Semiconductor device

By employing a silicon carbide semiconductor device with carefully controlled carrier concentrations and point defect densities in its layers, the expansion of basal plane dislocations into stacking faults is prevented, stabilizing device characteristics and reducing conduction loss.

JP2024135356AActive Publication Date: 2024-10-04KK TOSHIBA +1

Patent Information

Application Number
JP2023045991
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04
Estimated Expiration
2043-03-22

AI Technical Summary

Technical Problem

Semiconductor devices using silicon carbide substrates face challenges in maintaining stable characteristics due to the expansion of basal plane dislocations into stacking faults, which increase conduction loss and operating voltage.

Method used

The semiconductor device is structured with specific layers of silicon carbide, where the second semiconductor layer has a carrier concentration equal to or lower than the first layer and a higher point defect density, acting as recombination centers to prevent the expansion of basal plane dislocations into stacking faults, thereby stabilizing the device characteristics.

Benefits of technology

This structure effectively suppresses the expansion of stacking faults, reducing conduction loss and maintaining stable operating voltage, thus enhancing the performance and reliability of the semiconductor device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024135356000001_ABST
    Figure 2024135356000001_ABST
Patent Text Reader

Abstract

To provide a semiconductor device having stable characteristics.SOLUTION: One embodiment provides a semiconductor device containing silicon carbide. The semiconductor device includes a semiconductor substrate, a first semiconductor layer, a second semiconductor layer, a third semiconductor layer, and a fourth semiconductor layer. The first to third semiconductor layers are of a first conductivity type, and the fourth semiconductor layer is of a second conductivity type. A carrier concentration of the second semiconductor layer is the same as or lower than a carrier concentration of the first semiconductor layer. The carrier concentration of the second semiconductor layer is the same as or higher than a carrier concentration of the third semiconductor layer. A point defect density in the second semiconductor layer is the same as or higher than a point defect density of the first semiconductor layer, and is higher than a point defect density of the third semiconductor layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD An embodiment of the present invention relates to a semiconductor device. [Background technology]

[0002] For example, there is a semiconductor device using a substrate containing silicon carbide (SiC). It is desirable for the semiconductor device to have stable characteristics. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2022-38594 A Summary of the Invention [Problem to be solved by the invention]

[0004] An object of the embodiments of the present invention is to provide a semiconductor device having stable characteristics. [Means for solving the problem]

[0005] The semiconductor device according to the embodiment includes a semiconductor substrate of a first conductivity type having a first surface and a second surface located opposite to the first surface and containing silicon carbide, a first semiconductor layer of the first conductivity type provided on the first surface and containing silicon carbide, a second semiconductor layer of the first conductivity type provided on the first semiconductor layer and containing silicon carbide, a third semiconductor layer of the first conductivity type provided on the second semiconductor layer and containing silicon carbide, and a fourth semiconductor layer of the second conductivity type provided on the third semiconductor layer and containing silicon carbide. The carrier concentration of the first conductivity type of the second semiconductor layer is the same as or lower than the carrier concentration of the first conductivity type of the first semiconductor layer. The carrier concentration of the first conductivity type of the second semiconductor layer is the same as or higher than the carrier concentration of the first conductivity type of the third semiconductor layer. The point defect density of the second semiconductor layer is the same as or higher than the point defect density of the first semiconductor layer and is higher than the point defect density of the third semiconductor layer. [Brief description of the drawings]

[0006] [Figure 1] 1 is a schematic cross-sectional view illustrating a semiconductor device according to a first embodiment. [Diagram 2] 2A to 2C are schematic cross-sectional views illustrating a part of a method for manufacturing the semiconductor device according to the first embodiment. [Diagram 3] 2A to 2C are schematic cross-sectional views illustrating a part of a method for manufacturing the semiconductor device according to the first embodiment. [Figure 4] 2A to 2C are schematic cross-sectional views illustrating a part of a method for manufacturing the semiconductor device according to the first embodiment. [Diagram 5] 5A to 5C are schematic cross-sectional views illustrating a part of a modified example of the method for manufacturing the semiconductor device according to the first embodiment. [Figure 6] 5A to 5C are schematic cross-sectional views illustrating a part of a modified example of the method for manufacturing the semiconductor device according to the first embodiment. [Figure 7] 10A to 10C are schematic cross-sectional views illustrating a part of another modified example of the method for manufacturing the semiconductor device according to the first embodiment. [Figure 8] 10A to 10C are schematic cross-sectional views illustrating a part of another modified example of the method for manufacturing the semiconductor device according to the first embodiment. [Figure 9] 3 is a schematic cross-sectional view for explaining the operation of the semiconductor device according to the first embodiment. FIG. [Figure 10] 11 is a schematic cross-sectional view for explaining the operation of a semiconductor device of a comparative example. FIG. [Figure 11] 1A to 1C are schematic cross-sectional views illustrating semiconductor devices according to modified examples of the first embodiment. [Figure 12] 5A to 5C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to a modified example of the first embodiment. [Figure 13] 5A to 5C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to a modified example of the first embodiment. [Figure 14] 10A to 10C are schematic cross-sectional views illustrating a part of a modified example of the manufacturing method of the semiconductor device according to the modified example of the first embodiment. [Figure 15]10A to 10C are schematic cross-sectional views illustrating a part of a modified example of the manufacturing method of the semiconductor device according to the modified example of the first embodiment. [Figure 16] 10A to 10C are schematic cross-sectional views illustrating semiconductor devices according to other modified examples of the first embodiment. [Figure 17] 10A to 10C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to another modified example of the first embodiment. [Figure 18] 10A to 10C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to another modified example of the first embodiment. [Figure 19] 10A to 10C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to another modified example of the first embodiment. [Figure 20] 10 is a schematic cross-sectional view illustrating a semiconductor device according to a second embodiment. FIG. [Figure 21] 21 is a schematic cross-sectional view taken along line BB in FIG. 20. [Figure 22] FIG. 21 is a schematic enlarged view of part C in FIG. 20. [Figure 23] 5A to 5C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to a second embodiment. [Figure 24] 5A to 5C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to a second embodiment. [Diagram 25] 6A to 6C are schematic cross-sectional views illustrating the operation of the semiconductor device according to the second embodiment. [Figure 26] FIG. 26 is a schematic cross-sectional view taken along line DD in FIG. 25. [Figure 27] 11A and 11B are schematic cross-sectional views illustrating the operation of a semiconductor device according to a comparative example. [Figure 28] 28 is a schematic cross-sectional view taken along line EE in FIG. 27. [Figure 29] 13 is a schematic cross-sectional view illustrating a semiconductor device according to a modified example of the second embodiment. FIG. [Diagram 30] FIG. 30 is a schematic enlarged view of part F in FIG. 29. [Diagram 31] 10A to 10C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to a modified example of the second embodiment. [Diagram 32] 10A to 10C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to a modified example of the second embodiment. [Diagram 33] 13 is a schematic cross-sectional view illustrating a semiconductor device according to another modified example of the second embodiment. FIG. [Diagram 34] FIG. 34 is a schematic enlarged view of part G in FIG. 33. [Diagram 35] 10A to 10C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to another modified example of the second embodiment. [Diagram 36] 10A to 10C are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to another modified example of the second embodiment. [Figure 37] 11 is a schematic cross-sectional view illustrating a semiconductor device according to a third embodiment. FIG. [Figure 38] 38 is a schematic cross-sectional view taken along line HH in FIG. 37. [Figure 39] 13A to 13C are schematic cross-sectional views for explaining the operation of the semiconductor device according to the third embodiment. [Diagram 40] 40 is a schematic cross-sectional view taken along line II in FIG. 39. [Diagram 41] 11 is a schematic cross-sectional view for explaining an operation of a semiconductor device according to a comparative example. FIG. [Diagram 42] 42 is a schematic cross-sectional view taken along line JJ in FIG. 41. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Hereinafter, embodiments of the present invention will be described with reference to the drawings. The drawings are schematic or conceptual, and the relationship between the thickness and width of each part, the size ratio between parts, etc. are not necessarily the same as those in reality. Even when the same part is shown, the dimensions and ratios of each part may be different depending on the drawing. In this specification and each drawing, elements similar to those already explained are given the same reference numerals and detailed explanations are omitted as appropriate. In the following description and drawings, n + , n- , p + When the symbols are written as "+" and "p", they represent the relative levels of each impurity concentration. In other words, a symbol with "+" indicates a relatively higher impurity concentration than a symbol with neither "+" nor "-" attached, and a symbol with "-" indicates a relatively lower impurity concentration than a symbol with neither attached. When both p-type and n-type impurities are included in each region, these symbols represent the relative levels of the net impurity concentration after the impurities compensate for each other. The carrier concentration shall be regarded as the effective impurity concentration. In each embodiment described below, the p-type and n-type of each semiconductor region may be reversed to implement each embodiment.

[0008] (First embodiment) FIG. 1 is a schematic cross-sectional view illustrating the semiconductor device according to the first embodiment. 1, the semiconductor device 1 according to this embodiment includes a semiconductor substrate 10, a first semiconductor layer 20, a second semiconductor layer 30, and a third semiconductor layer 40. The semiconductor device 1 further includes a fourth semiconductor layer 50, a first electrode 62, and a second electrode 64.

[0009] The first semiconductor layer 20 is provided on a semiconductor substrate 10. The second semiconductor layer 30 is provided on the first semiconductor layer 20. The third semiconductor layer 40 is provided on the second semiconductor layer 30. The fourth semiconductor layer 50 is provided on the third semiconductor layer 40. The first electrode 62 is provided on the surface of the semiconductor substrate 10 opposite to the surface on which the first semiconductor layer 20 is arranged. The second electrode 64 is provided on the surface of the fourth semiconductor layer 50 opposite to the surface on which the third semiconductor layer 40 is arranged.

[0010] The semiconductor substrate 10, the first semiconductor layer 20, the second semiconductor layer 30, the third semiconductor layer 40 and the fourth semiconductor layer 50 contain silicon carbide (SiC).

[0011] The semiconductor substrate 10, the first semiconductor layer 20, the second semiconductor layer 30 and the third semiconductor layer 40 are of a first conductivity type. The fourth semiconductor layer 50 is of a second conductivity type. For example, the first conductivity type is n-type and the second conductivity type is p-type.

[0012] The impurity concentration of the first semiconductor layer 20 is higher than the impurity concentration of the third semiconductor layer 40. The impurity concentration of the second semiconductor layer 30 is the same as or higher than the impurity concentration of the third semiconductor layer 40. The impurity concentration of the second semiconductor layer 30 is the same as or lower than the impurity concentration of the first semiconductor layer 20. The semiconductor device 1 is, for example, a PiN diode.

[0013] The semiconductor substrate 10 has a first surface 11a and a second surface 11b. The second surface 11b is the surface opposite to the first surface 11a. A first semiconductor layer 20 is provided on the first surface 11a, and a first electrode 62 is provided on the second surface 11b. The semiconductor substrate 10 is, for example, a SiC bulk single crystal substrate.

[0014] In the following, a three-dimensional orthogonal coordinate system of XYZ may be used for explanation. The XY plane is a plane parallel to the first surface 11a or the second surface 11b. The Z axis is perpendicular to the XY plane. As described in relation to FIG. 9, the X axis is inclined with respect to the [11-20] axis perpendicular to the {11-20} surface of the semiconductor substrate 10. The [11-20] axis is inclined by an off angle θoff with respect to the X axis. The angle is defined as positive in the counterclockwise direction with respect to the reference axis. The Y axis is parallel to the [1-100] axis perpendicular to the {1-100} surface of the semiconductor substrate 10. The Z axis is inclined with respect to the

[0001] axis perpendicular to the {0001} surface of the semiconductor substrate 10. The

[0001] axis is inclined with respect to the Z axis by an off angle θoff. In other words, the {0001} surface is inclined with respect to the XY plane by an off angle θoff around the Y axis or the [1-100] axis. As shown in Fig. 9, the coordinate axes for the crystal axes may be shown together with the XYZ coordinate axes. In this case, the [1-100] axis that overlaps with the Y axis is shown below the Y axis. The same applies to Figs. 10, 20, 25, 27, 39 and 41. As mentioned above, the [1-100] axis is parallel to the Y axis, and the positive and negative directions are opposite.

[0015] The first semiconductor layer 20 contains, for example, SiC and nitrogen (N) as an impurity. For example, phosphorus (P) may be contained instead of N, or both N and P may be contained. For example, the impurity concentration of N in the first semiconductor layer 20 is 10 -19 [cm -3 ] is lower. By appropriately setting the impurity concentration, the first semiconductor layer 20 forms point defects that become recombination centers, shortens the recombination time of minority carriers injected from the fourth semiconductor layer 50, and suppresses the intrusion of minority carriers, thereby suppressing the amount of recombination energy generated. In addition, the first semiconductor layer 20 converts basal plane dislocations (BPDs) generated in the semiconductor substrate 10 into threading edge dislocations (TEDs). By converting BPDs into TEDs, the first semiconductor layer 20 suppresses the expansion of BPDs into single Shockley stacking faults (1SSFs).

[0016] The second semiconductor layer 30 includes a first element as an impurity. The first element includes at least one selected from the group consisting of N, P, aluminum (Al), and boron (B). The second semiconductor layer 30 may include a second element instead of the first element. The second element includes at least one selected from the group consisting of iron (Fe), nickel (Ni), chromium (Cr), magnesium (Mg), zinc (Zn), copper (Cu), calcium (Ca), vanadium (V), gold (Au), and platinum (Pt). The second semiconductor layer 30 may include the second element together with the first element.

[0017] The first semiconductor layer 20 and the second semiconductor layer 30 have a point defect density higher than the point defect density of the semiconductor substrate 10 and the third semiconductor layer 40. The second semiconductor layer 30 has a point defect density equal to or higher than the point defect density of the first semiconductor layer 20.

[0018] The second semiconductor layer 30 has a point defect density higher than the point defect densities of the semiconductor substrate 10, the first semiconductor layer 20, and the third semiconductor layer 40, thereby promoting the recombination of minority carriers injected from the fourth semiconductor layer 50, shortening the lifetime of the minority carriers, and suppressing the generation of recombination energy due to the recombination of minority carriers. The second semiconductor layer 30 prevents the BPD from expanding to 1SSF by suppressing the generation of recombination energy.

[0019] When the semiconductor device 1 operates in the forward direction as a diode, majority carriers of the first conductivity type flow through the third semiconductor layer 40 to pass a forward current. When the semiconductor device 1 operates in the reverse blocking direction as a diode, the third semiconductor layer 40 forms a depletion layer and realizes a desired withstand voltage between the second electrode 64, which is an anode electrode, and the first electrode 62, which is a cathode electrode.

[0020] The fourth semiconductor layer 50 is joined to the third semiconductor layer 40 to realize a pn junction. When the semiconductor device 1 operates as a diode in the forward direction, majority carriers of the second conductivity type run through the fourth semiconductor layer 50 to pass a forward current. When the semiconductor device 1 operates as a diode in the reverse blocking direction, the fourth semiconductor layer 50, together with the third semiconductor layer 40, realizes a desired withstand voltage between the second electrode 64, which is an anode electrode, and the first electrode 62, which is a cathode electrode.

[0021] The first electrode 62 is ohmic-connected to the semiconductor substrate 10 and functions as one of the main electrodes of the semiconductor device 1. The second electrode 64 is ohmic-connected to the fourth semiconductor layer 50 and functions as the other main electrode of the semiconductor device 1. When the semiconductor device 1 is a diode, the first electrode 62 is a cathode electrode and the second electrode 64 is an anode electrode.

[0022] A method for manufacturing the semiconductor device 1 according to this embodiment will be described. 2 to 4 are schematic cross-sectional views illustrating a part of the method for manufacturing the semiconductor device according to the first embodiment. 2 to 4 show a cross section of a portion corresponding to part A in Fig. 1. In this embodiment, when a cross section of a semiconductor device is shown in other drawings, it is assumed that the cross section corresponds to part A in Fig. 1 unless otherwise specified. 2, a first semiconductor layer 20 is formed on a prepared semiconductor substrate 10. The first semiconductor layer 20 is formed by epitaxial growth.

[0023] As shown in FIG. 3, the second semiconductor layer 30 is formed on the first semiconductor layer 20. The second semiconductor layer 30 is formed by epitaxial growth. When the second semiconductor layer 30 is epitaxially grown, a first element (N, P, Al, B) is doped to form a recombination center for Auger recombination. After the second semiconductor layer 30 is formed by epitaxial growth, a second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt) may be introduced into the second semiconductor layer 30 by thermal diffusion. When the second element is introduced instead of the first element, the second element is preferable because it forms point defects that become recombination centers without increasing the impurity concentration of the second semiconductor layer 30.

[0024] 4, the third semiconductor layer 40 is formed on the second semiconductor layer 30. The third semiconductor layer 40 is formed by epitaxial growth.

[0025] Thereafter, the fourth semiconductor layer 50 is formed on the third semiconductor layer 40, and the first electrode 62 and the second electrode 64 are formed, thereby completing the semiconductor device 1.

[0026] 5 and 6 are schematic cross-sectional views illustrating a part of a modified example of the method for manufacturing the semiconductor device according to the first embodiment. 5, as described in relation to FIG. 2, a first semiconductor layer 20 is formed on a prepared semiconductor substrate 10, and an intermediate semiconductor layer 140 is formed on the first semiconductor layer 20 by epitaxial growth. For example, the impurity concentration of the intermediate semiconductor layer 140 is the same as that of the third semiconductor layer 40 shown in FIG. 1. That is, the impurity concentration of the intermediate semiconductor layer 140 is lower than that of the first semiconductor layer 20. For example, the intermediate semiconductor layer 140 is formed under the same conditions as those for forming the third semiconductor layer 40.

[0027] As shown in FIG. 6, the second semiconductor layer 30 is formed on the first semiconductor layer 20. The second semiconductor layer 30 is formed by ion implanting a third element into the intermediate semiconductor layer 140 shown in FIG. 5. The third element includes at least one selected from the group consisting of hydrogen (H), helium (He), argon (Ar), neon (Ne) and xenon (Xe). H introduced into the intermediate semiconductor layer 140 by ion implantation is introduced as a proton. The ion implantation energy is set according to the thickness of the intermediate semiconductor layer 140. The third element is desorbed by a subsequent normal thermal process. Therefore, by ion implanting the third element into the intermediate semiconductor layer 140, the second semiconductor layer 30 having a high density of point defects can be formed without increasing the impurity density.

[0028] The second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt) may be used instead of the third element for ion implantation into the intermediate semiconductor layer 140. These elements form deep levels in the forbidden band of the intermediate semiconductor layer 140 and function as recombination centers, making it possible to form the second semiconductor layer 30 having a high density of point defects without increasing the impurity density.

[0029] 7 and 8 are schematic cross-sectional views illustrating a part of another modified example of the manufacturing method of the semiconductor device according to the first embodiment. 7, an intermediate semiconductor layer 120 is formed by epitaxial growth on a prepared semiconductor substrate 10. In this case, the intermediate semiconductor layer 120 is formed to be thicker than the first semiconductor layer 20 described in relation to Fig. 2. The intermediate semiconductor layer 120 has a thickness obtained by adding the thickness of the second semiconductor layer 30 to the thickness of the first semiconductor layer 20.

[0030] As shown in FIG. 8, the second semiconductor layer 30 is formed by ion implanting a third element into the intermediate semiconductor layer 120. By adjusting the ion implantation energy, the second semiconductor layer 30 can be formed on the first semiconductor layer 20. The ion implantation into the second semiconductor layer 30 may be performed with the second element instead of the third element. In either case, the second semiconductor layer 30 having a point defect density higher than the point defect density of the first semiconductor layer 20 can be formed without increasing the impurity density of the second semiconductor layer 30 higher than the impurity density of the first semiconductor layer 20.

[0031] The operation and effects of the semiconductor device 1 according to this embodiment will be described. FIG. 9 is a schematic cross-sectional view for explaining the operation of the semiconductor device according to the first embodiment. FIG. 9 shows the crystal axes of SiC along with the XYZ coordinate system. The [11-20] axis is inclined in the positive direction by an off angle θoff with respect to the X axis, centered on the Y axis and the [1-100] axis. The

[0001] axis is inclined by an off angle θoff with respect to the Z axis, centered on the Y axis and the [1-100] axis. That is, the {0001} plane of SiC forming the semiconductor substrate 10, the first semiconductor layer 20, the second semiconductor layer 30, and the third semiconductor layer 40 is inclined by an off angle θoff with respect to the XY plane, centered on the Y axis and the [1-100] axis. The off angle θoff is, for example, about 4°.

[0032] 9, holes h+, which are minority carriers injected from the fourth semiconductor layer 50 shown in FIG. 1, are injected into the second semiconductor layer 30 through the third semiconductor layer 40. In the second semiconductor layer 30, point defects formed at high density function as minority carrier recombination centers, recombining holes h+ and electrons e- in a short lifetime and causing them to disappear. Therefore, in the second semiconductor layer 30, the BPD that obtains the recombination energy of the minority carriers is prevented from expanding to 1SSF.

[0033] For example, dislocation B1, which is a BPD in the semiconductor substrate 10, may be formed along the {0001} plane of SiC. That is, dislocation B1 is formed at an inclination of an off angle θoff with respect to the XY plane. When dislocation B1 reaches the first semiconductor layer 20, it is converted into dislocation T1, which is a TED, in the first semiconductor layer 20.

[0034] Dislocations T1 are formed along the

[0001] axis direction. Holes h+ traveling in the third semiconductor layer 40 travel almost along the Z axis direction. Since the Z axis and the

[0001] axis have an off angle θoff of about 4°, dislocations T1 do not impede the travel of holes h+. Therefore, the conversion of dislocations B1 to dislocations T1 in the first semiconductor layer 20 does not increase the resistance of the semiconductor device 1 during conduction.

[0035] The minority carriers that have passed through the third semiconductor layer 40 are quickly recombined at the recombination centers of the second semiconductor layer 30, and therefore hardly supply recombination energy to the dislocations B1 formed in the semiconductor substrate 10. Even if a very small portion of the minority carriers pass through the second semiconductor layer 30, they are quickly recombined at the recombination centers of the first semiconductor layer 20, and therefore the dislocations B1 are prevented from expanding to 1SSF.

[0036] FIG. 10 is a schematic cross-sectional view illustrating a semiconductor device according to a comparative example. In the semiconductor device according to the comparative example in FIG. 10, the second semiconductor layer 30 shown in FIG. 9 is not provided on the first semiconductor layer 20, and a third semiconductor layer 40 is provided directly on the first semiconductor layer 20.

[0037] 10, in the semiconductor device of the comparative example, dislocations B1 that are not converted to dislocations T1 in the second semiconductor layer 30 obtain recombination energy between holes h+ and electrons e-, and are expanded into defects S1, which are 1SSF. As long as the recombination energy is supplied, the defects S1 are expanded in the third semiconductor layer 40 along the [11-20] axis toward the positive direction of the Z axis. Since the defects S1 impede the travel of carriers, the forward voltage for the forward current of the semiconductor device 1 increases, which may lead to increased losses.

[0038] Conventionally, the phenomenon that BPD expands to 1SSF by obtaining recombination energy due to recombination of holes and electrons is known. In order to promote the recombination of holes and electrons and to prevent the expansion from BPD to 1SSF, a recombination-promoting buffer layer into which high concentration nitrogen is introduced is provided (for example, Patent Document 1, etc.). In this technology, the concentration of nitrogen introduced into the recombination-promoting buffer layer is increased, thereby improving the point defect density and promoting the recombination of holes and electrons. On the other hand, when the nitrogen concentration is increased to 10 -19 [cm -3 It is known that introduction of more than 1000 .mu.m of dopant in the recombination-promoting buffer layer adversely affects the quality of the epitaxial crystal of the low-concentration drift layer adjacent to the recombination-promoting buffer layer.

[0039] The semiconductor device 1 according to this embodiment includes a second semiconductor layer 30 having an impurity concentration lower than the impurity concentration of a first semiconductor layer 20 corresponding to a recombination-promoting buffer layer and having a point defect density higher than the point defect density of the first semiconductor layer 20. A third semiconductor layer 40 corresponding to a low-concentration drift layer is connected to the first semiconductor layer 20 and the semiconductor substrate 10 via the second semiconductor layer 30.

[0040] The second semiconductor layer 30 has an impurity concentration equal to or lower than that of the first semiconductor layer 20, and a point defect density equal to or higher than that of the first semiconductor layer 20. Therefore, the low impurity concentration suppresses the influence on the crystal quality of the third semiconductor layer 40, while the high point defect density promotes the recombination of holes and electrons, preventing the recombination energy from reaching the BPD. Therefore, by providing the second semiconductor layer 30, it is possible to suppress the expansion of the BPD to the 1SSF. Even if the BPD expands to the 1SSF, the second semiconductor layer 30 is located between the third semiconductor layer 40 and the first semiconductor layer 20, and does not supply recombination energy to the 1SSF expanded from the BPD in the first semiconductor layer 20. Therefore, it is possible to prevent the 1SSF from expanding further upward beyond the second semiconductor layer 20.

[0041] Point defects in the second semiconductor layer 30 are formed by introducing a first element (N, P, Al, B) into the second semiconductor layer 30, as well as a second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt). The second element functions as a recombination center but does not function as an impurity. Therefore, the second semiconductor layer 30 can achieve a point defect density higher than that of the first semiconductor layer 20 at an impurity concentration lower than that of the first semiconductor layer 20.

[0042] In addition to the above, point defects can also be formed in the second semiconductor layer 30 by introducing a third element (H, He, Ar, Ne, Xe). After being introduced into the second semiconductor layer 30, the third element itself disappears by going through a normal heating process of the semiconductor device 1. Therefore, while the third element forms point defects, it does not function as an impurity, and therefore the second semiconductor layer 30 can achieve a high point defect density with a low impurity concentration.

[0043] (Variation 1) FIG. 11 is a schematic cross-sectional view illustrating a semiconductor device 1a according to a modification of the first embodiment. As shown in Fig. 11, the semiconductor device 1a differs from the semiconductor device 1 shown in Fig. 1 in that it further includes a fifth semiconductor layer 42. In other respects, the semiconductor device 1a is the same as the semiconductor device 1, and the same components are denoted by the same reference numerals and detailed description thereof will be omitted.

[0044] The fifth semiconductor layer 42 is provided between the first semiconductor layer 20 and the second semiconductor layer 30. The impurity concentration of the first conductivity type of the fifth semiconductor layer 42 is approximately the same as the impurity concentration of the third semiconductor layer 40. The point defect density of the fifth semiconductor layer 42 is approximately the same as the point defect density of the third semiconductor layer 40. In other words, the impurity concentration of the second semiconductor layer 30 is approximately the same as or higher than the impurity concentration of the fifth semiconductor layer 42. The point defect density of the second semiconductor layer 30 is higher than the point defect density of the fifth semiconductor layer 42. The point defect density of the second semiconductor layer 30 is preferably the same as or higher than the point defect density of the first semiconductor layer 20.

[0045] 12 and 13 are schematic cross-sectional views illustrating a part of a manufacturing method for a semiconductor device according to a modification of the first embodiment. 2, the first semiconductor layer 20 is formed by epitaxial growth on the prepared semiconductor substrate 10. As shown in FIG. 12, the fifth semiconductor layer 42 is formed by epitaxial growth on the first semiconductor layer 20. For example, the fifth semiconductor layer 42 is formed so as to have an impurity concentration substantially equal to that of the third semiconductor layer 40. For example, the fifth semiconductor layer 42 is formed under the same conditions as those of the third semiconductor layer 40.

[0046] As shown in Fig. 13, the second semiconductor layer 30 is formed on the fifth semiconductor layer 42. The second semiconductor layer 30 is formed by epitaxial growth. As described in relation to Fig. 3, the second semiconductor layer 30 is formed by doping with a first element (N, P, Al, B). Furthermore, the second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt) may be thermally diffused to form point defects as recombination centers.

[0047] Thereafter, the third semiconductor layer 40, the fourth semiconductor layer 50 and the first electrode 62 are formed on the second semiconductor layer 30, and the second electrode 64 is formed on the semiconductor substrate 10, thereby completing the semiconductor device 1a.

[0048] 14 and 15 are schematic cross-sectional views illustrating a part of a modified example of the manufacturing method for a semiconductor device according to the modified example of the first embodiment. 14, the intermediate semiconductor layer 42a is formed by epitaxial growth on the first semiconductor layer 20. For example, the intermediate semiconductor layer 42a is formed under the same conditions as those for the third semiconductor layer 40. The intermediate semiconductor layer 42a to be formed has a thickness obtained by adding the thickness of the fifth semiconductor layer 42 and the thickness of the second semiconductor layer 30 together.

[0049] As shown in Fig. 15, the second semiconductor layer 30 is formed by ion implantation into the intermediate semiconductor layer 42a shown in Fig. 14. As described in relation to Fig. 6, the second semiconductor layer 30 is formed by implanting a third element (H, He, Ar, Ne, Xe) into the intermediate semiconductor layer 42a. The introduction of the third element forms point defects as recombination centers in the second semiconductor layer 30. Instead of the third element, the second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt) may be ion implanted.

[0050] Thereafter, the third semiconductor layer 40, the fourth semiconductor layer 50 and the first electrode 62 are formed on the second semiconductor layer 30, and the second electrode 64 is formed on the semiconductor substrate 10, thereby completing the semiconductor device 1a.

[0051] (Variation 2) FIG. 16 is a schematic cross-sectional view illustrating a semiconductor device according to another modification of the first embodiment. As shown in FIG. As shown in Fig. 16, the semiconductor device 1b according to this modification includes a second semiconductor layer 130 instead of the second semiconductor layer 30 shown in Fig. 1. Other components of the semiconductor device 1b are the same as those of the semiconductor device 1, and the same components are denoted by the same reference numerals and detailed description thereof will be omitted.

[0052] The second semiconductor layer 130 is provided on the first semiconductor layer 20. A third semiconductor layer 40 is provided on the second semiconductor layer 130. The second semiconductor layer 130 includes a first layer 32 and a second layer 34. The first layer 32 is provided on the first semiconductor layer 20. The second layer 34 is provided on the first layer 32. The third semiconductor layer 40 is provided on the second layer 34.

[0053] The first layer 32 and the second layer 34 are both of the first conductivity type. The impurity concentration of the first layer 32 is the same as or higher than the impurity concentration of the second layer 34. The impurity concentration of the first layer 32 is the same as or higher than the impurity concentration of the first semiconductor layer 20. The impurity concentration of the second layer 34 is the same as or higher than the impurity concentration of the third semiconductor layer 40. The impurity concentration of the second layer 34 is the same as or lower than the impurity concentration of the first semiconductor layer 20.

[0054] The point defect density of the first layer 32 and the point defect density of the second layer 34 are approximately the same, and are equal to or higher than the point defect density of the first semiconductor layer 20 .

[0055] A method for manufacturing the semiconductor device 1b according to this modification will be described. 17 to 19 are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to another modification of the first embodiment. 17, a first intermediate semiconductor layer 20a is formed on a prepared semiconductor substrate 10. The first intermediate semiconductor layer 20a is formed to have a thickness obtained by adding the thickness of the first layer 32 of the second semiconductor layer 30 to the thickness of the first semiconductor layer 20.

[0056] As shown in FIG. 18, a second intermediate semiconductor layer 44 is formed on the first intermediate semiconductor layer 20a by epitaxial growth.

[0057] 19, a third element (proton, He, Ar, Ne, Xe) is introduced by ion implantation into the first intermediate semiconductor layer 20a and the second intermediate semiconductor layer 44. The energy during the ion implantation is set so as to correspond to the thickness of the second semiconductor layer 30 out of the thicknesses of the first intermediate semiconductor layer 20a and the second intermediate semiconductor layer 44.

[0058] Thereafter, the third semiconductor layer 40, the fourth semiconductor layer 50 and the first electrode 62 are formed on the second semiconductor layer 30, and the second electrode 64 is formed on the semiconductor substrate 10, thereby completing the semiconductor device 1a.

[0059] In this manner, the semiconductor devices 1a and 1b according to the modified examples are formed. The semiconductor devices 1a and 1b according to the modified examples have the same effects as the semiconductor device 1 shown in FIG.

[0060] Second Embodiment FIG. 20 is a schematic cross-sectional view illustrating the semiconductor device according to the second embodiment. As shown in FIG. FIG. 21 is a schematic cross-sectional view taken along line BB in FIG. 20 and 21, a semiconductor device 201 according to this embodiment includes a semiconductor substrate 10, a first semiconductor layer 20, a plurality of first semiconductor regions 230, and a sixth semiconductor layer 240. The semiconductor device 201 is different from the semiconductor device 1 shown in FIG. 1 in that the plurality of first semiconductor regions 230 and the sixth semiconductor layer 240 are included, but is otherwise the same as the semiconductor device 1. The same components are denoted by the same reference numerals, and detailed descriptions thereof will be omitted as appropriate.

[0061] The multiple first semiconductor regions 230 are provided on the first semiconductor layer 20. The multiple first semiconductor regions 230 each extend in the Y-axis direction on the first semiconductor layer 20. The multiple first semiconductor regions 230 are arranged spaced apart in the X-axis direction. In this example, the multiple first semiconductor regions 230 are arranged at approximately equal intervals in the X-axis direction.

[0062] As described in relation to FIG. 1, the XY plane is parallel to the first surface 11a or the second surface 11b of the semiconductor substrate 10, and the [11-20] axis of the semiconductor substrate 10 is inclined by an off angle θoff with respect to the X axis around the Y axis. The

[0001] axis of the semiconductor substrate 10 is inclined by an off angle θoff with respect to the Z axis around the Y axis. The Y axis is parallel to the [1-100] axis perpendicular to the {1-100} plane of the semiconductor substrate 10. That is, the multiple first semiconductor regions 230 each extend along the [1-100] axis of the semiconductor substrate 10. Each of the multiple first semiconductor regions 230 is disposed at approximately equal intervals with respect to the [11-20] axis of the semiconductor substrate 10.

[0063] The sixth semiconductor layer 240 is provided on the first semiconductor layer 20. The sixth semiconductor layer 240 is also provided between two adjacent first semiconductor regions 230 of the multiple first semiconductor regions 230. The sixth semiconductor layer 240 is also provided on each of the multiple first semiconductor regions 230.

[0064] The semiconductor substrate 10, the first semiconductor layer 20, the plurality of first semiconductor regions 230, and the sixth semiconductor layer 240 contain impurities of a first conductivity type. The first conductivity type is, for example, n-type.

[0065] The first semiconductor region 230 includes SiC and a first element as an impurity, similar to the second semiconductor layer 30 of the semiconductor device 1 shown in FIG. 1. The first element includes at least one selected from the group consisting of N, P, Al, and B. Similarly to the semiconductor device 1, the first semiconductor region 230 may include a second element instead of the first element or together with the first element. The second element includes at least one selected from the group consisting of Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, and Pt.

[0066] The impurity concentration of the multiple first semiconductor regions 230 is the same as or lower than the impurity concentration of the first semiconductor layer 20. The impurity concentration of the multiple first semiconductor regions 230 is the same as or higher than the impurity concentration of the sixth semiconductor layer 240.

[0067] The point defect density of the multiple first semiconductor regions 230 is the same as or higher than the point defect density of the first semiconductor layer 20. The point defect density of the multiple first semiconductor regions 230 and the point defect density of the first semiconductor layer 20 are higher than both the point defect density of the semiconductor substrate 10 and the point defect density of the sixth semiconductor layer 240.

[0068] FIG. 22 is a schematic enlarged view of part C in FIG. FIG. 22 shows the relationship between the distances W1, W2 and the thickness h1. Distance W1 represents the distance in the X-axis direction between two adjacent first semiconductor regions 230 among the multiple first semiconductor regions 230. Distance W1 represents the width of each of the multiple first semiconductor regions 230. Thickness h1 represents the thickness of each of the multiple first semiconductor regions 230.

[0069] In FIG. 22, the distance W1 is the distance between the bottom ends 230B or the top ends 230T of two adjacent first semiconductor regions 230.

[0070] From the viewpoint of preventing the expansion of the BPD to 1SSF, it is preferable that W1 is small and W2 is large. The semiconductor device 1 described in relation to FIG. 1 is an example in which W1=0. The first semiconductor region 230 has a recombination center due to a point defect, which promotes the recombination of holes and electrons. On the other hand, the first semiconductor region 230 is disposed in the current path, and the resistance value becomes high depending on the impurity concentration of the first semiconductor region 230, so it is preferable to make W2 small.

[0071] The 1SSF expands along the {0001} plane of SiC that is tilted from the XY plane at the off angle θoff. Therefore, from the viewpoint of suppressing the expansion of the 1SSF in the first semiconductor region 230, it is preferable that the relationship between W1, W2, and h1 is set based on the off angle θoff.

[0072] The relationship between W1 and h1 can be expressed using the angle θ1. W1 can be expressed by the following formula (1).

[0073] W1=h / tan(θ1) (1)

[0074] The relationship between θ1 and the off angle θoff in formula (1) is set, for example, by the following formula (2).

[0075] 2θoff≧θ1≧0.5θoff (2)

[0076] In the formula (2), the coefficient of θoff is appropriately set depending on the manufacturing variation when the first semiconductor region 230 is formed.

[0077] A method for manufacturing the semiconductor device 201 according to this embodiment will be described. 23 and 24 are schematic cross-sectional views illustrating a part of the manufacturing method of the semiconductor device according to the second embodiment. As shown in FIG. 2, the first semiconductor layer 20 is formed by epitaxial growth on the prepared semiconductor substrate 10. As shown in FIG. 23, the intermediate semiconductor layer 240a is formed on the first semiconductor layer 20. The intermediate semiconductor layer 240a is formed under the same conditions as the sixth semiconductor layer 240 shown in FIG. 20, for example. After the intermediate semiconductor layer 240a is formed, a mask M1 is formed on the intermediate semiconductor layer 240a. In the mask M1, an opening AP is provided at a position where the first semiconductor region 230 is to be formed. Through the mask M1, a second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt) or a third element (H, He, Ar, Ne, Xe) is introduced into the intermediate semiconductor layer 240a by ion implantation.

[0078] 24, the mask M1 is removed. The intermediate semiconductor layer 240b is formed in the area where the mask M1 was provided, and the first semiconductor region 230 is formed in the area where the opening AP of the mask M1 was provided.

[0079] Thereafter, a semiconductor layer is further formed by epitaxial growth on the first semiconductor region 230 and the intermediate semiconductor layer 240a, to form the sixth semiconductor layer 240 shown in FIG.

[0080] The operation and effects of the semiconductor device 201 according to this embodiment will be described. FIG. 25 is a schematic cross-sectional view illustrating the operation of the semiconductor device according to the second embodiment. FIG. 26 is a schematic cross-sectional view taken along line DD in FIG. In Fig. 25, the crystal axes of SiC are shown together with the XYZ coordinate system. The relationship between the [11-20] axis, the [1-100] axis and the

[0001] axis is the same as that explained in relation to Fig. 9. The same is true for Figs. 27, 28 and 39 to 42 described later. FIG. 26 is shown as a cross-section taken along the

[0001] axis.

[0081] 25 and 26, in the semiconductor device 201 according to this embodiment, the sixth semiconductor layer 240 has a portion provided on the first semiconductor layer 20. In this portion, the BPD generated in the first semiconductor layer or the semiconductor substrate 10 can obtain recombination energy of minority carriers and expand into a defect S1, which is a 1SSF. The defect S1 expands upward at an off angle θoff with respect to the XY plane, centered on the Y axis.

[0082] As shown in Fig. 26, the 1SSF extends in a triangular shape on a plane parallel to the {0001} plane of SiC with the BPD as the starting point. In the semiconductor device 201 according to this embodiment, the starting point of the defect S1 extended to the 1SSF is in the sixth semiconductor layer 240, and the sixth semiconductor layer 240 has few point defects that become recombination centers, and minority carriers are continuously injected into the sixth semiconductor layer 240, and the recombination of minority carriers is also continuously performed. Therefore, the defect S1 obtains recombination energy and extends in the sixth semiconductor layer 240 between two adjacent first semiconductor regions 230.

[0083] In the first semiconductor region 230, point defects that function as recombination centers formed by the first element, the second element, or the third element are formed at a high density. Therefore, in the first semiconductor region 230, the lifetime of minority carriers is shortened and the intrusion of minority carriers is suppressed, thereby reducing the generated recombination energy. When the defect S1 reaches the first semiconductor region 230, the defect S1 cannot receive the supply of recombination energy, and therefore the expansion stops.

[0084] In this manner, a semiconductor device 201 with little conduction loss is realized.

[0085] FIG. 27 is a schematic cross-sectional view illustrating the operation of the semiconductor device according to the comparative example. FIG. 28 is a schematic cross-sectional view taken along line EE in FIG. As shown in FIGS. 27 and 28, in the semiconductor device according to the comparative example, the first semiconductor region 230 is not provided, and a sixth semiconductor layer 240c is provided on the first semiconductor layer 20. In the comparative example, as shown in FIG.

[0086] In the semiconductor device of the comparative example, the minority carriers supplied to the sixth semiconductor layer 240c recombine in the sixth semiconductor layer 240c and continue to supply recombination energy to the defect S2, which is a 1SSF. As long as the defect S2 receives the supply of recombination energy, the defect S2 continues to spread in a planar shape having a triangular outer periphery. Since the planar defect S2 spreads along the {0001} plane of the SiC of the sixth semiconductor layer 240, the defect S2 is formed almost perpendicular to the current path. Therefore, the conduction of the current in the semiconductor device is hindered, and the operating voltage increases.

[0087] In this manner, in the semiconductor device 201 according to this embodiment, the first semiconductor region 230 stops the expansion of the 1SSF, and it is possible to prevent an increase in loss when the semiconductor device 201 is conductive.

[0088] In a semiconductor device, forward conduction of a pn junction is achieved by the travel of minority carriers. The first semiconductor region 230 provides a high density of recombination centers, and therefore may impede the travel of minority carriers. Therefore, by arranging a plurality of first semiconductor regions 230 at intervals, the expansion of the BPD to the 1SSF is restricted. In this way, the formation of the 1SSF is impeded while ensuring the travel of minority carriers, and a semiconductor device with low conduction loss can be stably achieved.

[0089] As shown in FIG. 22, by appropriately setting the arrangement intervals and thicknesses of the multiple first semiconductor regions 230, it is possible to realize a semiconductor device 201 that can reliably prevent the expansion of 1SSF.

[0090] (Variation 1) FIG. 29 is a schematic cross-sectional view illustrating a semiconductor device according to a modification of the second embodiment. As shown in FIG. As shown in Fig. 29, in the semiconductor device 201a according to this modification, the configurations of the multiple first semiconductor regions 230a and the sixth semiconductor layer 240d are different from those of the semiconductor device 201 shown in Fig. 20. In other respects, the semiconductor device 201a according to this modification is the same as the semiconductor device 201, and the same components are denoted by the same reference numerals and detailed descriptions thereof will be omitted as appropriate.

[0091] The multiple first semiconductor regions 230a are provided on the first semiconductor layer 20. As with the multiple first semiconductor regions 230 of the semiconductor device 201 shown in Figures 20 and 21, the multiple first semiconductor regions 230a each extend along the Y-axis. Also, as with the multiple first semiconductor regions 230 of the semiconductor device 201, the multiple first semiconductor regions 230a are arranged spaced apart from each other in the X-axis direction.

[0092] The sixth semiconductor layer 240d is provided on the first semiconductor layer 20. The sixth semiconductor layer 240d is provided between the first semiconductor layer 20 and each of the multiple first semiconductor regions 230a. As in the case of the sixth semiconductor layer 240 of the semiconductor device 201, the sixth semiconductor layer 240d is provided between the adjacent first semiconductor regions 230a. As in the case of the sixth semiconductor layer 240 of the semiconductor device 201, the sixth semiconductor layer 240d is provided on the multiple first semiconductor regions 230a.

[0093] Each of the multiple first semiconductor regions 230a contains a first element (N, P, Al, B) or a second element as an impurity. The impurity concentration of the multiple first semiconductor regions 230a is the same as or lower than the impurity concentration of the first semiconductor layer 20. The impurity concentration of the multiple first semiconductor regions 230a is the same as or higher than the impurity concentration of the sixth semiconductor layer 240d.

[0094] The point defect density of the multiple first semiconductor regions 230a is equal to or higher than the point defect density of the first semiconductor layer 20. The point defect density of the multiple first semiconductor regions 230a and the point defect density of the first semiconductor layer 20 are higher than both the point defect density of the semiconductor substrate 10 and the point defect density of the sixth semiconductor layer 240d.

[0095] FIG. 30 is a schematic enlarged view of part F in FIG. Fig. 30 shows the relationship between the distances W1, W2 and the thickness h1 for two adjacent first semiconductor regions 230a, similar to the case shown in Fig. 22. In Fig. 30, the thickness h2 indicates the thickness of the sixth semiconductor layer 240d between the first semiconductor layer 20 and the lower end 230aB of the first semiconductor region 230a. Note that the distance W1 is the distance between the lower ends 230aB or between the upper ends 230aT of two adjacent first semiconductor regions 230, similar to the example shown in Fig. 22.

[0096] The 1SSF expands along the {0001} plane of SiC tilted from the XY plane at the off angle θoff. Therefore, from the viewpoint of suppressing the expansion of the 1SSF in the first semiconductor region 230a, it is preferable that the relationship between W1, W2, and h1 is set based on the off angle θoff. As is clear from FIG. 30, in this example as well, the relationship between W1 and h1 in the example shown in FIG. 22 can be expressed using the angle θ2. W1 is expressed by the following formula (3), and the range of the angle θ2 can be set by formula (4) taking into account the manufacturing variation and the like.

[0097] W1=h / tan(θ2) (3) 2θoff≧θ2≧0.5θoff (4)

[0098] A method for manufacturing the semiconductor device 201a according to this modification will be described. 31 and 32 are schematic cross-sectional views illustrating a part of a manufacturing method for a semiconductor device according to a modification of the second embodiment. As shown in FIG. 2, the first semiconductor layer 20 is formed by epitaxial growth on the prepared semiconductor substrate 10. As shown in FIG. 31, the intermediate semiconductor layer 240e is formed on the first semiconductor layer 20. The intermediate semiconductor layer 240e is formed under the same conditions as the sixth semiconductor layer 240 shown in FIG. 20, for example. After the intermediate semiconductor layer 240e is formed, a mask M2 is formed on the intermediate semiconductor layer 240e. In the mask M2, an opening AP is provided at a position where the first semiconductor region 230a is to be formed. A second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt) or a third element (H, He, Ar, Ne, Xe) is introduced into the intermediate semiconductor layer 240a by ion implantation through the mask M2. The ion implantation energy is set so as to obtain a thickness h2 between the bottom 230aB of the first semiconductor region 230a and the first semiconductor layer 20.

[0099] 32, the mask M1 is removed. The intermediate semiconductor layer 240f is formed in the area where the mask M1 was provided, and the first semiconductor region 230a is formed in the area where the opening AP of the mask M2 was provided.

[0100] Thereafter, a semiconductor layer is further formed by epitaxial growth on the first semiconductor region 230a and the intermediate semiconductor layer 240f, to form the sixth semiconductor layer 240d shown in FIG.

[0101] (Variation 2) FIG. 33 is a schematic cross-sectional view illustrating a semiconductor device according to another modification of the second embodiment. As shown in FIG. As shown in Fig. 33, in the semiconductor device 201b according to this modification, the configurations of the first semiconductor layer 220, the multiple first semiconductor regions 230b, and the sixth semiconductor layer 240g are different from those of the semiconductor device 201 shown in Fig. 20. In other respects, the semiconductor device 201b according to this modification is the same as the semiconductor device 201, and the same components are denoted by the same reference numerals and detailed descriptions thereof will be omitted as appropriate.

[0102] The first semiconductor layer 220 is provided on the semiconductor substrate 10. A plurality of first semiconductor regions 230b are provided on the first semiconductor layer 220. The first semiconductor layer 220 is also provided between adjacent first semiconductor regions 230b.

[0103] 20 and 21, the multiple first semiconductor regions 230b each extend along the Y-axis. Also, like the multiple first semiconductor regions 230 of the semiconductor device 201, the multiple first semiconductor regions 230b are disposed spaced apart from each other in the X-axis direction.

[0104] The sixth semiconductor layer 240g is provided on the first semiconductor layer 220. As in the case of the sixth semiconductor layer 240 of the semiconductor device 201, the sixth semiconductor layer 240g is provided between adjacent first semiconductor regions 230b. As in the case of the sixth semiconductor layer 240 of the semiconductor device 201, the sixth semiconductor layer 240g is provided on a plurality of first semiconductor regions 230b.

[0105] The impurity concentration of the first semiconductor layer 220 is the same as the impurity concentration of the first semiconductor layer 20 of the semiconductor device 201 shown in Fig. 20. In other words, the impurity concentration of the first semiconductor layer 220 is higher than the impurity concentration of the sixth semiconductor layer 240g.

[0106] Each of the multiple first semiconductor regions 230b contains a first element (N, P, Al, B) or a second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt) as an impurity. The impurity concentration of the multiple first semiconductor regions 230b is the same as or lower than the impurity concentration of the first semiconductor layer 220. The impurity concentration of the multiple first semiconductor regions 230b is the same as or higher than the impurity concentration of the sixth semiconductor layer 240g.

[0107] The point defect density of the multiple first semiconductor regions 230b is the same as or higher than the point defect density of the first semiconductor layer 220. The point defect density of the multiple first semiconductor regions 230b and the point defect density of the first semiconductor layer 220 are higher than both the point defect density of the semiconductor substrate 10 and the point defect density of the sixth semiconductor layer 240g. FIG. 34 is a schematic enlarged view of part G in FIG. Fig. 34 shows the relationship between the distances W1, W2 and the thickness h1 for two adjacent first semiconductor regions 230b, similar to the case shown in Fig. 22. In Fig. 34, the thickness h1 is the length from the top end 230bT of the first semiconductor region 230b to the boundary line 230bB between the bottom 230bB1 of the first semiconductor region 230b and the first semiconductor layer 220 on the side of the first semiconductor region 230b. The thickness h3 is the length from the bottom 230bB1 of the first semiconductor region 230b to the boundary line 230bB between the bottom 230bB1 of the first semiconductor region 230b and the first semiconductor layer 220 on the side of the first semiconductor region 230b.

[0108] As in the case of the semiconductor device 201 shown in Fig. 20, from the viewpoint of suppressing the expansion of the 1SSF in the first semiconductor region 230b, it is preferable that the relationship between W1, W2, and h1 is set based on the off angle θoff. As is clear from Fig. 34, in this example as well, the relationship between W1 and h1 in the example shown in Fig. 22 can be expressed using the angle θ3. W1 is expressed by the following formula (5), and the range of the angle θ2 can be set by formula (6) taking into account the variation during manufacturing, etc.

[0109] W1=h / tan(θ3) (5) 2θoff≧θ3≧0.5θoff (6)

[0110] A method for manufacturing the semiconductor device 201b according to this modification will be described. 35 and 36 are schematic cross-sectional views illustrating a part of a method for manufacturing a semiconductor device according to another modification of the second embodiment. As shown in FIG. 35, the first semiconductor layer 220a is formed by epitaxial growth on the prepared semiconductor substrate 10. The intermediate semiconductor layer 240h is formed on the first semiconductor layer 220a. The intermediate semiconductor layer 240h is formed under the same conditions as the sixth semiconductor layer shown in FIG. 20, for example. After the intermediate semiconductor layer 240h is formed, a mask M3 is formed on the intermediate semiconductor layer 240h. In the mask M3, an opening AP is provided at a position where the first semiconductor region 230b is to be formed. A second element (Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, Pt) or a third element (H, He, Ar, Ne, Xe) is introduced into the intermediate semiconductor layer 240h by ion implantation through the mask M3. At this time, the ion implantation energy is set so that the intermediate semiconductor layer 240h is deeper by a thickness h3 than the thickness of the intermediate semiconductor layer 240h.

[0111] As shown in Fig. 36, the mask M3 is removed. An intermediate semiconductor layer 240k is formed in a portion where the mask M3 was provided, and a first semiconductor region 230b is formed in a portion where an opening AP of the mask M3 was provided. The first semiconductor region 230b is formed in the intermediate semiconductor layer 240k. The first semiconductor region 230b penetrates the intermediate semiconductor layer 240k, and a part of the first semiconductor region 230b is also formed in the first semiconductor layer 220b.

[0112] Thereafter, a semiconductor layer is further formed by epitaxial growth on the first semiconductor region 230b and the intermediate semiconductor layer 240k, to form the sixth semiconductor layer 240g shown in FIG.

[0113] In this manner, the semiconductor devices 201a and 201b according to the modified examples are formed. The semiconductor devices 201a and 201b according to the modified examples have the same effects as the semiconductor device 201 shown in FIG.

[0114] (Third embodiment) FIG. 37 is a schematic cross-sectional view illustrating the semiconductor device according to the third embodiment. As shown in FIG. FIG. 38 is a schematic cross-sectional view taken along line HH in FIG. 37 and 38, the semiconductor device 301 according to this embodiment includes a semiconductor substrate 10, a first semiconductor layer 20, a plurality of first semiconductor regions 330a, a plurality of second semiconductor regions 330b, and a sixth semiconductor layer 340. The semiconductor device 301 differs from the semiconductor device 201 shown in FIG. 20 in the configurations of the plurality of first semiconductor regions 330a, the plurality of second semiconductor regions 330b, and the sixth semiconductor layer 340, but is otherwise the same as the semiconductor device 201. The same components are denoted by the same reference numerals, and detailed description thereof will be omitted as appropriate.

[0115] The multiple first semiconductor regions 330a are provided on the first semiconductor layer 20. The multiple first semiconductor regions 330a each extend in the Y-axis direction on the first semiconductor layer 20. The multiple first semiconductor regions 330a are arranged spaced apart in the X-axis direction. In this example, the multiple first semiconductor regions 330a are arranged at approximately equal intervals in the X-axis direction.

[0116] The multiple second semiconductor regions 330b are provided on the first semiconductor layer 20. The multiple second semiconductor regions 330b each extend in the X-axis direction on the first semiconductor layer 20. The multiple second semiconductor regions 330b are arranged spaced apart in the Y-axis direction. In this example, the multiple second semiconductor regions 330b are arranged at approximately equal intervals in the Y-axis direction. In other words, the first semiconductor regions 330a and the second semiconductor regions 330b are arranged to intersect on the XY plane, forming a lattice shape.

[0117] As described in relation to FIG. 1, the XY plane is parallel to the first surface 11a or the second surface 11b of the semiconductor substrate 10, and the [11-20] axis of the semiconductor substrate 10 is inclined by an off angle θoff with respect to the X axis around the Y axis. The

[0001] axis of the semiconductor substrate 10 is inclined by an off angle θoff with respect to the Z axis around the Y axis. The Y axis is parallel to the [1-100] axis perpendicular to the {1-100} plane of the semiconductor substrate 10. That is, the multiple first semiconductor regions 330a each extend along the [1-100] axis of the semiconductor substrate 10. Each of the multiple first semiconductor regions 330a is disposed at approximately equal intervals with respect to the [11-20] axis of the semiconductor substrate 10. Also, the multiple second semiconductor regions 330b each extend along the [11-20] axis of the semiconductor substrate 10. The plurality of second semiconductor regions 330b are arranged at approximately equal intervals with respect to the [1-100] axis of the semiconductor substrate 10.

[0118] The sixth semiconductor layer 340 is provided on the first semiconductor layer 20. The sixth semiconductor layer 340 is also provided on the first semiconductor layer 20 in a portion surrounded by two adjacent and opposing first semiconductor regions 330a and two adjacent and opposing second semiconductor regions 330b. The sixth semiconductor layer 340 is provided on each of the multiple first semiconductor regions 330a and on each of the multiple second semiconductor regions 330b.

[0119] The semiconductor substrate 10, the first semiconductor layer 20, the first semiconductor regions 330a, the second semiconductor regions 330b, and the sixth semiconductor layer 340 contain impurities of a first conductivity type. The first conductivity type is, for example, n-type.

[0120] The first semiconductor region 330a and the second semiconductor region 330b contain SiC and a first element as an impurity, similar to the second semiconductor layer 30 of the semiconductor device 1 shown in FIG. 1. The first element contains at least one selected from the group consisting of N, P, Al, and B. Similarly to the semiconductor device 1, the second semiconductor region 330b may contain a second element instead of the first element or together with the first element. The second element contains at least one selected from the group consisting of Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, and Pt.

[0121] The multiple first semiconductor regions 330a and the multiple second semiconductor regions 330b have the same impurity concentration. The impurity concentrations of the first semiconductor regions 330a and the second semiconductor regions 330b are the same as or lower than the impurity concentration of the first semiconductor layer 20. The impurity concentrations of the first semiconductor regions 330a and the second semiconductor regions 330b are the same as or higher than the impurity concentration of the sixth semiconductor layer 340.

[0122] The multiple first semiconductor regions 330a and the multiple second semiconductor regions 330b have the same point defect density. The point defect density of the first semiconductor region 330a and the second semiconductor region 330b is the same as or higher than the point defect density of the first semiconductor layer 20. The point defect density of the first semiconductor region 330a, the point defect density of the second semiconductor region 330b, and the point defect density of the first semiconductor layer 20 are higher than the point defect density of the semiconductor substrate 10 and the point defect density of the sixth semiconductor layer 340.

[0123] The relationship between the distance between adjacent first semiconductor regions 330a and the thickness of the first semiconductor regions 330a can be the same as that in the example shown in FIG. 22, from the viewpoint of preventing the expansion of 1SSF.

[0124] The semiconductor device 301 according to this embodiment can be manufactured in the same manner as the semiconductor device 201 shown in Fig. 20. That is, the first semiconductor region 330a and the second semiconductor region 330b can be formed by positioning the openings AP of the mask M1 shown in Fig. 23 at positions corresponding to the first semiconductor region 330a and the second semiconductor region 330b that intersect in a lattice pattern.

[0125] The operation of the semiconductor device 301 according to this embodiment will be described. FIG. 39 is a schematic cross-sectional view illustrating the operation of the semiconductor device according to the third embodiment. FIG. 40 is a schematic cross-sectional view taken along line II in FIG. 39 and 40, in the semiconductor device 301 according to this embodiment, the sixth semiconductor layer 340 has a portion provided on the first semiconductor layer 20. In this portion, the BPD generated in the first semiconductor layer or the semiconductor substrate 10 can obtain recombination energy of minority carriers and expand into a defect S3 that is a 1SSF. The defect S3 expands upward at an off angle θoff with respect to the XY plane, centered on the Y axis.

[0126] In addition to the triangular shape shown in FIG. 26 and FIG. 28, the 1SSF is also known to expand into a bar shape. The bar-shaped defect S3 expands the {0001} plane of SiC in both the [1-100] axial direction and the

[1100] axial direction. Therefore, in the semiconductor region 230 of the semiconductor device 201 shown in FIG. 20, even if the expansion in the [11-20] axial direction can be prevented, the expansion of the 1SSF in the [1-100] axial direction and the

[1100] axial direction may not be prevented. In the semiconductor device 301 according to this embodiment, the first semiconductor region 330a and the second semiconductor region 330b are crossed, and the expansion of the bar-shaped defect is prevented by the first semiconductor region 330a and the second semiconductor region 330b.

[0127] FIG. 41 is a schematic cross-sectional view illustrating the operation of the semiconductor device according to the comparative example. FIG. 42 is a schematic cross-sectional view taken along line JJ in FIG. The configuration of the semiconductor device of the comparative example in Figures 41 and 42 is the same as the configuration of the semiconductor device shown in Figures 27 and 28. That is, as shown in Figures 41 and 42, in the semiconductor device according to the comparative example, the first semiconductor region 330a and the second semiconductor region 330b are not provided, and a sixth semiconductor layer 240c is provided on the first semiconductor layer 20.

[0128] In the semiconductor device of the comparative example, the minority carriers supplied to the sixth semiconductor layer 240c recombine in the sixth semiconductor layer 240c and continue to supply recombination energy to the defect S4, which is a 1SSF. As long as the defect S4 receives the supply of recombination energy, the defect S4 continues to spread in the third semiconductor layer 40 in a planar shape having a triangular outer periphery shape and can reach the interface with the fourth semiconductor layer 50. Since the planar defect S4 spreads along the {0001} plane of SiC in the sixth semiconductor layer 240c, the defect S4 is formed almost perpendicular to the current path. Therefore, the conduction of the semiconductor device is hindered and the operating voltage increases.

[0129] In this manner, in the semiconductor device 301 of this embodiment, the first semiconductor region 330a and the second semiconductor region 330b intersecting in a lattice pattern can stop the expansion of any type of 1SSF, thereby preventing an increase in loss when the semiconductor device 301 is conductive.

[0130] In the semiconductor device 301 of this embodiment, the modified example of the second embodiment described in relation to Figures 29 and 33 can be applied to the first semiconductor region and the second semiconductor region, and similar effects can be obtained.

[0131] In the above-mentioned embodiments and modifications, the semiconductor device has been described as being mainly a PiN diode. However, the semiconductor device is not limited to a PiN diode as long as it has a PiN structure in which a semiconductor layer of a second conductivity type is joined to a semiconductor layer of a first conductivity type with a low impurity concentration. For example, a MOSFET of a DMOS structure may be applied as the semiconductor device of each embodiment and each modification.

[0132] In this manner, a semiconductor device having stable characteristics can be realized.

[0133] Although some embodiments of the present invention have been illustrated above, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, modifications, etc. can be made without departing from the gist of the invention. These embodiments and their modifications are included in the scope and gist of the invention, and are included in the scope of the invention and its equivalents described in the claims. In addition, the above-mentioned embodiments can be implemented in combination with each other.

[0134] The embodiments include the following aspects.

[0135] (Appendix 1) a semiconductor substrate of a first conductivity type including silicon carbide, the semiconductor substrate having a first surface and a second surface opposite to the first surface; a first semiconductor layer of a first conductivity type including silicon carbide provided on the first surface; a second semiconductor layer of a first conductivity type including silicon carbide provided on the first semiconductor layer; a third semiconductor layer of the first conductivity type that is provided on the second semiconductor layer and contains silicon carbide; a fourth semiconductor layer of a second conductivity type including silicon carbide provided on the third semiconductor layer; Equipped with a carrier concentration of the first conductivity type of the second semiconductor layer is equal to or lower than a carrier concentration of the first conductivity type of the first semiconductor layer; a carrier concentration of the first conductivity type of the second semiconductor layer is equal to or higher than a carrier concentration of the first conductivity type of the third semiconductor layer; A semiconductor device, wherein the point defect density of the second semiconductor layer is equal to or higher than the point defect density of the first semiconductor layer and is higher than the point defect density of the third semiconductor layer.

[0136] (Appendix 2) a fifth semiconductor layer of the first conductivity type that contains silicon carbide and is provided between the first semiconductor layer and the second semiconductor layer; a carrier concentration of the first conductivity type of the second semiconductor layer is equal to or higher than a carrier concentration of the first conductivity type of the fifth semiconductor layer; 2. The semiconductor device according to claim 1, wherein the second semiconductor layer has a point defect density higher than a point defect density of the fifth semiconductor layer.

[0137] (Appendix 3) the second semiconductor layer includes a first layer provided on the first semiconductor layer and a second layer provided on the first layer, a carrier concentration of the first conductivity type of the first layer is equal to or lower than a carrier concentration of the first conductivity type of the first semiconductor layer; a carrier concentration of the first conductivity type of the second layer is equal to or lower than a carrier concentration of the first conductivity type of the first layer, and is equal to or higher than a carrier concentration of the first conductivity type of the third semiconductor layer; a point defect density of the first layer and a point defect density of the second layer are equal to or higher than a point defect density of the first semiconductor layer; 3. The semiconductor device according to claim 1, wherein the point defect density is higher than that of the third semiconductor layer.

[0138] (Appendix 4) a semiconductor substrate of a first conductivity type including silicon carbide, the semiconductor substrate having a first surface and a second surface opposite to the first surface; a first semiconductor layer of a first conductivity type including silicon carbide provided on the first surface; a plurality of first semiconductor regions of a first conductivity type including silicon carbide provided on the first semiconductor layer; a sixth semiconductor layer of the first conductivity type that is provided on the first semiconductor layer and contains silicon carbide; a fourth semiconductor layer of a second conductivity type including silicon carbide provided on the sixth semiconductor layer; Equipped with the first surface is parallel to a plane including a first direction and a second direction intersecting the first direction; the first semiconductor regions each extend along the first direction and are spaced apart along the second direction; a {0001} plane of the silicon carbide forms a first angle with the first plane about a [1-100] axis perpendicular to the {1-100} plane of the silicon carbide; the second direction is parallel to the direction in which the [1-100] axis extends; a carrier concentration of the first conductivity type in the plurality of first semiconductor regions is equal to or lower than a carrier concentration of the first conductivity type in the first semiconductor layer; a carrier concentration of the first conductivity type in the plurality of first semiconductor regions is equal to or higher than a carrier concentration of the first conductivity type in the sixth semiconductor layer; A semiconductor device, wherein the point defect density of the plurality of first semiconductor regions is equal to or higher than the point defect density of the first semiconductor layer and is higher than the point defect density of the sixth semiconductor layer.

[0139] (Appendix 5) 5. The semiconductor device according to claim 4, wherein the sixth semiconductor layer is provided on the first semiconductor layer and between the first semiconductor layer and each of the plurality of first semiconductor regions.

[0140] (Appendix 6) 6. The semiconductor device according to claim 4, wherein the first semiconductor layer is provided between two adjacent first semiconductor regions among the plurality of first semiconductor regions.

[0141] (Appendix 7) a second semiconductor region of a first conductivity type including silicon carbide provided on the first semiconductor layer; the second semiconductor regions each extend along the second direction and are spaced apart along the first direction; the sixth semiconductor layer is surrounded by two first semiconductor regions of the plurality of first semiconductor regions and two second semiconductor regions of the plurality of second semiconductor regions on the first semiconductor layer; a carrier concentration of the first conductivity type in the plurality of second semiconductor regions is equal to or lower than a carrier concentration of the first conductivity type in the first semiconductor layer; the first conductivity type carrier concentration of the second semiconductor regions is equal to or higher than the first conductivity type carrier concentration of the sixth semiconductor layer; The point defect density of the plurality of second semiconductor regions is equal to or higher than the point defect density of the first semiconductor layer, and 5. The semiconductor device according to claim 4, wherein the point defect density is higher than that of the sixth semiconductor layer.

[0142] (Appendix 8) The semiconductor device according to any one of appendixes 4 to 7, wherein a distance between two adjacent first semiconductor regions among the plurality of first semiconductor regions is set based on thicknesses of the plurality of first semiconductor regions and the first angle.

[0143] (Appendix 9) a carrier of the first conductivity type in the second semiconductor layer includes a first element; 4. The semiconductor device according to claim 1, wherein the first element includes at least one selected from the group consisting of N, P, Al, and B.

[0144] (Appendix 10) the second semiconductor layer includes a second element; The semiconductor device according to any one of claims 1 to 3, wherein the second element includes at least one selected from the group consisting of Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au, and Pt. [Explanation of symbols]

[0145] 1, 1a, 1b, 201, 201a, 201b, 301...semiconductor device, 10...semiconductor substrate, 20, 220, 220a...first semiconductor layer, 30, 130...second semiconductor layer, 32...first layer, 34...Second layer, 40...third semiconductor layer, 42...fifth semiconductor layer, 50...fourth semiconductor layer, 62...first electrode, 64...second electrode, 230, 230a, 230b, 330a...first semiconductor region, 240, 240d, 240g, 340...sixth semiconductor layer, 330b...second semiconductor region

Claims

1. a semiconductor substrate of a first conductivity type including silicon carbide, the semiconductor substrate having a first surface and a second surface opposite to the first surface; a first semiconductor layer of a first conductivity type including silicon carbide provided on the first surface; a second semiconductor layer of a first conductivity type including silicon carbide provided on the first semiconductor layer; a third semiconductor layer of the first conductivity type provided on the second semiconductor layer and containing silicon carbide; a fourth semiconductor layer of a second conductivity type including silicon carbide provided on the third semiconductor layer; Equipped with a carrier concentration of the first conductivity type of the second semiconductor layer is equal to or lower than a carrier concentration of the first conductivity type of the first semiconductor layer; a carrier concentration of the first conductivity type of the second semiconductor layer is equal to or higher than a carrier concentration of the first conductivity type of the third semiconductor layer; A semiconductor device, wherein the point defect density of the second semiconductor layer is equal to or higher than the point defect density of the first semiconductor layer and is higher than the point defect density of the third semiconductor layer.

2. a fifth semiconductor layer of the first conductivity type that contains silicon carbide and is provided between the first semiconductor layer and the second semiconductor layer; a carrier concentration of the first conductivity type of the second semiconductor layer is equal to or higher than a carrier concentration of the first conductivity type of the fifth semiconductor layer; The semiconductor device according to claim 1 , wherein the second semiconductor layer has a point defect density higher than a point defect density of the fifth semiconductor layer.

3. the second semiconductor layer includes a first layer provided on the first semiconductor layer and a second layer provided on the first layer, a carrier concentration of the first conductivity type of the first layer is equal to or lower than a carrier concentration of the first conductivity type of the first semiconductor layer; a carrier concentration of the first conductivity type of the second layer is equal to or lower than a carrier concentration of the first conductivity type of the first layer, and is equal to or higher than a carrier concentration of the first conductivity type of the third semiconductor layer; a point defect density of the first layer and a point defect density of the second layer are equal to or higher than a point defect density of the first semiconductor layer; 2. The semiconductor device according to claim 1, wherein the point defect density is higher than that of the third semiconductor layer.

4. a semiconductor substrate of a first conductivity type including silicon carbide, the semiconductor substrate having a first surface and a second surface opposite to the first surface; a first semiconductor layer of a first conductivity type including silicon carbide provided on the first surface; a plurality of first semiconductor regions of a first conductivity type including silicon carbide provided on the first semiconductor layer; a sixth semiconductor layer of the first conductivity type including silicon carbide provided on the first semiconductor layer; a fourth semiconductor layer of a second conductivity type including silicon carbide provided on the sixth semiconductor layer; Equipped with the first surface is parallel to a plane including a first direction and a second direction intersecting the first direction; the first semiconductor regions each extend along the first direction and are spaced apart along the second direction; the {0001} plane of the silicon carbide forms a first angle with the first plane about a [1-100] axis perpendicular to the {1-100} plane of the silicon carbide; the second direction is parallel to the direction in which the [1-100] axis extends; a carrier concentration of the first conductivity type in the plurality of first semiconductor regions is equal to or lower than a carrier concentration of the first conductivity type in the first semiconductor layer; a carrier concentration of the first conductivity type in the plurality of first semiconductor regions is equal to or higher than a carrier concentration of the first conductivity type in the sixth semiconductor layer; A semiconductor device, wherein the point defect density of the plurality of first semiconductor regions is equal to or higher than the point defect density of the first semiconductor layer and is higher than the point defect density of the sixth semiconductor layer.

5. The semiconductor device according to claim 4 , wherein the sixth semiconductor layer is provided on the first semiconductor layer and between the first semiconductor layer and each of the plurality of first semiconductor regions.

6. The semiconductor device according to claim 4 , wherein the first semiconductor layer is provided between two adjacent first semiconductor regions of the plurality of first semiconductor regions.

7. a second semiconductor region of a first conductivity type including silicon carbide provided on the first semiconductor layer; the second semiconductor regions each extend along the second direction and are spaced apart along the first direction; the sixth semiconductor layer is surrounded by two first semiconductor regions of the plurality of first semiconductor regions and two second semiconductor regions of the plurality of second semiconductor regions on the first semiconductor layer; a carrier concentration of the first conductivity type in the plurality of second semiconductor regions is equal to or lower than a carrier concentration of the first conductivity type in the first semiconductor layer; a carrier concentration of the first conductivity type in the plurality of second semiconductor regions is equal to or higher than a carrier concentration of the first conductivity type in the sixth semiconductor layer; The point defect density of the plurality of second semiconductor regions is equal to or higher than the point defect density of the first semiconductor layer, and 5. The semiconductor device according to claim 4, wherein the point defect density is higher than that of the sixth semiconductor layer.

8. 5. The semiconductor device according to claim 4, wherein a distance between two adjacent first semiconductor regions among the plurality of first semiconductor regions is set based on thicknesses of the plurality of first semiconductor regions and the first angle.

9. a carrier of the first conductivity type in the second semiconductor layer includes a first element; 2. The semiconductor device according to claim 1, wherein the first element includes at least one element selected from the group consisting of N, P, Al, and B.

10. the second semiconductor layer includes a second element; 2. The semiconductor device according to claim 1, wherein the second element includes at least one selected from the group consisting of Fe, Ni, Cr, Mg, Zn, Cu, Ca, V, Au and Pt.

Citation Information

Patent Citations

  • Bipolar semiconductor element

    JP2011109018A

  • Silicon carbide semiconductor device and method of manufacturing silicon carbide semiconductor device

    JP2020077720A

  • Silicon carbide semiconductor device and manufacturing method thereof

    JP2022163554A

  • Semiconductor device and method for manufacturing semiconductor device

    JP2024018648A

  • Semiconductor device including silicon carbide body and method of manufacturing

    US20200203513A1

Cited By

  • Low thermal expansion alloy

    CN121592949A

  • Low thermal expansion alloy

    EP4696793A1