Film inspection device
The film inspection device addresses the inadequacies of conventional methods by using a roll with a cylindrical metal on an elastic layer to apply pressure and generate electrical discharge, ensuring rapid and precise detection of defects in resin films.
Patent Information
- Application Number
- JP2023059206
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-03-31
AI Technical Summary
Conventional methods for inspecting resin films for defects such as foreign matter and pinholes are inadequate in reducing roll resistance and accurately detecting defective areas.
A film inspection device that nips a resin film between a pair of rolls, one of which has a cylindrical metal on an elastic layer, allowing for precise application of pressure and electrical discharge to detect defects.
Enables quick and accurate detection of defects over the entire length of the resin film, preventing damage and ensuring reliable identification of foreign matter and pinholes.
Smart Images

Figure 2024146360000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an inspection device that inspects resin films molded into a strip for the presence of defects such as the attachment of foreign matter or pinholes, and in particular to a film inspection device that can detect the presence of defects while nipping and running a film between a pair of conductive rolls to which a predetermined voltage is applied. [Background technology]
[0002] Resin films (including porous resin films) are used for a wide variety of purposes, such as packaging materials, electrical insulating materials (separators for electrochemical elements, etc.), metal deposition materials, plate-making materials, magnetic recording materials, display materials, transfer materials, window lining materials, display materials, and health care materials.
[0003] As an example of a resin film for a separator in an electrochemical element, a porous resin film mainly composed of polyolefin is used alone or in the form of a laminate in which a coating film of inorganic particles or the like is laminated.
[0004] However, if metal powder or other foreign matter adheres to or is mixed into the resin film, or if defects such as pinholes are formed, the electrical insulation cannot be maintained at these defective areas, or the insulating material may be damaged during the molding of electrochemical elements, causing the film to be unable to be used for its intended purposes.
[0005] A method for inspecting defective parts in such resin films is a voltage resistance test (insulation defect detection). In a voltage resistance test, electrodes are placed on both sides of the resin film and a high voltage is applied between the electrodes, and the presence of defects such as foreign matter or pinholes is detected by the current flowing in the location of the defect. In such a voltage resistance test, a method has been proposed in which the resin film is nipped between a metal roll and a conductive elastic roll, and a voltage is applied between the rolls while the film is running to detect defective parts, and the running of the material is stopped to detect or remove the defective parts (see Patent Document 1). [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Japanese Patent Application Publication No. 9-229907 Summary of the Invention [Problem to be solved by the invention]
[0007] The conventional defect inspection method described in the above Patent Document 1 can inspect a strip-shaped resin film while it is nipped and running in the longitudinal direction, making it possible to detect defective parts that occur after the pressing process, while keeping the size of fracture holes that occur in the defective parts small, and enabling inspection of a large-area resin film in a short time. Also, by making at least one surface of the rolls that nip the resin film a conductive elastic roll made of carbon-containing rubber, metal powder-containing rubber, carbon sheet, conductive plastic, or the like, it is possible to prevent the resin film from being damaged by protrusions or scratches on the roll surface that occur when the film runs between a pair of metal rolls.
[0008] However, the above-mentioned conventional inspection method has a problem in that it is not possible to sufficiently reduce the resistance value of the surface of the conductive elastic roll, and therefore it is not possible to inspect defective portions with high accuracy.
[0009] The present disclosure is intended to solve the above-mentioned conventional problems, and aims to realize a film inspection device that can quickly and accurately inspect for defective areas in a resin film over the entire length of the resin film. [Means for solving the problem]
[0010] In order to solve the above problems, the film inspection device disclosed in the present application is an inspection device that nip and run a resin film between a pair of rolls to which a predetermined voltage is applied, and is characterized in that one of the pair of rolls has a support, an elastic layer arranged on the support, and a cylindrical metal arranged on the surface of the elastic layer. Effect of the Invention
[0011] In the film inspection device disclosed in the present application, one of a pair of rolls to which a predetermined voltage is applied is a roll including a support, an elastic layer disposed on the support, and a cylindrical metal disposed on the surface of the elastic layer, so that a withstand voltage test can be performed in a state in which a predetermined pressure is applied to the resin film traveling between the rolls, and discharge can be generated in a portion of the resin film containing foreign matter, thereby making it possible to reliably detect defective portions. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a schematic diagram for explaining the overall configuration of a film inspection device. [Diagram 2] FIG. 4 is a schematic perspective view for explaining the shape of a roll that nips a resin film. [Diagram 3] 13 is a diagram illustrating the state after a voltage withstand test is performed by nipping a resin film on a portion where metal powder is present. FIG. [Figure 4] 13 is a diagram for explaining the state after a voltage resistance test is performed on a portion where metal powder is present without applying pressure to the resin film. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] The film inspection device disclosed in the present application is an inspection device that nip and run a resin film between a pair of rolls to which a predetermined voltage is applied, one of the pair of rolls comprising a support, an elastic layer disposed on the support, and a cylindrical metal disposed on the surface of the elastic layer.
[0014] In this way, the film inspection device disclosed in the present application can apply an appropriate amount of pressure to the resin film being inspected, thereby generating a discharge in areas where foreign matter such as metal powder is present, making it possible to reliably detect defective areas.
[0015] In the film inspection device having the above-mentioned configuration, it is preferable that the elastic layer is formed of silicone sponge rubber. In this way, the one roll having a metal cylinder disposed on its surface can be made into a metal-surfaced roll that applies an appropriate pressing force to the resin film and has durability.
[0016] It is also preferred that the cylindrical metal has a thickness of 0.05 mm to 0.3 mm and is bonded to the surface of the elastic layer, which makes it easy to place the metal cylinder on the surface of the elastic layer and prevents the metal cylinder from being displaced in the axial direction due to the running of the resin film.
[0017] In addition, it is preferable that the film inspection device further includes a defect inspection unit having an imaging unit that images the surface of the resin film that has run between the pair of rolls. In this way, it is possible to realize a film inspection device that can continuously perform a withstand voltage inspection and an optical inspection.
[0018] (Embodiment) Hereinafter, a film inspection device according to the present disclosure will be described with reference to the drawings.
[0019] FIG. 1 is a conceptual diagram illustrating the overall configuration of a film inspection device according to this embodiment.
[0020] As shown in FIG. 1, the inspection device 100 of this embodiment includes an unwinding roll 10, a voltage resistance inspection section 20, an optical inspection section 30, and a winding roll 40, and voltage resistance inspection and optical inspection are performed while the resin film 1 is run between the unwinding roll 10 and the winding roll 40 at a maximum speed of 200 m / min, for example.
[0021] In this embodiment, the resin film 1 to be inspected was four types of laminated films (separators for non-aqueous electrolyte secondary batteries), laminated films 1 to 4, which were formed by coating one surface of a polyolefin microporous film having a thickness of 9.5 to 19 μm and a porosity of approximately 50%, and an inorganic particle film having a thickness of 3 to 4.5 μm (proportion of boehmite particles: 95% by mass) in which boehmite particles were bonded with a resin binder, as shown in Table 1 below.
[0022] [Table 1]
[0023] In the voltage endurance testing section 20, a first roll 22 and a second roll 23 are arranged to sandwich the resinous film 1 that has passed through the position restricting rolls 21 from above and below, and the resinous film is nipped.
[0024] FIG. 2 shows an enlarged image diagram for explaining the configuration of the first roll 22 and the second roll 23 in the voltage resistance inspection section.
[0025] As shown in FIG. 2, in the withstand voltage inspection section 20 of the inspection device 100 according to this embodiment, the first roll 22 and the second roll 23 nip the resin film 1 to be inspected. In the inspection device according to this embodiment, the first roll 22 arranged above the resin film 1 to be inspected is a metal-surfaced rubber roll in which an elastic layer 22b is arranged on a support 22a and a metal cylinder 22c is bonded to the surface of the elastic layer 22b with an adhesive. On the other hand, the second roll 23 arranged below the resin film 1 is a stainless steel metal roll. In this embodiment, the linear pressure applied to the nipped resin film 1 is 8 g / mm and 150 g / mm, and measurements were performed under each condition.
[0026] The first roll, the metal-surfaced rubber roll 22, is made of a chrome-plated nickel support 22a having a diameter of 75.3 mm, on which an elastic layer 22b made of silicon sponge rubber having a thickness of about 10 mm is placed, and a metal cylinder 22c having a thickness of 0.1 mm is placed on the surface of this elastic layer 22b, and the metal cylinder 22c is bonded to the surface of the elastic layer 22b with a silicon-based adhesive, thereby preventing the metal cylinder 22c from shifting in the axial direction of the metal-surfaced roll 22 when the resin film 1 is run. The metal cylinder 22c and the second roll 23 are electrically connected to high-voltage power sources provided in the voltage resistance test section 20 so that discharge can be performed between them.
[0027] The support 22a including the central shaft portion can be made of a material having high rigidity and high conductivity, such as metals such as iron and aluminum alloys, carbon fiber reinforced plastics, etc., in addition to the above-mentioned stainless steel. If the diameter of the support 22a is large, the weight of the support 22a can be reduced by making the inside hollow.
[0028] The elastic layer 22b may be made of a foam such as acrylonitrile butadiene rubber, ethylene propylene rubber, chloroprene rubber, or urethane rubber, in addition to the above-mentioned silicone sponge rubber. The elastic layer 22b preferably has a Poisson's ratio of 0.4 or less, and more preferably has a Poisson's ratio of 0.2 or less. The thickness of the elastic layer 22b is preferably 3 mm or more and 15 mm or less.
[0029] In addition, an intermediate layer formed by molding ebonite, FRP, rubber, resin, etc. can be placed between the support body 22a and the elastic layer 22b. By placing the intermediate layer, the adhesion between the support body 22a and the elastic layer 22b can be improved.
[0030] Metal cylinder 22c can be a metal sleeve having a thickness of 0.05 mm to 0.3 mm and made of nickel, stainless steel, chromium, etc. By making the surface of metal cylinder 22c have a maximum thickness (JIS B 0601:2013) Rz of 0.2 μm or less, it is possible to prevent the surface smoothness of nipped resin film 1 from being impaired.
[0031] The elastic layer 22b and the metal cylinder 22c can be bonded together by applying a silicone adhesive to the surface of the elastic layer 22b and then inserting the contracted elastic layer 22b into the metal cylinder 22c.
[0032] The second roll 23 can be made of metal such as stainless steel, iron, aluminum alloy, or carbon fiber reinforced plastic. The diameter of the second roll 23 used in the film inspection device according to this embodiment is 60 mm. The relationship between the diameter of the metal surface rubber roll 22 and the diameter of the second roll 23 can be approximately the same, or the diameter of the metal surface rubber roll 22 can be 1% to 20% larger than the diameter of the second roll 23. The roll diameters of the first roll and the second roll are preferably different from each other, and are also preferably different from the roll systems of other rolls provided in the inspection device. In this way, it becomes easy to determine which roll a defect occurring in a roll is caused by.
[0033] In the film inspection device 100 according to this embodiment, a voltage resistance test is performed by running the resinous film 1 at a predetermined speed (50 to 200 m / min, for example) while applying a predetermined voltage (0.5 to 1.6 kV, for example) between the metal-surfaced rubber roll 22 and the second roll. Although not shown in FIG. 1, the voltage resistance test section 20 is equipped with a detection mechanism that detects discharges occurring between the metal-surfaced rubber roll 22 and the second roll 23, and is capable of grasping the position at which a discharge has occurred on the running resinous film 1 as the running distance (i.e., the distance from the end on the running start side to the point where the discharge has occurred).
[0034] Table 2 shows examples of applied voltages that can correctly detect pinholes.
[0035] [Table 2]
[0036] Table 2 shows the range of voltage to be applied to the laminated film to obtain a result in which, when pinholes are formed at regular intervals in advance in the four types of laminated film (Laminated Film 1 to Laminated Film 4) shown in Table 1 above and the film is run at a speed of 200 m / min, a discharge always occurs at the position of the pinhole and no discharge occurs at a position where there is no pinhole, that is, to correctly identify and detect the pinhole. When the voltage applied to the laminated film is smaller than the range shown in Table 2, there were cases where no discharge occurred at one or more pinholes. On the other hand, when the applied voltage is larger than the range shown in Table 2, a discharge occurred at one or more positions where there is no pinhole.
[0037] As a result of the inventors' investigations, it was confirmed that defects in the resinous film 1 can be correctly detected by applying an appropriate voltage even when the resinous film is run at a speed of 200 m / min. Similar measurements were performed by changing the running speed of the resinous film 1 to 50 m / min, 100 m / min, and 150 m / min, and the range of applied voltage in which defects can be correctly detected was approximately the same as that in the case of running the resinous film 1 at 200 m / min shown in Table 2 above.
[0038] Since the resin film 1 is wound up in a roll, defective areas due to foreign matter contamination often appear periodically at specified intervals, and since the results of the inventors' verification described above are periodic, it can be determined that defective areas in the resin film have been correctly detected.
[0039] The resin film 1 is nipped between the metal-surfaced rubber roll 22 and the second roll, and then passes through a second regulating roll 24 and travels to an optical inspection section 30 .
[0040] In the optical inspection section 30, the surface condition of the resinous film 1 is observed by a camera 31 arranged on the upper side. Note that, in order to easily detect defective parts such as pinholes in the resinous film 1, an illumination device 32 is arranged opposite to the lens optical axis 33 of the camera 31 with the resinous film 1 in between.
[0041] In the optical inspection section 30, foreign matter such as metal powder recognized as black dots on the resin film and defects such as pinholes recognized as white dots can be detected according to the travel distance of the resin film based on images captured by the imaging section of the camera 31. In particular, by enlarging and analyzing images captured using a lens that is less likely to cause image distortion, such as a telecentric lens, through data processing, it is expected that metal foreign matter and defects of a size of about several tens of μm can be detected.
[0042] The resinous film 1 that has run through the optical inspection section 30 is sequentially wound around the take-up roll 40, whereupon the withstand voltage inspection and optical inspection are completed.
[0043] Here, a detection situation of foreign matter (metal powder) contained in a resin film in the film inspection device 100 shown in the above embodiment will be described.
[0044] Figure 3 is a micrograph showing the state of metal powder contained in a resin film and its surroundings when a voltage withstand test was performed by nipping the resin film between a pair of rolls at a linear pressure of 8 g / mm and running it at a speed of 200 m / min to which a voltage of 1.1 kV was applied.
[0045] FIG. 3(a) shows the results of observation of the metal powder by reflected light as viewed from the side on which the inorganic particle film was formed, FIG. 3(b) shows the results of observation of the metal powder by reflected light as viewed from the original film side, FIG. 3(c) shows the results of observation of the metal powder by transmitted light as viewed from the side on which the inorganic particle film was formed, and FIG. 3(d) shows the results of observation of the metal powder by transmitted light as viewed from the original film side. Each of FIG. 3(a) to FIG. 3(d) is image data captured by an optical microscope at 300x magnification. The thin lines shown in each figure are drawn to measure dimensions.
[0046] The granular matter indicated by the arrows in Figures 3(a) and 3(b) and the black parts in Figures 3(c) and 3(d) are metal powder, and the white parts next to the metal powder in Figures 3(c) and 3(d) are pinholes with a major axis of about 70 μm that were generated by heat generated when discharge occurred when the metal powder passed between the rolls. By generating discharge at the position of the metal powder and by generating pinholes next to the metal powder due to this discharge, the presence of foreign matter can be easily detected by using the inspection device of this embodiment.
[0047] FIG. 4 is a micrograph showing, as a comparative example, metal powder contained in a resin film and the state of its surroundings when a voltage resistance test was conducted by passing the resin film between rolls without nipping.
[0048] As in the figures in Fig. 3, Fig. 4(a) shows the results of observation of the metal powder by reflected light as viewed from the side on which the inorganic particle film was formed, Fig. 4(b) shows the results of observation of the metal powder by reflected light as viewed from the side on which the original film was formed, Fig. 4(c) shows the results of observation of the metal powder by transmitted light as viewed from the side on which the inorganic particle film was formed, and Fig. 4(d) shows the results of observation of the metal powder by transmitted light as viewed from the side on which the original film was formed. As in Fig. 3, the images shown are image data captured by an optical microscope at 300x magnification.
[0049] As shown in Fig. 4, it can be confirmed that no discharge occurred and no pinholes were generated even when a voltage of 1.1 kV, the same as that used in the voltage withstand test, was applied without nipping (without applying pressure). In the inventors' study, even when metal powder was mixed into the resin film, discharge was confirmed at the position of the metal powder in only two out of 450 locations without nipping. Therefore, it was confirmed that when inspecting without applying pressure, rather than nipping the resin film with a roll, as with the inspection device shown in this embodiment, the presence of foreign matter cannot be easily detected even if a high voltage is applied.
[0050] As described above, in the inspection device 100 according to the present embodiment, when inspecting a resin film by running it at 200 m / min, it was confirmed that it is possible to discharge at a portion where foreign matter such as metal powder exists on the resin film by setting the applied voltage to 1.1 kV when the linear pressure is 8 (g / mm). It was also confirmed that it is possible to discharge at a position where a fine defect such as a pinhole exists. Of course, it is necessary to adjust the linear pressure for nipping the resin film and the value of the voltage applied between the metal surface roll and the second roll according to the material, film thickness, laminated structure, and number of laminated layers of the resin film to be inspected, and according to the running speed of the resin film during inspection. However, it was confirmed that the inspection device according to the present embodiment can accurately detect foreign matter and defects existing on the resin film.
[0051] In addition, by using the above-mentioned metal-surfaced rubber roll as one of the two rolls when performing the voltage resistance test, it was confirmed that roll edge marks, which occur on the resin film when both rolls are metal rolls, do not occur. Furthermore, in the voltage resistance test using two metal rolls, it was confirmed that the roll jumps at the protruding parts, which are unmelted parts called wedges, contained in the resin film, but it was confirmed that such jumping does not occur when one of the rolls shown in this embodiment is a metal-surfaced rubber roll.
[0052] In the above embodiment, an inspection device equipped with both a charging inspection unit and an optical inspection unit is exemplified, but the optical inspection unit is not a required component of the inspection device disclosed in the present application, and the inspection device may have only a charging inspection unit.
[0053] Furthermore, unlike the inspection device described in the above embodiment, the inspection device disclosed in the present application can be incorporated as part of a resin film manufacturing device that applies a film made of specified inorganic particles to a resin substrate, rather than as an inspection device that re-inspects the manufactured resin film. This makes it possible to carry out the manufacturing and inspection of resin films in a seamless manner. [Industrial Applicability]
[0054] The film inspection device disclosed herein is extremely useful as an inspection device that can reliably detect defective areas such as foreign objects and defects while running the resin film at high speed, by making one of the rollers that nip the resin film to be inspected a roll with a metal cylinder arranged on the surface of the elastic layer. [Explanation of symbols]
[0055] 1 Plastic film 20. Voltage Testing Department 22 Metal surface rubber roll (first roll) 23 Second Roll 30 Optical Inspection Department 100 Film Inspection Equipment
Claims
1. An inspection device in which a resin film is nipped and run between a pair of rolls to which a predetermined voltage is applied, A film inspection device, wherein one of the pair of rolls comprises a support, an elastic layer disposed on the support, and a cylindrical metal disposed on the surface of the elastic layer.
2. 2. The film inspection device according to claim 1, wherein the elastic layer is made of silicone sponge rubber.
3. 2. The film inspection device according to claim 1, wherein the cylindrical metal has a thickness of 0.05 mm to 0.3 mm, and the cylindrical metal is adhered to the surface of the elastic layer.
4. 2. The film inspection device according to claim 1, further comprising a defect inspection unit having an imaging unit that images a surface of the resinous film that has run between the pair of rolls.
Citation Information
Patent Citations
JP1978013180U
Method and device for film defect inspection
JP1992069563A
Method and device for detecting insulation defect of electric insulation material
JP1997229907A
Defect detection device for nonwoven fabric
JP2015045511A
Inspection method of exterior film for electrochemical device
JP2016057271A