Semiconductor device having super junction structure and manufacturing method thereof
The semiconductor device with multi-stage saw-shaped columns and insulator/filler layers addresses manufacturing instability and on-resistance issues, achieving improved performance through precise etching and ion implantation processes.
Patent Information
- Application Number
- JP2023054027
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-10
AI Technical Summary
Existing semiconductor devices with superjunction structures face issues such as void formation during epitaxial growth, leading to unstable manufacturing and increased on-resistance due to varying distances between conductivity types, which affect impurity concentration and breakdown voltage.
A semiconductor device with a superjunction structure featuring multi-stage saw-shaped second conductivity type columns, arranged to fit with adjacent columns, and a filling layer of insulator or semiconductor, formed through precise etching and ion implantation processes to stabilize manufacturing and enhance on-resistance characteristics.
The solution enables stable manufacturing of semiconductor devices with improved on-resistance characteristics by reducing voids and optimizing impurity concentration, allowing for reduced on-resistance and enhanced breakdown voltage performance.
Smart Images

Figure 2024142059000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a semiconductor device having a superjunction structure and a manufacturing method thereof. [Background technology]
[0002] Patent Documents 1 and 2 disclose a semiconductor device having a superjunction structure. In the semiconductor device described in Patent Document 1, a groove is formed in a first conductivity type semiconductor by etching. A second conductivity type layer is formed in the groove by epitaxial growth. As a result, a superjunction SJ structure is obtained. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2013-102087 A [Patent Document 2] U.S. Patent No. 8,476,698 Summary of the Invention [Problem to be solved by the invention]
[0004] However, in the semiconductor device described in Patent Document 1, when the second conductivity type layer is formed in the groove by epitaxial growth, the opening of the groove is likely to be blocked, and therefore voids tend to remain inside the groove, making it difficult to stably form the groove.
[0005] In addition, in the semiconductor device described in Patent Document 2, the distance between adjacent first conductivity types and the distance between adjacent second conductivity types in the superjunction structure vary depending on the position in the thickness direction in a cross-sectional view, which makes it impossible to increase the impurity concentration, resulting in an increase in on-resistance.
[0006] The present disclosure has been made to solve the above-mentioned problems. An object of the present disclosure is to provide a semiconductor device having a superjunction structure that can be stably manufactured and has improved on-resistance characteristics, and a manufacturing method thereof. [Means for solving the problem]
[0007] The semiconductor device having a superjunction structure according to the present disclosure includes: A drain layer formed of a first conductivity type semiconductor; a drift layer formed of a first conductivity type semiconductor on one surface of the drain layer; a column structure in which a plurality of first conductivity type columns and a plurality of second conductivity type columns are alternately arranged in the drift layer; Equipped with the second conductivity type column has an outer portion having a multi-stage sawtooth shape in cross section; The semiconductor device has a superjunction structure in which the multi-stage sawtooth outer portion of the second conductivity type column is arranged to fit into the multi-stage sawtooth outer portion of another adjacent second conductivity type column.
[0008] The second conductivity type column is a second conductivity type impurity layer; A filling layer formed inside the impurity layer; It is an aspect of the present disclosure that the present invention is provided with the above.
[0009] In one aspect of the present disclosure, the filling layer is made of an insulator or a semiconductor.
[0010] The impurity concentration of the impurity layer is 1.0×10 17 cm -3 Above 1.0×10 20 cm -3 The following is one aspect of the present disclosure.
[0011] In one aspect of the present invention, the pitch between adjacent columns of the second conductivity type is 4 μm or less.
[0012] the first conductivity type column is formed of first conductivity type silicon carbide; According to one aspect of the present invention, the impurity layer is made of second conductivity type silicon carbide.
[0013] A method for manufacturing a semiconductor device having a superjunction structure according to the present disclosure includes the steps of: a drift layer forming step of forming a drift layer of the first conductivity type by epitaxial growth on a drain layer formed of a semiconductor of the first conductivity type; a second conductivity type column forming step of forming a plurality of second conductivity type columns in the drift layer so as to define an outer portion of a multi-stage sawtooth shape in cross section; Equipped with The second conductivity type column forming step includes: an etching step of performing etching using a first mask having openings formed at positions corresponding to regions in which a plurality of second conductivity type columns that are not adjacent to each other are to be formed among the plurality of second conductivity type columns; A first step including: a second step including an ion implantation step of ion-implanting impurities using a second mask having openings formed at positions corresponding to a region in which the plurality of second conductivity type columns whose formation has begun in the first step and a plurality of adjacent second conductivity type columns will be formed, and an etching step of etching a part of the ion-implanted region using the second mask as it is; The present invention provides a method for manufacturing a semiconductor device having a superjunction structure including the above-mentioned components.
[0014] In one aspect of the present disclosure, the etching depth in the first etching step is half the etching depth in the second etching step.
[0015] In one embodiment of the present disclosure, the ion implantation process and the etching process in the second step are repeated to form a plurality of columns of the second conductivity type so that the outer portion has a multi-stage sawtooth shape in cross section.
[0016] In one embodiment of the present disclosure, the ion implantation step implants ions such that a portion of a region in which the impurities are present extends outside the opening of the mask in a top view.
[0017] In one embodiment of the present disclosure, after the ion implantation process and the etching process in the second step are repeated, a filling process is included in which a groove formed by the etching process is filled with an insulator or a semiconductor. Effect of the Invention
[0018] According to the present disclosure, it is possible to stably manufacture a semiconductor device having a superjunction structure with improved on-resistance characteristics. [Brief description of the drawings]
[0019] [Figure 1] FIG. 1 is a cross-sectional view of a semiconductor device in the first embodiment. [Diagram 2] FIG. 2 is a cross-sectional view of a comparative example. [Diagram 3] FIG. 3 is a diagram showing the relationship between the SJ pitch P and the on-resistance. [Figure 4] FIG. 4 is a cross-sectional view illustrating the method for manufacturing the semiconductor device in the first embodiment. [Diagram 5] FIG. 5 is a diagram for illustrating a method of forming an impurity layer of a second conductivity type of the semiconductor device in the first embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] The embodiments will be described with reference to the accompanying drawings. In each drawing, the same or corresponding parts are denoted by the same reference numerals. Duplicate descriptions of the parts will be appropriately simplified or omitted.
[0021] Embodiment 1 FIG. 1 is a cross-sectional view of a semiconductor device 1 according to the first embodiment.
[0022] 1, the semiconductor device 1 is a silicon carbide planar type MOSFET having a superjunction structure. The semiconductor device 1 includes a drain layer 2, a drift layer 3, a plurality of body layers 4, a plurality of source layers 5, a plurality of body contact layers 6, a plurality of gate insulating layers 7, a plurality of gate electrode layers 8, a plurality of interlayer insulating layers 9, a plurality of source electrode layers 10, a wiring electrode layer 11, a drain electrode layer 12, a plurality of impurity layers 13, and a plurality of filling layers 14.
[0023] The drain layer 2 is made of silicon carbide of a first conductivity type. For example, the drain layer 2 is made of n + The drift layer 3 is formed of first conductivity type 4H silicon carbide. For example, the drain layer 2 is formed using nitrogen as an impurity. The drift layer 3 is formed on a first surface (upper surface in FIG. 1 ) of the drain layer 2. The drift layer 3 is formed of first conductivity type silicon carbide having a lower impurity concentration than the drain layer 2. For example, the drift layer 3 is formed of n - For example, the drift layer 3 is formed on the drain layer 2 by epitaxial growth.
[0024] The body layers 4 are formed in the drift layer 3. The body layers 4 are made of silicon carbide of a second conductivity type. For example, the body layers 4 are p-type layers. For example, the body layers 4 are formed by ion implantation using aluminum as an impurity. The source layers 5 are formed in each of the body layers 4. The source layers 5 are made of silicon carbide of a first conductivity type having a higher impurity concentration than the drift layer 3. For example, the source layers 5 are n-type layers. + For example, the source layers 5 are formed by ion implantation using nitrogen as an impurity. The body contact layers 6 are formed in each of the body layers 4. In each of the body layers 4, the body contact layer 6 is surrounded by the source layer 5. The body contact layers 6 are made of silicon carbide of the second conductivity type having a higher impurity concentration than the body layers 4. For example, the body contact layers 6 are made of p + For example, the body contact layers 6 are formed by ion implantation using aluminum as an impurity.
[0025] The multiple gate insulating layers 7 are formed so as to contact the respective source layers 5 of the adjacent body layers 4. Specifically, the multiple gate insulating layers 7 are formed so as to span the body layers 4 adjacent to the drift layer 3 and the respective source layers 5 present inside the body layers 4. For example, the multiple gate insulating layers 7 are formed of silicon dioxide layers by thermal oxidation. The multiple gate electrode layers 8 are formed on the multiple gate insulating layers 7, respectively. For example, the multiple gate electrode layers 8 are formed of polysilicon by a CVD method.
[0026] The interlayer insulating layers 9 are formed so as to cover the gate electrode layers 8, respectively. For example, the interlayer insulating layers 9 are formed of silicon dioxide by a CVD method. The source electrode layers 10 are formed corresponding to the body layers 4, respectively. The source electrode layers 10 are formed so as to contact the source layers 5. The source electrode layers 10 may be formed so as to straddle the body contact layers 6. For example, the source electrode layers 10 are formed by depositing Ni or the like by a sputtering method or the like, followed by heat treatment. The wiring electrode layer 11 is formed so as to cover the source electrode layers 10. For example, the wiring electrode layer 11 is formed of an aluminum alloy or the like by a sputtering method or the like.
[0027] The drain electrode layer 12 is formed on the second surface (the lower surface in FIG. 1) of the drain layer 2. For example, the drain electrode layer 12 is formed by depositing Ni or the like by a sputtering method or the like and subjecting it to a heat treatment.
[0028] In this embodiment, a column structure C is formed in the drift layer 3. In the column structure C, a plurality of first conductivity type columns C1 and a plurality of second conductivity type columns C2 are arranged alternately. The plurality of first conductivity type columns C1 are part of a layer formed as the drift layer 3. The plurality of second conductivity type columns C2 are formed separately from the layer formed as the drift layer 3.
[0029] Each of the multiple second-conductivity type columns C2 is formed below the source electrode layer 10. In each of the multiple second-conductivity type columns C2, the upper part is surrounded by the body layer 4, the source layer 5, and the body contact layer 6. Each of the multiple second-conductivity type columns C2 has a multi-stage sawtooth-shaped outer part in a cross-sectional view. Specifically, in each of the multiple second-conductivity type columns C2, multiple first inclined portions A1 and multiple second inclined portions A2 are alternately arranged in the thickness direction of the drift layer 3. The first inclined portion A1 is formed so as to widen in the lateral direction from one surface (upper surface in FIG. 1) of the drain layer 2 to the other surface (lower surface in FIG. 1). The second inclined portion A2 is formed so as to narrow in the lateral direction from one surface of the drain layer 2 to the other surface. In this case, the second inclined portion A2 is formed so as to narrow more rapidly than the first inclined portion A1 widens.
[0030] More specifically, each of the multiple columns C2 of the second conductivity type includes an impurity layer 13 and a filling layer 14. The impurity layer 13 forms an outer portion of the column C2 of the second conductivity type. The impurity layer 13 is made of silicon carbide of the second conductivity type. The impurity layer 13 is a p-type layer. For example, the impurity layer 13 is formed by ion implantation using aluminum as an impurity. The impurity concentration of the impurity layer 13 is 1.0×10 17 cm -3 Above 1.0×10 20 cm -3 The filling layer 14 is formed inside the impurity layer 13. The filling layer 14 is made of an insulator or a semiconductor. For example, the filling layer 14 is made of silicon dioxide.
[0031] Thus, in this embodiment, a trench structure is formed in the drift layer 3 by alternating a plurality of first conductivity type columns C1 and a plurality of second conductivity type columns C2. When a reverse voltage is applied to this structure, a depletion layer spreads laterally. As a result, a depletion layer is formed to the depth of the trench. At this time, the depletion layer spreads only by half the distance between the trenches, and a depletion layer with a thickness equal to the depth of the trench is formed.
[0032] In the superjunction structure, it is preferable that the grooves and the intervals between the grooves are as narrow and deep as possible. Although the column C shown in FIG. 1 is formed partway through the drift layer 3, it may be formed over the entire drift layer 3. This allows the on-resistance to be further reduced. The impurity concentration of the drift layer 3 can be increased to about five times that of a non-superjunction structure. As described above, in the superjunction structure, the breakdown voltage is ensured by a mechanism different from that of conventional MOSFETs. Therefore, performance exceeding the so-called silicon limit or SiC limit is brought out, and the on-resistance can be reduced.
[0033] 1, adjacent columns C2 of the second conductivity type are arranged so that their multi-stage sawtooth outer parts fit together. That is, adjacent columns C2 of the second conductivity type are arranged so as to be shifted from each other by half a stage of the sawtooth outer parts in the depth direction. In other words, in a cross-sectional view, the laterally expanding parts and the constricted parts of the impurity layers 13 of adjacent columns C2 of the second conductivity type are arranged in a positional relationship that approximately corresponds to each other.
[0034] The maximum width 13MaxW of the impurity layer 13 in a cross-sectional view shown in Fig. 1 is 0.3 µm, and the minimum width 13MinW of the impurity layer 13 in a cross-sectional view shown in Fig. 1 is 0.1 µm.
[0035] Here, the superjunction structure pitch (hereinafter referred to as "SJ pitch") P shown in Fig. 1 indicates the interval at which adjacent second-conductivity type columns C2 are arranged. The distance L1 shown in Fig. 1 indicates the distance between the horizontally expanding portion of the second-conductivity type column C2 on the left side as you face it in Fig. 1 and the narrowed portion of the second-conductivity type column C2 on the right side as you face it in Fig. 1, which are arranged in a corresponding positional relationship.
[0036] Distance L2 shown in Fig. 1 indicates the distance between the constricted portion of column C2 of second conductivity type on the left side of Fig. 1 and the horizontally expanding portion of column C2 of second conductivity type on the right side of Fig. 1, which are arranged in a corresponding positional relationship. When SJ pitch P is 4 μm and groove width W of filling layer 14 is 1 μm, distance L1 and distance L2 are both 2.6 μm. These distances are the maximum inter-column distances.
[0037] Next, a comparative example will be described. FIG. 2 is a cross-sectional view of the comparative example. As shown in FIG. 2, in the comparative example, adjacent columns C2 of the second conductivity type are not arranged so that their multi-stage sawtooth outer parts fit together. That is, adjacent columns C2 of the second conductivity type are not arranged to be shifted by half a step of the sawtooth outer parts in the depth direction. In other words, in a cross-sectional view, the horizontally spreading parts of the impurity layer 13 of adjacent columns C2 of the second conductivity type are arranged in a corresponding positional relationship as shown by the distance L5, and the constricted parts of the impurity layer 13 are arranged in a corresponding positional relationship as shown by the distance L4. In the comparative example, when the SJ pitch P is 4 μm and the groove width W of the filling layer 14 is 1 μm, the distance between the constricted parts of the impurity layer 13 of adjacent columns C2 of the second conductivity type, that is, the maximum distance L4 between the columns, is 2.8 μm. Moreover, the distance L5 between the spreading portions of the impurity layers 13 of the adjacent second-conductivity type columns C2 is 2.4 μm.
[0038] Table 1 shows the parameters of the present invention and comparative examples when the SJ pitch P is 2 μm, 4 μm, and 10 μm when the withstand voltage of the semiconductor element is about 1200 V.
[0039] [Table 1]
[0040] As shown in Table 1, for both the present invention and the comparative example, the maximum inter-column distance is smaller for the present invention than the inter-column distance L4 for the comparative example at any SJ pitch P. When the same reverse voltage is applied, the present invention makes it possible to pinch off the depletion layer between adjacent columns C2 even if the concentration of the impurity layer 13 is increased to reduce the spread of the depletion layer. By increasing the concentration of the impurity layer 13, the on-resistance can be further reduced.
[0041] FIG. 3 is a diagram showing the relationship between SJ pitch P and on-resistance. The solid line shows the on-resistance value at each SJ pitch P of the present invention, and the dashed line shows the on-resistance value at each SJ pitch P of the comparative example. As shown in FIG. 3, the on-resistance value of the present invention is lower than that of the comparative example at each SJ pitch P. Here, the dashed dotted line shows the improvement rate of the on-resistance value of the present invention compared to the comparative example. As shown in FIG. 3, it can be seen that the smaller the SJ pitch P, the higher the improvement rate. In other words, it can be said that the present invention can achieve greater effects as semiconductor devices become more miniaturized.
[0042] Next, a method for manufacturing the semiconductor device 1 shown in FIG. 1 will be described. First, a drift layer forming step is performed. In the drift layer forming step, the drift layer 3 is formed on the drain layer 2. Then, three types of ion implantation steps are performed. In each of the three types of ion implantation, a resist pattern is first formed. Then, the ion implantation is performed. Then, the resist pattern is removed. As a result, a p-type ion implanted portion and an n-type ion implanted portion are formed. + Type ion implantation area and p + The p-type ion implanted portion becomes the body layer 4. + The ion-implanted portion of the p-type layer becomes the source layer 5. + The ion-implanted portion of the mold becomes the body contact layer 6.
[0043] Thereafter, a mask pattern forming process is performed. The processes after the mask pattern forming process will be described with reference to FIG. 4. FIG. 4 is a cross-sectional view for explaining the manufacturing method of the semiconductor device 1. Note that the second conductivity type column is formed in the region where the body layer 4, the source layer 5, and the body contact layer 6 are formed, but these are omitted in FIG. 4 for convenience of explanation.
[0044] As shown in FIG. 4(a), in the mask pattern formation step, a silicon dioxide layer is formed on the drift layer 3. Then, a resist pattern is formed. Then, dry etching is performed. Then, the resist pattern is removed. As a result, a first mask pattern 15 made of silicon dioxide is formed.
[0045] The first mask pattern 15 has openings formed at positions corresponding to regions where a plurality of second conductivity type columns that are not adjacent to each other will be formed in a later step.
[0046] Here, as shown in FIG. 4(a), a part of the drift layer 3 is etched. The amount of etching at this time is half the amount of one step that forms the multi-step sawtooth shape of the outer part of the second conductivity type column in a cross-sectional view formed in a later process. For example, the amount of etching can be 0.25 μm. Although not shown, impurities may be ion-implanted using the first mask pattern 15 before etching the drift layer 3. Then, the first mask pattern 15 is removed.
[0047] 4(b), a second mask pattern 16 made of silicon dioxide is formed. The second mask pattern 16 is formed to be thicker than the first mask pattern 15.
[0048] For example, in silicon carbide etching by ICP-RIE in an SF6-O2-Ar atmosphere, the selectivity between the first mask pattern 15 and silicon dioxide, which is the material of the second mask pattern 16, can be 8. In this case, even if the second mask pattern 16 is reduced in the etching process, the ion implantation process and the etching process can be repeated multiple times using the same mask pattern. For example, when the film thickness of the second mask pattern 16 is set to 2 μm, the selectivity is 8, so that the silicon carbide layer can be etched to a film thickness of 16 μm. This means that etching can be performed deeper than the thickness (about 10 μm) of the drift layer 3 of a silicon carbide semiconductor device having a breakdown voltage of about 1200 V without a superjunction structure. Here, it is necessary to set the thickness of the second mask pattern 16 appropriately, taking into consideration not only the etching selectivity but also the penetration depth of the impurities into the second mask pattern 16 by ion implantation, so that the impurities do not penetrate the second mask pattern 16 and penetrate into the drift layer 3. For example, when the drift layer 3 is etched by 10 μm using the second mask pattern 16 with a selection ratio of 8, the loss of the second mask pattern 16 is 1.25 μm. Furthermore, the thickness required for the second mask pattern 16 to function as a mask during ion implantation is about 1 μm when the mask material is silicon dioxide. In this case, the thickness of the second mask pattern 16 needs to be at least 2.25 μm. In consideration of the manufacturing margin, the thickness of the second mask pattern 16 is preferably set to, for example, 2.5 μm. When the drift layer 3 is 10 μm, the film thickness of the second mask pattern 16 can be set to, for example, 2.5 μm, and the semiconductor device 1 with improved on-resistance characteristics can be manufactured more stably.
[0049] The second mask pattern 16 has openings formed at positions corresponding to the regions where the multiple second conductivity type columns whose formation has begun by the first mask pattern 15 and the multiple second conductivity type columns adjacent to these will be formed.
[0050] Next, an ion implantation process is performed as shown in Fig. 4(c). Specifically, in the ion implantation process, impurities such as aluminum are ion-implanted into the drift layer 3 at positions corresponding to the openings of the second mask pattern 16. At this time, the ion implantation is performed so that a part of the region where the impurities exist extends outward beyond the openings of the mask pattern in top view. As a result, a p-type impurity layer 13 is formed.
[0051] 4(d), an etching process is performed using the second mask pattern 16 as it is. In the etching process, the impurity layer 13 is etched at positions corresponding to the openings of the second mask pattern 16. At this time, the second mask pattern 16 is also reduced in accordance with the etching selectivity.
[0052] Next, as shown in Fig. 4(e), an ion implantation process is performed again using the second mask pattern 16 as it is. The ion implantation process is performed again in the same manner as described in Fig. 4(c). After that, although not shown, an etching process is performed in the same manner as described in Fig. 4(d).
[0053] Thereafter, the ion implantation step described in FIG. 4(c) and the etching step described in FIG. 4(d) are repeated a desired number of times. In this manner, the ion implantation step and the etching step are alternately performed multiple times. When the final etching step described in FIG. 4(d) is completed, a multi-stage sawtooth impurity layer 13 is formed as shown in FIG. 1. Thereafter, a step of removing the second mask pattern 16 is performed. In the mask pattern removing step, the second mask pattern 16 is removed.
[0054] Then, a carbon cap forming step is performed. In the carbon cap forming step, a carbon cap layer is formed. Then, an annealing step is performed. In the annealing step, an annealing treatment is performed in a high temperature atmosphere to activate the ion-implanted impurity element (dopant). Then, a carbon cap removing step is performed. In the carbon cap removing step, the carbon cap layer is removed.
[0055] Then, a filling step is performed. In the filling step, silicon dioxide is used by, for example, a CVD method to fill the grooves formed in the etching step. Then, an etch-back step is performed. In the etch-back step, silicon dioxide is removed down to the top surface of the drift layer 3. As a result, a filling layer 14 is formed.
[0056] Then, a gate insulating layer forming process is performed. In the gate insulating layer forming process, a gate insulating film is formed by a thermal oxidation method or the like. Then, a resist pattern is formed. Then, the gate insulating film is etched. Then, the resist pattern is removed. As a result, a gate insulating layer 7 is formed.
[0057] Thereafter, a gate electrode layer forming process is performed. In the gate electrode layer forming process, a polysilicon film is formed by a CVD method or the like. Then, a resist pattern is formed. Then, the polysilicon film is etched. Then, the resist pattern is removed. As a result, a gate electrode layer 8 is formed. Then, a source electrode layer forming process is performed. In the source electrode layer forming process, a metal film such as Ni is formed by a sputtering method or the like. Then, a resist pattern is formed. Then, the metal film is etched. Then, the resist pattern is removed. Then, a heat treatment such as metal sintering is performed. As a result, a source electrode layer 10 is formed.
[0058] Thereafter, an interlayer insulating layer forming process is performed. In the interlayer insulating layer forming process, an interlayer insulating layer 9 such as silicon dioxide is formed by a CVD method or the like. Thereafter, a wiring electrode layer forming process is performed. In the wiring electrode layer forming process, a wiring electrode layer 11 such as an aluminum alloy is formed by a sputtering method or the like. Thereafter, a drain electrode layer forming process is performed. In the drain electrode layer forming process, a metal film such as Ni is formed by a sputtering method or the like. Then, a heat treatment such as laser annealing is performed. As a result, a drain electrode layer 12 is formed.
[0059] Next, a method for forming the second conductivity type impurity layer 13 will be described with reference to FIG. FIG. 5 is a diagram for illustrating a method of forming an impurity layer of a second conductivity type in the semiconductor device according to the first embodiment.
[0060] FIG. 5 shows a profile when aluminum is used as an impurity and ion-implanted from the top of the figure into one central point of the silicon carbide drift layer 3. As shown in FIG. 5, in each ion-implantation process, the impurity spreads radially into the silicon carbide drift layer 3. At this time, the impurity reaches a depth of, for example, about 0.5 μm to 0.7 μm. The lateral spread of the impurity is, for example, 0.2 μm to 0.3 μm. Although not shown in FIG. 5, by repeating such ion implantation while changing the depth by etching the silicon carbide drift layer 3 as described above, in each of the multiple second conductivity type columns C2, the outer part is formed into a multi-stage sawtooth shape in which multiple first inclined portions A1 and multiple second inclined portions A2 are alternately arranged in the thickness direction of the drift layer 3.
[0061] According to the first embodiment described above, the plurality of second-conductivity type columns C2 have a multi-stage sawtooth outer portion in a cross-sectional view, and the multi-stage sawtooth outer portion of the plurality of second-conductivity type columns C2 is arranged so as to fit with the multi-stage sawtooth outer portion of another adjacent second-conductivity type column. That is, the adjacent second-conductivity type columns C2 are arranged to be shifted by half of one stage of the sawtooth outer portion in the depth direction. The second-conductivity type column C2 is formed by the impurity layer 13 and the filling layer 14. Therefore, it is possible to easily manufacture the semiconductor device 1 having a superjunction structure with improved on-resistance characteristics.
[0062] In addition, in a cross-sectional view of the multiple second conductivity type columns C2, the impurity layer 13 above the body layer 4 or the body contact layer 6 may be omitted. In this case, the number of ion implantation steps is reduced, and the semiconductor device 1 with improved on-resistance characteristics can be manufactured more inexpensively.
[0063] Furthermore, the filling layer 14 is made of an insulator or a semiconductor, which makes it easier to manufacture the semiconductor device 1 with improved on-resistance characteristics.
[0064] The impurity concentration of the impurity layer 13 is 1.0×10 17 cm -3 Above 1.0×10 20 cm -3 As a result, improved on-resistance characteristics can be obtained more reliably.
[0065] The first conductivity type column C1 is made of silicon carbide of the first conductivity type. The impurity layer 13 is made of silicon carbide of the second conductivity type. This improves the on-resistance characteristics of the silicon carbide semiconductor device 1, and allows it to be manufactured stably.
[0066] Furthermore, in the drift layer 3, a plurality of columns C2 of the second conductivity type are formed so as to define an outer portion of a multi-stage sawtooth shape in cross section. This makes it possible to easily manufacture a semiconductor device 1 with improved on-resistance characteristics.
[0067] Furthermore, by repeating the etching process and the ion implantation process, a plurality of second conductivity type columns C2 are formed so that the outer portion has a multi-stage sawtooth shape in cross section. In the etching process, the mask pattern is used repeatedly. Therefore, it is not necessary to form a mask silicon dioxide layer for each stage, perform photolithography, etching, remove resist, or remove the mask.
[0068] One method for forming an impurity layer on the trench sidewall of column C2 in a deep region with a high aspect ratio without using the present invention is to implant ions obliquely from the opening. As the aspect of the trench becomes higher, the ion implantation angle approaches horizontal from the perpendicular direction to the trench sidewall of column C2, which is the implantation surface. In this case, the ions are reflected by the surface and are difficult to penetrate into the trench sidewall, resulting in poor ion implantation efficiency. In order to achieve the necessary impurity concentration in the impurity layer 13, a larger dose is required than in the case of vertical ion implantation, which takes a long time and reduces productivity. In addition, it becomes difficult to make the concentration of the impurity layer 13 uniform between the upper and lower parts of column C2.
[0069] In the ion implantation method of the present invention, the lateral spread in the silicon carbide drift layer 3 due to vertical ion implantation can be utilized. This reduces the difficulty of the ion implantation process described above. As a result, the semiconductor device 1 with improved on-resistance characteristics can be easily manufactured.
[0070] In addition, in the ion implantation process, the ions are implanted so that a part of the region where the impurities are present extends outside the opening of the mask pattern when viewed from above, which makes it possible to easily manufacture the semiconductor device 1 with improved on-resistance characteristics.
[0071] Furthermore, after the ion implantation process and the etching process are repeated, the grooves formed by the etching process are filled with an insulator or a semiconductor. Therefore, voids are less likely to occur than when the grooves are filled with silicon carbide of the second conductivity type by an epitaxial method. As a result, the semiconductor device 1 with improved on-resistance characteristics can be easily manufactured.
[0072] The semiconductor device 1 may also be a silicon carbide trench MOSFET having a superjunction structure. In the trench MOSFET semiconductor device 1, the multiple second-conductivity type columns C2 also have a multi-stage sawtooth outer portion in a cross-sectional view, and the multiple-stage sawtooth outer portion of the multiple second-conductivity type columns C2 are arranged so as to fit with the multiple-stage sawtooth outer portion of another adjacent second-conductivity type column. That is, the adjacent second-conductivity type columns C2 are arranged to be shifted by half of one stage of the sawtooth outer portion in the depth direction. The second-conductivity type columns C2 are formed by the impurity layer 13 and the filling layer 14. This makes it possible to easily manufacture the trench MOSFET semiconductor device 1 having a superjunction structure with improved on-resistance characteristics.
[0073] In the semiconductor device 1 of the first embodiment, the first conductivity type may be p-type and the second conductivity type may be n-type, with the result that improved on-resistance characteristics can be obtained.
[0074] Moreover, the configuration of the first embodiment may be applied to the semiconductor device 1 whose main component is silicon. In this case as well, improved on-resistance characteristics can be obtained.
[0075] Having described several aspects of at least one embodiment, it should be understood that various alterations, modifications, and improvements will readily occur to those skilled in the art and are intended to be part of this disclosure, and are intended to be within the scope of this disclosure.
[0076] It is to be understood that the embodiments of the method and apparatus described herein are not limited in their application to the details of construction and the arrangement of components set forth in the above description or illustrated in the accompanying drawings, and the method and apparatus can be implemented in other embodiments and practiced or carried out in various ways.
[0077] The specific implementations are provided herein for illustrative purposes only and are not intended to be limiting.
[0078] The phraseology and terminology used in this disclosure are for the purpose of description and should not be regarded as limiting. The use of "including," "comprising," "having," "including" and variations thereof herein means the inclusion of the items listed thereafter and equivalents thereof as well as additional items.
[0079] References to "or" may be construed as meaning that any term described using "or" refers to one, more than one, and all of those described terms.
[0080] All references to front, back, left, right, top, bottom, up, down, horizontal, vertical, front and back are intended for convenience of description. Such references are not intended to limit the components of this disclosure to any one positional or spatial orientation. Accordingly, the foregoing description and drawings are by way of example only. [Explanation of symbols]
[0081] REFERENCE SIGNS LIST 1 semiconductor device, 2 drain layer, 3 drift layer, 4 body layer, 5 source layer, 6 body contact layer, 7 gate insulating layer, 8 gate electrode layer, 9 interlayer insulating layer, 10 source electrode layer, 11 wiring electrode layer, 12 drain electrode layer, 13 impurity layer, 14 filling layer, 15, 16 silicon dioxide layer
Claims
1. A drain layer formed of a first conductivity type semiconductor; a drift layer formed on one surface of the drain layer and made of a semiconductor of a first conductivity type; a column structure in which a plurality of first conductivity type columns and a plurality of second conductivity type columns are alternately arranged in the drift layer; Equipped with the second conductivity type column has an outer portion having a multi-stage sawtooth shape in cross section; A semiconductor device having a superjunction structure in which the multi-stage sawtooth outer portion of the second conductivity type column is arranged to fit into the multi-stage sawtooth outer portion of another adjacent second conductivity type column.
2. The second conductivity type column is an impurity layer of a second conductivity type; A filling layer formed inside the impurity layer; The semiconductor device according to claim 1 ,
3. The semiconductor device according to claim 2 , wherein the filling layer is made of an insulator or a semiconductor.
4. The impurity concentration of the impurity layer is 1.0×10 17 cm -3 Above 1.0 x 10 20 cm -3 4. The semiconductor device according to claim 2, wherein:
5. 2. The semiconductor device according to claim 1, wherein the pitch between adjacent second conductivity type columns is 4 [mu]m or less.
6. the first conductivity type column is formed of first conductivity type silicon carbide; 4. The semiconductor device according to claim 2, wherein the impurity layer is made of silicon carbide of the second conductivity type.
7. a drift layer forming step of forming a drift layer of the first conductivity type by epitaxial growth on a drain layer formed of a semiconductor of the first conductivity type; a second conductivity type column forming step of forming a plurality of second conductivity type columns in the drift layer so as to define an outer portion of a multi-stage sawtooth shape in cross section; Equipped with The second conductivity type column forming step includes: an etching step of performing etching using a first mask having openings formed at positions corresponding to regions in which a plurality of second conductivity type columns that are not adjacent to each other are to be formed among the plurality of second conductivity type columns; A first step including: a second step including an ion implantation step of ion-implanting impurities using a second mask having openings formed at positions corresponding to a region in which the plurality of second conductivity type columns whose formation has begun in the first step and a plurality of adjacent second conductivity type columns are to be formed, and an etching step of etching a part of the region in which the ions have been implanted using the second mask as it is; A method for manufacturing a semiconductor device having a superjunction structure comprising:
8. 8. The method for manufacturing a semiconductor device according to claim 7, wherein the depth etched in the first etching step is half the depth etched in the second etching step.
9. 8. The method for manufacturing a semiconductor device according to claim 7, wherein the ion implantation process and the etching process in the second step are repeated to form a plurality of columns of the second conductivity type so that the outer portion has a multi-stage sawtooth shape in cross section.
10. 10. The method for manufacturing a semiconductor device according to claim 7, wherein the ion implantation step includes implanting ions such that a part of a region in which the impurity is present extends outside the opening of the mask when viewed from above.
11. 11. The method for manufacturing a semiconductor device according to claim 9, further comprising a filling step of filling a groove formed by the etching step with an insulator or a semiconductor after the ion implantation step and the etching step are repeated in the second step.
Citation Information
Patent Citations
Semiconductor device having super junction structure
JP2013102087A
Corner layout for superjunction device
US8476698B2