Repair method of seal ring groove

The insertion of a shim plate into the seal ring groove addresses the issue of corrosion-induced deformation, providing a cost-effective repair solution that maintains sealing integrity.

JP2024134642AActive Publication Date: 2024-10-04NAN SEIKO CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023044939
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Existing methods are inadequate for repairing seal ring grooves corroded by corrosion without deforming the surrounding area, leading to costly replacement of components.

Method used

A method involving the insertion of a shim plate, preferably made of stainless steel, into the seal ring groove to cover the corroded bottom surface, followed by fitting the seal ring into the groove, with a caulking agent applied to enhance sealing.

Benefits of technology

The method effectively repairs the seal ring groove without deforming the surrounding area, ensuring reliable sealing performance at reduced costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024134642000001_ABST
    Figure 2024134642000001_ABST
Patent Text Reader

Abstract

To provide a method which can reliably repair a seal ring groove, such as an O ring groove, eroded by corrosion without deforming a surrounding portion.SOLUTION: A repair method of a sealing ring groove of the invention comprises: a step in which a seal ring 13 is taken out from a seal ring groove 12 in which a groove bottom surface 14 is eroded; a step in which a thin sim plate 20 in which an end is obliquely cut out is inserted into the groove bottom surface 14 of the seal ring groove 12; and a step in which the seal ring 13 is fitted in the seal ring groove 12 into which the sim plate 20 is inserted.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for repairing a seal ring groove whose sealing performance has been reduced due to corrosion. [Background technology]

[0002] Seal rings, such as O-rings, are incorporated into many devices to seal fluids such as gases and liquids. A seal ring groove that is shallower than the thickness of the seal ring is formed in the sealing part, and the seal ring fitted inside is crushed by the mating part, and the repulsive force of the seal ring creates a sealing effect.

[0003] A schematic diagram is shown in Figure 1. In Figure 1, 10 is a cylinder, and 11 is a shaft with a circular cross section that slides inside it. A seal ring groove 12 is formed on the inner peripheral surface of cylinder 10, and an O-ring, or seal ring 13, is fitted inside it. Seal ring 13 is crushed by shaft 11, and the repulsive force causes it to adhere closely to the outer peripheral surface of shaft 11, sealing the fluid inside cylinder 10.

[0004] When the rubber elasticity of such a seal ring 13 decreases after long-term use, it can be replaced with a new seal ring 13. However, when the seal ring 13 is used to seal a hydraulic cylinder, for example, the inside of the seal ring groove 12 can be corroded and eroded by additives contained in the hydraulic oil, and a dent 15 can occur in the bottom surface 14 of the groove as shown diagrammatically in Figure 2.

[0005] If a depression 15 occurs in the groove bottom 14 of the seal ring groove 12, the seal ring 13 will sink further into the groove bottom 14 side than its normal position, and the repulsive force will decrease accordingly, impairing the sealing performance and potentially resulting in oil leakage.

[0006] Therefore, when such a depression 15 occurs in the seal ring groove 12, it is possible to fill the depression 15 by build-up welding and repair the groove bottom surface 14. However, there is a risk that the peripheral portion of the seal ring groove 12 will deform due to the heat applied in that case, so this repair method is difficult to adopt.

[0007] Patent Document 1 discloses that a crevice corrosion detector can be incorporated into a pump or other structure to enable early detection of crevice corrosion. However, this is only a crevice corrosion detection method, not a repair method. Furthermore, even after searching other patent documents, we were unable to find any patent documents related to repairing O-ring grooves or the like.

[0008] As described above, there has been no known effective method for repairing a seal ring groove, and in the case where the seal ring groove 12 is eroded, the actual situation is that the member itself in which the seal ring groove 12 is formed (cylinder 10 in the case of FIG. 2) is replaced, which requires a lot of cost. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] Republished Patent Publication WO2016 / 158146 Summary of the Invention [Problem to be solved by the invention]

[0010] Therefore, an object of the present invention is to solve the above-mentioned conventional problems and to provide a method for repairing a seal ring groove that can reliably and inexpensively repair a seal ring groove that has been eroded by corrosion without deforming the surrounding area. [Means for solving the problem]

[0011] The method of repairing a seal ring groove of the present invention, devised to solve the above-mentioned problems, is characterized by comprising the steps of: removing a seal ring from a seal ring groove whose groove bottom surface is corroded; inserting a thin shim plate with an obliquely cut end into the seal ring groove to cover the groove bottom surface; and fitting a seal ring into the seal ring groove with the shim plate inserted.

[0012] The thin shim plate is preferably made of a stainless steel plate having a thickness of 0.05 to 0.20 mm, and the angle of the notch at the end of the thin shim plate is preferably 30 to 60 degrees with respect to the longitudinal direction of the shim plate. After the shim plate is inserted into the seal ring groove, a caulking agent can be filled between the notches at the end of the shim plate. Effect of the Invention

[0013] According to the method for repairing a seal ring groove of the present invention, a seal ring groove eroded by corrosion can be repaired reliably and inexpensively without deforming the surrounding area. [Brief description of the drawings]

[0014] [Figure 1] FIG. 2 is a schematic diagram of a seal structure using a seal ring. [Diagram 2] 1 is a schematic diagram showing a state in which a dent is formed on the bottom surface of a seal ring groove. FIG. [Diagram 3] FIG. [Figure 4] FIG. 1 is a schematic diagram showing a shim plate being inserted into a seal ring groove having a recess. [Diagram 5] 1 is a schematic diagram showing a state in which a seal ring is fitted into a seal ring groove with a shim plate inserted therein; FIG. [Figure 6] FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] A preferred embodiment of the present invention will be described below. In this embodiment, the seal ring is an O-ring, and the seal ring groove is an O-ring groove. The following description will be based on the same schematic diagrams as those in Figs. 1 and 2, but it goes without saying that the present invention is not limited to these.

[0016] 2, if a dent occurs in the groove bottom surface 14 and the sealing ability of the seal ring 13 is reduced, first remove the seal ring 13 from the seal ring groove 12 to expose the groove bottom surface 14. If any foreign matter is attached to the groove bottom surface 14, it may cause erosion, so it is removed by cleaning.

[0017] Next, the shim plate 20 shown in FIG. 3 is prepared. The shim plate 20 is inserted into the seal ring groove 12. The shim plate 20 has a shape in which a part of a thin metal plate is cut out obliquely. The shim plate 20 needs to have enough rigidity to support the seal ring 13 inside the seal ring groove 12, so the thickness of the shim plate 20 cannot be made extremely thin. Conversely, if the thickness is made too thick, the seal ring 13 will be strongly pushed out from the inside of the seal ring groove 12. For this reason, the thickness of the shim plate 20 needs to be appropriately selected according to the size of the seal ring groove 12, and in many cases, it is preferable to set the thickness to 0.05 to 0.20 mm.

[0018] The material of the shim plate 20 is preferably an elastic metal, and is preferably stainless steel, which is resistant to corrosion. However, it does not necessarily have to be stainless steel, and a steel plate or an aluminum plate can be used depending on the place of use. The shim plate 20 can be formed into a ring shape in advance, as shown in FIG. 3.

[0019] The width of the shim plate 20 needs to be set so that it fits inside the seal ring groove 12. However, if the width of the shim plate 20 is too narrow, it will shift to one side in the width direction of the seal ring groove 12 and will not be able to properly support the seal ring 13. For this reason, it is preferable that the width of the shim plate 20 is about 70 to 95% of the groove width of the seal ring groove 12. It goes without saying that the longitudinal size of the shim plate 20 is determined in accordance with the length of the groove bottom surface 14.

[0020] Since the shim plate 20 is brought into close contact with the groove bottom surface 14 of the seal ring groove 12 to cover it, it is preferable that the shim plate 20 be elastic. To this end, both ends of the shim plate 20 are cut out at an angle, and a slit-shaped notch 21 is formed between the ends. The width of the notch 21 may be determined according to the size of the seal ring groove 12. However, if the width of the notch 21 is too narrow, it becomes difficult to insert the shim plate 20 into the seal ring groove 12, and if it is too wide, fluid may easily flow through the notch 21, reducing the sealing performance.

[0021] The angle of the notch 21 at the end is preferably 30 to 60 degrees with respect to the longitudinal direction of the shim plate 20, and is 45 degrees in this embodiment. The reason why the notch 21 is inclined in this manner is that if it is at a right angle (90 degrees) with respect to the longitudinal direction of the shim plate 20, fluid may easily flow through the notch 21, which may reduce sealing performance. If this angle is less than 30 degrees, it becomes difficult to insert the shim plate 20 into the seal ring groove 12.

[0022] When the shim plate 20 having the above structure is inserted into the seal ring groove 12 as shown in Fig. 4, the depression 15 on the bottom surface 14 of the groove is covered by the shim plate 20. Then, the seal ring 13 is fitted into the seal ring groove 12 with the shim plate 20 inserted as shown in Fig. 5. The amount of protrusion of the seal ring 13 from the seal ring groove 12 increases by the thickness of the shim plate 20, but since the rubber seal ring 13 has elasticity, a perfect seal can be ensured without any problems if the thickness of the shim plate 20 is set to about 0.05 to 0.20 mm. Fig. 6 shows the state after the repair is completed.

[0023] In the above embodiment, the notch 21 between the ends of the shim plate 20 is left open, but a more complete seal can be obtained by filling the notch 21 with a caulking agent after inserting the shim plate 20 into the seal ring groove 12. By adopting this method, the present invention can be applied not only to repairing the seal ring groove 12 for sealing between fixed members, but also to repairing the seal ring groove 12 for sealing between sliding members such as a hydraulic cylinder and a piston rod.

[0024] As explained above, the seal ring groove repair method of the present invention involves simply fitting the shim plate 20 into the seal ring groove 12, and does not require a heating process as in the case of welding build-up. Therefore, no thermal distortion occurs around the seal ring groove 12, and the present invention has the advantage of being able to reduce repair costs because it only uses the inexpensive shim plate 20. In the above embodiment, the seal ring groove 12 is an O-ring groove, but the method can be applied to other seal ring grooves as long as the groove bottom surface 14 is a flat surface. [Explanation of symbols]

[0025] 10 Cylinder 11 Axis 12 Seal ring groove 13 Seal ring 14 Groove bottom surface 15. Hollow 20 Shim plate 21 Notch

Claims

1. removing the seal ring from the seal ring groove whose groove bottom surface is corroded; a step of inserting a thin shim plate having an obliquely cut end into the seal ring groove to cover the bottom surface of the groove; and fitting a seal ring into the seal ring groove with the shim plate inserted therein.

2. 2. The method for repairing a seal ring groove according to claim 1, wherein the thin shim plate is made of a stainless steel plate having a thickness of 0.05 to 0.20 mm.

3. 3. The method for repairing a seal ring groove according to claim 1, wherein the angle of the notch at the end of the thin shim plate is 30 to 60 degrees with respect to the longitudinal direction of the shim plate.

4. 3. The method for repairing a seal ring groove according to claim 1, further comprising the step of filling a gap between the notches at the end of the shim plate with a caulking agent after inserting the shim plate into the seal ring groove.