Soil volume reduction test apparatus and electroosmotic consolidation process utilizing soil volume reduction test apparatus
The electroosmotic consolidation method using adjustable potential gradients and specialized electrodes addresses the inefficiencies of conventional dewatering methods, achieving rapid water drainage and volume reduction in clay soils for efficient disposal and disaster prevention.
Patent Information
- Application Number
- JP2023055106
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-11
AI Technical Summary
Conventional methods for dewatering clay soil, such as those used in dredged soil disposal and disaster prevention, are inefficient due to low water permeability and reliance on hydraulic conductivity, leading to slow drainage and volume reduction.
An electroosmotic consolidation test device and method using electrodes with adjustable potential gradients and titration capabilities to enhance dehydration, along with RS electrodes and titration electrodes, to promote rapid and targeted water drainage.
The method achieves rapid and efficient water drainage and volume reduction in clay soils, contributing to both soil disposal efficiency and disaster mitigation by shortening consolidation times and improving drainage speed.
Smart Images

Figure 2024142786000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a soil volume reduction test device, for example, clayey soil, and an electro-osmotic consolidation method using said test device. [Background technology]
[0002] A large amount of dredged soil is generated every year by dredging for the purpose of ensuring and increasing the water depth in front of sea channels, anchorages, and revetments. The dredged soil is used as solidified treated soil for landfilling behind quays and revetments, and is also dumped into coastal disposal sites.
[0003] In order to utilize landfill sites efficiently, it is necessary to promote the reduction of the volume of dredged soil by dewatering. In addition, the disposal of dredged soil, which is generated continuously, is a problem all over Japan, and it is extremely necessary, important, and urgent to propose a method of reducing the volume of dredged soil in order to utilize landfill sites efficiently.
[0004] However, the present invention is directed to the volume reduction of, for example, dredged soil by electro-osmosis, and relates to a soil mechanical evaluation of the electro-osmosis dewatering mechanism and electro-osmosis specifications for efficient volume reduction, in other words, electro-osmosis consolidation test equipment to be used in the electro-osmosis consolidation method, as well as electrodes to be used in the test equipment, and an electro-osmosis consolidation method to be actually applied on site using the results of tests conducted using these test equipment.
[0005] Meanwhile, with climate change causing weather disasters to become more severe and frequent, and the occurrence of large-scale earthquakes such as the Nankai Trough earthquake and the Tokyo metropolitan area earthquake imminent, there is an urgent need to develop innovative disaster prevention and mitigation technologies that protect both lives and the living environment. In order to achieve more efficient and effective disaster prevention and mitigation, it is essential to focus on the mechanisms of disaster occurrence and develop countermeasure technologies that directly affect the factors that trigger disasters.
[0006] The trigger for many ground disasters is the behavior of "water." For example, landslides occur when the ground loosens due to prolonged rain, so it is important to prevent water from stagnating in the ground and to constantly drain it. Also, in order to quickly remediate contaminated ground, it is necessary to freely manipulate the heavy metal ions and water present in the ground and accumulate them in a specific location, so controlling the water in the ground is also required in the remediation of contaminated ground. From these examples, it can be said that controlling water in the ground holds the key to innovative disaster prevention and mitigation technologies.
[0007] However, clay soil in particular has poor permeability, and the conventional infiltration dewatering method using head difference or load loading cannot promote rapid drainage. In order to quickly and appropriately drain and collect water in the ground, a permeation dewatering technology that is not dependent on the permeability coefficient of the ground is required.
[0008] This technology is a consolidation and dewatering technology using electro-osmosis, and it is believed that tests using the electro-osmosis consolidation test device of the present invention, as well as on-site electro-osmosis consolidation methods using the test results, will be useful not only for reducing the volume of dredged soil as mentioned above, but also as a disaster prevention and mitigation technology. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] Special Publication No. 2008-515156 Summary of the Invention [Problem to be solved by the invention]
[0010] The present invention has been devised based on the above-mentioned conventional problems and proposals, and aims to provide an electro-osmotic consolidation test device which is an infiltration dewatering technology that does not depend on the permeability coefficient of the ground in order to quickly and appropriately drain and collect water from within the ground, and which not only reduces the volume of dredged soil but also contributes to disaster prevention and mitigation technology, as well as an electro-osmotic consolidation method that can be performed on site using the test results from said test device. [Means for solving the problem]
[0011] The present invention relates to The electro-osmotic consolidation test device is configured to include a pair of electrodes housed in a test container, a test soil housed between the pair of electrodes, a current-carrying member that applies current to the electrodes, and a loading member that is loaded above the electrodes and compresses the test soil, and performs a test to detect the shrinkage state of the soil by applying current and loading, For electrical testing, any one of the following electrodes or a combination of any one of the following electrodes can be used: a normal electrode, in which the entire electrode surface is configured as an electrode surface and the dehydration direction of the test soil stored between a pair of electrodes proceeds in a straight line toward the opposing electrode; an RS electrode, in which the resistance of the test soil stored between the electrodes can be changed so that the potential gradient of the test soil in the center between the electrodes becomes larger by adjusting the initial potential of the test soil stored between the electrodes; or a titration electrode, in which hydrogen ions and hydroxide ions generated at the electrodes are neutralized on the electrode surface, thereby maintaining the pH of the test soil between the electrodes near neutrality; and it can be confirmed which of the above electrodes has the greatest dehydration effect on the test soil and the shortest dehydration time. It is characterized by: or Each of the electrodes has a plurality of holes penetrating from the electrode surface to the electrode back surface. It is characterized by: or The dehydration effect of the test soil can be detected by detecting the contraction state of the test soil due to dehydration within the test soil. It is characterized by: or The test vessel has a vertical hollow portion therein, the pair of electrodes are arranged horizontally within the vertical hollow portion, and the test soil is accommodated between the arranged electrodes; A deformation detection material is provided between the stored test soil and the side wall of the test container to detect the lateral shrinkage of the test soil, and the shrinkage state of the test soil due to dehydration can be detected by the deformation of the deformation detection material. It is characterized by: or The test soil is taken from the target ground at the site, and the test soil is used with an electro-osmotic consolidation test device that can be used to confirm whether any of the following electrodes or a combination of electrodes has a large dehydration effect on the test soil and a short dehydration time: a normal electrode in which the entire electrode surface is configured as an electrode surface and the dehydration direction of the test soil stored between a pair of electrodes proceeds in a straight line toward the opposing electrode; an RS electrode that can change the resistance of the test soil stored between the electrodes by adjusting the initial potential of the test soil stored between the electrodes so that the potential gradient of the test soil in the center between the electrodes becomes large; or a titration electrode that neutralizes hydrogen ions and hydroxide ions generated at the electrodes on the electrode surface and keeps the pH of the test soil between the electrodes near neutral. Select an electrode that has a large dehydration effect and a short dehydration time for the test soil obtained from the test results, and perform electro-osmotic consolidation of the target ground at the site. It is characterized by the above. Effect of the Invention
[0012] According to the present invention, it is possible to provide an infiltration dewatering technology that is not dependent on the permeability coefficient of the ground in order to quickly and appropriately drain and collect water from within the ground, and it is also possible to provide an electro-osmotic consolidation test device that not only reduces the volume of dredged soil but also contributes to disaster prevention and mitigation technology, as well as an electro-osmotic consolidation method that can be performed on site using the test results from said test device, which has the excellent effect of providing such a device. [Brief description of the drawings]
[0013] [Figure 1] FIG. 1 is an explanatory diagram illustrating the configuration of an electroosmotic consolidation testing device according to the present invention. [Diagram 2] FIG. 2 is an explanatory diagram illustrating a schematic configuration of an RS electrode. [Diagram 3] FIG. 2 is an explanatory diagram for explaining a normal flow of potential of an electrode. [Figure 4] FIG. 4 is an explanatory diagram for explaining the flow of potential of an RS electrode. [Diagram 5]FIG. 11 is an explanatory diagram for comparing the amount of dehydration and the dehydration time of a normal electrode and an RS electrode. [Figure 6] FIG. 2 is an explanatory diagram illustrating a schematic configuration of a titration electrode. [Figure 7] FIG. 13 is an explanatory diagram illustrating a hexagonal electrode arrangement. [Figure 8] FIG. 13 is an explanatory diagram illustrating an opposing electrode arrangement. [Figure 9] FIG. 13 is an explanatory diagram for explaining a comparative experiment with other construction methods. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] In order to apply the electro-osmotic consolidation method to the site based on the soil volume reduction test results using the electro-osmotic consolidation test device of the present invention for the purpose of soil volume reduction, various specifications must be determined in the following procedure.
[0015] In other words, the specifications include selecting the optimal electrode material, selecting the optimal application method and applied current value, selecting the optimal electrode spacing, and understanding the mechanical properties of the ground before and after applying the electro-osmotic consolidation method at the site, based on the results of soil volume reduction tests using an electro-osmotic consolidation test device on the target ground (specimen 1) at the site.
[0016] (1) To select the optimal electrode material, application method, and applied current value by conducting a soil volume reduction test using the target ground (specimen 1) using an electro-osmotic consolidation test device.
[0017] In (1), a test device capable of performing an electro-osmotic consolidation test is required. In consideration of the above demand, the present inventors have invented a new electrode and an electro-osmotic consolidation test device using the newly invented electrode.
[0018] Here, a test using an electro-osmotic consolidation tester involves using a specimen 1 made of, for example, saturated clay, with a diameter of 60 mm and a height of 20 mm, restraining its lateral displacement and allowing drainage from above and below to determine the compressibility and consolidation rate used to estimate the amount of settlement and time of settlement of the saturated clay ground. Note that consolidation refers to the phenomenon in which saturated clay increases in density with a time lag when subjected to a static load.
[0019] The electro-osmotic consolidation testing apparatus according to the present invention described above may be of a configuration similar to that of conventional testing apparatus, and may have a diameter of 60 mm for the cylindrical vertical hollow portion of the consolidation vessel 2, as in the conventional apparatus, and may have a mechanism capable of loading a vertical load and measuring the vertical displacement (subsidence).
[0020] Even with the electro-osmotic consolidation test device of the present invention, if the clay specimen 1 is consolidated by applying a load without passing an electric current through it, the conventional soil consolidation test using stepwise loading (JGS-0411-2009) can also be performed. Therefore, by using the electro-osmotic consolidation test device of the present invention, it is possible to compare test results such as consolidation curves obtained by conventional methods with test results obtained with an electric current applied.
[0021] First, the configuration of the electro-osmotic consolidation test device according to the present invention will be described with reference to Fig. 1. In Fig. 1, reference numeral 1 denotes a specimen made of saturated clay. The specimen 1 is placed, for example, in the vertical hollow part of a consolidation vessel 2 that is vertically erected and has a roughly cylindrical shape. However, the internal shape of the vertical hollow part of the consolidation vessel 2 is not limited to a roughly cylindrical shape.
[0022] As can be seen from FIG. 1, electrodes 10 are closely attached to the upper end surface and the other end surface of the specimen 1 placed in the pressure-tight container 2, respectively.
[0023] Reference numeral 3 denotes a DC power supply. The DC power supply 3 is installed outside the pressure-tight vessel 2, and the DC power supply 3 and the electrode 10 are connected by a connection line 12. Furthermore, electricity can be applied from the DC power supply 3 to the electrode 10 via, for example, an electrode rod 4 for current application.
[0024] Reference numeral 5 denotes a loading device composed of a Bellofram cylinder or the like. For example, an inverted T-shaped loading member 6, which is a component of the loading device 5, is placed on the upper surface of the test specimen 1 and is configured to apply a vertical load to the test specimen 1 while allowing the load to vary.
[0025] The process of conducting a consolidation test using the electro-osmotic consolidation test apparatus of the present invention is as follows: a lower electrode 10 is placed in the vertical hollow section of a consolidation vessel 2 which serves as a sample stage, and filter paper 8 is laid on top of the electrode 10 to prevent the clay specimen 1 from flowing out, and then the specimen 1 is placed on top of the filter paper 8.
[0026] At that time, a deformation detection material 7 composed of a membrane or the like is abutted against the inner circumferential surface of the vertical hollow portion of the pressure-tight vessel 2, and the deformation detection material 7 is tightly attached to the inner circumferential surface of the vertical hollow portion of the pressure-tight vessel 2.
[0027] When electricity is passed through the specimen 1 to perform electro-osmosis, the specimen 1 dehydrates and shrinks, so the deformation detection material 7 is attached to the specimen 1 to provide a mechanism for measuring the amount of lateral deformation of the specimen 1. Specifically, a deformation detection material 7 is attached to the inner circumferential surface of the side of the vertical hollow part of the pressure vessel 2, and a certain lateral pressure is applied to measure the volume change (lateral deformation) caused by the shrinkage of the specimen 1. Since the inner circumferential surface of the side of the vertical hollow part of the pressure vessel 2 and the deformation detection material 7 need to be in close contact with each other when the specimen 1 is inserted, holes are made in, for example, two places on the side of the pressure vessel 2 so that a vacuum can be drawn from inside the vertical hollow part of the pressure vessel 2.
[0028] The specimen 1 is placed, for example, up to the 20 mm height line from the upper opening into the storage space formed by the vertical hollow section in the pressure vessel 2. After placement, filter paper 8 is laid on top of the specimen 1 to prevent the specimen 1 from flowing out.
[0029] Next, a mounting plate 9 made of, for example, porous stone or the like, to which an upper electrode 10 is attached, is placed on the upper surface of the specimen 1 on which the filter paper 8 is laid. Next, the storage section of the pressure-tight container 2 is filled with water up to a predetermined position.
[0030] Since gas is generated near the electrode 10 due to electro-osmosis, the electrode 10 and the mounting plate 9 are provided with holes penetrating vertically, for example by punching. The electrode 10 and the mounting plate 9 are configured so that the generated gas and dehydrated water can pass from the upper surface of the electrode 10 through the mounting plate 9 and between the mounting plate 9 and the loading member 6 loaded thereon. Therefore, it is preferable that the contact surface of the loading member 6 that contacts the mounting plate 9 is configured as a tapered surface to create a gap. This allows the generated gas and dehydrated water to pass through smoothly.
[0031] And, for example, above it, a gas-liquid separation device 11 composed of a gas-liquid separator or the like is installed, which is configured to recover, separate and collect the generated gas and the dehydrated water that have passed through.
[0032] Furthermore, in order to apply a vertical load approximately equal to the lateral confinement pressure, the loading device 5 is operated, and the cock that had been drawing a vacuum to create a vacuum in the deformation detection material 7 is closed to apply the lateral confinement pressure.
[0033] As shown in FIG. 1, a vertical displacement meter 14 is installed, and the electrode 10 is connected to the DC power supply 3 using a connection wire 12 made of a lead wire or the like to the electrode rod 4 installed at the upper side of the mounting plate 9 and the electrode rod 4 installed at the lower side of the pressure-tight container 2, which serves as the sample stage.
[0034] The DC power supply 3 is turned on and a predetermined current is applied. After that, the vertical displacement, lateral displacement, vertical load, water pressure, current and voltage values, etc. are measured by a measuring device 13 consisting of, for example, a data logger. Furthermore, the water drained from the gas-liquid separator 11 is sampled on an electronic balance and the amount of drainage is measured.
[0035] According to the above-mentioned procedure, a consolidation test of the target ground is carried out using the electro-osmotic consolidation test device of the present invention, and the dewatering effect due to electro-osmotic consolidation, which is the test result, i.e., the volume reduction state of the target ground, is understood and examined.
[0036] In other words, taking into consideration data such as the optimal dewatering effect from the test results, which electrode resulted in a volume reduction state of the target ground, and what the appropriate applied current value and current flow conditions (constant current or constant voltage) are, the appropriate electrode, appropriate applied current value, and current flow conditions (constant current or constant voltage) for applying the electro-osmotic consolidation method at the site are determined.
[0037] By the way, in the consolidation test by step loading of soil using conventional testing equipment, the loading steps are 10, 20, 40, 80, 160, 320, 640, 1280kN / m 2 The consolidation test was conducted in eight stages, and since each stage required 24 hours for loading, the consolidation test took a long time.
[0038] However, in the electro-osmotic consolidation test carried out using the electro-osmotic consolidation test apparatus of the present invention, the test yielded a compression rate of 80 kN / m in about 3 to 5 hours. 2 It can be seen that the moisture content decreases to the moisture content obtained at the loading stage of 80 kN / m. 2 The time to the loading stage took approximately 94 hours.
[0039] For this reason, by using the electro-osmotic consolidation testing device of the present invention to electrically force drainage and reduce the volume, it is possible to obtain the effect of dramatically shortening the consolidation time.
[0040] (2) Selection and setting of the optimal electrodes 10 and electrode 10 intervals in tests using the electro-osmotic consolidation test device of the present invention
[0041] When conducting an electroosmotic consolidation test using the electroosmotic consolidation test apparatus of the present invention, taking into consideration the area and volume of the ground to which the electroosmotic consolidation method will be applied at the actual site, selecting appropriate electrodes 10 and selecting and setting appropriate spacing between electrodes 10 are important settings for subsequently applying the electroosmotic consolidation method at the actual site based on the test results.
[0042] Conventionally, a normal electrode has been used as the electrode 10 used in consolidation tests using an electro-osmotic consolidation tester or in on-site electro-osmotic consolidation methods. Here, a normal electrode refers to an electrode 10 in which a cathode potential (or an anode potential) is arranged on the entire cathode (or the entire anode). However, the inventors of this invention have newly invented a rail splitter electrode (hereinafter referred to as RS electrode) and a titration electrode that are different from ordinary electrodes.
[0043] (RS electrode) As described above, the conventional electrode 10 is an electrode 10 in which a cathode potential (or an anode potential) is disposed over the entire cathode (or anode) surface. In contrast, the RS electrode 15 refers to a cathode (or an anode) configured by arranging electrode blocks having a cathode potential (or an anode potential) and electrode blocks of an arbitrary potential in an alternating striped pattern (see FIG. 2).
[0044] That is, to further explain the structure of the RS electrode 15, the RS electrode 15 has electrode blocks divided into individual blocks at arbitrary intervals in the vertical direction, for example, and each divided electrode block is connected in an insulated state.
[0045] In this case, the electrode blocks are arranged vertically at an arbitrary interval, alternately with the electrode blocks of cathode potential (or anode potential) and those of an arbitrary potential smaller than the cathode potential (or anode potential), as described above, and the two types of potential are applied alternately to each electrode block.
[0046] Here, the RS electrode can be said to be an electrode that can adjust the initial potential near the RS electrode to a specified gradient. The resulting potential gradient causes dehydration, and the soil resistance increases from the dehydrated area. In other words, the resistance of the soil is proportional to the hardness of the soil, and the more it dehydrates, the harder the soil becomes and the greater the resistance becomes.
[0047] The potential distribution in the test soil also changes depending on the soil's resistance. In other words, a large potential is applied to areas with high resistance. Therefore, by using RS electrodes, a large potential gradient acts near the electrodes in the early stages of current flow, causing dehydration near the electrodes and increasing the resistance of the soil near the electrodes.
[0048] On the other hand, the center of the electrodes is the farthest from the positive and negative electrodes, so dehydration proceeds slowly and the soil resistance is low in this region.
[0049] When the resistance is large, it becomes easier to apply a potential, so the potential is high near the electrodes and low in the center between the electrodes, resulting in a large potential gradient between the electrodes. This potential gradient causes dehydration in the center between the electrodes. Eventually, the entire test soil is dehydrated uniformly.
[0050] With the above-described configuration, dehydration from one electrode toward the opposing other electrode does not proceed as with a normal electrode 10, but rather proceeds at a predetermined incline.
[0051] Furthermore, since the potentials of the electrode blocks are alternately different, dehydration is performed alternately between each electrode block due to the difference between the cathode potential (or anode potential) and an arbitrary potential smaller than that.
[0052] Therefore, if the difference between the cathode potential (or anode potential) and any other potential smaller than that can be adjusted, the resistance change of the test soil can be adjusted in any way by promoting dehydration near the electrodes. As a result, the direction of dehydration can be adjusted by adjusting the resistance change of the test soil.
[0053] However, in the present invention, by using the RS electrode 15, both electroosmotic dehydration caused by the potential gradient between the anode and cathode and electroosmotic dehydration caused by the potential gradient generated between each electrode block in the vertical direction on the surface of the RS electrode occur simultaneously, thereby not only increasing the dehydration speed of the specimen 1 but also expanding the dehydration range.
[0054] Conventionally, in the electro-osmotic consolidation method, it is common to use an electrode in which a cathode potential (anode potential) is arranged over the entire cathode (or entire anode) surface. However, by using the above-mentioned RS electrode 15 or the titration electrode described below, the dehydration range, dehydration speed, and final dehydration amount of the test specimen 1 are significantly increased.
[0055] In fact, when comparing the dehydration process, i.e., the volume reduction process, of the normal electrode 10 and the RS electrode 15, as shown in Figure 3, with the normal electrode 10, voltage is easily applied to clay that has already been dehydrated, and it is difficult to apply voltage to undehydrated parts. Therefore, there is a tendency for the area near the cathode to not be sufficiently dehydrated.
[0056] On the other hand, with the RS electrode 15, as shown in Figure 4, it became possible to apply voltage even to undehydrated parts of the clay by controlling the potential gradient of the electrode, resulting in overall dehydration. Comparing the final amount of dehydration, the RS electrode 15 showed a greater amount of dehydration than the normal electrode 10 (Figure 5).
[0057] In this test, considering that the use of the RS electrode 15 widens the dehydration range, in other words the water collection range, it is considered that the wider the electrode spacing, the greater the effect on the dehydration speed. Therefore, it can be inferred that the use of the RS electrode 15 will significantly increase the dehydration speed.
[0058] (titration electrode) When the target ground at an actual site is marine clay, the pore water is seawater, so the resistance of the clay is low and the voltage applied to the clay is small initially when the current is applied; therefore, it is necessary to increase the applied current value under constant current conditions in order to promote rapid drainage.
[0059] However, when a large current is applied, a large amount of OH- is generated on the cathode side and a large amount of H + This may result in the formation of an oxide layer inside the specimen 1, which may hinder electro-osmosis, or the pH of the specimen 1 may change, making it difficult for electro-osmosis to occur.
[0060] In such a situation, it is recommended to use a titration electrode. A titration electrode is an electrode that neutralizes the hydrogen ions and hydroxide ions generated at the electrode on the electrode surface, keeping the pH of the clay close to neutral (Figure 6). The chemical equations for the generation of hydroxide ions and hydrogen ions are as follows:
[0061] Hydroxide ion generation (cathode) O2+H2O+4e - →4OH - , 2H2O+4e - →4OH - +H2 Generation of hydrogen ions (anode) Al 3+ +3H2O→Al(OH)3+3H + +3e - , 2H2O→O2+4H + +4e -
[0062] Here, since the coefficients of electrons and hydroxide ions are the same for both reactions, the amount of electrons consumed and the mass of hydroxide ions produced are the same regardless of which reaction is occurring.
[0063] In addition, since the amount of electrons consumed is proportional to the applied current, it is possible to calculate the mass of hydroxide ions produced by measuring the applied current. An acid solution sufficient to neutralize the calculated mass of hydroxide ions produced is pumped and injected into the electrode. The pump is controlled by the external input terminal of the pump, with the voltage obtained from the current measuring unit being adjusted by the voltage adjusting unit.
[0064] In this way, by using optimal electrodes and setting optimal electrode spacing for the target ground to which the electro-osmotic consolidation method is to be applied in an actual field, it is possible to rapidly consolidate and dewater clayey ground, which was not possible with conventional electro-osmotic consolidation methods.
[0065] Regarding titration electrodes, there are two types: titration electrodes that have a titration function added to a normal electrode, and RS titration electrodes that have a titration function added to an RS electrode.
[0066] (Selection of electrodes and setting of electrode spacing) From the test results using the electroosmotic consolidation test apparatus according to the present invention, if the voltage applied to the test specimen 1 at the beginning of the energization is about 10 V, and if there is almost no change in voltage even after one hour of energization, the electrode 10 used in the electroosmotic consolidation method performed on site will not be a normal electrode but an RS electrode 15, or a titration electrode with a titration function added to the normal electrode 10, or an RS titration electrode with a titration function added to the RS electrode 15.
[0067] In addition, in the electro-osmotic consolidation method performed on-site, if the depth of the ground to be consolidated is at most 1m and the distance between the electrodes is less than 1m, there is almost no difference in the amount and speed of dewatering between RS electrodes and normal electrodes. In such cases, normal electrodes are used. This is because the electrical circuit when using normal electrodes is simpler than when using RS electrodes and is therefore easier to handle.
[0068] Next, the electrode spacing is set using the test results of the electro-osmotic consolidation test device as follows. (1) An electro-osmotic consolidation test is carried out using the test device according to the present invention, and the characteristics of the ground material of the test specimen 1 with respect to electro-osmotic consolidation dehydration are understood. For example, it is possible to understand whether the ground material is one that dehydrates quickly or not. (2) Based on the results of measuring the time and power required for dewatering in an electro-osmotic consolidation test using the test device of the present invention, it will be determined whether the electrode spacing can be set to 1 to 2 m, which is the conventional drain installation spacing. (3) Based on the soil material properties investigated in (1), the electrode materials to be used (conventional electrode, RS electrode, titration electrode) are selected. (4) The power required for the area (volume) of the ground area at the site where construction work is to be carried out is estimated based on the current and voltage values measured in the electro-osmotic consolidation test using the test equipment of the present invention, and the specific electrode spacing is set.
[0069] Like the drain installation interval in the conventional vacuum consolidation method, the electrode spacing in the electro-osmotic consolidation method varies depending on the characteristics of the ground material. If the ground material has a high electro-osmotic dewatering effect, the electrode spacing can be set to, for example, 2 m. If the electro-osmotic dewatering effect is small, it is possible to use RS electrodes 15 or other devices to install the electrodes at short intervals of, for example, 1 to 2 m.
[0070] Incidentally, even for ground materials with a high electro-osmotic dewatering effect, if there is a possibility that the electrode interval can be set to, for example, 2 m or more by using the RS electrodes 15, it is also possible to set the electrode interval to be wider.
[0071] (Applicability of electro-osmotic consolidation method using 3D model soil tank) In addition to conducting tests using the electro-osmotic consolidation test apparatus of the present invention, the inventors also constructed a so-called three-dimensional model soil tank and used it to examine the applicability of the electro-osmotic consolidation method.
[0072] In this case, tests were conducted for a case in which six anodes were placed around a central cathode (see Fig. 7) and a case in which three anodes were placed around the periphery, as shown in the figure.
[0073] At this time, in order to make the anode surface area the same in both cases, the diameter of the anode in the case with three anodes was twice that of the case with six anodes.The test results showed that there was almost no difference in the amount of water removed and the dewatering time in both cases.From this, it was confirmed that, during on-site construction, rather than arranging the electrodes in a hexagonal arrangement as in Figure 7, if the electrodes are arranged facing each other in a square as in Figure 8 and the anode surface area is made roughly the same, a sufficient electro-osmotic consolidation dewatering effect can be obtained.
[0074] Therefore, in an actual field test, by arranging electrodes facing each other in a square shape as shown in Figure 8, it was possible to dehydrate the entire external area, which is roughly rectangular, including the corners. It was confirmed that electro-osmosis dehydration is possible in every corner even when the area to be consolidated and dehydrated is a wide rectangular area.
[0075] As a result, it was confirmed that dehydration was progressing not only between the anode and cathode, but also in the clay between the anode and the wall, and that the clay ground, whose initial moisture content was 100%, eventually dropped to an average moisture content of as low as 47%.
[0076] In other words, it was confirmed that extremely efficient consolidation and dewatering of the ground is possible by arranging the electrodes face-to-face as shown in Figure 8 and applying the electro-osmotic consolidation method in three dimensions to a rectangular, three-dimensional area.
[0077] What this means is that when applying the electro-osmotic consolidation method of the present invention on-site, the number of electrodes installed can be reduced by adjusting the surface area of the electrodes, and further, as described above, by arranging the electrodes face-to-face as shown in Figure 8, the construction efficiency of a three-dimensional rectangular construction area can be greatly improved. In addition, in Figs. 7 and 8, the square electrodes represent cathodes, and the circular electrodes represent anodes.
[0078] (Understanding the geomechanical properties before and after electro-osmotic consolidation) The necessity of understanding the mechanical properties of the ground after application of the electro-osmotic consolidation method will be explained. In order to understand the mechanical properties of the ground, it is necessary to carry out mechanical tests such as uniaxial tests and triaxial tests on the electro-osmotically consolidated specimen 1. In this regard, by using a consolidation vessel 2 that is larger than the consolidation vessel 2 of the electro-osmotic consolidation test apparatus of the present invention described above, it becomes possible to prepare a specimen for mechanical testing from the electro-osmotically consolidated specimen 1.
[0079] In addition, conventional consolidation and dewatering methods for clay ground include consolidation by embankment loading and vacuum consolidation, and comparative tests with other methods are also necessary. The electro-osmotic consolidation test device of the present invention described above is capable of loading a vertical load, so that consolidation tests by loading can also be performed.
[0080] In addition, because the system is capable of draining water from both sides, a vacuum consolidation test can be performed by connecting a vacuum pump to the drainage path. Because the consolidation test by load, the vacuum consolidation test, and the electro-osmosis consolidation test can be performed under the same conditions with the electro-osmosis consolidation test device of the present invention, it is also possible to compare the dewatering effect with other construction methods (Figure 9).
[0081] (Feasibility) The currently mainstream consolidation methods using embankment loading and vacuum consolidation are dewatering methods that depend on the permeability coefficient of the soil, and as mentioned above, have issues such as the long dewatering time required because the permeability coefficient of clay is very low.
[0082] The present invention dramatically increases the dewatering speed when electrochemically forcibly dewatering pore water in clay ground, and is extremely advantageous in that it is a dewatering method that does not depend on permeability, thereby solving the problems of the conventional method.
[0083] In addition, the installation costs of the electro-osmosis consolidation method are not significantly different from those of consolidation by filling soil or vacuum consolidation, making it highly feasible to implement. Furthermore, as the electro-osmosis consolidation method becomes more widespread in the future, it will be possible to set the optimal applied current value, electrode material, current application time, etc. based on the properties of the ground material.
[0084] In addition, in order to obtain the ground parameters required for conducting numerical analysis of ground deformation during and after ground improvement by electro-osmotic consolidation, the electro-osmotic consolidation testing device of the present invention has the advantage that consolidation tests and mechanical tests after consolidation can be carried out quickly and easily. [Explanation of symbols]
[0085] 1 Specimen 2. Pressure vessel 3 DC power supply 4 electrode rod 5 Loading device 6 Loading member 7 Deformation detection material 8. Filter Paper 9 Mounting plate 10 electrodes 11 Gas-liquid separator 12 Connecting wire 13. Measurement Equipment 14 Vertical displacement gauge 15 RS electrode
Claims
1. The electro-osmotic consolidation test device is configured to include a pair of electrodes housed in a test container, a test soil housed between the pair of electrodes, a current-carrying member that applies current to the electrodes, and a loading member that is loaded above the electrodes and compresses the test soil, and performs a test to detect the shrinkage state of the soil by applying current and loading, For electrical testing, any one of the following electrodes or a combination of any one of the following electrodes can be used: a normal electrode, in which the entire electrode surface is configured as an electrode surface and the dehydration direction of the test soil stored between a pair of electrodes progresses toward the opposing electrode; an RS electrode, in which the resistance of the test soil stored between the electrodes can be changed so that the potential gradient of the test soil in the center between the electrodes becomes larger by adjusting the initial potential of the test soil stored between the electrodes; or a titration electrode, in which hydrogen ions and hydroxide ions generated at the electrode are neutralized on the electrode surface, thereby maintaining the pH of the test soil between the electrodes near neutrality; and it can be confirmed which of the above electrodes has the greatest dehydration effect on the test soil and the shortest dehydration time. This is an electro-osmotic consolidation test device characterized by the above.
2. Each of the electrodes has a plurality of holes penetrating from the electrode surface to the electrode back surface.
2. The electro-osmotic consolidation testing device according to claim 1.
3. The dehydration effect of the test soil can be detected by detecting the contraction state of the test soil due to dehydration within the test soil.
2. The electro-osmotic consolidation testing device according to claim 1.
4. The test vessel has a vertical hollow portion therein, the pair of electrodes are arranged horizontally within the vertical hollow portion, and the test soil is accommodated between the arranged electrodes; A deformation detection material is provided between the stored test soil and the side wall of the test container to detect the lateral shrinkage of the test soil, and the shrinkage state of the test soil due to dehydration can be detected by the deformation of the deformation detection material.
2. The electro-osmotic consolidation testing device according to claim 1.
5. The test soil is taken from the target ground at the site, and the test soil is used with an electro-osmotic consolidation test device that can be used to confirm whether any of the following electrodes or a combination of electrodes has a large dehydration effect on the test soil and a short dehydration time: a normal electrode in which the entire electrode surface is configured as an electrode surface and the dehydration direction of the test soil stored between a pair of electrodes progresses toward the opposing electrode; an RS electrode that can change the resistance of the test soil stored between the electrodes by adjusting the initial potential of the test soil stored between the electrodes so that the potential gradient of the test soil in the center between the electrodes becomes large; or a titration electrode that neutralizes hydrogen ions and hydroxide ions generated at the electrodes on the electrode surface and keeps the pH of the test soil between the electrodes near neutral. Select an electrode that has a large dehydration effect and a short dehydration time for the test soil obtained from the test results, and perform electro-osmotic consolidation of the target ground at the site. An electro-osmotic consolidation method for on-site target ground, characterized by: