Manufacturing method of semiconductor device
By aligning ion implantation regions with grooves and forming protective films with the groove bottom inside, the method prevents gallium nitride decomposition during annealing, ensuring accurate alignment and efficient semiconductor device production.
Patent Information
- Application Number
- JP2023044612
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-20
- Publication Date
- 2024-10-03
- Estimated Expiration
- 2043-03-20
AI Technical Summary
Grooves formed on semiconductor substrates as alignment marks can lead to thinner protective film thickness at their boundaries, causing gallium nitride decomposition during annealing treatment.
A method involving protective film formation with the groove bottom within the film and aligned ion implantation regions, followed by annealing, to maintain sufficient film thickness and alignment, thereby suppressing gallium nitride decomposition.
The method effectively prevents gallium nitride decomposition during annealing while ensuring precise alignment for groove formation, enhancing the manufacturing process of semiconductor devices.
Smart Images

Figure 2024134353000001_ABST
Abstract
Description
[Technical field]
[0001] The technology disclosed in this specification relates to a method for manufacturing a semiconductor device. [Background technology]
[0002] Patent Document 1 discloses a technique for forming a p-type semiconductor region in a gallium nitride (GaN)-based semiconductor substrate by ion implantation. In this technique, after p-type impurities are implanted, a protective film is formed on the surface of the semiconductor substrate. After the protective film is formed, the semiconductor substrate is annealed. During annealing, the protective film suppresses decomposition of gallium nitride. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2019-175905 A Summary of the Invention [Problem to be solved by the invention]
[0004] Grooves may be formed on the surface of a semiconductor substrate as alignment marks. When a protective film is formed on the surface of the semiconductor substrate with the grooves formed thereon, the thickness of the protective film may become thin at the boundary between the bottom and side surfaces of the grooves. When such a portion occurs, gallium nitride in the semiconductor substrate is likely to decompose at that portion during annealing. This specification provides a technology for forming grooves for alignment while suppressing decomposition of gallium nitride during annealing. [Means for solving the problem]
[0005] This specification discloses a method for manufacturing a semiconductor device. The manufacturing method may include a step of forming a protective film (48) on a surface (10c) of a semiconductor substrate (10) made of a gallium nitride semiconductor, the protective film being formed such that a groove (42) exists on the surface of the protective film and the bottom of the groove is located within the protective film, and an ion implantation step of implanting ions into the semiconductor substrate to form an ion implantation region (30). The protective film formation step and the ion implantation step may be performed such that the groove and the ion implantation region are aligned with each other. The manufacturing method may further include an annealing step of performing an annealing treatment on the semiconductor substrate after the step of forming the protective film and the step of forming the ion implantation region, and a processing step of forming processed portions (50, 52, 54) on the semiconductor substrate in a state aligned with the groove after the annealing step.
[0006] In the above technology, the term "gallium nitride semiconductor" refers to a semiconductor whose main component is GaN, such as GaN, AlGaN, or InGaN.
[0007] In the above technique, the order in which the protective film forming step and the ion implantation step are performed is not particularly limited. That is, the ion implantation step may be performed after the protective film forming step, or the protective film forming step may be performed after the ion implantation step. Furthermore, the ion implantation step may be performed during the protective film forming step.
[0008] In the above technique, "alignment" includes both direct alignment and indirect alignment. That is, "the groove and the ion implantation region are aligned with each other" may mean that the groove and the ion implantation region are directly aligned with each other, or that the groove and the other member are aligned with each other and that the ion implantation region and the other member are aligned with each other, thereby indirectly aligning the groove and the ion implantation region with each other. Also, "forming the processed portion (50, 52, 54) on the semiconductor substrate in a state aligned with the groove" may mean that the processed portion is formed in a state directly aligned with the groove, or that the processed portion is formed in a state in which it is aligned with the other member that is aligned with the groove, thereby forming the processed portion in a state in which it is indirectly aligned with the groove.
[0009] A protective film is formed on the surface of the semiconductor substrate, in which a groove is formed with its bottom located within the protective film. By adjusting the depth of the groove, a sufficient thickness of the protective film can be ensured at the bottom of the groove to suppress decomposition of gallium nitride. This suppresses decomposition of gallium nitride during annealing. In addition, the groove and the ion implantation region are aligned with each other before performing the annealing process. In addition, after performing the annealing process, a processed portion is formed on the semiconductor substrate in a state where the groove is aligned. Therefore, the processed portion can be formed in a state where it is aligned with the ion implantation region. In this way, according to the above configuration, it is possible to suppress decomposition of gallium nitride during annealing while forming a groove for alignment. [Brief description of the drawings]
[0010] [Figure 1] 10A to 10C are diagrams for explaining a first cap film forming step in the first embodiment. [Diagram 2] FIG. 4 is a diagram for explaining a first groove forming step in the first embodiment. [Diagram 3] 10A to 10C are views for explaining a first cap film removal step in the first embodiment. [Figure 4] FIG. 2 is a diagram for explaining an ion implantation process in the first embodiment. [Diagram 5] 10A to 10C are diagrams for explaining a second cap film forming step and an annealing step in the first embodiment. [Figure 6] FIG. 11 is a view for explaining a second cap film removal step in the first embodiment. [Figure 7] FIG. 2 is a diagram for explaining an electrode forming step in the first embodiment. [Figure 8] 13 is a view for explaining a recess forming step in the second embodiment. FIG. [Figure 9] FIG. 11 is a view for explaining a second cap film removal step in the second embodiment. [Figure 10] FIG. 11 is a diagram for explaining an electrode forming step in Example 2. [Figure 11] 11A to 11C are diagrams for explaining an ion implantation process in the third embodiment. [Figure 12] 13A to 13C are diagrams for explaining a cap film forming step in the third embodiment. [Figure 13] 13A to 13C are diagrams illustrating a groove forming step and an annealing step in Example 3. [Figure 14] 13A to 13C are diagrams for explaining a cap film removing step in the third embodiment. [Figure 15] FIG. 11 is a diagram for explaining an electrode forming step in Example 3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] In one embodiment of the present technology, the protective film forming step includes a first protective film forming step of forming a first protective film (20) and a second protective film forming step of forming a second protective film (40), and these steps are performed in the order of the first protective film forming step, the ion implantation step, and the second protective film forming step. In the first protective film forming step, the first protective film is formed on the surface of the semiconductor substrate such that a first groove (22) is present in the surface of the first protective film, a bottom of the first groove is located within the first protective film, and the first protective film has an opening through which the surface of the semiconductor substrate is exposed. In the ion implantation step, the ion implantation region is formed within the opening in a state aligned with the first groove. In the second protective film forming step, the second protective film is formed to cover the opening and the first protective film. In the second protective film forming step, a second groove (42) is formed on the surface of the second protective film along the first groove, and the second groove may be the groove.
[0012] This configuration also makes it possible to form grooves for alignment while suppressing decomposition of gallium nitride during annealing.
[0013] In one embodiment of the present technology, the protective film forming step may be performed after the ion implantation step, and in the protective film forming step, the groove may be formed in a state aligned with the ion implantation region.
[0014] This configuration also makes it possible to form grooves for alignment while suppressing decomposition of gallium nitride during annealing.
[0015] The method may further include the steps of forming a recess (112) on the surface of the semiconductor substrate by deepening the groove so as to reach the semiconductor substrate after the annealing step, and removing the protective film after the recess is formed. In the processing step, the processed portion may be formed in a state aligned with the recess.
[0016] This configuration also makes it possible to form a groove for alignment while suppressing decomposition of gallium nitride during annealing. In particular, since a recess is formed that reaches the semiconductor substrate, the recess is highly visible when forming a processed portion in a state where the processed portion is aligned with the recess.
[0017] Example 1 A method for manufacturing a semiconductor device according to a first embodiment will be described. The semiconductor device is manufactured from a semiconductor substrate 10 shown in FIG. 1. The semiconductor substrate 10 is made of gallium nitride (GaN). In a modified example, the semiconductor substrate 10 may be made of a GaN-based semiconductor containing GaN as a main component, such as AlGaN or InGaN. The semiconductor substrate 10 has a drain layer 10a and a drift layer 10b. The drain layer 10a and the drift layer 10b are both n-type semiconductor regions. The n-type impurity concentration of the drain layer 10a is higher than the n-type impurity concentration of the drift layer 10b. The semiconductor substrate 10 has a front surface 10c and a back surface 10d. The front surface 10c is a part of the drift layer 10b. The back surface 10d is a part of the drain layer 10a.
[0018] The manufacturing method of Example 1 includes a first cap film forming step, a first groove forming step, a first cap film removing step, an ion implantation step, a second cap film forming step, an annealing step, a second cap film removing step, and an electrode forming step.
[0019] In the first cap film formation step, as shown in Fig. 1, a first cap film 20 is formed on the front surface 10c and back surface 10d of the semiconductor substrate 10. The first cap film 20 is made of AlN, AlGaN, ScN, ScAlN, C, etc. Although Fig. 1 shows the first cap film 20 made of a single layer, the first cap film 20 may be a laminated structure of two or more layers. The first cap film 20 is an example of a "first protective film."
[0020] 2, in the first groove forming step, a first groove 22 is formed in the surface of the first cap film 20. The first groove 22 is formed by, for example, etching. The first groove 22 is formed so that its bottom is located within the first cap film 20.
[0021] 3, in the first cap film removal step, a part of the first cap film 20 is removed. Specifically, the first cap film 20 is selectively etched to remove the first cap film 20 from the region other than the vicinity of the first groove 22. In the region from which the first cap film 20 has been removed, the surface 10c of the semiconductor substrate 10 is exposed.
[0022] In the ion implantation process, as shown in Fig. 4, p-type impurities and n-type impurities are selectively implanted into the surface 10c within the exposed area. This forms an ion implantation region 30 in the drift layer 10b. During the ion implantation, the first groove 22 is used as an alignment mark. That is, the ion implantation region 30 is formed in a state aligned with the first groove 22. Therefore, the first groove 22 and the ion implantation region 30 are aligned with each other.
[0023] The ion implantation region 30 includes a body layer 32, a source layer 34, and a contact layer 36. The body layer 32 and the contact layer 36 are p-type semiconductor regions. The source layer 34 is an n-type semiconductor region. The p-type impurity concentration of the body layer 32 is lower than the p-type impurity concentration of the contact layer 36. The n-type impurity concentration of the source layer 34 is higher than the n-type impurity concentration of the drift layer 10b.
[0024] In the second cap film forming step, as shown in FIG. 5, a second cap film 40 is formed on the upper part of the semiconductor substrate 10. In the range where the surface 10c is exposed, the second cap film 40 is formed so as to cover the surface 10c. In the range where the first cap film 20 exists, the second cap film 40 is formed so as to overlap the first cap film 20. The second cap film 40 is formed so as to cover the first cap film 20. A second groove 42 is formed on the surface of the second cap film 40 along the first groove 22 formed in the first cap film 20. Since the second groove 42 is formed along the first groove 22, the second groove 42 and the ion implantation region 30 are aligned with each other. The first cap film 20 and the second cap film 40 complete the protective film 48. The protective film 48 covers the entire surface 10c of the semiconductor substrate 10. A second groove 42 is provided on the surface of the protective film 48. The bottom of the second groove 42 is located within the protective film 48. The second cap film 40 is an example of a "second protective film."
[0025] In the annealing step, an annealing process is performed on the semiconductor substrate 10 with the protective film 48 formed (i.e., in the state shown in FIG. 5). The annealing process activates the ion implantation region 30. Since the entire surface 10c of the semiconductor substrate 10 is covered with the protective film 48, decomposition of gallium nitride on the surface 10c during annealing is suppressed.
[0026] 6, in the second cap film removal step, a portion of the second cap film 40 is removed. Specifically, the second cap film 40 is selectively etched to remove the second cap film 40 from the region other than the vicinity of the second groove 42. In the region from which the second cap film 40 has been removed, the surface 10c of the semiconductor substrate 10 is exposed.
[0027] In the electrode formation step, as shown in FIG. 7, a gate insulating film 50, a gate electrode 52, and a source electrode 54 are formed on the upper part of the ion implantation region 30. Here, the second groove 42 is used as an alignment mark to form the gate insulating film 50, the gate electrode 52, and the source electrode 54. That is, the gate insulating film 50, the gate electrode 52, and the source electrode 54 are formed by aligning with the second groove 42. As described above, the ion implantation region 30 is aligned with the first groove 22, and the second groove 42 is aligned with the first groove 22, so that the ion implantation region 30 is aligned with the second groove 42. Therefore, by aligning the gate insulating film 50, the gate electrode 52, and the source electrode 54 with the second groove 42, the second groove 42 can be aligned with the ion implantation region 30. The gate insulating film 50 is formed in a range spanning from the surface of the source layer 34 to the surface of the drift layer 10b. The gate electrode 52 is formed on the upper part of the gate insulating film 50. The source electrode 54 is formed in an area spanning the surfaces of the source layer 34 and the contact layer 36. The gate insulating film 50, the gate electrode 52, and the source electrode 54 are an example of a "processed portion".
[0028] In the electrode formation step, a drain electrode 56 is formed in contact with the rear surface 10d. Through the above steps, a semiconductor device (for example, a MOSFET (Metal Oxide Semiconductor Field Effect Transistor)) is completed.
[0029] In this manner, with the above-described configuration, it is possible to suppress decomposition of gallium nitride during annealing while forming the second grooves 42 for alignment.
[0030] Example 2 Next, a manufacturing method of Example 2 will be described. In the manufacturing method of Example 2, the first cap film forming step to the annealing step are performed in the same manner as in Example 1. That is, processing is performed until the state shown in Fig. 5 is reached. In the manufacturing method of Example 2, after the annealing step, a recess forming step, a second cap film removing step, and an electrode forming step are performed.
[0031] In the recess forming step, as shown in Fig. 8, the second trench 42 is deepened to form a recess 112 that reaches the semiconductor substrate 10 (more specifically, the drift layer 10b). The recess 112 is formed by deepening the second trench 42, for example, by etching. As described above, the second trench 42 and the ion implantation region 30 are aligned. Since the recess 112 is formed by deepening the second trench 42, the recess 112 and the ion implantation region 30 are aligned with each other.
[0032] 9, in the second cap film removal step, the first cap film 20 and the second cap film 40 are entirely removed by etching. When the second cap film removal step is performed, the surface 10c of the semiconductor substrate 10 is exposed.
[0033] Next, in the electrode formation step, as shown in FIG. 10, the gate insulating film 50, the gate electrode 52, and the source electrode 54 are formed. Here, the recess 112 is used as an alignment mark to form the gate insulating film 50, the gate electrode 52, and the source electrode 54. As described above, the recess 112 is aligned with the ion implantation region 30. Therefore, by forming the gate insulating film 50, the gate electrode 52, and the source electrode 54 while aligning them with the recess 112, the gate insulating film 50, the gate electrode 52, and the source electrode 54 can be aligned with the ion implantation region 30. In addition, in the electrode formation step, a drain electrode 56 in contact with the rear surface 10d is formed. Through the above steps, the semiconductor device is completed.
[0034] The configuration of Example 2 also makes it possible to suppress decomposition of gallium nitride during annealing while forming the recesses 112 for alignment. In particular, the configuration of Example 2 makes it possible to form the recesses 112 deeper than the second grooves 42, so that the recesses 112 are easily recognized as alignment marks.
[0035] Example 3 Next, a description will be given of a manufacturing method of Example 3. The manufacturing method of Example 3 includes an ion implantation step, a cap film formation step, a groove formation step, an annealing step, a cap film removal step, and an electrode formation step.
[0036] In the ion implantation process, as shown in FIG. 11, ion implantation regions 30 and 230 are formed. Specifically, ions are first selectively implanted into the semiconductor substrate 10 to form the source layer 34 and the ion implantation region 230 in the range exposed on the surface 10c. At this stage, the ion implantation region 230 is visible. Next, ion implantation is performed using the ion implantation region 230 as an alignment mark to form the contact layer 36 and the body layer 32. Thus, the ion implantation region 230 and the ion implantation region 30 are aligned with each other.
[0037] 12, in the cap film formation step, a cap film 20 is formed on the front surface 10c and the back surface 10d of the semiconductor substrate 10. The cap film 20 is transparent.
[0038] In the groove forming step, as shown in FIG. 13, a groove 22 is formed on the surface of the cap film 20. The groove 22 is formed by, for example, etching. Since the cap film 20 is transparent, the ion implantation region 30 can be optically detected from the outside. Here, the ion implantation region 30 is used as an alignment mark to form the groove 22 in the cap film 20. That is, the groove 22 is formed in a state of being aligned with the ion implantation region 30. Here, the groove 22 is formed on the upper part of the ion implantation region 230. The groove 22 is formed so that its bottom is located within the cap film 20. In addition, the groove 22 is formed to a depth such that the cap film 20 having a thickness (for example, 40 nm or more) that does not decompose gallium nitride during annealing treatment remains at the bottom of the groove 22.
[0039] In the annealing step, an annealing process is performed on the semiconductor substrate 10 with the cap film 20 formed (i.e., in the state shown in FIG. 13). The annealing process activates the ion implantation region 30. Since the entire surface 10c of the semiconductor substrate 10 is covered with the cap film 20, decomposition of gallium nitride on the surface 10c during annealing is suppressed. When the annealing process is performed, the ion implantation region 230 changes color and cannot be visually recognized. For this reason, the groove 22 is used as an alignment mark after the annealing process is performed.
[0040] After the annealing process, a cap film removal process is performed. In the cap film removal process, a part of the cap film 20 is removed as shown in Fig. 14. Specifically, the cap film 20 is selectively etched to remove the cap film 20 from the region other than the vicinity of the groove 22. In the region from which the cap film 20 has been removed, the surface 10c of the semiconductor substrate 10 is exposed.
[0041] 15, in the electrode formation step, the grooves 22 are used as alignment marks to form the gate insulating film 50, the gate electrode 52, and the source electrode 54. Therefore, the gate insulating film 50, the gate electrode 52, and the source electrode 54 can be formed in alignment with the ion implantation region 30. Also, in the electrode formation step, a drain electrode 56 is formed.
[0042] In the configuration of the third embodiment, the grooves 22 for alignment can be formed while suppressing the decomposition of gallium nitride during annealing.
[0043] In the configurations of Example 1 and Example 2, the process of forming the cap film is performed twice (a first cap film forming process and a second cap film forming process). In contrast, in the configuration of Example 3, the cap film forming process only needs to be performed once. Therefore, the manufacturing process of the semiconductor device can be simplified.
[0044] In the modified example of the third embodiment, instead of performing the cap film removing step and the electrode forming step after performing the annealing step, each step after the recess forming step in the second embodiment may be performed.
[0045] Specific examples of the technology disclosed in this specification have been described in detail above, but these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and variations of the specific examples exemplified above. The technical elements described in this specification or drawings exhibit technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. In addition, the technology exemplified in this specification or drawings can achieve multiple objectives simultaneously, and achieving one of these objectives is itself technically useful. [Explanation of symbols]
[0046] 10: semiconductor substrate, 10a: drain layer, 10b: drift layer, 10c: front surface, 10d: back surface, 20: first cap film, 22: first trench, 30: ion implantation region, 32: body layer, 34: source layer, 36: contact layer, 40: second cap film, 42: second trench, 48: protective film, 50: gate insulating film, 52: gate electrode, 54: source electrode, 56: drain electrode, 112: recess, 230: ion implantation region
Claims
1. A method for manufacturing a semiconductor device, comprising: a protective film forming step of forming a protective film (48) on a surface (10c) of a semiconductor substrate (10) made of a gallium nitride semiconductor, the protective film being formed so that a groove (42) is present on the surface of the protective film and the bottom of the groove is located within the protective film; an ion implantation step of implanting ions into the semiconductor substrate to form an ion implantation region (30); having performing the protective film forming step and the ion implantation step such that the groove and the ion implantation region are aligned with each other; an annealing step of performing an annealing treatment on the semiconductor substrate after the step of forming the protective film and the step of forming the ion implantation region; a processing step of forming processed portions (50, 52, 54) in the semiconductor substrate in a state aligned with the grooves after the annealing step; The method of manufacturing further comprises:
2. The protective film forming step includes a first protective film forming step of forming a first protective film (20) and a second protective film forming step of forming a second protective film (40), performing the first protective film forming step, the ion implantation step, and the second protective film forming step in this order; In the first protective film forming step, a first groove (22) is formed on the surface of the first protective film, the bottom of the first groove is located within the first protective film, and the first protective film has an opening through which the surface of the semiconductor substrate is exposed; In the ion implantation step, the ion implantation region is formed in the opening in a state aligned with the first groove, In the second protective film forming step, the second protective film is formed so as to cover the opening and the first protective film; In the second protective film forming step, a second groove (42) is formed on a surface of the second protective film along the first groove, The second groove is the groove. The method of claim 1 .
3. The protective film forming step is carried out after the ion implantation step; In the protective film forming step, the groove is formed in a state aligned with the ion implantation region. The method of claim 1 .
4. forming a recess (112) in the surface of the semiconductor substrate by deepening the trench so as to reach the semiconductor substrate after the annealing step; removing the protective film after forming the recess; and In the processing step, the processed portion is formed in a state aligned with the recess. The method according to any one of claims 1 to 3.
Citation Information
Patent Citations
Method of manufacturing semiconductor device
JP2018010970A
Method of manufacturing semiconductor device
JP2018170334A
Method of manufacturing semiconductor device
JP2020141105A
Method for manufacturing nitride semiconductor device