Assembly method of retainer ring

The assembly method for a retainer ring in CMP apparatuses corrects initial template deflections by bending the center upward, addressing uneven polishing rates and slip-out issues, resulting in stable and efficient polishing.

JP2024140486APending Publication Date: 2024-10-10TOKYO SEIMITSU CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023051642
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

Templates in CMP apparatuses exhibit initial deflections that lead to uneven polishing rates and potential slip-out of workpieces due to uneven contact with the polishing pad, either causing the center to lift off or press excessively, affecting the efficiency and safety of the polishing process.

Method used

A method for assembling a retainer ring in a CMP apparatus that includes a template with a holder, using a jig to correct initial deflections by applying adhesive and weight to the template, ensuring the center side is slightly bent upward from the outer circumference, enhancing uniform contact with the polishing pad.

Benefits of technology

The method stabilizes the polishing process by suppressing drops in polishing rate and slip-out, ensuring efficient and safe polishing of workpieces by maintaining consistent contact across the surface.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024140486000001_ABST
    Figure 2024140486000001_ABST
Patent Text Reader

Abstract

To provide an assembly method of a retainer ring which can suppress reduction of a polishing rate and slip out, caused by initial bending.SOLUTION: There is provided an assembly method of a retainer ring 40, comprising: a step for mounting a toric template 41 which has initial bending, has on a substantially center part, a pocket 41a capable of storing a workpiece W, and has a lower face 41c which can contact a polishing pad 5, between multiple positioning parts 92 of a jig 90 which has the multiple positioning parts 92 arranged at higher positions than that of the template 41 on its periphery, and has a salient 91 which has a diameter larger than that of the pocket 41a on the center; a step for applying an adhesive agent to a space between the template 41 and the holder 42 in a ring-shape; a step for positioning the holder 42 on the periphery of the top surface 41b of the template 41, according to the multiple positioning parts 92 for arranging the same; a step for mounting a weight 93 on the holder 42, and crimping the holder 42 and the template 41 whose center side is bent toward the top surface 41b side relative to its periphery part, according to the height of the salient 91.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for assembling a retainer ring that is used in a CMP apparatus and is capable of housing a workpiece. [Background technology]

[0002] 2. Description of the Related Art In the field of semiconductor manufacturing, CMP apparatuses are known that planarize semiconductor wafers such as silicon wafers (hereinafter referred to as "workpieces").

[0003] The polishing apparatus described in Patent Document 1 is a polishing apparatus that applies chemical mechanical polishing, or so-called CMP (Chemical Mechanical Polishing) technology. In this polishing apparatus, an elastic base material is attached to the upper surface of a circular template that is pressed against a polishing cloth during polishing, a backing film is interposed between the elastic base material and a wafer accommodated in a pocket of the template, and an air chamber is formed between the carrier of the polishing head and the elastic member. When air is supplied to the air chamber, the elastic base material elastically deforms downward due to the air pressure, and the workpiece is pressed against the polishing cloth to be polished. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2016-159385 A Summary of the Invention [Problem to be solved by the invention]

[0005] Incidentally, the templates have different initial deflections. As shown in Fig. 9, the template 101 having a storage pocket 101a formed in the center constitutes a retainer ring 100 together with a holder 102 that is pressed against the outer periphery of an upper surface 101b of the template 101 to hold the template 101, and the workpiece W held by a backing film 103 and a lower surface 101c of the template 101 are pressed against a polishing pad 104. At this time, the deflection on the outer periphery side of the template 101 is corrected by the holder 102, while the initial deflection generated on the central side of the template 101 remains.

[0006] 10, if the initial deflection of the upward warp in which the central side of the template 101 is located excessively closer to the upper surface 101b than the outer periphery remains in the template 101, the workpiece W is likely to fall off without being adhered to the backing film 103, and the central side of the template 101 is excessively raised from the polishing pad 104, which may cause slip-out, that is, the workpiece W jumping out from the gap between the template 101 and the polishing pad 104. Furthermore, when the workpiece W is polished, the outer periphery of the template 101 comes into contact with the polishing pad 104, which tends to reduce the polishing rate of the workpiece W.

[0007] Furthermore, as shown in FIG. 11, if the initial downward bending of the template 101 remains in the template 101, in which the central side of the template 101 is located closer to the lower surface 101c than the outer periphery, there is a risk that the polishing rate of the workpiece W will decrease significantly due to the central side of the lower surface 101c being pressed excessively against the polishing pad 104.

[0008] Therefore, a technical problem arises that must be solved in order to polish a workpiece efficiently and safely, and an object of the present invention is to solve this problem. [Means for solving the problem]

[0009] In order to achieve the above-mentioned object, the method of assembling a retainer ring according to the present invention is used in a CMP apparatus which polishes a workpiece by pressing it against a polishing pad, and is provided with a template capable of accommodating the workpiece and a holder which holds the template, and includes the steps of: preparing the template, which has an initial deflection, a pocket capable of accommodating the workpiece formed approximately in the center, and a circular template whose underside is capable of contacting the polishing pad, and which has a plurality of positioning portions on its outer periphery which are higher than the template, and which has a convex portion in its center which has a larger diameter than the pocket, between the plurality of positioning portions of a jig; applying adhesive between the template and the ring-shaped holder; positioning and placing the holder on the outer periphery of the upper surface of the template in accordance with the plurality of positioning portions; and loading a weight on the holder, and pressing the holder against the template, the central side of which is deflected upward from the outer periphery in accordance with the height of the convex portion. Effect of the Invention

[0010] The present invention can suppress a decrease in the polishing rate and slip-out caused by initial deflection, and can polish a workpiece efficiently and safely. [Brief description of the drawings]

[0011] [Figure 1] 1 is a perspective view showing a schematic diagram of a CMP apparatus according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a vertical cross-sectional view showing a schematic view of a main part of a polishing head. [Diagram 3] FIG. 2A is a longitudinal sectional view showing the structure of an elastic pressing member, and FIG. 2B is a bottom view showing the positional relationship of four zones divided within the elastic pressing member. [Figure 4] Schematic diagrams showing a procedure for assembling the retainer ring. [Diagram 5] 5A to 5C are schematic diagrams showing a procedure for measuring a step of a retaining ring. [Figure 6] 1 is a graph showing the evaluation results of Experimental Example 1. [Figure 7] 13 is a graph showing the evaluation results of Experimental Example 2. [Figure 8]1 is a graph showing the relationship between the polishing rate and the step height. [Figure 9] FIG. 13 is a schematic diagram showing the structure of a conventional retainer ring. [Figure 10] FIG. 13 is a schematic diagram showing a state of polishing using a conventional template in which an excessive initial warp remains. [Figure 11] FIG. 13 is a schematic diagram showing a state of polishing using a conventional template in which initial bending of downward curvature remains. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] An embodiment of the present invention will be described with reference to the drawings. In the following, when the number, numerical value, amount, range, etc. of components are mentioned, the number is not limited to the specific number, and may be more or less than the specific number, unless otherwise specified or when it is clearly limited to a specific number in principle.

[0013] In addition, when referring to the shape or positional relationship of components, etc., this includes things that are substantially similar or approximate to those shapes, etc., unless otherwise specified or considered to be clearly different in principle.

[0014] In addition, the drawings may exaggerate characteristic parts to make the features easier to understand, and the dimensional ratios of the components may not be the same as the actual ones. In addition, in cross-sectional views, hatching of some components may be omitted to make the cross-sectional structure of the components easier to understand.

[0015] 1 is a perspective view showing a schematic diagram of a CMP apparatus 1 according to an embodiment of the present invention. The CMP apparatus 1 polishes one surface of a workpiece W flatly. The workpiece W is, for example, a silicon wafer, but is not limited to this. The CMP apparatus 1 includes a platen 2 and a polishing head 10.

[0016] The platen 2 is formed in a disk shape and is connected to a rotating shaft 3 arranged below the platen 2. The rotating shaft 3 is rotated by the drive of a motor 4, causing the platen 2 to rotate in the direction of arrow D1 in Fig. 1. A polishing pad 5 is attached to the upper surface of the platen 2, and CMP slurry, which is a mixture of an abrasive and a chemical agent, is supplied onto the polishing pad 5 from a nozzle (not shown).

[0017] The polishing head 10 is formed in a disk shape with a smaller diameter than the platen 2, and is connected to a rotating shaft 10a disposed above the polishing head 10. The rotating shaft 10a is rotated by a motor (not shown), causing the polishing head 10 to rotate in the direction of arrow D2 in FIG. 1. The polishing head 10 can be raised and lowered in the vertical direction V by a lifting device (not shown). When polishing the workpiece W, the polishing head 10 descends to press the workpiece W against the polishing pad 5. The workpiece W to be polished by the polishing head 10 is delivered by a wafer transport mechanism (not shown).

[0018] The operation of the CMP apparatus 1 is controlled by a control unit (not shown). The control unit controls each of the components constituting the CMP apparatus 1. The control unit is, for example, a computer, and is composed of a CPU, memory, etc. The functions of the control unit may be realized by control using software, or may be realized by something that operates using hardware.

[0019] Next, the polishing head 10 will be described with reference to Fig. 2. Fig. 2 is a vertical cross-sectional view that shows a schematic view of a main part of the polishing head 10. Note that an elastic pressing member 70, which will be described later, is omitted in Fig. 2.

[0020] The polishing head 10 includes a head body 20 , a carrier 30 , a retainer ring 40 , a membrane film 50 , and a backing film 60 .

[0021] The head body 20 is connected to a rotating shaft 10a, and rotates together with the rotating shaft 10a when the rotating shaft 10a is rotated by a motor (not shown). The head body 20 is connected to a carrier 30 disposed below the head body 20 via a rotating part 21, and the head body 20 and the carrier 30 rotate in unison.

[0022] The carrier 30 is provided with airlines 31 arranged at equal intervals around the periphery of the carrier 30. The lower ends of the airlines 31 open into an air chamber A formed between the lower surface 30a of the carrier 30 and the membrane film 50. The airlines 31 are connected to an air supply source serving as an air supply means (not shown), and air is introduced into the air chamber A via the airlines 31. The pressure of the air supplied to the airlines 31 is adjusted by a regulator (not shown). The air supplied into the air chamber A forms an air layer above the membrane film 50 by a rim formed on the outer periphery of the carrier 30, and presses the entire surface of the membrane film 50 downward.

[0023] A carrier pressing means 32 is provided between the head body 20 and the carrier 30. The carrier pressing means 32 is an air bag or the like that is inflated by air supplied from an air supply source (not shown). The pressure of the air supplied from the air supply source is adjusted by a regulator (not shown). The carrier pressing means 32 presses the workpiece W against the polishing pad 5 via the carrier 30 according to the pressure of the supplied air.

[0024] The retainer ring 40 is disposed so as to surround the periphery of the carrier 30. The retainer ring 40 includes a template 41 and a holder 42.

[0025] The template 41 is made of a resin such as glass epoxy, polyether ether ketone (PEEK), polyphenylene sulfide (PPS), etc. The template 41 is formed in an annular shape and has an accommodation pocket 41a for accommodating the workpiece W in approximately the center.

[0026] The holder 42 is formed in a ring shape, and holds the template 41 by having a lower surface 42a joined to the outer periphery of an upper surface 41b of the template 41 via a membrane film 50. The holder 42 is attached to a retainer pressing member 44 via a snap ring 43. A retainer pressing means 45 is provided between the head main body 20 and the retainer pressing member 44. Reference numeral 46 denotes a cover that covers the upper part of the snap ring 43.

[0027] The retainer pressing means 45 is an air bag or the like that is inflated by air supplied from an air supply source (not shown). The pressure of the air supplied from the air supply source is adjusted by a regulator (not shown). The retainer pressing means 45 presses the retainer ring 40 against the polishing pad 5 according to the pressure of the supplied air.

[0028] The membrane film 50 is attached to the upper surface 41b of the template 41 so as to cover the storage pocket 41a, and its peripheral edge is clamped by the retainer ring 40. When compressed air is introduced into the air chamber A, the membrane film 50 elastically deforms downward within the storage pocket 41a.

[0029] The membrane film 50 is preferably made of a material having both appropriate strength and flexibility, such as a resin such as polyether ether ketone (PEEK), polyphenylene sulfide (PPS), or polyethylene terephthalate (PET). From the viewpoints of physical properties and availability, PEEK is particularly preferable for the membrane film 50, but PPS and PET are also preferable because they have a Young's modulus close to that of PEEK and are relatively easily available.

[0030] The backing film 60 is, for example, a suede film. The backing film 60 is attached to the membrane film 50 with its center positioned on the rotation axis 10a of the polishing head 10. When compressed air is introduced into the air chamber A, the backing film 60 elastically deforms in accordance with the elastic deformation of the membrane film 50, and pressurizes the workpiece W.

[0031] As shown in Fig. 3(a), an elastic pressing member 70 is provided on the lower surface 30a of the carrier 30 and is arranged coaxially with the rotation shaft 10a of the polishing head 10. The elastic pressing member 70 is made of, for example, polyethylene terephthalate resin (PET), fluororesin (PFA), or polyphenylene sulfide (PPS). PFA has low water absorption, is moderately flexible, and is resistant to stretching and deformation. PPS has low water absorption, is resistant to stretching and deformation, and is less expensive than PFA.

[0032] Four rims 71 are provided on the upper surface of the elastic pressing member 70, and each rim 71 is inserted into annular groove 81 of a layout base 80 interposed between the carrier 30 and the elastic pressing member 70. The rims 71 are detachably attached to the layout base 80 with a two-component epoxy resin adhesive or the like. The layout base 80 is fastened to the carrier 30 with bolts (not shown).

[0033] The elastic pressing member 70 is divided into four zones with the rim 71 as a boundary. Each zone is connected to an air supply source via a zone air line 82, and can be expanded independently by air supplied from the air supply source. This allows the elastic pressing member 70 to be configured such that the four divided zones can be expanded independently. Hereinafter, the regions into which the elastic pressing member 70 is divided will be referred to as "zones Z1 to Z4" in order from the outer periphery side to the inner periphery side of the polishing head 10, as shown in FIG. 3(b).

[0034] With this configuration, as shown in FIG. 3(a), the CMP apparatus 1 transmits the pressing force applied to the carrier 30 by the compressed air supplied into the air chamber A through the membrane film 50, thereby enabling the workpiece W to be pressed against the polishing pad 5 with uniform pressure distribution, thereby polishing the workpiece W.

[0035] Moreover, by expanding each of the zones Z1 to Z4 of the elastic pressing member 70 independently in response to the pressure of the compressed air, the zones Z1 to Z4 can be selectively pressurized, and the workpiece W can be locally polished.

[0036] That is, in the CMP apparatus 1, the polishing pressure acting on the workpiece W is the sum of the pressure with which the elastic pressing member 70 presses the membrane film 50 in response to the air pressure in zones Z1 to Z4, and the pressure with which the membrane film 50 presses the workpiece W in response to the air pressure in air chamber A.

[0037] In the CMP apparatus 1, a pressure drop occurs near the boundaries of the zones Z1 to Z4 because the hard elastic pressing member 70 does not press the membrane film 50. However, the rigidity of the membrane film 50 absorbs the pressure drop near the boundaries of the elastic pressing member 70, so that the pressure acting on the workpiece W is continuous over the entire surface of the workpiece W, resulting in a polished shape that changes gradually.

[0038] Next, a method of assembling the retainer ring 40 will be described with reference to FIG.

[0039] First, the template 41 is prepared. Next, the membrane film 50 is attached to the upper surface 41b of the template 41, and then the backing film 60 is attached to the membrane film 50 inside the storage pocket 41a. As a result, the template 41, the membrane film 50, and the backing film 60 are integrated together, as shown in FIG. 4(a).

[0040] Next, as shown in FIG. 4(b), the template 41 is placed on the jig 90 with the upper surface 41b facing upward. At this time, the center side of the template 41 is supported by a convex portion 91 formed in the center of the jig 90. The outer diameter of the convex portion 91 is set to be larger than the diameter of the storage pocket 41a. For example, when the diameter of the storage pocket 41a is 101 mm, the outer diameter of the convex portion 91 is set to be 107 mm. The height of the convex portion 91 is set to be smaller than the height at which the template 41 and the backing film 60 are significantly distorted, for example, 0.7 mm, and the convex portion 91 corresponding to the template 41 made of PEEK with a thickness of 0.123 mm and an outer diameter of about 177 mm is set to a height of 0.18 mm. The height of the convex portion 91 is not limited to 0.18 mm, and can be arbitrarily changed according to the material and outer diameter of the template 41.

[0041] Furthermore, a plurality of positioning portions 92 are formed on the outer periphery of the jig 90. For example, six positioning portions 92 are provided at equal intervals in a substantially concentric pattern. The height of the positioning portions 92 is set to be higher than the height of the template 41. The positioning portions 92 come into contact with the outer periphery of the template 41, thereby positioning the template 41 so that the center of the template 41 substantially coincides with the center of the jig 90. Furthermore, the positioning portions 92 prevent the template 41 from shifting when the retaining ring 40 is assembled.

[0042] Next, the holder 42 is placed on the upper surface 41b of the template 41. The outer peripheral surface of the holder 42 is in contact with the positioning portion 92 or is arranged according to the positioning portion 92, so that the holder 42 is positioned so that the center of the holder 42 approximately coincides with the center of the template 41. Then, adhesive is applied between the upper surface 41b of the template 41 and the lower surface 42a of the holder 42, and as shown in FIG. 4(c), a weight 93 is placed on the holder 42 to press the holder 42 onto the template 41. The pressing time of the holder 42 can be appropriately adjusted according to the time required for the adhesive to dry, and is set to, for example, 24 hours.

[0043] At this time, the weight 93 presses the outer periphery of the template 41 against the jig 90 via the holder 42, so that the initial deflection in the outer periphery of the template 41 is corrected to be approximately flat. Also, with the protrusion 91 supporting the center side of the template 41, the weight 93 presses the outer periphery of the top surface 41b of the template 41 downward, so that the center side of the template 41 is slightly deflected higher toward the top surface 41b than the outer periphery side.

[0044] 4(d), the jig 90 and the weight 93 are removed. In the retainer ring 40 from which the jig 90 and the weight 93 have been removed, compressive stress remains at the joint between the template 41 and the holder 42, bending the center side of the template 41 toward the upper surface 41b from the outer periphery, and an initial bending corresponding to the height of the protrusion 91 remains in the template 41.

[0045] In this way, by imparting an initial deflection to the template 41 such that the central side of the template 41 is slightly bowed upward toward the upper surface 41b rather than the outer periphery, the workpiece W is safely adsorbed to the backing film 60, and the template 41 can come into appropriate contact with the polishing pad 5 from the central side to the outer periphery, preventing the workpiece W from slipping out. Furthermore, excessive contact of a part of the template 41 with the polishing pad 5 is prevented, allowing the workpiece W to be polished efficiently.

[0046] As a result of extensive research, the inventors of the present application have found that it is possible to stably obtain a template 41 suitable for polishing a workpiece W by managing the "step" calculated according to the initial deflection of the template 41. Hereinafter, a method for evaluating the template 41 will be described with reference to FIG.

[0047] First, as shown in FIG. 5(a), with the upper surface 41b side of the template 41 facing downward, the retaining ring 40 is placed on the first measurement stage 94 so that the template 41 is supported by the first measurement stage 94.

[0048] Next, with the outer periphery of the template 41 pressed against the first measuring table 94 and the initial deflection of the template 41 corrected, the measuring instrument 95 measures the flatness (first flatness) of the lower surface 60a of the backing film 60 from the lower surface 41c side of the template 41.

[0049] Next, as shown in FIG. 5(b), with the upper surface 41b side of the template 41 facing downward, the retaining ring 40 is placed on the second measurement stage 96 so that the holder 42 is supported by the second measurement stage 96.

[0050] Next, in a state where the outer periphery of the template 41 is pressed against the second measurement table 96 and an initial deflection of the template 41 occurs, the measuring device 95 measures the flatness (second flatness) of the lower surface 60a of the backing film 60 from the lower surface 41c side of the template 41. Note that the height of the outer periphery end of the lower surface 41c of the template 41 is set to zero for the first and second flatnesses, and the upward direction is set to be positive. Also, for example, a dial gauge (model number: 1D-C112) manufactured by Mitutoyo Corporation can be used as the measuring device 95.

[0051] Then, a value obtained by subtracting the second flatness from the first flatness (hereinafter referred to as "step") is calculated. An example of the step of the template 41 showing an excessive initial deflection of upward curvature shown in FIG. 10 is a first flatness of 0.133 mm, a second flatness of -0.352 mm, and a step of 0.469 mm. An example of the step of the template 41 showing an initial deflection of downward curvature shown in FIG. 11 is a first flatness of 0.102 mm, a second flatness of -0.021 mm, and a step of 0.123 mm. On the other hand, as shown in FIG. 4(d), an example of the step of the template 41 in which a PEEK template 41 having a thickness of 0.123 mm and an outer diameter of about 177 mm is formed with a protrusion 91 having a height of 0.18 mm and a moderate initial deflection of upward curvature is a first flatness of 0.128 mm, a second flatness of -0.119 mm, and a step of 0.245 mm. EXAMPLES

[0052] (Experimental Example 1) Example 1, which is a retainer ring assembled according to the procedure of the embodiment described above, and Comparative Examples 1 and 2, which are retainer rings assembled by a conventional method, were prepared, and the polishing rates of the workpiece W when the workpiece W was polished using each of them were compared. The assembly method of Comparative Examples 1 and 2 was the same as the above-mentioned method of assembling the retainer ring according to the present invention, except that the template 41 was bent upward using a jig 90, and the holder 42 was crimped onto the upper surface 41b of the template 41.

[0053] In this experimental example, a template 41 according to Example 1 was prepared by forming an initial upward deflection with a convex portion 91 having a height of 0.18 mm on a PEEK template 41 having a thickness of 0.123 mm and an outer diameter of about 177 mm. The step of the template 41 according to Example 1 thus obtained was 0.245 mm. The steps of the templates according to Comparative Examples 1 and 2 were 0.285 mm and 0.123 mm, respectively. That is, the templates according to Example 1 and Comparative Example 1 exhibit a moderate initial upward deflection, and the template according to Comparative Example 2 exhibits an initial downward deflection in which the central side is lower on the lower surface side than the outer periphery side.

[0054] The main polishing conditions set in this evaluation are as shown in Table 1. In addition, the pressure in zone Z1, which is 45 to 65 mm from the center of rotation of the polishing head in the radial direction, was set to 3.9 psi, and the pressure in the other zones Z2 to Z4 was set to 0 psi.

[0055] [Table 1]

[0056] 6(a) and (b) are graphs showing the results of this experimental example, with the polishing rate on the vertical axis and the radial coordinate with the rotation center of the polishing head as the origin on the horizontal axis. A high polishing rate (high rate) falling within a predetermined range is judged to be a pass rate, and a retainer ring that realizes a polishing rate within the pass rate range is judged to be a pass rate. Hereinafter, a high rate within the predetermined range that is judged to be a pass rate is referred to as a "pass rate range." The pass rate range is, for example, 210 mm / min to 250 mm / min, but is not limited to this range. In addition, the average value of the polishing rate over the entire surface of the workpiece W shown in FIGS. 6(a) and (b) (hereinafter simply referred to as "average polishing rate") was 220 mm / min for Example 1, 239 mm / min for Comparative Example 1, and 184 mm / min for Comparative Example 2.

[0057] 6(a) and (b), it can be seen that Example 1 exhibits an average polishing rate that is comparable to that of Comparative Example 1, and exhibits a stable polishing rate over the entire surface of the workpiece W. It can also be seen that Example 1 exhibits a stable and superior polishing rate over the entire surface of the workpiece W, as compared to Comparative Example 2.

[0058] (Experimental Example 2) Next, Examples 1 to 5, which are retainer rings assembled according to the procedure of the above-mentioned embodiment, and Comparative Examples 1 to 13, which are retainer rings assembled by a conventional method, were prepared, and the step of each template was measured. Also, the polishing rate and the occurrence of slip-out when polishing the workpiece W were evaluated, and the results are shown in FIG. 7. The assembly method of Examples 2 to 4 used in this experimental example was the same as the assembly method of Example 1 used in Experimental Example 1, and the assembly method of Comparative Examples 3 to 13 used in this experimental example was the same as the assembly method of Comparative Examples 1 and 2 used in Experimental Example 1. The polishing conditions of this experimental example were the same as the polishing conditions described in Experimental Example 1.

[0059] In Fig. 7, the vertical axis represents the step height. According to Fig. 7, Comparative Examples 1, 3, 4, and 10 to 12 and Experimental Examples 1 to 5 exhibited high polishing rates (non-defective product rates). The step heights ranged from 0.18 to 0.33.

[0060] On the other hand, Comparative Examples 6 and 7 showed lower polishing rates (intermediate rates) compared to Experimental Examples 1 to 5, etc. Comparative Example 2 showed an even lower polishing rate (low rate) than Comparative Examples 6 to 7. Furthermore, in Comparative Examples 5, 8, 9, and 13, suction errors occurred for the workpiece W, and slip-out occurred. That is, according to this experiment, it is found that by imparting to the template 41 an initial upward deflection corresponding to the step difference of 0.13 to 0.33 surrounded by the solid line in FIG. 7, it is possible to stably obtain a template 41 capable of suppressing a decrease in the polishing rate and slip-out of the workpiece W resulting from the initial deflection.

[0061] Next, Table 2 shows the template step height and the polishing rate of the retainer ring in Examples 1 to 5 and Comparative Examples 2, 4, 5, 8, and 11. The relationship between the step height and the polishing rate shown in Table 2 is shown in Fig. 8. In Fig. 8, the vertical axis represents the polishing rate (average polishing rate), and the vertical axis represents the step height.

[0062] [Table 2]

[0063] The dashed and dotted lines in FIG. 8 show the linear approximation equations of the points corresponding to Examples 1 to 5 and Comparative Examples 2, 4, and 11. According to the linear approximation equations, it can be seen that the template step corresponding to the lower limit (210 nm / min) of the non-defective product rate range is 0.18 mm. It can also be seen that when the template step is set to 0.18 to 0.33 mm, the polishing rate shows a non-defective product rate. Furthermore, it can be seen that when the template step is significantly larger than 0.33 mm, as in Comparative Examples 5 and 8, the polishing rate falls outside the non-defective product rate range.

[0064] Furthermore, the present invention can be modified in various ways other than those described above without departing from the spirit of the present invention, and it goes without saying that the present invention extends to such modifications. [Explanation of symbols]

[0065] 1:CMP equipment 2: Platen 3: Rotation axis 4: Motor 5: Polishing pad 10: Polishing head 10a: Rotating shaft 20: Head body 21: Rotating part 30: Career 30a: (Carrier) bottom surface 31: Airlines 32: Carrier pressing means 40: Retainer ring 41: Template 41a: Storage pocket 41b: Top surface (of template) 41c: Bottom surface (of template) 42: Holder 42a: (holder) bottom surface 43: Snap ring 44: Retainer pressing member 45: Retainer pressing means 50:Membrane film 60: Backing film 60a: Bottom surface (of backing film) 70: Elastic pressing member 71: Rim 80: Layout-based 81: Annular groove 82: Zone Airlines 90: Jig 91: Convex 92: Positioning section 93: Weight 94: First measuring platform 95: Measuring instruments 96: Second measuring platform A: Air chamber W: Work

Claims

1. A method for assembling a retainer ring used in a CMP apparatus that polishes a workpiece by pressing the workpiece against a polishing pad, the retainer ring including a template capable of accommodating the workpiece and a holder that holds the template, the method comprising the steps of: a step of placing the template, which has an initial deflection, a pocket capable of accommodating the workpiece formed at approximately the center, and has a circular shape whose lower surface is capable of contacting the polishing pad, between a plurality of positioning parts of a jig, the jig having a plurality of positioning parts on an outer periphery that are higher than the template and a protrusion in the center that has a diameter larger than that of the pocket; applying an adhesive between the template and the ring-shaped holder; positioning the holder on an outer periphery of an upper surface of the template according to the positioning portions; a step of placing a weight on the holder and pressing the holder against the template, the central side of which is bent upward relative to the outer periphery in accordance with the height of the protrusion; A method for assembling a retainer ring, comprising:

2. 2. The method for assembling a retainer ring according to claim 1, wherein the height of the protrusion is set to be equal to or greater than 0.18 mm and less than 0.7 mm.

3. 3. The method for assembling a retainer ring according to claim 2, wherein the initial deflection of the template is set to 0.18 mm to 0.33 mm.

Citation Information

Patent Citations

  • Retainer ring for polishing head

    JP2008177248A

  • Manufacturing method of polishing head and polishing device

    JP2014233815A

  • Wafer polishing device

    JP2016159385A

  • Holder and manufacturing method for holder

    JP2018161732A

  • Mechanically stabilized retaining ring for chemical mechanical polishing

    US6068548A