Coating film treatment method

The method addresses the inefficiencies of traditional paint film removal by applying a paint film and using a high-evaporation solvent to soften and peel off old paint films, enhancing workability and reducing construction time.

JP2024142679APending Publication Date: 2024-10-11BEKKU KK
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023054926
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing paint film removal methods using stripping agents are time-consuming and result in the remover remaining on the base material, prolonging the construction period and interfering with the next process.

Method used

A method involving applying a paint to form a film, followed by using a specific stripping agent to soften and peel off the old paint film, utilizing an organic solvent with a high evaporation rate and a coating containing a resin and powder component to facilitate easy removal.

Benefits of technology

The method allows for quick and efficient removal of old paint films, preventing remover residue and reducing construction time by improving workability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024142679000001
    Figure 2024142679000001
Patent Text Reader

Abstract

To provide a coating film treatment method in which coating material (I) is applied to an old coating film and dried to form a coating film (I), and then the old coating film is peeled together with the coating film (I) by a specific peeling agent.SOLUTION: The present invention is a method of treating an old coating film on a substrate, comprising: a step of applying coating material (I) to a surface of the old coating film and drying the coating material to form a coating film (I); a step of applying a peeling agent to a surface of the coating film (I) to soften the coating film (I), and then peeling off the coating film (I) and the old coating film, where: the peeling agent includes an organic solvent having relative evaporation rate of 100 or more when evaporation rate of butyl acetate is 100.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a novel coating treatment method. [Background technology]

[0002] Methods for treating coating films (old coating films) formed on the surfaces of buildings, civil engineering structures, etc. include removing weak parts (defective parts) of the old coating film, and then painting with new paint or attaching building materials (e.g., sheets, decorative boards, wallpaper, etc.). Methods for removing old coatings include physical methods such as sanding, blasting, high-pressure water spraying, and chisel chipping, as well as chemical methods using chemicals and solvents. Recently, chemical methods using stripping agents have been used to prevent problems such as damage to the base and scattering of dust, and to be environmentally friendly (see, for example, Patent Documents 1-2, etc.). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-131651 A [Patent Document 2] JP 2018-70725 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the coating removal method using a release agent, the old coating is softened with the release agent and then removed with a scraper or the like, but removing the weak parts of the old coating can be time-consuming. In addition, after removing the weak parts (defective parts) of the old coating, the release agent may remain on the substrate or on the strong parts (sound parts) of the old coating, which may cause problems in the next process and extend the construction period.

[0005] The present invention has been made in consideration of the above-mentioned points, and has as its object to provide a coating film treatment method which is easy to use. [Means for solving the problem]

[0006] In order to solve such problems, the inventors of the present invention conducted extensive research and came up with the idea of ​​a coating film treatment method in which paint (I) is applied to an old coating film, the coating film (I) is formed by drying, and then the old coating film is peeled off together with the coating film (I) using a specific peeling agent, thereby completing the present invention.

[0007] That is, the present invention has the following features. 1. A method for treating an old coating on a substrate, comprising the steps of: A step of applying paint (I) to the surface of the old coating film and drying it to form a coating film (I); A step of applying a release agent to the surface of the coating film (I), softening the coating film (I), and then peeling off the coating film (I) and the old coating film; Including, The coating treatment method according to the present invention, wherein the stripping agent contains an organic solvent having a relative evaporation rate of 100 or more when the evaporation rate of butyl acetate is taken as 100. 2. The coating treatment method according to claim 1, wherein the stripping agent contains 50% by weight or more of an organic solvent having a relative evaporation rate of 100 or more when the evaporation rate of butyl acetate is taken as 100. 3. The coating film treatment method according to 1, wherein the coating material (I) contains a resin component and a powder component in the solid content of the coating material (I). Effect of the Invention

[0008] According to the coating film treatment method of the present invention, the old coating film can be easily peeled off. In particular, the weak parts (defective parts) of the old coating film can be quickly and easily peeled off, and the stripping agent can be prevented from remaining on the surface (the substrate or the tough parts of the old coating film) after the weak part removal treatment. This improves workability and allows the old coating film to be treated without prolonging the construction period. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, an embodiment of the present invention will be described.

[0010] The present invention relates to a method for treating an old coating film on a substrate, which includes a step of peeling off a coating film (old coating film) formed on the surface of a substrate such as a building or civil engineering structure. Examples of the substrate include concrete, mortar, slate board, calcium silicate board, ALC board, extrusion molded board, slate roofing tiles, cement roofing tiles, new roofing tiles, porcelain tiles, siding boards, metals, glass, wood, and plywood. The old coating film is a coating film that has been applied onto the above-mentioned substrate, and examples thereof include coating films formed by JIS K5621 "General-purpose rust-preventive paint", JIS K5651 "Amino alkyd resin coating", JIS K5658 "Weather-resistant topcoat coating for architecture", JIS K5659 "Weather-resistant coating for steel structures", JIS K5660 "Glossy synthetic resin emulsion paint", JIS K5661 "Fireproof coating for architecture", JIS K5663 "Synthetic resin emulsion paint", JIS K5668 "Synthetic resin emulsion pattern coating", JIS K5665 "Pavement marking coating", JIS K5667 "Multicolored pattern coating", JIS K5670 "Acrylic resin-based non-aqueous dispersion coating", JIS K5674 "Lead- and chromium-free rust-preventive paint", JIS K5675 "High solar reflectance coating for roofs", JIS A6909 "Architectural finishing coating material", and the like. The old coating film may be a single-layer coating film or a multi-layer coating film. Furthermore, the present invention is suitable for removing an old coating film that is easily dissolved by a remover and is difficult to remove, or an old coating film that has a defective portion such as insufficient strength, poor adhesion, or blistering.

[0011] The coating film treatment method of the present invention comprises the steps of: A step (hereinafter also referred to as "first step") of applying paint (I) to the surface of the old coating film and drying it to form a coating film (I); A step of applying a release agent to the surface of the coating film (I), softening the coating film (I), and then peeling off the coating film (I) and the old coating film (hereinafter also referred to as the "second step"); The present invention is characterized by comprising: According to the coating film treatment method of the present invention, even when it is difficult to directly apply a release agent to the old coating film (for example, when the old coating film is easily dissolved by the release agent), the old coating film can be easily peeled off by integrating the old coating film with the coating film (I), improving workability and reducing peeling residue. Furthermore, since the weak parts (defective parts) of the old coating film can be quickly and easily peeled off and the release agent can be prevented from remaining on the surface (the substrate or the tough parts of the old coating film) after the weak part removal treatment, the old coating film can be treated without prolonging the construction period.

[0012] The coating material (I) in the first step is not particularly limited, but preferably contains a resin component and a powder component. As the resin component, various synthetic resins can be used. Examples of the types of synthetic resins include vinyl acetate resin, polyester resin, alkyd resin, vinyl chloride resin, epoxy resin, acrylic resin, urethane resin, acrylic silicone resin, fluororesin, and the like, or composite resins thereof. These can be used alone or in combination of two or more. These resin components may have crosslinking reactivity. Examples of the form of such resin components include solvent-soluble resin, non-aqueous dispersion resin, water-soluble resin, and water-dispersible resin (synthetic resin emulsion), and it is particularly desirable to include a water-dispersible resin (hereinafter referred to as "synthetic resin emulsion").

[0013] Examples of synthetic resin emulsions include vinyl acetate resin emulsions, vinyl chloride resin emulsions, epoxy resin emulsions, acrylic resin emulsions, urethane resin emulsions, acrylic silicone resin emulsions, fluororesin emulsions, and the like, as well as composites thereof, etc. These may be used alone or in combination of two or more.

[0014] In addition, the synthetic resin emulsion is preferably one having crosslinking reactivity. This makes the formed coating film (I) less likely to be dissolved by the stripping agent, so that in the step of stripping the coating film, the coating film (I) can be stripped while generally maintaining a film (sheet) shape. This can further enhance the effects of the present invention.

[0015] The synthetic resin emulsion having crosslinking reactivity may be either one that undergoes a crosslinking reaction by itself or one that undergoes a crosslinking reaction by a crosslinking agent that is mixed separately. Such crosslinking reactivity can be imparted by combining reactive functional groups such as a carboxyl group and a metal ion, a carboxyl group and a carbodiimide group, a carboxyl group and an epoxy group, a carboxyl group and an aziridine group, a carboxyl group and an oxazoline group, a hydroxyl group and an isocyanate group, a carbonyl group and a hydrazide group, an epoxy group and an amino group, or two alkoxyl groups.

[0016] The synthetic resin preferably has a glass transition temperature (Tg) of 20° C. or lower (more preferably, −50 to 10° C., and even more preferably, −45 to 0° C.). In such a case, the formed coating film (I) has flexibility, which is advantageous in terms of peelability. Note that, in the present invention, Tg is a value calculated by the Fox formula from the types and the composition ratio of the monomers constituting the synthetic resin.

[0017] The coating material (I) preferably contains a crosslinking agent. As the crosslinking agent, for example, one or more of polyvalent metal oxides, polyvalent metal hydroxides, oxazoline compounds, carbodiimide compounds, hydrazine compounds, epoxy compounds, isocyanate compounds, etc. are preferably used. Among these, polyvalent metal oxides are preferred.

[0018] Preferred examples of the polyvalent metal oxide include magnesium oxide, calcium oxide, strontium oxide, barium oxide, cerium oxide, titanium oxide, zirconium oxide, niobium oxide, manganese oxide, iron oxide, cobalt oxide, nickel oxide, palladium oxide, copper oxide, zinc oxide, aluminum oxide, tin oxide, bismuth oxide, etc. These can be used alone or in combination of two or more.

[0019] The powder component is not particularly limited, but it is preferable that the powder component contains at least an extender pigment. Examples of extender pigments include heavy calcium carbonate, light calcium carbonate, kaolin, clay, china clay, diatomaceous earth, hydrous fine powder of silicic acid, talc, mica, barite powder, barium sulfate, precipitated barium sulfate, barium carbonate, magnesium carbonate, silica powder, aluminum hydroxide, etc. These can be used alone or in combination of two or more.

[0020] The particle size of the extender pigment is preferably 0.1 to 50 μm (more preferably 1 to 30 μm). The extender pigment also preferably has an oil absorption of 5 to 150 ml / 100 g (more preferably 10 to 100 ml / 100 g). The oil absorption is a value measured in accordance with JIS K 5101-13-1 (refined linseed oil method).

[0021] By including such powder components, the permeability of the stripping agent is increased, and the stripping agent can penetrate to the old coating film underneath the coating film (I). In addition, the dissolved components of the old coating film can be efficiently adsorbed. Furthermore, it is possible to thicken the coating film (I), which improves the work efficiency during stripping.

[0022] The content of the powder component is preferably 50 to 500 parts by weight (more preferably 80 to 300 parts by weight) per 100 parts by weight (solid content) of the synthetic resin emulsion. When this range is satisfied, the above-mentioned effects can be fully exhibited.

[0023] The paint (I) may contain a known color pigment as a powder component. When the paint (I) contains a color pigment, uneven application of the paint (I) can be prevented. Examples of color pigments include inorganic chromatic pigments such as ferric oxide (red oxide), yellow iron oxide, ultramarine, and cobalt green; organic chromatic pigments such as azo, naphthol, pyrazolone, anthraquinone, perylene, quinacridone, disazo, isoindolinone, benzimidazole, phthalocyanine, and quinophthalone; black pigments such as carbon black, iron-manganese composite oxide, iron-copper-manganese composite oxide, iron-chromium-cobalt composite oxide, copper-chromium composite oxide, copper-manganese-chromium composite oxide, and black iron oxide; white pigments such as titanium oxide, zinc oxide, and alumina; and pearl pigments, aluminum pigments, photoluminescent pigments, phosphorescent pigments, and fluorescent pigments. These can be used alone or in combination of two or more. The average particle size of the color pigment is preferably less than 1 μm, more preferably 0.01 to 0.9 μm. In the present invention, the average particle size of the pigment is an average value measured using a laser diffraction particle size distribution measuring device (measurement temperature: 25° C.).

[0024] In addition to the above-mentioned components, various other components can be mixed into the paint (I) to the extent that they do not affect the effects of the present invention. Examples of such components include plasticizers, preservatives, antifungal agents, anti-algae agents, antifoaming agents, leveling agents, pigment dispersants, anti-settling agents, anti-sagging agents, anti-skinning agents, dehydrating agents, ultraviolet absorbers, light stabilizers, antioxidants, catalysts, etc. The paint (I) can be produced by uniformly stirring and mixing the above-mentioned components by a conventional method.

[0025] In addition, the coating material (I) preferably has a non-volatile content of 60% by weight or more and 95% by weight or less (more preferably 65 to 90% by weight). When the coating material has such a non-volatile content, the coating film (I) can be thickened, and the permeability and peelability of the stripping agent can be further improved. Furthermore, it is preferable that the resin component ratio to the non-volatile content is 20% by weight or more (preferably 25% by weight or more and 60% by weight or less). By containing a large amount of resin components in the non-volatile content in this way, a uniform coating film (I) can be formed on the surface of the old coating film. On the other hand, the formed coating film (I) is softened by the stripping agent but is difficult to dissolve, and in the step of stripping the coating film, the coating film (I) can be stripped while maintaining its shape (film-like). The non-volatile content is the non-volatile content at the time of coating (application), and when the coating material (I) is diluted before coating, it refers to the non-volatile content after dilution. The non-volatile content in the present invention is the heating residue measured by the method of JIS K5601-1-2, the heating temperature is 105°C, and the heating time is 60 minutes.

[0026] When applying (painting) the coating material (I), various methods can be used, such as spray painting, roller painting, brush painting, etc. The amount of paint applied during painting is preferably 10 to 800 g / m 2 (More preferably 20 to 500 g / m 2 The number of coats of the coating material (I) may be appropriately determined depending on the surface condition of the old coating film, etc., but is preferably 1 to 2 coats. The thickness of the coating film (I) formed is preferably 0.1 to 1.0 mm (more preferably 0.2 to 0.6 mm). In such a case, the effect of the present invention can be further enhanced.

[0027] The drying time for the coating material (I) is preferably 8 hours or more (more preferably 16 hours or more). The drying temperature is preferably from -5 to 50°C (more preferably from 0 to 40°C).

[0028] After the first step, in the second step, a release agent is applied to the surface of the coating film (I), the coating film (I) is softened, and then the coating film (I) and the old coating film are peeled off. In the second step, the weak parts (defective parts) of the old coating film are particularly peeled off, and the weak parts (defective parts) of the old coating film are peeled off together with the coating film (I). The release agent in the second step is characterized by containing an organic solvent (S) (hereinafter also simply referred to as "organic solvent (S)") having a relative evaporation rate (measurement temperature 20°C) of 100 or more (preferably 300 or more, more preferably 500 or more) when the evaporation rate of butyl acetate is taken as 100. By containing such an organic solvent (S), it is possible to suppress the release agent from remaining in the tough parts of the substrate or the old coating film, so that the old coating film can be treated without prolonging the construction period.

[0029] The release agent preferably contains 50% by weight or more (more preferably 60% by weight or more and 95% by weight or less) of the organic solvent (S), which can further enhance the effects of the present invention.

[0030] As such an organic solvent (S), for example, one or more selected from acetone (relative evaporation rate 720), methyl ethyl ketone (relative evaporation rate 465), methyl isobutyl ketone (relative evaporation rate 145), methylene chloride (relative evaporation rate 1253), etc. can be used.

[0031] In addition to the organic solvent (S), the stripping agent of the present invention can contain, as a constituent, one or more selected from, for example, dibasic acid esters, benzyl alcohol, N,N-dimethylformamide, N-methyl-2-pyrrolidone, cyclopentanone, cyclohexanone, isophorone, diethylene glycol dimethyl ether, dipropylene glycol dimethyl ether, tetrahydrofuran, dimethyl sulfoxide, methanol, ethanol, isopropyl alcohol, sodium hydroxide, potassium hydroxide, sodium oleate, potassium oleate, and the like.

[0032] In addition to the above components, the release agent of the present invention may also contain known additives (e.g., thickeners, oxidizing agents, reducing agents, waxes, volatilization inhibitors, resins, solvents, drying regulators, surfactants, fragrances, colorants, dyes, etc.).

[0033] The release agent is applied to the surface of the coating film (I) at a rate of preferably 0.1 to 3.0 kg / m 2 (More preferably 0.2 to 3.0 kg / m 2 The coating tool is not particularly limited, and for example, a roller, a brush, a trowel, a spatula, a spray, a gun, or the like may be used for coating.

[0034] In the second step, the release agent is applied, and peeling can be started when the coating film (I) is softened (when shrinkage or the like occurs in the coating film), but peeling can be started preferably within 30 minutes (more preferably within 20 minutes) immediately after application. There are no particular limitations on the peeling tool, and peeling can be performed using, for example, a trowel, spatula, scraper, or the like.

[0035] In the coating treatment method of the present invention, a repair step can be carried out as a third step after the first step and the second step. Examples of the repair process include painting with paint (e.g., base preparation material, undercoat material, intermediate coating material, top coating material, etc.) and attaching building materials (e.g., sheets, wallpaper, tiles, decorative boards, etc.). These can be carried out by selecting paint and building materials having the desired functionality and design, and by using known methods. The repair process in the third step can be carried out preferably 24 hours (more preferably 48 hours) after the second step, which can shorten the construction period. EXAMPLES

[0036] [Old paint film] A slate board (300 x 300 x 6 mm) was coated on one side with JIS K5670 "acrylic resin non-aqueous dispersion paint" at a rate of 0.3 kg / m. 2This was exposed to an accelerated weathering tester "Eye Super UV Tester" (manufactured by Iwasaki Electric Co., Ltd.) for 400 hours to obtain the old coating film.

[0037] [Paint (I)] ·Paint 1 Paint 1 was produced by uniformly mixing 100 parts by weight of acrylic resin emulsion (solid content: 50% by weight, Tg: -30°C), 100 parts by weight of heavy calcium carbonate (average particle size: 5 μm, oil absorption: 15 ml / 100 g), and additives (dispersant, thickener, film-forming aid, etc.). ·Paint 2 Paint 2 was produced by uniformly mixing 100 parts by weight of acrylic resin emulsion (solid content: 50% by weight, Tg: 3°C), 100 parts by weight of heavy calcium carbonate (average particle size: 5 μm, oil absorption: 15 ml / 100 g), and additives (dispersant, thickener, film-forming aid, etc.). ·Paint 3 Paint 3 was produced by uniformly mixing 100 parts by weight of acrylic resin emulsion (solid content: 50% by weight, Tg: 3°C), 300 parts by weight of heavy calcium carbonate (average particle size: 5 μm, oil absorption: 15 ml / 100 g) and additives (dispersant, thickener, film-forming aid, etc.).

[0038] [Removal Agent] Stripping agent 1 Methylene chloride 82% by weight, dimethylformamide 3% by weight, and additives (thickener, dryness regulator, etc.) 15% by weight (total 100% by weight) were mixed uniformly to produce Release Agent 1. Stripping agent 2 Release agent 2 was produced by uniformly mixing 30% by weight of N-methylpyrrolidone, 55% by weight of dibutyl ether, and 15% by weight of additives (thickener, dryness regulator, etc.) (total 100% by weight).

[0039] <Test 1> Place the old paint surface vertically and apply paint (I) at a rate of 0.3 kg / m 2 After that, it was dried for 24 hours to form a coating film (I). Next, a release agent was applied in an amount of 0.8 kg / m2 Immediately after that, the coating film (I) and the old coating film were peeled off with a spatula. The peelability at this time was evaluated. All steps were carried out in an environment with a temperature of 23 degrees and a relative humidity of 50%. The coating material (I) and the release agent used in Test Examples 1 to 7 are shown in Table 1. In Test Examples 6 and 7, the release agent was directly applied to the old coating film by roller coating. The peelability was evaluated on a four-point scale, with "A" indicating smooth peeling without any problems and excellent peeling effect, and "D" indicating difficult and not smooth peeling. The results are shown in Table 1. Furthermore, the time (drying property) until the next process (repair process) could be carried out after the peeling process was measured. Drying property was evaluated as "○" when it was possible to paint within 24 hours after the peeling process at 23°C, and "×" when it took more than 24 hours to dry.

[0040] [Table 1]

Claims

1. 1. A method for treating an old coating on a substrate, comprising: A step of applying paint (I) to the surface of the old coating film and drying it to form a coating film (I); A step of applying a release agent to the surface of the coating film (I), softening the coating film (I), and then peeling off the coating film (I) and the old coating film; Including, The coating film treatment method according to the present invention, wherein the stripping agent contains an organic solvent having a relative evaporation rate of 100 or more when the evaporation rate of butyl acetate is taken as 100.

2. 2. The coating treatment method according to claim 1, wherein the stripping agent contains 50% by weight or more of an organic solvent having a relative evaporation rate of 100 or more when the evaporation rate of butyl acetate is taken as 100.

3. 2. The coating film treatment method according to claim 1, wherein the coating material (I) contains a resin component and a powder component in the solid content of the coating material (I).

Citation Information

Patent Citations

  • Coated film peeling agent and coated film peeling method

    JP2018070725A

  • Coated film release agent

    JP2019131651A