Metal powder for additive manufacturing

A copper-containing powder with a rust prevention layer and reduction layer addresses inefficiencies in additive manufacturing by enhancing laser absorption and preventing oxidation, ensuring high-density and conductive models.

JP2024138621APending Publication Date: 2024-10-09JX NIPPON MINING & METALS CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023049192
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-27
Publication Date
2024-10-09

AI Technical Summary

Technical Problem

Copper and copper alloy powders used in additive manufacturing face challenges due to low laser absorption rates and high thermal conductivity, leading to inefficient melting or sintering, and oxidation during storage and modeling results in copper oxide formation, causing voids and reduced density in the modeled object.

Method used

A metal powder comprising copper-containing particles coated with a rust prevention layer, such as chromium oxide, to enhance laser absorption and suppress oxidation, along with a reduction layer to remove oxygen during modeling.

Benefits of technology

The solution effectively suppresses oxidation, improves laser absorption, and ensures high-density modeling by preventing copper oxide formation and maintaining electrical conductivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024138621000001_ABST
    Figure 2024138621000001_ABST
Patent Text Reader

Abstract

To provide a metal powder for additive manufacturing that effectively inhibits oxidation.SOLUTION: A metal powder for use in additive manufacturing comprises a copper-containing particle 1, and an anticorrosive layer 2 that covers at least part of the surrounding area of the copper-containing particle 1.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This specification discloses metal powders for use in additive manufacturing. [Background technology]

[0002] In metal additive manufacturing, which is one of the additive manufacturing (AM) technologies, for example, a laser beam or electron beam is irradiated onto a thin layer of metal powder based on cross-sectional data of the object to be created, and a layer is formed by melting and solidifying or sintering some of it. By repeatedly depositing metal powder on top of that and irradiating it with a laser beam, etc., the layers are stacked to create the object.

[0003] In order to manufacture a copper or copper alloy object, which has excellent electrical and thermal conductivity, by such additive manufacturing, copper powder or copper alloy powder is used as the metal powder.

[0004] Here, copper and copper alloys not only have low laser absorptivity, but also have high thermal conductivity, so that heat from the laser beam easily escapes. For this reason, copper powder and copper alloy powder cannot be sufficiently melted or sintered unless a laser beam with a higher output than normal is irradiated for a relatively long time, and additive manufacturing may not be performed efficiently. In response to this, for example, Patent Document 1 proposes "copper powder for 3D printers that has high absorptivity during laser irradiation and can be fused and bonded with a low-energy laser by enabling efficient heat input, and a method for manufacturing the same" with the aim of "providing copper powder for 3D printers that has high absorptivity during laser irradiation and can be fused and bonded with a low-energy laser by enabling efficient heat input, and a method for manufacturing the same." The copper powder has an absorptivity of 18.9% to 65.0% for light with a wavelength of λ=1060 nm, and an index indicated by the absorptivity / oxygen concentration for light with a wavelength of λ=1060 nm is 3.0 or more.

[0005] Furthermore, regarding copper alloy powder, Patent Document 2 describes "a metal powder for additive manufacturing, containing 0.10% by mass or more and 1.00% by mass or less of at least one of chromium and silicon, the total amount of the chromium and the silicon being 1.00% by mass or less, and the remainder being copper." Patent Document 2 states that such a "metal powder" "provides an additive manufacturing product made of a copper alloy that can achieve both mechanical strength and electrical conductivity." [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2018-178239 A [Patent Document 2] JP 2016-211062 A Summary of the Invention [Problem to be solved by the invention]

[0007] However, when additive manufacturing is performed using copper powder or copper alloy powder, copper oxide is generated by oxidation during storage or manufacturing, and this may remain without melting. This is undesirable because it causes voids to occur in the molded product after manufacturing and reduces the density of the molded product. Therefore, there is a demand for copper powder or copper alloy powder that can suppress the formation of copper oxide and can perform additive manufacturing well.

[0008] This specification provides a metal powder for additive manufacturing that can effectively suppress oxidation. [Means for solving the problem]

[0009] The metal powder for additive manufacturing disclosed in this specification contains copper-containing particles that contain copper, and an anti-rust layer that covers at least a portion of the periphery of the copper-containing particles. Effect of the Invention

[0010] According to the above-mentioned metal powder for additive manufacturing, oxidation can be effectively suppressed. [Brief description of the drawings]

[0011] [Figure 1] FIG. 2 is a cross-sectional view showing a schematic diagram of a surface-treated particle contained in the metal powder for additive manufacturing according to one embodiment. [Diagram 2] FIG. 4 is a cross-sectional view showing a schematic diagram of a surface-treated particle contained in a metal powder for additive manufacturing according to another embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, the embodiment of the metal powder for additive manufacturing and the manufacturing method thereof will be described in detail with reference to the drawings. Note that, although reference numerals will be used as necessary in the description, the reference numerals may be omitted when not necessary.

[0013] (metal powder) One embodiment of the metal powder for additive manufacturing (hereinafter, also simply referred to as "metal powder") includes surface-treated particles 3 in which at least a portion of the periphery of copper-containing particles 1 containing copper is covered with an anticorrosive layer 2, as shown typically in Fig. 1. The metal powder includes an aggregate of the copper-containing particles 1 and the surface-treated particles 3 including the anticorrosive layer 2.

[0014] The copper-containing particle 1 is made of copper or a copper alloy containing copper. In the case of the copper-containing particle 1 made of copper, the copper content of the metal powder is, for example, 99.9 mass% or more. In the case of the copper-containing particle 1 made of a copper alloy, the metal powder contains, for example, 90 mass% to 99.9 mass% copper, and may contain, as an alloy element, one or more selected from the group consisting of Al, Cr, Fe, Ni, Nb, P, Si, Zn, and Zr, or, when multiple types are included, may contain them in a total amount of 0.1 mass% to 10 mass%. The copper and alloy element contents of the metal powder can be measured by inductively coupled plasma optical emission spectrometry (ICP-OES).

[0015] Although copper and copper alloys can oxidize, the copper-containing particles 1 are prevented from oxidizing by preventing oxygen from penetrating into them due to the anticorrosive layer 2. This effectively prevents the formation of copper oxide due to oxidation of the copper-containing particles 1 during storage of the metal powder or during modeling when the metal powder is used in additive manufacturing, and ultimately prevents the generation of voids in the modeled object due to the copper oxide, which is believed to enable the production of high-density models.

[0016] Furthermore, when the anti-rust layer 2 has a higher laser absorptivity than the copper-containing particle 1, the anti-rust layer 2 may be able to improve the laser absorptivity of the surface-treated particle 3. This is presumably because the copper-containing particle 1 is coated with the anti-rust layer 2, and the heat from the laser beam is easily absorbed by the copper-containing particle 1 during molding due to the coating of the anti-rust layer 2, which has a relatively high laser absorptivity, and this promotes melting or sintering of the copper-containing particle 1. Furthermore, depending on the material of the anti-rust layer 2, many of its components are gasified and lost during molding, so that the effect of the anti-rust layer 2 on the molded product can be kept small.

[0017] The anticorrosive layer 2 may be any layer capable of suppressing oxidation of the copper-containing particle 1, and specifically includes, for example, a layer containing chromium oxide such as Cr2O3, zinc phosphate, manganese phosphate, or other phosphates, or an organic coating such as benzotriazole. Therefore, the anticorrosive layer 2 may contain at least one selected from the group consisting of chromium oxide, phosphate, and benzotriazole.

[0018] Among them, the anticorrosive layer 2 containing chromium oxide is preferable because the reduction does not proceed up to high temperatures and therefore a high laser absorptivity can be maintained up to high temperatures. As chromium oxide, there are several chromium oxides (CrO, Cr2O3, CrO2, CrO3, etc.) according to the oxidation number of chromium, and it is preferable that the anticorrosive layer 2 contains Cr2O3 among them. This is because when Cr2O3 is contained, it is stable up to high temperatures.

[0019] It can be confirmed by X-ray photoelectron spectroscopy (XPS) that the anticorrosive layer 2 covering the periphery of the copper-containing particle 1 contains the above-mentioned chromium oxide or phosphate. In the case of chromium oxide, a peak appears at a binding energy of about 40-50 eV, and in the case of phosphate, a peak appears at a binding energy of about 125-135 eV. Benzotriazole in the anticorrosive layer 2 can be confirmed by Fourier transform infrared spectroscopy (FT-IR) or the like.

[0020] When the rust-preventive layer 2 of the surface-treated particles 3 contains chromium oxide, the metal powder containing such surface-treated particles 3 contains chromium. The chromium content of the metal powder is preferably 50 ppm by mass to 1000 ppm by mass, more preferably 100 ppm by mass to 700 ppm by mass. If the chromium content is too low, the laser absorptivity may not be improved significantly. On the other hand, if the chromium content is too high, the electrical conductivity of a molded object produced using the metal powder may decrease. The chromium content of the metal powder can be measured by inductively coupled plasma optical emission spectrometry (ICP-OES).

[0021] In addition, the coverage of the anticorrosive layer 2 is related to the degree of inhibition of oxidation of the copper-containing particle 1 by the anticorrosive layer 2. If the anticorrosive layer 2 is formed so as to cover at least a part of the periphery of the copper-containing particle 1, the oxidation of the copper-containing particle 1 can be inhibited. From the viewpoint of further inhibiting oxidation, the anticorrosive layer 2 preferably covers the periphery of the copper-containing particle 1 at a coverage of 50% or more of the entire surface area of ​​the copper-containing particle 1. It is particularly preferable that the coverage of the anticorrosive layer 2 is approximately 100%. The coverage of chromium can be calculated by performing image processing such as binarization on an image obtained using a detection method capable of identifying the position of an element, such as WDS (wavelength dispersive X-ray analysis). WDS can identify the amount of Cr element present in which part of the metal powder, and therefore can be used as an index of the coverage of Cr that covers the metal powder. More specifically, for example, the WDS mapping obtained by JXA-8530F manufactured by JEOL Ltd. is binarized at a position of 1 / 10 of the maximum signal intensity using the accompanying software, and the area occupied by Cr (area of ​​the part that is 1 / 10 or more of the maximum signal intensity) is calculated from the total area occupied by the metal powder, thereby calculating the coverage rate. Here, the area of ​​the part that is 1 / 10 or more of the maximum signal intensity means the area calculated by excluding by binarization the part that is less than 1 / 10 of the maximum signal intensity detected by the detector when the entire metal powder is analyzed by WDS. For example, if the signal intensity when the entire metal powder is scanned is 15 to 400, the corresponding part will have a signal intensity of 40 to 400.

[0022] The metal powder may contain oxygen. Oxygen may be contained in the metal powder due to, for example, chromium oxide or phosphate that may be contained in the anticorrosive layer 2, manufacturing conditions, a naturally generated oxide film, unavoidably mixed oxygen, and the like. The oxygen content of the metal powder is preferably 50 ppm by mass to 2000 ppm by mass, and more preferably 100 ppm by mass to 1000 ppm by mass. If the oxygen content is too low, there is a possibility that a coating such as the anticorrosive layer 2 will not adhere and the effect of inhibiting oxidation cannot be obtained. On the other hand, if the oxygen content is too high, there is a concern that voids may easily occur in the molded product due to the generation of copper oxide during molding.

[0023] The oxygen content of metal powder can be measured by the inert gas fusion method. Here, two measurements are taken for a 1g sample of metal powder using a LECO TCH600, and the average value is taken as the oxygen content.

[0024] In order to reduce the oxygen content of the metal powder and suppress the generation of voids in the molded product, the anticorrosive layer 2 is desirably formed around the copper-containing particles 1 to a thickness of 10 nm to 200 nm, and further 10 nm to 100 nm, when the anticorrosive layer 2 contains oxygen in the form of chromium oxide or the like as described above. The thickness of the anticorrosive layer 2 can be measured using X-ray photoelectron spectroscopy (XPS) under the following device and conditions by irradiating the surface-treated particles 3 with Ar ions to dig into the particles and detect the thickness. Depending on the particle size of the metal powder, the detection area described below may include one to three surface-treated particles 3. Equipment: PHI 5000 Versa Probe II manufactured by ULVAC-PHI Inc. Ultimate vacuum: 8.2×10 -8 Pa Excitation source: Monochromatic AlKα Output: 25.0W Detection area: 100μmΦ Sputter rate: 2kV 2mm×2mm (4.2nm / min) (SiO2 equivalent)

[0025] As shown in Fig. 2, the metal powder preferably includes a surface-treated particle 13 further including a reduction layer 14 that covers at least a portion of the periphery of the anticorrosive layer 12. When the reduction layer 14 is provided on the anticorrosive layer 12, it is expected that oxygen that may be contained in the anticorrosive layer 12, etc., is removed by the reduction layer 14 during shaping. In particular, when the reduction layer 14 is formed on the anticorrosive layer 12 that contains chromium oxide, it is presumed that the chromium oxide of the anticorrosive layer 12 is reduced by the reduction layer 14 during shaping, and oxygen is removed, while chromium is diffused into the copper-containing particle 11 or the shaped object. The diffusion of chromium can improve the heat dissipation properties of the shaped object.

[0026] The reduced layer 14 may contain one or more of a group of carbon materials including inorganic carbon such as graphite and organic matter. Among them, the reduced layer 14 preferably contains graphite in terms of laser absorptivity and heat resistance. When the reduced layer 14 contains graphite, oxygen contained in chromium oxides and the like in the rust-preventive layer 12 may be gasified and lost in the form of carbon monoxide, carbon dioxide, and the like during shaping. In consideration of this, it is desirable to adjust the graphite or carbon content in the metal powder so that no carbon remains in the shaped object obtained after shaping.

[0027] The fact that the reduced layer 14 contains graphite can be confirmed by Raman spectroscopy. More specifically, in a Raman spectrum obtained by Raman spectroscopy, a Raman shift of 1300 cm -1 ~1700cm -1 When a peak of scattering intensity is present within the range, it is recognized that the material contains graphite. For the analysis by Raman spectroscopy, inVia (registered trademark) manufactured by Renishaw Corporation can be used.

[0028] The metal powder may contain carbon due to the reduced layer 14 containing graphite, etc. The carbon content of the metal powder is preferably 20 ppm by mass to 800 ppm by mass. If the carbon content is too low, there is a concern that oxygen may not be sufficiently removed by reduction during shaping. On the other hand, if the carbon content is too high, carbon may remain in the shaped product, which may easily cause voids in the shaped product.

[0029] The carbon content of metal powders can be measured by the inert gas fusion method, in which a 1g sample of metal powder is measured twice using a LECO TCH600, and the average value is taken as the carbon content.

[0030] The average particle diameter D50 of the metal powder is preferably 10 μm to 150 μm. By not making the average particle diameter D50 too small, the metal powder is less likely to fly around during molding, making it easier to handle, and the required fluidity is exhibited, allowing it to be spread in the intended location, improving moldability. By keeping the average particle diameter D50 at a certain level, the energy required to melt or sinter the metal powder with a laser beam can be kept small, and the precision of the molding can be improved.

[0031] The above-mentioned average particle diameter D50 means the particle diameter at which the cumulative volume-based frequency of the metal powder is 50% in the particle diameter histogram (particle diameter distribution graph) obtained by measuring the particle diameter of the metal powder using a laser diffraction / scattering type particle diameter distribution measuring device, and is measured based on JIS Z8825 (2013). More specifically, the average particle diameter D50 can be measured using MT3300EXII manufactured by Microtrack Bell, Inc., with pure water as the solvent and a refractive index of 1.33.

[0032] (Manufacturing method) To produce the metal powder as described above, for example, copper powder or copper alloy powder is first prepared. The copper powder or copper alloy powder may be prepared by purchasing already produced powder or by other methods, but may also be produced by atomization or other methods.

[0033] The copper powder mainly contains copper-containing particles, and the copper content is preferably 99.9% by mass or more (purity of 3N or more). The copper alloy powder mainly contains copper-containing particles made of a copper alloy. The copper alloy powder may contain at least one alloy element selected from the group consisting of Al, Cr, Fe, Ni, Nb, P, Si, Zn, and Zr, and may have a copper content of 80% by mass or more, further 85% by mass or more, further 90% by mass or more, and further 99% by mass or more.

[0034] The copper powder or copper alloy powder is preferably adjusted in particle size by sieving or the like as necessary to have an average particle diameter D50 of 10 μm to 150 μm. This average particle diameter D50 is the same as the average particle diameter D50 described above for the metal powder, and can be measured by the same method.

[0035] The copper powder or copper alloy powder may contain oxygen. When the oxygen content of the copper powder or copper alloy powder is 500 mass ppm or more, it is preferable to perform a treatment to remove oxygen from the copper powder or copper alloy powder and reduce the oxygen content prior to the formation of the rust-proof layer described below. The oxygen removal treatment may be, for example, a method such as washing with an acid.

[0036] Thereafter, the copper-containing particles in the copper powder or copper alloy powder are subjected to a rust-preventive treatment in order to form a rust-preventive layer that covers at least a part of the periphery of the particles. Specifically, when forming a rust-preventive layer containing chromium oxide, the copper powder or copper alloy powder is immersed in a dichromate solution having a concentration of 0.1 to 5.0% and a liquid temperature of room temperature to 80° C. for 5 to 180 minutes, and then the copper-containing particles are subjected to a chromate treatment. The chromium content attached to the copper-containing particles can be increased or decreased by changing the concentration of the potassium dichromate solution or the treatment time. Alternatively, to form a rust-preventive layer containing phosphate, the copper-containing particles can be subjected to a phosphate treatment. Specifically, for example, the copper powder or copper alloy powder is immersed in a zinc phosphate solution. By such a rust-preventive treatment, the copper powder or copper alloy powder becomes a metal powder containing surface-treated particles 3 as shown in FIG. 1.

[0037] When producing a metal powder containing surface-treated particles 13 as shown in FIG. 2, the metal powder after the rust-proofing treatment is further subjected to a treatment for forming a reduction layer that covers at least a part of the periphery of the rust-proofing layer.

[0038] Here, for example, a ball mill or a mortar can be used to mix the metal powder after the rust prevention treatment with the carbon-based material for the reduction layer. Alternatively, the metal powder after the rust prevention treatment can be brought into contact with a liquid carbon-based material by immersion or the like, and then heated in an inert atmosphere such as nitrogen at a temperature of, for example, 400°C to 1000°C for 2 hours to 12 hours to form a reduction layer around the rust prevention layer. Alternatively, the reduction layer can be formed by chemical vapor deposition (CVD) using a carbon-based material. Examples of carbon-based materials include carbon black, coal tar, pitch, coke, and organic compounds.

[0039] At this time, it is desirable to form a reduction layer around the rust-preventive layer while adjusting the carbon content to an appropriate level according to the oxygen content of the metal powder.

[0040] By carrying out the above-described process, a metal powder including copper-containing particles, an anticorrosive layer, and a reduced layer can be produced. EXAMPLES

[0041] Next, the metal powder for additive manufacturing described above was prototyped and its effects were confirmed, which will be described below. However, the description here is merely for illustrative purposes and is not intended to be limiting.

[0042] Pure copper powder having an average particle size D50 of about 30 μm to 45 μm was prepared. The copper content of this copper powder was 99.9 mass %, and the oxygen content was 100 mass ppm.

[0043] Example 1 The above copper powder was immersed in a 5% by mass aqueous solution of potassium dichromate, and the copper-containing particles of the copper powder were coated with an anti-rust layer to produce a metal powder.

[0044] Example 2 The above copper powder was immersed in a 1 mass % aqueous potassium dichromate solution, and the copper-containing particles of the copper powder were coated with an anti-rust layer to produce a metal powder.

[0045] Example 3 The above copper powder was immersed in a 5% by mass aqueous solution of potassium dichromate to coat the copper-containing particles of the copper powder with an anti-rust layer, and then immersed in a coal tar solution and heat-treated at 800°C for 8 hours in a nitrogen atmosphere to produce a metal powder in which a reduced layer with a controlled carbon content was formed around the anti-rust layer.

[0046] Comparative Example 1 The copper powder was used as it was as metal powder without any surface treatment.

[0047] (evaluation) The average particle diameter D50, chromium content, coverage of the anticorrosive layer, carbon content, and oxygen content (amount of O before oxidation) of each of the above metal powders measured by the above-mentioned method are shown in Table 1. The metal powders of Examples 1 to 3 were analyzed by the above-mentioned method, and it was confirmed that the metal powders contained chromium oxide Cr2O3.

[0048] To confirm the effect of each metal powder, an accelerated oxidation test was conducted by heating the metal powder in air at 150°C for 24 hours. The oxygen content of the metal powder after the test (O content after oxidation) was measured, and the oxidation rate was calculated as the ratio of the oxygen content before and after the test. If the oxidation rate exceeded 1000%, it was determined that the oxidation of the metal powder had progressed. The results are shown in Table 1.

[0049] [Table 1]

[0050] In Comparative Example 1, the oxidation rate was 1100%, and oxidation progressed, whereas in Examples 1 to 3, oxidation hardly progressed and all oxidation rates were less than 1000%, confirming that the formation of an anti-rust layer by surface treatment is effective in suppressing oxidation.

[0051] From the above, it was found that the above-mentioned metal powder is one in which oxidation is effectively suppressed. [Explanation of symbols]

[0052] 1, 11 Copper-containing particles 2, 12 Anti-rust layer 3, 13 Surface-treated particles 14 Reduction layer

Claims

1. A metal powder for use in additive manufacturing, comprising: A metal powder for additive manufacturing comprising copper-containing particles that contain copper and an anti-rust layer that covers at least a portion of the periphery of the copper-containing particles.

2. The metal powder for additive manufacturing according to claim 1 , wherein the anti-corrosive layer contains at least one selected from the group consisting of chromium oxide, phosphate, and benzotriazole.

3. The anticorrosive layer contains Cr as the chromium oxide. 2 O 3 The metal powder for additive manufacturing according to claim 2, comprising:

4. The metal powder for additive manufacturing according to claim 3, wherein the chromium content is 50 ppm by mass to 1000 ppm by mass.

5. The metal powder for additive manufacturing according to claim 3, having an oxygen content of 50 ppm by mass to 2000 ppm by mass.

6. The metal powder for additive manufacturing according to any one of claims 1 to 5, wherein the average particle diameter D50 is 10 µm to 150 µm.

Citation Information

Patent Citations

  • Copper powder

    JP2019183242A

  • Additively manufactured components and methods

    JP2020529516A

  • Sinterable metal pastes for use in additive manufacturing

    JP2022028730A

  • Copper alloy powder, manufacturing method of laminate molded article and laminate molded article

    JP2016211062A

  • Copper powder, manufacturing method therefor, and manufacturing method of solid molded article