Slide member
The sliding member design with a Bi phase and intrusion portion in the lining layer addresses the need for complex cleaning by enhancing adhesive force through a controlled Bi phase-to-intrusion part ratio, improving bonding efficiency.
Patent Information
- Application Number
- JP2023048474
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-07
- Estimated Expiration
- 2043-03-24
AI Technical Summary
Conventional methods to improve bonding force between a Cu-based lining layer and a coating layer in sliding members require extensive cleaning processes to remove Bi-Ni compounds, which are time-consuming and labor-intensive.
A sliding member design with a lining layer containing Bi phase and a covering layer forming an intrusion portion that intrudes into the lining layer, setting a ratio of Bi phase area to intrusion part area (R=1.00≦R≦9.00) to enhance adhesive force while reducing cleaning steps.
The design ensures improved adhesive force between the lining and coating layers by minimizing Bi-Ni compound formation, reducing cleaning complexity, and maintaining workability.
Smart Images

Figure 2024137096000001_ABST
Abstract
Description
[Technical field]
[0001] The present embodiment relates to a sliding member. [Background technology]
[0002] Conventionally, a sliding member in which an overlay layer is provided on the surface of a Cu-based lining layer is known (Patent Document 1). In Patent Document 1, the second phase component contained in the lining layer is removed from the surface of the lining layer to improve the bonding strength between the lining layer and the overlay layer. It is also disclosed that a Ni coating layer is provided on the surface of the lining layer to stabilize the overlay layer. However, Bi, which is a second phase component contained in the lining layer, generates a Bi-Ni compound at the interface with the coating layer depending on the temperature conditions during operation of the applied equipment. This Bi-Ni compound causes a decrease in the adhesive strength between the lining layer and the coating layer. Therefore, when adopting a configuration such as that of Patent Document 1, it is necessary to thoroughly remove the Bi phase present on the surface of the lining layer, i.e., the surface in contact with the coating layer. Removal of this Bi phase requires long cleaning times, such as cleaning with an acid or ultrasonic cleaning by irradiating ultrasonic waves, and there is a problem that it requires a large number of steps. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2009-203504 A Summary of the Invention [Problem to be solved by the invention]
[0004] Therefore, an object of the present invention is to provide a slide member which improves the adhesive strength between the lining layer and the coating layer while reducing the number of steps required for removing Bi. [Means for solving the problem]
[0005] In order to solve the above problems, the slide member of this embodiment includes a lining layer containing a Bi phase, and a coating layer containing Ni, provided on the surface of the lining layer, and forming a penetration part that partially penetrates into the lining layer at the interface with the lining layer. In any observation region including the interface between the lining layer and the coating layer, the ratio R=S1 / S2 of the maximum area S1 of the Bi phase contained in the lining layer to the maximum area S2 of the penetration part that has penetrated into the lining layer satisfies 1.00≦R≦9.00.
[0006] In the sliding member of this embodiment, a value R of the ratio between the maximum area S1 of the Bi phase and the maximum area S2 of the intrusion portion is set. When the Bi phase is removed by cleaning or the like, a recess corresponding to the removed Bi phase is formed in the lining layer. Therefore, the recess corresponding to the removed Bi phase is replaced by Ni or Ni alloy forming the coating layer. This reduces the generation of Bi-Ni compounds. Also, even if a part of the Bi phase remains in the lining layer, Ni or Ni alloy invades as an intrusion portion into the recess formed by removing the Bi phase. Therefore, the intrusion portion that invades the recess is in a state of being bitten into the lining layer. As a result, the coating layer is in a state of being caught by the lining layer in a predetermined shape, and even if a Bi-Ni compound is formed, peeling from the lining layer is reduced. As a result, even if the cleaning of the Bi phase contained in the lining layer is insufficient, the bonding force between the lining layer and the coating layer is ensured. Therefore, the adhesive force between the lining layer and the coating layer can be improved while reducing the man-hours for removing Bi. [Brief description of the drawings]
[0007] [Figure 1] FIG. 1 is a schematic diagram showing a cross section of a sliding member according to an embodiment; [Diagram 2] Schematic diagram of an enlarged observation area in Figure 1 [Diagram 3] Enlarged schematic diagram of part III in Figure 2 [Figure 4] FIG. 1 is a schematic diagram showing evaluation results of examples and comparative examples of a sliding member according to an embodiment. [Diagram 5]FIG. 1 is a schematic diagram showing evaluation results of examples of a sliding member according to an embodiment; [Figure 6] FIG. 1 is a schematic diagram showing evaluation results of examples of a sliding member according to an embodiment; [Figure 7] FIG. 1 is a schematic diagram showing evaluation results of examples of a sliding member according to an embodiment; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] Hereinafter, a sliding member according to an embodiment will be described with reference to the drawings. As shown in FIG. 1, the sliding member 10 includes a lining layer 11 and a coating layer 12. The sliding member 10 is formed, for example, in a cylindrical or halved shape and is used in a bearing device or the like. The lining layer 11 is provided on one end surface of the backing metal layer 13. The sliding member 10 also includes an overlay layer 14 on the side of the coating layer 12 opposite to the backing metal layer 13. In other words, the coating layer 12 is an intermediate layer provided between the lining layer 11 and the overlay layer 14. The surface of the overlay layer 14 forms a sliding surface 15 that slides against a counter material (not shown). The sliding member 10 is not limited to a cylindrical half-shaped member divided into two, but may be divided into three or more parts in the circumferential direction.
[0009] The lining layer 11 is formed of a Cu-based alloy. The lining layer 11 is mainly composed of Cu and contains Bi. The lining layer 11 contains 0.1 to 2.0 mass% of Bi. Bi contributes to improving the workability of the formed lining layer 11 during mechanical processing such as cutting and polishing. The lining layer 11 is not limited to a Cu-based alloy, and may be a Sn-based alloy or an Al-based alloy. The thickness of the overlay layer is preferably set to 10 μm to 30 μm. In the case of the lining layer 11, it is preferably set to 0.1 mm to 1.5 mm. In this case, the thickness of the coating layer 12 is preferably set to 1 μm to 5 μm.
[0010] The coating layer 12 is made of Ni. The coating layer 12 may be a Ni alloy. In this case, the coating layer 12 may contain 30 mass% or less of Cr in Ni. The coating layer 12 is formed on the surface of the lining layer 11 opposite to the back metal layer 13 by, for example, plating. The boundary between the lining layer 11 and the coating layer 12 is an interface 16. The back metal layer 13 is made of an alloy containing Fe as a main component, such as steel. One or more layers, such as an intermediate layer (not shown), may be provided between the lining layer 11 and the back metal layer 13. The overlay layer 14 is made of, for example, Sn or an alloy containing Sn as a main component. The overlay layer 14 may be made of other elements or alloys instead of Sn or an Sn-based alloy.
[0011] The lining layer 11 contains a Bi phase 17 in its structure, which is derived from Bi added to the Cu-based alloy, as shown in FIG. 2. The Bi phase 17 is not only contained in the structure of the Cu-based alloy, but also exposed at the interface 16. After the lining layer 11 is formed on the surface of the backing metal layer 13, it is washed with, for example, acid or water. As a result, most of the Bi phase 17 exposed at the interface 16 among the Bi phase 17 contained in the lining layer 11 is removed by washing. The interface 16 between the lining layer 11 and the coating layer 12 is preferably formed to be approximately flat. However, this interface 16 is not limited to being flat. When the Bi phase 17 is removed at the interface 16 of the lining layer 11, the portion from which the Bi phase 17 has been removed forms a recess 18 recessed toward the lining layer 11 side. When the coating layer 12 of Ni or Ni alloy is formed by, for example, plating on the interface 16 including the recess 18, a part of the Ni or Ni alloy constituting the coating layer 12 penetrates into the recess 18 of the lining layer 11. That is, the recess 18 formed by removing the Bi phase 17 at the interface 16 is filled with the Ni or Ni alloy constituting the coating layer 12. As a result, the coating layer 12 forms an intrusion part 19 at the interface 16 with the lining layer 11 where a part of the coating layer 12 penetrates into the lining layer 11 side. This intrusion part 19 bites into the inside of the lining layer 11 on the back metal layer 13 side further than the interface 16 between the lining layer 11 and the coating layer 12.
[0012] In this embodiment, in any observation region 20 shown in FIG. 1 and FIG. 2, the maximum area S1 of the Bi phase 17 contained in the lining layer 11 and the maximum area S2 of the penetration portion 19 that has penetrated into the lining layer 11 are measured. The ratio value R is calculated as R=S1 / S2 using the measured maximum area S1 and maximum area S2. In this embodiment, the observation region 20 is set as an arbitrary range including the penetration portion 19 in a cross section including the interface 16 between the lining layer 11 and the coating layer 12. The dimensions of the observation region 20 are set, for example, as a range of 450 μm in the thickness direction × 600 μm in width. Note that the dimensions of the observation region 20 are merely examples, and can be set to any dimensions within a range in which the penetration portion 19 can be observed.
[0013] The maximum area S1 of the Bi phase 17 contained in the lining layer 11 is the area of the Bi phase having the largest area among the Bi phases 17 contained in this observation region 20. The area of the Bi phase 17 correlates with the area of the particles that would have been present at the interface and the area of the particles contained inside the lining layer 11. Here, the maximum area S1 of the Bi phase 17 is measured based on the particles of the Bi phase 17 contained inside the lining layer 11. For example, when a plurality of particles of the Bi phase 17 are contained in the observation region 20 as shown in FIG. 2, the area of the Bi phase 17 having the largest area is the maximum area S1. The observation region 20 is a cross section cut in the thickness direction, such as along the axis of the sliding member 10 or perpendicular to the axis, and can be set in any direction as long as the intrusion portion 19 can be observed. In this case, the observation region 20 is set to have a length in the width direction perpendicular to the thickness direction, such as 450 μm in the thickness direction × 600 μm in width, which is larger than the length in the thickness direction of the lining layer 11.
[0014] As shown in FIG. 3, the intrusion portion 19 is defined as a region on the lining layer 11 side of the imaginary straight line L that connects the vertices 21 and 22 of the intrusion portion 19 on the interface 16 side. That is, the intrusion portion 19 is the shaded region in FIG. 3. The area of the region on the lining layer 11 side of the straight line L is the area of the intrusion portion 19. When a plurality of intrusion portions 19 are observed in the observation region 20 as shown in FIG. 2, the area of the intrusion portion 19 with the largest area among these intrusion portions 19 is the maximum area S2. The ratio value R is calculated from the maximum area S1 and the maximum area S2 obtained from these. In this embodiment, the ratio value R is 1.00≦R≦9.00.
[0015] The Bi phase 17 contained in the lining layer 11 has a maximum area S1 of S1≦810 μm 2 It is preferable that the maximum area S1 of the Bi phase 17 is set to 20 μm. If the maximum area S1 of the Bi phase 17 is set in this way, the adhesive strength between the lining layer and the coating layer is further improved. Furthermore, the Bi phase 17 is essential for improving the workability during processing such as cutting of the lining layer 11. Therefore, from the viewpoint of ensuring the workability of the lining layer 11, the maximum area S1 of the Bi phase 17 is set to 20 μm. 2 The maximum area S1 of the Bi phase 17 contained in the lining layer 11 is preferably S1≦810 μm 2 The maximum area S2 of the intrusion portion 19 is preferably 20 μm 2 ≦S2≦90μm 2 By setting the maximum area S1 of the Bi phase 17 in this manner, it is possible to improve both the workability during machining such as cutting of the lining layer 11 and the adhesive strength with the coating layer 12.
[0016] When the coating layer 12 containing Ni is formed on the surface of the lining layer 11, when Bi 17 added to the lining layer 11 is exposed to the coating layer 12, Bi in the Bi phase 17 diffuses into the coating layer 12. For example, when the temperature of the sliding member 10 is 100°C to 250°C, Bi in the Bi phase 17 contained in the lining layer 11 that is in contact with the coating layer 12 at the interface 16 diffuses toward the coating layer 12. Therefore, a Bi-Ni compound is likely to be generated from Bi originating from the lining layer 11 and Ni originating from the coating layer 12 near the interface 16. This Bi-Ni compound reduces the adhesive force between the lining layer 11 and the coating layer 12. Therefore, in the conventional case, the interface 16 of the lining layer 11 requires thorough and advanced cleaning with a large number of steps in order to remove almost the entire Bi phase while avoiding the remaining Bi phase 17.
[0017] On the other hand, in this embodiment, although the interface 16 of the lining layer 11 is cleaned, advanced cleaning as in the past is not required. In this embodiment, most of the Bi phase 17 exposed at the interface 16 is removed by simple cleaning with, for example, acid. Then, the lining layer 11 forms a recess 18 at the interface 16 by removing the Bi phase 17 at the interface 16. The coating layer 12 laminated on the lining layer 11 penetrates into the recess 18 formed in the lining layer 11 and forms an intrusion portion 19. As a result, the formed coating layer 12 is in a state in which the intrusion portion 19 penetrates and engages with the lining layer 11. In this embodiment, the ratio value R is set to 1.00≦R≦9.00. As a result, even if the Bi phase 17 that could not be removed remains in the recess 18, the intrusion portion 19 that penetrates into the lining layer 11 sufficiently engages with the lining layer 11, and the strength, i.e., the adhesive force, at the interface 16 between the lining layer 11 and the coating layer 12 is improved. Therefore, the number of steps required for removing the Bi phase 17 can be reduced, and the adhesive strength between the lining layer 11 and the coating layer 12 can be improved.
[0018] Next, a method for manufacturing the slide member 10 of this embodiment will be described. The lining layer 11 has a fine dispersion of the Bi phase 17 in a Cu-based alloy. Such a lining layer 11 is formed, for example, by using sintering. Sintering is performed by mixing bronze powder, which is the main component of the Cu-based alloy forming the lining layer 11, with Bi powder, which forms the Bi phase 17. The particle size of the Bi phase 17 in the lining layer 11 is controlled by changing the particle size of the Bi powder used as a material. The particle size of the Bi phase is adjusted, for example, by blending particles classified into particle sizes of 75 μm or less, 38 μm or less, etc.
[0019] In the primary sintering in which the mixed powder is sintered, the sintering temperature is set to 600°C to 800°C, which is about 4 / 5 of the conventional sintering temperature. As a result, in the primary sintering of the powder, the powders can be bonded together with relatively fine necks formed, and the Cu-based lining layer 11 becomes porous. As a result, the particles of the Bi phase 17 contained in the lining layer 11 after the primary sintering exist in a finely dispersed state in the porous portion of the lining layer 11. After that, post-treatment such as rolling was performed to produce the lining phase 11.
[0020] The lining layer 11 that has been subjected to the post-treatment is washed with an acid in order to remove the oxide film at the interface 16. As a result, the Bi phase 17 contained in the lining layer 11 is removed prior to Cu, which is the main component of the lining layer 11, due to the difference in ionization tendency. The portion at the interface 16 from which the Bi phase 17 has been removed forms a recess 18. The lining layer 11 that has been washed with acid is washed with water, and then the coating layer 12 is formed. The coating layer 12 is formed, for example, by plating with Ni or a Ni alloy. In this embodiment, the lining layer 11 is not subjected to strict cleaning other than washing with acid and water. That is, the lining layer 11 of this embodiment may have a small amount of Bi remaining in the recess 18, etc. A part of the coating layer 12 formed by plating or the like penetrates into the recess 18. As a result, the coating layer 12 forms an intrusion portion 19 that penetrates into the lining layer 11 side.
[0021] Examples of the sliding member 10 of this embodiment will now be described. In the examples and comparative examples, the sliding member 10 was evaluated based on the adhesive strength between the lining layer 11 and the coating layer 12. The adhesive strength was evaluated by cross-cut evaluation specified in "JIS K5600-5-6" for evaluating the adhesive strength of plating. The heat treatment temperature and time conditions set before the cross-cut evaluation according to the said regulations are strict evaluation conditions, so "Classification 0", "Classification 1" and "Classification 2" were deemed to be acceptable. The test pieces in the examples and comparative examples were produced according to the above-mentioned manufacturing method, and then heat-treated at 150°C for 500 hours to reproduce the usage conditions, after which the adhesive strength was evaluated.
[0022] FIG. 4 shows an evaluation of the effect of the ratio value R on the adhesive strength. In all of Examples 1 to 3 and Comparative Example 1, the concentration C of Bi contained in the lining layer 11 is set to 2.0 mass%. As shown in Examples 1 to 3, if the ratio value R is in the range of 1.00≦R≦9.00, it is classified as "Class 2" and it is found that there is no effect on the adhesive strength. On the other hand, Comparative Example 1, in which the ratio value R is greater than 9.00, is classified as "Class 3" and it is found that the adhesive strength is reduced. The lower limit of the ratio value R is set to 1.00 in consideration of the workability of the slide member 10, particularly the machinability.
[0023] FIG. 5 shows an evaluation of the effect of the maximum area S1 of the Bi phase 17 on the adhesive strength. In all of Examples 4 to 7, the concentration C of Bi contained in the lining layer 11 is set to 2.0 mass%. As shown in Examples 4 to 7, when the ratio value R is constant, the smaller the maximum area S1 of the Bi phase 17, the higher the adhesive strength. However, as described above, if the maximum area S1 of the Bi phase 17 becomes too small, it affects the workability of the lining layer 11. Therefore, the maximum area S1 of the Bi phase 17 is set to 20 μm 2 It is preferable that the amount is equal to or more than that.
[0024] 6 shows an evaluation of the effect of the maximum area S2 of the intrusion part 19 on the adhesive strength. In all of Examples 8 to 11, the concentration C of Bi contained in the lining layer 11 is set to 2.0 mass%. As shown in Examples 8 to 11, when the ratio R is constant, the smaller the maximum area S2 of the intrusion part 19, the higher the adhesive strength.
[0025] FIG. 7 shows an evaluation of the effect of the concentration C of Bi added to the lining layer 11 on the adhesive strength. If the ratio value R is constant, the smaller the concentration C, the higher the adhesive strength. However, as mentioned above, the concentration of Bi affects the workability of the lining layer 11. Therefore, it is a prerequisite that the lining layer 11 contains Bi, and from a practical standpoint, the lower limit is set to 0.1 mass%.
[0026] The present invention described above is not limited to the above-described embodiment, and can be applied to various embodiments without departing from the gist of the invention. [Explanation of symbols]
[0027] In the drawing, 10 denotes a sliding member, 11 denotes a lining layer, 12 denotes a coating layer, 17 denotes a Bi phase, 19 denotes an intrusion portion, and 20 denotes an observation area.
Claims
1. a lining layer including a Bi phase; a coating layer containing Ni, provided on the surface of the lining layer, the coating layer forming an intrusion portion partly intruding into the lining layer at the interface with the lining layer; A sliding member comprising: In any observation region including the penetration portion at the interface between the lining layer and the coating layer, a ratio R=S1 / S2 of a maximum area S1 of the Bi phase contained in the lining layer to a maximum area S2 of the penetration portion that has penetrated into the lining layer is 1.00≦R≦9.
00. Sliding member.
2. The maximum area S1 of the Bi phase is S1≦810 μm 2 That is, The sliding member according to claim 1.
3. The maximum area S2 of the intrusion portion is 20μm 2 ≦S2≦90 μm 2 That is, The sliding member according to claim 1.
4. The concentration C of Bi contained in the lining layer is 0.1 mass% ≦ C ≦ 1.5 mass%; The sliding member according to claim 1.
Citation Information
Patent Citations
Copper-lead bearing alloy material excellent in corrosion resistance and its production
JP1994322462A
Sliding member
JP2009203504A
Wear-resistant lead-free alloy sliding element and method for manufacturing the same
JP2014505161A