Printed wiring board and related structure using water-glass as insulating material

Water glass is used as an insulating material to address impedance mismatch and reduce CO2 emissions in multilayer printed wiring boards by forming a uniform dielectric constant without high-temperature firing, enhancing manufacturing efficiency and environmental sustainability.

JP2024136189AActive Publication Date: 2024-10-04M3 CORP
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2023047216
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-23
Publication Date
2024-10-04
Estimated Expiration
2043-03-23

AI Technical Summary

Technical Problem

The increasing complexity and fineness of multilayer printed wiring boards lead to issues such as characteristic impedance mismatch and CO2 emissions due to the use of glass cloths and ceramics, which affect the uniformity of dielectric constants and require high-temperature manufacturing processes.

Method used

Utilizing water glass containing sodium silicate as an insulating material for printed wiring boards, forming an insulating layer by applying liquid water glass to a wiring pattern and curing it, then peeling off protective sheets to create a uniform dielectric constant without the need for high-temperature firing.

Benefits of technology

This approach reduces the influence on characteristic impedance and minimizes CO2 emissions by avoiding high-temperature processes, resulting in a simpler and more environmentally friendly manufacturing process for multilayer printed wiring boards.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024136189000001_ABST
    Figure 2024136189000001_ABST
Patent Text Reader

Abstract

To solve the problem of characteristic impedance mismatch of wiring patterns due to multilayering and miniaturization of printed wiring boards, the problem of CO2 emissions generated in the manufacturing process of ceramic substrates, and the problem of insufficient consideration of the SDGs.SOLUTION: A water-glass with sodium silicate as the main ingredient is used as a material for an insulating layer of a printed wiring board. The liquid water-glass is applied or added to the wiring pattern generated on a protective sheet, etc., and cured to form the insulating layer between the wiring layers of the printed wiring board. The protective sheet is then peeled off to produce a printed wiring board with the cured coating film of water-glass as the insulating layer.SELECTED DRAWING: Figure 20
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a multilayer printed wiring board having a rigid area and a flexible area, the multilayer printed wiring board having a wiring pattern. [Background technology]

[0002] In recent years, as printed wiring boards have become more multi-layered and wiring patterns have become finer, the manufacturing methods for printed wiring boards have become more complex, and printed wiring boards using ceramics or organic materials are being used in servers, etc.

[0003] These are convenient for normal use, but they have issues such as inconsistencies in the characteristic impedance of wiring patterns as they become more multi-layered and miniaturized, and the difficulty of manufacturing while taking CO2 emissions into consideration. Furthermore, there is the issue that they do not take sufficient consideration of the SDGs. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent 7029033 [Patent Document 2] Patent Publication No. 2007-324439 [Patent Document 3] Patent Publication No. 2006-63489 [Patent Document 4] Patent Publication No. 2020-105683 [Patent Document 5] Patent Publication 2020-150016 [Patent Document 6] Patent Publication No. 2021-82759 [Patent Document 7] Patent Publication No. 2023-823 [Patent Document 8] Patent Publication No. 2023-8061 Summary of the Invention [Problem to be solved by the invention]

[0005] The above Patent Document 1 describes glass cloth for printed wiring boards, but the glass cloth itself has characteristics such as relative dielectric constant, and the material between the glass cloth also has characteristics such as relative dielectric constant. Therefore, as the wiring pattern becomes finer, the characteristic impedance of the wiring pattern may change due to the influence of the glass cloth and the material between the glass cloth. Furthermore, Patent Document 2 uses ceramics to improve the strength of the printed wiring board, but the manufacturing process of ceramics requires a high-temperature firing process, and it may be difficult to reduce CO2 emissions during the manufacturing process.

[0006] In order to solve the above-mentioned problem of mismatching in characteristic impedance, measures such as making the glass cloth as fine as possible have been considered, as proposed in Patent Document 1 etc. In addition, in order to improve the strength of the printed wiring board, which is the above-mentioned problem, the use of ceramics has been considered, as proposed in Patent Document 2 etc.

[0007] However, even if the glass cloth is made finer, if adjacent wiring patterns are also made finer, differences in properties such as the dielectric constant of the glass cloth and in properties such as the dielectric constant of the materials between the glass cloths may affect the non-uniformity of the characteristic impedance of the wiring patterns.

[0008] In addition, the use of ceramics can improve the strength of printed wiring boards, but the ceramic manufacturing process requires a firing process, which means that it may be difficult to reduce CO2 emissions from the printed wiring board manufacturing process.

[0009] An object of the present invention is to provide a printed wiring board using water glass as an insulating material in order to improve mismatch of characteristic impedance and CO2 emissions during the manufacturing process. [Means for solving the problem]

[0010] The present invention uses water glass, the main component of which is sodium silicate, as a material for the insulating layer of a printed wiring board. Liquid water glass is applied or added to a wiring pattern formed on a protective sheet or the like, and then cured to form an insulating layer between the wiring layers of the printed wiring board. The protective sheet is then peeled off to produce a printed wiring board with a cured coating of water glass as the insulating layer. Effect of the Invention

[0011] The present invention utilizes water glass as a material for the insulating layer of a printed wiring board. Liquid water glass is applied or added to a wiring pattern formed on a protective sheet or the like, and then cured to form an insulating layer between the wiring layers of a printed wiring board. The protective sheet is then peeled off to produce a printed wiring board with a cured coating of water glass as the insulating layer.

[0012] Here, the cured water glass coating film does not contain glass cloth, etc., and therefore the properties of the cured water glass coating film, such as the relative dielectric constant, are uniform, and therefore the effect on the characteristic impedance of the wiring pattern can be reduced, compared to insulating layer materials that contain glass cloth, etc.

[0013] In addition, the manufacturing process of ceramics and other materials requires a firing step at high temperatures, making it difficult to reduce CO2 emissions from the manufacturing process. However, when hardening water glass, a high-temperature environment is not generally required, making it possible to reduce CO2 emissions compared to the manufacturing of ceramics and other materials. [Brief description of the drawings]

[0014] [Figure 1] FIG. 1 shows a copper foil on a first protective sheet 1 having a pattern 2 formed by etching. [Diagram 2]FIG. 2 shows a first protective sheet 1 having a wiring pattern 2 and a guide 3 for preventing liquid leakage formed around the periphery of the first protective sheet 1. [Diagram 3] FIG. 3 shows a first protective sheet 1 having a wiring pattern 2 and a guide 3 for preventing liquid leakage, to which liquid water glass 4 has been applied or added. [Figure 4] Figure 4 shows a state in which liquid water glass 4 formed on a first protective sheet 1 having a wiring pattern 2 and a liquid outflow prevention guide 3 has become a hardened water glass coating film 5, after which the liquid outflow prevention guide 3 and first protective sheet 1 have been removed. [Diagram 5] FIG. 5 shows a pattern 2 formed in FIG. 1, with a second protective sheet 6 formed on the surface opposite to the first protective sheet 1. [Figure 6] FIG. 6 shows the state of FIG. 5 after first protective sheet 1 has been peeled off. [Figure 7] FIG. 7 shows the state in which the device is turned upside down from the state in FIG. [Figure 8] FIG. 8 shows a second protective sheet 6 having a wiring pattern 2 and a guide 3 for preventing liquid leakage formed around the periphery of the second protective sheet 6. In FIG. [Figure 9] FIG. 9 shows a second protective sheet 6 having a wiring pattern 2 and a guide 3 for preventing the liquid from leaking, to which liquid water glass 4 has been applied or added. [Figure 10] FIG. 10 shows a state in which liquid water glass 4 formed on a second protective sheet 6 having a wiring pattern 2 and a liquid outflow prevention guide 3 has become a hardened water glass coating film 6, after which the liquid outflow prevention guide 3 and second protective sheet 6 have been removed. [Figure 11] FIG. 11 is a thick copper 8 with an etching resist 7 . [Figure 12] FIG. 12 shows a state in which the thick copper 8 having the etching resist 7 of FIG. 11 is etched from the etching resist 7 side. [Figure 13] FIG. 13 shows the state after removing the etching resist 7 of FIG. [Figure 14]FIG. 14 shows the thick copper of FIG. 13 turned upside down, with a third protective sheet 9 added to the etched side and an etching resist 7 added to the non-etched side. [Figure 15] FIG. 15 shows the thick copper of FIG. 14, which has been etched from the etching resist 7 side. [Figure 16] FIG. 16 shows the thick copper of FIG. 15 with the etching resist 7 removed and a liquid outflow prevention guide 3 added. [Figure 17] FIG. 17 shows the state of FIG. 16 to which liquid water glass 4 has been applied or added. [Figure 18] FIG. 18 shows a state in which the liquid water glass 4 in the state shown in FIG. 17 has turned into a hardened coating film 6 of water glass, and the liquid outflow prevention guide 3 has been removed. [Figure 19] FIG. 19 shows the metal surface of the via 10 exposed by polishing the hardened water glass coating 6 of FIG. [Figure 20] FIG. 20 shows the cured water glass coating film 6 having the wiring pattern 2 and vias 10 of FIG. 19 with the third protective sheet 9 removed. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, an embodiment will be described with reference to the drawings.

[0016] In the description of the drawings, the same elements are given the same reference numerals and redundant description will be omitted. In addition, the drawings are for the purpose of understanding, and the actual dimensional ratios do not necessarily correspond to the actual ones.

[0017] FIG. 1 shows a copper foil on a first protective sheet 1 having a pattern 2 formed by etching.

[0018] 2 shows a first protective sheet 1 having a wiring pattern 2 and a liquid outflow prevention guide 3 formed around the periphery thereof. By providing this liquid outflow prevention guide 3, it becomes possible to effectively prevent the liquid water glass 4 from outflowing outside the first protective sheet 1 when the liquid water glass 4 is applied or added.

[0019] In Fig. 3, liquid water glass 4 is applied or added to a first protective sheet 1 having a wiring pattern 2 and a guide 3 for preventing the liquid from leaking. In this state, the liquid water glass 4 at room temperature changes into a hardened water glass coating film 5. To hasten the hardening conditions, it is also possible to handle the process under conditions where the temperature is changed to a high temperature.

[0020] 4 shows a state in which liquid water glass 4 formed on first protective sheet 1 having wiring pattern 2 and liquid outflow prevention guide 3 has become a hardened water glass coating film 5, after which liquid outflow prevention guide 3 and first protective sheet 1 have been removed. In this state, wiring pattern 2 has been formed on the surface of hardened water glass coating film 5.

[0021] Furthermore, in this state, there is a possibility that the wiring pattern 2 may peel off from the hardened water glass coating film 5. Next, an embodiment for avoiding this state will be described.

[0022] FIG. 5 shows a pattern 2 formed in FIG. 1, with a second protective sheet 6 formed on the surface opposite to the first protective sheet 1.

[0023] FIG. 6 shows the state of FIG. 5 after first protective sheet 1 has been peeled off.

[0024] FIG. 7 shows the state in which the device is turned upside down from the state in FIG.

[0025] 8 shows a liquid outflow prevention guide 3 formed around the second protective sheet 6 having the wiring pattern 2. By providing this liquid outflow prevention guide 3, it becomes possible to effectively prevent the liquid water glass 4 from flowing out of the second protective sheet 6 when the liquid water glass 4 is applied or added.

[0026] In Fig. 9, liquid water glass 4 is applied or added to a second protective sheet 6 having a wiring pattern 2 and a liquid outflow prevention guide 3. In this state, the liquid water glass 4 at room temperature changes into a hardened water glass coating film 5. To hasten the hardening conditions, it is also possible to handle the process under conditions where the temperature is changed to a high temperature.

[0027] 10 shows a state in which liquid water glass 4 formed on second protective sheet 6 having wiring pattern 2 and liquid outflow prevention guide 3 has become a hardened water glass coating film 6, after which liquid outflow prevention guide 3 and second protective sheet 6 have been removed. In this state, compared to FIG. 4, the lower base, which is the longer side of the trapezoidal shape of wiring pattern 2, is present inside hardened water glass coating film 5, so that wiring pattern 2 has the characteristic of being less likely to peel off from hardened water glass coating film 5.

[0028] Next, an embodiment of via formation will also be described.

[0029] FIG. 11 is a thick copper 8 with an etching resist 7 .

[0030] FIG. 12 shows a state in which the thick copper 8 having the etching resist 7 of FIG. 11 is etched from the etching resist 7 side.

[0031] FIG. 13 shows the state after removing the etching resist 7 of FIG.

[0032] FIG. 14 shows the thick copper of FIG. 13 turned upside down, with a third protective sheet 9 added to the etched side and an etching resist 7 added to the non-etched side.

[0033] Fig. 15 shows the thick copper of Fig. 14, which has been etched from the etching resist 7 side. By adjusting the type and concentration of the etching solution or the etching time, it is possible to form vias 10.

[0034] Fig. 16 shows the thick copper of Fig. 15 with the etching resist 7 removed and a liquid outflow prevention guide 3 added. By providing this liquid outflow prevention guide 3, it becomes possible to effectively prevent the liquid water glass 4 from flowing out of the third protective sheet 9 when the liquid water glass 4 is applied or added.

[0035] Fig. 17 shows the state of Fig. 16 to which liquid water glass 4 has been applied or added. In this state, the liquid water glass 4 at room temperature changes into a hardened water glass coating film 5. To hasten the hardening process, it is also possible to change the temperature to a higher temperature.

[0036] FIG. 18 shows a state in which the liquid water glass 4 in the state shown in FIG. 17 has turned into a hardened coating film 6 of water glass, and the liquid outflow prevention guide 3 has been removed.

[0037] FIG. 19 shows a state in which the hardened water glass coating film 6 of FIG. 18 is polished to expose the metal surface of the via 10 to the outside of the hardened water glass coating film 6.

[0038] FIG. 20 shows the cured water glass coating film 6 having the wiring pattern 2 and vias 10 of FIG. 19 with the third protective sheet 9 removed.

[0039] As explained above, in the printed wiring board and related structures using water glass as an insulating material according to the present invention, liquid water glass is applied or added to a wiring pattern formed on a protective sheet or the like, and then cured to form an insulating layer between wiring layers of the printed wiring board. The protective sheet or the like is then peeled off to produce a printed wiring board with a cured coating of water glass as an insulating layer.

[0040] Here, the cured water glass coating film does not contain glass cloth, etc., so the properties of the cured water glass coating film, such as the relative dielectric constant, are uniform, and therefore the effect on the characteristic impedance of the wiring pattern can be reduced, compared to insulating layer materials that contain glass cloth, etc.

[0041] In addition, the manufacturing process for ceramics and other materials requires a firing step at high temperatures, making it difficult to reduce CO2 emissions from the manufacturing process. However, hardening water glass does not require a high-temperature environment, making it possible to reduce CO2 emissions compared to the manufacturing of ceramics and other materials.

[0042] Furthermore, compared to the manufacturing method of multilayer printed wiring boards having rigid and flexible regions with wiring patterns, this method has the advantage of being a simple process. [Industrial Applicability]

[0043] In the printed wiring board and related structures using water glass as an insulating material according to the present invention, liquid water glass is applied or added to a wiring pattern formed on a protective sheet or the like, and then cured to form an insulating layer between wiring layers of the printed wiring board. The protective sheet is then peeled off to produce a printed wiring board having a cured coating of water glass as an insulating layer. Here, the cured water glass coating film does not contain glass cloth, etc., so the properties of the cured water glass coating film, such as the relative dielectric constant, are uniform, and therefore the effect on the characteristic impedance of the wiring pattern can be reduced, compared to insulating layer materials that contain glass cloth, etc. In addition, the manufacturing process for ceramics and other materials requires a firing step at high temperatures, making it difficult to reduce CO2 emissions from the manufacturing process. However, hardening water glass does not require a high-temperature environment, making it possible to reduce CO2 emissions compared to the manufacturing of ceramics and other materials. [Explanation of symbols]

[0044] 1. First protective sheet 2. Wiring pattern 3. Liquid spill prevention guide 4. Liquid water glass 5. Hardened water glass coating 6. Second protective sheet 7. Etching resist 8. Thick copper 9. Third protective sheet 10. Via

Claims

1. A printed wiring board with a wiring structure for electrical conduction on the surface of a hardened coating of water glass.

2. The water glass of claim 1 contains fine particles of aluminum oxide, aluminum nitride, or the like.

3. The water glass of claim 1 has an elastic function by adjusting the component ratio of sodium silicate, which is the main component of the water glass.

4. 13. A printed wiring board according to claim 1 laminated to another type of printed wiring board.

5. 13. A printed wiring board according to claim 1 bonded to another type of electronic component.

6. 13. A printed wiring board according to claim 1 laminated to another type of organic material.

7. 2. The printed wiring board of claim 1, further comprising a via structure for electrical conduction.

Citation Information

Patent Citations

  • Electric insulating member and manufacture thereof

    JP2001052526A

  • Substrate with insulating layer, semiconductor device using the same, photoelectric conversion element, light-emitting element, and electronic circuit

    JP2013084894A

  • Flexible alkali metal silicate glass products

    US4824807A

  • Process for attaching a silicon chip to a circuit board using a block of encapsulated wires and the block of wires manufactured by the process

    US5807766A

  • Method for producing flat glass fiber woven fabric

    JP2006063489A