Printed wiring board and manufacturing method for the same

The method of filled plating and blasting process forms a conductor layer on the side surface of cavities in printed wiring boards, addressing resist mask tearing issues and ensuring the integrity of the conductor layer during wiring formation.

JP2024145090AInactive Publication Date: 2024-10-15가부시키가이샤신코세이사쿠쇼
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023057333
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods for forming conductor layers on the side surfaces of cavities in printed wiring boards are prone to resist mask tearing, especially when the cavity area is large, leading to the removal of the conductive layer during wiring formation.

Method used

A method involving filled plating to form a conductor layer on the side surface of a cavity, where the conductor layer is partially exposed and in contact with a copper layer, with the insulating layer on the cavity bottom lower than the copper layer surface, and a manufacturing process that includes forming an opening, laser processing, and blasting to create the cavity.

Benefits of technology

Prevents resist mask tearing and allows for the formation of a conductor layer on the side surface of a cavity without damaging the resist mask, ensuring the integrity of the wiring board.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024145090000001_ABST
    Figure 2024145090000001_ABST
Patent Text Reader

Abstract

To provide a printed wiring board in which a cavity side surface has a conductor layer and to provide a manufacturing method for the same, in which any problem of a resist mask being torn is solved.SOLUTION: A printed wiring board with three or more layers has a cavity in the form of a recess. A conductor layer is partially exposed on a side surface of the cavity. The conductor layer is filled plating or filled plating of 40 to 60 μm in width. Furthermore, a copper layer on the bottom surface of the cavity is divided into at least two parts. There is a copper layer and an insulating layer on the bottom surface of the cavity. The conductor layer is in contact with the copper layer.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a printed wiring board having a metal conductor layer on the side surface of a cavity, and a method for manufacturing the same. [Background technology]

[0002] 2. Description of the Related Art Printed wiring boards are manufactured with recesses called cavities for accommodating electronic components such as semiconductor elements. Generally, in order to form a conductive layer on the side surface of a cavity, the cavity is formed and then the conductive layer is formed by electroless plating or the like.

[0003] In addition, in the process of producing a printed wiring board with a cavity, a through opening that becomes a cavity is formed in a copper-clad laminate, and another copper-clad laminate is laminated to obtain a printed wiring board with a cavity such as a three-layer board or a four-layer board. Alternatively, a printed wiring board with a cavity is obtained by later forming an opening that becomes a cavity in the laminated three-layer board or four-layer board. After the cavity is formed, an etching resist mask is formed on the front and back surfaces of the substrate, and necessary wiring is formed.

[0004] When forming wiring after forming a cavity in this way, if the area of ​​the cavity is large, a problem occurs in that the etching resist mask for forming the wiring is torn. If the resist mask is torn, the conductive layer (plating layer) formed on the side surface of the cavity is removed by the etching solution for forming the wiring.

[0005] Patent Document 1 discloses a technique in which an electroless plating layer is formed in a groove formed along the outer shape of the cavity, and then a part of the groove is formed as the side of the cavity. With the technique described in Patent Document 1, the cavity is formed by cutting the connection part later, so there is no need to worry about the resist mask breaking, but the cavity formed by cutting the connection part is a through hole without a bottom. In addition, this manufacturing method cannot form a cavity later on in a laminated substrate such as a three-layered board or a four-layered board. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Japanese Patent Application Publication No. 10-270829 Summary of the Invention [Problem to be solved by the invention]

[0007] In view of the above circumstances, an object of the present invention is to provide a printed wiring board having a conductor layer on the side surface of a cavity, and a method for manufacturing the same, which solves the problem of the resist mask breaking. [Means for solving the problem]

[0008] The present invention relates to a printed wiring board in which a filled plating conductor layer is exposed on the side surface of a cavity, and a method for manufacturing the same. A first aspect of the present invention is a printed wiring board having three or more layers, the printed wiring board having a cavity in the form of a recess, a conductor layer partially exposed on the side surface of the cavity, the conductor layer being filled with plating, a copper layer and an insulating layer being present on the bottom surface of the cavity, and the conductor layer being in contact with the copper layer.

[0009] A second aspect of the present invention is a printed wiring board in which the conductor layer in the first aspect has a width of 40 to 60 μm.

[0010] A third aspect of the present invention is the printed wiring board according to the first aspect, wherein the copper layer on the bottom surface of the cavity is divided into at least two parts.

[0011] A fourth aspect of the present invention is the printed wiring board according to the first aspect, wherein the surface of the insulating layer at the bottom of the cavity is located lower than the surface of the copper layer at the bottom of the cavity.

[0012] A fifth aspect of the present invention is a method for manufacturing a printed wiring board, comprising the steps of: preparing a substrate having an insulating layer having a copper layer thereon, which is to become a printed wiring board; removing, by etching, the copper layer at a portion of the substrate that is in contact with the outside of an external shape at a position that will become a cavity on the surface side of the substrate, to form an opening; laser processing the portion to form an opening in the insulating layer exposed at the opening; forming a conductor layer by filling plating in the copper layer and the opening in the insulating layer; removing the copper layer at a position that will become the cavity on the surface side of the substrate, and removing a portion of the copper layer by etching so that the copper layer at a position that will become the bottom of the cavity on the back side of the substrate is divided into at least two portions; forming a blast resist mask on the surface side of the substrate, which has an opening at a position that will become the cavity, and forming a blast resist mask on the back side of the substrate, which covers the entire surface of the substrate; and forming a cavity on the surface side of the substrate, which is on the side where the conductor layer formed by the filling plating is exposed, and which has a copper layer divided into at least two portions at its bottom, by blasting.

[0013] A sixth aspect of the present invention is a method for producing a printed wiring board, wherein the conductor layer formed by filling plating in the fifth aspect has a width of 40 to 60 μm. Effect of the Invention

[0014] A printed wiring board having a conductor layer formed on the side surface of the cavity can be obtained without damaging the resist mask for forming the wiring. [Brief description of the drawings]

[0015] [Figure 1] 1A and 1B are plan views showing examples of openings that contact the outside of the external shape of the cavity of the present invention, where FIG. 1(a) shows an example of an opening that is provided in a "L" shape, and FIG. 1(b) shows an example of an opening that is provided in a "U" shape. [Diagram 2] 1 is a plan view of a printed wiring board according to the present invention; [Figure 3-1] 1A to 1E are manufacturing flow diagrams (1) to (5) of a printed wiring board according to the present invention in which a conductive layer is formed on the side surface of a cavity. [Figure 3-2] 6A to 6C are diagrams (6) to (10) showing a manufacturing flow of a printed wiring board according to the present invention in which a conductive layer is formed on the side surface of a cavity. [Figure 3-3] FIG. 11 is a manufacturing flow diagram (11) of a printed wiring board according to the present invention in which a conductor layer is formed on the side surface of a cavity. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] The printed wiring board according to the present invention will be described as a three-layer printed wiring board having a cavity on the upper surface side, however, the printed wiring board according to the present invention is not limited to a three-layer board. The copper layers on the front and back sides are in a state prior to the formation of wiring. In conventional manufacturing processes, through holes, via holes, cavities, etc. are formed in the three-layer substrate by drilling, laser processing, etc. Next, a conductor layer is formed on the side surfaces of the through holes, via holes, cavities, etc. by electroless plating or the like. Then, the copper layers on the front and back sides on which the resist masks are formed are etched to form wiring, thereby obtaining a printed wiring board.

[0017] However, in order to form wiring after forming the cavity, a resist mask is required to cover the cavity, and if the area of ​​the cavity is large, the resist mask may break. Therefore, based on the technical idea that by not forming a cavity in a three-layer substrate before wiring is formed on both sides, but instead forming the necessary through holes, via holes, etc., and forming an opening that contacts the outside of the cavity's outer shape, the resist mask will not be torn, the structure and manufacturing process of printed wiring boards were carefully examined and the present invention was arrived at.

[0018] Therefore, in the printed wiring board according to the present invention, an opening is formed in contact with the outside of the external shape of the cavity, and a copper plating film is formed on the inner surface of the opening by electroless plating. The opening is preferably formed to have a width of about 40 to 60 μm. Figure 1 shows an example of such an opening, where Fig. 1(a) shows an example where the exposed portion of the conductor layer is provided at the corner in a "L" shape, and Fig. 1(b) shows an example where the conductor layer is provided so as to be exposed on the side of the cavity in a "U" shape. Symbol 1 is the cavity provided in the substrate, symbol 2 is the opening (conductor layer 4 after hole-filling plating process), and symbol 3 is the external shape of the cavity. Then, electroless plating is performed for interlayer connection, and a conductor layer is formed by filling plating at the opening that contacts the outside of the cavity's outer shape. Next, the copper layers on the front and back sides are etched to form wiring, but since the cavity portion has not yet been formed, there is no need to worry about the resist mask being torn.

[0019] After the wiring is formed, a resist mask for blasting is formed, and a recess that becomes a cavity is formed by blasting. Therefore, the conductive layer formed by the filled plating is not processed by the blasting treatment, so the insulating layer of the board is removed to obtain a printed wiring board in which the conductive layer formed by the filled plating is exposed on the side surface of the cavity. Also, the copper layer on the bottom surface of the cavity is not processed by the blasting treatment, so the insulating layer on the bottom surface of the cavity is lowered below the surface of the copper layer on the bottom surface of the cavity by the blasting treatment. EXAMPLES

[0020] The present invention will be described in detail below with reference to a process flow diagram of the manufacturing method. The numerical values ​​of dimensions appearing in the following description are those of a printed wiring board actually used in the manufacture, and represent one embodiment of the present invention.

[0021] A printed wiring board A3 having a cavity 1 on the surface side is formed as shown in Fig. 2. In Fig. 2, reference numeral 4 denotes the conductor layer after filling plating (opening 2 before filling plating), reference numeral 4a denotes an exposed portion of the conductor layer on the side of the cavity, reference numeral 10 denotes an insulating layer, reference numeral 20 denotes a surface copper layer, reference numeral 21 denotes an inner copper layer exposed on the bottom of the cavity, reference numeral 30 denotes an insulating layer (prepreg material), reference numeral 400 denotes an exposed portion of the insulating layer on the side of the cavity, reference numeral 600 denotes a side of the cavity, and reference numeral A denotes a core substrate.

[0022] For the production, the following core substrate A was prepared. As the core substrate A, a substrate having 35 μm thick copper layers 20 and 21 on both sides of an insulating layer 10 made of 60 μm thick glass cloth and epoxy resin as shown in FIG. 3-1(1) was prepared, and necessary wiring and the like were processed in the copper layer that would become the inner copper layer 21. This inner copper layer 21 is the part that will become the bottom surface of the cavity portion to be formed later. Next, as shown in Figure 3-1 (2), a prepreg material 30 made of glass cloth and epoxy resin was laminated with 35 μm copper foil (back copper layer) 40 to create a three-layer test board. Note that it is desirable to use a prepreg material with a lower elastic modulus than the insulating layer used in core substrate A. This is because the workability of the blasting process used to form the cavity is affected by the elastic modulus.

[0023] Next, as shown in Figure 3-1 (3), a resist layer 100 was formed on the surface of the front copper layer 20 of the test substrate, and an etching resist mask was formed with an opening at the position where the conductor on the side of the cavity would be formed. At this time, the opening was 50 μm wide and in contact with the outside of the external shape (35 x 35 mm) of the cavity 1 as seen in Figure 1. In addition, an etching resist mask 101 was formed on the surface of the back copper layer 40, covering the entire surface. (See Figure 3-1 (3)) Then, as shown in FIG. 3-1(4), an etching process was carried out to remove the surface copper layer 20 exposed from the openings of the etching resist mask, and thereafter, the etching resist masks on both sides were removed. Next, as shown in FIG. 3-1(5), the exposed insulating layer 10 was removed by laser processing to form an opening 200.

[0024] Next, as shown in Fig. 3-2(6), a copper plating film was formed by electroless plating on the inner surface of the opening 200 that contacts the outside of the external shape 3 of the cavity. Furthermore, a conductor layer 4 was formed by filling plating by hole filling plating. Next, as shown in FIG. 3-2( 7 ), etching resist masks 300 and 301 are formed on the surfaces of the front surface copper layer 20 and the back surface copper layer 40 .

[0025] Then, as shown in Fig. 3-2(8), etching is performed to remove the front copper layer 20 and the back copper layer 40 exposed from the openings of the etching resist mask, and the outer layer circuit wiring is formed. At that time, the insulating layer in the cavity part is also exposed. (Insulating layer exposed part 400) After that, the etching resist masks on both sides are removed. Next, as shown in Fig. 3-2(9), a blast resist mask 500 was formed using a dry film resist so as to expose the insulating layer exposed portion 400 in the cavity portion on the front surface of the substrate. In addition, a blast resist mask 501 was formed using a dry film resist on the rear surface of the substrate so as to cover the entire surface. Next, as shown in FIG. 3-2(10), a cavity is formed by blasting so that the conductive layer 4 formed by filling plating is exposed on the side surface 600 of the cavity. Then, as shown in FIG. 3-3(11), the resist mask for blasting is removed to form the printed wiring board A3 in the form shown in FIG. 2. Note that an opening may be formed that extends or branches from the outer shape of the cavity to a position away from the cavity, forming a conductive layer by filling plating (see FIG. 1). [Explanation of symbols]

[0026] 1 Cavity 2 Opening 3. Outline of the cavity 4 Conductor Layer 4a Exposed conductor layer on the side of the cavity 10 Insulating layer (core substrate) 20 Core substrate surface copper layer (3-layer substrate surface copper layer) 21 Copper layer on the back of the core substrate (3-layer board inner copper layer) 30 Insulating layer (prepreg material) 40 copper layer (3-layer board back copper layer) 100 Etching resist mask (surface) 101 Etching resist mask (back side) 200 Opening 300 Etching resist mask (surface) 301 Etching resist mask (back side) 400 Exposed insulation layer 500 Blasting resist mask (surface) 501 Blasting resist mask (back side) 600 Cavity Side A Core Base Material A3 Printed Wiring Board

Claims

1. A printed wiring board having three or more layers, A printed wiring board having a recessed cavity, a conductor layer partially exposed on the side of the cavity, the conductor layer being filled with plating, a copper layer and an insulating layer being disposed on the bottom surface of the cavity, and the conductor layer being in contact with the copper layer.

2. 2. The printed wiring board according to claim 1, wherein the conductor layer has a width of 40 to 60 μm.

3. 2. The printed wiring board according to claim 1, wherein the copper layer on the bottom surface of the cavity is divided into at least two parts.

4. 2. The printed wiring board according to claim 1, wherein the surface of the insulating layer on the bottom of the cavity is located lower than the surface of the copper layer on the bottom of the cavity.

5. A step of preparing a substrate having an insulating layer and a copper layer to become a printed wiring board; a step of removing the copper layer by etching at a portion of the surface of the base material that is in contact with the outside of an external shape of a position that will become a cavity, thereby forming an opening; forming an opening in the insulating layer exposed at the opening by laser processing the portion; forming a conductor layer by filling plating in the openings of the copper layer and the insulating layer; removing the copper layer at a position on the front surface side of the base material that will become a cavity; removing a portion of the copper layer by etching so that the copper layer at a position that will become a bottom surface of a cavity on the rear surface side of the base material is divided into at least two portions; forming a blast resist mask having an opening at a position to be a cavity on the front surface side of the base material, and forming a blast resist mask covering the entire surface on the back surface side of the base material; forming a cavity having at least two divided copper layers on a bottom surface of the cavity, the bottom surface being a side surface where the conductive layer formed by the filling plating is exposed, on the front surface side of the base material by blasting; A method for manufacturing a printed wiring board comprising the steps of:

6. 6. The method for producing a printed wiring board according to claim 5, wherein the conductive layer formed by the filling plating has a width of 40 to 60 μm.

Citation Information

Patent Citations

  • Manufacture of wiring board

    JP1998270829A