Secondary battery system

By integrating a fluorine-based liquid material with the sulfide solid electrolyte in the positive electrode active material layer and controlling charging to maintain high potentials, the secondary battery system effectively mitigates resistance increases, addressing the decomposition issue in conventional batteries.

JP2024146112AActive Publication Date: 2024-10-15TOYOTA JIDOSHA KK
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023058833
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15
Estimated Expiration
2043-03-31

AI Technical Summary

Technical Problem

Conventional secondary batteries exhibit increased resistance in high voltage regions, such as 4.3V (vs. Li/Li+) or higher, due to the decomposition of sulfide solid electrolytes.

Method used

Incorporating a fluorine-based liquid material, such as perfluoropolyether, into the positive electrode active material layer of a secondary battery, along with a sulfide solid electrolyte, and controlling the charging to maintain a positive electrode potential above 4.3V (vs. Li/Li+) to prevent direct contact and decomposition.

Benefits of technology

The integration of a fluorine-based liquid material suppresses the decomposition of the sulfide solid electrolyte, thereby reducing resistance increases at high potentials, ensuring stable battery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024146112000001_ABST
    Figure 2024146112000001_ABST
Patent Text Reader

Abstract

To provide a secondary battery containing sulfide solid electrolyte capable of suppressing the increase in resistance of the secondary battery in the high voltage range.SOLUTION: A disclosed secondary battery system includes a secondary battery and a control unit. The secondary battery includes a positive electrode active material layer, an electrolyte layer, and a negative electrode active material layer. The positive electrode active material layer contains a positive electrode active material, a sulfide solid electrolyte, and a fluorine-based liquid material. The control unit controls the charge of the secondary battery so that the positive electrode potential at the end of the charge of the secondary battery is 4.3 V (vs. Li / Li+) or more.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present application discloses a secondary battery system. [Background technology]

[0002] Patent Document 1 discloses that a sulfide solid electrolyte is used together with a positive electrode active material in a positive electrode active material layer of a secondary battery. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-125510 A Summary of the Invention [Problem to be solved by the invention]

[0004] Conventional secondary batteries are prone to an increase in resistance in the high voltage region (for example, 4.3 V (vs. Li / Li+) or higher). [Means for solving the problem]

[0005] The present application discloses the following aspects as means for solving the above problems. <Aspect 1> A secondary battery system comprising a secondary battery and a control unit, The secondary battery includes a positive electrode active material layer, an electrolyte layer, and a negative electrode active material layer, The positive electrode active material layer includes a positive electrode active material, a sulfide solid electrolyte, and a fluorine-based liquid material, The control unit controls charging of the secondary battery so that a positive electrode potential at a charge end potential of the secondary battery is 4.3 V (vs. Li / Li+) or higher. Secondary battery system. <Aspect 2> The secondary battery system of aspect 1, The positive electrode active material layer contains perfluoropolyether as the fluorine-based liquid material, Secondary battery system. <Aspect 3> Aspect 1 or 2 A secondary battery system, The positive electrode active material is a Li-containing oxide. Secondary battery system. <Aspect 4> A secondary battery system according to aspect 3, The Li-containing oxide contains at least one transition metal element selected from the group consisting of Mn, Ni, and Co. Secondary battery system. Effect of the Invention

[0006] According to the secondary battery system of the present disclosure, an increase in resistance of the secondary battery in a high voltage region is reduced. [Brief description of the drawings]

[0007] [Figure 1] 1 illustrates an example of a configuration of a secondary battery system. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, one embodiment of the secondary battery system of the present disclosure will be described, but the secondary battery system of the present disclosure is not limited to the embodiment described below.

[0009] As shown in Fig. 1, a secondary battery system 100 according to one embodiment includes a secondary battery 10 and a control unit 20. The secondary battery 10 includes a positive electrode active material layer 12, an electrolyte layer 13, and a negative electrode active material layer 14. The positive electrode active material layer 12 contains a positive electrode active material, a sulfide solid electrolyte, and a fluorine-based liquid material. The control unit 20 controls the charging of the secondary battery 10 so that the positive electrode potential at the end-of-charge potential of the secondary battery 10 is 4.3 V (vs. Li / Li+) or higher.

[0010] 1. Secondary battery The secondary battery 10 includes a positive electrode active material layer 12, an electrolyte layer 13, and a negative electrode active material layer 14. As shown in Fig. 1, the secondary battery 10 may also include a positive electrode current collector 11 in contact with the positive electrode active material layer 12. The secondary battery 10 may also include a negative electrode current collector 15 in contact with the negative electrode active material layer 14.

[0011] 1.1 Cathode active material layer The positive electrode active material layer 12 includes a positive electrode active material, a sulfide solid electrolyte, and a fluorine-based liquid material. The positive electrode active material layer 12 may also include a conductive assistant or a binder. The positive electrode active material layer 12 may also include other electrolytes. The content of each component in the positive electrode active material layer 12 may be appropriately determined according to the intended battery performance. For example, the positive electrode active material layer 12 may include 1 vol% or more and 25 vol% or less of the fluorine-based liquid material. The content of the fluorine-based liquid material included in the positive electrode active material layer 12 may be, for example, 1 vol% or more, 3 vol% or more, 5 vol% or more, 7 vol% or more, 8 vol% or more, 9 vol% or more, 10 vol% or more, 11 vol% or more, or 12 vol% or more, and may be 25 vol% or less, 24 vol% or less, 22 vol% or less, 20 vol% or less, 18 vol% or less, 16 vol% or less, 14 vol% or less, or 12 vol% or less. The volume ratio of the fluorine-based liquid material in the positive electrode active material layer 12 can be measured, for example, as follows. That is, the volume of the positive electrode active material layer 12 is measured in advance using an optical microscope or SEM. The volume of the fluorine-based liquid material contained in the positive electrode active material layer 12 may be specified by washing the positive electrode active material layer 12 with a solvent (one that can dissolve the fluorine-based liquid material and does not dissolve other electrode materials), recovering the filtrate in which the fluorine-based liquid material has been dissolved by suction filtration or the like, and analyzing the recovered solvent by GC-MS, or, if the boiling point of the solvent is significantly different from that of the fluorine-based liquid material, the volume of the fluorine-based liquid material may be directly measured by extracting the fluorine-based liquid material by distillation, for example. In this way, the volume ratio of the fluorine-based liquid material to the total volume of the positive electrode active material layer 12 measured in advance is calculated. Furthermore, the content of the positive electrode active material may be 40 mass% or more, 50 mass% or more, 60 mass% or more, or 70 mass% or more, or may be less than 100 mass%, 95 mass% or less, or 90 mass% or less, relative to 100 mass% of the total solid content of the positive electrode active material layer 12. Furthermore, the content of the sulfide solid electrolyte may be more than 0 mass%, 5 mass% or more, or 10 mass% or more, or may be 60 mass% or less, 50 mass% or less, 40 mass% or less, or 30 mass% or less, relative to 100 mass% of the total solid content of the positive electrode active material layer 12.Alternatively, taking the entire positive electrode active material layer 12 as 100% by volume, the positive electrode active material, the sulfide solid electrolyte, the fluorine-based liquid material, and optionally other electrolytes, conductive aids, and binders may be contained in a total amount of 85% by volume or more, 90% by volume or more, or 95% by volume or more, and the balance may be voids or other components. The shape of the positive electrode active material layer 12 is not particularly limited, and may be, for example, a sheet shape having a substantially flat surface. The thickness of the positive electrode active material layer 12 is not particularly limited, and may be, for example, 0.1 μm or more, 1 μm or more, or 10 μm or more, and may also be 2 mm or less, 1 mm or less, or 500 μm or less.

[0012] 1.1.1 Positive Electrode Active Material The positive electrode active material may be, for example, at least one selected from Li-containing compounds, elemental sulfur, sulfur compounds, etc. In particular, when the positive electrode active material contains a Li-containing compound, a higher effect is more easily obtained. The positive electrode active material may be used alone as one kind, or two or more kinds may be used in combination. In one embodiment, the positive electrode active material may be a Li-containing oxide. The Li-containing oxide may contain at least one element M, Li, and O. The element M may be, for example, at least one selected from Mn, Ni, Co, Al, Mg, Ca, Sc, V, Cr, Cu, Zn, Ga, Ge, Y, Zr, Sn, Sb, W, Pb, Bi, Fe, and Ti, and may also be at least one selected from the group consisting of Mn, Ni, Co, Al, Fe, and Ti. More specifically, the Li-containing oxide is lithium cobaltate, lithium nickelate, lithium manganate, lithium nickel cobaltate, lithium nickel manganate, lithium cobalt manganate, lithium nickel cobalt manganate (Li 1±α Ni x Co y Mn z O 2±δ (for example, 0 < x < 1, 0 < y < 1, 0 < z < 1, x + y + z = 1), spinel-type lithium compound (Li 1+x Mn 2-x-y M yLi-Mn spinel substituted with different elements having a composition represented by the formula: O4 (M is one or more selected from Al, Mg, Co, Fe, Ni, and Zn), etc.), lithium nickel cobalt aluminate (for example, Li 1±α Ni p Co q Al r O 2±δ (e.g., p+q+r=1), lithium titanate, lithium metal phosphate (LiMPO4, etc., M is one or more selected from Fe, Mn, Co, and Ni), and the like. In particular, when the Li-containing oxide as the positive electrode active material contains at least one transition metal element selected from Mn, Ni, and Co as a constituent element, higher performance is likely to be obtained. Alternatively, when the positive electrode active material contains at least one element selected from Ni, Co, and Al as a constituent element, higher performance is likely to be obtained. The shape of the positive electrode active material is not particularly limited, and may be, for example, particulate. The positive electrode active material particles may be solid particles, hollow particles, or particles having voids. The positive electrode active material particles may be primary particles, or may be secondary particles formed by agglomeration of a plurality of primary particles. The average particle diameter (D50) of the positive electrode active material particles may be, for example, 1 nm or more and 500 μm or less. The lower limit may be 5 nm or more or 10 nm or more, and the upper limit may be 100 μm or less, 50 μm or less, or 30 μm or less. In this application, the average particle size D50 refers to the particle size (median size) at an integrated value of 50% in a volume-based particle size distribution determined by a laser diffraction / scattering method.

[0013] A protective layer containing an ion-conductive oxide may be formed on the surface of the positive electrode active material. This makes it easier to suppress the reaction between the positive electrode active material and the sulfide solid electrolyte. Examples of the ion-conductive oxide include Li3BO3, LiBO2, Li2CO3, LiAlO2, Li4SiO4, Li2SiO3, Li3PO4, Li2SO4, Li2TiO3, and Li4Ti5O 12, Li2Ti2O5, Li2ZrO3, LiNbO3, Li2MoO4, Li2WO4, etc. The ion conductive oxide may be one in which some elements are replaced with a doping element such as P or B. The coverage (area ratio) of the protective layer to the surface of the positive electrode active material may be, for example, 70% or more, 80% or more, or 90% or more. The thickness of the protective layer may be, for example, 0.1 nm or more or 1 nm or more, and may be 100 nm or less, or 20 nm or less.

[0014] 1.1.2 Sulfide solid electrolyte The sulfide solid electrolyte may be any known solid electrolyte having lithium ion conductivity. The sulfide solid electrolyte may be a glass-based sulfide solid electrolyte (sulfide glass), a glass ceramic-based sulfide solid electrolyte, or a crystalline sulfide solid electrolyte. When the sulfide solid electrolyte has a crystalline phase, examples of the crystalline phase include a Thio-LISICON-type crystalline phase, a LGPS-type crystalline phase, and an Argyrodite-type crystalline phase. The sulfide solid electrolyte may contain, for example, a Li element, an X element (X is at least one of P, As, Sb, Si, Ge, Sn, B, Al, Ga, and In), and an S element. In particular, the sulfide solid electrolyte containing Li, P, and S as constituent elements has high performance. In addition, the sulfide solid electrolyte may further contain at least one of an O element and a halogen element. In particular, the sulfide solid electrolyte containing Li, P, S, and a halogen element as constituent elements has high performance. The composition of the sulfide solid electrolyte is not particularly limited, but examples thereof include xLi2S·(100-x)P2S5 (70≦x≦80), yLiI·zLiBr·(100-yz)(xLi2S·(1-x)P2S5) (0.7≦x≦0.8, 0≦y≦30, 0≦z≦30), etc. Alternatively, the sulfide solid electrolyte may be represented by the general formula: Li 4-x Ge 1-x P xIt may have a composition represented by S4(0 < x < 1). In the above general formula, at least a part of Ge may be substituted with at least one of Sb, Si, Sn, B, Al, Ga, In, Ti, Zr, V, and Nb. In the above general formula, at least a part of P may be substituted with at least one of Sb, Si, Sn, B, Al, Ga, In, Ti, Zr, V, and Nb. In the above general formula, a part of Li may be substituted with at least one of Na, K, Mg, Ca, and Zn. In the above general formula, a part of S may be substituted with a halogen (at least one of F, Cl, Br, and I). Alternatively, the sulfide solid electrolyte is Li 7-a PS 6-a X a (X is at least one of Cl, Br, and I, and a is a number of 0 or more and 2 or less) and may have a composition represented by. a may be 0, or may be greater than 0. In the latter case, a may be 0.1 or more, may be 0.5 or more, or may be 1 or more. Also, a may be 1.8 or less, may be 1.5 or less. The shape of the sulfide solid electrolyte is not particularly limited, and for example, it may be particulate. Only one kind of sulfide solid electrolyte may be used alone, or two or more kinds may be used in combination.

[0015] 1.1.3 Fluorine-based liquid materials The fluorine-based liquid material is a liquid material containing fluorine as a constituent element. According to the findings of the present inventor, in the positive electrode active material layer 12, the fluorine-based liquid material is present at the interface between the positive electrode active material and the sulfide solid electrolyte. That is, the fluorine-based liquid material suppresses direct contact between the positive electrode active material and the sulfide solid electrolyte. As a result, even if the positive electrode potential becomes high, the sulfide solid electrolyte is less likely to be exposed to the high potential, and decomposition of the sulfide solid electrolyte is suppressed. As a result, even if the positive electrode potential becomes high, the increase in resistance of the secondary battery 10 is reduced. In addition, the fluorine-based liquid material has low reactivity with other battery materials. Therefore, even if the positive electrode active material layer 12 contains a fluorine-based liquid material, the positive electrode active material, the sulfide solid electrolyte, and the like can exist stably. The fluorine-based liquid material may be, for example, an organic fluorine compound in which fluorine is bonded to a carbon chain. For example, the positive electrode active material layer 12 may contain perfluoropolyether as the fluorine-based liquid material. Since perfluoropolyether as a fluorine-based liquid material has an ether bond, it is considered to have a high affinity for the surfaces of other battery materials, and it is considered that it can be appropriately present, for example, in gaps between active material materials, gaps between sulfide solid electrolyte materials, and gaps between active material materials and sulfide solid electrolyte materials. This further suppresses direct contact between the positive electrode active material and the sulfide solid electrolyte. In addition, as described above, perfluoropolyether has low reactivity with other battery materials.

[0016] The positive electrode active material layer 12 may contain, as a fluorine-based liquid material, a perfluoropolyether represented by the following formula (1). E1-Rf1-R F -O-Rf2-E2(1) [In formula (1), Rf1 and Rf2 each independently represent a C1-16 divalent alkylene group optionally substituted by one or more fluorine atoms, E1 and E2 are each independently a monovalent group selected from the group consisting of a fluorine group, a hydrogen group, a hydroxyl group, an aldehyde group, a carboxylic acid group, a C1-10 alkyl ester group, an amide group which may have one or more substituents, and an amino group which may have one or more substituents; R F is a divalent fluoropolyether group.

[0017] In the above formula (1), Rf1 and Rf2 are each independently a C1-16 divalent alkylene group optionally substituted with one or more fluorine atoms. In one embodiment, the "C1-16 divalent alkylene group" in the C1-16 divalent alkylene group optionally substituted with one or more fluorine atoms may be linear or branched, preferably a linear or branched C1-6 alkyl alkylene group, particularly a C1-3 alkylene group, more preferably a linear C1-6 alkylene group, particularly a C1-3 alkylene group. In one embodiment, the "C1-16 divalent alkylene" in the C1-16 divalent alkylene group optionally substituted by one or more fluorine atoms may be linear or branched, and is preferably a linear or branched C1-6 fluoroalkylene group, in particular a C1-3 fluoroalkylene group, specifically -CF2CH2- and -CF2CF2CH2-, and more preferably a linear C1-6 perfluoroalkylene group, in particular a C1-3 perfluoroalkylene group, specifically a group selected from the group consisting of -CF2-, -CF2CF2- and -CF2CF2CF2-.

[0018] In the above formula (1), E1 and E2 are each independently a monovalent group selected from the group consisting of a fluorine group, a hydrogen group, a hydroxyl group, an aldehyde group, a carboxylic acid group, a C1-10 alkyl ester group, an amide group which may have one or more substituents, and an amino group which may have one or more substituents. As described above, perfluoropolyether has low reactivity with the sulfide solid electrolyte described below. Therefore, even when perfluoropolyether comes into contact with a sulfide solid electrolyte, the ion conductivity is unlikely to decrease due to alteration or deterioration of the sulfide solid electrolyte. In particular, when the perfluoropolyether has a non-polar group as an end group, the reaction between the perfluoropolyether and the sulfide solid electrolyte is further suppressed, and even higher effects can be expected. In this regard, the above E1 and E2 are each independently preferably a fluorine group. In one embodiment, E1-Rf1 and E2-Rf2 may each independently be a group selected from the group consisting of -CF3, -CF2CF3, and -CF2CF2CF3.

[0019] In the above formula (1), R F R is independently at each occurrence a divalent fluoropolyether group. F is preferably represented by formula (2): -(OC6F 12 ) a -(OC5F 10 ) b -(OC4F8) c -(OC3R Fa 6) d -(OC2F4) e -(OCF2) f - (2) [In formula (2): R Fa is independently at each occurrence a hydrogen atom, a fluorine atom, or a chlorine atom; a, b, c, d, e, and f each independently represent an integer of 0 to 200; the sum of a, b, c, d, e, and f is greater than or equal to 1; The order of occurrence of each repeating unit enclosed in parentheses with a, b, c, d, e, or f is arbitrary in the formula, However, all RFa is a hydrogen atom or a chlorine atom, at least one of a, b, c, e and f is 1 or greater.] R is a group represented by the formula: Fa is preferably a hydrogen atom or a fluorine atom, more preferably a fluorine atom. a, b, c, d, e and f may each independently be an integer of 0 to 100. The sum of a, b, c, d, e and f is preferably 5 or more, more preferably 10 or more, for example 15 or more or 20 or more. The sum of a, b, c, d, e and f is preferably 200 or less, more preferably 100 or less, further preferably 60 or less, for example 50 or less or 30 or less.

[0020] These repeating units may be linear or branched. F In the formula, the ratio of d to f (hereinafter referred to as "d / f ratio") may be 0.5 to 4, preferably 0.6 to 3, more preferably 0.7 to 2, and even more preferably 0.8 to 1.4. By making the d / f ratio 4 or less, the lubricity and chemical stability are further improved. The smaller the d / f ratio, the more the lubricity is improved. On the other hand, by making the d / f ratio 0.5 or more, the stability of the compound can be further increased. The larger the d / f ratio, the more the stability of the fluoropolyether structure is improved. In this case, the value of f is preferably 0.8 or more. In the above, R F The number average molecular weight of the portion is not particularly limited, but is, for example, 500 to 30,000, preferably 1,500 to 30,000, and more preferably 2,000 to 10,000. F The number average molecular weight of 19 This is a value measured by F-NMR.

[0021] 1.1.4 Other ingredients The other electrolyte that may be included in the positive electrode active material layer 12 may be a solid electrolyte, a liquid electrolyte (electrolytic solution), or a combination thereof. The solid electrolyte may be an inorganic solid electrolyte or an organic polymer electrolyte. Examples of inorganic solid electrolytes other than the sulfide solid electrolyte include oxide solid electrolytes, halide solid electrolytes, and complex hydride solid electrolytes. The electrolytic solution may be, for example, a carbonate-based solvent in which a lithium salt is dissolved at a predetermined concentration. Examples of the carbonate-based solvent include fluoroethylene carbonate (FEC), ethylene carbonate (EC), and dimethyl carbonate (DMC). Examples of the lithium salt include lithium amide salts such as LiTFSI and LiFSI, and LiPF6.

[0022] Examples of the conductive assistant that may be included in the positive electrode active material layer 12 include carbon materials such as vapor grown carbon fiber (VGCF), acetylene black (AB), ketjen black (KB), carbon nanotubes (CNT), and carbon nanofibers (CNF); and metal materials such as nickel, aluminum, and stainless steel. The conductive assistant may be, for example, particulate or fibrous, and the size is not particularly limited. Only one type of conductive assistant may be used alone, or two or more types may be used in combination.

[0023] Examples of binders that can be included in the positive electrode active material layer 12 include butadiene rubber (BR)-based binders, butylene rubber (IIR)-based binders, acrylate butadiene rubber (ABR)-based binders, styrene butadiene rubber (SBR)-based binders, polyvinylidene fluoride (PVdF)-based binders, polytetrafluoroethylene (PTFE)-based binders, polyimide (PI)-based binders, etc. Only one type of binder may be used alone, or two or more types may be used in combination.

[0024] 1.2 Electrolyte layer The electrolyte layer 13 is disposed between the positive electrode active material layer 12 and the negative electrode active material layer 14, and can function as a separator. The electrolyte layer 13 includes at least an electrolyte, and may further include a binder or the like. For example, the electrolyte layer 13 may include the above-mentioned sulfide solid electrolyte. The electrolyte layer 13 may further include other components such as a dispersant or the above-mentioned fluorine-based liquid material. The content of each component in the electrolyte layer 13 is not particularly limited, and may be appropriately determined according to the intended battery performance. The shape of the electrolyte layer 13 is not particularly limited, and may be, for example, a sheet having a substantially flat surface. The thickness of the electrolyte layer 13 is not particularly limited, and may be, for example, 0.1 μm or more or 1 μm or more, and may be 2 mm or less or 1 mm or less.

[0025] 1.3 Negative electrode active material layer The negative electrode active material layer 14 includes at least a negative electrode active material, and may further include an electrolyte, a conductive assistant, a binder, and the like. The negative electrode active material layer 14 may also include various additives. The negative electrode active material may be appropriately selected from known active materials such as silicon-based active materials, carbon-based active materials, and oxide-based active materials. The content of each component in the negative electrode active material layer 14 may be appropriately determined according to the intended battery performance. For example, the total solid content of the negative electrode active material layer 14 is taken as 100 mass%, and the content of the negative electrode active material may be 40 mass% or more, 50 mass% or more, 60 mass% or more, or 70 mass% or more, or 100 mass% or less, 95 mass% or less, or 90 mass% or less. The shape of the negative electrode active material layer is not particularly limited, and may be, for example, a sheet-like negative electrode active material layer having a substantially flat surface. The thickness of the negative electrode active material layer 14 is not particularly limited, and may be, for example, 0.1 μm or more, 1 μm or more, or 10 μm or more, and may be 2 mm or less, 1 mm or less, or 500 μm or less.

[0026] 1.4 Other configurations The positive electrode collector 11 and the negative electrode collector 15 of the secondary battery 10 can be any of those generally used as collectors for secondary batteries. The secondary battery 10 may be one in which each of the above-mentioned components is housed inside an exterior body. Any of the exterior bodies known as exterior bodies for batteries can be used as the exterior body. In addition, a plurality of secondary batteries 10 may be electrically connected and stacked in any manner to form an assembled battery. In this case, the assembled battery may be housed inside a known battery case. The secondary battery 10 may also have other obvious configurations such as necessary terminals. Examples of the shape of the secondary battery 10 include a coin type, a laminate type, a cylindrical type, and a square type. The secondary battery 10 can be manufactured by a method such as that disclosed in Patent Document 1 (JP Patent Publication No. 2019-125510), etc., except that the positive electrode active material layer 12 contains a fluorine-based liquid material together with the above-mentioned positive electrode active material and sulfide solid electrolyte. That is, each layer constituting the secondary battery 10 may be manufactured by wet molding, dry molding, or the like.

[0027] 2. Control Unit 1, the secondary battery system 100 includes a control unit 20. The control unit 20 is not particularly limited in configuration as long as it is capable of controlling the charging and discharging of the secondary battery 10. The control unit 20 includes a known configuration required for controlling the charging and discharging of the secondary battery 10, and may include, for example, a CPU, a RAM, a ROM, and the like.

[0028] The control unit 20 controls the charging of the secondary battery 10 so that the positive electrode potential at the end-of-charge potential of the secondary battery 10 is 4.3 V (vs. Li / Li+) or more. When a conventional secondary battery is charged until the positive electrode potential becomes a high potential of 4.3 V (vs. Li / Li+) or more, decomposition of the sulfide solid electrolyte occurs, and the resistance of the secondary battery is likely to increase. In contrast, in the secondary battery system 100 according to the present embodiment, as described above, the positive electrode active material layer 12 of the secondary battery 10 contains a fluorine-based liquid material in addition to the positive electrode active material and the sulfide solid electrolyte, so that even when the positive electrode potential of the secondary battery 10 becomes a high potential of 4.3 V (vs. Li / Li+) or more, decomposition of the sulfide solid electrolyte is likely to be suppressed, and an increase in the resistance of the secondary battery 10 is likely to be reduced.

[0029] The control unit 20 may control the charging of the secondary battery 10 so that the positive electrode potential at the end-of-charge potential of the secondary battery 10 is 4.4 V (vs. Li / Li+) or more, 4.5 V (vs. Li / Li+) or more, 4.6 V (vs. Li / Li+) or more, or 4.7 V (vs. Li / Li+) or more. The upper limit of the end-of-charge potential is not particularly limited. For example, the control unit 20 may control the charging of the secondary battery 10 so that the positive electrode potential at the end-of-charge potential of the secondary battery 10 is 4.3 V (vs. Li / Li+) or more and 5.0 V (vs. Li / Li+) or less. As described above, the control unit 20 controls the charging of the secondary battery 10, but may also control the discharging of the secondary battery 10 in addition to the charging. The discharge end potential of the secondary battery 10 may be appropriately determined according to the performance of the secondary battery 10, etc. EXAMPLES

[0030] The technology of the present disclosure will be described in more detail below with reference to examples, but the technology of the present disclosure is not limited to the following examples.

[0031] 1. Preparation of Positive Electrode 1.1 Examples 1 to 4, Comparative Examples 7 and 8 In an organic solvent, a binder (PVdF), a conductive additive (VGCF), a sulfide solid electrolyte (LiI-LiBr-Li2S-P2S5), and a positive electrode active material (LiNi1 / 3 Co 1 / 3 Mn 1 / 3 A positive electrode composite slurry was obtained by kneading a mixture of 02) and perfluoropolyether (PFPE, Perfluoro(polyoxypropylene ethyl ether) 2700 manufactured by Fujifilm Wako Pure Chemical Industries, Ltd., using an ultrasonic homogenizer. The obtained positive electrode composite slurry was applied onto an Al foil and dried to obtain a positive electrode for pressing, which had a positive electrode active material layer on an Al foil as a positive electrode current collector. Here, the volume ratio of PFPE in the composite was set to 8 volume %.

[0032] 1.2 Comparative Examples 1 to 6 Positive electrodes for pressing were obtained in the same manner as in Examples 1 to 4 and Comparative Examples 7 and 8, except that PFPE was not added to the positive electrode mixture.

[0033] 2. Preparation of the Electrolyte Layer A binder (PVdF) and a sulfide solid electrolyte (LiI-LiBr-Li2S-P2S5) were added to an organic solvent and mixed using an ultrasonic homogenizer to obtain an electrolyte mixture slurry. The obtained electrolyte mixture slurry was applied onto an Al foil and dried to form a solid electrolyte layer on the Al foil substrate.

[0034] 3. Battery Preparation The positive electrode for pressing was cut into a rectangular shape. The cut positive electrode active material layer and the solid electrolyte layer were overlapped and roll pressed at 165°C with a pressure of 50 kN / cm, and the Al foil as the substrate was peeled off to transfer the solid electrolyte layer to the surface of the positive electrode active material layer. A Li foil punched to φ13.00 mm was overlapped on the surface of the solid electrolyte layer to obtain a laminate having a configuration of Al foil / positive electrode active material layer / solid electrolyte layer / Li foil. A current extraction tab was attached to the laminate, and the laminate was sealed in an aluminum laminate using a vacuum lami sealer to prepare a battery for evaluation.

[0035] 4. Battery performance evaluation The prepared batteries were charged to the end-of-charge voltage (upper limit voltage), and trickle tests were performed at the upper limit voltages (maintained at each upper limit voltage for one week), and the resistance values ​​before and after the trickle tests were measured. Specifically, the voltage of each battery before and after the trickle test was adjusted to 3.7V, and the resistance value was calculated from the voltage drop after 5 seconds when the battery was discharged at a 5C rate. The resistance value after the trickle test was measured relative to the resistance value before the trickle test, and this was taken as the resistance increase rate. The results are shown in Table 1 below. In Table 1 below, the resistance increase rate for Comparative Example 1 is taken as the reference (100%), and the resistance increase rates for Comparative Examples 2 to 8 and Examples 1 to 4 are shown relative to each other.

[0036] [Table 1]

[0037] As is clear from the results shown in Table 1, when the positive electrode active material layer contains a sulfide solid electrolyte together with the positive electrode active material and does not contain PFPE (Comparative Examples 1 to 6), the resistance of the battery does not increase even after the trickle test when the positive electrode potential in the trickle test is less than 4.3 V (vs. Li / Li+) (Comparative Examples 1 and 2), whereas the resistance of the battery increases after the trickle test when the positive electrode potential in the trickle test is 4.3 V (vs. Li / Li+) or more (Comparative Examples 3 to 6). In Comparative Examples 3 to 6, it is believed that the sulfide solid electrolyte was exposed to a high potential, causing the sulfide solid electrolyte to decompose, resulting in an increase in the resistance of the battery.

[0038] On the other hand, when the positive electrode active material layer contains a sulfide solid electrolyte together with the positive electrode active material and also contains PFPE (Comparative Examples 7 and 8, Examples 1 to 4), when the positive electrode potential in the trickle test is less than 4.3 V (vs. Li / Li+), the advantageous effect of including PFPE is not particularly exhibited (Comparative Examples 1 and 2 and Comparative Examples 7 and 8). On the other hand, when the positive electrode potential in the trickle test is 4.3 V (vs. Li / Li+) or more, it is found that the inclusion of PFPE can suppress the increase in the resistance of the battery (Comparative Examples 3 to 6 and Examples 1 to 4). In Examples 1 to 4, the PFPE suppresses direct contact between the positive electrode active material and the sulfide solid electrolyte, and even when the positive electrode potential becomes high, the sulfide solid electrolyte is less likely to be exposed to high potential, and the decomposition of the sulfide solid electrolyte is suppressed, and as a result, it is considered that the increase in the resistance of the battery is reduced even when the positive electrode potential becomes high.

[0039] 5. Supplementary Information In the above embodiment, a specific PFPE is exemplified as the fluorine-based liquid material, but the type of the fluorine-based liquid material is not limited to the PFPE. In addition, in the above embodiment, a specific battery material (NCM as the positive electrode active material, LiI-LiBr-Li2S-P2S5 as the sulfide solid electrolyte, PVdF as the binder, VGCF as the conductive additive, and Li foil as the negative electrode active material) is used as an example, but even if a battery material other than these is used, it is considered that the above effect can be achieved by using a fluorine-based liquid material together with the positive electrode active material and the sulfide solid electrolyte in the positive electrode active material layer.

[0040] 6. Summary From the above results, it can be said that a secondary battery system having the following configuration can reduce an increase in resistance of the secondary battery in a high potential region. (1) The secondary battery system includes a secondary battery and a control unit. (2) The secondary battery includes a positive electrode active material layer, an electrolyte layer, and a negative electrode active material layer. (3) The positive electrode active material layer includes a positive electrode active material, a sulfide solid electrolyte, and a fluorine-based liquid material. (4) The control unit controls charging of the secondary battery so that the positive electrode potential at the end-of-charge potential of the secondary battery is 4.3 V (vs. Li / Li+) or higher. [Explanation of symbols]

[0041] 100 Secondary battery system 10 Secondary battery 11 Positive electrode current collector 12 Cathode active material layer 13 Electrolyte layer 14 Negative electrode active material layer 15 Negative electrode current collector 20 Control section

Claims

1. A secondary battery system comprising a secondary battery and a control unit, The secondary battery includes a positive electrode active material layer, an electrolyte layer, and a negative electrode active material layer, The positive electrode active material layer includes a positive electrode active material, a sulfide solid electrolyte, and a fluorine-based liquid material, The control unit controls charging of the secondary battery so that a positive electrode potential at a charge end potential of the secondary battery is 4.3 V (vs. Li / Li+) or more. Secondary battery system.

2. The secondary battery system according to claim 1 , The positive electrode active material layer contains perfluoropolyether as the fluorine-based liquid material, Secondary battery system.

3. The secondary battery system according to claim 1 or 2, The positive electrode active material is a Li-containing oxide. Secondary battery system.

4. The secondary battery system according to claim 3, The Li-containing oxide contains at least one transition metal element selected from the group consisting of Mn, Ni, and Co. Secondary battery system.

Citation Information

Patent Citations

  • Novel solid-liquid battery with lithium metal negative electrode and high-voltage positive electrode

    CN110931843A

  • Lithium composite metal oxide, cathode active material, cathode and nonaqueous electrolyte secondary battery

    JP2016185905A

  • Lithium ion secondary battery

    WO2014080870A1

  • Inorganic solid electrolyte-containing composition, sheet for all-solid secondary batteries, electrode sheet for all-solid secondary batteries, all-solid secondary battery, method for manufacturing sheet for all-solid secondary batteries, and method for manufacturing all-solid secondary battery

    WO2021060541A1

  • Positive electrode mixture for all-solid battery, positive electrode for all-solid battery, all-solid battery and manufacturing methods thereof

    JP2019125510A