Etching method and method for manufacturing semiconductor device

The etching method for semiconductor devices addresses the challenge of processing accuracy in high aspect ratio recesses by forming a protective layer through oxidation and silylation, ensuring precise control of recess dimensions in three-dimensional memory structures.

JP2024134038AInactive Publication Date: 2024-10-03KIOXIA CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023044121
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-20
Publication Date
2024-10-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The challenge in manufacturing semiconductor devices is to improve the processing accuracy of recesses with high aspect ratios, particularly in three-dimensional memory structures.

Method used

An etching method involving the formation of a precursor film on the inner wall of a recess, followed by oxidation and silylation to create a protective layer, which is then etched to maintain precise dimensions, using a semiconductor manufacturing apparatus with controlled plasma and gas supply.

Benefits of technology

This method enhances the processing accuracy of recesses by uniformly controlling their dimensions from top to bottom, even in high aspect ratio structures, thereby improving the manufacturing precision of semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024134038000001_ABST
    Figure 2024134038000001_ABST
Patent Text Reader

Abstract

To increase the accuracy of finishing of a recess.SOLUTION: An etching method includes: supplying a precursor of an oxide having silicon atoms to a recess provided in a surface of an object to be processed, thereby forming a precursor film having a first region in contact with an inner wall surface of the recess; performing oxidation treatment to oxidize part of the first region from an upper part toward a lower part of the inner wall surface, thereby forming a first portion having an oxide; supplying a silylation reagent to the recess to silylate the first portion, thereby forming a second portion; and removing the remainder of the first region with the second portion remaining, and processing the recess.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD An embodiment of the present invention relates to an etching method and a method for manufacturing a semiconductor device. [Background technology]

[0002] 2. Description of the Related Art In a method for manufacturing a semiconductor device such as a three-dimensional memory, a technique for forming a recess having a high aspect ratio in an object to be processed by etching is known. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2022-45178 [Patent Document 2] JP 2022-115656 A Summary of the Invention [Problem to be solved by the invention]

[0004] The problem to be solved by the present invention in the embodiments is to improve the machining accuracy of the recesses. [Means for solving the problem]

[0005] In an embodiment of the etching method, a precursor of an oxide having silicon atoms is supplied to a recess provided on the surface of an object to be processed, thereby forming a precursor film having a first region in contact with the inner wall surface of the recess, a part of the first region is oxidized from the top to the bottom of the inner wall surface by oxidation treatment to form a first portion having an oxide, a silylation agent is supplied to the recess to silylate the first portion to form a second portion, and the remainder of the first region is removed by etching while leaving the second portion, thereby processing the recess. [Brief description of the drawings]

[0006] [Figure 1]1 is a flowchart for explaining an example of an etching method and an example of a method for manufacturing a semiconductor device. [Diagram 2] 1 is a schematic diagram showing an example of a semiconductor manufacturing apparatus that can be used in the example of an etching method and the example of a method for manufacturing a semiconductor device; [Diagram 3] 1 is a schematic cross-sectional view showing a structural example of an object 10 to be processed. [Figure 4] FIG. 11 is a schematic cross-sectional view illustrating a precursor supplying step S2. [Diagram 5] 2 is a schematic diagram for explaining an example of forming a precursor film 107. FIG. [Figure 6] FIG. 11 is a schematic cross-sectional view illustrating an example of an oxidation step S3. [Figure 7] 1 is a schematic diagram for explaining an example of oxidation of a precursor film 107. FIG. [Figure 8] FIG. 11 is a schematic cross-sectional view illustrating an example of a silylation step S4. [Figure 9] FIG. 2 is a schematic diagram for explaining an example of the formation of a silylated portion 108. [Figure 10] FIG. 11 is a schematic cross-sectional view for explaining an example of the etching step S5. [Figure 11] FIG. 11 is a schematic cross-sectional view for explaining an example of a memory layer forming step S6. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Hereinafter, the embodiments will be described with reference to the drawings. The relationship between the thickness and planar dimensions of each component, the thickness ratio of each component, etc. shown in the drawings may differ from the actual product. In addition, in the embodiments, substantially the same components are given the same reference numerals and the description will be omitted as appropriate.

[0008] 1 is a flow chart for explaining an example of an etching method and an example of a manufacturing method of a semiconductor device according to an embodiment. The semiconductor device is, for example, a three-dimensional memory. The manufacturing method of the semiconductor device includes a preparation step S1, a precursor supply step S2, an oxidation step S3, a silylation step S4, an etching step S5, and a memory layer formation step S6. These steps may be performed in order using separate devices, or may be performed consecutively using the same device without exposing the target to the atmosphere.

[0009] [Semiconductor manufacturing equipment] Fig. 2 is a schematic diagram showing an example of a semiconductor manufacturing apparatus as a processing apparatus usable in the etching method example and the semiconductor device manufacturing method example of the embodiment. Fig. 2 shows an example of a semiconductor manufacturing apparatus (e.g., an etching apparatus) capable of continuously performing a precursor supplying step S2, an oxidation step S3, a silylation step S4, and an etching step S5.

[0010] The semiconductor manufacturing apparatus 1 shown in FIG. 2 includes a chamber 2, a holder 3, a power supply unit 4, a gas supply unit 5, and a gas exhaust unit 6.

[0011] The chamber 2 is a space in which the workpiece 10 can be etched by sputtering using plasma (plasma etching).

[0012] The holder 3 is provided in the chamber 2. The holder 3 functions as a mounting table for mounting the workpiece 10. The holder 3 has, for example, an electrostatic chuck. The holder 3 may be connected to a temperature regulator.

[0013] The power supply unit 4 includes a high frequency power supply 41 and a high frequency power supply 42 .

[0014] The high frequency power supply 41 has a function of supplying high frequency power to the chamber 2. This makes it possible to generate plasma in the chamber 2. The high frequency power is, for example, not less than 50 W and not more than 5000 W. The frequency of the high frequency power is, for example, not less than 20 MHz and not more than 200 MHz.

[0015] The high frequency power supply 42 has a function of supplying high frequency power to the holder 3. This makes it possible to control the energy of ions colliding with the workpiece 10. The high frequency power is, for example, not less than 100 W and not more than 10,000 W. The frequency of the high frequency power is, for example, not less than 0.1 MHz and not more than 13.56 MHz.

[0016] The gas supply unit 5 includes, for example, a gas supply source 51 that supplies a first gas, a gas supply source 52 that supplies a second gas, a gas supply source 53 that supplies a third gas, and a gas supply source 54 that supplies a fourth gas. Each of the gas supply sources 51 to 54 is connected to the chamber 2. The gas supply unit 5 may further include a mass flow controller, and the flow rate of each of the first to fourth gases may be controlled by each mass flow controller.

[0017] The gas exhaust unit 6 is connected to the chamber 2. The gas exhaust unit 6 has a function of reducing the pressure inside the chamber 2 to create a vacuum state, and also has a function of exhausting the gas inside the chamber 2. The gas exhaust unit 6 is composed of, for example, a valve and a vacuum pump connected to the chamber 2.

[0018] The power supply unit 4, the gas supply unit 5, and the gas exhaust unit 6 may be controlled by a control circuit. The control circuit is configured using hardware that uses, for example, a processor or the like. Each operation may be stored as an operation program in a computer-readable recording medium such as a memory, and each operation may be executed by appropriately reading out the operation program stored in the recording medium by the hardware.

[0019] [Preparation process S1] In an example of the preparation step S1, the object 10 to be etched in the etching step S5 is prepared. The object 10 is placed on the holder 3 using a transfer arm and held under vacuum.

[0020] Fig. 3 is a cross-sectional schematic diagram showing a structural example of the object 10. Fig. 3 shows a part of an XZ cross section of the object 10. Fig. 3 shows an X-axis, a Y-axis perpendicular to the X-axis, and a Z-axis perpendicular to the X-axis and Y-axis.

[0021] The object 10 has a substrate 101, a lower layer 102, a first layer 103, a second layer 104, an upper layer 105, a mask layer 106, and a recess H. The object 10 is not limited to the configuration shown in FIG.

[0022] Examples of the substrate 101 include semiconductor substrates (wafers) such as silicon substrates and silicon carbide substrates, insulating substrates such as glass substrates, quartz substrates and sapphire substrates, and compound semiconductor substrates such as GaAs substrates. The surface of the substrate 101 extends along, for example, the X-axis and the Y-axis. The thickness direction of the substrate 101 is along, for example, the Z-axis.

[0023] The lower layer 102 is provided on the substrate 101. The lower layer 102 includes, for example, an insulating layer such as a silicon oxide layer or a silicon nitride layer, or a conductive layer between the insulating layers. The lower layer 102 is not necessarily provided.

[0024] The first layer 103 and the second layer 104 are alternately stacked on the lower layer 102 to form a stack. When the lower layer 102 is not provided, the first layer 103 or the second layer 104 is formed on the substrate 101. The number of stacked first layers 103 and second layers 104 is not limited to the number shown in FIG.

[0025] The first layer 103 is a sacrificial layer. The sacrificial layer is an area where a conductive layer will be formed later. The first layer 103 includes, for example, a silicon nitride film.

[0026] The second layer 104 includes, for example, a silicon oxide film.

[0027] The upper layer 105 is provided on a stack of the first layer 103 and the second layer 104. The upper layer 105 includes an insulating layer such as a silicon oxide layer or a silicon nitride layer, or a conductive layer between insulating layers. The upper layer 105 is not necessarily provided.

[0028] The mask layer 106 is provided on the upper layer 105. The mask layer 106 functions as a mask for etching a portion of the upper layer 105. Examples of the mask layer 106 include an organic hard mask, etc. The mask layer 106 may be removed after etching a portion of the upper layer 105.

[0029] The recess H penetrates the upper layer 105 to expose a portion of the laminate of the first layer 103 and the second layer 104. The recess H has an inner wall surface HA and an inner bottom surface HB. The inner wall surface HA extends in a direction intersecting with the laminate direction of the first layer 103 and the second layer 104. The inner bottom surface HB extends in a direction intersecting with the inner wall surface HA. The recess H has, for example, a hole shape in the XY plane. The shape of the recess H is not limited to a hole shape. The recess H can be formed in the laminate of the first layer 103 and the second layer 104 by, for example, reactive ion etching (RIE).

[0030] [Precursor supply process S2] 4 is a schematic cross-sectional view for explaining an example of the precursor supplying step S2, and shows a part of the XZ cross section of the object 10 to be processed.

[0031] In an example of the precursor supplying step S2, a precursor of an oxide having silicon atoms is supplied to the recess H to form a precursor film 107. The precursor film 107 covers each of the inner wall surface HA and the inner bottom surface HB of the recess H. The precursor film 107 has a region R1 facing the inner wall surface HA and a region R2 facing the inner bottom surface HB. The precursor film 107 does not have to be formed on the inner bottom surface HB of the recess H.

[0032] In an example of the precursor supplying step S2, for example, the first gas is supplied from the gas supply source 51 to the chamber 2 without supplying high-frequency power from the power supply unit 4 shown in FIG.

[0033] The first gas contains a precursor of an oxide having a silicon atom. The precursor preferably has a Si-H bond and does not have a Si-O bond. The precursor may have a Si-N bond. Examples of the precursor include dichlorosilane (DCS), tetrachlorosilane (SiCl4), bis(t-butylamino)silane (BTBAS), bis(diethylamino)silane (BDEAS), and the like.

[0034] When the first gas is formed by vaporizing the precursor liquid, the gas supply source 51 has a liquid supplier 511 that supplies the precursor liquid and a vaporizer 512 that vaporizes the precursor liquid, as shown in Fig. 2. When the precursor is a gas, the gas supply source 51 supplies the first gas to the chamber 2 without having the liquid supplier 511 and the vaporizer 512.

[0035] The precursor is adsorbed onto the surfaces of the inner wall surface HA and the inner bottom surface HB to form a precursor film 107. After the precursor film 107 is formed, the gas within the chamber 2 is exhausted via the gas exhaust part 6.

[0036] FIG. 5 is a schematic diagram for explaining an example of forming the precursor film 107. FIG. 5 shows a part of the XZ cross section. FIG. 5 shows an example in which the precursor film 107 is formed on the first layer 103 and the second layer 104 of the inner wall surface HA. When the precursor is BTBAS, the Si-N bond in the molecule of BTBAS is cut, and the cut part of the silicon atom is bonded to the nitrogen atom on the surface of the first layer 103 of the inner wall surface HA to form an -N-Si-H bond, and the cut part of the silicon atom is bonded to the oxygen atom on the surface of the second layer 104 of the inner wall surface HA to form an -O-Si-H bond. Thus, the precursor film 107 has silicon atoms, hydrogen atoms, oxygen atoms, and nitrogen atoms. The same reaction as that on the inner wall surface HA may also occur on other parts of the surface of the recess H, such as the surface of the inner bottom surface HB. Thus, the precursor film 107 can be formed. The number of -O-Si-H bonds and -N-Si-H bonds is not limited to the number shown in FIG. 5.

[0037] [Oxidation step S3] 6 is a schematic cross-sectional view for illustrating an example of the oxidation step S3. FIG 6 shows a part of the XZ cross section of the object 10 to be processed.

[0038] In an example of the oxidation step S3, a part of the region R1 is oxidized from the top to the bottom of the inner wall surface HA by oxidation treatment. The oxidation treatment is, for example, oxygen plasma treatment. The oxygen plasma treatment can be performed, for example, by supplying a second gas containing oxygen from the gas supply source 52 shown in FIG. 2 to the chamber 2 and supplying high frequency power from the power supply unit 4 to generate oxygen plasma in the chamber 2. The supply of the second gas and the supply of the high frequency power are stopped after the oxidation treatment.

[0039] FIG. 7 is a schematic diagram for explaining an example of oxidation of the precursor film 107. FIG. 7 shows a part of the XZ cross section. FIG. 7 shows an example in which the first layer 103 and the second layer 104 of a part of the region R1 formed on the inner wall surface HA are oxidized. The oxygen plasma treatment breaks the Si-H bonds on the surface of the precursor film 107, and the broken parts of the silicon atoms bond with oxygen atoms in the second gas to form -O-Si- bonds. This allows the formation of an oxidized portion 171 having an oxide. On the other hand, the remaining part of the region R1 and the region R2 corresponding to the lower region of the oxidized portion 171 become non-oxidized parts that are not oxidized by the oxidation treatment, and the surface layer still has a part of the precursor film 107 having -O-Si-H bonds and -N-Si-H bonds. The -O-Si- bonds are formed on the surface parts of the first layer 103 and the second layer 104 of the precursor film 107. The number of -O-Si- bonds is not limited to the number shown in FIG. 7.

[0040] The length of oxidized portion 171 in the depth direction of recess H is preferably, for example, 80% or more of the depth of recess H during the oxidation treatment. This makes it possible to suppress unnecessarily processing of inner wall surface HA by the etching step S5, which would increase the width, such as the diameter, of recess H. The length of oxidized portion 171 can be adjusted, for example, by changing the treatment time of the oxygen plasma treatment. After the oxidation treatment, the gas in chamber 2 is exhausted via gas exhaust part 6.

[0041] The precursor supplying step S2 and the oxidation step S3 are repeatedly performed until the thickness of the precursor film 107 reaches or exceeds a desired value.

[0042] [Silylation step S4] 8 is a schematic cross-sectional view for illustrating an example of the silylation step S4. FIG 8 shows a part of the XZ cross section of the object 10.

[0043] In an example of the silylation step S4, a silylation agent is supplied to the recess H to silylate the oxidized portion 171, thereby forming a silylated portion 108 on the oxidized portion 171. The silylation agent is supplied to the chamber 2 by supplying a third gas containing the silylation agent from the gas supply source 53 to the chamber 2 without supplying high-frequency power from the power supply unit 4 shown in FIG. 2. The supply of the third gas is stopped after silylation. When the third gas is generated by vaporizing the liquid of the silylation agent, the gas supply source 53 may be provided with a liquid supplier and a vaporizer, similar to the gas supply source 51.

[0044] The silylating agent is, for example, a silane compound containing a silicon atom, a hydrogen atom, and a carbon atom. The silylating agent may have a Si-N bond. Examples of the silylating agent include aminosilane compounds, chlorosilane compounds, methoxysilane compounds, and cyclic silane compounds.

[0045] Examples of aminosilane compounds include N-(trimethylsilyl)dimethylamine (TMSDMA), hexamethyldisilazane (HMDS), n-octyldimethyl(dimethylamino)silane (ODMDMAS), etc. The silylating agent is C n H 2n+2 (n is a natural number of 2 or more), and the like.

[0046] Examples of chlorosilane compounds include octadecyltrichlorosilane (ODTC). Examples of methoxysilane compounds include octadecyltrimethoxysilane (ODMS). Examples of cyclic silane compounds include N-methyl-aza-2,2,4-methylsilacyclopentane (CAZ).

[0047] FIG. 9 is a schematic diagram for explaining an example of the formation of the silylated portion 108. FIG. 9 shows a part of the XZ cross section. For example, when the silylation agent is TMSDMA, the Si-N bond in the molecule of TMSDMA is broken by the silylation reaction, and the broken part of the silicon atom is bonded to an oxygen atom on the oxidized portion 171 to form a Si-O-Si-(CH3)3 bond. Thus, the silylated portion 108 has a silicon atom, an oxygen atom, a carbon atom, and a hydrogen atom. The Si-O-Si-(CH3)3 bond is formed on the surface portion of the first layer 103 and the second layer 104 of the oxidized portion 171. The number of Si-O-Si-(CH3)3 bonds is not limited to the number shown in FIG. 9.

[0048] On the other hand, the remainder of region R1 and region R2 are unoxidized portions that have not been oxidized by the oxidation process, and therefore still have -O-Si-H bonds. Therefore, they have hydrogen atoms at their ends. In these portions, the silylation reaction does not occur. Therefore, silylated portions 108 are not formed on the remainder of region R1 and on region R2. After the silylation step S4, the gas in chamber 2 is exhausted via gas exhaust section 6.

[0049] [Etching process S5] 10 is a schematic cross-sectional view for explaining an example of the etching step S5, and shows a part of the XZ cross section of the object 10.

[0050] 10, in an example of the etching step S5, the remainder of the region R1 and the region R2 are removed by etching while leaving the silylated portion 108, and the recess H is processed. This etches the exposed portion of the inner wall surface HA and the inner bottom surface HB. As a result, the first layer 103 and the second layer 104 located below the inner bottom surface HB are further processed, and the depth of the recess H is increased.

[0051] The etching is, for example, RIE. The etching is performed by supplying a fourth gas from the gas supply source 54, supplying high-frequency power from the power supply unit 4 to generate plasma from the fourth gas, and removing the remainder of the region R1 and the region R2 by sputtering using the plasma, and processing the recess H. The supply of the fourth gas and the supply of the high-frequency power are stopped after the etching.

[0052] The fourth gas may include, for example, carbon atoms, hydrogen atoms, and fluorine atoms. x H y F z (wherein C represents carbon, H represents hydrogen, F represents fluorine, x represents an integer of 1 or more, y represents an integer of 0 or more, and z represents an integer of 2 or more).

[0053] The silylated portion 108 functions as a protective film for suppressing etching by plasma generated from the fourth gas, thereby suppressing etching of the region R1 covered with the silylated portion 108. In addition, the remainder of the region R1 where the silylated portion 108 is not formed and the region R2 can be removed, and the recess H can be processed.

[0054] By etching, a film 109 may be formed on the silylated portion 108. The film 109 has carbon atoms, nitrogen atoms, and fluorine atoms. The film 109 functions as a protective film for suppressing etching by plasma generated from the fourth gas. The film 109 may contain, for example, 40 atomic % to 60 atomic % carbon (C), 10 atomic % to 20 atomic % nitrogen (N), and 20 atomic % to 30 atomic % fluorine (F) in total, which amounts to 100 atomic %.

[0055] The silylated portion 108 and film 109 formed in the etching step S5 are removed together with the oxidized portion 171 by a method such as ashing using oxygen plasma at a temperature of 250° C. or higher before the memory layer formation step S6.

[0056] In the exemplary etching method and exemplary semiconductor device manufacturing method of the embodiment, these steps are repeated until the aspect ratio of the recess H becomes equal to or greater than a desired value.

[0057] When etching is performed using an etching gas containing a fluorinated hydrocarbon compound, the recess tends to taper from the top to the bottom. This is because the plasma generated from the etching gas has difficulty reaching the bottom of the inner wall surface of the recess or the area closer to the inner bottom surface of the recess, and etching tends to proceed at the top of the inner wall surface of the recess. As a result, a dimensional difference tends to occur from the top to the bottom of the recess H.

[0058] In contrast, in the etching method example and the semiconductor device manufacturing method example of the embodiment, before the silylation step, an oxidized portion having silicon atoms is formed on a part of the inner wall surface from the top to the bottom of the recess, and then the oxidized portion is silylated to form a silylated portion, which suppresses the progress of etching in the upper part of the inner wall surface of the recess, and allows the lower part of the inner wall surface and the inner bottom surface to be etched. Therefore, even when forming a recess H having a high aspect ratio, the processing accuracy of the recess H can be improved. As a result, it becomes possible to uniformly control the dimensions of the recess H from the top to the bottom of the recess H.

[0059] [Memory layer formation process S6] 11 is a schematic cross-sectional view for explaining an example of the memory layer forming step S6. FIG 11 shows a part of the XZ cross section of the object 10.

[0060] In the memory layer formation step S6, a memory film 203 including a block insulating film 233, a charge storage layer 232, and a tunnel insulating film 231, a semiconductor channel layer 202, and a core insulating film 201 are formed in this order in the recessed portion H. The core insulating film 201, the semiconductor channel layer 202, and the memory film 203 function as a memory layer constituting a memory cell.

[0061] The core insulating film 201 may be, for example, a silicon oxide film. The semiconductor channel layer 202 may be, for example, a polysilicon layer. The tunnel insulating film 231 may be, for example, a stacked film having a silicon oxide film and a silicon oxynitride film. The charge storage layer 232 may be, for example, a silicon nitride film. The block insulating film 233 may be, for example, a silicon oxide film.

[0062] After forming the memory film 203, the first layer 103 is removed, a cavity is formed between the second layer 104, and a plurality of conductive films are laminated in the cavity to form the conductive layer 110. The conductive layer 110 functions as, for example, a gate electrode (word line). Furthermore, contact plugs, wiring, interlayer insulating films, etc. are formed. In this way, a semiconductor device can be manufactured.

[0063] Although a memory hole in which a memory layer is formed is exemplified as an example of the recess H in this embodiment, the application of this embodiment is not limited to the memory hole. For example, this embodiment can be applied to various recesses such as a trench (ST) for replacing a sacrificial layer with a conductive layer 110 and a hole for forming a contact plug connected to the conductive layer 110.

[0064] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]

[0065] 1...semiconductor manufacturing apparatus, 2...chamber, 3...holder, 4...power supply unit, 5...gas supply unit, 6...gas exhaust unit, 10...object to be processed, 41...high frequency power supply, 42...high frequency power supply, 51...gas supply source, 52...gas supply source, 53...gas supply source, 54...gas supply source, 101...substrate, 102...lower layer, 103...first layer, 104...second layer, 105...upper layer, 106...mask layer, 107...precursor film, 108...silylated portion, 109...film, 110... Conductive layer, 171...oxidized portion, 201...core insulating film, 202...semiconductor channel layer, 203...memory film, 231...tunnel insulating film, 232...charge storage layer, 233...block insulating film, 511...liquid supplier, 512...vaporizer, H...recess, HA...inner wall surface, HB...inner bottom surface, R1...region, R2...region, S1...preparation step, S2...precursor supply step, S3...oxidation step, S4...silylation step, S5...etching step, S6...memory layer formation step.

Claims

1. supplying a precursor of an oxide having silicon atoms into a recess provided in a surface of an object to be processed, thereby forming a precursor film having a first region in contact with an inner wall surface of the recess; forming a first portion having the oxide by oxidizing a portion of the first region from the upper portion to the lower portion of the inner wall surface through an oxidation process; supplying a silylation agent to the recess to silylate the first portion to form a second portion; removing the remainder of the first region while leaving the second portion by etching, and forming the recess; Etching method.

2. The precursors are dichlorosilane (DCS), tetrachlorosilane (SiCl 4 ), bis(t-butylamino)silane (BTBAS), or bis(diethylamino)silane (BDEAS).

3. The etching method of claim 1 , wherein the silylation agent includes silicon atoms, hydrogen atoms, and carbon atoms.

4. 2. The etching method according to claim 1, wherein the oxidation treatment oxidizes a part of the first region and does not oxidize a remainder of the first region.

5. 2. The etching method of claim 1, wherein the first portion is formed by an oxygen plasma.

6. The etching is carried out by using a compound of formula C x H y F z 2. The etching method according to claim 1, wherein the etching is performed using a fluoride gas represented by the formula: (C represents carbon, H represents hydrogen, F represents fluorine, x represents an integer of 1 or more, y represents an integer of 0 or more, and z represents an integer of 2 or more).

7. a film is formed on the silylated first portion by the etching; The etching method of claim 1 , wherein the film comprises carbon, fluorine, and nitrogen.

8. The etching method according to claim 1 , wherein the silylation is performed after the formation of the precursor film and the oxidation are alternately switched multiple times.

9. The etching method of claim 1 , wherein the first and second portions are removed after the etching.

10. 2. The etching method according to claim 1, wherein the formation of the precursor film, the oxidation, the silylation, and the etching are performed successively using a same semiconductor manufacturing apparatus without exposing the workpiece to the atmosphere.

11. preparing an object to be processed having a plurality of layers stacked on a substrate and a recess penetrating the plurality of layers; supplying a precursor of an oxide having silicon atoms into the recess to form a precursor film having a first region in contact with an inner wall surface of the recess; forming a first portion having the oxide by oxidizing a portion of the first region from the upper portion to the lower portion of the inner wall surface through an oxidation process; supplying a silylation agent to the recess to silylate the first portion to form a second portion; removing the remainder of the first region while leaving the second portion by etching, and forming the recess; A method for manufacturing a semiconductor device.

Citation Information

Patent Citations

  • Semiconductor manufacturing device and method for manufacturing semiconductor device

    JP2022045178A

  • Manufacturing method of semiconductor device

    JP2022115656A