compared to the case where the source contact regions 72a, 72b and the base contact regions 5a, 5b are in contact with each other, there is no damage caused by ion implantation for forming the source extension regions 71a, 71b in the base contact regions 5a, 5b, and leakage defects can be suppressed.
[0100] (Fourth embodiment) As shown in FIG. 20, the silicon carbide semiconductor device in accordance with the fourth embodiment has n + The semiconductor device according to the second embodiment differs from the silicon carbide semiconductor device according to the first embodiment shown in FIG. 1 in that source extension regions 71a, 71b are formed thin.
[0101] Other configurations of the silicon carbide semiconductor device in accordance with the fourth embodiment are substantially similar to those of the silicon carbide semiconductor device in accordance with the first embodiment, and therefore duplicated descriptions will be omitted.
[0102] In the method for manufacturing a silicon carbide semiconductor device according to the fourth embodiment, ion implantation for source extension region 71 is not performed in the procedure shown in Fig. 6. In the procedure shown in Fig. 7, n-type impurities such as nitrogen (N) are selectively ion-implanted using patterned oxide film 20 as an ion implantation mask to implant n-type impurities into parts of the upper surface sides (upper portions) of base regions 6a, 6b. + A source contact region 72 is selectively formed in the SiO 2 layer.
[0103] When ion implantation is performed for the source contact region 72, the 4H-SiC structure on the upper surface of the base region 6 is destroyed to form an amorphous structure. At this time, ion implantation always generates a concentration gradient on the deeper side, so a low concentration portion naturally occurs on the deeper side. The low concentration portion becomes a 4H-SiC structure after heat treatment, so this 4H-SiC is called n +The other steps of the method for manufacturing a silicon carbide semiconductor device in accordance with the fourth embodiment are substantially similar to those of the method for manufacturing a silicon carbide semiconductor device in accordance with the first embodiment, and therefore a duplicated description will be omitted.
[0104] According to the fourth embodiment, even if the source extension regions 71a, 71b are thin, they can be in ohmic contact with low resistance without the silicide layer 16. Therefore, the silicide layer 16 is not required on the contact junction surfaces of the source contact regions 72a, 72b, and peeling of the silicide layer 16 can be suppressed.
[0105] Furthermore, according to the fourth embodiment, the base regions 6a, 6b made of 4H-SiC are interposed between the source contact regions 72a, 72b containing 3C-SiC and the base contact regions 5a, 5b made of 4H-SiC. Therefore, compared to the case where the source contact regions 72a, 72b and the base contact regions 5a, 5b are in contact with each other, there is no damage caused by ion implantation for forming the source extension regions 71a, 71b in the base contact regions 5a, 5b, and leakage defects can be suppressed.
[0106] (Other embodiments) As described above, the first to fourth embodiments of the present disclosure have been described, but the descriptions and drawings forming a part of this disclosure should not be understood as limiting the present disclosure. Various alternative embodiments, examples, and operating techniques will be apparent to those skilled in the art from this disclosure.
[0107] For example, a MOSFET is exemplified as the semiconductor device according to the first to fourth embodiments. + Instead of the drain region of type 1, p + The present invention can also be applied to insulated gate bipolar transistors (IGBTs) that have a collector region of a type other than IGBTs. In addition to IGBTs alone, the present invention can also be applied to reverse conducting IGBTs (RC-IGBTs) and reverse blocking insulated gate bipolar transistors (RB-IGBTs).
[0108] In addition, the configurations disclosed in the first to fourth embodiments can be appropriately combined within a range that does not cause a contradiction. For example, in the semiconductor device according to the third and fourth embodiments, + In the above example, the n-type source contact regions 72a and 72b are in contact with the gate insulating film 11 inside the trench 10. However, as in the semiconductor device according to the second embodiment, + The source contact regions 72a and 72b may be spaced apart from the gate insulating film 11 inside the trench 10.
[0109] Thus, the present disclosure naturally includes various embodiments not described herein. Therefore, the technical scope of the present disclosure is defined only by the invention-specifying matters related to the scope of the claims appropriate from the above description. [Explanation of symbols]
[0110] 1...Drain region (SiC substrate) 2. Drift layer 4a, 4c...Buried area 4b…Gate protection area 5a, 5b...Base contact region 6, 6a, 6b...Base region 7a, 7b…Source region 10. Trench 11...Gate insulating film 12...Gate electrode 13...Interlayer insulating film 13a, 13b...Contact holes 14...Barrier metal layer 15…Source wiring layer 16...Silicide layer 17…Drain electrode 20, 21, 22...Oxide film 71a, 71b...Source extension area 72, 72a, 72b...Source contact region
Claims
1. a drift layer of a first conductivity type made of silicon carbide; a second conductivity type base region made of silicon carbide and provided on an upper surface side of the drift layer; a first conductivity type source contact region made of silicon carbide having a 3C structure, the source contact region being provided on an upper surface side of the base region; a gate insulating film provided inside a trench penetrating the source contact region and the base region; a gate electrode provided inside the trench via the gate insulating film; a second conductivity type base contact region provided on an upper surface side of the drift layer, the second conductivity type base contact region being made of silicon carbide having a 4H structure and having a higher impurity concentration than the base region; a semiconductor region made of silicon carbide having a 4H structure provided between the source contact region and the base contact region; a main electrode provided in contact with the source contact region; A silicon carbide semiconductor device comprising:
2. The source contact region contacts the trench. The silicon carbide semiconductor device according to claim 1 .
3. The source contact region is spaced from the trench. The silicon carbide semiconductor device according to claim 1 .
4. a source extension region of a first conductivity type provided in contact with a lower surface of the source contact region and made of silicon carbide having a 4H structure; The silicon carbide semiconductor device according to claim 1 .
5. The semiconductor region is a part of the source extension region. The silicon carbide semiconductor device according to claim 4 .
6. The semiconductor region is a part of the base region. The silicon carbide semiconductor device according to claim 1 .
7. a first conductivity type source extension region made of silicon carbide having a 4H structure and provided in contact with a lower surface of the source contact region; A portion of the base region is disposed between the source extension region and the base contact region. The silicon carbide semiconductor device according to claim 6 .
8. The upper surface of the gate electrode is located deeper than the lower surface of the source contact region. The silicon carbide semiconductor device according to claim 1 .
9. The upper surface of the gate electrode is flush with the lower surface of the source contact region or is located shallower than the lower surface of the source contact region. The silicon carbide semiconductor device according to claim 3 .
10. The impurity concentration of the source extension region is lower than the impurity concentration of the source contact region. The silicon carbide semiconductor device according to claim 4 .
11. The impurity concentration of the source extension region is the same as the impurity concentration of the source contact region. The silicon carbide semiconductor device according to claim 4 .
12. The lower surface of the base contact region is aligned with the lower surface of the base region or is located shallower than the lower surface of the source contact region. The silicon carbide semiconductor device according to claim 1 .
13. The ratio of the 3C structure contained in the source contact region is 10% or more and 100% or less. The silicon carbide semiconductor device according to claim 1 .
14. The source contact region contains phosphorus or arsenic as an impurity. The silicon carbide semiconductor device according to claim 1 .
15. The impurity concentration of the source contact region is 1×10 20 / cm 3 That's it, 1 x 10 22 / cm 3 is less than or equal to The silicon carbide semiconductor device according to claim 1 .
16. The impurity concentration of the source extension region is 1×10 16 / cm 3 That's it, 1 x 10 20 / cm 3 is less than or equal to The silicon carbide semiconductor device according to claim 4 .
17. The source extension region contains nitrogen or phosphorus as an impurity. The silicon carbide semiconductor device according to claim 4 .
18. The impurity concentration of the base contact region is 1×10 19 / cm 3 That's it, 1 x 10 21 / cm 3 is less than or equal to The silicon carbide semiconductor device according to claim 1 .
19. The base contact region contains aluminum as an impurity. The silicon carbide semiconductor device according to claim 1 .
20. The main electrode includes a silicide layer in contact with the base contact region. The silicon carbide semiconductor device according to claim 1 .
Citation Information
Patent Citations
Semiconductor device and manufacturing method thereof
JP2009049198A
Semiconductor device and semiconductor device manufacturing method
JP2013058601A
Silicon carbide semiconductor device and method of manufacturing the same
JP2014033223A
Semiconductor device
JP2017168667A
Silicon carbide epitaxial substrate and manufacturing method therefor, silicon carbide semiconductor device and manufacturing method therefor
JP2020161735A