Decorative plate
The decorative board with a resin-impregnated surface protection layer using isocyanate and blocked isocyanate addresses resin leakage and stain resistance issues, enhancing dimensional stability and productivity.
Patent Information
- Application Number
- JP2023047633
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-03-24
AI Technical Summary
Existing decorative laminates face issues with resin leakage contaminating manufacturing equipment, poor stain resistance, and inadequate dimensional stability, particularly when used in flooring applications.
A decorative board comprising a core layer, decorative layer, and surface protection layer, where the surface protection layer is impregnated with a resin containing isocyanate and blocked isocyanate, which suppresses resin leakage and enhances dimensional stability.
The solution effectively prevents equipment contamination, improves stain resistance, and enhances dimensional stability, particularly in flooring applications, while reducing resin and filler usage for improved productivity and cost-effectiveness.
Smart Images

Figure 2024136499000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a decorative board. [Background technology]
[0002] Thermosetting resin decorative panels are available in a wide range of colors and patterns, and have excellent physical and chemical properties such as impact resistance, flexural strength, and stain resistance, as well as ease of maintenance, so they are used in a wide range of applications, from furniture and fixtures in public facilities such as stores and medical and welfare facilities to residential furniture.
[0003] In general, thermosetting resin decorative boards can be manufactured by laminating a decorative layer, a core layer, etc., and thermocompressing them. The decorative layer can be manufactured by using resin-impregnated decorative paper made by impregnating a fibrous base material with a resin liquid containing a thermosetting resin such as melamine resin and drying it, and the core layer can be manufactured by using one or more prepregs made by impregnating a fibrous base material with a resin liquid containing a binder resin (e.g., phenolic resin) and drying it. In addition, a backing layer and a surface protective layer are provided as necessary.
[0004] In the past, the applicant invented a decorative laminated material with excellent cushioning properties and high flexibility. Specifically, the decorative laminated material was obtained by sequentially laminating a resin-impregnated core paper impregnated with a mixed resin liquid containing unsaturated polyester resin and melamine resin as essential components on a base layer of a polyvinyl chloride resin sheet, a resin-impregnated decorative paper impregnated with a resin liquid containing melamine resin as the main component, and a resin-impregnated surface paper (Patent Document 1). This decorative laminated material was capable of absorbing shocks when walking or when a heavy object was dropped, had good bending properties at room temperature, and had high adhesion to the surface layer. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 09-300553
[0006] Generally, when manufacturing decorative boards, they are sandwiched between plates for thermo-compression molding, but depending on the type of resin liquid impregnated, the resin may seep out and contaminate the plates, affecting the productivity of the decorative board. Furthermore, because decorative boards are used as surface materials for furniture and fixtures, they also need to be resistant to contamination by chemicals contained in everyday products.
[0007] In addition, as described in Patent Document 1, a method is known for using a decorative board as a flooring material by laminating a decorative board as a surface material using, for example, a vinyl chloride resin sheet as a base layer, as described in Patent Document 1. Here, the decorative laminate described in Patent Document 1 has excellent impact resistance, but tends to be somewhat lacking in dimensional stability. In particular, when using a decorative board for flooring, the thickness is made as thin as possible, so there is a tendency for the influence of dimensional changes to be greater. Therefore, the decorative board may expand and contract depending on the temperature and humidity at the construction site, which may lead to workability during construction and defects after construction, and there is room for improvement. Summary of the Invention [Problem to be solved by the invention]
[0008] The problem to be solved by the present invention is to provide a decorative board in which contamination of the facing board is suppressed, contamination resistance to chemical substances is good, and dimensional stability is improved. [Means for solving the problem]
[0009] The present invention provides a decorative board comprising a core layer, a decorative layer, and a surface protective layer, the surface protective layer including a resin-impregnated surface paper, the resin-impregnated surface paper being formed by impregnating a fibrous base material with a resin liquid including a thermosetting resin and a blocked isocyanate, and then drying the resin liquid. Effect of the Invention
[0010] The decorative board according to the present invention has the advantages of suppressing contamination of the front board, providing good resistance to contamination by chemical substances, and improving dimensional stability. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] <Decorative board> The decorative board according to the present invention includes a core layer, a decorative layer, and a surface protective layer. A manufacturing example thereof includes a method in which the decorative layer and the surface protective layer are laminated in this order with the core layer as the bottom layer, and then sandwiched between hot press plates for hot press molding, and hot press molding is performed under conditions of a temperature of 120 to 160°C, a pressure of 2 to 10 MPa, and a time of about 30 minutes to 3 hours.
[0012] (Core layer) The decorative board according to the present invention includes a core layer, which is made of one or more prepregs made by impregnating a fibrous base material with a resin liquid containing a binder resin and the like and then drying the prepreg.
[0013] Examples of the fibrous base material include organic fiber base materials and inorganic fiber base materials.
[0014] As the organic fiber substrate, it is preferable to use wood pulp fibers because the biomass ratio is improved, and examples thereof include paper made from bleached or unbleached kraft pulp of softwood or hardwood, sulfite pulp, other wood pulps, etc., either alone or in combination. Other examples include fibers made from polyethylene, polypropylene, vinylon, polyvinyl chloride, polyvinylidene chloride, polyacrylonitrile, polyamide, polyester, polyurethane, and modified products thereof, as well as fibers made from various copolymers such as ethylene-vinyl acetate copolymers, and composite fibers made from mixtures of these.
[0015] Examples of inorganic fiber substrates include nonwoven fabrics and woven fabrics containing glass fiber, rock wool, carbon fiber, and the like.
[0016] In the case of inorganic fiber substrates, the flame retardancy of the decorative board is improved compared to organic fiber substrates, and therefore it is suitable for use. In particular, when nonwoven fabrics or woven fabrics containing glass fibers are used, the heat resistance, flame resistance, and resin liquid impregnation property tend to be further improved.
[0017] The basis weight of the fibrous base material is 30 to 400 g / m2, taking into consideration the strength and impregnation efficiency of the decorative board. 2 It is preferable that the thickness is 50 to 350 g / m 2 By keeping the thickness within these ranges, the smoothness of the core layer is improved, so that the appearance of the decorative sheet is good, and the impregnation of the resin liquid tends to be improved.
[0018] The resin liquid contains a binder resin such as an acrylic resin emulsion, an amino-formaldehyde resin, or a phenol-formaldehyde resin, as well as a filler and additives.
[0019] As the acrylic resin emulsion, for example, an acrylic resin emulsion having a glass transition temperature (Tg) of -20°C or higher is preferably used because it improves adhesion and moldability. Among them, for example, fine particles having an average particle size of about 20 to 600 nm are more preferable because they have excellent smoothness and can improve adhesion to the decorative layer described below and bending workability of the decorative sheet. The average particle size is a measurement based on scattered light detected during laser irradiation using a laser light diffraction / scattering type particle size measuring device (product name: ELS-8000, manufactured by Otsuka Electronics Co., Ltd.).
[0020] The acrylic resin emulsion can be obtained by emulsion polymerization or suspension polymerization in an aqueous solution using a (meth)acrylic acid ester as the main monomer. Examples of the monomers used include methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, butyl (meth)acrylate, and hydroxyethyl (meth)acrylate. In addition to these monomers, other copolymerizable monomers or polyfunctional monomers may be copolymerized.
[0021] Examples of the amino-formaldehyde resin include initial condensates obtained by reacting an amino compound with an aldehyde compound, and modified products thereof.
[0022] Examples of the amino compounds include melamine, urea, ethylene urea, urea derivatives, benzoguanamine, and acetoguanamine. Examples of the aldehyde compounds include formaldehyde, paraformaldehyde, trioxane, acetaldehyde, paraldehyde, glyoxal, hexamethylenetetramine, phenylacetaldehyde, o-tolualdehyde, and benzaldehyde.
[0023] It can also be etherified with a lower alcohol such as methyl alcohol, ethyl alcohol, or butyl alcohol, or modified with a reactive modifier such as paratoluenesulfonamide that promotes plasticization.
[0024] Among these, melamine-formaldehyde resins are preferably used because of their excellent heat resistance and abrasion resistance.
[0025] Examples of phenol-formaldehyde resins include condensates obtained by reacting a phenolic compound with an aldehyde compound in the presence of an acidic or basic catalyst, and modified products thereof.
[0026] Examples of the phenol-based compounds include phenol, cresol, xylenol, octylphenol, phenylphenol, bisphenol A, bisphenol S, and bisphenol F, and examples of the aldehyde-based compounds include the compounds mentioned above.
[0027] In addition, the resin may be modified with a reactive modifier that promotes plasticization, such as urea, ethylene urea, urea derivatives, paratoluenesulfonamide, tung oil, phosphates, and glycols.
[0028] Examples of acidic catalysts used in the synthesis of phenol-aldehyde resins include arylsulfonic acid, paratoluenesulfonic acid, hydrochloric acid, sulfuric acid, nitric acid, adipic acid, succinic acid, phosphoric acid, boric acid, acetic acid, formic acid, oxalic acid, etc. Examples of basic catalysts include hydroxides of alkali metals and alkaline earth metals, amines such as triethylamine and triethanolamine, and ammonia.
[0029] Furthermore, the resin liquid may contain a filler, which is mainly an inorganic filler, such as a heat absorbing metal hydroxide or other fillers.
[0030] Examples of endothermic metal hydroxides include aluminum hydroxide, magnesium hydroxide, calcium hydroxide, etc., and it is particularly preferable to use aluminum hydroxide. These contain water of crystallization, and since they decompose at high temperatures and release water, which is an endothermic reaction, they have the effect of suppressing temperature rise during combustion, and tend to improve the non-combustibility of the decorative board according to the present invention.
[0031] The average particle size of the endothermic metal hydroxide can be, for example, in the range of 0.1 to 500 μm. Within this range, the dispersibility in the resin liquid is improved, and the impregnation into the fibrous substrate tends to be improved. Furthermore, the surface of the decorative board tends to be finished smoothly. The average particle size in the present invention is an arithmetic mean diameter calculated from the particle size distribution (volume distribution) detected by the laser diffraction / scattering method (Microtrack method).
[0032] Other fillers include, for example, carbonates such as calcium carbonate, magnesium carbonate, and zinc carbonate, silica, talc, and fly ash, and it is particularly preferable to use calcium carbonate. By using calcium carbonate, the workability in the manufacturing process and the machinability after manufacturing tend to improve. As calcium carbonate, for example, heavy calcium carbonate, light calcium carbonate (precipitated calcium carbonate), etc. can be used.
[0033] When other fillers are used, the average particle size thereof can be, for example, in the range of 0.05 to 300 μm. By keeping the average particle size within this range, there is a tendency for the impregnation into the fibrous base material to be improved.
[0034] When the fibrous base material is impregnated with the resin liquid, the impregnation rate is preferably 200 to 1500%, and particularly preferably 300 to 1200%, as calculated by the following formula (1). By being within this range, the impregnation of the resin liquid tends to be improved. Furthermore, since the adhesion between the core layers and between the core layer and the decorative layer is improved, delamination of the decorative board tends to be suppressed. In formula (1), the weight before impregnation is the weight of the fibrous base material itself, and the weight after impregnation is the weight after it is impregnated with the resin liquid and dried. Impregnation rate (%) = (weight after impregnation - weight before impregnation) / weight before impregnation × 100 (1)
[0035] (Decorative layer) The decorative board according to the present invention includes a decorative layer. The decorative layer is made of resin-impregnated decorative paper obtained by impregnating a fibrous base material with a resin liquid containing a thermosetting resin such as melamine resin and drying the resin liquid. It is preferable to use decorative paper for decorative boards as the fibrous base material.
[0036] The basis weight of decorative paper is 20 to 500 g / m 2 It is preferable that the thickness is 30 to 300 g / m 2 It is particularly preferable that the thickness is within this range. By being within this range, the surface properties of the decorative board and the impregnation of the resin liquid tend to be improved. As the decorative paper, colored paper or paper with various patterns printed thereon can be appropriately used.
[0037] As the thermosetting resin, in addition to the above-mentioned amino-formaldehyde resin and phenol-formaldehyde resin, radical polymerization type thermosetting resin, etc. can be used.
[0038] Examples of the radical polymerization type thermosetting resin include unsaturated polyester resin, vinyl ester resin, diallyl phthalate resin, and mixtures thereof. In particular, the use of unsaturated polyester resin and vinyl ester resin tends to impart flexibility to the decorative board and suppress shrinkage upon curing.
[0039] The unsaturated polyester resin can be obtained by adding a polymerizable monomer to an unsaturated polyester obtained by reacting a dihydric alcohol with a dibasic acid through esterification.
[0040] Examples of the dihydric alcohol include ethylene glycol, diethylene glycol, propylene glycol, dipropylene glycol, 1,3-butylene glycol, and neopentyl glycol. Examples of the dibasic acid include maleic acid, maleic anhydride, fumaric acid, isophthalic acid, terephthalic acid, phthalic acid, phthalic anhydride, and adipic acid.
[0041] Examples of the polymerizable monomer include styrene, orthochlorostyrene, diallyl phthalate, methyl methacrylate, etc. When curing, an organic peroxide such as benzoyl peroxide, methyl ethyl ketone peroxide, cyclohexanone peroxide, acetylacetone peroxide, acetoacetic acid peroxide, etc., or a curing accelerator such as a cobalt complex salt, etc., may be added as a curing agent.
[0042] The vinyl ester resin can be obtained by reacting an epoxy resin with an unsaturated monobasic acid in the presence of an esterification catalyst.
[0043] Examples of epoxy resins include bisphenol A-based epoxy resins, halogenated bisphenol A-based epoxy resins, diglycidyl ethers of adducts of bisphenol A with alkylene oxides such as ethylene oxide or propylene oxide, bisphenol F-based epoxy resins, novolac-based epoxy resins, and cresol novolac-based epoxy resins.
[0044] Examples of unsaturated monobasic acids include acrylic acid, methacrylic acid, crotonic acid, monomethyl maleate, monopropyl maleate, sorbic acid, and mono(2-ethylhexyl) maleate. Examples of polybasic acids used in combination with unsaturated monobasic acids include succinic acid, maleic acid, fumaric acid, itaconic acid, phthalic acid, isophthalic acid, terephthalic acid, adipic acid, azelaic acid, 1,12-dodecanedioic acid, and dimer acid. Examples of dibasic acid anhydrides include maleic anhydride and phthalic anhydride. Modified products using trimellitic anhydride as a tribasic acid anhydride can also be used.
[0045] Examples of the esterification catalyst include tertiary amines such as dimethylbenzylamine and tributylamine; quaternary ammonium salts such as trimethylbenzylammonium chloride; inorganic salts such as lithium chloride and chromium chloride; imidazole compounds such as 2-ethyl-4-methylimidazole; phosphonium salts such as tetramethylphosphonium chloride, diethylphenylpropylphosphonium chloride, triethylphenylphosphonium chloride, benzyltriethylphenylphosphonium chloride, dibenzylethylmethylphosphonium chloride, benzylmethyldiphenylphosphonium chloride, and tetraphenylphosphonium bromide; secondary amines; tetrabutylurea; triphenylphosphine; tritolylphosphine; triphenylstibine, etc.
[0046] When the fibrous substrate is impregnated with the resin liquid, the impregnation rate is preferably 10 to 500%, and more preferably 20 to 300%, as calculated by the above formula (1). Within this range, stickiness after resin impregnation tends to be suppressed.
[0047] (Surface protective layer) The decorative board according to the present invention includes a surface protective layer. The surface protective layer includes a resin-impregnated surface paper. The resin-impregnated surface paper is made by impregnating a fibrous base material with a resin liquid containing a thermosetting resin and a blocked isocyanate and then drying the resin-impregnated surface paper.
[0048] As the fibrous substrate, a surface paper for a decorative plate can be used, for example, α-cellulose paper, woven fabric, nonwoven fabric, etc. In particular, it is preferable to use α-cellulose paper that becomes transparent or translucent after the thermosetting resin is cured.
[0049] Also, a surface paper having abrasion resistance in which abrasion-resistant powder is mixed can be used, in which case the abrasion resistance of the decorative board tends to be improved. Examples of the abrasion-resistant powder include inorganic powders such as aluminum oxide, silicon carbide, and silicon oxide. The abrasion-resistant surface paper has an abrasion-resistant powder mixed in an amount of 1 to 40%, more preferably 5 to 30%, by weight relative to the α-cellulose paper, and has a basis weight of 10 to 60 g / m. 2 When the content is within this range, there is a tendency that deterioration in the clarity of the decorative layer can be suppressed.
[0050] The resin liquid contains a thermosetting resin and a blocked isocyanate.
[0051] As the thermosetting resin, in addition to the above-mentioned amino-formaldehyde resin and phenol-formaldehyde resin, radical polymerization type thermosetting resin, etc. can be used. Among these, in order to improve heat resistance and abrasion resistance, it is preferable to use amino-formaldehyde resin, and it is particularly preferable to use melamine-formaldehyde resin. In addition, the resin liquid can also contain the above-mentioned filler appropriately.
[0052] Blocked isocyanates are compounds in which the terminal isocyanate groups of polyisocyanates are blocked with a blocking agent, and the progress of the reaction is suppressed. Each type of blocked isocyanate has its own dissociation temperature, and when the temperature reaches that range, the blocking agent dissociates and the crosslinking reaction proceeds.
[0053] Examples of the basic structure of polyisocyanate include various types such as HDI (hexamethylene diisocyanate), MDI (diphenylmethane diisocyanate), and TDI (toluene diisocyanate), and examples of the blocking agent include various types of compounds such as oxime-based, amine-based, and methylene-based compounds.
[0054] In the present invention, it is preferable to use an HDI-based polyisocyanate as the basic skeleton. When the skeleton is an HDI-based polyisocyanate, it is an aliphatic compound, and tends to be highly stable and easy to handle.
[0055] The inventors of the present invention found that the dimensional stability of a decorative board is improved while maintaining the general physical properties by using, in particular, an amine-based blocked isocyanate in the resin liquid in the surface protective layer, and thus completed the present invention. This is believed to be due to the fact that the dissociation temperature of the amine-based blocked isocyanate is mainly about 100°C to 140°C, which is within the range of general molding temperatures when manufacturing a decorative board, and therefore the crosslinking reaction is likely to proceed. In addition, the dissociation temperature of the oxime-based blocked isocyanate is about 140°C to 180°C, and although a decorative board can be manufactured without problems, it is preferable to use, in particular, an amine-based blocked isocyanate from the viewpoint of dimensional stability.
[0056] Generally, decorative boards use fibrous substrates as the substrate, but because fibrous substrates have a fiber direction, their dimensional stability varies depending on the direction. Specifically, in the fiber direction (hereafter referred to as the vertical direction), the expansion rate is low and dimensional stability is excellent, whereas in the direction perpendicular to the fiber direction (hereafter referred to as the horizontal direction), the expansion rate varies greatly depending on the type of substrate and resin, and dimensional stability tends to change. Therefore, the present invention aims to improve dimensional stability, especially in the horizontal direction.
[0057] Furthermore, the inventors of the present invention have found that when a blocked isocyanate is used, the impregnation rate in the surface protective layer can be reduced compared to that of a general decorative board. Although simply reducing the impregnation rate tends to cause contamination of the board, the present invention achieves both a reduction in the impregnation rate and suppression of contamination of the board by adding a blocked isocyanate. Therefore, the decorative board of the present invention can be manufactured using a smaller amount of resin and filler than usual, which improves productivity and reduces production costs.
[0058] When the fibrous substrate is impregnated with the resin liquid, the impregnation is preferably performed so that the impregnation rate is 20 to 450%, and more preferably 30 to 300%, as calculated by the above formula (1). If the impregnation rate is within this range, stickiness after the resin impregnation tends to be suppressed.
[0059] The mixing ratio of the blocked isocyanate in the resin liquid is preferably 0.01 to 100 parts by weight, more preferably 0.1 to 50 parts by weight, and particularly preferably 1 to 30 parts by weight, relative to 100 parts by weight of the above-mentioned thermosetting resin. By mixing within this range, the decorative board can be produced efficiently, and the productivity tends to improve.
[0060] The decorative board according to the present invention can be obtained by laminating a core layer, a decorative layer, and a surface protective layer, and subjecting the laminate to hot-press molding using a press such as a flat press or a continuous press.
[0061] <Flooring> The decorative board obtained in the above manner has improved dimensional stability and can therefore be suitably used as a surface material for flooring.
[0062] Examples of the base layer of the flooring material include thermoplastic resin sheets such as polyolefin resin, polyvinyl chloride resin, urethane resin, and various elastomers. In this case, the flooring material is manufactured by bonding a decorative board and a thermoplastic resin sheet with an adhesive. The thermoplastic resin sheet may be either non-foamed or foamed, and the foaming ratio is preferably 1.5 to 40 times, and either an open-cell foam or a closed-cell foam may be used.
[0063] Among the above thermoplastic resin sheets, polyvinyl chloride resin sheets and foamed polyethylene have cushioning properties, easily absorb unevenness and irregularities in the base, and are inexpensive and suitable for use. The thickness of the sheet can be in the range of 1 to 10 mm.
[0064] The present invention will be described in more detail below with reference to examples and comparative examples, but the present invention is not limited to these descriptions. In the examples, parts by weight are values calculated as solid content. EXAMPLES
[0065] <Example 1> (1) Manufacturing of the core layer As a fibrous base material, the basis weight is 76 g / m 2 A glass fiber nonwoven fabric having the following characteristics was prepared. In addition, a resin liquid was obtained consisting of 12 parts by weight of an acrylic resin emulsion having 2-ethylhexyl acrylate and methyl methacrylate as main monomers, with a glass transition temperature (Tg) of 60°C and an average particle size of 200 nm, 4 parts by weight of an acrylic resin emulsion having ethyl acrylate and methyl methacrylate as main monomers, with a glass transition temperature (Tg) of 88°C and an average particle size of 180 nm, and 52 parts by weight of calcium carbonate. Water was then added to the resin liquid, and a glass fiber nonwoven fabric was impregnated with the resin so that the impregnation rate was 750% as calculated by the formula (1), and the fabric was dried to produce a prepreg to be used for the core layer. (2) Manufacturing of the decorative layer As a fibrous base material, the basis weight is 80 g / m 2 We prepared decorative paper with a wood grain pattern. Also, a vinyl ester resin liquid containing 63% bisphenol vinyl ester, 15% methacrylic monomer, 20% propylene glycol monomethyl ether acetate (diluent), and 2% acrylic acid was obtained. The decorative paper was then impregnated with vinyl ester resin so that the impregnation rate was 40% as calculated by the formula (1), and then dried to produce a resin-impregnated decorative paper to be used in the decorative layer. (3) Manufacturing of the surface protection layer As a fibrous base material, the basis weight is 23 g / m 2 A surface paper (α-cellulose paper) was prepared. Also, a resin liquid containing 100 parts by weight of melamine-formaldehyde resin, 5 parts by weight of amine-based blocked isocyanate (product name: BI522, manufactured by LANXESS), and 0.2 parts by weight of a curing catalyst (product name: Catanit A) was obtained. The surface paper was then impregnated with the resin liquid so that the impregnation rate was 170% as calculated by the formula (1), and then dried to produce a resin-impregnated surface paper to be used in the surface protective layer. (4) Manufacture of decorative panels A single prepreg was placed on the bottom layer as a core layer, and then resin-impregnated decorative paper as the decorative layer and resin-impregnated surface paper as the surface protection layer were laminated in that order.Then, using a hot-press molding press plate, the laminate was hot-press molded under conditions of 135°C, 6 MPa, and 60 minutes to obtain the decorative board of Example 1.
[0066] Example 2 was carried out in the same manner as Example 1, except that an amine-based blocked isocyanate (product name: BI120, manufactured by LANXESS) was used. Example 3 was carried out in the same manner as Example 1, except that an amine-based blocked isocyanate (product name: BI220, manufactured by LANXESS) was used. Example 4 was carried out in the same manner as Example 3, except that the amount of the amine-based blocked isocyanate was 10 parts by weight. Example 5 was carried out in the same manner as Example 1, except that an oxime-based blocked isocyanate was used. Comparative Example 1 was carried out in the same manner as in Example 1, except that no blocked isocyanate was used.
[0067] The following physical property evaluations were carried out for the examples and comparative examples. The evaluation results are shown in Table 1. Plate contamination: The appearance of the plate after thermocompression was visually observed. Plates with no contamination were rated ◯, plates with contamination only partially observed were rated △, and plates with contamination over the entire plate were rated ×. Dimensional stability: Based on JIS K 6902, the percentage of expansion and contraction (%) in the longitudinal and transverse directions was measured, and the total percentage of expansion and contraction was taken as the rate of change (%). Stain resistance: A drop of Tabasco (commercial product), mouthwash (trade name: Isodine), iodine alcohol (1% aqueous solution), and hair dye (trade name: Bigen) was placed on a decorative panel, and left to stand for 24 hours under conditions of temperature: 23°C and humidity: 50%, after which the panel was rinsed with water and the surface of the decorative panel was visually checked for staining. Those with no visible staining were rated as ◯, and those with partial staining were rated as ×.
[0068] [Table 1]
Claims
1. The laminated laminated sheet includes a core layer, a decorative layer, and a surface protective layer, The surface protective layer includes a resin-impregnated surface paper, The resin-impregnated surface paper is a decorative board formed by impregnating a fibrous base material with a resin liquid containing a thermosetting resin and a blocked isocyanate, and then drying the liquid.
2. 2. The decorative board according to claim 1, wherein the blocking agent of the blocked isocyanate is an amine compound.
3. 2. The decorative board according to claim 1, wherein the dissociation temperature of the blocked isocyanate is 100°C to 140°C.
4. 2. The decorative board according to claim 1, wherein the thermosetting resin is at least one compound selected from the group consisting of amino-formaldehyde resins, phenol-formaldehyde resins, and radical polymerization type thermosetting resins.
5. 5. The decorative board according to claim 1, which is used as a flooring material.
6. A flooring material comprising a base layer and the decorative board according to any one of claims 1 to 4 laminated thereon.
Citation Information