Piezoelectric substrate, sensor, actuator, and biological information acquisition device
The piezoelectric base material with a waterproof coating and oriented fibers addresses water absorption issues in fibrous polypeptides, maintaining sensitivity by preventing vapor contact and coating defects.
Patent Information
- Application Number
- JP2023047337
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-23
- Publication Date
- 2024-10-04
AI Technical Summary
Fibrous optically active polypeptides like silk absorb water, leading to decreased piezoelectric sensitivity due to water vapor contact, which causes bubble formation and cracks in resin coatings, compromising waterproof function and sensitivity.
A piezoelectric base material with a waterproof coating containing 2 mg or less water per meter, oriented fibers with a degree of orientation F of 0.50 to 1.00, and a spiral winding of piezoelectric bodies around an internal conductor with a helical angle of 20° to 70°, along with an outer conductor for insulation.
Maintains good piezoelectric sensitivity by preventing water vapor contact and minimizing coating defects, ensuring stable performance under varying conditions.
Smart Images

Figure 2024136265000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a piezoelectric substrate, a sensor, an actuator, and a bioinformation acquisition device. [Background technology]
[0002] In recent years, applications of piezoelectric materials containing optically active polypeptides (hereinafter referred to as "optically active polypeptides") to piezoelectric devices such as sensors and actuators have been considered. In addition, the use of fibrous optically active polypeptides such as silk threads as optically active polypeptides has been considered. For example, Patent Document 1 describes a piezoelectric substrate that uses silk, a fibrous optically active polypeptide, as a piezoelectric material. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2018 / 092886 DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]
[0004] Fiber-like optically active polypeptides such as silk are prone to absorbing moisture, and contact of the optically active polypeptide with water vapor in the air may lead to a decrease in the piezoelectric sensitivity of the piezoelectric substrate. Therefore, from the viewpoint of maintaining the piezoelectric sensitivity, it is desirable to cover the periphery of the piezoelectric body with a resin or the like to suppress contact between the piezoelectric body and water vapor in the air. However, the fibrous optically active polypeptide may contain a certain amount of moisture under normal circumstances. For this reason, for example, when the piezoelectric body comes into contact with the molten resin during the formation of the coating, the moisture contained in the optically active polypeptide may suddenly evaporate, which may cause bubbles to form in the coating, cracks in the coating, etc. As a result, the coating formed around the piezoelectric body may not perform a sufficient waterproofing function, and good piezoelectric sensitivity may not be maintained.
[0005] In view of the above circumstances, an object of one embodiment of the present disclosure is to provide a piezoelectric substrate, a sensor, an actuator, and a bioinformation acquisition device that maintain good piezoelectric sensitivity. [Means for solving the problem]
[0006] Means for solving the above problems include the following embodiments. <1> A long inner conductor; a piezoelectric body covering an outer circumferential surface of the internal conductor; A piezoelectric substrate comprising a waterproof coating covering an outer peripheral surface of the piezoelectric body, The amount of moisture contained per 1 m of the piezoelectric substrate is 2 mg or less, The piezoelectric body includes fibers made of an optically active polypeptide, the length direction of the piezoelectric body is approximately parallel to the main orientation direction of the optically active polypeptide; A piezoelectric substrate, in which the degree of orientation F of the fibers made of the optically active polypeptide, which is determined by X-ray diffraction measurement using the following formula (a), is 0.50 or more and less than 1.00. Orientation degree F=(180°-α) / 180° … Formula (a) [In formula (a), α represents the half-width (°) of the peak due to the orientation.] <2> The waterproof coating comprises a resin. <1> The piezoelectric substrate according to claim 1 . <3> and an outer conductor disposed between the piezoelectric body and the waterproof coating, the outer conductor being electrically insulated from the inner conductor. <1> or <2> The piezoelectric substrate according to claim 1 . <4> The piezoelectric body is a long piezoelectric body. <1> ~ <3> 13. The piezoelectric substrate according to claim 12, wherein the piezoelectric substrate is a piezoelectric material. <5> The long piezoelectric body is wound in a spiral shape around an outer circumferential surface of the internal conductor. <4> The piezoelectric substrate according to claim 1 . <6> a helix angle between the axial direction of the internal conductor and the longitudinal direction of the elongated piezoelectric body is 20° to 70°; <4> or <5> The piezoelectric substrate according to claim 1 . <7> The optically active polypeptide has a β-sheet structure. <1> ~ <6> 13. The piezoelectric substrate according to claim 12, wherein the piezoelectric substrate is a piezoelectric material. <8> The optically active polypeptide comprises fibroin; <1> ~ <7> 13. The piezoelectric substrate according to claim 12, wherein the piezoelectric substrate is a piezoelectric material. <9> The fiber made of the optically active polypeptide is silk. <1> ~ <8> 13. The piezoelectric substrate according to claim 12, wherein the piezoelectric substrate is a piezoelectric material. <10> The piezoelectric body is a filamentous piezoelectric body, and the twist number of the filamentous piezoelectric body is 500 T / m or less. <1> ~ <9> 13. The piezoelectric substrate according to claim 12, wherein the piezoelectric substrate is a piezoelectric material. <11> <1> ~ <10> A sensor comprising the piezoelectric substrate according to any one of claims 1 to 5. <12> <1> ~ <10> An actuator comprising the piezoelectric substrate according to any one of claims 1 to 5. <13> <1> ~ <10> A bioinformation acquisition device comprising the piezoelectric substrate according to any one of claims 1 to 5.
[0007] According to the present disclosure, a piezoelectric substrate, a sensor, an actuator, and a bioinformation acquisition device are provided that maintain good piezoelectric sensitivity. [Brief description of the drawings]
[0008] [Figure 1A] FIG. 2 is a schematic side view illustrating the appearance of a piezoelectric substrate according to an embodiment of the present disclosure. [Figure 1B] FIG. 1B is a cross-sectional view taken along line IB-IB of FIG. [Diagram 2] FIG. 2 is a schematic side view illustrating the appearance of a piezoelectric substrate according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] In the present disclosure, a numerical range expressed using "to" means a range that includes the numerical values before and after "to" as the lower and upper limits.
[0010] <Piezoelectric substrate> The piezoelectric substrate of the present disclosure is A long inner conductor; a piezoelectric body covering an outer circumferential surface of the internal conductor; A piezoelectric substrate comprising a waterproof coating covering an outer peripheral surface of the piezoelectric body, The amount of moisture contained per 1 m of the piezoelectric substrate is 2 mg or less, The piezoelectric body includes fibers made of an optically active polypeptide, the length direction of the piezoelectric body is approximately parallel to the main orientation direction of the optically active polypeptide; The degree of orientation F of the fibers made of the optically active polypeptide, which is determined by X-ray diffraction measurement using the following formula (a), is 0.50 or more and less than 1.00. Orientation degree F=(180°-α) / 180° … Formula (a) [In formula (a), α represents the half-width (°) of the peak due to the orientation.]
[0011] The piezoelectric substrate of the present disclosure is provided with a waterproof coating that covers the outer peripheral surface of the piezoelectric body. This effectively prevents the piezoelectric body from coming into contact with water vapor in the air. Furthermore, the piezoelectric substrate of the present disclosure contains 2 mg or less of water per 1 m of the piezoelectric substrate. This means that the waterproof coating that covers the outer peripheral surface of the piezoelectric body is less prone to bubble formation and cracks during formation, and exhibits excellent waterproof performance. As a result, good piezoelectric sensitivity is maintained.
[0012] From the viewpoint of forming a good waterproof coating, the amount of moisture contained per 1 m of the piezoelectric substrate is preferably 1 mg or less, and more preferably 0.5 mg or less.
[0013] In the present disclosure, an "optically active polypeptide" refers to a polypeptide that has an asymmetric carbon atom and has a bias in the abundance of optical isomers. In the present disclosure, "substantially parallel" means that, when the angle between two line segments is expressed in the range of 0° to 90°, the angle between the two line segments is 0° or more and less than 30° (preferably 0° or more and 22.5° or less, more preferably 0° or more and 10° or less, even more preferably 0° or more and 5° or less, and particularly preferably 0° or more and 3° or less). In the present disclosure, the degree of orientation F of a piezoelectric body is an index showing the degree of orientation of an optically active polypeptide contained in the piezoelectric body.
[0014] (Piezoelectric substrate) The piezoelectric substrate includes an elongated internal conductor and a piezoelectric body covering the outer peripheral surface of the internal conductor. The shape of the piezoelectric substrate is not particularly limited, and may be, for example, in the form of a cord or ribbon.
[0015] The manner in which the piezoelectric body covers the outer circumferential surface of the internal conductor is not particularly limited. For example, a long piezoelectric body may be wound around the internal conductor. The shape of the long piezoelectric body is not particularly limited, and may be a thread, cord, ribbon, or other shape.
[0016] The method of winding the piezoelectric body around the internal conductor is not particularly limited. For example, the piezoelectric body may be wound spirally around the axial direction of the internal conductor, or may not be wound spirally around the axial direction of the internal conductor. From the viewpoint of improving the piezoelectric sensitivity of the piezoelectric substrate, it is preferable that the piezoelectric body is wound spirally around the axial direction of the internal conductor. The piezoelectric body may be wound so as to overlap, or may be wound so as not to overlap. From the viewpoint of piezoelectric sensitivity, it is preferable that the piezoelectric body covers the entire outer circumferential surface of the internal conductor. The piezoelectric body may be wound directly around the outer circumferential surface of the internal conductor, or may be wound indirectly (for example, with an electrical insulator or the like disposed between the internal conductor and the piezoelectric body).
[0017] In the piezoelectric substrate, when a shear stress is applied to the helically wound piezoelectric body, electric charges are easily generated, which makes it easy for the piezoelectricity to be expressed. The shear stress can be applied to the piezoelectric body by deforming the piezoelectric body. For example, the shear stress can be applied to the piezoelectric body by a first non-plastic deformation, a second non-plastic deformation, a third non-plastic deformation, or the like. The first non-plastic deformation refers to the entire helically wound piezoelectric body being stretched in the direction of the helical axis. The second non-plastic deformation refers to twisting a part of the helically wound piezoelectric body (i.e., twisting a part of the piezoelectric yarn around the helical axis). The third non-plastic deformation refers to bending a part or the whole of the helically wound piezoelectric body.
[0018] The piezoelectric body is preferably wound spirally in one direction around the internal conductor. "Spiral wound in one direction" refers to a first winding manner or a second winding manner. The first winding mode indicates that the piezoelectric yarn is wound spirally around the internal conductor so as to be left-handed (i.e., counterclockwise) from the front side to the back side when viewed from one end of the piezoelectric substrate. The second winding manner indicates that the piezoelectric body is wound in a spiral shape around the internal conductor so as to be right-handed (ie, clockwise) from the front side to the back side when viewed from one end of the piezoelectric substrate. When the piezoelectric body is wound in a spiral shape in one direction, the phenomenon in which the polarities of the generated charges cancel each other out (i.e., the phenomenon in which the piezoelectricity decreases) is suppressed, and therefore the piezoelectricity of the piezoelectric substrate is further improved.
[0019] The embodiment having a piezoelectric body in which the piezoelectric substrate is spirally wound in one direction includes not only an embodiment having only one layer made of a piezoelectric body, but also an embodiment in which multiple layers made of a piezoelectric body are stacked. An example of an embodiment in which multiple layers made of piezoelectric material are stacked on top of each other is an embodiment in which a first layer made of piezoelectric material is spirally wound in one direction, and a second layer made of piezoelectric material is stacked on top of the first layer made of piezoelectric material and spirally wound in the same direction as the first direction. An embodiment of the piezoelectric substrate may include a first layer in which a piezoelectric body is spirally wound in one direction, and a second layer in which a piezoelectric body is spirally wound in a direction different from that of the piezoelectric body in the first layer. In this embodiment, the chirality of the optically active polypeptide contained in the first layer is different from the chirality of the optically active polypeptide contained in the second layer.
[0020] When the piezoelectric body is wound helically around the internal conductor, the helix angle of the piezoelectric body is preferably 20° to 70°, more preferably 25° to 65°, and even more preferably 30° to 60°. In this disclosure, the "helical angle" refers to the angle between the axial direction of the internal conductor and the longitudinal direction of the piezoelectric body. The helical angle is measured by photographing the appearance of the piezoelectric substrate with the piezoelectric body wound helically around the internal conductor (with the external conductor removed, if the piezoelectric substrate has an external conductor, as described below) using an optical microscope. The angles are measured by image processing at five points on the observed piezoelectric substrate, excluding the portion where the angle of the piezoelectric body is extremely misaligned, and the average of the measured values is taken as the helical angle of the piezoelectric body.
[0021] The thickness of the piezoelectric body is not particularly limited, but is preferably 0.02 mm or more and 2.00 mm or less, and more preferably 0.05 mm or more and 1.00 mm or less.
[0022] The piezoelectric body includes fibers made of an optically active polypeptide. Hereinafter, the fibers made of an optically active polypeptide are also referred to as "optically active polypeptide fibers." When the piezoelectric material contains optically active polypeptide fibers, the piezoelectric substrate exhibits piezoelectricity.
[0023] The optically active polypeptide fiber may be contained in a filamentous piezoelectric material. Hereinafter, the filamentous piezoelectric material will also be referred to as "piezoelectric yarn." The piezoelectric yarn may be a twisted yarn or a non-twisted yarn. In particular, the piezoelectric yarn is preferably a twisted yarn from the viewpoint of piezoelectricity. Examples of the non-twisted yarn include a single original yarn (fiber) and an aggregate of multiple original yarns (fibers). The number of original yarns (fibers) constituting the twisted yarn is not particularly limited, and is preferably 3 to 120, and more preferably 4 to 30, from the viewpoint of ensuring the strength of the piezoelectric yarn. The fibers contained in the piezoelectric yarn may be only optically active polypeptide fibers, or a combination of optically active polypeptide fibers and fibers that are not optically active polypeptides. From the viewpoint of improving the piezoelectric sensitivity of the piezoelectric substrate, it is preferable that the fibers contained in the piezoelectric yarn are only optically active polypeptide fibers.
[0024] The twist number of the piezoelectric yarn is preferably 500 T / m or less, more preferably 300 T / m or less. When the twist number of the piezoelectric yarn is within this range, the piezoelectric yarn is less likely to break, and the piezoelectric sensitivity of the piezoelectric substrate is superior.
[0025] The thickness of the piezoelectric yarn (when the piezoelectric yarn is an assembly of multiple fibers, the thickness of the entire assembly) is not particularly limited, and is preferably 0.0001 mm to 2 mm, more preferably 0.001 mm to 1 mm, and even more preferably 0.005 mm to 0.8 mm. When the piezoelectric yarn is a single original yarn or an assembly of multiple original yarns, the fineness of each original yarn is preferably 0.01 denier to 10,000 denier, more preferably 0.1 denier to 1,000 denier, and even more preferably 1 denier to 100 denier.
[0026] The piezoelectric yarn may be in the form of an aggregate of a plurality of piezoelectric yarns. The aggregate of a plurality of piezoelectric yarns may be in the form of a cord, a ribbon, etc. The aggregate of a plurality of piezoelectric yarns may be in the form of a bond between the piezoelectric yarns by a resin or the like.
[0027] The optically active polypeptide fiber is preferably a long fiber, in which case the shear stress applied to the piezoelectric substrate is easily transmitted to the piezoelectric substrate, resulting in excellent piezoelectric sensitivity. In the present disclosure, the term "long fiber" refers to a fiber having a length that allows it to be wound continuously from one end to the other end in the longitudinal direction of a piezoelectric substrate. Examples of long fiber optically active polypeptide fibers include silk, wool, mohair, cashmere, camel, llama, alpaca, vicuna, angora, and spider silk. Among these, silk and spider silk are preferred from the viewpoint of piezoelectricity.
[0028] In the present disclosure, the degree of orientation F of the optically active polypeptide fiber is within the range of 0.50 or more and less than 1.00. When the degree of orientation F of the optically active polypeptide fiber is 0.50 or more, the piezoelectric property of the piezoelectric substrate is good.When the degree of orientation F of the optically active polypeptide fiber is less than 1.00, the productivity of the piezoelectric substrate is good. The degree of orientation F of the optically active polypeptide fiber is preferably 0.50 or more and 0.99 or less, more preferably 0.70 or more and 0.98 or less, and even more preferably 0.80 or more and 0.97 or less. An orientation degree F of an optically active polypeptide fiber of 1.00 indicates that the main orientation direction of the optically active polypeptide contained in the optically active polypeptide fiber is parallel to the length direction of the optically active polypeptide fiber. Furthermore, an orientation degree F of an optically active polypeptide fiber of 0.80 or more and less than 1.00 indicates that the main orientation direction of the optically active polypeptide contained in the optically active polypeptide fiber is approximately parallel to the length direction of the optically active polypeptide fiber. The degree of orientation F of an optically active polypeptide fiber is determined by fixing a sample (piezoelectric body) to a sample holder, measuring the azimuth angle distribution intensity near the peak due to orientation (for example, near 2θ=20° in the case of silk) from X-ray diffraction measurement, and calculating using the following formula (a), and means the degree of c-axis orientation. Orientation degree F=(180°-α) / 180° … Formula (a) [In formula (a), α represents the half-width (°) of the peak due to the orientation.]
[0029] In the present disclosure, it is preferable that the length direction of the piezoelectric body and the main orientation direction of the optically active polypeptide contained in the piezoelectric body are approximately parallel. When the length direction of the piezoelectric body is approximately parallel to the main orientation direction of the optically active polypeptide contained in the piezoelectric body, the piezoelectric properties of the piezoelectric substrate are well expressed. Furthermore, since the length direction of the piezoelectric body and the main orientation direction of the optically active polypeptide contained in the piezoelectric body are approximately parallel, the piezoelectric body has excellent tensile strength in the length direction and is less likely to break. When the piezoelectric body is in the form of a piezoelectric thread containing optically active polypeptide fibers (e.g., silk or spider silk), during the process of production of the silk or spider silk, the length direction of the piezoelectric body becomes approximately parallel to the main orientation direction of the optically active polypeptide (e.g., fibroin or spider silk protein) contained in the piezoelectric body. The fact that the length direction of the piezoelectric body and the main orientation direction of the optically active polypeptide contained in the piezoelectric body are approximately parallel can be confirmed by comparing the installation direction of the sample (piezoelectric body) and the azimuth angle of the crystal peak in X-ray diffraction measurement. An example of a method for making the length direction of a piezoelectric body approximately parallel to the main orientation direction of an optically active polypeptide contained in the piezoelectric body is to form a piezoelectric body using optically active polypeptide fibers having an orientation degree F of 0.80 or more and less than 1.00. Specifically, a method for using a twisted yarn made from optically active polypeptide fibers having an orientation degree F of 0.80 or more and less than 1.00 as the piezoelectric body is exemplified.
[0030] From the viewpoints of the piezoelectricity and strength of the piezoelectric body, the optically active polypeptide fiber is preferably made of an optically active polypeptide having a β-sheet structure.
[0031] Examples of optically active polypeptides having a β-sheet structure include optically active animal proteins and optically active synthetic proteins. Examples of optically active animal proteins include fibroin, spider silk protein, sericin, collagen, keratin, elastin, etc. As the spider silk protein, the spider silk protein described in Patent Document 1 can be used. As the spider silk protein, artificial spider silk obtained by an artificial synthesis method can be used. In particular, the optically active polypeptide preferably contains at least one of fibroin and spider silk protein, and more preferably contains fibroin. Examples of synthetic proteins having optical activity include synthetic spider silk (e.g., "QMONOS (registered trademark)", synthetic bagworm silk, synthetic proteins (e.g., "Brewed Protein (registered trademark)", etc.). The form of the synthetic protein having optical activity is preferably thread-like. Thread-like fibers containing the above synthetic proteins can also be obtained from threads or clothing containing "Brewed Protein (registered trademark)".
[0032] Examples of fibers made of optically active polypeptides having a β-sheet structure include fibers made of optically active animal proteins, such as silk, wool, mohair, cashmere, camel, llama, alpaca, vicuna, angora, and spider silk. Among these, from the viewpoint of piezoelectricity, the optically active polypeptide fiber preferably contains at least one of silk and spider silk, more preferably consists of at least one of silk and spider silk, and particularly preferably consists of silk.
[0033] Examples of silk include raw silk, refined silk, regenerated silk, and fluorescent silk. As the silk, raw silk or refined silk is preferred, and refined silk is particularly preferred. "Refined silk" refers to silk that has had sericin removed from raw silk, which has a double structure of sericin and fibroin. "Refining" refers to the process of removing sericin from raw silk. Raw silk is a dull white color, but by removing sericin from raw silk (i.e., refining), the color changes from dull white to a lustrous silvery white. Refining also enhances the silk's soft texture.
[0034] When covering the outer periphery of the internal conductor with the piezoelectric body, an adhesive may be used. By using an adhesive, the state in which the piezoelectric body covers the outer periphery of the internal conductor is maintained favorably. As a result, when external stress is applied to the piezoelectric substrate, shear stress caused by the external stress is more likely to act on the piezoelectric yarn.
[0035] Specific examples of adhesives include epoxy-based adhesives, urethane-based adhesives, vinyl acetate resin-based emulsion-type adhesives, ethylene vinyl acetate-based emulsion-type adhesives, acrylic resin-based emulsion-type adhesives, styrene butadiene rubber-based latex-type adhesives, silicone resin-based adhesives, α-olefin-based adhesives, vinyl chloride resin-based solvent-type adhesives, rubber-based adhesives, elastic adhesives, chloroprene rubber-based solvent-type adhesives, nitrile rubber-based solvent-type adhesives, and cyanoacrylate-based adhesives.
[0036] (inner conductor) The piezoelectric substrate includes an elongated inner conductor. The inner conductor functions as the core of the piezoelectric substrate. The internal conductor is preferably a good electrical conductor, such as copper wire, aluminum wire, SUS (Steel Use Stainless) wire, metal wire coated with an insulating film, carbon fiber, resin fiber integrated with carbon fiber, tinsel wire, organic conductive material, etc. The tinsel wire is formed by spirally winding copper foil around a fiber. The outer diameter of the fiber is appropriately adjusted according to the desired characteristics of the piezoelectric substrate, and is preferably 0.1 mm or more and 10 mm or less. Among these, the internal conductor is preferably made of tinsel wire or carbon fiber from the viewpoints of improving the piezoelectric sensitivity and stability of the piezoelectric output and imparting high flexibility, and in particular, tinsel wire is preferable from the viewpoint of low electrical resistance.
[0037] (Outer conductor) From the viewpoint of improving piezoelectric sensitivity and electrostatic shielding properties, the piezoelectric substrate preferably further includes an external conductor. The outer conductor is disposed on the outer periphery of the piezoelectric body, and the inner conductor and the outer conductor are not electrically connected to each other.
[0038] The outer conductor serves as a companion conductor to the inner conductor, for example, to detect electrical signals from the piezoelectric substrate. The external conductor may be disposed on a portion of the outer circumferential surface of the piezoelectric layer, or may be disposed on the entire outer circumferential surface of the piezoelectric layer.
[0039] The outer conductor may or may not be fixed to the piezoelectric body.
[0040] The external conductor is formed, for example, by winding a long conductor around the outer periphery of the piezoelectric body. The cross-sectional shape of the long-sized conductor may be, for example, a circular shape, an elliptical shape, a rectangular shape, an irregular shape, etc. Among these, from the viewpoint of closely adhering to the piezoelectric substrate in a plane and improving the piezoelectric sensitivity of the piezoelectric substrate, the cross-sectional shape of the long-sized conductor is preferably a rectangular shape. The material of the long conductor is not particularly limited, and the following are main examples depending on the cross-sectional shape: Examples of long conductors having a rectangular cross section include copper foil ribbons and aluminum foil ribbons which are formed by rolling copper wires having a circular cross section into a flat plate. Examples of long conductors having a circular cross section include copper wire, aluminum wire, SUS wire, metal wire coated with an insulating film, carbon fiber, resin fiber integrated with carbon fiber, and tinsel wire in which copper foil is spirally wound around fiber. The long conductor may be an organic conductive material coated with an insulating material. Methods for winding a long conductor include, for example, a method of spirally winding copper foil or the like around a piezoelectric substrate, a method of braiding copper wire or the like into a tubular shape and wrapping the piezoelectric substrate, and a method of enclosing the piezoelectric substrate in a cylindrical shape.
[0041] (Waterproof coating) The piezoelectric substrate is provided with a waterproof coating that covers the outer periphery of the piezoelectric body. The waterproof coating may directly cover the outer circumferential surface of the piezoelectric body, or may cover it indirectly (for example, with an external conductor disposed between the piezoelectric body and the waterproof coating).
[0042] The material of the waterproof coating is not particularly limited, but is preferably a material that exhibits waterproofness and electrical insulation properties, such as resin. Suitable resins for use in waterproof coatings include polyvinyl chloride resin, polyethylene resin, polypropylene resin, ethylene-tetrafluoroethylene copolymer (ETFE), tetrafluoroethylene-hexafluoropropylene copolymer (FEP), polytetrafluoroethylene resin (PTFE), tetrafluoroethylene-perfluoropropyl vinyl ether copolymer (PFA), fluororubber, polyester resin, polyimide resin, polyamide resin, polyethylene terephthalate resin (PET), rubber (including elastomers), and the like. Among the above resins, tetrafluoroethylene-hexafluoropropylene copolymer (FEP), tetrafluoroethylene-perfluoropropyl vinyl ether copolymer (PFA) and ethylene-tetrafluoroethylene copolymer (ETFE) are preferred from the viewpoint of waterproofing.
[0043] The waterproof coating may be formed from a molten resin or in another state, for example, by winding a strip of waterproof coating material in a spiral shape along the length of the piezoelectric substrate. From the viewpoint of waterproofing, the waterproof coating is preferably in a state formed from a molten resin, and more preferably in a state formed by extrusion molding using a molten resin.
[0044] The thickness of the waterproof coating (if the thickness is not constant, the minimum thickness) is not particularly limited. From the viewpoint of ensuring sufficient waterproofness, the thickness of the waterproof coating is preferably 2 μm or more, more preferably 10 μm or more, and even more preferably 25 μm or more. From the viewpoint of ensuring sufficient piezoelectric sensitivity, the thickness of the waterproof coating is preferably 500 μm or less, more preferably 100 μm or less, and even more preferably 50 μm or less.
[0045] The waterproof coating may consist of one layer or two or more layers. If the waterproofing coating consists of two or more layers, the materials of each layer may be the same or different.
[0046] The waterproof coating may function as an outer electrical insulator (hereinafter referred to as "first insulator"). The first insulator is disposed on the outermost periphery of the piezoelectric substrate. In other words, at least a part of the outer periphery of the piezoelectric substrate may be constituted by the first insulator. It is preferable that the first insulator covers the entire outermost periphery of the piezoelectric substrate. In other words, it is preferable that the entire outer periphery of the piezoelectric substrate is composed of the first insulator. This makes it possible to electrostatically shield the internal conductor. As a result, it is possible to suppress changes in piezoelectric sensitivity caused by external static electricity.
[0047] When the piezoelectric substrate includes an external conductor, it may further include an inner electrical insulator (hereinafter referred to as a "second insulator"), for example, disposed between the piezoelectric body and the internal conductor and / or between the piezoelectric body and the external conductor. This can further prevent short circuits from occurring between the internal conductor and the external conductor, or between the piezoelectric body and the external conductor. The second insulator is formed, for example, by winding a long insulator in a spiral shape around the outer circumferential surface of the outer conductor, or by extrusion molding using a molten insulator. Examples of materials for the second insulator include the same materials as those exemplified as the materials for the first insulator.
[0048] (Functional layer) The piezoelectric substrate may further include a functional layer, such as an easy-adhesion layer, a hard coat layer, a refractive index adjustment layer, an antireflection layer, an antiglare layer, an easy-slip layer, an antiblock layer, a protective layer, an antistatic layer, a heat dissipation layer, an ultraviolet absorbing layer, an anti-Newton ring layer, a light scattering layer, a polarizing layer, a gas barrier layer, a hue adjustment layer, an electrode layer, and the like. The piezoelectric substrate may include only one type of functional layer, or two or more types of functional layers. The material of the functional layer is appropriately selected depending on the function required for the functional layer, and examples thereof include inorganic substances such as metals and metal oxides, organic substances such as resins, composite compositions containing resins and fine particles, etc. Examples of the resin include cured products obtained by curing with temperature or active energy rays.
[0049] (Wiring materials) The piezoelectric substrate may further include a wiring member electrically connected to the internal conductor. When the piezoelectric substrate includes an external conductor, the piezoelectric substrate may further include a wiring member electrically connected to the external conductor.
[0050] The form of the wiring member is not particularly limited as long as it can be electrically connected to the internal conductor of the piezoelectric substrate. The wiring member may be, for example, a coaxial cable including a long internal conductor, a dielectric insulating layer disposed around the internal conductor, and an external conductor disposed around the dielectric insulating layer. When the wiring member is a coaxial cable, the inner conductor of the coaxial cable and the inner conductor of the piezoelectric substrate may be electrically connected, and the outer conductor of the piezoelectric substrate may be electrically connected to the outer conductor of the coaxial cable.
[0051] (Example of the structure of the piezoelectric substrate) Specific examples of the configuration of the piezoelectric substrate will be described below with reference to the drawings, but the present disclosure is not limited to the following specific examples. For ease of explanation, the waterproof coating is omitted in the following drawings.
[0052] Fig. 1A is a schematic side view illustrating the appearance of a piezoelectric substrate 10A according to an embodiment of the present disclosure, and Fig. 1B is a cross-sectional view taken along line IB-IB of Fig. 1A.
[0053] 1A, the piezoelectric substrate 10A includes an elongated internal conductor 12A and a piezoelectric layer 14A. The piezoelectric layer 14A is spirally wound in one direction along the outer circumferential surface of the internal conductor 12A from one end to the other end at a helix angle β1 without any gaps. The piezoelectric layer 14A is formed by winding a piezoelectric yarn 140A counterclockwise around the outer circumferential surface of the internal conductor 12A. The piezoelectric yarn 140A includes an optically active polypeptide fiber. In FIG. 1A, helix angle β1 is the angle between the direction of helix axis G1 (the axial direction of internal conductor 12A) and the length direction of piezoelectric yarn 140A in side view. 1A, the double-headed arrow E1 indicates the main orientation direction of the optically active polypeptide contained in the piezoelectric layer 14A. That is, the main orientation direction of the optically active polypeptide contained in the piezoelectric yarn 140A is approximately parallel to the length direction of the piezoelectric yarn 140A.
[0054] The effects of the piezoelectric substrate 10A will be described below. For example, when tension is applied in the longitudinal direction of the piezoelectric substrate 10A, a shear stress is applied to the optically active polypeptide contained in the piezoelectric layer 14A, and the optically active polypeptide is polarized. This polarization of the optically active polypeptide is thought to occur in phase with the radial direction of the piezoelectric substrate 10A, as shown by the arrows in Figure 1B. This causes the piezoelectricity of the piezoelectric substrate 10A to be expressed.
[0055] FIG. 2 is a schematic side view showing the appearance of a piezoelectric substrate 20A according to an embodiment of the present disclosure. The piezoelectric substrate 20A differs from the piezoelectric substrate 10A shown in FIG. 1A in that, in addition to the internal conductor 12A and the piezoelectric layer 14A, the piezoelectric substrate 20A includes an external conductor 22A disposed around the piezoelectric layer 14A.
[0056] 2, the piezoelectric substrate 20A includes an internal conductor 12A, a piezoelectric layer 14A, and an external conductor 22A. The external conductor 22A is disposed on the outer periphery side of the piezoelectric layer 14A. The external conductor 22A is formed by spirally winding a long conductor (e.g., copper foil) around the piezoelectric layer 14A.
[0057] As shown in Fig. 2, in the piezoelectric substrate 20A, the end of the piezoelectric layer 14A is misaligned with the end of the external conductor 22A. This electrically insulates the internal conductor 12A from the external conductor 22A. However, the method of electrically insulating the internal conductor 12A from the external conductor 22A in the present disclosure is not limited to the configuration shown in Fig. 2.
[0058] Since the piezoelectric substrate 20A includes the internal conductor 12A, an electrical signal (voltage signal or charge signal) generated in the piezoelectric layer 14A can be more easily extracted via the internal conductor 12A. Furthermore, since the piezoelectric substrate 20A includes the external conductor 22A, the inside of the piezoelectric substrate 20A (the piezoelectric layer 14A and the internal conductor 12A) can be electrostatically shielded by the external conductor 22A. This makes it possible to suppress voltage changes in the internal conductor 12A caused by static electricity outside the piezoelectric substrate 20A, resulting in more stable piezoelectricity.
[0059] (Applications of piezoelectric substrates) The applications of the piezoelectric substrate are not particularly limited, and examples thereof include sensors, actuators, energy harvesters, and bioinformation acquisition devices. That is, embodiments of the present disclosure include sensors, actuators, energy harvesters, and biometric acquisition devices that include the piezoelectric substrates of the present disclosure. Specific examples of sensors include force sensors, pressure sensors, displacement sensors, deformation sensors, motion sensors, vibration sensors, impact sensors, and ultrasonic sensors.
[0060] The bioinformation acquisition device detects the biosignals of a human subject or animal subject (hereinafter, collectively referred to as "subject") using a piezoelectric substrate to acquire the bioinformation of the subject. The biosignals include presence / absence, body movement, pulse wave signal (heart rate signal), respiratory signal, body movement signal, ballistocardiogram, biotremor, etc. Biotremor means rhythmic involuntary movement of a body part (fingers, hand, forearm, upper limb, etc.). The detection of ballistocardiogram also includes the detection of the force effect due to the cardiac function of the body. That is, when the heart pumps blood into the aorta and pulmonary artery, the body experiences a recoil force in the opposite direction to the blood flow. The magnitude and direction of this recoil force change with the functional stage of the heart. This recoil force is detected by sensing the ballistocardiogram outside the body.
[0061] The article to which the biometric information acquisition device is applied is not particularly limited. For example, the biometric information acquisition device may be applied to an article that the subject comes into contact with, such as a seat, a steering wheel, a seat, a seat belt, a shift knob, an armrest, a headrest, a handle, etc. Alternatively, the biometric information acquisition device may be applied to an article that the subject wears, such as clothing, a hat, a wristwatch, etc. The bioinformation acquisition device of the present disclosure is preferably used as a detection unit of an information processing device. The information processing device acquires a biosignal of a subject from the bioinformation acquisition device, and detects abnormalities or abnormal physical conditions of the subject based on the acquired biosignal. The information processing device may utilize artificial intelligence (AI).
[0062] Hereinafter, the embodiments of the present invention will be described in detail with reference to examples. However, the present invention is not limited to the description of these examples.
[0063] [Example 1] (Preparation of piezoelectric yarn) As the optically active polypeptide fiber, 21 denier raw silk was prepared. Raw silk is a long fiber made of optically active polypeptide. The thickness of the raw silk was 0.06 mm to 0.04 mm. The raw silk described above was twisted into six strands (twist number 150 T / m) by a known method, and the resulting yarn was refined to produce a piezoelectric yarn made of refined silk.
[0064] Using a wide-angle X-ray diffraction device (Rigaku's "RINT2550", accessories: rotating sample stage, X-ray source: CuKα, output: 40kV 370mA, detector: scintillation counter), the piezoelectric yarn was fixed to a holder and the azimuthal distribution intensity of the crystal plane peak [2θ=20°] was measured. In the obtained azimuth angle distribution curve (X-ray interference diagram), the degree of orientation F (c-axis orientation) of the optically active polypeptide fiber contained in the piezoelectric yarn was calculated from the half-width (α) of the peak according to the following formula (a). The result was 0.86. Orientation degree (F)=(180°-α) / 180° … (a) (α is the half-width of the peak due to the orientation)
[0065] Since the orientation degree F of the optically active polypeptide fibers contained in the piezoelectric yarn was 0.86 and six-strand single-twisted yarn (piezoelectric yarn) was produced using refined silk, it can be evaluated that the length direction of the piezoelectric yarn and the main orientation direction of the optically active polypeptide contained in the piezoelectric yarn are approximately parallel.
[0066] (Preparation of piezoelectric substrate) As the internal conductor, a tinsel wire "U24-01-00" (wire diameter 0.26 mm, length 200 m) manufactured by Meisei Sangyo Co., Ltd. was prepared. A layer of piezoelectric yarn (piezoelectric yarn layer) was formed on the outer periphery of the internal conductor by winding the piezoelectric yarn counterclockwise so that the helix angle was about 45°. The formed piezoelectric yarn layer covered the entire outer periphery of the internal conductor. In other words, the outer periphery of the internal conductor was not exposed. An adhesive called "901H3" (a cyanoacrylate adhesive) manufactured by Toagosei Co., Ltd. was dropped onto the outer periphery of the piezoelectric yarn layer and allowed to soak into the interior of the piezoelectric yarn layer. After that, the excess adhesive was immediately wiped off from the outer periphery of the piezoelectric yarn with a Kimwipe, and the adhesive was allowed to harden at room temperature.
[0067] A rolled copper foil ribbon with a rectangular cross section (width: 0.3 mm, thickness: 30 μm) was prepared as the external conductor. This rolled copper foil ribbon was wound clockwise around the outer peripheral surface of the piezoelectric thread layer to form an external conductor on the outer peripheral surface of the piezoelectric thread layer. The external conductor covered the entire outer peripheral surface of the piezoelectric thread layer. In other words, the outer peripheral surface of the piezoelectric thread layer was not exposed.
[0068] The piezoelectric substrate on which the external conductor was formed was wound around an aluminum bobbin and dried under reduced pressure for 6 hours in a vacuum oven at 125° C. After that, the piezoelectric substrate was taken out of the vacuum oven and immediately placed in an aluminum foil moisture-proof pack while still wound around the bobbin and stored.
[0069] After drying under reduced pressure, a portion of the piezoelectric substrate was cut into a length of approximately 0.2 g to prepare a measurement sample, and the moisture content was measured at a heating temperature of 150°C using Karl Fischer coulometric titration. From the measurement results, the amount of moisture contained per 1 m of the piezoelectric substrate was calculated, which was 0.16 mg.
[0070] A waterproof coating was formed on the outer periphery of the external conductor of the piezoelectric substrate taken out of the aluminum foil moisture-proof pack using tetrafluoroethylene-hexafluoropropylene copolymer (FEP) (AGC: NP-101). Specifically, a waterproof coating with a thickness of approximately 130 μm was formed by passing the material through a die for normal molten resin coating from an extrusion molding machine. When the formed waterproof coating was observed under an electron microscope, no significant bubbles were found.
[0071] (Measurement of piezoelectric sensitivity) The initial value of the piezoelectric sensitivity was measured using the prepared piezoelectric substrate. Specifically, both ends of the piezoelectric substrate were fixed to a tensile testing machine (distance between chucks: 150 mm), and a stress ranging from 1.0 N to 2.0 N was repeatedly applied in a triangular wave shape at 0.5 Hz periodically. The amount of charge generated on the front and back of the piezoelectric substrate was measured using an electrometer (Keithley's programmable electric meter "617"). The amount of generated charge per unit tensile force was calculated from the slope of the correlation line of the scatter plot with the measured amount of generated charge Q [C] on the Y axis and the tensile force F [N] of the piezoelectric substrate on the X axis, and this was used as the initial value of the piezoelectric sensitivity. The result was 2.5 pC / N mm.
[0072] (High temperature and humidity storage test) The piezoelectric substrate was cut to a length of 1m, and a hot melt medium-volume glue gun (SANYO Life Material's "TEC806-12") was used to form a resin part around the end, which was the cut surface of the piezoelectric substrate, using polyolefin resin (SANYO Life Material's "912K"). By forming the resin part so that the distance from the surface of the resin part to the end of the piezoelectric substrate was 5mm to 10mm, the infiltration of moisture from outside the resin part to the end was suppressed. Next, the piezoelectric substrate with the sealed ends was placed in a constant temperature and humidity chamber ("IG-420" manufactured by Yamato Scientific) set to an environment of 85°C temperature and 85%rh humidity to conduct a constant temperature and humidity test. At this time, of the 1m length of the piezoelectric substrate with the sealed ends, approximately 25cm portions from the midpoint to both ends were placed inside the constant temperature chamber, and the piezoelectric substrate was fixed so that the 25cm portions from both ends to the midpoint could be exposed outside the constant temperature chamber through the cable hole or open door. After placing it in a thermo-hygrostat at 85°C and 85% RH for 24 hours, the amount of generated charge (piezoelectric sensitivity) was measured using only the 50 cm section placed in the thermo-hygrostat. The time from removing the piezoelectric substrate from the thermo-hygrostat to measuring the amount of generated charge was between 30 minutes and 1 hour in an environment of 23°C and 50% RH. The result was 2.0 pC / N mm, indicating that sufficient sensitivity was maintained.
[0073] [Comparative Example 1] The piezoelectric substrate on which the external conductor was formed in Example 1 was wound around a bobbin and left in a normal environment for 3 days. Thereafter, the amount of moisture contained per square meter of the piezoelectric substrate was measured in the same manner as in Example 1. The result was 3.6 mg. Thereafter, a waterproof coating was formed on the outer periphery of the external conductor of the piezoelectric substrate using a tetrafluoroethylene-hexafluoropropylene copolymer (FEP) in the same manner as in Example 1. When the formed waterproof coating was observed under an electron microscope, a large number of air bubbles were generated, and some of the coating was cracked, indicating that the coating did not provide sufficient waterproofing. For this reason, a high-temperature, high-humidity storage test was not performed in Comparative Example 1.
Claims
1. A long inner conductor; a piezoelectric body covering an outer circumferential surface of the internal conductor; A piezoelectric substrate comprising a waterproof coating covering an outer peripheral surface of the piezoelectric body, The amount of moisture contained per 1 m of the piezoelectric substrate is 2 mg or less, The piezoelectric body includes fibers made of an optically active polypeptide, the length direction of the piezoelectric body is approximately parallel to the main orientation direction of the optically active polypeptide; A piezoelectric substrate, wherein the degree of orientation F of the fibers made of the optically active polypeptide, as determined by X-ray diffraction measurement using the following formula (a), is 0.50 or more and less than 1.
00. Orientation degree F=(180°-α) / 180°...Formula (a) [In formula (a), α represents the half-width (°) of the peak due to the orientation.]
2. The piezoelectric substrate of claim 1 , wherein the waterproof coating comprises a resin.
3. The piezoelectric substrate of claim 1 , further comprising an outer conductor disposed between the piezoelectric body and the waterproof coating, the outer conductor being electrically insulated from the inner conductor.
4. The piezoelectric substrate according to claim 1 , wherein the piezoelectric element is an elongated piezoelectric element.
5. The piezoelectric substrate according to claim 4 , wherein the long piezoelectric element is wound in a spiral shape around an outer circumferential surface of the internal conductor.
6. 5. The piezoelectric substrate according to claim 4, wherein a helical angle between an axial direction of the internal conductor and a longitudinal direction of the elongated piezoelectric body is 20° to 70°.
7. The piezoelectric substrate according to claim 1 , wherein the optically active polypeptide has a β-sheet structure.
8. The piezoelectric substrate of claim 1 , wherein the optically active polypeptide comprises fibroin.
9. The piezoelectric substrate according to claim 1 , wherein the fiber made of the optically active polypeptide is silk.
10. The piezoelectric substrate according to claim 1 , wherein the piezoelectric body is a thread-like piezoelectric body, and the twist number of the thread-like piezoelectric body is 500 T / m or less.
11. A sensor comprising the piezoelectric substrate according to any one of claims 1 to 10.
12. An actuator comprising the piezoelectric substrate according to any one of claims 1 to 10.
13. A bioinformation acquisition device comprising the piezoelectric substrate according to any one of claims 1 to 10.
Citation Information
Patent Citations
Piezoelectric base material, sensor, actuator, biological information acquisition device, and piezoelectric fiber structure
EP3534419A1
Piezoelectric actuator element
JP1992155876A
Piezoelectric actuator, its manufacturing process, ink jet head, and ink jet recorder
JP2004025474A
Polymer piezoelectric material, manufacturing method thereof and composition for polymer piezoelectric material
JP2014086703A
Piezoelectric actuator and method of manufacture therefor, and ink jet head and ink jet type recording device
US20030234834A1