Automatic lamination apparatus, and method of manufacturing thermoplastic resin composite material sheet
The automatic lamination device addresses oxidative deterioration and residual stress in thermoplastic resin composite sheets by heating from both inside and outside with laser light and radiant heat, achieving high productivity and improved mechanical properties in the final products.
Patent Information
- Application Number
- JP2023050804
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing methods for producing thermoplastic resin composite sheets face issues such as oxidative deterioration, residual stress due to temperature differences, and insufficient fusion bonding between layers, especially when using high resin flow initiation temperature materials, leading to decreased mechanical properties and molding challenges.
An automatic lamination device that heats thermoplastic resin composite tapes from both inside and outside using distinct methods, including laser light for reinforcing fibers and radiant heat or thermal conduction for the resin, with temperature control and pressure application to ensure uniform heating and bonding.
The device achieves high productivity in producing thermoplastic resin composite sheets with improved quality by preventing resin deterioration and ensuring sufficient fusion bonding without carbonization, resulting in molded products with reduced residual stress and enhanced mechanical properties.
Smart Images

Figure 2024139873000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an automatic lamination device for producing a thermoplastic resin composite sheet by automatically laminating a thermoplastic resin composite tape containing a thermoplastic resin and reinforcing fibers, and a method for producing a thermoplastic resin composite sheet by laminating a thermoplastic resin composite tape containing a thermoplastic resin and reinforcing fibers. [Background technology]
[0002] Molded articles obtained by molding thermoplastic composite materials containing reinforcing fibers, such as prepregs, are lightweight and have excellent mechanical properties, and therefore are widely used in a variety of applications, from sports and leisure to industrial applications such as automobiles and aircraft.
[0003] As a method for molding a thermoplastic resin composite sheet, for example, a laminate molding method is used in which a tape-shaped thermoplastic resin composite sheet is heated by a laser or the like, a thermoplastic resin composite sheet is arranged, and the sheet is cooled while being pressurized to obtain a molded product. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2018-149729 A Summary of the Invention [Problem to be solved by the invention]
[0005] In Patent Document 1, two heating devices are provided, but both of the heating methods use radiation heat or thermal conduction, and one of the heating devices heats the surface to be attached, not the thermoplastic resin composite tape. Since the area around the area to be attached is widely heated, oxidation deterioration of the resin of the thermoplastic resin composite sheet that is already in place progresses. In addition, since only the surface is heated by radiation or thermal conduction, a temperature difference occurs between the inside and outside of the thermoplastic resin composite tape, and residual stress occurs even after cooling. If heating by radiation or conduction is increased in order to reduce the temperature difference between the inside and outside, the outside will melt more, causing the resin to flow and making it difficult to transport the tape.
[0006] The present invention aims to provide an automatic lamination device capable of automatically laminating thermoplastic resin composite tapes to obtain a thermoplastic resin composite sheet, and capable of realizing the production of a molded product with high productivity while suppressing deterioration in quality. The present invention also aims to provide a manufacturing method for a thermoplastic resin composite sheet capable of producing a molded product by molding a thermoplastic resin composite sheet with high productivity while suppressing deterioration in quality of the thermoplastic resin composite sheet obtained by laminating thermoplastic resin composite tapes. Note that the problems solved by each embodiment of the present invention may be explicitly or implicitly disclosed in this specification. In addition, when using a thermoplastic resin composite tape made of a resin with a high resin flow starting temperature, such as engineering plastics or super engineering plastics, the laser output must be increased. Furthermore, in order to increase the molding speed, the output must be increased, and rapid heating can lead to carbonization of the resin, making molding impossible. Conversely, lowering the output can lead to insufficient fusion between the layers, resulting in a decrease in mechanical properties. Another object of the present invention is to provide an automatic lamination device that can perform lamination in such cases without carbonizing the resin and with sufficient fusion between the layers. [Means for solving the problem]
[0007] The present invention includes the following aspects. [1] An automatic lamination apparatus for automatically laminating a thermoplastic resin composite tape containing a thermoplastic resin and reinforcing fibers on a table to manufacture a thermoplastic resin composite sheet, the automatic lamination apparatus comprising: a means (A) for heating the thermoplastic resin of the thermoplastic composite tape; a means (B) separate from the means (A) for heating the reinforcing fibers of the thermoplastic resin composite tape; a means (C) for laminating the thermoplastic resin composite tape; and a means (D) for applying pressure to the laminated thermoplastic resin composite tape.
[0008] [2] The automatic lamination apparatus according to [1], wherein the means (B) includes a heating means using a laser beam. [3] The automatic lamination apparatus according to [2], wherein the wavelength of the laser light is 800 to 2500 nm. [4] The automatic lamination apparatus according to any one of [1] to [3], comprising, as the means (A), at least one heating means selected from the group consisting of radiant heat and thermal conduction. [5] The automatic lamination apparatus according to [3], wherein the at least one heating means selected from the group consisting of an infrared heater, hot air, and a hot plate is used as the at least one heating means of radiant heat and thermal conduction. [6] The automatic lamination apparatus according to any one of [1] to [5], further comprising a means (E) for controlling the temperature of the thermoplastic resin composite tape. [7] The automatic lamination apparatus according to any one of [1] to [6], wherein the means (E) includes a means for detecting temperature and a means for adjusting the output of the heating device. [8] The automatic laminating apparatus according to [7], wherein the means (E) is provided between the thermoplastic resin composite tape and the table.
[0009] [9] A method for manufacturing a thermoplastic resin composite sheet by laminating thermoplastic resin composite tapes containing a thermoplastic resin and reinforcing fibers, the method comprising the steps of: a step (A) of heating the thermoplastic resin in the thermoplastic resin composite tape; a step (B) of heating the reinforcing fibers in a thermoplastic resin composite tape separate from step (A); a step (C) of laminating the thermoplastic resin composite tapes; and a step (D) of pressing the laminated thermoplastic resin composite tapes.
[0010]
[10] The method for producing a thermoplastic resin composite sheet according to [9], comprising the step of heating with laser light as the step (B).
[11] The method for producing a thermoplastic resin composite sheet according to
[10] , wherein the wavelength of the laser light is 800 to 2500 nm.
[12] A method for producing a thermoplastic resin composite sheet according to any one of [9] to
[11] , comprising, as the step (A), at least one heating step of radiant heat and thermal conduction.
[13] The method for producing a thermoplastic resin composite sheet according to
[12] , wherein the at least one heating step of radiant heat and thermal conduction includes at least one heating step selected from an infrared heater, hot air, and a hot plate.
[14] The method for producing a thermoplastic resin composite sheet according to any one of [9] to
[13] , further comprising a step (E) of controlling the temperature of the thermoplastic resin composite tape.
[15] The method for producing a thermoplastic resin composite sheet according to
[14] , wherein step (E) includes a step of detecting temperature and a step of adjusting the output of a heating device. Effect of the Invention
[0011] According to the present invention, an automatic lamination device is provided that can be applied to molding of thermoplastic resin composite sheets by automatic lamination, and can achieve high productivity of molded products while suppressing deterioration in quality. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a diagram showing an example of the automatic lamination device of the present invention. [Diagram 2] FIG. 2 is a diagram showing an example of the automatic lamination device of the present invention. [Diagram 3] FIG. 3 is a diagram showing an example of the automatic lamination device of the present invention. [Figure 4] FIG. 4 is a diagram showing an example of the automatic lamination device of the present invention. [Diagram 5] FIG. 5 is a diagram showing an example of the automatic lamination device of the present invention. [Figure 6] FIG. 6 is a diagram showing an example of the automatic lamination device of the present invention. [Figure 7] FIG. 7 is a schematic diagram showing heating of a thermoplastic resin by radiant heat or thermal conduction. [Figure 8] FIG. 8 is a schematic diagram showing heating of reinforcing fibers and a thermoplastic resin by laser light. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] [Automatic stacking device] The automatic lamination apparatus of the present invention is an automatic lamination apparatus for producing a thermoplastic resin composite sheet by automatically laminating a thermoplastic resin composite tape containing a thermoplastic resin and reinforcing fibers, and is equipped with a means (A) for heating the thermoplastic resin of the thermoplastic composite tape, a means (B) separate from the means (A) for heating the reinforcing fibers of the thermoplastic resin composite tape, a means (C) for laminating the thermoplastic resin composite tape, and a means (D) for pressurizing the laminated thermoplastic resin composite tape.
[0014] By providing means (A) and means (B) different from means (A), the thermoplastic resin composite tape is heated from the inside and outside, the temperature of the thermoplastic resin composite tape can be uniformly increased throughout the thickness direction, and temperature control is also made easier.
[0015] In addition, the order of the means (A) and the means (B) may be any, since the thermoplastic resin composite tape may be heated by the means (A) after the thermoplastic resin is heated simultaneously with or following the heating of the reinforcing fibers in the means (B), and the outside and inside of the thermoplastic resin composite tape can be heated. Also, the means (A) for heating the thermoplastic resin and the means (B) for heating the reinforcing fibers may be performed simultaneously, but the heating means are different.
[0016] The automatic lamination device of the present invention will be described below. Note that the dimensions and device configurations shown in the drawings in the following description are merely examples, and the present invention is not necessarily limited thereto, and can be appropriately modified and implemented within the scope of the present invention.
[0017] <Means (A)> Means (A) is a means for heating the thermoplastic resin. This means (A) may be any type that can heat the thermoplastic resin composite sheet from the outside. For example, means (A) may be at least one heating means selected from radiant heat and direct heat conduction from a heat source. Specifically, means (A) may be at least one heating means selected from a hot plate, an infrared heater, and hot air. It is preferable that the amount of heat emitted by each of means (A) is adjustable.
[0018] When the means (A) is radiant heat or direct heat conduction from a heat source, the thermoplastic resin composite sheet can be effectively heated from the outside. The heating temperature in means (A) is preferably controlled to be between the glass transition temperature and the melting point if the resin raw material of the thermoplastic resin composite sheet is a crystalline resin, and to be between the glass transition temperature and the glass transition temperature + 100°C if the resin raw material is an amorphous resin.
[0019] <Means (B)> The means (B) is a means for heating the reinforcing fibers separately from the means (A). As described above, the means (B) may be a means for heating the thermoplastic resin when heating the reinforcing fibers or following heating of the reinforcing fibers, but it is a means for mainly heating the reinforcing fibers rather than the thermoplastic resin.
[0020] Such a means (B) preferably includes a heating means using laser light. When the means (B) is a heating means using laser light, the laser light preferably has a wavelength of 800 to 2500 nm. Light with a wavelength of 800 to 2500 nm can usually pass through the resin and heat the reinforcing fibers. Furthermore, the heat of the heated reinforcing fibers can be transferred to the resin, and the thermoplastic resin composite sheet can be heated from the inside. The wavelength of the laser light is more preferably 900 nm or more, and even more preferably 1000 nm or more, while more preferably 2000 nm or less, and even more preferably 1500 nm or less. By being equal to or more than the lower limit, the reinforcing fibers can be heated, while by being equal to or less than the upper limit, the thermoplastic resin is not directly heated, and the reinforcing fibers can be efficiently heated. The output of the laser light used in the means (B) for heating the reinforcing fibers is preferably 0.5 kW or more, more preferably 1 kW or more, and even more preferably 3 kW or more, while it is preferably 25 kW or less, more preferably 15 kW or less, and even more preferably 12 kW or less. By being below the upper limit, excess heat is not generated and the resin is not burned, and by being above the lower limit, the reinforcing fibers can be heated.
[0021] This means (B) is not limited to a heating means using laser light, but may be any means having a heat source capable of locally heating the reinforcing fibers in the thermoplastic resin composite sheet. The wavelength of the laser light used in the means (B) 2 for heating the reinforcing fibers is preferably 800 nm or more, more preferably 900 nm or more, and even more preferably 1000 nm or more, while it is preferably 2500 nm or less, more preferably 2000 nm or less, and even more preferably 1500 nm or less. By being equal to or more than the lower limit, the reinforcing fibers can be heated, and by being equal to or less than the upper limit, the thermoplastic resin is not heated, so that the reinforcing fibers can be efficiently heated. The output of the laser light used in the means (B) for heating the reinforcing fibers is preferably 0.5 kW or more, more preferably 1 kW or more, and even more preferably 3 kW or more, while it is preferably 25 kW or less, more preferably 15 kW or less, and even more preferably 12 kW or less. By being below the upper limit, excess heat is not generated and the resin is not burned, and by being above the lower limit, the reinforcing fibers can be heated.
[0022] <Means (C)> The heated thermoplastic resin composite tape is laminated by means (C). Specifically, means (C) is preferably laminated by a robot arm.
[0023] The thermoplastic resin composite tape may be directly laminated on the attachment portion on which the tape on the table on which the thermoplastic resin composite tape is laminated by the means (C) is placed, or a mold may be placed, or a thermoplastic resin composite tape may already be placed. When a mold is placed, the thermoplastic resin composite tape is placed on the mold. When a thermoplastic resin composite sheet is already placed on the mold, a thermoplastic resin composite tape may be further placed on the thermoplastic resin composite sheet already placed. In particular, when a thermoplastic resin composite tape is further placed on a thermoplastic resin composite sheet, a method of heating the newly placed thermoplastic resin composite sheet with laser light is preferable, since a new thermoplastic resin composite tape can be placed without heating the thermoplastic resin composite sheet already placed.
[0024] <Means (D)> The means (D) is a means for pressurizing the laminated thermoplastic resin composite tape. By using this means (D), the thermoplastic resin composite tape can be pressed onto the target portion.
[0025] The means (D) is preferably performed by a pressure roll. The material, shape and dimensions of the pressure roll are not particularly limited and may be appropriately designed, but it is recommended to use a pressure roll having elasticity and excellent temperature controllability.
[0026] <Means (E)> The automatic laminating apparatus of the present invention preferably comprises a means (E) for controlling the temperature of the thermoplastic resin composite tape.
[0027] The means (E) preferably includes a non-contact thermometer or thermography as a means for measuring temperature, and measures the temperature of the thermoplastic resin composite tape being fed. By detecting the temperatures at these locations, the temperature of the thermoplastic resin composite tape can be accurately known. The temperature control means preferably has a means for measuring the temperature of the thermoplastic resin composite tape and an output adjustment means for changing the output of at least one of the means (A) for heating the thermoplastic resin and the means (B) for heating the reinforcing fibers. The means for measuring the temperature of the thermoplastic resin composite tape may be a means for directly measuring the temperature of the thermoplastic resin composite tape itself, or a means for indirectly measuring the temperature of the thermoplastic resin composite tape by measuring the temperature of a table or the like that is in thermal equilibrium with the thermoplastic resin composite tape.
[0028] <Transportation section> The automatic laminating apparatus of the present invention is usually equipped with a conveying section, which is provided with rolls or the like so that the thermoplastic resin composite tape wound on a bobbin or the like is fed out and supplied parallel to the molding surface. The position of the transport roll is arbitrary, and any roll may be used as long as the transport can be performed without bending or turning over. The material, shape and dimensions of the transport roll are not particularly limited and may be appropriately designed. Examples of the roll include a metal roll, a resin roll, a rubber roll, a silicon roll and a ceramic roll.
[0029] <Thermoplastic resin tape> The thermoplastic resin composite tape is not particularly limited, and examples thereof include a thermoplastic resin composite material containing a thermoplastic resin and a reinforcing fiber. Specific examples of the thermoplastic resin composite material include a prepreg in which a reinforcing fiber is impregnated with a thermoplastic resin, and a laminate in which a reinforcing fiber and a thermoplastic resin film are laminated.
[0030] (Reinforced Fiber) Examples of reinforcing fibers include carbon fibers, glass fibers, and metal fibers. Among them, carbon fibers are preferred from the viewpoint of rigidity and strength. As the reinforcing fibers, one type may be used alone, or two or more types may be used in combination. Examples of carbon fibers include polyacrylonitrile (PAN)-based, petroleum / coal pitch-based, rayon-based, and lignin-based. In addition, carbon fiber is preferable because it can more efficiently absorb laser light and convert it into heat.
[0031] A reinforcing fiber bundle can be produced by bundling a plurality of reinforcing fibers and applying a sizing agent thereto. As the reinforcing fiber bundle, a tow consisting of 3,000 to 60,000 reinforcing fibers (filaments) is preferred because it has excellent productivity on an industrial scale and mechanical properties.
[0032] In terms of facilitating the production of molded articles having excellent tensile strength, the strand strength of the reinforcing fiber bundle is preferably 4000 MPa or more, and more preferably 5000 MPa or more. In terms of the ease of developing sufficient rigidity in a molded article, the strand modulus of the reinforcing fiber bundle is preferably 200 GPa or more, more preferably 230 GPa or more. In terms of the ease of suppressing the decrease in strength in the fiber cross-sectional direction and compressive strength in the fiber axial direction by reducing the graphite crystal size on the surface and inside of the reinforcing fiber, the strand modulus of the reinforcing fiber bundle is preferably 380 GPa or less, more preferably 350 GPa or less. The lower and upper limits of the strand modulus of the reinforcing fiber bundle can be arbitrarily combined, and for example, 200 to 380 GPa is preferable. The strand strength and strand modulus of the reinforcing fiber bundle are measured by a method in accordance with ASTM D4018.
[0033] A reinforcing fiber substrate can be formed by orienting the reinforcing fiber bundles. Examples of the form of the reinforcing fiber substrate include a unidirectional continuous fiber form in which continuous reinforcing fiber bundles are aligned in one direction, a plain weave, twill weave, satin weave, non-crimp fabric (NCF), three-dimensional fabric, and other woven forms using continuous reinforcing fiber bundles, and a continuous strand mat or chopped strand mat using reinforcing fiber bundles. In order to maintain the arrangement of the fabric, a fixing method such as stitching with reinforcing fibers or welding of thermosetting resin or thermoplastic resin fibers can be applied.
[0034] The proportion of the reinforcing fibers in the reinforcing fiber substrate is preferably 80 mass % or more, more preferably 90 mass % or more, further preferably 95 mass % or more, and particularly preferably 100 mass %, based on the total mass of the reinforcing fiber substrate.
[0035] In order to obtain molded products having excellent mechanical properties, the sizing agent adhesion rate of the reinforcing fiber substrate is preferably 0.1% by mass or more, and more preferably 0.2% by mass or more, since the reinforcing fibers are sufficiently converged to prevent fuzzing during the production of the molding material. The sizing agent adhesion rate of the reinforcing fiber substrate is preferably 5.0% by mass or less, more preferably 3.0% by mass or less, and even more preferably 1.5% by mass or less. The lower and upper limits of the sizing agent adhesion rate of the reinforcing fiber substrate can be arbitrarily combined, and for example, 0.1 to 5.0% by mass is preferable, 0.2 to 3.0% by mass is more preferable, and 0.2 to 1.5% by mass is even more preferable.
[0036] (thermoplastic resin) The thermoplastic resin is not particularly limited, and examples thereof include polypropylene resin, polyamide resin, polycarbonate resin, polyphenylene sulfide resin, polyether sulfone resin, polyether imide resin, polyether ether ketone resin, and polyether ketone ketone resin. Among them, the thermoplastic resin preferably includes polyamide resin, polyphenylene sulfide resin, polyether imide resin, polyether ether ketone resin, or polyether ketone ketone resin. The thermoplastic resin may be used alone or in combination of two or more kinds.
[0037] As long as the effects of the invention are not impaired, various additives such as known thermosetting resins, fillers, heat stabilizers, antioxidants, antiaging agents, flame retardants, and pigments may be contained in the thermoplastic resin as necessary. The method for producing the thermoplastic composite material is not particularly limited, and may involve impregnating a molten thermoplastic resin into a reinforcing fiber substrate, impregnating a monomer or low molecular weight substance that forms a thermoplastic resin into a reinforcing fiber substrate and then polymerizing the same, or may involve a laminate in which a thermoplastic resin is disposed on a reinforcing fiber substrate.
[0038] The method for producing the thermoplastic resin composite tape is not particularly limited, and known methods can be used. For example, the method can be performed by using a drawing die by drawing. The melting temperature can be appropriately adjusted depending on the type and mixing ratio of the resin, and the presence or absence and type of additives. For example, the cooling can be performed by contacting the tape with a cooling machine such as a cooled roll.
[0039] From the viewpoint of lamination efficiency, the thickness of the thermoplastic resin composite tape is preferably 0.015 mm or more, and more preferably 0.040 mm or more. From the viewpoint of heating efficiency, the thickness of the molding material is preferably 0.5 mm or less, and more preferably 0.35 mm or less. The lower limit and the upper limit of the thickness of the thermoplastic resin composite tape can be arbitrarily combined, and for example, 0.015 to 0.5 mm are preferable, and 0.040 to 0.35 mm are more preferable.
[0040] For ease of arrangement of the thermoplastic resin composite tape, the width of the thermoplastic resin composite tape is preferably 0.3 mm or more and 500 mm or less, and particularly preferably 5 mm or more and 30 mm or less.
[0041] From the standpoint of strength, the fiber volume content (Vf) of the thermoplastic resin composite tape is preferably 20 to 75 volume %, and more preferably 40 to 65 volume %.
[0042] <Thermoplastic resin composite sheet> A thermoplastic resin composite sheet can be obtained by laminating a plurality of thermoplastic resin composite tapes. The obtained thermoplastic resin composite sheet can be used to manufacture a molded article. The thermoplastic resin composite sheet obtained by directly attaching the thermoplastic resin composite tape to a mold can also be directly molded into a molded article. The obtained molded article has little residual stress and little warping or distortion because the thermoplastic resin composite sheet is uniformly heated and arranged in the thickness direction. In addition, since it is not excessively heated, there is little resin deterioration and little deterioration in the physical properties of the molded article.
[0043] [Method of manufacturing thermoplastic resin composite sheet] The method for producing a thermoplastic resin composite sheet of the present invention is a method for producing a thermoplastic resin composite sheet by laminating thermoplastic resin composite tapes containing a thermoplastic resin and reinforcing fibers, and includes a step (A) of heating the thermoplastic resin in the thermoplastic resin composite tape, a step (B) of heating the reinforcing fibers in the thermoplastic resin composite tape different from the step (A), a step (C) of laminating the thermoplastic resin composite tapes, and a step (D) of pressing the laminated thermoplastic resin composite tapes. The method for producing a thermoplastic resin composite sheet of the present invention preferably further includes a step (E) of controlling the temperature of the thermoplastic resin composite tape.
[0044] The method for producing a thermoplastic resin composite sheet of the present invention can be carried out by using the above-mentioned automatic lamination device of the present invention. Therefore, each step of steps (A) to (E) in the method for producing a thermoplastic resin composite sheet of the present invention corresponds to each means of means (A) to (E) in the automatic lamination device of the present invention. Therefore, the preferred conditions of steps (A) to (E) can be determined according to the preferred conditions of means (A) to (E).
[0045] [Examples of automatic lamination equipment] [Fig. 1] Fig. 1 shows an example of an automatic lamination device of the present invention. This automatic lamination device is provided with a conveying section 11 for conveying a thermoplastic resin composite tape 17, a means 14 (corresponding to the means (A)) for heating the thermoplastic resin of the thermoplastic resin composite tape, a means 12 (corresponding to the means (B)) for heating the reinforcing fibers, a table 16 on which the thermoplastic resin composite tape is laminated, and a pressure roll 13 for pressing the laminated thermoplastic resin composite tape. [Fig. 2] Fig. 2 shows an example in which the arrangement of the two heating means in the automatic lamination device in Fig. 1 is changed to heating means 22 and 24. [Fig. 3] Fig. 3 shows an example in which a temperature control means 38 is added to the automatic lamination device of Fig. 1. FIG. 4 shows an example in which a temperature control means 48 is added to the automatic lamination device of FIG. FIG. 5 shows an example in which the arrangement of the temperature control means in the automatic lamination apparatus of FIG. 3 is changed to a temperature control means 58. [Fig. 6] Fig. 5 shows an example in which the arrangement of the temperature control means in the automatic lamination apparatus of Fig. 4 is changed to a temperature control means 68.
[0046] [summary] As described above, the automatic laminating apparatus of the present invention is capable of heating the thermoplastic resin composite sheet from both the inside and the outside (surface) by having the means (A) and the means (B). Being able to heat the thermoplastic resin composite sheet from both the inside and outside (surface) makes it easier to control the temperature, improves the interlayer adhesion of the thermoplastic resin composite sheet, and prevents resin deterioration (carbonization) due to overheating. This is particularly effective when using thick thermoplastic resin composite sheets to increase lamination efficiency, and enables thick molded articles to be easily produced with high productivity.
[0047] In addition, the components in the above-described embodiments can be replaced with well-known components as appropriate without departing from the spirit of the present invention. [Explanation of symbols]
[0048] [Figures 1-6] 11, 21, 31, 41, 51, 61 Transport section 12, 22, 32, 42, 52, 62 Heating means (corresponding to means (B)) 13, 23, 33, 43, 53, 63 Pressure roll 14, 24, 34, 44, 54, 64 Heating means (corresponding to means (A)) 15, 25, 35, 45, 55, 65 Transport roll 16, 26, 36, 46, 56, 66 tables 17, 27, 37, 47, 57, 67 Thermoplastic resin composite sheet 38, 48, 58, 68 Temperature control means [Figures 7 and 8] 71 Radiation or thermal conduction 72, 82 Thermoplastic resin 73, 83 Heated resin 74, 84 Reinforced fiber 85 Laser Light
Claims
1. An automatic lamination device for automatically laminating a thermoplastic resin composite tape containing a thermoplastic resin and a reinforcing fiber to manufacture a thermoplastic resin composite sheet, A means (A) for heating the thermoplastic resin of the thermoplastic composite tape; a means (B) for heating the reinforcing fibers of the thermoplastic resin composite tape, which is separate from the means (A); A means for laminating the thermoplastic composite tape (C), and A means (D) for compressing the laminated thermoplastic resin composite tape is provided. Automatic lamination equipment.
2. 2. The automatic lamination apparatus according to claim 1, wherein the means (B) includes a heating means using a laser beam.
3. 3. The automatic lamination apparatus according to claim 2, wherein the wavelength of the laser light is 800 to 2500 nm.
4. 3. The automatic lamination apparatus according to claim 1, wherein the means (A) includes at least one heating means selected from the group consisting of radiant heat and thermal conduction.
5. 5. The automatic lamination apparatus according to claim 4, wherein the at least one heating means using radiation heat or heat conduction includes at least one heating means selected from an infrared heater, hot air, and a hot plate.
6. 3. The automatic laminating apparatus according to claim 1 or 2, further comprising a means (E) for controlling the temperature of the thermoplastic resin composite tape.
7. 7. The automatic lamination apparatus according to claim 6, wherein said means (E) includes a means for detecting a temperature and a means for adjusting an output of a heating device.
8. 7. The automatic laminating apparatus according to claim 6, wherein said means (E) is provided between the thermoplastic composite tape and the table.
9. A method for producing a thermoplastic resin composite sheet by laminating thermoplastic resin composite tapes containing a thermoplastic resin and reinforcing fibers, comprising: A step (A) of heating the thermoplastic resin in the thermoplastic resin composite tape; A step (B) of heating the reinforcing fibers in a thermoplastic resin composite tape separate from the step (A); (C) laminating the thermoplastic resin composite tape; and Step (D) of compressing the laminated thermoplastic resin composite tape A method for producing a thermoplastic resin composite sheet having the following structure:
10. The method for producing a thermoplastic resin composite sheet according to claim 9 , wherein the step (B) includes a heating step using a laser beam.
11. The method for producing a thermoplastic resin composite sheet according to claim 10, wherein the wavelength of the laser light is 800 to 2500 nm.
12. The method for producing a thermoplastic resin composite sheet according to claim 9 or 10, comprising, as the step (A), at least one heating step of radiant heat and thermal conduction.
13. The method for producing a thermoplastic resin composite sheet according to claim 12, wherein the at least one heating step of the radiant heat and the thermal conduction includes at least one heating step selected from an infrared heater, hot air, and a hot plate.
14. The method for producing a thermoplastic resin composite sheet according to claim 9, further comprising the step (E) of controlling the temperature of the thermoplastic resin composite tape.
15. The method for producing a thermoplastic resin composite sheet according to claim 14, wherein step (E) includes the steps of detecting a temperature and adjusting an output of a heating device.
Citation Information
Patent Citations
Fiber bundle sticking device
JP2018149729A
Cited By
Method for processing recycled cellulose fibers, and processed recycled cellulose fibers
US12331456B2