Low resistivity polycrystalline based substrate or wafer
Low resistivity and bow polycrystalline silicon carbide wafers, achieved by bonding techniques, address the issues of high resistivity and warpage in silicon carbide wafers, enhancing device functionality and reducing defects and costs.
Patent Information
- Application Number
- JP2024055150
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2024-03-22
- Filing Date
- 2024-03-29
- Publication Date
- 2024-10-16
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Silicon carbide wafers in the semiconductor industry face challenges with high resistivity and warpage, leading to defects and increased manufacturing costs due to cracked or broken wafers, which limit the functionality and efficiency of electronic devices.
Development of polycrystalline silicon carbide wafers with low resistivity (≤2 mohm-cm) and low bow (≤75 μm) by bonding a monocrystalline silicon carbide wafer to a polycrystalline silicon carbide wafer using surface-activated bonding techniques, optionally with conductive layers to enhance electrical conductivity and mechanical stability.
The solution reduces on-resistance, enhances signal transport efficiency, and minimizes mechanical and electrical defects, resulting in improved functionality and reduced manufacturing waste of electronic devices.
Smart Images

Figure 2024147519000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to silicon carbide based substrates and wafers having low resistivity and low warpage. [Background technology]
[0002] The semiconductor industry has shown considerable interest in silicon carbide (SiC), particularly for the manufacture of electronic devices or components such as diodes, transistors, or other similar power applications.
[0003] The development and manufacture of silicon carbide based electronic devices is limited by factors such as the electrical and mechanical properties from forming the silicon carbide wafer. Many manufactured silicon carbide wafers have a higher resistivity than is beneficial for the final product. Another issue is the amount of warpage resulting from the manufacture of the wafer. Higher resistivity limits the ability of electrical signals to travel through the silicon carbide wafer. Higher amounts of warpage can result in defects from polishing processes, etc., in manufacturing the final electronic device, or an increased number of cracked or broken wafers or substrates during processing and manufacture.
[0004] These polycrystalline SiC wafers can be manufactured by a method of bonding a monocrystalline wafer onto a polycrystalline SiC wafer. For example, there are wafer manufacturing methods in which a polycrystalline SiC wafer and a monocrystalline SiC wafer are bonded and integrated together by direct bonding. In power devices, these crystal defects, high resistivity, and high warpage can be problematic because these factors limit the functionality of the power devices, resulting in the power devices functioning outside of selected tolerances. In such situations, these devices can be discarded (e.g., scrapped), which increases manufacturing costs due to reduced yields. Summary of the Invention
[0005] A polycrystalline SiC wafer having low resistivity is beneficial to the function of the electronic device in which it resides. The present disclosure is directed to providing at least one embodiment of a wafer including a polycrystalline silicon carbide wafer or substrate having low resistivity and low bow. Electronic devices or components made from the wafer are more optimized in use and have fewer or no crystal defects. Wafers formed according to embodiments of the present disclosure have low or very low resistivity compared to existing SiC wafers.
[0006] At least one embodiment includes a wafer that includes a polycrystalline silicon carbide (SiC) wafer or substrate having a resistivity of 2 mohm-cm (milliohm-cm) or less and a bow of 75 μm (micrometers) or less. In some embodiments, the wafer may include a bond region between the polycrystalline silicon carbide (SiC) wafer and a single crystal silicon carbide (SiC) wafer, where the single crystal silicon carbide (SiC) wafer is bonded to the polycrystalline silicon carbide (SiC) wafer by the bond region. The low resistivity of the polycrystalline silicon carbide (SiC) wafer (e.g., 2 mohm-cm) reduces the "on" resistance (R on ) to improve the overall signal transport function and efficiency of a power device that includes the wafer or a portion of the wafer. The low bow of polycrystalline SiC wafers (e.g., 75 μm or less) reduces or prevents the possibility of mechanical or electrical defects in the bonding layer. The low bow of polycrystalline SiC wafers also reduces or prevents the possibility of mechanical or electrical defects between the bonding layer, the monocrystalline silicon carbide layer, and the polycrystalline silicon carbide layer. [Brief description of the drawings]
[0007] For a better understanding of the embodiments, reference will now be made, by way of example, to the accompanying drawings, in which like reference numbers identify the same or similar elements or acts, unless the context otherwise dictates. The sizes and relative proportions of elements in the drawings are not necessarily drawn to scale. For example, some of these elements may be enlarged and positioned to improve the readability of the drawings. [Figure 1] 1A and 1B depict a perspective side view of an embodiment of a wafer of the present disclosure. [Diagram 2] 1A-1C depict perspective side views of alternative embodiments of the wafer of the present disclosure. [Diagram 3] 2 is a perspective side view of an embodiment of a polycrystalline layer or substrate utilized in an embodiment of a wafer such as that shown in FIG. 1 or within an alternative embodiment of a wafer such as that shown in FIG. [Figure 4] 4 is an enhanced enlarged view of cross section 4-4 as shown in FIG. 1 of an embodiment of a wafer of the present disclosure. [Figure 5A] 2 is a flow chart of a method of manufacturing an embodiment of a wafer of the present disclosure as shown in FIG. 1. [Figure 5B] 4 is a flow chart of an embodiment of a method for manufacturing an embodiment of a polycrystalline substrate as shown in FIG. 3. [Figure 5C] 4 is a flow chart of an alternative embodiment of a method for manufacturing an embodiment of a polycrystalline substrate as shown in FIG. 3. [Figure 5D] 4 is a flow chart of another alternative embodiment of a method for manufacturing an embodiment of a polycrystalline substrate as shown in FIG. 3. [Figure 6A] 5B is a side view of at least some of the steps of an embodiment of a manufacturing method as shown in FIG. 5A for manufacturing an embodiment of a wafer as shown in FIG. 1. [Figure 6B] 5B is a side view of at least some of the steps of an embodiment of a manufacturing method as shown in FIG. 5A for manufacturing an embodiment of a wafer as shown in FIG. 1. [Figure 6C]5B is a side view of at least some of the steps of an embodiment of a manufacturing method as shown in FIG. 5A for manufacturing an embodiment of a wafer as shown in FIG. 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] In the following description, specific details are set forth to provide a thorough understanding of various embodiments of devices, methods, and articles. However, one of ordinary skill in the art will understand that other embodiments may be practiced without these details. In other instances, well-known structures and methods related to, for example, silicon carbide substrates or layers (e.g., polycrystalline silicon carbide, single crystal silicon carbide, etc.), semiconductor manufacturing processes, etc. have not been shown or described in detail in some figures to avoid unnecessarily obscuring the description of the embodiments.
[0009] Unless the context otherwise requires, throughout the following specification and claims, the word "comprise" and variations thereof, such as "comprising" and "comprises," are to be interpreted in their open and inclusive sense, i.e., "including, but not limited to."
[0010] References throughout this specification to "one embodiment" or "an embodiment" mean that a particular feature, structure, or characteristic described in connection with that embodiment is included in at least one embodiment. Thus, the appearances of the phrases "in one embodiment" or "in an embodiment" in various places throughout this specification do not necessarily refer to the same embodiment or all embodiments. Furthermore, the particular features, structures, or characteristics may be combined in any suitable manner in one or more embodiments to yield further embodiments.
[0011] Each heading is provided for convenience only and does not interpret the scope or meaning of the disclosure or claims.
[0012] The sizes and relative positions of elements in the figures are not necessarily drawn to scale, for example, the shapes and angles of various elements may not be drawn to scale, and some of these elements may be enlarged and positioned to improve the legibility of the figures.
[0013] The use of "transverse" means that a surface, sidewall, or similar or similar structure or feature is at an angle to another respective surface, sidewall, or similar or similar respective structure or feature. For example, if a first surface is transverse to a first sidewall, the first surface can be at an angle equal to 25 degrees, 35 degrees, 45 degrees, 75 degrees, 90 degrees, 120 degrees, etc.
[0014] Polycrystalline silicon carbide (SiC) substrates, wafers, or layers are commonly utilized within various electronic devices and components (e.g., semiconductor chips, semiconductor packages, semiconductor transistors, etc.). These polycrystalline SiC substrates, wafers, or layers have a resistivity that results in a resistance that exists along an electrical path that passes through or along the polycrystalline silicon carbide (SiC) substrate. This resistance opposes an electrical signal as it passes through or along the electrical path, and is referred to as on-resistance (R on ) The on-resistance (R on ) limits the efficiency or electrical characteristics of electronic devices fabricated from polycrystalline SiC substrates. For example, the on-resistance (R on If the on-resistance (R) associated with a polycrystalline silicon carbide (SiC) substrate, wafer, or layer is high, an electrical signal may be prevented from passing completely through the polycrystalline SiC substrate to reach its destination, resulting in functional errors within the electronic device or component. onIn view of this problem, the present disclosure is directed to providing a polycrystalline silicon carbide (SiC) substrate, wafer, or layer having a resistivity lower than that of current polycrystalline silicon carbide (SiC) substrates. For example, polycrystalline silicon carbide (SiC) substrates, wafers, or layers already utilized within these respective industries may have resistivities in the range of 2 mohm-cm (milliohm centimeters) to 10 mohm-cm (milliohm centimeters).
[0015] A polycrystalline SiC wafer with low resistivity is beneficial to the function of the electronic device in which the polycrystalline SiC wafer is present. The present disclosure is directed to providing at least one embodiment of a wafer including a polycrystalline silicon carbide wafer or substrate with low resistivity and low warpage. Electronic devices or components made from the wafer are further optimized in use and have fewer or no crystal defects. Wafers formed according to the embodiments of the present disclosure have low or very low resistivity compared to existing SiC wafers. The low amount of warpage in at least one embodiment of the wafer of the present disclosure prevents or reduces the possibility of defects from polishing processes, etc., in manufacturing the final electronic device, or results in a reduction in the number of cracked or broken wafers or substrates during processing and manufacturing.
[0016] At least one embodiment of a device of the present disclosure is summarized as follows: The device includes a polycrystalline silicon carbide (SiC) wafer having a resistivity of 2 mohm-cm (milliohm-centimeter) or less. The polycrystalline silicon carbide wafer includes a first surface having a roughness of 20 angstroms (Å) or less. A single crystal silicon carbide (SiC) wafer is bonded to the first surface of the polycrystalline silicon carbide (SiC) wafer.
[0017] At least one embodiment of the device of the present disclosure is summarized as follows: The device includes a substrate having a polycrystalline silicon carbide (SiC) layer. The polycrystalline silicon carbide (SiC) layer includes a first surface, a second surface opposite the first surface, a first dimension extending from the first surface to the second surface, and a resistivity of 2 mohm-cm (milliohm-centimeter) or less. The monocrystalline silicon carbide (SiC) layer is bonded to the second surface of the polycrystalline silicon carbide (SiC) layer. The monocrystalline silicon carbide layer includes a third surface on the second surface of the polycrystalline silicon carbide (SiC) layer, a fourth surface opposite the third surface, and a second dimension extending from the third surface to the fourth surface, the third surface of the monocrystalline silicon carbide (SiC) layer being on the bonding layer and facing toward the first surface of the polycrystalline silicon carbide (SiC) layer. The second dimension is less than the first dimension.
[0018] At least one embodiment of the device is summarized as follows: The device includes a polycrystalline silicon carbide substrate having a first surface, a second surface opposite the first surface, a thickness extending from the first surface to the second surface that is equal to or greater than 150 μm (micrometers), a resistivity equal to or less than 2 mohm-cm (milliohm-centimeters), and a bow less than 75 μm.
[0019] At least one embodiment of the method of the present disclosure is summarized as follows: The method includes forming a polycrystalline silicon carbide (SiC) substrate having a resistivity of 2 mohm-cm or less, forming a single crystal silicon carbide (SiC) substrate, and bonding the single crystal SiC substrate to the polycrystalline SiC substrate.
[0020] 1 is a side view of one embodiment of a wafer 100 of the present disclosure. The wafer 100 includes a first side 102 and a second side 104 opposite the first side 102. The wafer 100 further includes a polycrystalline silicon carbide (SiC) layer 106, a bond region 108, and a single crystal silicon carbide (SiC) layer 110 bonded to the polycrystalline silicon carbide layer 106 at the bond region 108. The polycrystalline silicon carbide layer 106 may be referred to as a polycrystalline silicon carbide substrate, a polycrystalline silicon carbide wafer, a polycrystalline silicon carbide layer, or in some other suitable manner. The single crystal silicon carbide (SiC) layer 110 may be referred to as a single crystal silicon carbide substrate, a single crystal silicon carbide wafer, a single crystal silicon carbide layer, or in some other suitable manner. The polycrystalline silicon carbide (SiC) layer 106 may be referred to herein within this disclosure as a polycrystalline layer 106, and the single crystal silicon carbide (SiC) layer 110 may be referred to herein within this disclosure as a single crystal layer 110. In at least one embodiment, the single crystal layer 110 has a density of 3.26 g / cm 3 In at least one embodiment, the polycrystalline layer 106 has a density equal to 3.2 g / cm 3 ~3.3g / cm 3 In at least one embodiment, the polycrystalline layer 106 has a density in the range of 3.25 g / cm 3 ~3.3g / cm 3 or equal to the upper and lower ends of this range.
[0021] The polycrystalline layer 106 has a low resistivity, for example, a resistivity of 2 mohm-cm or less, or a resistivity of 1 mohm-cm or less. This low resistivity of the polycrystalline layer 106 allows electrical signals (e.g., electrons) to pass through the polycrystalline layer 106 without being impeded by the polycrystalline layer 106, so that the electrical signals can travel faster through the polycrystalline layer 106 and reach their destination with a higher strength than if the polycrystalline layer 106 had a higher resistivity. In other words, the on-resistance (R on) is low (i.e., has low resistivity), an electrical signal will pass more easily and efficiently through the polycrystalline layer 106 without being impeded by the polycrystalline layer 106 as it travels to its destination within the electronic device (e.g., a semiconductor package, a semiconductor chip, or some other similar or similar electronic device in which the polycrystalline layer 106 may be present).
[0022] The polycrystalline layer 106 includes a first surface 112 and a second surface 114 opposite the first surface 112. The first surface 112 of the polycrystalline layer 106 is on the first side 104 of the wafer 100. The monocrystalline layer 110 includes a third surface 116 and a fourth surface 118 opposite the third surface 116. The fourth surface 118 of the monocrystalline layer 110 is on the second side 106 of the wafer 100.
[0023] The polycrystalline layer 106 has a first thickness T1, which may be referred to as a first dimension. The first thickness T1 extends from a first surface 112 of the polycrystalline layer 106 to a second surface 114 of the polycrystalline layer 106. In some embodiments, the first thickness T1 may be in the range 150 to 1500 micrometers (μm) or equal to the upper and lower ends of this range (e.g., the first thickness T1 may be equal to 150 micrometers (μm) or equal to 1000 micrometers (μm)). In some embodiments, the first thickness may be equal to 1 millimeter (mm) or less.
[0024] The monocrystalline layer 110 has a second thickness T2, which may be referred to as a second dimension. The second thickness T2 extends from the third surface 116 of the monocrystalline layer 110 to the fourth surface 118 of the monocrystalline layer 110. The second thickness T2 of the monocrystalline layer 110 may be less than the first thickness T1 of the polycrystalline layer 106. The second thickness T2 of the monocrystalline layer 110 may be in the range 0.3 to 2 micrometers (μm) or equal to the upper and lower ends of this range (e.g., the second thickness T2 may be equal to 0.3 micrometers (μm) or equal to 2 micrometers (μm)). In some embodiments, the second thickness may be in the range 0.3 to 1 micrometers (μm) or equal to the upper and lower ends of this range (e.g., the second thickness T2 may be equal to 0.3 micrometers (μm) or equal to 1 micrometer (μm)). In some embodiments, the second thickness T2 of the single crystal layer 110 can be equal to 0.5 micrometers (μm). In some embodiments, the second thickness T2 can be equal to or less than 20-200 micrometers (μm), or equal to the upper and lower ends of this range (e.g., the second thickness T2 can be equal to 20 micrometers (μm) or equal to 200 micrometers (μm)). In some embodiments, the second thickness T2 can be equal to 120 micrometers (μm).
[0025] In some embodiments, the sum of the first thickness T1 and the second thickness T2 can be in the range of 200 micrometers (μm) to 1500 micrometers (μm), or can be equal to the upper and lower ends of this range. For example, in some embodiments, the sum of the first thickness T1 and the second thickness T2 can be equal to 200 micrometers (μm), can be equal to 1500 micrometers (μm), or can be equal to some other thickness between 200 and 1500 micrometers (μm). In some embodiments, the sum of the first thickness T1 and the second thickness T2 can be equal to 250 micrometers (μm), can be equal to 500 micrometers (μm), or can be equal to some other thickness between 250 micrometers (μm) and 500 micrometers (μm). In some embodiments, the sum of the first thickness T1 and the second thickness T2 can be equal to 700 micrometers (μm), can be equal to 800 micrometers (μm), or can be equal to some other thickness between 700 micrometers (μm) and 800 micrometers (μm).
[0026] In at least one embodiment, the monocrystalline layer 110 may have a resistivity less than 25 mohm-cm or preferably 18 mohm-cm, or in the range 15-20 mohm-cm or equal to the upper and lower ends of this range. In at least one embodiment, the polycrystalline layer 106 has a void density of 3% or less. As shown in FIG. 1, in an embodiment of the wafer 100, a bond region 108 exists between a first surface 112 of the polycrystalline layer 106 and a second surface 114 of the monocrystalline layer 110, the bond region 108 being where the second surface 114 of the polycrystalline layer 106 is directly and physically bonded to the monocrystalline layer 110. In some embodiments, the monocrystalline layer 110 is directly and physically bonded to the polycrystalline layer 106 by utilizing a surface activated bonding (SAB) technique. For example, in a surface activated bonding technique, the second surface 114 of the polycrystalline layer 106 and the third surface 116 of the monocrystalline layer 110 may be bombarded with argon (Ar) ions or neutral atoms (e.g., a particle beam, which may be argon (Ar), neutral atoms, or some other similar or similar type of particles or atoms, which may be suitable) in an ultra-high vacuum to clean and activate the second surface 114 of the polycrystalline layer 106 and the third surface 116 of the monocrystalline layer 110. After the second surface 114 of the polycrystalline layer 106 and the third surface 116 of the monocrystalline layer 110 are cleaned and activated, the second surface 114 of the polycrystalline layer 106 and the third surface 116 of the monocrystalline layer 110 are naturally bonded by contacting the second surface 114 of the polycrystalline layer 106 with the third surface 116 of the monocrystalline layer 106. This contacting of the second surface 114 of the polycrystalline layer 106 with the third surface 114 of the monocrystalline layer 110 may occur without a heat treatment.
[0027] The wafer 100 further includes at least one sidewall 120 (e.g., circular in the embodiment as shown in FIG. 1 ) where the at least one first sidewall 120a of the polycrystalline layer 106 and the at least one second sidewall 120b of the monocrystalline layer 110 are respectively coplanar and flush with each other. In other words, the at least one sidewall 120 includes and is defined by the respective sidewalls of the polycrystalline layer 106, the bonding layer 108, and the monocrystalline layer 110. The bonding layer 108 includes a sidewall 120c that is coplanar with the sidewall 120a of the polycrystalline layer 106 and the sidewall 120b of the monocrystalline layer 110.
[0028] As previously discussed herein, the polycrystalline layer 106 has a low resistivity, for example, a resistivity of 2 mohm-cm (milliohm centimeters) or less, or a resistivity of 1 mohm-cm (milliohm centimeters) or less. This low resistivity of the polycrystalline layer 106 allows electrical signals (e.g., electrons) to pass through the polycrystalline layer 106 without being impeded by the polycrystalline layer 106, so that the electrical signals may travel faster through the polycrystalline layer 106 and reach their destination with a higher strength than if the polycrystalline layer 106 had a higher resistivity. In other words, the on-resistance (R on ) is low (i.e., has low resistivity), an electrical signal will pass more easily and efficiently through the polycrystalline layer 106 without being impeded by the polycrystalline layer 106 as it travels to its destination within the electronic device (e.g., a semiconductor package, a semiconductor chip, or some other similar or similar electronic device in which the polycrystalline layer 106 may be present).
[0029] Although not shown in FIG. 1, in some alternative embodiments of wafer 100, a silicon oxide (e.g., SiO2) layer may be present in bond region 108 such that the silicon oxide layer is between polycrystalline layer 106 and monocrystalline layer 110.
[0030] Wafer 100 has a diameter D1 extending from opposite points along the peripheral edge of wafer 100. Diameter D1 may be in the range of 150 to 300 millimeters (mm) and may be equal to the upper and lower ends of this range. For example, diameter D1 may be equal to 150 mm, may be equal to 200 mm, or may be equal to 300 mm.
[0031] An embodiment of the wafer 100 may have some warping, which may be some bending or bowing within the embodiment of the wafer 100, causing the second surface 114 of the polycrystalline layer 106 to be slightly curved or have a slight curvature. However, while some warping may be present in the wafer 100, the warping of the wafer 100 may be 75 micrometers (μm) or less, or 45 micrometers (μm) or less. The warping may be measured as the distance from the center point of the wafer in a direction across the second surface 114 of the wafer to a point at or near the edge of the wafer. The warping is relative to the horizontal flatness of the wafer 100 and may be readily seen at and along each of the surfaces 112, 114, 116, 118, respectively.
[0032] The second surface 114 of the polycrystalline layer 106 may have a roughness of 20 angstroms (Å) or less. In some embodiments, the second surface 114 of the polycrystalline layer 106 may have a roughness in the range of 1 to 5 angstroms (Å), equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). This roughness of the second surface 114 may be obtained by polishing the second surface 114.
[0033] The third surface 116 of the monocrystalline layer 110 may have a roughness of 20 angstroms (Å) or less. In some embodiments, the third surface 116 of the monocrystalline layer 110 may have a roughness in the range of 1 to 5 angstroms (Å), equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). This roughness of the third surface 116 may be obtained by polishing the third surface 116.
[0034] The fourth surface 118 of the monocrystalline layer 110 may have a roughness of 20 angstroms (Å) or less. In some embodiments, the fourth surface 118 of the monocrystalline layer 110 may have a roughness in the range of 1 to 5 angstroms (Å), and may be equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). This roughness of the fourth surface 118 may be obtained by polishing or planarizing the fourth surface 116. In some embodiments, the roughness at the first surface 104 of the polycrystalline layer 106 may be equal to or greater than the roughness of the second surface 114 of the polycrystalline layer 106. This roughness of the first surface 104 may be obtained by polishing or planarizing the first surface 104.
[0035] Wafer 100, or a portion of each wafer, may be present in a semiconductor package formed using wafer 100. For example, wafer 100 may be used to form a vertical device that includes wafer 100, or a portion of wafer 100. For example, additional layers may be formed on single crystal layer 110.
[0036] Figure 2 relates to a perspective side view of an alternative embodiment of wafer 200, which has some of the same or similar features as the embodiment of wafer 100 as shown in Figure 1. The same or similar features of wafer 200 relative to wafer 100 have the same or similar reference numerals. Thus, the following discussion of the alternative embodiment of wafer 200 as shown in Figure 2 will focus on different or additional features or details as compared to the embodiment of wafer 100 as shown in Figure 1.
[0037] Unlike the embodiment of wafer 100 as shown in FIG. 1, in which second surface 114 of polycrystalline layer 106 is directly and physically bonded to third surface 116 of monocrystalline layer 110, in the embodiment of wafer 200 as shown in FIG. 2, bonding layer 202 is present in bonding region 108 and bonds polycrystalline layer 106 to monocrystalline layer 110 together. For example, a first conductive layer may be formed on second surface 114 of polycrystalline layer 106 and a second conductive layer may be formed on third surface 116 of monocrystalline layer 110 before a surface activated bonding (SAB) technique as previously discussed herein is performed. The first conductive layer and the second conductive layer may be made of the same or different conductive materials that are suitable to be bonded together utilizing SAB techniques. In some embodiments, the first conductive layer and the second conductive layer may be formed on the second surface 114 of the polycrystalline layer 112 and the third surface 116 of the single crystal layer 110, respectively, by a sputtering technique or by some other technique suitable for forming a first conductive layer and a second conductive layer on the second surface 114 of the polycrystalline layer 112 and the third surface 116 of the single crystal layer 110, respectively.
[0038] After the first conductive layer and the second conductive layer are formed on the second surface 114 of the polycrystalline layer 106 and the third surface 116 of the monocrystalline layer 110, respectively, a surface activation bonding technique is performed, whereby the first conductive layer and the second conductive layer are bombarded by argon (Ar) ions or neutral atoms (e.g., a particle beam which may be argon (Ar), may be neutral atoms, or some other similar or similar type of particles or atoms which may be suitable) in ultra-high vacuum to clean and activate the first conductive layer and the second conductive layer on the second surface 114 of the polycrystalline layer 106 and the third surface 116 of the monocrystalline layer 110, respectively. After the first and second conductive layers are cleaned and activated, the first conductive layer on the second surface 114 of the polycrystalline layer 106 and the second conductive layer on the third surface 116 of the monocrystalline layer 110 are naturally bonded by contacting the first conductive layer on the second surface 114 of the polycrystalline layer 106 with the second conductive layer on the third surface 116 of the monocrystalline layer 106. This contact between the first conductive layer on the second surface 114 of the polycrystalline layer 106 and the second conductive layer on the third surface 114 of the monocrystalline layer 110 can be made without a heat treatment. When the first conductive layer on the second surface 114 of the polycrystalline layer 106 is bonded to the second conductive layer on the third surface 116 of the monocrystalline layer 110, a bonding layer 202 is formed between the polycrystalline layer 106 and the monocrystalline layer 110. In other words, the bonding layer 202 may be a conductive layer formed by bonding a first conductive layer on the second surface 114 to a second conductive layer on the third surface 116 .
[0039] In some alternative embodiments, instead of forming both the first and second conductive layers as discussed above, only one of the first conductive layer or the second conductive layer may be formed on only one of the second surface 114 of the polycrystalline layer 106 or the third surface 116 of the monocrystalline layer 110. After only one of the first conductive layer or the second conductive layer is formed, the SAB technique is performed in the same or similar manner as previously discussed herein with respect to either FIG. 1 or FIG. 2, except that at least one of the second surface 114 of the polycrystalline layer 106 or the third surface 116 of the monocrystalline layer 110 remains uncovered and is exposed to an argon or neutral atom beam.
[0040] If the first material of the polycrystalline layer 106 is incompatible with directly and physically bonding to the second material of the monocrystalline layer 110, then either both the first conductive layer and the second conductive layer, or at least one of the first conductive layer or the second conductive layer, may be formed. In other words, if the first material of the polycrystalline layer 106 is incompatible with the second material of the monocrystalline layer 110, then either both the first conductive layer and the second conductive layer, or at least one of the first conductive layer or the second conductive layer, may be formed to facilitate bonding the polycrystalline layer 106 to the monocrystalline layer 110 together.
[0041] When the bonding layer 202 is between the second surface 114 of the polycrystalline layer 106 and the third surface of the monocrystalline layer 110, the bonding layer 202 has a third thickness T3, which may be referred to as a third dimension. The third thickness T3 extends from the second surface 114 of the polycrystalline layer 106 to the third surface 116 of the monocrystalline layer 110. The third thickness T3 may be less than the first thickness T1. The third thickness T3 of the bonding layer 108 may be in the range of 0.2 to 5 micrometers (μm) and may be equal to the upper and lower ends of this range (e.g., the third thickness T3 may be equal to 0.2 micrometers (μm) or may be equal to 5 micrometers (μm)). In some embodiments, the third thickness may be equal to 0.5 micrometers (μm).
[0042] Alternative embodiments of the wafer 200 may have some warping, which may be some bending or bowing in the alternative embodiments of the wafer 200, causing the second surface 114 of the polycrystalline layer 106 to be slightly curved or have a slight curvature. However, while some warping may be present in alternative embodiments of the wafer 200, the warping in alternative embodiments of the wafer 200 may be 75 micrometers (μm) or less, or 45 micrometers (μm) or less. The second surface 114 of the polycrystalline layer 106 may have a roughness of 20 angstroms (Å) or less. In some embodiments, the second surface 114 of the polycrystalline layer 106 may have a roughness in the range of 1 to 5 angstroms (Å), and may be equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or may be equal to 5 angstroms (Å)). This roughness of the second surface 114 may be obtained by polishing the second surface 114 .
[0043] The third surface 116 of the monocrystalline layer 110 may have a roughness of 20 angstroms (Å) or less. In some embodiments, the third surface 116 of the polycrystalline layer 106 may have a roughness in the range of 1 to 5 angstroms (Å), which may be equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). This roughness of the third surface 116 may be obtained by polishing the third surface 116.
[0044] The fourth surface 118 of the monocrystalline layer 110 may have a roughness of 20 angstroms (Å) or less. In some embodiments, the fourth surface 118 of the monocrystalline layer 110 may have a roughness in the range of 1 to 5 angstroms (Å), equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). This roughness of the fourth surface 118 may be obtained by polishing or planarizing the fourth surface 116.
[0045] In some embodiments, the roughness at the first surface 104 of the polycrystalline layer 106 may be equal to or greater than the roughness of the second surface 114 of the polycrystalline layer 106. This roughness of the first surface 104 may be obtained by polishing or planarizing the first surface 104.
[0046] In yet another alternative embodiment of the wafer 200, the bonding layer 202 is instead a monolayer of silicon. The monolayer of silicon includes a thickness T3 as shown in FIG. 2. When the bonding layer 202 is a monolayer of silicon, the thickness T3 of the monolayer of silicon can be in the range of 0.2 nanometers (nm) to 0.7 nanometers (nm), or equal to the upper and lower ends of this range. The monolayer of silicon is formed on the second surface 114 of the polycrystalline layer 106 when the monocrystalline layer 110 is not so suitable to be directly and physically bonded to the second surface 114 of the polycrystalline layer 106. The monolayer of silicon to be the bonding layer 202 is formed by atomic layer deposition or sputtering, resulting in a monolayer of silicon being present on the second surface 114 of the polycrystalline layer 106, so that the monocrystalline layer 110 can be easily adhered to the polycrystalline layer 106 via the monolayer of silicon, which is again the bonding layer 202. Alternatively, instead of a monolayer of silicon, the bonding layer 202 can be a monolayer of carbon, a bilayer of carbon, or a layer of silicon dioxide (SiO2). The monolayer of carbon can have a thickness in the range of 0.4 nanometers (nm) to 2 nanometers (nm), or equal to the upper and lower ends of this range. The bilayer of carbon can have a thickness in the range of 1 nanometer (nm) to 5 nanometers (nm), or equal to the upper and lower ends of this range. The layer of SiO2 can have a thickness in the range of 2 nm (nanometers) to 7 nm (nanometers), or equal to the upper and lower ends of this range.
[0047] 3 is a perspective side view of an embodiment of a polycrystalline substrate 300, which may be a polycrystalline wafer before a monocrystalline substrate or wafer (e.g., monocrystalline layer 110) is bonded or joined to the polycrystalline substrate 300. The polycrystalline substrate 300 has a diameter D1. The polycrystalline substrate 300 may be utilized in forming the polycrystalline layer 106 in the embodiment of the wafer 100 and in the alternative embodiment of the wafer 200. The polycrystalline substrate 300 includes a first surface 302, a second surface 304 opposite the first surface 302, and a sidewall 306 extending from the first surface 302 to the second surface 304 and transverse to the first surface 302 and the second surface 304. The second surface 304 of the polycrystalline substrate 300 may correspond to the second surface 114 of the polycrystalline layer 106, as in the embodiment of the wafer 100 and in the alternative embodiment of the wafer 200. Sidewall 306 of polycrystalline substrate 300 may correspond to at least one first sidewall 120 a of polycrystalline layer 106 , as in the embodiment of wafer 100 and the alternative embodiment of wafer 200 .
[0048] The fourth thickness T4 of polycrystalline substrate 300 extends from first surface 302 to second surface 304 of polycrystalline substrate 300. The fourth thickness T4 may be greater than or equal to the third thickness T3 of polycrystalline layer 106, as in the embodiment of wafer 100 and the alternative embodiment of wafer 200. The fourth thickness T4 may be in the range of 150 micrometers (μm) to 1000 micrometers (μm), or equal to the lower and upper ends of this range.
[0049] Polycrystalline substrate 300 has a low resistivity, for example a resistivity of 2 mohm-cm or less, or a resistivity of 1 mohm-cm or less.
[0050] The embodiment of the polycrystalline substrate 300 may have some warping, which may be some bending or warping within the embodiment of the polycrystalline substrate 300, causing the second surface 304 of the polycrystalline layer 106 to be slightly curved or have a slight curvature. However, while some warping may be present in the polycrystalline substrate 300, the warping in the polycrystalline substrate 300 may be 75 micrometers (μm) or less, or 45 micrometers (μm) or less.
[0051] The second surface 304 of the polycrystalline substrate 300 may have a roughness of 20 angstroms (Å) or less. In some embodiments, the second surface 304 of the polycrystalline substrate 300 may have a roughness in the range of 1 to 5 angstroms (Å), which may be equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). This roughness of the second surface 304 may be obtained by polishing the second surface 304.
[0052] FIG. 4 is an exaggerated close-up view of cross section 4-4 as shown in FIG. 1 of an embodiment of wafer 100 as shown in FIG. 1. Polycrystalline layer 106 includes grains 402 of silicon carbide (e.g., SiC, SiC2, etc.) that may be bonded together (see FIG. 5A of this disclosure). This exaggerated close-up view as shown in FIG. 4 may represent the grain structure of polycrystalline layer 106 in an alternative embodiment of wafer 200 as shown in FIG. 2, or the grain structure of an embodiment of polycrystalline substrate 300 as shown in FIG. 3. Polycrystalline layer 106 is a non-columnar type polycrystalline such that polycrystalline layer 106 has random or amorphous oriented grains and does not have a columnar type structure. This random and amorphous oriented grains and non-columnar structure of polycrystalline layer 106 may be referred to as a non-oriented grain structure. This non-oriented grain structure may help reduce the overall resistivity of polycrystalline layer 106. The polycrystalline layer 106 may include micropores 404 that may be present along grain boundaries 406 between the grains 402. The grain boundaries 406 are present between adjacent pairs of each grain of the grains 402. Carbon may be present at the grain boundaries 406 to adhere the grains 402 to one another within the polycrystalline layer 106. The grains 402 may have a size of 1 millimeter (mm) or less.
[0053] The size of the grains 402 is relatively uniform throughout the polycrystalline layer 106, from the first surface 112 to the second surface 114 of the polycrystalline layer 106. In other words, the size of the grains 402 remains relatively uniform throughout the polycrystalline layer 106, regardless of the position along the polycrystalline layer 106 between the first surface 112 and the second surface 114, and the position within the polycrystalline layer. For example, the grain sizes of the grains 402 at the first surface 112 of the polycrystalline layer 106, the second surface 114 of the polycrystalline layer 106, and at intermediate positions along the polycrystalline layer 106 between the first surface 112 and the second surface 114 are uniform and substantially equal to one another.
[0054] In view of the grain size being relatively uniform along the entirety of polycrystalline layer 106, the respective densities of polycrystalline layer 106 at these various locations are relatively uniform and equal to one another. In other words, polycrystalline layer 106 has a density that is relatively uniform throughout polycrystalline layer 106.
[0055] As previously discussed herein, the polycrystalline layer 106 has a low resistivity, which may be formed utilizing a polycrystalline substrate 300. The polycrystalline layer 106 may have a low resistivity by either reducing or limiting the number of micropores 404 between the grains 402 along the grain boundaries 406, such that the polycrystalline layer 106 has a resistivity of 2 mohm-cm or less, or by having a high doping of nitrogen (N) in the polycrystalline layer 106 to reduce and counteract the effect of the presence of the micropores 404 in the polycrystalline layer 106. For example, the polycrystalline layer 106 may have a low resistivity such that the concentration of nitrogen (N) is less than 2000 nm in the polycrystalline layer 106. 3 3E+19 atoms per unit (i.e., 3×10 19 atoms / cm 3 ) or may be doped with so much nitrogen that the concentration of nitrogen in polycrystalline layer 106 may be equal to the upper and lower ends of this range. In some embodiments, the concentration of nitrogen (N) doped in polycrystalline layer 106 is greater than or equal to cm 3 5E+19 atoms per unit (i.e., 5×10 19 atoms / cm 3 ) or more.
[0056] Figure 5A relates to a flowchart 500 of an embodiment of a method for manufacturing an embodiment of a wafer 100 as shown in Figure 1 of the present disclosure. Figures 6A-6C relate to side views of respective steps 502, 504, 506, 508 of the flowchart 500 of an embodiment of a method for manufacturing an embodiment of a wafer 100 of the present disclosure.
[0057] In a polycrystalline substrate formation step 502, a polycrystalline substrate 300 having low resistivity is formed. In a single crystal substrate formation step 504, a single crystal substrate 504 is formed. The polycrystalline substrate formation step 502 and the single crystal substrate formation step 504 may occur simultaneously within a semiconductor foundry (FAB) or may occur at different times within the FAB. The polycrystalline substrate formation step 502 and the single crystal substrate formation step 504 may be performed at different locations within the FAB.
[0058] The polycrystalline substrate formation step 502 for forming a polycrystalline substrate 300 having low resistivity can be performed using at least one of the embodiments of the method for forming the polycrystalline substrate 300 illustrated in the chemical vapor deposition (CVD) flow chart 502a as shown in Fig. 5B, the sintering flow chart 502b as shown in Fig. 5C, or the sublimation flow chart 502c as shown in Fig. 5C. In other words, the polycrystalline substrate 300 can be formed using any one of the methods in the CVD flow chart 502a, the sintering flow chart 502b, and the sublimation flow chart 502c.
[0059] When the polycrystalline substrate 300 is formed utilizing the method of CVD flow chart 502a as shown in Figure 5B, in a first step 510, a carrier is inserted or introduced into a chamber of a CVD tool configured to perform or execute a CVD process to form the polycrystalline substrate 300. The carrier may be a plate, a carrier substrate, or any other suitable type of carrier on which the polycrystalline substrate is formed. The carrier may be a polycrystalline carrier substrate or plate, a graphite carrier substrate or plate, or any other suitable type of carrier substrate or plate on which the polycrystalline substrate is formed.
[0060] After a first step 510 in which a carrier is inserted or introduced into the chamber of a CVD tool, in a second step 512, the chamber is sealed and a carrier gas is introduced into the chamber of the CVD tool. The carrier gas may be hydrogen gas, a hydrogen-based gas, argon gas, an argon-based gas, or any other suitable carrier gas or an inert carrier gas. The carrier gas is configured to promote a chemical reaction in the chamber of the CVD tool to grow polycrystalline silicon carbide (SiC) on the carrier in the chamber of the CVD tool. In some embodiments, during the second step 512, the chamber of the CVD tool may be heated within a range of 1500 degrees Celsius (° C.) to 1700 degrees Celsius (° C.), or may be heated to a temperature equal to the upper and lower ends of this range (e.g., a temperature equal to 1500 degrees Celsius (° C.) or equal to 1700 degrees Celsius (° C.)). In some alternative embodiments, during the second step 512, the chamber of the CVD tool may be heated within a range of 950 degrees Celsius (° C.) to 1350 degrees Celsius (° C.), or may be heated to a temperature equal to the upper and lower ends of this range (e.g., a temperature equal to 950 degrees Celsius (° C.) or a temperature equal to 1350 degrees Celsius (° C.)).
[0061] After a second step 512 in which a carrier gas is introduced into the chamber of the CVD tool and the chamber of the CVD tool is heated or heating is started, in a third step 514, a carbon or carbon-based gas, a silicon-containing or silicon-based gas (e.g., silane, trichlorosilane (TCS), or any other similar silicon-containing or silicon-based gas), and a nitrogen or nitrogen-based gas are introduced into the chamber of the CVD tool. For example, a carbon or carbon-based gas may be introduced into the chamber of the CVD tool by introducing a carbon source into the chamber of the CVD tool, a silicon-containing or silicon-based gas may be introduced into the chamber of the CVD tool by introducing a silicon-containing or silicon-based gas source into the chamber of the CVD tool, and a nitrogen or nitrogen-based gas may be introduced into the chamber of the CVD tool by introducing a nitrogen source into the chamber of the CVD tool. Alternatively, the respective fluid paths in fluid communication with the chamber of the CVD tool may be opened to introduce carbon or carbon-based gas, silicon-containing or silicon-based gas, and nitrogen or nitrogen-based gas. When these respective gases are introduced into the chamber of the CVD tool at this stage, these respective gases chemically react with each other, resulting in the formation of nitrogen-doped silicon carbide (SiC) and deposition on the carrier substrate, such that polycrystalline silicon carbide is formed on the carrier surface of the carrier. If the carrier is a polycrystalline silicon carbide carrier substrate or plate, the polycrystalline silicon carbide formed by the reaction in the chamber of the CVD tool is deposited on the polycrystalline silicon carbide carrier substrate or plate. If the carrier is a graphite carrier substrate or plate, the polycrystalline silicon carbide formed by the reaction in the chamber of the CVD tool is deposited on the graphite carrier substrate or plate. When the polycrystalline silicon carbide is formed in the chamber of the CVD tool, the polycrystalline silicon carbide is doped with nitrogen, such that nitrogen-doped polycrystalline silicon carbide is formed on the carrier.
[0062] After a third step 514 in which carbon or carbon-based gas, silicon-containing or silicon-based gas, and nitrogen or nitrogen-based gas are introduced into the chamber of the CVD tool and heated simultaneously to form nitrogen-doped polycrystalline silicon carbide on the carrier, in a fourth step 516, the chamber of the CVD tool and the polycrystalline substrate 300 formed on the carrier are cooled to room temperature. As the polycrystalline substrate 300 cools on the carrier, some warping of the polycrystalline substrate 300 may occur due to the difference in thermal conductivity between the polycrystalline substrate 300 and the carrier. However, this warping of the polycrystalline substrate may be 75 micrometers (μm) or less, or 45 micrometers (μm) or less. Once cooled to room temperature, the polycrystalline substrate 300 bonded to the carrier and the carrier are removed from the chamber of the CVD tool. After the polycrystalline substrate 300 and carrier are removed from the chamber, the polycrystalline substrate 300 may be removed from the carrier and then further processed (e.g., polishing techniques, planarizing techniques, etc.), a portion of the polycrystalline substrate 300 may be sliced from the polycrystalline substrate 300 either while bonded to the carrier or after being removed from the carrier, or before or after further processing, to form the polycrystalline layer 106, or the polycrystalline substrate may undergo other suitable types of processing techniques to further refine or process the polycrystalline substrate 300 to form various electronic devices or components.
[0063] After the polycrystalline substrate 300 is formed, the polycrystalline substrate 300 may be utilized to form an embodiment of the wafer 100 as shown in FIG. 1, or an alternative embodiment of the wafer 200 as shown in FIG. 2. For example, in at least one situation, the second surface 304 of the polycrystalline layer 300 is polished or planarized such that the second surface 304 of the polycrystalline layer 300 has a roughness of 20 angstroms (Å) or less. In some embodiments, the second surface 304 of the polycrystalline layer 300 has a roughness in the range of 1 to 5 angstroms (Å), or equal to the lower or upper ends of this range (e.g., the roughness can be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). After second surface 304 of polycrystalline layer 300 is polished or planarized, polycrystalline layer 300 may then be utilized to form an embodiment of wafer 100 as shown in FIG. 1, or an alternative embodiment of wafer 200 as shown in FIG. 2.
[0064] When the polycrystalline substrate 300 is formed utilizing the method of sintering flowchart 502b as shown in FIG. 5C, in a first step 518, a doped powder (e.g., silicon carbide powder doped with nitrogen) is inserted or introduced into a container that may be present in a sintering tool or may be inserted or introduced into the sintering tool after being filled with the doped powder.
[0065] After the first step 518 where the doped powder is introduced into the container, then in a second step 520, the container is heated by a sintering tool and pressure is applied to the doped powder in the container using the sintering tool. A temperature of 2000 degrees Celsius (°C) or more may be applied to the doped powder. In some embodiments, a pressure may be applied to the doped powder that is in the range of 300 millibar (mbar) to 1 ATM (1013 mbar) or equal to the lower and upper ends of this range (e.g., equal to 300 mbar or equal to 1 ATM). In some embodiments, a pressure may be applied to the doped powder that is in the range of 750 millibar (mbar) to 950 millibar (mbar) or equal to the lower and upper ends of this range (e.g., equal to 750 mbar or equal to 950 mbar). By subjecting the doped powder in the container to this temperature and pressure using a sintering tool, a nitrogen doped polycrystalline silicon carbide body will be formed in the container. 3 3E+19 atoms per unit (i.e., 3×10 19 atoms / cm 3 ) or may be doped with a dopant having a concentration of cm 3 3E+19 atoms per unit (i.e., 3×10 19 atoms / cm 3 In some embodiments, the dopant may be nitrogen (N). For example, the doped powder may have a concentration of more than cm 3 5E+19 atoms per unit (i.e., 5×10 19 atoms / cm 3 ) with a dopant having a concentration equal to
[0066] After a second step 520 in which a polycrystalline body is formed in the container by applying heat and pressure to the doped powder in the container, the polycrystalline body is removed from the container in a third step 522. Before removing the polycrystalline body from the container, the container and polycrystalline body may be cooled to room temperature. After the polycrystalline body is removed from the container, the polycrystalline body may have a cylindrical shape or profile.
[0067] After the polycrystalline body is removed from the container in a third step 522, in a fourth step 524, the polycrystalline body is further processed to form polycrystalline substrates 300. For example, if the polycrystalline body removed from the container has a cylindrical shape or profile, as previously discussed herein, the polycrystalline body may have a length between both ends of the cylindrical polycrystalline body such that the length exceeds the fourth thickness T4 such that multiple lengths of polycrystalline substrates 300 may be formed, so that the polycrystalline body may be sliced into multiple polycrystalline substrates 300.
[0068] After the polycrystalline substrate 300 is formed, the polycrystalline substrate 300 may be utilized to form an embodiment of the wafer 100 as shown in FIG. 1, or an alternative embodiment of the wafer 200 as shown in FIG. 2. For example, in at least one situation, the second surface 304 of the polycrystalline layer 300 is polished or planarized such that the second surface 304 of the polycrystalline layer 300 has a roughness of 20 angstroms (Å) or less. In some embodiments, the second surface 304 of the polycrystalline substrate 300 may have a roughness in the range of 1 to 5 angstroms (Å), or may have a roughness equal to the lower or upper end of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). After second surface 304 of polycrystalline layer 300 is polished or planarized, polycrystalline layer 300 may then be utilized to form an embodiment of wafer 100 as shown in FIG. 1, or an alternative embodiment of wafer 200 as shown in FIG. 2.
[0069] When the polycrystalline substrate 300 is formed using the method of sublimation flow chart 502c as shown in FIG. 5D, in a first step 526, sublimation powder, nitrogen gas or a nitrogen-based gas, and a carrier gas are introduced or inserted into the chamber of a sublimation growth tool.
[0070] After a first step 526 in which the sublimation powder, nitrogen gas or nitrogen-based gas, and carrier gas are introduced or inserted into the chamber of the sublimation growth tool, in a second step 528, heat is applied to the sublimation powder, nitrogen gas or nitrogen-based gas, and carrier gas in the chamber of the sublimation growth tool. The temperature of the chamber of the sublimation tool can be in the range of 2000-2500 degrees Celsius (°C) or equal to the lower and upper ends of this range (e.g., a temperature equal to 2000 degrees Celsius (°C) or equal to 2500 degrees Celsius (°C)). When heat is applied to the sublimation powder, sublimation gas is generated (e.g., sublimed) from the sublimation powder. The sublimation gas generated by heating the sublimation powder reacts with the carrier gas and the nitrogen gas or nitrogen-based gas to result in a polycrystalline body made of doped polycrystalline silicon carbide material forming and growing in the chamber of the sublimation growth tool. For example, polycrystalline silicon carbide material can be deposited and grown on a surface in a sublimation growth tool.
[0071] After the second step 528, in which heat is applied to the sublimated powder, nitrogen gas or nitrogen-based gas, and carrier gas in the chamber of the sublimation growth tool, the polycrystalline body grown and formed in the chamber is removed from the chamber of the sublimation growth tool in a third step 530. The polycrystalline body is allowed to cool to room temperature before being removed from the chamber of the sublimation growth tool.
[0072] After the third step 530, in which the polycrystalline body is removed from the chamber of the sublimation growth tool, in a fourth step 532, the polycrystalline body is further processed and purified to form the polycrystalline substrate 300. For example, in the fourth step 532 of the sublimation flow chart 502c, the polycrystalline body may be further purified or processed in the same or similar manner as previously discussed herein with respect to the further processing or purification of the polycrystalline body in the fourth step 524 of the sintering flow chart 502b. However, in some alternative embodiments, the polycrystalline body may already be in the form of the polycrystalline substrate 300, such that the polycrystalline body removed from the chamber of the sublimation growth tool is already in the form of the polycrystalline substrate 300.
[0073] After the polycrystalline substrate 300 is formed, the polycrystalline substrate 300 may be utilized to form an embodiment of the wafer 100 as shown in FIG. 1, or an alternative embodiment of the wafer 200 as shown in FIG. 2. For example, in at least one situation, the second surface 304 of the polycrystalline layer 300 is polished or planarized such that the second surface 304 of the polycrystalline layer 300 has a roughness of 20 angstroms (Å) or less. In some embodiments, the second surface 304 of the polycrystalline substrate 300 may have a roughness in the range of 1 to 5 angstroms (Å), or may have a roughness equal to the lower or upper end of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). After second surface 304 of polycrystalline layer 300 is polished or planarized, polycrystalline layer 300 may then be utilized to form an embodiment of wafer 100 as shown in FIG. 1, or an alternative embodiment of wafer 200 as shown in FIG. 2.
[0074] In the single crystal substrate formation step 504, a single crystal substrate 600 (see FIG. 6B) may be formed utilizing methods known in the semiconductor industry. For example, the single crystal substrate may be formed by melting high purity semiconductor grade silicon and then utilizing a seed crystal to initiate the formation of the single crystal substrate.
[0075] Once polycrystalline substrate 300 and monocrystalline substrate 600 are formed, in a bonding or joining step 506 of flowchart 500 for forming an embodiment of wafer 100, second surface 304 of polycrystalline substrate 300 is bonded to third surface 602 of monocrystalline substrate 600 utilizing a surface activated bonding (SAB) technique. Third surface 602 of monocrystalline substrate 600 may correspond to third surface 116 of monocrystalline layer 110 of wafer 100.
[0076] When the SAB technique is utilized, the second surface 304 of the polycrystalline substrate 300 is exposed to a beam of neutral atoms or argon (Ar) atoms, as represented by arrow 603 in FIG. 6A, to activate and clean the second surface 304 of the polycrystalline substrate 300. The second surface 304 of the polycrystalline substrate 300 may be planarized to be substantially flat and horizontal, and may be polished to have a roughness of 20 angstroms (Å) or less. In some embodiments, the second surface 304 of the polycrystalline substrate 300 may have a roughness in the range of 1 to 5 angstroms (Å), or may have a roughness equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)) prior to exposure to the beam of neutral atoms or argon (Ar) atoms.
[0077] When the SAB technique is utilized, the third surface 602 of the single crystal substrate 600 is exposed to a beam of neutral atoms or argon (Ar) atoms (not shown) to activate and clean the third surface 602 of the single crystal substrate 600. The third surface 602 of the single crystal substrate 600 may be polished to have a roughness of 20 angstroms (Å) or less, as well as planarized to be substantially flat and level. In some embodiments, the third surface 602 of the single crystal substrate 600 may have a roughness in the range of 1 to 5 angstroms (Å), or equal to the lower and upper ends of this range, prior to exposure to the beam of neutral atoms or argon (Ar) atoms (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)).
[0078] The fourth surface 610 of the second portion 602b of the single crystal substrate 600 may have a roughness of 20 angstroms (Å) or less. In some embodiments, the fourth surface 610 of the second portion 600b of the single crystal substrate 600 may have a roughness in the range of 1 to 5 angstroms (Å), or equal to the lower and upper ends of this range (e.g., the roughness may be equal to 1 angstrom (Å) or equal to 5 angstroms (Å)). This roughness of the fourth surface 610 may be obtained by polishing or planarizing the fourth surface 610.
[0079] In some embodiments, the roughness at the first surface 302 of the polycrystalline substrate 300 may be equal to or greater than the roughness of the second surface 304 of the polycrystalline substrate 300. This roughness of the first surface 302 may be obtained by polishing or planarizing the first surface 302.
[0080] After the second surface 304 of the polycrystalline substrate 300 and the third surface 602 of the single crystal substrate 600 are cleaned and activated, the single crystal substrate 600 is flipped over and the cleaned and activated third surface 602 of the single crystal substrate 600 is brought into contact with the cleaned and activated second surface 304 of the polycrystalline substrate 300, such that the cleaned and activated second surface 304 bonds with the cleaned and activated third surface 602, and the single crystal substrate 600 is naturally bonded to the polycrystalline substrate 300 at the bonding region 604. When the single crystal substrate 600 is bonded to the polycrystalline substrate 300, the sidewall 606 of the single crystal substrate 600 is flush with the sidewall 306 of the polycrystalline substrate 300. The single crystal substrate 600 has a fifth thickness T5 that extends from a third surface 602 of the single crystal substrate 600 to a fourth surface 608 of the single crystal substrate 600 opposite the third surface 602 of the single crystal substrate 600.
[0081] After a bonding step 506 in which the single crystal substrate 600 is bonded to the polycrystalline substrate 300, a first portion 600a of the single crystal substrate 600 is removed from the second portion 600b in a removing step 508. The first portion 600a may be removed from the second portion 600b by slicing the single crystal substrate 600 forming the first portion 600a and the second portion 600b. After the second portion 600b is removed from the first portion 600a, the second portion 600b of the single crystal substrate 600 may be reused to form another wafer that is the same or similar to the wafer 100, for example, by performing the bonding step 506 and the removing step 508 of the manufacturing method in the flowchart 500. By removing the first portion 600a from the second portion 600b, the sidewall 606 is divided into a first sidewall 606a of the first portion 600a and a second sidewall 606b of the second portion 600b. After the first portion 600a is removed, the second sidewall 606b of the second portion 600b remains flush and coplanar with the sidewall 306 of the polycrystalline substrate 300. After the first portion 600a is removed, the second portion 600b remains bonded to the polycrystalline substrate 300 at the bond region 604. After the first portion 600a is removed from the second portion 600b, the second portion 600b has a second thickness T2 extending between a third surface 602 of the second portion 600b and a fourth surface 610 of the second portion 600b formed by removing the first portion 600a from the second portion 600b. After the first portion 600a is removed from the second portion 600b, the first portion has a sixth thickness T6 that extends from a fourth surface 608 of the first portion 600a to a fifth surface 612 of the first portion 600a opposite the fourth surface of the first portion 600a. The sixth thickness T6 is less than the fifth thickness T5.
[0082] The second portion 600b of the monocrystalline substrate 600 may correspond to the monocrystalline layer 110 of the wafer 100, the polycrystalline substrate 300 may correspond to the polycrystalline layer 106 of the wafer 100, and the bonded region 604 may correspond to the bonded region 108 of the wafer 100. In other words, in some embodiments, the wafer 100 is fabricated after the first portion 600a is removed from the second portion 600b. In some alternative embodiments, some further processing steps, such as grinding the first surface 302 of the polycrystalline substrate 300, may be performed to complete the fabrication of the wafer 300.
[0083] Since the single crystal substrate 600 generally has a higher manufacturing cost than the polycrystalline substrate 300, by bonding the single crystal substrate 600 to the low resistivity polycrystalline substrate 300 as a support and removing the first portion 600a from the second portion 600b, the single crystal substrate 600 can be used to form multiple substrates of the wafer 100, thereby reducing the manufacturing cost. In other words, the cost of manufacturing the single crystal substrate 600 may be expensive, but the cost of manufacturing the single crystal substrate 600 can be distributed across multiple substrates of the wafer 100 manufactured using the manufacturing method as in the flowchart 500.
[0084] In an alternative embodiment of the manufacturing method of flowchart 500, the first portion 600a of the single crystal substrate 600 may be removed from the second portion 600b of the single crystal substrate 600 prior to bonding the single crystal substrate 600 to the polycrystalline substrate 300. After the first portion 600a is removed from the second portion 600b, the third surface 602 of the second portion 600b of the single crystal substrate 600 is bonded to the second surface 304 of the polycrystalline substrate 300. In other words, the removing step 508 occurs before the bonding step 506 in this alternative embodiment of the method of manufacturing the wafer 100.
[0085] Although the above method as discussed in detail with respect to the flowchart 500 of FIG. 5A is described for forming the wafer 100, the above method as discussed in detail with respect to the flowchart 500 of FIG. 5A may be modified by forming a first conductive layer on the second surface 304 of the polycrystalline substrate 300, forming a second conductive layer on the third surface 602 of the monocrystalline substrate 600 using a sputtering technique, or forming only one of the first conductive layer and the second conductive layer, and then bonding the polycrystalline substrate 300 to the monocrystalline substrate 600 utilizing both the first conductive layers or only one of the first conductive layer or the second conductive layer. This sputtering step may be performed or carried out between the first step 502 and the second step 504 of the method as discussed in detail with respect to the flowchart 500 of FIG. 5A. When this sputtering step is performed or carried out, a bonding layer 202 as shown in FIG. 2 is formed, resulting in the production of an alternative embodiment of the wafer 200.
[0086] 5A flowchart 500 is described for forming a wafer 100, the method as discussed in detail above with respect to flowchart 500 of FIG. 5A may be modified by forming a monolayer of silicon, a bilayer of carbon, a monolayer of carbon, or a layer of silicon dioxide (SiO2) on the second surface 304 of the polycrystalline substrate 300. After one of these respective material layers is formed on the second surface 304 of the polycrystalline substrate 300, in at least one embodiment, the respective material layer of the material on the second surface 304 of the polycrystalline layer is exposed to a beam of neutral atoms or argon (Ar) atoms, as represented by arrow 603.
[0087] Although not shown, the wafer 100 as shown in FIG. 6C may be further processed and refined (e.g., additional layers (e.g., conductive and non-conductive) formed on the monocrystalline layer 110, singularizing the wafer 100, backgrinding the wafer 100, etc.) and utilized in forming electronic devices and components, such as, for example, semiconductor packages or semiconductor devices. For example, a first electrode may be formed on a first side 104 of the wafer 100 and a second electrode may be formed on a second side 106 of the wafer 100 such that an electric current may pass through the wafer 100, and the wafer 100 having a low resistivity allows electrical signals to pass through the wafer 100 unimpeded.
[0088] At least one embodiment of a device of the present disclosure may be summarized as including a polycrystalline silicon carbide (SiC) wafer having a resistivity of 2 mohm-cm (milliohm-centimeter) or less.
[0089] The device may further include a bonding layer on the first surface of the polycrystalline silicon carbide (SiC) wafer.
[0090] The device may further include a monocrystalline silicon carbide (SiC) wafer on the bonding layer on the first surface of the polycrystalline silicon carbide (SiC) wafer.
[0091] The polycrystalline silicon carbide (SiC) wafer may include a second surface opposite the first surface of the polycrystalline silicon carbide (SiC) layer and a first dimension extending from the second surface to the first surface. The monocrystalline silicon carbide (SiC) wafer may include a third surface facing the first surface of the polycrystalline silicon carbide (SiC) wafer, a fourth surface facing away from the third surface and opposite the third surface, and a second dimension extending from the third surface to the fourth surface, the second dimension being different from the first dimension.
[0092] The second dimension can be less than the first dimension.
[0093] The first dimension may be less than or equal to 1000 μm (micrometers). The second dimension may be less than or equal to 1 μm (micrometers).
[0094] The device may further include a monocrystalline wafer bonded directly to the first surface of the polycrystalline silicon carbide (SiC) wafer.
[0095] The resistivity can be less than or equal to 1 mohm-cm (milliohm-centimeter).
[0096] The warpage of the polycrystalline silicon carbide (SiC) wafer can be less than 75-μm (micrometers).
[0097] The warpage of the polycrystalline silicon carbide (SiC) wafer can be less than 45-μm (micrometers).
[0098] Polycrystalline silicon carbide (SiC) wafers can have a columnar structure.
[0099] Polycrystalline silicon carbide (SiC) wafers can include grains that are 1 mm (millimeter) or smaller.
[0100] At least one embodiment of the device of the present disclosure may be summarized as including: a substrate including: a polycrystalline silicon carbide (SiC) layer including a first surface, a second surface opposite the first surface, a first dimension extending from the first surface to the second surface, and a resistivity of 2 mohm-cm (milliohm-centimeter) or less; and a monocrystalline silicon carbide (SiC) layer including a third surface on the second surface of the polycrystalline silicon carbide (SiC) layer, a fourth surface opposite the third surface, and a second dimension extending from the third surface to the fourth surface, wherein the third surface of the monocrystalline silicon carbide (SiC) layer is on a bonding layer and faces toward the first surface of the polycrystalline silicon carbide (SiC) layer, and the second dimension is less than the first dimension.
[0101] The polycrystalline silicon carbide (SiC) layer may include grains that are 1 mm (millimeter) or smaller.
[0102] The polycrystalline silicon carbide (SiC) layer may have a columnar structure.
[0103] At least one embodiment of a device of the present disclosure may be summarized as including: a polycrystalline silicon carbide substrate comprising: a first surface; a second surface opposite the first surface; a thickness extending from the first surface to the second surface that is equal to or greater than 150 μm (micrometers); a resistivity equal to or less than 2 mohm-cm (milliohm centimeters); and a warp less than 75 μm.
[0104] The resistivity can be less than or equal to 1 mohm-cm (milliohm-centimeter).
[0105] Polycrystalline silicon carbide (SiC) substrates may include grains that are 1 mm (millimeter) or smaller and may have a non-columnar structure.
[0106] The warpage can be 75 μm (micrometers) or less.
[0107] The thickness can be at least one of the following: in the range of 150 to 1000 μm (micrometers), equal to 150 μm (micrometers), and equal to 1000 μm (micrometers).
[0108] At least one embodiment of the method of the present disclosure may be summarized as including the following: a method including forming a polycrystalline silicon carbide (SiC) substrate having a resistivity of 2 mohm-cm (milliohm-centimeter) or less, forming a single crystal silicon carbide (SiC) substrate, and bonding the single crystal SiC substrate to the polycrystalline SiC substrate.
[0109] The method may further include removing the first portion of the single crystal SiC substrate from the single crystal SiC substrate, leaving a second portion of the single crystal SiC substrate bonded to the polycrystalline SiC substrate.
[0110] The second portion of the single crystal SiC substrate can have a thickness in the range of 0.3 to 2 micrometers (μm), equal to 0.3 micrometers (μm), or equal to 2 micrometers (μm).
[0111] A polycrystalline SiC substrate can be formed on a carrier in a chemical vapor deposition (CVD) chamber of a CVD tool by introducing a silicon-containing gas.
[0112] A polycrystalline SiC substrate can be formed on a carrier in a chemical vapor deposition (CVD) chamber of a CVD tool by introducing carbon gas and nitrogen gas.
[0113] A polycrystalline SiC substrate may be formed by introducing a doped powder into a reservoir of a sintering tool and sintering the doped powder in the reservoir using the sintering tool.
[0114] Sintering the doped powder can include subjecting the doped powder to a temperature of 2000 degrees Celsius (C) or greater.
[0115] Polycrystalline SiC substrates can be formed using a sublimation process.
[0116] The various embodiments described above can be combined to provide further embodiments. Aspects of the embodiments can be modified, if necessary, to employ concepts from various patents, applications, and publications to provide further embodiments.
[0117] These modifications can be made to the embodiments in light of the above detailed description. In general, in the following claims, the terms used should not be construed to limit the scope of the claims to the specific embodiments disclosed in the specification and claims, but should be construed to include all possible embodiments along with the full scope of equivalents to which such claims are entitled. Accordingly, the claims are not limited by this disclosure.
Claims
1. A device, comprising: a polycrystalline silicon carbide (SiC) wafer having a resistivity of 2 mohm-cm (milliohm-centimeter) or less, the polycrystalline silicon carbide (SiC) wafer including a first surface having a roughness of 20 angstroms (Å) or less; a monocrystalline silicon carbide (SiC) wafer bonded to the first surface of the polycrystalline silicon carbide (SiC) wafer; A device comprising:
2. 10. The device of claim 1, further comprising a bonding layer on the first surface of the polycrystalline silicon carbide (SiC) wafer.
3. 3. The device of claim 2, wherein the single crystal silicon carbide (SiC) wafer is on the bonding layer on the surface of the polycrystalline silicon carbide (SiC) wafer and is bonded to the first surface of the polycrystalline silicon carbide (SiC) wafer by the bonding layer.
4. The polycrystalline silicon carbide (SiC) wafer is a second surface of a polycrystalline silicon carbide (SiC) layer opposite the first surface; and a first dimension extending from the second surface to the first surface; The single crystal silicon carbide (SiC) wafer is a third surface facing the first surface of the polycrystalline silicon carbide (SiC) wafer; and a fourth surface facing away from and opposite the third surface; and 4. The device of claim 3, comprising a second dimension extending from the third surface to the fourth surface, the second dimension being different than the first dimension.
5. The device of claim 4 , wherein the second dimension is less than the first dimension.
6. the first dimension is less than 1000 μm (micrometers); The device of claim 5 , wherein the second dimension is equal to or less than 1 μm (micrometer).
7. 10. The device of claim 1, wherein the single crystal silicon carbide (SiC) wafer is directly and physically bonded to the first surface of the polycrystalline silicon carbide (SiC) wafer.
8. The device of claim 1 , wherein the resistivity is less than or equal to 1 mohm-cm (milliohm-centimeter).
9. The device of claim 1 , wherein the polycrystalline silicon carbide (SiC) wafer has a bow of less than 75-μm (micrometer).
10. 9. The device of claim 8, wherein the bow of the polycrystalline silicon carbide (SiC) wafer is less than 45-μm (micrometer).
11. The device of claim 1 , wherein the polycrystalline silicon carbide (SiC) wafer has a columnar structure.
12. 10. The device of claim 1, wherein the polycrystalline silicon carbide (SiC) wafer comprises grains that are 1 mm (millimeter) or smaller.
13. A device comprising a substrate, the substrate comprising: A polycrystalline silicon carbide (SiC) layer, A first surface; and a second surface opposite the first surface; and a first dimension extending from the first surface to the second surface; a polycrystalline silicon carbide (SiC) layer having a resistivity of 2 mohm-cm or less; a monocrystalline silicon carbide (SiC) layer bonded to the second surface of the polycrystalline silicon carbide (SiC) layer, a third surface on the second surface of the polycrystalline silicon carbide (SiC) layer; and a fourth surface opposite the third surface; and a second dimension extending from the third surface to the fourth surface; and wherein the third surface of the monocrystalline silicon carbide (SiC) layer is on a bonding layer and faces toward the first surface of the polycrystalline silicon carbide (SiC) layer, and the second dimension is less than the first dimension.
14. 14. The device of claim 13, wherein the polycrystalline silicon carbide (SiC) layer includes grains that are 1 mm (millimeter) or smaller.
15. The device of claim 13 , wherein the polycrystalline silicon carbide (SiC) layer has a columnar structure.
16. A device comprising a polycrystalline silicon carbide substrate, The polycrystalline silicon carbide substrate is A first surface; and a second surface opposite the first surface; and a thickness extending from the first surface to the second surface, the thickness being equal to or greater than 150 μm (micrometers); A resistivity of 2 mohm-cm or less (milliohm-centimeter); and a warpage of less than 75 μm.
17. The device of claim 16, wherein the resistivity is less than or equal to 1 mohm-cm (milliohm-centimeter).
18. 17. The device of claim 16, wherein the polycrystalline silicon carbide (SiC) substrate comprises grains that are 1 mm (millimeter) or smaller and has a columnar structure.
19. 17. The device of claim 16, wherein the warpage is less than or equal to 75 μm (micrometers).
20. 17. The device of claim 16, wherein the thickness is at least one of the following: in the range of 150 to 1000 μm (micrometers), equal to 150 μm (micrometers), and equal to 1000 μm (micrometers).
21. forming a polycrystalline silicon carbide (SiC) substrate having a resistivity of 2 mohm-cm or less; Providing a single crystal silicon carbide (SiC) substrate; bonding the single crystal SiC substrate to the polycrystalline SiC substrate; A method comprising:
22. 22. The method of claim 21 , further comprising removing a first portion of the single crystal SiC substrate from the single crystal SiC substrate leaving a second portion of the single crystal SiC substrate bonded to the polycrystalline SiC substrate.
23. 23. The method of claim 22, wherein the second portion of the single crystal SiC substrate has a thickness in a range of 0.3 to 2 micrometers (μm), equal to 0.3 micrometers (μm), or equal to 2 micrometers (μm).
24. 22. The method of claim 21 , wherein the polycrystalline SiC substrate is formed on a carrier in a chemical vapor deposition (CVD) chamber of a CVD tool by introducing a silicon-containing gas.
25. 25. The method of claim 24, wherein the polycrystalline SiC substrate is formed on the carrier in the CVD chamber of the CVD tool by introducing carbon gas and nitrogen gas.
26. 22. The method of claim 21 , wherein the polycrystalline SiC substrate is formed by introducing a doped powder into a reservoir of a sintering tool and sintering the doped powder in the reservoir with the sintering tool.
27. 27. The method of claim 26, wherein sintering the doped powder comprises exposing the doped powder to a temperature of 2000 degrees Celsius (C) or greater.
28. 22. The method of claim 21 , wherein the polycrystalline SiC substrate is formed using a sublimation process.
29. 22. The method of claim 21 , wherein bonding the single crystal SiC substrate to the polycrystalline SiC substrate further comprises directly physically bonding a first surface of the single crystal SiC substrate to a second surface of the polycrystalline SiC substrate.
Citation Information
Cited By
SiC bonded substrate and semiconductor device
JP7816659B1
SiC bonded substrates and semiconductor devices
JP7841668B1
SiC bonded substrates and semiconductor devices
JP7841669B1
SiC bonded substrates and semiconductor devices
JP7841670B1
Digital-to-analog converter
US12355466B2