Method for manufacturing dry electrode on current collector with aid of roller device, roller device, dry electrode, computer program product, and computer-readable medium

The method addresses issues of incomplete layers in dry electrode production by adjusting the laminate gap based on a homogeneous powder layer and using a removal device, resulting in high-quality, efficient, and cost-effective electrode manufacturing.

JP2024144404AActive Publication Date: 2024-10-11パワーコエスエー

Patent Information

Application Number
JP2024057281
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-03-29
Publication Date
2024-10-11
Estimated Expiration
2044-03-29

AI Technical Summary

Technical Problem

The production of dry electrodes using multi-roll calenders or roller devices is often hindered by incomplete layers on the rollers, leading to poor quality electrodes and potential roller damage due to clogging when incomplete layers are transferred to the current collector.

Method used

A method involving a roller device with a controller unit that adjusts the laminate gap based on the formation of a homogeneous thin layer of powder on the rollers, ensuring precise deposition on the current collector, and includes a removal device to handle incomplete layers, thereby preventing clogging and improving electrode quality.

Benefits of technology

This method enhances the efficiency, reliability, and cost-effectiveness of dry electrode production by ensuring high-quality electrodes are produced without roller damage or clogging, reducing maintenance efforts and powder consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024144404000001_ABST
    Figure 2024144404000001_ABST
Patent Text Reader

Abstract

To provide a method for manufacturing dry electrodes on a current collector with the aid of a roller device.SOLUTION: A method for manufacturing dry electrodes on a current collector with the aid of a roller device, the roller device including at least three rollers and a current collector 12, includes the steps of: rotating a first roller 13 and a second roller 14 in opposite rotational directions; pouring powder into a calendar gap 20 formed by the first rotating roller 13 and the second rotating roller 14 and guiding the powder on the second roller 14; triggering a signal with the aid of a control unit for adjusting a laminating gap 18 between the second roller 14 and a third roller 15, and moving the third roller 15 and / or the first roller 13 and the second roller 14 toward each other in the direction of the current collector 12; moving at least the third roller 15 in the opposite direction of the second roller 14; and moving the current collector 12 through the laminating gap 18.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates generally to the field of electrode manufacturing, and more particularly to dry electrode manufacturing. In particular, the present invention relates to a method for manufacturing a dry electrode on a current collector using a roller apparatus, a roller apparatus, a dry electrode, a computer program product, and a computer readable medium.

[0002] When manufacturing dry electrodes using a multi-roller calender or roller apparatus, conditions can arise where imperfect layers are present on the rollers at the start of the process, and when these imperfect layers are laminated to the current collector, they result in the production of poor quality or even unusable electrodes.

[0003] Furthermore, conditions can arise where an incomplete layer is not completely transferred to the current collector, and thus coating material remains on the roller, whereupon new material is fed into the film-forming gap, which can cause the roller gap to become clogged, requiring the process to be stopped, or in the worst case scenario, causing damage to the roller.

[0004] The object of the present invention is to at least partially eliminate the above-mentioned drawbacks. In particular, the object of the present invention is to increase the efficiency and reliability of a method for producing a dry electrode and to reduce the costs of producing a dry electrode by said method. Furthermore, the object of the present invention is to increase the quality of the dry electrodes produced by said method.

[0005] The above problem is solved by a method for producing a dry electrode on a current collector by means of a roller apparatus having the features of claim 1, a roller apparatus having the features of claim 8, a dry electrode having the features of claim 10, a computer program product having the features of claim 11 and a computer-readable medium having the features of claim 12. Further features and details of the invention can be taken from the respective dependent claims, the description and the drawings, whereby the features and details explained in relation to the method according to the invention naturally also apply in relation to the roller apparatus, the dry electrode, the computer program product and / or the computer-readable medium according to the invention and vice versa, so that the disclosures of the individual aspects of the invention are always mutually associated or can be associated with each other.

[0006] Embodiments of the present invention advantageously provide an improved method for manufacturing a dry electrode on a current collector using a roller apparatus, which method can produce high quality dry electrodes at low cost and with high reliability.

[0007] One aspect of the present disclosure relates to a method for manufacturing a dry electrode on a current collector using a roller apparatus, the roller apparatus comprising at least three rollers and a current collector disposed between a second roller and a third roller of the at least three rollers, the method comprising the steps of: rotating a first roller and a second roller of the at least three rollers in opposite rotational directions; shaking the powder into a calender gap formed by a rotating first roller and a rotating second roller and guiding the powder at the second roller; triggering a signal using the controller unit to adjust a lamination gap between the second roller and the third roller, and moving the third roller and / or the first roller and the second roller relative to each other toward the current collector; rotating at least a third roller of the at least three rollers in a counter-rotating direction relative to the second roller; moving the current collector through the laminate gap; wherein the lamination gap is adjusted so that the powder is deposited as a thin layer onto the current collector to form a dry electrode.

[0008] In other words, in the method for producing a dry electrode on a current collector using a roller device, it is proposed to start the roller device before the powder is applied to the current collector as a thin layer in the first place. Two states or two operating states can therefore be distinguished: before the signal for adjusting the lamination gap is triggered, the roller device can be driven in a starting mode or in a starting state; after the signal for adjusting the lamination gap is triggered, the roller device can be driven in a normal operating mode or in a normal operating state.

[0009] The lamination gap can be the gap between two rollers in which the current collector is placed and preferably passed through. Unlike the lamination gap, the calender gap is the space between two rollers in which the powder can be shaken. There is usually only one roller between the lamination gap and the calender gap. In the post-compression process, there can be two rollers between the lamination gap and the calender gap.

[0010] The powder may be a powdered material. The powder is preferably solvent-free and is transferred into a layer using a roller device. The powder includes, in particular, an active material, a conductive additive and a binder. The components of the powder may be mixed in a preliminary step of the process for producing a dry electrode. The electrode may be referred to as a bilayer or a monolayer layer deposited on a substrate. The electrode may be, for example, a bilayer cathode material and / or a bilayer anode material.

[0011] The current collector may also be referred to as a current collector or a substrate. The current collector may have a main function of being used as a substrate for a thin layer.

[0012] The quality of the produced electrodes can depend on the distribution of the powder or powder-like material as a thin layer. A high-quality electrode is preferably formed from a homogeneous thin layer. It has therefore proven to be advantageous to apply the powder to the current collector only when the powder guided onto the second roller forms a homogeneous thin layer.

[0013] For this purpose, the method provides for rotating rollers which together form a calender gap, in which powder is preferably already shaken, which is guided against or on a second roller. The powder can therefore at least partially form a thin layer by the calendering process in the calender gap. However, usually the powder can only form an incomplete thin layer or a layer which may have defects for the time being. A partially thin layer of powder can have cracks, holes, etc. Such an incomplete or defective layer is therefore unusable for the electrode or results in an electrode of low quality.

[0014] The method is therefore configured to adjust the lamination gap only after a signal is triggered by the controller unit. Triggering a signal may be synonymous with a transition to a normal operating state. The signal is preferably triggered when the powder has formed a homogeneous thin layer on the second roller. The signal is preferably triggered when the layer supported by the roller is completely present on the roller.

[0015] Specifically, the controller unit can trigger a signal upon command of a user, and the user of the roller device can determine by observing the powder or thin layer that the lamination gap should be adjusted accordingly, particularly to allow the powder to be deposited on the current collector as a thin layer to form a dry electrode.

[0016] Alternatively or additionally, the controller unit can trigger a signal according to a set number of roller revolutions based on empirical values.Alternatively or additionally, a removal device, for example arranged on the second roller, can calculate how much powder has been removed from the corresponding roller, whereby the controller unit can trigger a signal based on the calculated amount of powder removal.

[0017] When the signal for adjusting the lamination gap is triggered, the controller unit can control the rollers of the roller device so that the lamination gap across the current collector is reduced. All rollers arranged on one side of the current collector can be moved synchronously in the radial direction towards the current collector. Alternatively, the rollers on one side of the current collector and the rollers on the other side can be moved radially towards the current collector. If the powder is applied on the current collector as a thin layer on both sides, it has proven advantageous to move the rollers from both sides of the current collector towards the current collector. When adjusting the lamination gap, the distance between two adjacent rollers arranged across the current collector can be adjusted and made particularly small. It should be noted that the lamination gap does not have to be constant when driving the roller device.

[0018] The width of the lamination gap can still be adjusted under normal operating conditions by the controller unit. The adjustment of the lamination gap can be performed by force control or by displacement control.

[0019] The lamination gap can be changed when the powder is applied as a thin layer. The lamination gap can be changed as long as the powder can still be applied as a thin layer when changed. The force-controlled adjustment of the lamination gap takes into account the force or pressure on the current collector when the powder is applied as a thin layer. If the force and / or pressure on the current collector increases, the lamination gap is adjusted to be wider. However, this also means that the thin layer becomes thicker. For this reason, the force-controlled adjustment of the lamination gap can be configured to post-process the manufactured electrode in order to adapt the thickness of the electrode.

[0020] When the lamination gap is adjusted by displacement control, the actual distance between the current collector and the adjacent roller or the actual distance between two adjacent rollers sandwiching the current collector is adjusted. When the lamination gap is adjusted by displacement control, it can be constant throughout the normal operating mode or normal operating conditions.

[0021] The remaining rollers of the roller arrangement can be adjusted so that as soon as they are rotated, the lamination gap can be adjusted and at this point the powder can be applied as a thin layer onto the current collector. Alternatively, the remaining rollers of the roller arrangement can be moved simultaneously relative to the current collector. However, it is important that the remaining rollers upstream of the junction of the lamination gap first rotate or at least are free to rotate, since otherwise cracks in the web may occur. In an embodiment in which a thin layer is applied only on one side of the current collector, the third roller is now rotated. In an embodiment of a roller arrangement symmetrical about the current collector, it is also conceivable that all rollers of the roller arrangement are rotated before the lamination gap is adjusted. It is important that all rollers adjacent to the shaking device are already rotated before the lamination gap is adjusted.

[0022] Immediately after adjusting or triggering the signal to adjust the lamination gap, the current collector can be moved or run through the second and third rollers. The current collector and current collecting film can be stationary for the entire time that the lamination gap is too wide to allow the powder to deposit on the current collector in the first place, thus saving energy.

[0023] It should be noted that a double-sided dry electrode can be produced if the roller arrangement is constructed symmetrically around the current collector, which allows the powder to be shaken in two calendar gaps and the two layers to be guided accordingly on each roller adjacent to the current collector.

[0024] The method can efficiently and accurately provide high quality electrodes, as well as avoid or at least reduce clogging of the roller apparatus, and reduce the maintenance effort of the roller apparatus for producing dry electrodes.

[0025] According to one embodiment of the method, the method further comprises the following steps: - calculating the thickness of the layer of powder at the second roller; and triggering a signal by the controller unit based on the calculated thickness; Includes at least one of the following:

[0026] In order to avoid the powder being applied on the current collector as an incomplete thin layer, it is possible to configure the thickness of the thin layer of powder to be calculated at the second roller or additionally at the third roller. The calculation here can be performed by a layer thickness sensor. Alternatively or additionally, the second roller and alternatively the third roller can be photographed by a camera and the photographs can be played back on a user interface. Based on the photographs of the second roller and / or the third roller, the user can calculate whether the thickness of the thin layer of powder meets a set criterion, for example a set thickness. Alternatively or additionally, an artificial intelligence-based program can also be executed via the photographs taken by the camera.

[0027] It should be noted that the layer here should not only have a set thickness, but also have a constant thickness (at least for the most part) over a set interval. In other words, a signal can be triggered by means of the controller unit if the calculated thickness meets a set criterion. The set criterion can be a surface load, a minimum area without defects, etc.

[0028] This allows the time point at which the signal is triggered to be adjusted more precisely, which can further improve the quality of the produced electrodes.

[0029] According to one embodiment of the method, the method further comprises the following step, namely removing the powder guided at the second roller, in particular the powder resulting from the defective layer, by a removal device arranged downstream of the lamination gap in the direction of rotation. If the powder guided at the second roller is removed, this may be a defective layer present on the second roller, i.e. for example a layer with an incorrect or irregular thickness. The removal of the powder guided at the second roller, preferably the powder resulting from the at least partially defective layer, can be carried out during the start-up mode.

[0030] This allows the material or powder not deposited on the current collector to be removed at the corresponding roller during the start-up mode or during the normal operation mode of the roller device, thereby minimizing the risk of clogging at the corresponding roller of the roller device.

[0031] The powder or material removed from the removal device can be fed back to the shaking device. The powder can thus be reused, which reduces powder consumption during the manufacture of the electrodes. It has been found to be advantageous to treat the removed powder in a preceding process step before it can be guided again.

[0032] According to one embodiment of the method, the rotation speed of the first roller, the second roller, the third roller and / or the running speed of the current collector are controlled by the controller unit, preferably based on the calculated thickness of the thin layer of powder.

[0033] In other words, the roller device, in particular the rollers of the roller device, can be controlled such that set criteria are met, such as surface load of the powder layer, thickness of the layer, etc. The thickness of the powder layer may depend on the rotation speed of the rollers of the roller device and vice versa.

[0034] This allows the production of high quality electrodes.

[0035] According to one embodiment of the method, when removing the guided powder at the second roller, in particular the defective thin layer of powder, said powder is captured and / or sucked up by a removal device.

[0036] According to one embodiment of the method, a signal for adjusting a lamination gap between the second roller and the third roller is triggered after a predetermined time.

[0037] The roller device may have, for example, a virtual hyperbola. Based on simulations or tests with the virtual hyperbola of the roller device, it may be known that after a predefined time the thickness of the laminated powder, the surface load and / or another parameter meets the set criteria. Such a predefined time may be stored, for example, in a storage medium of the controller unit. Thus, a signal for adjusting the lamination gap can be automatically triggered after a predefined time.

[0038] The predetermined time may likewise be based on experimental and / or empirical data, and thus may be stored by a user in a storage medium of the controller unit, for example by means of a user interface.

[0039] Furthermore, the predetermined time can be configured to define a maximum time. In other words, the signal can be triggered after the maximum time, for example, independent of the calculated thickness. This has proven to be advantageous, for example, if the controller unit is configured to trigger the signal only upon, for example, a user's command. In this way, it is possible to avoid the roller device operating in the starting mode or in the starting state for an unnecessarily long time, even if the user forgets to output a command.

[0040] Likewise, if it is not possible to reliably trigger a signal based on the calculated thickness, for example because a layer thickness sensor has malfunctioned, it has proven advantageous to trigger the signal after a predetermined time has elapsed.

[0041] According to one embodiment of the method, the method further comprises the following steps: Calculating the amount of powder shaken into the calender gap, and / or - calculating the rotation made by the second roller; triggering a signal by the controller unit based on the calculated powder amount and / or the calculated number of revolutions made by the second roller; Includes at least one of the following:

[0042] It can be arranged to calculate the amount of powder removed from the metering unit in order to calculate how much powder has been shaken into the calender gap.

[0043] It should be noted that the exact opposite procedure can be followed in order to prevent unusable coating from being transferred to the current collector when the roller device is stopped. In other words, when the roller device is stopped, the lamination gap can first be adjusted so that the powder cannot be deposited on the current collector as a thin layer. Only after the lamination gap has been adjusted accordingly, i.e., after the lamination gap has been enlarged, can the corresponding roller be stopped.

[0044] A second aspect of the present disclosure relates to a roller apparatus for manufacturing a dry electrode on a current collector. The roller apparatus comprises a controller unit, at least three rollers, and a current collector arranged in a lamination gap configured to capture the thin layer of powder. Here, the lamination gap defines a gap between a first roller and a second roller of the at least three rollers. The roller apparatus further comprises a shaking device configured to shake the powder into a calendar gap. The calendar gap defines a gap between the first roller and the second roller. The roller apparatus further comprises a removal device configured to remove the powder guided in the second roller. The removal device is arranged downstream of the lamination gap in the direction of rotation. In this case, the controller unit is configured to trigger a signal for adjusting the lamination gap, in particular a signal for adjusting the thickness of the lamination gap.

[0045] The advantages described above and below for the method apply equally to the roller device.

[0046] According to one embodiment of the roller device, the roller device further comprises a layer thickness sensor configured to determine the thickness of the thin layer of powder at the second roller, in particular upstream of the lamination gap in the direction of rotation.

[0047] A third aspect of the present disclosure relates to a dry electrode manufactured using the methods described above and below.

[0048] A fourth aspect of the present disclosure relates to a computer program product comprising instructions which, when executed, cause a controller unit of a roller device to carry out at least partial steps of the methods described above and below as described above and below.

[0049] A fifth aspect of the present disclosure relates to a computer-readable medium having stored thereon the computer program product described above.

[0050] All of the disclosures and advantages discussed above and below with respect to one aspect of the disclosure apply equally to all further aspects of the disclosure.

[0051] In the following, an embodiment of the invention will be described with reference to the figures. [Brief description of the drawings]

[0052] [Figure 1] FIG. 2 is a side view showing a schematic diagram of a roller device according to an embodiment; [Diagram 2] FIG. 2 is a plan view showing a roller device according to an embodiment; [Diagram 3] FIG. 11 is a side view showing a schematic view of a roller device according to another embodiment. [Figure 4] FIG. 11 is a side view showing a schematic view of a roller device according to another embodiment. [Diagram 5] FIG. 2 is a schematic diagram showing a roller of a roller device according to an embodiment. [Figure 6] FIG. 2 is a schematic diagram showing a roller of a roller device according to an embodiment. [Figure 7]FIG. 11 is a side view showing a schematic view of a roller device according to another embodiment. [Figure 8] FIG. 11 is a side view showing a schematic view of a roller device according to another embodiment. [Figure 9] FIG. 11 is a side view showing a schematic view of a roller device according to another embodiment.

[0053] In the figures, similar elements, elements with similar functions, identical elements or elements with equivalent functions are provided with similar or identical reference signs. The figures are only schematic and are not drawn to scale.

[0054] In FIG. 1, a roller device 100 according to an embodiment is shown in schematic side view. Such a roller device 100 can be used to carry out a method for producing a dry electrode 10 on a current collector 12. The roller device 100 of FIG. 1 has four rollers. Between the first roller 13 and the second roller 14, a gap called the calender gap 20 is provided. The first roller 13 can also be called an application roller. The gap between the third roller 15 and the fourth roller 16 is also called the calender gap 20. Such a pressure roller unit can have one or more rollers. In contrast, between the second roller 14 and the third roller 15, a gap called the lamination gap 18 is provided. The current collector 12 is arranged in the lamination gap 18. The second roller 14 and the third roller 15 can be part of the pressure roller unit. The second roller 14 and the third roller 15 can therefore also be called pressure rollers. The lamination gap 18, which may also be called a compression gap, can be configured to transfer the thin layer of powder 11 from the rollers of the compression roller unit, i.e. from the second roller 14 and / or the third roller 15, to one side, possibly two sides, of the current collector 12 by means of a compression force. It should be noted that the rollers are cylindrically shaped and are preferably arranged parallel to one another with respect to the roller axis.

[0055] The roller device 100 of FIG. 1 is substantially symmetrically constructed around the current collector 12. That is, a thin layer of powder 11 can be deposited on both sides of the current collector 12. It should be noted that the elements and / or components described with respect to one side of the current collector 12 of the roller device 100 of FIG. 1 can be similarly located in mirror symmetry on the other side of the current collector 12 of the roller device 100 of FIG. 1. By depositing a thin layer on both sides of the current collector 12, the efficiency of the dry electrode 10 can be improved. The manufactured dry electrode 10 is composed of a thin layer and the current collector 12. Depending on whether a thin layer is deposited on both sides of the current collector 12, it can be referred to as a one-sided dry electrode 10 or a two-sided dry electrode 10. Asymmetric embodiments are possible as well (see FIG. 7).

[0056] In the roller device 100 of FIG. 1, two rollers are arranged on a first side of the current collector 12 or on the left side of the current collector 12, namely the first roller 13 and the second roller 14. A shaking device 26 configured to shake the powder 11 may be arranged at least partially in the two calender gaps 20 of the roller device 100. The shaking device 26 may also be referred to as a metering unit. A separate removal device 22 may be provided on each one of the two sides of the current collector 12. The two rollers arranged closest to the current collector 12 may be provided with such a removal device 22. The removal device 22 may have a doctor blade 23 and a capture device 24.

[0057] The first roller 13 and the second roller 14 are configured to rotate in opposite directions of rotation. The powder 11 can be shaken by a shaking device 26 into the calendar gap 20 between the first roller 13 and the second roller 14. The powder 11 is then guided in the second roller 14.

[0058] The roller apparatus 100 of Fig. 1 is in operation, and in particular in a normal operating mode, as can be seen from Fig. 1, because the lamination gap 18 is adjusted so that the powder 11 shaken into each calendar gap 20 is formed into a thin layer and deposited on the current collector 12 as a thin layer to form the dry electrode 10. That is, the lamination gap 18 is small enough to allow the powder 11 to be deposited on the current collector 12 in a thin layer.

[0059] In Fig. 2, a roller device 100 according to an embodiment is shown in a schematic plan view. The roller device 100 in Fig. 2 can be, for example, the roller device 100 in Fig. 1. Unless otherwise stated, the roller device 100 in Fig. 2 has the same elements and features as the roller device 100 in Fig. 1. In this case, two thin layers are deposited on the current collector 12, guided respectively on the second roller 14 and on the third roller 15. To be able to adjust the predetermined width of the dry electrode 10, at least one edge section 30, preferably two edge sections 30 per roller, is provided. The edge section 30 can precisely define or cut the edge or border of the dry electrode 10. The edge section 30 allows the width of the electrode 10 to be adjusted. To remove the material or powder 11 remaining beyond the edge or the layered powder 11, a removal unit 28 is preferably arranged directly next to the edge section 30. The removal unit 28 can remove or capture the material. The removal unit 28 can have a capture container. The removal unit 28 may furthermore have a doctor blade 23 by means of which the corresponding rollers can be cleaned.

[0060] The powder 11 guided over the second roller 14 and the third roller 15 forms a thin layer. As soon as the thin layer is deposited on the current collector 12, this thin layer can be called a dry electrode 10. In order to be able to produce a functional dry electrode 10, the thin layer must be formed as uniformly as possible. The thin layer must be formed without defects or flaws. For example, cracks, holes and / or breaks in the layer can be considered as defects. Preferably, the thin layer also has a set minimum layer thickness. The thin layer or dry electrode 10 of FIG. 2 is defect-free. It can be seen that the roller device 100 of FIG. 2 is also in operation as in the above-mentioned example, in particular in the normal operating mode. This is because the roller device 100 according to the invention is designed so that the thin layer of powder 11 can only be captured by the current collector 12 in the normal operating mode.

[0061] A roller apparatus 100 according to one embodiment is shown in schematic side view in Figure 3. Unless otherwise noted, the roller apparatus 100 of Figure 3 has the same elements and features as the roller apparatus 100 of Figures 1 and 2.

[0062] Unlike the roller device 100 of Figures 1 and 2, the roller device 100 of Figure 3 is in a start-up mode, i.e. has not yet entered into a normal operating mode. The gap between the second roller 14 and the third roller 15, i.e. the lamination gap 18, is larger in the start-up mode than in the normal operating mode. The lamination gap 18 of the roller device 100 of Figure 3 is adjusted so that the powder 11 and / or the partially laminated powder 11 cannot be applied to the current collector 12. It has therefore been found to be advantageous, for example to save energy, not to move the current collector 12 through the lamination gap 18 during the start-up mode.

[0063] At the second roller 14 and the third roller 15 of the roller arrangement 100 in FIG. 3, blocks 19 or particles of powder 11 are shown. The blocks 19 may form a layer with defects. The powder 11 shaken into the calender gap 20 is not yet thinned in the starting mode. Rather, the thin layer itself is only just beginning to form, which leads to the formation of blocks 19 or particles of powder 11. The powder 11 is only partially thinned in the starting state. In other words, the quality of the thin layer is not yet sufficient to form a dry electrode 10 from this thin layer. It is therefore advantageous to remove the blocks 19 or particles of powder 11. This is achieved by a removal device 22. The removal device 22 can be configured to remove the powder 11 at the second roller and / or the third roller 15, preferably downstream of the lamination gap 18 in the direction of rotation. Additionally, the removal device 22 can be configured to wash or clean the corresponding roller when removing the powder 11 or the block 19. For this purpose, the removal device 22 may have a doctor blade 23. To remove material, i.e. the powder 11 and / or the block 19, from the corresponding roller, the removal device 22 preferably has a catcher device 24. The catcher device 24 can mechanically catch the material and / or aspirate the material.

[0064] The roller arrangement 100 of Fig. 3 further comprises a layer thickness sensor 17, which is preferably arranged upstream of the lamination gap 18 in the direction of rotation. It is also conceivable to arrange a further layer thickness sensor 17 on the third roller 15 of the roller arrangement 100 of Fig. 3, since the powder 11 is also guided in a thin layer on the third roller 15.

[0065] By means of the layer thickness sensor 17, the thickness of the at least partially laminated powder 11 can be calculated or measured. When the thickness of the powder 11 and / or the at least partially laminated powder 11 is calculated, it can be determined or determined by the controller unit whether the calculated thickness meets the set criteria. If the calculated thickness meets the set criteria, the controller unit can trigger a signal to adjust the lamination gap 18. When adjusting the lamination gap 18, the third roller 15, in particular together with the fourth roller 16 and / or the first roller 13 and the second roller 14 can be moved relative to each other towards the current collector 12.

[0066] A roller apparatus 100 according to one embodiment is shown in schematic side view in Figure 4. Unless otherwise stated, the roller apparatus 100 of Figure 4 has the same elements and features as the roller apparatus 100 of Figures 1-3.

[0067] In FIG. 4, it is clear that no dry electrode 10 or thin layer has been deposited on the current collector 12. From this, it can be identified that the roller device 100 in FIG. 4 is still in the start-up mode. However, unlike FIG. 3, the powder 11 guided in the second roller 14 and the third roller 15 forms a uniform thin layer. In other words, the roller device 100 has been driven in the start-up mode for a sufficient time and is therefore ready to move to the normal operation mode. The controller unit (not shown here) of the roller device 100 can therefore trigger a signal to adjust the lamination gap 18 so that a thin layer of powder 11 can now be deposited on the current collector 12. To adjust the lamination gap 18, the rollers can be moved in pairs, i.e. the first roller and the second roller 14 together and / or the third roller and the fourth roller 16 together, in the radial direction towards the current collector 12. The movement of the rollers in pairs allows the respective calender gaps 20 to be kept constant. In an embodiment in which the roller device 100 is asymmetric, it is conceivable, for example, to move only two rollers on one side of the current collector 12 towards the current collector 12. The corresponding roller is moved radially towards the current collector 12 until a thin layer of powder 11 can be deposited on the current collector 12. The radial movement or movements are indicated by arrows in FIG.

[0068] Figures 5 and 6 show schematic views of rollers of roller apparatus 100 according to one embodiment. The roller shown in Figures 5 and 6 may be third roller 15. If the roller in Figures 5 and 6 were viewed in a mirror image, it would be second roller 14 of roller apparatus 100.

[0069] As explained with reference to Figs. 1 to 4, a removal device 22 can be arranged on the second roller 14 and alternatively on the third roller 15. The removal device 22 is used on the one hand for removing material from the corresponding roller and on the other hand for cleaning the corresponding roller. To clean the corresponding roller, the removal device 22 can have a brush 25. The brush 25 can be a rotating brush. Downstream of the removal device 22 in the direction of rotation of the roller, a cleaning device 34 can further be provided. The cleaning device 34 can clean the surface of the roller in addition to the removal device 22. The cleaning device 34 can have one or more cleaning rollers 38 configured to apply a woven or nonwoven fabric to the surface of the corresponding roller or to press it against the roller. This allows a higher cleaning effect to be obtained. The woven fabric can be unwound via the cleaning roller 38 from one bobbin 33 to the other bobbin 33 and subsequently rewound again. In the embodiment of Fig. 6, it can further be configured to apply a cleaning agent to the woven fabric and / or to the surface of the corresponding roller. In the embodiment of FIG. 5, cleaning of the rollers can be performed dry.

[0070] 7-9 show schematic side views of another embodiment of a roller device 100. Unless otherwise stated, the roller device 100 of Figures 7-9 has the same elements and features as the roller device 100 of Figures 1-4.

[0071] Basically, all configurations of rollers are conceivable, which allow the formation of a thin layer on one or both sides of the current collector 12. It is also conceivable to produce a dry electrode 10 on only one side. In the latter case, the roller arrangement 100 can have only three rollers. For example, only the lower three rollers of the roller arrangement 100 of FIG. 7 need to be provided. In FIG. 9, four rollers can also be provided for transferring the thin layer to the current collector 12. In other words, it is conceivable to provide a pressure roller unit with four pressure rollers. The powder 11 to be pressed flat is thus guided in the example of FIG. 9 over two second rollers 14, 14' and likewise over two third rollers 15, 15'.

[0072] As an additional note, it should be noted that the words "comprising" and "having" do not exclude other elements, and the indefinite articles "a" and "an" do not exclude a plurality. Furthermore, it is pointed out that features and steps described with reference to one of the above embodiments can also be used in combination with other features and steps of another embodiment described above. Reference signs in the claims should not be considered as limiting. [Explanation of symbols]

[0073] 10 electrodes 11 powder 12 Current collector 13 First Roller 14 The Second Roller 15 The Third Roller 16 The Fourth Roller 17 Layer Thickness Sensor 18 Laminate Gap 19 Blocks 20 Calendar Gap 22 Removal device 23 Doctor Blade 24 Capture device 25 Brushes 26 Shaking device 28 Removal unit 30 Edge Section 33 Bobbin 34 Cleaning device 38 Cleaning roller 100 Roller device

Claims

1. A method for producing a dry electrode (10) on a current collector (12) using a roller apparatus (100), the roller apparatus (100) comprising at least three rollers (13, 14, 15) and a current collector (12) disposed between a second roller (14) and a third roller (15) of the at least three rollers, the method comprising: rotating a first roller (13) and a second roller (14) of the at least three rollers in opposite rotational directions; shaking the powder (11) into a calender gap (20) formed by the rotating first roller (13) and the rotating second roller (14) and guiding the powder (11) in the second roller (14); triggering a signal using a controller unit to adjust a lamination gap (18) between the second roller (14) and the third roller (15) and move the third roller (15) and / or the first roller (13) and the second roller (14) toward the current collector (12) relative to one another; rotating at least the third roller (15) of the at least three rollers in a counter-rotating direction relative to the second roller (14); moving the current collector (12) through the lamination gap (18); Including, The lamination gap (18) is adjusted so that the powder (11) is deposited on the current collector (12) as a thin layer to form the dry electrode (10). method.

2. The method further comprises: Calculating the thickness of the thin layer of powder (11) on the second roller (14); and triggering a signal by the controller unit based on the calculated thickness; The method of claim 1 , comprising at least one of:

3. 3. The method according to claim 1 or 2, further comprising a step of removing the powder (11) guided in the second roller (14), in particular the defective thin layer powder (11), by means of a removal device (22) arranged downstream of the lamination gap (18) in the direction of rotation.

4. 4. The method according to claim 1, wherein the rotation speeds of the first roller (13), the second roller (14), the third roller (15) and / or the running speed of the current collector (12) are controlled by the controller unit, preferably based on the calculated thickness of the thin layer of powder (11).

5. 5. The method according to claim 1, wherein when removing the powder (11) guided at the second roller (14), in particular the powder (11) in the form of a thin layer having defects, the powder (11) is captured and / or sucked up by the removal device (22).

6. 6. The method according to claim 1, wherein a signal for adjusting the lamination gap (18) between the second roller (14) and the third roller (15) is triggered after a predetermined time.

7. The method further comprises: Calculating the amount of powder shaken into the calendar gap (20), calculating the rotations made by said second roller (14); triggering a signal by said controller unit based on the calculated powder amount and / or the calculated revolutions made by said second roller (14); The method according to any one of claims 1 to 6, further comprising at least one of the following steps:

8. A roller apparatus (100) for producing a dry electrode (10) on a current collector (12), comprising: A controller unit; At least three rollers; a current collector (12) disposed within a lamination gap (18) configured to capture the thin layer of powder (11), wherein the lamination gap (18) defines a distance between a first roller (13) and a second roller (14) of the at least three rollers; a shaking device (26) configured to shake the powder (11) into a calender gap (20) defining a space between the first roller (13) and the second roller (14); a removal device (22) configured to remove the powder (11) guided in the second roller (14) and arranged downstream of the lamination gap (18) in the direction of rotation; Equipped with the controller unit is configured to trigger a signal for adjusting the lamination gap (18), in particular a signal for adjusting the thickness of the lamination gap (18); A roller device (100).

9. 9. The roller device (100) according to claim 8, further comprising a layer thickness sensor (17) configured to determine the thickness of the thin layer of powder (11) at the second roller (14), in particular upstream of the lamination gap (18) in the direction of rotation.

10. A dry electrode (10) manufactured by the method of any one of claims 1 to 7.

11. A computer program product comprising instructions which, when executed, cause a controller unit of a roller device (100) according to claim 8 or 9 to carry out at least part steps of the method according to any one of claims 1 to 7.

12. A computer readable medium having stored thereon the computer program product of claim 11.

Citation Information

Patent Citations

  • Three-roller type membrane thinning and compounding mechanism

    CN218101311U

  • Electrode manufacturing method

    JP2017098176A

  • Dry film manufacturing method, rolling device, dry film, and substrate coated with dry film

    JP2020522090A

  • Wet powder coating device and coating film manufacturing method

    JP2021159814A

  • Electrode manufacturing method

    JP2022133110A

Cited By

  • Trimming and stripping system for manufacturing dry electrodes

    JP2026086382A