Sequential molding method
The method addresses surface irregularities in sequential forming by pressing and leveling the metal plate to improve precision and appearance, suitable for automobile panels.
Patent Information
- Application Number
- JP2023048579
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-07
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional sequential forming methods result in minute irregularities around the forming part, leading to insufficient surface precision and appearance quality, particularly in applications like automobile exterior panels.
A method where a tool is pressed against a metal plate to form a three-dimensional shape, followed by leveling out minute irregularities on the metal plate to improve surface accuracy and appearance quality.
The method effectively eliminates or minimizes visible irregularities, enhancing surface precision and appearance quality, making it suitable for high-quality applications such as automobile exterior panels.
Smart Images

Figure 2024137168000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an incremental forming method for incrementally forming a metal plate into a three-dimensional shape by pressing and moving a tool against the metal plate. [Background technology]
[0002] A conventional incremental forming method is described, for example, in Patent Document 1. Patent Document 1 describes an incremental forming apparatus in which a rod-shaped tool is arranged on the upper surface side of a metal plate, a receiving tool is arranged on the lower surface side of the same metal plate, and a liftable support plate having a work holder is provided. In this incremental forming apparatus and method, the periphery of the metal plate is held by the work holder, and the tool is pressed against the metal plate and moved while the support plate is lowered, thereby gradually deforming the metal plate to fit the receiving tool and forming it into a three-dimensional shape. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2013-244493 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in the conventional incremental forming method as described above, the edges of the formed portion are not clamped, and the tool movement path is set only to the formed portion, which can result in tiny irregularities around the formed portion. This poses the problem that the surface precision and appearance quality are insufficient for application to, for example, the outer panels of automobiles, and improvements were desired.
[0005] The present invention has been made in consideration of the above-mentioned conventional situation, and aims to provide a sequential molding method that can make minute irregularities that occur around the molded part less noticeable, thereby improving surface precision and appearance quality. [Means for solving the problem]
[0006] The incremental forming method according to the present invention is a method for forming a three-dimensional shape by gradually deforming a metal plate in the thickness direction by pressing and moving the tip of a tool against the metal plate. This incremental forming method is characterized in that after forming a concave or convex formed portion in the metal plate, the tip of a tool is pressed against and moved against minute irregularities occurring outside the formed portion in the metal plate to smooth out the minute irregularities. Effect of the Invention
[0007] By adopting the above-mentioned configuration, the incremental molding method of the present invention can eliminate or make less noticeable minute irregularities that occur around the molded portion, thereby improving surface precision and appearance quality, making it highly useful for application to automobile exterior panels, etc. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is an exploded perspective view illustrating an incremental forming apparatus applicable to an incremental forming method according to a first embodiment of the incremental forming method according to the present invention. [Diagram 2] 2 is a perspective view showing a state in which incremental forming is performed by the incremental forming apparatus shown in FIG. 1. [Diagram 3] FIG. 4 is a cross-sectional view showing changes in a metal plate during incremental forming. [Figure 4] FIG. 4 is an explanatory plan view showing a load acting on a metal plate during incremental forming. [Diagram 5] FIG. 2 is a plan view illustrating minute irregularities occurring on a metal plate. [Figure 6] FIG. 13 is a perspective explanatory view showing measurement of the amount of distortion. [Figure 7] FIG. [Figure 8] FIG. 11 is an explanatory plan view showing a moving path of a tool during smooth forming. [Figure 9] FIG. 2 is a perspective view showing an area where smoothing molding is performed. [Figure 10] FIG. 13 is a perspective view showing the range of another example where smoothing molding is performed. [Figure 11] The upper part is a cross-sectional view with an enlarged view showing the state during smoothing molding, and the lower part is a cross-sectional view showing the state after smoothing molding. [Figure 12] FIG. 4 is a perspective view showing the metal plate and the formed portion after smoothing. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] First embodiment 1 and 2 are diagrams illustrating an incremental forming apparatus applicable to the incremental forming method according to the present invention. The incremental forming apparatus shown in Fig. 1 includes a lower die 1, a pad 2 for sandwiching and holding a metal sheet P between the lower die 1 and the pad 2, and a rod-shaped tool T.
[0010] The lower mold 1 has a molding space 1A disposed in the center thereof and a plurality of positioning tools 1B for positioning the edge of the metal sheet W. The molding space 1A in the illustrated example has a rectangular concave shape in a plan view. Therefore, in this embodiment, the molding portion (symbol F in FIG. 6) to be molded in the metal sheet W has a rectangular concave shape in a plan view corresponding to the molding space 1A.
[0011] The metal plate W in the illustrated example has a gently curved surface, but may have a flat surface. The pad 2 has an opening 2A that is open upward and downward at a position corresponding to the molding space 1A of the lower mold 1. The tool T is, for example, attached to the hand of a working robot and is movable in three orthogonal axial directions and may be rotatable about each axis.
[0012] 2, the incremental forming device holds the metal sheet W between the lower die 1 and the pad 2, and moves a tool T through an opening 2A of the pad 2 while pressing it against the metal sheet W, thereby forming a concave formed portion (symbol F in FIGS. 4 to 6) in the metal sheet W along the inner surface of the forming space 1A. More specifically, the tool T is pressed against the metal sheet W and moved in a circular motion, and then the pitch feed and circular motion of the tool T are alternately repeated to form a concave shape into a contour line, gradually deforming the metal sheet W so as to be pressed down into the forming space 1A, thereby forming the concave formed portion (F).
[0013] In the incremental forming, when the tool T is pressed against the metal sheet W, the bending moment shown by the arrow in Fig. 3 may cause distortion (microscopic irregularities) in the metal sheet W. In addition, when the forming space 1A is rectangular in plan view as in the illustrated example, the metal sheet W is pulled toward the forming portion F in the portions along the sides, and the metal sheet W is pulled toward the forming portion F in the corner portions, and the thickness is increased due to compressive stress from the sides on both sides. As a result, the formed metal sheet W tends to have microscopic protrusions Q1 in the portions along the sides of the forming portion F and microscopic recesses Q2 in the corner portions of the forming portion F, as shown in Fig. 5.
[0014] The minute irregularities are on the order of several tens to several hundreds of micrometers and do not affect the strength, etc., of the metal sheet W, but are undesirable in terms of appearance because the surface of the metal sheet W appears distorted to the naked eye. In addition, as shown in Figs. 4 and 5, the minute irregularities do not occur uniformly around the entire circumference of the molded portion F, but may occur partially with different sizes.
[0015] In contrast, in the incremental forming method, after forming a formed portion F on a metal sheet W, the tip of a tool T is pressed against and moved against the minute irregularities occurring on the outside of the formed portion F on the metal sheet W, thereby smoothing out the minute irregularities. In addition, in a more preferable embodiment of the incremental forming method described above, a minute protrusion Q1 among the minute irregularities is smoothed out, and at that time, the amount of distortion of the minute protrusion Q1 is measured, as shown in Fig. 6.
[0016] The incremental forming apparatus applicable to the incremental forming method may include a control device 3 and a measuring device 4 for a tool T shown in FIG. 6. The control device 3 has a function of controlling the drive of the tool T, i.e., the drive of the work robot, and has a measurement calculation unit 3A to which the measured value of the measuring device 4 is input, and can control the drive of the tool T based on the data of the measurement calculation unit 3A. The measuring device 4 is not particularly limited, but for example, a non-contact measuring device using an image or laser light, or a contact measuring device such as a dial gauge can be used. Note that the measuring device 4 may be one that measures manually. In this case, the measuring device 4 is not strictly a component of the incremental forming apparatus, but the measurement work is one step of the incremental forming method.
[0017] In the incremental forming method, the minute irregularities are smoothed out as shown in Fig. 7. In this case, in the incremental forming method, the metal sheet W on the lower die 1 is smoothed out without using the pad 2, but instead of the pad 2, a clamp or the like may be used to clamp the peripheral portion of the metal sheet W between the lower die 1.
[0018] In addition, in a more preferred embodiment of the incremental forming method, after forming the formed portion F, the amount of distortion of the minute protrusion Q1 is measured, and the measured lowest portion of the minute protrusion Q1 is set as the contact position with the tool T, and the minute protrusion Q1 is formed evenly. In this way, in the incremental forming method, the amount of distortion of the highest portion of the minute protrusion Q1 can be reliably reduced.
[0019] Furthermore, in a more preferred embodiment of the incremental forming method, after forming the formed portion F, the amount of distortion of the minute protrusion Q1 is measured, and the pushing amount of the tool T is set based on the measured value to smooth out the minute protrusion Q1. As a result, in the incremental forming method, the amount of distortion of the minute protrusion Q1 can be reliably reduced regardless of the magnitude of the generated distortion, and smoothing out becomes unnecessary, thereby realizing a reduction in the forming time.
[0020] 8, the incremental forming method moves a tool T around the periphery of the formed portion F of the metal sheet W, and the paths P1-P4 of the movement form contour lines from the periphery of the formed portion F outward and spread at equal intervals along the main surface of the metal sheet W to smooth out the minute protrusions Q1. As a result, the incremental forming method can more reliably and efficiently smooth out the entire range in which minute protrusions and recesses occur, thereby achieving a further improvement in the appearance quality of the metal sheet W.
[0021] In the incremental forming method illustrated in Fig. 8, adjacent paths P1 to P4 rotate in opposite directions to each other to perform smoothing, thereby suppressing the load and residual stress applied to the metal sheet W and more reliably smoothing the entire range of minute irregularities. Note that Fig. 8 omits the pitch feed paths performed between adjacent paths P1 to P4, and also illustrates four paths P1 to P4, but in practice the number and spacing of paths are set depending on the size of the area to be smoothed, etc.
[0022] Furthermore, in the incremental forming method, smoothing is performed on the entire area A including the surface distortion Q confirmed by visual inspection around the entire periphery of the outer region of the formed part F, as shown in Fig. 9. Therefore, in the incremental forming method, when the surface distortion Q is large (or small), smoothing is performed on the entire area A including the surface distortion Q, as shown in Fig. 10.
[0023] In this manner, in the above-mentioned incremental forming method, as shown in the upper part of Figure 11, the minute convex portion Q1 among the minute irregularities that have occurred in the metal plate W is eliminated, and a metal plate W having a formed portion F as shown in Figure 12 is obtained.
[0024] In this case, in the incremental forming method, the amount of distortion of the minute protrusions Q1 is measured and the minute recesses Q1 are smoothed out and formed, so that minute recesses Q2 remain on the metal sheet W, as shown in the lower part of Fig. 11. However, when the minute unevenness is visually inspected, it is found that the height difference between the minute protrusions Q1 and the minute recesses Q2 causes noticeable surface distortion. Therefore, in the incremental forming method, at least the minute protrusions Q1 of the minute unevenness are eliminated to reduce the height difference, and thus it is possible to form a metal sheet W with less noticeable surface distortion.
[0025] In the above-mentioned incremental molding method, the entire area of the fine irregularities is smoothed using the lower mold 1, which essentially means that smoothing is also performed on the fine recesses Q2. As a result, the height difference of the fine irregularities is further reduced, and the surface distortion becomes almost unnoticeable.
[0026] According to the incremental forming method described in the above embodiment, it is possible to improve the surface precision and the appearance quality by eliminating or making inconspicuous the minute irregularities occurring around the formed portion F. As a result, the metal sheet W having the formed portion F manufactured by the incremental forming method is extremely useful for application to metal sheets that require high appearance quality, such as the outer panels of automobiles.
[0027] The configuration of the incremental forming method according to the present invention is not limited to the above-mentioned embodiment, and can be appropriately modified within the scope of the present invention. In addition, the above-mentioned embodiment illustrates a case where a concave-shaped formed portion is formed in a metal plate, but the present invention can also be applied to a case where a convex-shaped formed portion is formed in a metal plate using, for example, a tool, clamps that hold the periphery of the metal plate and move up and down, and a lower die. [Explanation of symbols]
[0028] F Molding part P1~P4 circular movement route Q1 Micro convex part Q2 Micro recess T-tool W Metal plate
Claims
1. A method for forming a metal plate into a three-dimensional shape by gradually deforming the metal plate in a thickness direction by pressing and moving a tip of a tool against the metal plate, comprising the steps of: A sequential forming method characterized in that after forming a concave or convex formed portion in the metal plate, the tip of the tool is pressed against and moved against minute irregularities that have occurred on the outside of the formed portion in the metal plate, thereby smoothing out the minute irregularities.
2. The incremental forming method according to claim 1, further comprising the step of smoothing out minute convex portions of the minute irregularities.
3. The incremental forming method according to claim 2, characterized in that after the forming portion is formed, the amount of distortion of the micro-convex portion is measured, and the lowest point of the measured micro-convex portion is set as the contact position with the tool, and the micro-convex portion is smoothed and formed.
4. The incremental forming method according to claim 2, characterized in that after the forming portion is formed, the amount of distortion of the minute convex portion is measured, and the amount of depression of the tool is set based on the measured value, thereby smoothing out and forming the minute convex portion.
5. The incremental forming method according to claim 1, characterized in that the tool is moved circularly along the peripheral portion of the formed portion in the metal plate, and the path of the circular movement is expanded so as to form a contour line outward from the peripheral portion of the formed portion, thereby smoothing out the minute irregularities.
Citation Information
Patent Citations
Sequential forming method and apparatus
JP2013244493A