Coil component

The coil component design improves terminal electrode adhesion by incorporating bump electrodes that penetrate into the element body, enhancing contact area and using resin electrodes for better bonding, resulting in reliable electrical connections.

JP2024143656APending Publication Date: 2024-10-11TDK CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023056434
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing coil components face challenges in improving the adhesion of terminal electrodes, which are crucial for reliable electrical connections.

Method used

The coil component design includes a pair of bump electrodes that extend into the element body, with terminal electrodes penetrating and contacting the element body, enhancing adhesion by increasing the contact area and using resin electrodes for improved bonding.

Benefits of technology

The enhanced adhesion of terminal electrodes results in improved electrical connections and reliability, ensuring stable performance of the coil component.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143656000001_ABST
    Figure 2024143656000001_ABST
Patent Text Reader

Abstract

To provide a coil component with improved adhesion to a terminal electrode.SOLUTION: In a coil component 1, a terminal electrode 70 enters an opening 13 of an element body 10 and is joined to a bump electrode 60 within the element body 10. That is, the terminal electrode 70 contacts the terminal electrode 70 and also contacts the element body 10. Therefore, the contact area of the terminal electrode 70 is larger than when the bump electrode is exposed on the underside 10b of the element body 10, achieving high adhesion of the terminal electrode 70.SELECTED DRAWING: Figure 8
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a coil component. [Background technology]

[0002] In recent years, in order to accommodate high-density mounting, development has been underway of bottom terminal type coil components in which terminal electrodes are provided only on the bottom surface of an element body in which a coil conductor is provided. The following Patent Document 1 discloses a bottom terminal type coil component that includes a pair of bump electrodes extending from both ends of a coil conductor and exposed from the bottom surface of the element body, and in which the pair of bump electrodes are respectively connected to a pair of terminal electrodes provided on the bottom surface of the element body. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2020-155510 A Summary of the Invention [Problem to be solved by the invention]

[0004] The inventors have conducted extensive research into the adhesion of terminal electrodes of coil components, and as a result have discovered a new technique for improving the adhesion.

[0005] An object of the present invention is to provide a coil component in which the adhesion of terminal electrodes is improved. [Means for solving the problem]

[0006] A coil component according to one aspect of the present invention comprises a base body having an underside facing a mounting board, a coil conductor disposed within the base body, a pair of bump electrodes connected to both ends of the coil conductor and extending from both ends of the coil conductor toward the underside of the base body in a direction intersecting the underside, and a pair of terminal electrodes provided on the underside of the base body, portions of which extend into the base body and are respectively joined to the pair of bump electrodes within the base body.

[0007] In the coil component, the portion of the terminal electrode that is inserted into the element body is joined to the bump electrode and is in contact with the element body, thereby improving adhesion.

[0008] In a coil component according to another aspect, the terminal electrodes are made of resin electrodes.

[0009] In a coil component according to another aspect, the bonding surface of the bump electrode that is bonded to the terminal electrode is flat.

[0010] In a coil component according to another aspect, the thickness of the portion of the terminal electrode that is embedded in the body is greater than the thickness of the remaining portion.

[0011] In a coil component according to another aspect, at least a portion of the bump electrode gradually widens toward the lower surface of the element body. Effect of the Invention

[0012] According to the present invention, a coil component is provided in which the adhesion of terminal electrodes is improved. [Brief description of the drawings]

[0013] [Figure 1] FIG. 1 is a schematic perspective view showing a coil component according to an embodiment. [Diagram 2] 2 is a cross-sectional view taken along line II-II of the coil component shown in FIG. 1. [Diagram 3] 2 is a plan view showing a substrate of the coil device shown in FIG. 1. [Figure 4] 4 is a cross-sectional view taken along line IV-IV of the coil component shown in FIG. [Diagram 5] 2 is a cross-sectional view taken along line VV of the coil component shown in FIG. 1. [Figure 6] 6 is a cross-sectional view taken along line VI-VI of the coil component shown in FIG. [Figure 7] 7 is a cross-sectional view taken along line VII-VII of the coil component shown in FIG. [Figure 8]8 is an enlarged view of a cross section of a main portion of the coil component shown in FIG. 7. [Figure 9] FIG. 4 is a diagram showing the positional relationship of bump electrodes. [Figure 10] 2A to 2C are diagrams illustrating steps of a method for manufacturing the coil component illustrated in FIG. 1. [Figure 11] 2A to 2C are diagrams illustrating steps of a method for manufacturing the coil component illustrated in FIG. 1. [Figure 12] 2A to 2C are diagrams illustrating steps of a method for manufacturing the coil component illustrated in FIG. 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] Various embodiments and examples will be described below with reference to the drawings. Note that the same or corresponding parts in each drawing are denoted by the same reference numerals, and duplicated explanations will be omitted.

[0015] In this embodiment, a coil component 1, which is a type of electronic component, will be described. As shown in Fig. 1, the coil component 1 according to the embodiment has a rectangular parallelepiped outer shape. As one example, the coil component 1 may be designed with dimensions of a long side of 1.2 mm, a short side of 1.0 mm, and a height of 0.5 mm. Alternatively, as another example, the coil component 1 may be designed with dimensions of a long side of 2.0 mm, a short side of 1.2 mm, and a height of 0.6 mm.

[0016] The coil component 1 is configured to include an element body 10 and a coil portion 20 embedded in the element body 10 .

[0017] The element body 10 has a rectangular parallelepiped outer shape and has six faces 10a to 10f. Of the faces 10a to 10f of the element body 10, the top face 10a and the bottom face 10b are parallel to each other, the end faces 10c and 10d are parallel to each other, and the side faces 10e and 10f are parallel to each other. The bottom face 10b of the element body 10 is a face that faces in parallel to the mounting surface of the mounting board on which the coil component 1 is mounted, and is a flat surface that is substantially free of irregularities.

[0018] The element body 10 is made of a magnetic material. In this embodiment, the element body 10 is made of a resin containing a metal magnetic powder, which is a type of magnetic material. The resin containing a metal magnetic powder is a binding powder in which a metal magnetic powder is bound by a binder resin. The metal magnetic powder may be made of, for example, an iron-nickel alloy (permalloy alloy), carbonyl iron, an amorphous, non-crystalline or crystalline FeSiCr-based alloy, sendust, or the like. The binder resin is, for example, a thermosetting epoxy resin. In this embodiment, the content of the metal magnetic powder in the binding powder is 80 to 92 vol% in volume percent and 95 to 99 wt% in mass percent. From the viewpoint of magnetic properties, the content of the metal magnetic powder in the binding powder may be 85 to 92 vol% in volume percent and 97 to 99 wt% in mass percent.

[0019] The coil section 20 is configured to include a first coil body 30, a substrate 40, and a second coil body 50. Specifically, the first coil body 30 is provided on an upper surface 40a of the substrate 40 located on the upper surface side of the element body 10, and the second coil body 50 is provided on a lower surface 40b of the substrate 40 located on the lower surface side of the element body 10. In this embodiment, the pattern shape of the first coil body 30 viewed from the upper surface 40a side of the substrate 40 is the same as the pattern shape of the second coil body 50 viewed from the lower surface 40b side of the substrate 40.

[0020] The substrate 40 is a plate-like member extending parallel to the upper surface 10a and the lower surface 10b of the element body 10. The substrate 40 is disposed so that the distance between the substrate 40 and the lower surface 10b of the element body 10 is equal to the distance between the substrate 40 and the upper surface 10a of the element body 10. As shown in FIG. 3, the substrate 40 has an elliptical ring-shaped coil forming portion 41 extending along the long side direction of the element body 10, a pair of protrusions 46A, 46B extending from the coil forming portion 41 to the side surfaces 10e, 10f of the element body 10, respectively, and a pair of frame portions 47A, 47B extending along the short side direction of the element body 10 and sandwiching the coil forming portion 41 from both sides. The substrate 40 has approximately triangular through holes 43, 44 in each of the areas defined by the outer periphery of the coil forming portion 41 and the pair of frame portions 47A, 47B. Furthermore, the coil forming portion 41 is provided with a circular through hole 45 at the edge of the oval opening .

[0021] The substrate 40 may be a glass cloth impregnated with cyanate resin (BT (bismaleimide-triazine) resin: registered trademark) having a thickness of 60 μm. In addition to BT resin, polyimide, aramid, etc. may also be used. The substrate 40 may also be made of ceramic or glass. The substrate 40 is preferably made of a mass-produced printed circuit board material, and most preferably made of a resin material used for BT printed circuit boards, FR4 printed circuit boards, or FR5 printed circuit boards.

[0022] The first coil body 30 is provided on the substrate upper surface 40a in the coil forming portion 41. As shown in Fig. 2, the first coil body 30 includes a first planar coil 32 constituting a part of the coil 22 (coil conductor) of the coil component 1, a first insulator 34, and a first island electrode 36.

[0023] The first planar coil 32 is a substantially oval spiral air-core coil wound around the opening 42 of the coil forming portion 41 in the same layer on the upper surface 40a of the substrate 40. The number of turns of the first planar coil 32 may be one or more. In this embodiment, the number of turns of the first planar coil 32 is 3 to 4. The first planar coil 32 has an outer end 32a, an inner end 32b, and a first turn portion 32c connecting the outer end 32a and the inner end 32b. The outer end 32a is provided in a region covering the through hole 43 of the substrate 40 when viewed from the thickness direction of the substrate 40, and has a substantially triangular shape. More specifically, the outer end 32a has a triangular shape with rounded corners. More specifically, the side surface on the inner peripheral side of the outer end 32a faces the first turn portion 32c and is curved in an arc shape so as to follow the outer peripheral surface of the first turn portion 32c. When viewed in the thickness direction of substrate 40, inner end 32b is provided in a region covering through hole 45 of substrate 40 and has a circular shape. First planar coil 32 is made of, for example, Cu, and may be formed by electrolytic plating.

[0024] The first island electrode 36 is provided in a region overlapping with the through hole 44 of the substrate 40 when viewed from the thickness direction of the substrate 40, and has a substantially triangular shape. More specifically, the first island electrode 36 has a triangular shape with rounded corners. More specifically, the inner peripheral side surface of the first island electrode 36 faces the first turn portion 32c, and is curved in an arc shape so as to follow the outer peripheral surface of the first turn portion 32c. The first island electrode 36 is not in contact with the first planar coil 32 on the upper surface 40a of the substrate 40. The first island electrode 36 is a dummy electrode that is not necessary for forming the circuit of the coil portion 20. The first island electrode 36 is made of, for example, Cu, and can be formed by electrolytic plating.

[0025] The first insulator 34 is provided on the upper surface 40a of the substrate 40, and is a thick-film resist patterned by known photolithography. The first insulator 34 defines the growth regions of the first planar coil 32 and the first island-shaped electrode 36, and covers the first planar coil 32 in the same layer in which the first planar coil 32 is formed. In this embodiment, the first insulator 34 includes an outer wall 34a and an inner wall 34b that define the contour of the first planar coil 32, a partition wall 34c that separates the inner turn and the outer turn of the first turn portion 32c of the first planar coil 32, and an outer wall 34d that defines the contour of the first island-shaped electrode 36. The first insulator 34 is made of, for example, epoxy resin.

[0026] 5, the first coil body 30 further includes a protective film 38 that integrally covers the first planar coil 32 and the first insulator 34 from the top surface 10a side of the element body 10. The protective film 38 is made of, for example, epoxy resin. The protective film 38 improves the insulation between the metal magnetic powder contained in the element body 10 and the first planar coil 32.

[0027] The second coil body 50 is provided on the substrate lower surface 40b in the coil forming portion 41. As shown in Fig. 4, the second coil body 50 includes a second planar coil 52 constituting a part of the coil 22 of the coil device 1, a second insulator 54, and a second island-shaped electrode 56.

[0028] The second planar coil 52 is a substantially oval spiral air-core coil wound around the opening 42 of the coil forming portion 41 in the same layer on the lower surface 40b of the substrate 40. The number of turns of the second planar coil 52 may be one or more. In this embodiment, the number of turns of the second planar coil 52 is 3 to 4. The second planar coil 52 has an outer end 52a, an inner end 52b, and a second turn portion 52c connecting the outer end 52a and the inner end 52b. The outer end 52a is provided in a region covering the through hole 44 of the substrate 40 when viewed from the thickness direction of the substrate 40, and has a substantially triangular shape similar to the outer end 32a of the first planar coil 32. That is, the outer end 52a has a triangular shape with rounded corners, and the side surface on the inner circumferential side facing the second turn portion 52c is curved in an arc shape so as to follow the outer circumferential surface of the second turn portion 52c. Inner end 52b is provided in a region covering through hole 45 of substrate 40 when viewed in the thickness direction of substrate 40, and has a circular shape. Second planar coil 52 is made of, for example, Cu, and can be formed by electrolytic plating.

[0029] The second island electrode 56 is provided in an area overlapping the through hole 43 of the substrate 40 when viewed from the thickness direction of the substrate 40, and has a substantially triangular shape similar to that of the first island electrode 36. That is, the second island electrode 56 has a triangular shape with rounded corners, and the inner peripheral side surface of the second island electrode 56 facing the second turn portion 52c is curved in an arc shape so as to follow the outer peripheral surface of the second turn portion 52c. The second island electrode 56 is not in contact with the second planar coil 52 on the lower surface 40b of the substrate 40. The second island electrode 56 is made of, for example, Cu, and can be formed by electrolytic plating.

[0030] The second insulator 54 is provided on the lower surface 40b of the substrate 40, and is a thick-film resist patterned by known photolithography. The second insulator 54 defines the growth regions of the second planar coil 52 and the second island-shaped electrode 56, and covers the second planar coil 52 in the same layer in which the second planar coil 52 is formed. In this embodiment, the second insulator 54 includes an outer wall 54a and an inner wall 54b that define the contour of the second planar coil 52, a partition wall 54c that separates the inner turn and the outer turn of the second turn portion 52c of the second planar coil 52, and an outer wall 54d that defines the contour of the second island-shaped electrode 56. The second insulator 54 is made of, for example, epoxy resin.

[0031] 5, the second coil body 50 further includes a protective film 58 that integrally covers the second planar coil 52 and the second insulator 54 from the lower surface 10b side of the element body 10. The protective film 58 is made of, for example, epoxy resin. The protective film 58 improves the insulation between the metal magnetic powder contained in the element body 10 and the second planar coil 52.

[0032] A conductor 53 connected to the second island electrode 56 is provided on the lower surface 40b of the substrate 40. The conductor 53 functions as a power supply line when the coil 22 is formed by electrolytic plating, as described below. The conductor 53 is provided so as to straddle the coil forming portion 41 and the frame portion 47B. As shown in FIG. 1, the conductor 53 is exposed from the end surface 10c of the element body 10. The conductor 53 is electrically connected to the first planar coil 32 and the second planar coil 52 via the second island electrode 56.

[0033] As shown in Fig. 6, the through holes 45 of the substrate 40 are filled with via conductors 48. The first planar coil 32 provided on the upper surface 40a of the substrate 40 and the second planar coil 52 provided on the lower surface 40b of the substrate 40 are connected at their inner ends 32b, 52b through the via conductors 48 in the through holes 45 passing through the substrate 40 in the thickness direction. In this embodiment, the first planar coil 32, the second planar coil 52, and the via conductors 48 form an air-core coil 22 around the opening 42 of the substrate 40. The coil 22 has a coil axis parallel to the thickness direction of the substrate 40 (i.e., the opposing direction of the upper surface 10a and the lower surface 10b).

[0034] The first planar coil 32 and the second planar coil 52 are wound so that current flows in the same direction (i.e., the same winding direction when viewed from the thickness direction of the substrate 40) when a voltage is applied between both ends of the coil 22 (i.e., the outer end 32a of the first planar coil 32 and the outer end 52a of the second planar coil 52). In this embodiment, the first planar coil 32 has a clockwise winding direction from the outer end 32a to the inner end 32b as shown in FIG. 2, and the second planar coil 52 has a clockwise winding direction from the inner end 52b to the outer end 52a as shown in FIG. 4. Since current flows in the same direction in the first planar coil 32 and the second planar coil 52, the generated magnetic fluxes overlap and reinforce each other.

[0035] 7, the through holes 43 and 44 of the substrate 40 are filled with via conductors 49. The first island electrode 36 provided on the upper surface 40a of the substrate 40 and the outer end 52a of the second planar coil 52 provided on the lower surface 40b of the substrate 40 are connected through the via conductor 49 in the through hole 43 that passes through the substrate 40 in the thickness direction. Similarly, the outer end 32a of the first planar coil 32 provided on the upper surface 40a of the substrate 40 and the second island electrode 56 provided on the lower surface 40b of the substrate 40 are connected through the via conductor 49 in the through hole 44 that passes through the substrate 40 in the thickness direction.

[0036] In addition to the coil portion 20, a pair of bump electrodes 60 are embedded in the element body 10. The pair of bump electrodes 60 extend along the thickness direction of the substrate 40 so that both ends of the coil 22 are directed toward the lower surface 10b of the element body 10. One bump electrode 60A has an upper end 60a connected to one end 32a of the coil 22 via a second island electrode 56, and a lower end 60b extending to the vicinity of the lower surface 10b of the element body 10 but not reaching the lower surface 10b. The other bump electrode 60B has an upper end 60a connected to the other end 52a of the coil 22, and a lower end 60b extending to the vicinity of the lower surface 10b of the element body 10 but not reaching the lower surface 10b. Each bump electrode 60A, 60B can be made of a conductive material such as a metal or an alloy, and is, for example, a Cu-plated electrode.

[0037] In this embodiment, as shown in Fig. 8, at least one of the pair of bump electrodes 60 may have at least a portion that gradually widens toward the lower surface 10b of the element body 10. Specifically, the bump electrode 60 may have a cross-sectional area that gradually widens toward the lower surface 10b in a cross section parallel to the lower surface 10b of the element body 10. In the cross section shown in Fig. 8, the width W of the bump electrode 60A gradually widens over the entire length in the up-down direction.

[0038] The lower ends 60b of the pair of bump electrodes 60 do not reach the lower surface 10b of the element body 10, but remain inside the element body 10. The lower surface 61 of the lower ends 60b of the bump electrode 60 may be a flat surface, or may be a surface parallel to the lower surface 10b of the element body 10. There is no element body material between the lower surface 61 of the pair of bump electrodes 60 and the lower surface 10b of the element body 10, and an opening 13 extending upward from the lower surface 10b toward the lower ends 60b of the bump electrodes 60 is provided.

[0039] As shown in FIG. 9, each of the pair of bump electrodes 60 is located at a corner of a rectangular region 24 including the first coil body 30 and the second coil body 50, as viewed from the thickness direction of the substrate 40. The dashed line in FIG. 9 is a virtual line indicating the rectangular region 24. In this embodiment, the rectangular region 24 is circumscribed by the first coil body 30 and the second coil body 50, as viewed from the thickness direction of the substrate 40. Each bump electrode 60 has a substantially triangular cross-sectional shape in a plane perpendicular to the thickness direction of the substrate 40. More specifically, the cross-sectional shape of each bump electrode 60 is a triangle along the outer periphery of the first coil body 30 or the second coil body 50 and two sides that define the corners of the rectangular region 24. For example, bump electrode 60A has a generally triangular cross-sectional shape that follows two sides that define the corners of rectangular region 24 and the outer periphery of second coil body 50, and bump electrode 60B has a generally triangular cross-sectional shape that follows two sides that define the corners of rectangular region 24 and the outer periphery of first coil body 30. Each of bump electrodes 60A, 60B may have the same cross-sectional shape and the same cross-sectional dimensions over the entire length of substrate 40 in the thickness direction.

[0040] Note that none of the bump electrodes 60 overlaps with the first turn portion 32c of the first planar coil 32 or the second turn portion 52c of the second planar coil 52 in the thickness direction of the substrate 40. More specifically, at least the end portion (i.e., the upper end portion) of each of the bump electrodes 60 on the substrate 40 side does not overlap with the first turn portion 32c or the second turn portion 52c. The lower end portion of the bump electrode 60 may overlap with the first turn portion 32c and the second turn portion 52c in the thickness direction of the substrate 40.

[0041] The through holes 43, 44 and the via conductor 49 are located at the corners of the rectangular region 24, similar to the pair of bump electrodes 60. The cross-sectional shape of the via conductor 49 (i.e., the opening shape of the through holes 43, 44) is a substantially triangular shape along the outer periphery of the first coil body 30 or the second coil body 50 and two sides that define the corners of the rectangular region 24, similar to the cross-sectional shape of the pair of bump electrodes 60. The cross-sectional shape of the via conductor 49 may be the same shape as or similar to the cross-sectional shape of the bump electrode 60.

[0042] Like through holes 43 and 44, outer end 32a of first planar coil 32 overlapping through hole 43 and outer end 52a of second planar coil 52 overlapping through hole 44 are also located at the corners of rectangular region 24.

[0043] The first island electrode 36 and the second island electrode 56 are located at the corners of the rectangular region 24, like the pair of bump electrodes 60. The first island electrode 36 and the second island electrode 56 have a cross-sectional shape in a plane perpendicular to the thickness direction of the substrate 40 that is substantially triangular along the outer periphery of the first coil body 30 or the second coil body 50 and two sides that define the corners of the rectangular region 24. The cross-sectional shapes of the first island electrode 36 and the second island electrode 56 may be the same shape or similar shape to the cross-sectional shape of the bump electrode 60.

[0044] A pair of terminal electrodes 70 are provided on the lower surface 10b of the element body 10. Parts of the pair of terminal electrodes 70 enter openings 13 provided in the lower surface 10b of the element body 10 and are respectively joined to the pair of bump electrodes 60 within the element body 10. At this time, the pair of terminal electrodes 70 are in direct contact with the lower surfaces 61 of the lower ends 60b of the pair of bump electrodes 60. Of the pair of terminal electrodes 70, the terminal electrode 70A connected to the bump electrode 60A is provided on the lower surface 10b near the end surface 10c, and the terminal electrode 70B connected to the bump electrode 60B is provided on the lower surface 10b near the end surface 10d. Each of the terminal electrodes 70A, 70B is made of a resin electrode and can be made of a resin containing Ag powder, for example.

[0045] Each of the terminal electrodes 70A, 70B has a non-uniform thickness t based on the lower surface 10b of the element body 10. That is, the thickness t of each of the terminal electrodes 70A, 70B decreases as the pair of terminal electrodes 70A, 70B approach each other. The thickness t of each of the terminal electrodes 70A, 70B can be the distance between the lower surface 10b of the element body 10 and the lower surface 71 of each of the terminal electrodes 70A, 70B. For example, the thickness of the terminal electrode 70A shown in FIG. 8 is maximum near the end surface 10c of the element body 10, and gradually decreases (i.e., monotonically decreases) as it moves away from the end surface 10c. The thickness T of the portions of the terminal electrodes 70A, 70B that are embedded in the element body 10 is greater than the thickness t of the other portions that are not embedded in the element body 10.

[0046] A procedure for manufacturing the above-described coil device 1 will now be described with reference to FIGS.

[0047] When manufacturing the coil component 1, a substrate 40 is prepared as shown in FIG. 10(a). At this time, the substrate 40 is formed on a wafer, and a plurality of substrates 40 are arranged in a matrix on the wafer. A seed pattern S is formed on both sides 40a and 40b of the substrate 40. The seed pattern S includes patterns corresponding to the first planar coil 32, the first island electrode 36, the second planar coil 52, and the second island electrode 56, respectively. In addition, a conductor 53 is provided on the lower surface 40b of the substrate 40, which is connected to the pattern corresponding to the second island electrode 56 and is connected to a power source (not shown). Furthermore, the substrate 40 is provided with the above-mentioned through holes 43, 44, and 45, and the through holes 43, 44, and 45 are filled with via conductors 48 and 49, respectively. In FIG. 10(a), the through holes 43, 44, and 45 and the via conductors 48 and 49 are omitted from the illustration.

[0048] Then, as shown in FIG. 10(b), the first insulator 34 and the second insulator 54 are formed on both sides 40a, 40b of the substrate 40. The first insulator 34 and the second insulator 54 can be formed by patterning a thick-film resist by known photolithography. The first insulator 34 is formed so as to surround the seed pattern S corresponding to the first planar coil 32 and the first island-shaped electrode 36, and the second insulator 54 is formed so as to surround the seed pattern S corresponding to the second planar coil 52 and the second island-shaped electrode 56.

[0049] Next, as shown in FIG. 10(c), while supplying power from the conductor 53 to the seed pattern 51, electrolytic plating of Cu is performed to form the first planar coil 32, the first island electrode 36, the second planar coil 52, and the second island electrode 56, respectively. At this time, the space defined by the first insulator 34 and the second insulator 54 is filled with Cu. After the electrolytic plating, if necessary, surface treatment (e.g., blackening treatment, etc.) of the Cu exposed from the insulator can be performed. In the blackening treatment, a blackening layer (Cu oxide layer) is formed on the Cu plating. By forming a blackening layer with a roughened surface, the Cu plating and the protective films 38, 58 are firmly bonded to each other by the anchor effect.

[0050] Note that, as long as conductor 53 can be utilized for electrolytic plating of first planar coil 32 and second planar coil 52, it is sufficient that conductor 53 is electrically connected to either first planar coil 32 or second planar coil 52, and conductor 53 may be electrically connected to both first planar coil 32 and second planar coil 52. In this embodiment, conductor 53 is exposed from the surface (i.e., end surface 10c) of element body 10, and therefore, by checking the position where conductor 53 is exposed from the appearance of coil component 1, the position of second island electrode 56 to which conductor 53 is connected and the position of bump electrode 60A can be determined.

[0051] 11(a), the above-mentioned protective films 38, 58 are formed. The outer end 52a of the second planar coil 52 and the second island electrode 56 on which the bump electrode 60 is formed are not formed with the protective film 58 (or are removed after the protective film 58 is formed), and are exposed from the protective film 58. When the above-mentioned blackening treatment is performed, the blackened layer on the outer end 52a of the second planar coil 52 and the second island electrode 56 in the area exposed from the protective film 58 is removed by the reduction treatment. Through the above steps, the above-mentioned coil section 20 is obtained.

[0052] Next, as shown in FIG. 11(b), a thick resist 80 is formed on the lower surface 40b side of the substrate 40. The resist 80 has an opening 82 corresponding to the opening 42 of the substrate 40. The resist 80 also has openings 84A and 84B corresponding to the regions where a pair of bump electrodes 60 are to be formed (i.e., the outer end 52a of the second planar coil 52 and the second island electrode 56). Then, as shown in FIG. 11(c), electrolytic plating of Cu is performed using the outer end 52a of the second planar coil 52 and the second island electrode 56 exposed from the protective film 58 in the openings 84A and 84B of the resist 80. At this time, the internal spaces of the openings 84A and 84B are filled with Cu, and the bump electrodes 60 are formed in the openings 84A and 84B, respectively. Furthermore, as shown in FIG. 12(a), the resist 80 is removed to expose the bump electrodes 60.

[0053] Next, as shown in FIG. 12(b), the coil portion 20 and the bump electrode 60 are integrally covered with a magnetic material to form the element body 10 using a known method. At this time, the thickness of the element body 10 is designed to be larger than the thickness of the bump electrode 60, and the bump electrode 60 is completely embedded in the element body 10 and is not exposed from the lower surface 10b. The lower surface 10b of the element body 10 is appropriately polished for flattening. Thereafter, as shown in FIG. 12(c), the lower surface 10b of the element body 10 in the region corresponding to the bump electrode 60 is etched by a known method to form an opening 13 in the lower surface 10b, and the bump electrode 60 is exposed from the opening 13. Finally, the terminal electrode 70 having the above-mentioned shape is formed on the lower surface 10b of the element body 10, and the wafer is divided into individual pieces, thereby completing the manufacture of the coil component 1. At this time, by applying a terminal electrode 70 of a resin electrode to the underside 10b of the element body 10, the resin electrode enters the element body through the opening 13 in the underside 10b of the element body 10 and is bonded to the bump electrode 60 exposed from the opening 13 at its underside 61.

[0054] As explained above, in the above-mentioned coil component 1, the terminal electrode 70 enters the opening 13 of the element body 10 and is joined to the bump electrode 60 within the element body 10. That is, the terminal electrode 70 contacts the terminal electrode 70 and also contacts the element body 10 (specifically, the inner surface of the opening 13). Therefore, compared to the case where the bump electrode is exposed on the lower surface 10b of the element body 10, the contact area of ​​the terminal electrode 70 (particularly the area in contact with the element body 10) is larger, and high adhesion of the terminal electrode 70 is achieved.

[0055] The present invention is not limited to the above-described embodiment, and may be modified in various ways. For example, the coil is not limited to the above-described form, and may be, for example, a form that does not include a substrate. Furthermore, the coil is not limited to the above-described elliptical ring shape, and may be, for example, a circular ring shape or a rectangular ring shape.

[0056] As can be understood from the above description, the present specification discloses the following. [Appendix 1] an element body having a lower surface facing a mounting substrate; A coil conductor disposed within the element body; a pair of bump electrodes respectively connected to both ends of the coil conductor and extending from both ends of the coil conductor toward the bottom surface of the element body along a direction intersecting the bottom surface; a pair of terminal electrodes provided on a lower surface of the element body, a portion of which extends into the element body and is joined to the pair of bump electrodes within the element body; A coil component comprising: [Appendix 2] 2. The coil component described in claim 1, wherein the terminal electrode is made of a resin electrode. [Appendix 3] 3. The coil component according to claim 1, wherein a bonding surface of the bump electrode bonded to the terminal electrode is flat. [Appendix 4] 4. The coil component according to claim 1, wherein the thickness of the portion of the terminal electrode that is embedded in the element body is greater than the thickness of the remaining portion. [Appendix 5] 5. The coil component according to claim 1, wherein at least a portion of the bump electrode gradually expands toward the lower surface of the element body. [Explanation of symbols]

[0057] 1... coil component, 10... element body, 20... coil portion, 22... coil, 60, 60A, 60B... bump electrodes, 61... lower surface, 70, 70A, 70B... terminal electrodes.

Claims

1. an element body having a lower surface facing a mounting substrate; A coil conductor disposed within the element body; a pair of bump electrodes respectively connected to both ends of the coil conductor and extending from both ends of the coil conductor toward the bottom surface of the element body along a direction intersecting the bottom surface; a pair of terminal electrodes provided on the lower surface of the element body, a portion of which extends into the element body and is joined to the pair of bump electrodes within the element body; A coil component comprising:

2. The coil component according to claim 1 , wherein the terminal electrodes are made of resin.

3. The coil component according to claim 1 , wherein a joining surface of the bump electrode joined to the terminal electrode is flat.

4. The coil component according to claim 1 , wherein a thickness of the portion of the terminal electrode that is embedded in the element body is greater than a thickness of the remaining portion.

5. The coil component according to claim 1 , wherein at least a portion of the bump electrode gradually widens toward the lower surface of the element body.

Citation Information

Patent Citations

  • Electronic component

    JP2020155510A