Forming method of carrier tape
The method addresses scrap lifting and burr issues in carrier tape molding by using a die configuration with a narrower lower die side, ensuring efficient and reliable hole punching.
Patent Information
- Application Number
- JP2023053608
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing carrier tape molding methods result in thin skin burrs and scrap lifting during hole punching, leading to adhesion and deformation issues.
A method for forming carrier tape with a specific die hole configuration in the receiving die, where the lower die side is narrower than the upper die side, preventing scrap lifting by holding punched scraps in a narrower stepped portion.
Prevents scrap lifting, reduces burrs, and maintains die integrity, enhancing the reliability and longevity of the punching process.
Smart Images

Figure 2024141780000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for forming a carrier tape having a storage recess capable of storing components. [Background technology]
[0002] In a method for molding a carrier tape having feed holes and storage recesses in which components can be stored, a hole punching process is carried out to punch feed holes on the sides of the storage recesses and to punch bottom holes in the bottom surfaces of the storage recesses (see Patent Document 1).
[0003] In the hole punching process, a punching die equipped with a punch and a receiving die is used. In order to reduce the thread burrs (see FIG. 6) that occur at the opening edges of the feed holes and bottom holes, such a punching die has a larger hole diameter in the receiving die relative to the tip of the punch to provide a sufficient clearance. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2006-321502 A Summary of the Invention [Problem to be solved by the invention]
[0005] In this case, however, thin burrs (see Figure 6) are more likely to occur. Furthermore, the scrap punched by the punching die may not fall downward in the punching direction, but may adhere to the tip of the punch. This causes the scrap to rise above the die hole (on the surface of the receiving die), a phenomenon known as scrap rising.
[0006] Therefore, the present invention has been made in consideration of the above problems, and an object of the present invention is to provide a method for forming a carrier tape that can prevent slug lift-up. [Means for solving the problem]
[0007] (1) One aspect of the present invention is a method for molding a carrier tape having a storage recess capable of storing components, comprising: a storage recess molding step of molding the storage recess in a sheet base material; and a hole punching step of punching a through hole in a side of the storage recess in the sheet base material or in a bottom surface of the storage recess, wherein the hole punching step punches out the through hole using a punching die including a punch provided in an upper die and a receiving die provided in a lower die having a die hole for receiving the punch, and wherein the shape of the die hole of the receiving die is narrower in the portion on the lower die side than in the portion on the upper die side. (2) In the above aspect (1), the shape of the die hole may be such that, in a cross section cut in a direction perpendicular to the punching direction, the cross-sectional area of the portion on the lower die side is 5% or more smaller than the cross-sectional area of the portion on the upper die side. (3) In the above aspect (1) or (2), the die hole may have a two-stage shape. (4) In the above aspect (3), in the hole punching step, the punch may advance to a narrow step portion of the die hole on the lower mold side. Effect of the Invention
[0008] According to the present invention, it is possible to provide a method for forming a carrier tape that can prevent slug lift-up. [Brief description of the drawings]
[0009] [Figure 1] FIG. 2 is a perspective view of a carrier tape. [Diagram 2] 1 is a schematic diagram showing an example of a molding apparatus used in a molding method for a carrier tape according to an embodiment of the present invention. [Figure 3A] FIG. 2 is a schematic cross-sectional view showing a top dead center state of the punching die of the embodiment. [Figure 3B] FIG. 2 is a schematic cross-sectional view showing a bottom dead center state of the punching die of the embodiment. [Figure 3C] FIG. 4 is a schematic cross-sectional view showing the punching die of the embodiment during a return process. [Figure 4]FIG. 2 is a flow diagram showing a method for forming a carrier tape according to an embodiment of the present invention. [Figure 5A] FIG. 1 is a schematic cross-sectional view showing a top dead center state of a punching die of the prior art. [Figure 5B] FIG. 1 is a schematic cross-sectional view showing a bottom dead center state of a punching die of the prior art. [Figure 5C] FIG. 1 is a schematic cross-sectional view showing a conventional punching die during a return process. [Figure 6] FIG. 1 is a plan view showing the occurrence of burrs (threads, thin skin) in a carrier tape of the prior art. [Figure 7] Table 1 shows the results of an experiment observing the occurrence of burrs and swarf during the bottom hole punching process. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings. In the embodiments of this specification, the same members are denoted by the same reference numerals throughout.
[0011] FIG. 1 is a perspective view of a carrier tape 1. FIG. 1, the carrier tape 1 stores a plurality of components EP and serves to store, transport, and smoothly supply the components EP to a mounting machine that mounts the components P on a substrate. Examples of the components EP include electronic components and precision components.
[0012] The carrier tape 1 has a plurality of feed holes 2 and storage recesses 3 for storing parts EP, each of which is arranged at a predetermined pitch P1 in the longitudinal direction (transport direction) MD of a resin sheet base material 1a.
[0013] The feed holes 2 are circular in plan view, but the shape and spacing P2 of the feed holes 2 are formed to match the feed mechanism of the mounting machine, etc. The feed holes 2 may be formed on both sides of the storage recess 3 along two sides in the longitudinal direction of the tape.
[0014] On the other hand, the storage recess 3 is approximately rectangular in shape, but is formed to match the shape of the component EP, and further, a pedestal may be formed on the bottom surface of the storage recess 3, or a bottom hole 5 for inspection may be additionally formed.
[0015] The carrier tape 1 is formed of, for example, synthetic resins such as polyvinyl chloride, polystyrene, amorphous polyethylene terephthalate, polycarbonate, polypropylene, etc., or these resins kneaded with carbon to impart conductivity, or those with a conductive coating on the surface, etc. The width of the carrier tape 1 is not particularly limited, and may be 8 mm, 12 mm, 16 mm, 24 mm, etc.
[0016] 1, the length of the storage recess 3 is A, the width is B, and the depth is T, the distance from the end face of the carrier tape 1 to the center of the sprocket hole 2 is E1, the distance in the width direction WD from the center of the sprocket hole 2 to the center of the storage recess 3 is F, the pitch between adjacent storage recesses 3 is P1, and the distance in the longitudinal direction MD from the center of the sprocket hole 2 to the center of the storage recess 3 is P2. Depending on the specifications of the carrier tape 1, P1 may not equal 2×P2.
[0017] Next, the molding apparatus 100 and molding method for the carrier tape 1 will be described. FIG. 2 is a schematic diagram showing an example of a molding apparatus 100 used in the molding method of the carrier tape 1 according to the embodiment of the present invention.
[0018] The molding device 100 for the carrier tape 1 includes at least a heating section 110, a molding section 120, an accumulation section 130, a punching die 140, and an intermittent conveying section 150, as shown in FIG.
[0019] The heating section 110 is in the form of a rotating drum that conveys the sheet base material 1a, which is supplied from a supply device (not shown) or the like, to the forming section 120 while heating the sheet base material 1a in a conveying direction MD.
[0020] The molding section 120 embosses the storage recesses 3 in the sheet base material 1a, and is in the shape of a rotating drum having recesses on its surface. The molding section 120 may also mold dummy recesses (dummy embossments) 4 and waste recesses (waste embossments) in some cases. However, the molding section 120 may be formed by any molding method such as vacuum forming, pressure forming, or vacuum pressure forming, or may be press forming using a press die.
[0021] The accumulation section 130 is for retaining and temporarily cooling the sheet base material 1a on which the storage recess 3 is formed, thereby removing thermal stress that occurs when the storage recess 3 is formed.
[0022] The punching die 140 forms the feed holes 2 in the sheet base material 1a. The punching die 140 includes an upper die 141, a lower die 142, and a lifting means (not shown) for moving the upper die 141 and the lower die 142 toward and away from each other (up and down).
[0023] The punching die 140 also has a positioning mechanism 160 for positioning the sheet base material 1a. The positioning mechanism 160 is formed of a member having a tip end that is equal to or slightly smaller than the dimensions and shape of the storage recess 3, such as a pilot pin.
[0024] The intermittent conveying section 150 intermittently conveys the sheet base material 1a to the punching die 140 at a certain conveying pitch (for example, an integral multiple (four times, eight times, etc.) of the pitch P1 of the storage recesses 3).
[0025] Here, the punching die 140 will be described in detail. 3A to 3C are schematic cross-sectional views showing a punching die 140 of the embodiment, in which FIG. 3A is at the top dead center, FIG. 3B is at the bottom dead center, and FIG. 3C is in the middle of returning.
[0026] The punching die 140 also includes a punch 11 for punching a feed hole to punch a feed hole 2 as a through hole, and a receiving die 12 (see FIG. 3A). Note that the upper die 141 also includes a stripper plate 143 that guides the punch 11 and can be brought into contact with (sandwiched) with the sheet base material.
[0027] The punch 11 is cylindrical or polygonal prism-shaped, and has a diameter or outer shape (for example, about 1.0 mm to 3.0 mm) selected according to the dimensions and shape of the feed hole 2. The punch 11 is provided in an upper die 141.
[0028] On the other hand, the receiving die 12 has a die hole 121 for receiving the punch 11. This receiving die 12 is provided in a lower die 142. Therefore, the punching direction by the punching die 140 is vertically downward (gravity direction), but the punching direction may be vertically upward.
[0029] The die hole 121 is basically formed similarly to and slightly larger than the cross-sectional shape of the punch 11, but in this embodiment, the lower die 142 side is narrower than the upper die 141 side. Specifically, the die hole 121 is formed in a two-step shape in which the cross-sectional area of the narrow step portion 122 on the lower die 142 side is 5% or more smaller than the cross-sectional area of the effective step portion 123 on the upper die 141 side in a cross section cut in a direction perpendicular to the punching direction. However, the diameter of the narrow step portion 122 is not smaller than the diameter of the punch punch 11.
[0030] The effective step portion 123 may have a height at least equal to the thickness of the sheet base material 1a, for example, 1 mm or more and 5 mm or less. The narrow step portion 122 may also have a height of 1 mm or more and 5 mm or less. The shape of the die hole 121 may be tapered, but is preferably multi-stepped.
[0031] In addition, in this embodiment, the bottom surface of the storage recess 3 is provided with a bottom hole punch 11 and a receiving die 12 for punching a bottom hole 5 as a through hole, and these are installed in the same punching die 140, but may also be installed as separate dies upstream or downstream of the punching die 140.
[0032] The punch 11 and receiving die 12 for the bottom hole are basically of the same structure as the punch 11 and receiving die 12 for punching the feed holes, and are selected to correspond to the diameter of the bottom hole 5 (for example, about 0.1 mm to 1.5 mm). Specifically, the punch 11 has a diameter of 0.2 mm, the effective step 123 of the die hole 121 has a diameter of 0.23 mm, and the narrow step 122 has a diameter of 0.21 mm. In the embodiment, the die hole 121 (effective step 123 and narrow step 122) has a circular cross section when viewed from the punching direction.
[0033] Next, a method for forming the carrier tape 1 will be described. FIG. 4 is a flow diagram showing a method for forming the carrier tape 1 according to the embodiment of the present invention.
[0034] 4, the method for forming the carrier tape 1 includes at least a storage recess forming step S1 for forming at least a storage recess 3 in the sheet base material 1a being transported, an intermittent transport step S2 for intermittently transporting the sheet base material 1a to a punching die 140, a positioning step S3 for positioning the sheet base material 1a, and a feed hole punching step S4 for forming a feed hole 2 on a side of the storage recess 3. As described above, in this embodiment, a bottom hole punching step S5 for punching a bottom hole 5 in the bottom surface of the storage recess 3 is additionally included.
[0035] In the storage recess forming step S1, the forming unit 120 forms a plurality of storage recesses 3 in the sheet base material 1a along the conveyance direction MD, and also forms one row (single row) in the width direction WD perpendicular to the conveyance direction MD.
[0036] In the intermittent conveying process S2, the sheet base material 1a on which the storage recesses 3 are formed is intermittently conveyed at the above-mentioned predetermined conveying pitch to the punching die 140. In this intermittent conveying process S2, the sheet base material 1a is conveyed to a fixed position of the punching die 140, but since this is an intermittent operation, some conveying deviation occurs in the conveying direction MD and the width direction WD.
[0037] The positioning step S3 is for correcting a conveyance deviation of the sheet base material 1a conveyed in the intermittent conveying step S2 and for positioning the sheet base material 1a so that the feed holes 2 can be punched at accurate positions in the next feed hole punching step S4. In the positioning step S3, it is preferable to perform positioning by inserting a pilot pin or the like into the storage recess 3, or into the dummy recess 4 formed simultaneously with the storage recess 3, or into the feed hole 2.
[0038] In the feed hole punching process S4, a punching die 140 is used to form a feed hole 2 at a predetermined position on the side of a storage recess 3 formed in the sheet base material 1a (see FIG. 1). If a dummy recess 4 is formed at the intended position for punching the feed hole 2, the feed hole 2 may be punched while removing the dummy recess 4.
[0039] Finally, in the bottom hole punching step S5, a bottom hole 5 is formed at a predetermined position (center) on the bottom surface of the storage recess 3 formed in the sheet base material 1a (see FIG. 1). In this embodiment, this bottom hole punching step S5 is performed simultaneously with the previous feed hole punching step S4, but if they are not performed simultaneously, the positioning step S3 is performed immediately before each. Also, if a bottom hole 5 is not required on the bottom surface of the storage recess 3, this bottom hole punching step S5 is naturally omitted.
[0040] In such a feed hole punching step S4 and bottom hole punching step S5, first, as shown in FIG. 3A, the upper die 141 and the lower die 142 wait at the top dead center of their relative up and down movement until the sheet base material 1a is intermittently transported.
[0041] 3B, the upper die 141 and the lower die 142 are moved up and down relative to each other until they reach the bottom dead point, and the sheet base material 1a is sandwiched between the stripper plate 143 and the receiving die 12, and the through holes 2, 5 are punched out by the punch 11. At the bottom dead point, the punch 11 has advanced to the narrow step portion 122 on the lower die 141 (receiving die 12) side.
[0042] Incidentally, punching the through holes 2, 5 using the punch 11 is basically a shearing process, but since it also has a tensile (stretching) aspect, the shape and area of the punched waste DE does not completely match the shape and area of the tip of the punch 11, and has a slightly distorted shape (including thread burrs, etc.).
[0043] 3C, when the punch 11 returns to the top dead center, it retreats from the narrow step portion 122 to the effective step portion 123 and comes out of the die hole 121 of the receiving die 12. At this time, the distorted punched waste DE is held and remains in the narrow step portion 122.
[0044] The punching die 140 can punch the feed hole 2 or the bottom hole 5 by performing such up and down movement between the top dead center and the bottom dead center.
[0045] (Experimental Example) Here, a carrier tape 1 (made of polystyrene) having a width of 8 mm and a length of 100 m was molded using a molding device 100, with the pitch P1 of the storage recesses 3 being 4 mm, the diameter of the feed holes 2 being 1.5 mm, and the diameter of the bottom holes 5 being 0.2 mm or 1.0 mm. However, in Examples 1 and 2, the punch die 140 of this embodiment was used (see FIG. 3A), and in Comparative Examples 1 and 2, the punch die 240 of the prior art (see FIG. 5A) was used.
[0046] 5A to 5C are schematic cross-sectional views showing a conventional punching die 140, with FIG. 5A being at the top dead center, FIG. 5B being at the bottom dead center, and FIG. 5C being in the middle of returning.
[0047] The appearance of the carrier tape 1 was checked for the presence or absence of burrs at the opening edges of the bottom holes 5. In addition, the presence or absence of slugs was also observed.
[0048] Fig. 6 is a plan view showing the occurrence of burrs 6 (threads, thin skin) in a conventional carrier tape 1. Fig. 7 is Table 1 showing the results of an experiment observing the occurrence of burrs and slugs in the bottom hole punching step S5.
[0049] From the results in Table 1, no burrs were generated in either Comparative Example 1 or 2, but scum was generated. In particular, when the diameter of the bottom hole 5 was small, scum was generated at a frequency of about 1 in 1000 (0.1%).
[0050] On the other hand, in Examples 1 and 2, no burrs were generated on the opening edge of bottom hole 5, and no slugs were generated, regardless of the diameter of bottom hole 5. A similar experiment was also performed on feed hole 2, but no significant difference was observed compared to the case of bottom hole 5 (diameter 1.0 mm).
[0051] As described above, the molding method of the carrier tape 1 according to an embodiment of the present invention is a molding method of the carrier tape 1 having a storage recess 3 capable of storing a part EP, and includes a storage recess molding process S1 for molding the storage recess 3 in the sheet base material 1a, and a hole punching process (feed hole punching process S4 or bottom hole punching process S5) for punching through holes 2, 5 on the side of the storage recess 3 or on the bottom surface of the storage recess. The hole punching processes S4 and S5 are performed by punching the through holes 2, 5 using a punching die 140 including a punching punch 11 provided on an upper die 141 and a receiving die 12 provided on a lower die 142 and having a die hole 121 for receiving the punch 11. The shape (diameter) of the punch hole 121 of the receiving die 12 is narrower in the portion (narrow step portion) 122 on the lower die 142 (receiving die 12) side than in the portion (effective step portion) 123 on the upper die 141 side.
[0052] Furthermore, the punching die 140 of the carrier tape 1 according to the embodiment of the present invention comprises a punching punch 11 provided in an upper die 141 for punching out the through holes 2, 5, a receiving die 12 provided in a lower die 142 and having a die hole 121 for receiving the punching punch 11, and a lifting means for moving the punching punch 11 and the receiving die 12 relatively closer to or farther from each other, and the diameter of the die hole 121 is narrower in the portion (narrow step portion) 122 on the lower die 142 side than in the portion (effective step portion) 123 on the upper die 141 side.
[0053] This allows the scraps DE resulting from punching the feed holes 2 or bottom holes 5 in the sheet base material 1a to be held in the narrow step portion 122 of the die hole 121, and the scraps DE can be peeled off from the tip of the punch 11. This prevents the scraps DE from being discharged onto the surface of the receiving die 12, which is known as scrap lifting. This prevents various problems caused by scrap lifting, such as the adhesion of the scraps DE to the carrier tape 1, deformation and eccentricity of the punching punch due to clogging of the scraps in the punching die 140 (die hole 121), and shortened life of the punching die 140 due to uneven wear.
[0054] Furthermore, if the carrier tape 1 with the punched scraps DE attached is used in an electronic component mounting machine, it is expected that physical abnormalities such as deformation or image inspection abnormalities may lead to poor transport or machine stoppage, or that the punched scraps DE may adhere to the electronic components stored in the storage recesses 3, causing poor contact.
[0055] In the shape of the die hole 121 in the embodiment, in a cross section cut in a direction perpendicular to the punching direction, the cross-sectional area of the narrow step portion 122 on the lower die 142 side is 5% or more smaller than the cross-sectional area of the effective step portion 123 on the upper die 141 side. This makes it possible to make the cross-sectional area of the narrow step portion 122 equal to or close to the cross-sectional area of the punched waste DE, and the punched waste DE can be held in the narrow step portion 122 of the die hole 121.
[0056] The shape of the die hole 121 in the embodiment is two-step or multi-step. As a result, even if the opening edge (top surface or inner peripheral surface) of the die hole 121 of the receiving die 12 is worn down by contact with the punch 11, the height of the effective step portion 123 is reduced by (re)polishing the upper surface of the die hole 121 (the surface of the receiving die 12), but the cylindrical shape of the effective step portion 123 can be maintained. In addition, although the depth to the narrow step portion 122 also becomes shallow, the die hole 121 can be maintained in a structure consisting of the effective step portion 123 and the narrow step portion 122. Therefore, the receiving die 12 can be reused.
[0057] In the feed hole punching step S4 and / or the bottom hole punching step S5 of the embodiment, the punching punch 11 advances to the narrow step portion 122 on the lower die 142 side of the die hole 121. This allows the punched waste DE to advance more reliably to the narrow step portion 122.
[0058] In the embodiment, the die hole 121 has a shape in which the height of the effective step 123 on the upper die 141 side is 1 mm or more and 5 mm or less. This allows the height of the effective step 123 to be greater than the thickness of the carrier tape 1 (sheet base material 1a), making it possible to more reliably prevent scrap lifting. In addition, since the stroke of the lifting means is not long, the straightness of the punch 11 relative to the die hole 121 of the receiving die 12 can be maintained.
[0059] Although the preferred embodiments of the present invention have been described in detail above, the present invention is not limited to the above-described embodiments, and various modifications and changes are possible within the scope of the gist of the present invention described in the claims.
[0060] (Modification) In the above embodiment, a single row of carrier tapes 1 is formed from one sheet base material 1a, but multiple rows of carrier tapes 1 may be formed from a wide sheet base material 1a.
[0061] In the above embodiment, the scraps DE held in the narrow step portion 122 are discharged (fall) from the narrow step portion 122 as if being pushed out by the punch 11 in the next punching operation, but a suction means may be provided to suck them in. [Explanation of symbols]
[0062] 1 carrier tape, 1a sheet base material, 2 feed hole (through hole), 3 storage recess, 4 dummy recess, 5 bottom hole (through hole), 6 burr 11 punch, 12 receiving die, 121 die hole, 122 narrow step portion, 123 effective step portion 100 molding device, 110 heating section, 120 molding section, 130 accumulation section, 150 intermittent conveying section, 160 positioning mechanism 140 punching die, 141 upper die, 142 lower die, 143 stripper plate 21 punch, 22 receiving die, 221 die hole EP parts, DE scraps
Claims
1. A method for forming a carrier tape having a storage recess capable of storing a component, comprising the steps of: a storage recess forming step of forming the storage recess in the sheet base material; A hole punching step of punching a through hole in a side surface of the storage recess or a bottom surface of the storage recess in the sheet base material, The hole punching step includes punching the through hole using a punching die including a punch provided in an upper die and a receiving die provided in a lower die and having a die hole for receiving the punch, The shape of the die hole of the receiving die is such that the portion on the lower die side is narrower than the portion on the upper die side. A method for forming a carrier tape comprising the steps of:
2. The shape of the die hole is such that, in a cross section cut in a direction perpendicular to the punching direction, the cross-sectional area of the lower die side portion is smaller than the cross-sectional area of the upper die side portion by 5% or more.
2. The method for forming a carrier tape according to claim 1 .
3. The shape of the die hole is two-stage or multi-stage.
3. The method for forming a carrier tape according to claim 1 or 2.
4. In the hole punching step, the punch advances to a narrow step portion on the lower die side of the die hole.
4. The method for forming a carrier tape according to claim 3.
Citation Information
Patent Citations
Method and apparatus for removing hole burr of embossed carrier tape
JP2003136545A
Blister packaging machine
JP2015151174A
Molding method of carrier tape
JP2018193076A
Button die with anti-grissing mechanism
JP3172403U
Manufacturing method and manufacturing apparatus for carrier tape
JP2006321502A