Method of manufacturing screen mask
The described method enhances screen mask manufacturing by improving positional accuracy through alignment marks and maskless exposure, addressing the need for precise alignment in miniaturized electronic components.
Patent Information
- Application Number
- JP2023060937
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-04
- Publication Date
- 2024-10-17
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
There is a need for a screen mask manufacturing method that can improve positional accuracy, particularly in the context of miniaturized and high-quality electronic components.
A method involving a first and second film forming process, alignment process, detection of positional information from alignment marks, and exposure processes to enhance positional accuracy, utilizing maskless exposure techniques and alignment marks on the screen mask.
The method improves positional accuracy to 3 μm, reducing thermal expansion effects and eliminating the need for seasoning, while enabling precise alignment and three-dimensional pattern formation.
Smart Images

Figure 2024148051000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a screen mask. [Background technology]
[0002] Screen printing, which is one of the printing techniques, is a method of forming an arbitrary print on a substrate by using a screen mask having a predetermined pattern opening formed of a resin composition on a mesh substrate. This screen printing method is used for various printing such as printing of wiring, electrodes, fluorescent materials, etc., and is used in various fields including electronic parts.
[0003] In recent years, the miniaturization and high quality of electronic components has created a demand for high-precision screen masks.
[0004] For example, a screen mask includes a mesh having holes through which a coating material can pass, and a mask film having a pattern opening provided in the mesh. The pattern opening formed in the mask film has a shape corresponding to, for example, a printing pattern and a predetermined width. For example, after an emulsion that forms the mask film is applied to the mesh, the pattern opening is formed by an exposure process. In such a screen mask, the mask film may be formed by stacking multiple emulsion layers. For example, a positioning member that positions the frame of the mesh is provided on the stage, and multiple layers are exposed to light using an exposure pattern based on the positioning member. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2013-169783 A Summary of the Invention [Problem to be solved by the invention]
[0006] There is a demand for a method of manufacturing such a screen mask that can improve the positional accuracy. [Means for solving the problem]
[0007] A method for manufacturing a screen mask according to one embodiment includes a first film formation process for forming a first layer on a substrate, a first exposure process for exposing the first layer, a second film formation process for forming a second layer on the first layer, an alignment process for forming an alignment mark on the substrate or the first layer, a detection process for detecting position information of the alignment mark, and a second exposure process for exposing the second layer based on the position information. Effect of the Invention
[0008] According to an embodiment of the present invention, it is possible to provide a method for manufacturing a screen mask that can improve positional accuracy. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a plan view of a screen printing apparatus according to a first embodiment. [Diagram 2] FIG. [Diagram 3] FIG. 2 is a plan view showing a configuration of a portion of the screen mask according to the embodiment. [Figure 4] FIG. 2 is a cross-sectional view showing a configuration of a portion of the screen mask. [Diagram 5] 3A to 3C are explanatory views showing a method for manufacturing the screen mask. [Figure 6] 3A to 3C are explanatory views showing a method for manufacturing the screen mask. [Figure 7] FIG. 13 is a perspective view showing a configuration of a portion of a screen mask according to another embodiment. [Figure 8] FIG. 3 is a cross-sectional view of the screen mask according to the embodiment. [Figure 9] 8A to 8C are explanatory views showing a method for manufacturing a screen mask according to another embodiment. [Figure 10] 8A to 8C are explanatory views showing a method for manufacturing a screen mask according to another embodiment. [Figure 11] 8A to 8C are explanatory views showing a method for manufacturing a screen mask according to another embodiment. [Figure 12] 8A to 8C are explanatory views showing a method for manufacturing a screen mask according to another embodiment. [Figure 13] FIG. 11 is a plan view of a screen printing apparatus according to another embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] [First embodiment] A screen printing apparatus 10 and a screen mask 20 according to a first embodiment of the present invention will be described below with reference to Figs. 1 to 5. Fig. 1 is a plan view showing the screen printing apparatus 10 according to this embodiment, and Fig. 2 is a cross-sectional view. Fig. 3 is a cross-sectional view of the screen mask 20, and Figs. 4, 5, and 6 are plan views, cross-sectional views, and perspective views showing a portion of the configuration of the screen mask 20. Note that in each figure, the configuration is enlarged, reduced, or omitted as appropriate for the purpose of explanation. In the figures, arrows X, Y, and Z respectively indicate three directions that are mutually perpendicular.
[0011] As shown in FIG. 1, the screen printing apparatus 10 includes a screen mask 20, a squeegee 13 configured to be movable while in contact with the back surface (other surface) 20b opposite the printing surface of the screen mask 20, a moving unit for moving the squeegee 13, and a support unit 12 for supporting the screen mask 20 facing the printing medium.
[0012] The screen printing apparatus 10 forms various printing materials in a predetermined pattern on the surface of a printing medium. For example, the screen printing apparatus 10 is used in the manufacture of chip components (capacitors, chip resistors, inductors, thermistors, etc.), touch panels, liquid crystal display (LCD) seals, LTCC (Low Temperature Co-fired ceramics) substrates, solar cell electrodes, and other electronic components.
[0013] 1 to 6, the screen mask 20 includes a frame 21, a mesh 22 which is a base material stretched over the frame 21, and a mask film 23 formed on the mesh 22. In the screen mask 20, the side which faces the surface of the printing medium when printing is performed is called the front side, and the opposite side to which the coating material is supplied is called the back side.
[0014] The frame 21 has two pairs of parallel edges and is configured in a frame shape with, for example, a rectangular opening of a desired size. The frame 21 supports the outer periphery of the mesh 22, and the mesh 22 is stretched over the opening. As an example, in this embodiment, a frame 21 with an opening dimension of 275 mm in the Y direction and 275 mm in the X direction is used.
[0015] The frame 21 also functions as a frame for holding a predetermined amount of coating material on the rear surface side of the mask film 23. The frame 21 and the mesh 22 are joined at their joints by, for example, a synthetic rubber-based or cyanoacrylate-based adhesive.
[0016] The mesh 22 is a woven fabric formed by weaving warp threads 22a and weft threads 22b, and has a large number of holes 22c that are open to allow the coating material to pass through. The warp threads 22a and weft threads 22b are wires made of metal such as stainless steel, or fibers made of resin such as polyester. The warp threads 22a and weft threads 22b each extend obliquely with respect to the moving direction (first direction) of the squeegee 13, for example.
[0017] A mask film 23 having a predetermined pattern opening 24 is formed on the mesh 22. That is, the mesh 22 holds the mask film 23 in the opening portion of the frame 21.
[0018] The mask film 23 is a layer made of a photocurable resin composition, such as PVA, PVAc, silicone resin, acrylic resin, epoxy resin, etc. For example, the mask film 23 has a multi-layer structure having a plurality of layers. For example, in this embodiment, the mask film 23 has a two-layer structure in which a base layer 23b and a cover layer 23c are laminated as shown in FIG. 4. As an example, the cover layer 23c is made of a material that is softer than the base layer 23b.
[0019] The mask film 23 is configured to have a thickness of, for example, 10 μm to 100 μm.
[0020] The mask film 23 is formed on the mesh 22 and placed in the opening portion of the frame 21. A predetermined pattern opening 24 for printing is formed in the mask film 23 by exposure.
[0021] Furthermore, the mask film 23 may have steps such as recesses 25 in addition to the pattern openings 24 which are through holes.
[0022] The minimum opening width of the pattern opening 24, i.e., the width dimension of the opening at the narrowest part of the pattern opening 24, is 30 μm or less. Here, as an example, the dimension at the surface of the mask film 23, i.e., the surface facing the printing medium, is used as the standard.
[0023] The pattern opening 24 is a pattern hole having a shape corresponding to the printing pattern, and constitutes a slit penetrating the mask film 23 in the thickness direction (depth direction). The pattern opening 24 is configured to be able to hold a coating material. The shape of the printing pattern can be set appropriately. As an example, in this embodiment, the pattern shape has a plurality of identical pattern units arranged in a matrix.
[0024] As an example, the pattern opening 24 has a different depth dimension depending on the location. For example, the pattern opening 24 may have a plurality of independent openings, or may be a continuous opening with a different thickness depending on the location. For example, in a continuous line-shaped pattern opening 24, the coating thickness may be increased or decreased in some parts, or a plurality of pattern openings 24 with different coating thicknesses may be formed. For example, the pattern opening 24 can be set to various shapes, such as a slit-shaped line pattern, an angular opening, a circular opening, or the like.
[0025] Mask film 23 constitutes a printed portion where no photosensitive resin is present in pattern openings 24 and where the coating material can pass through holes in mesh 22 from the back surface to the front surface. Areas of mask film 23 other than pattern openings 24 and where holes in mesh 22 are blocked with photosensitive resin constitute non-printed portions that do not allow ink as a coating material to pass through.
[0026] Also, an alignment mark AM is formed at a corner of the mask film 23 outside the effective area A3. For example, the alignment mark AM is configured in a cross shape, and is configured to be detectable with the center position of this cross as a reference position. For example, the alignment mark AM is an indicator that can optically detect position information by having an opening or an OD value or color different from the surroundings. In this embodiment, the alignment mark AM is formed as a cross-shaped opening. The alignment mark AM is configured by removing a part of the mask film 23 by exposure and development. For example, the alignment mark AM is formed at each of the four corners of the mask film 23 on the mesh 22 outside the effective area A3 and within the frame 21.
[0027] The mesh 22 on which the mask film 23 is formed is configured to be elastically deformable so that it is flexed and deformed by, for example, the pressing force of the squeegee 13 and restored to its original shape when the pressing force is released. With the coating material held in the pattern openings 24 of the mask film 23, the mask film 23 is moved toward and away from the printing medium due to the elastic deformation of the mesh 22, whereby the coating material is transferred from the pattern openings 24 to the printing medium arranged opposite the printing surface side of the mask film 23.
[0028] The squeegee 13 is made of, for example, urethane rubber, silicone rubber, synthetic rubber, metal, plastic, or other material, and is formed, for example, in a thin plate shape. For example, the squeegee 13 is chamfered so that the thickness of the tip is reduced. The squeegee 13 is configured to be movable relative to the frame 21. For example, the squeegee 13 has a length that covers the entire length of the area of the mask film 23 in a direction perpendicular to the movement direction. The tip portion of the squeegee 13 abuts against the back surface of the screen mask 20 and is pressed against the front surface, and moves in the movement direction along the arrow in FIG. 1 to press the entire surface of the mask film 23 and push the coating material out to the front surface from the pattern openings 24 in which the coating material has been previously filled.
[0029] The support unit 12 supports the frame 21 in parallel with and at a predetermined interval from the print medium. For example, the support unit 12 includes a plurality of positioning pins 12a that regulate the position of the frame 21. The moving unit moves the squeegee 13 in a predetermined direction at a predetermined speed.
[0030] Next, a method for manufacturing the screen mask 20 according to the present embodiment will be described with reference to FIGS. 5 and 6. FIGS. 5 and 6 are explanatory diagrams showing the method for manufacturing the screen mask 20. The method for manufacturing the screen mask 20 includes a first layer forming step ST1 (first film forming process), a first patterning step ST2 (first exposure process), a first etching step (first development step) ST3, a second layer forming step ST4 (second film forming process), a second patterning step ST5 (second exposure process), and a second etching step (second development step) ST6. The method for manufacturing the screen mask 20 also includes an alignment process for forming an alignment mark on the base material or the first layer, and a detection process for detecting position information of the alignment mark AM at a predetermined timing after the alignment process and before the second patterning process. As an example, in this embodiment, the alignment mark AM is formed by the first patterning process, so the alignment process is included in the first patterning process.
[0031] In the first layer forming step ST1, the first emulsion Pm1 is applied to a support material having holes through which the coating material can pass, to form a first emulsion layer. The first emulsion Pm1 is, for example, a photocurable resin, and is a liquid that includes, for example, polyvinyl alcohol (PVA), polyvinyl acetate (PVAc), silicone resin, acrylic resin, epoxy resin, and the like. Specifically, first, in a state in which the mesh 22 is attached to the frame of the frame 21 so as to be substantially flat, the first emulsion Pm1 is applied onto the mesh 22 to form a flat base layer 23b on the mesh 22. At this time, since the thickness changes depending on the number of times of application, application is repeated multiple times as necessary. In addition, the film thickness is measured after drying, and additional coating may be performed depending on the circumstances. In this embodiment, the thickness of the emulsion Pm1 is set so that the emulsion thickness of the first emulsion layer is about 5 to 20 μm after drying.
[0032] Next, a first patterning step ST2 is performed in which the first emulsion layer is exposed to a predetermined first exposure pattern. As the first patterning step ST2, as shown in FIG. 6, a maskless exposure process is performed by a maskless exposure device 50 (maskless exposure machine). The exposure device 50 is an exposure device that draws a drawing pattern based on a preset target CAD data directly on the screen mask 20 by an irradiation head 52 without using a photomask. The exposure device 50 includes a support device 51 having a positioning pin AP, an irradiation head 52, an optical sensor 53, and a control unit 54 that controls the operation of each unit. The control unit 54 performs an exposure process in which light is irradiated from the printing surface side. Specifically, in a predetermined exposure pattern area, the surface side of the emulsion Pm is placed facing an irradiation head such as an ultraviolet lamp or an ultraviolet LED, and light is irradiated by the irradiation head to illuminate the surface of the emulsion Pm1. For example, a plurality of positioning pins AP are provided on the outer periphery of screen mask 20, and one or a plurality of positioning pins AP are provided on each of the outer sides of two sides in two different directions, similar to positioning pin 12a shown in FIG.
[0033] For example, in ST2, in a predetermined exposure pattern region, the surface side of the base layer 23b is placed facing an illumination such as an ultraviolet lamp or an ultraviolet LED, and light is irradiated from the illumination to illuminate the surface of the emulsion. A first exposed portion of the base layer 23b that is exposed by the first exposure process becomes a first cured portion Pa1 that is cured by ultraviolet light. On the other hand, a first non-exposed portion of the base layer 23b that is a portion other than the first exposed portion becomes an uncured portion Pb1 where the emulsion does not harden. The first uncured portion Pb1 (first non-exposed portion) constitutes a first removal target portion that forms the base opening 24b and the alignment mark AM by being removed in a later process. That is, in this embodiment, in the first patterning process, the portion that becomes the pattern opening 24 or the alignment mark AM is the uncured portion (first uncured portion Pb1), and the other region is the first cured portion Pa1.
[0034] The base layer 23b is patterned as described above, and is later removed by an etching process to form a first removal target portion in a portion including the base opening 24b and the alignment opening AMb constituting the alignment mark AM. That is, in this embodiment, the alignment mark AM is formed by the first patterning process. In other words, in this embodiment, the alignment process is included in the first patterning process.
[0035] Then, in a first etching step ST3 (first developing step), at least one side of the mask film is washed away with water or a solvent. This process forms a base opening 24b and an alignment opening AMb that penetrate from the front side to the back side in the thickness direction where the uncured portion Pb1 of the emulsion Pm1 is washed away.
[0036] Next, in the second layer forming step ST4, a coating process is performed to coat the base layer 23b with the second emulsion Pm2, so that the cover layer 23c is formed on the printing surface side of the base layer 23b by the second emulsion Pm2. At this time, since the thickness changes depending on the number of coatings, coating is repeated multiple times as necessary. In addition, the film thickness is measured after drying, and additional coating may be performed depending on the circumstances. In this embodiment, the thickness of the emulsion Pm2 is set so that the milk thickness of the cover layer 23c after drying is about 2 to 50 μm. In this second layer forming step ST4, the cover layer 23c is also formed in the alignment opening AMb. In this case, the need for a seasoning step is significantly reduced.
[0037] Next, a second patterning process ST5 is performed in which exposure is performed with a second exposure pattern different from the first exposure pattern. In the second patterning process ST5, a second maskless exposure process is performed, for example, by maskless exposure without using a photomask. At this time, the optical sensor 53 detects the OD value of the target area, detects the alignment mark formed on the base layer 23b from the difference in OD value with the surroundings, and obtains position information. Then, the position of the second exposure is determined based on the position information.
[0038] Specifically, the surface side of the emulsion Pm2 is placed in a predetermined second exposure pattern area facing an illumination such as an ultraviolet lamp or an ultraviolet LED, and light is irradiated from the illumination to illuminate the surface of the emulsion Pm2. The second exposure process hardens the ultraviolet ray-irradiated portion of the emulsion Pm2 corresponding to the portion of the exposure pattern area. That is, the second exposed portion of the cover layer 23c, which is the portion exposed by the second exposure process, forms the second hardened portion Pa2 that is hardened by the ultraviolet ray. A part of the second hardened portion Pa2 forms the wall of the pattern opening 24. On the other hand, the second non-exposed portion of the cover layer 23c, which is the portion excluding the second exposed portion, becomes the second unhardened portion Pb2 where the emulsion does not harden. The second unhardened portion Pb2 forms the second removal target portion including the cover opening 24c that will be removed in a later process to become the pattern opening 24 and the alignment opening AMc that forms the alignment mark AM. In the present embodiment, in the second patterning step, the portions that will become the pattern openings 24 and the alignment marks AM are designated as second uncured portions Pb2, and the other regions are designated as second cured portions Pa2.
[0039] The first exposure process and the second exposure process are both maskless exposure processes in which light is irradiated from the printing surface side, and the regions corresponding to the exposure patterns are hardened by exposing with a predetermined pattern. At this time, various three-dimensional shapes such as openings, recesses, or protrusions with steps can be easily formed by exposing with a second exposure pattern different from the first exposure pattern. For example, steps can be formed by making the patterning of the base opening 24b and the cover opening 24c different.
[0040] Thereafter, in a second etching step ST6 (second developing step), at least one side of the mask film is washed away with water or a solvent. By this treatment, the uncured portion Pb2 of the emulsion Pm2 is washed away, and a pattern opening 24 penetrating from the front side to the back side in the thickness direction is formed.
[0041] Next, a method for producing a printed matter by a screen printing method using the screen printing apparatus 10 according to the present embodiment will be described with reference to Figures 1 and 2. First, the front side of the screen mask 20 is placed facing the front surface of the print medium 30. At this time, the screen mask 20 is positioned by a positioning member such as the positioning pin 12a, for example.
[0042] Then, a highly viscous paste-like coating material is supplied from the back side of the screen mask 20, that is, the side opposite the print medium, and the coating material is filled into the pattern openings 24.
[0043] Next, the squeegee 13 is placed on the back surface of the screen mask 20, i.e., the surface opposite to the printing surface side. At this time, for example, the squeegee 13 is placed at a predetermined angle inclined with respect to the front surface of the printing medium. Then, the squeegee 13 is moved at a predetermined speed while pressing the mesh 22 and the back surface of the mask film 23 toward the printing medium side with a predetermined printing pressure. The squeegee 13 presses the mask film 23 in an area covering the entire back surface of the mask film 23. The pressure of the squeegee 13 causes the mask film 23 to deform so that the pressed portion is displaced toward the front side and comes into contact with the printing medium. The coating material pressed by the passage of the squeegee 13 is pushed out from the pattern opening 24 toward the printing medium side.
[0044] After the squeegee 13 has passed, the mask film 23 and mesh 22 deform so as to restore their original shape and are separated from the print medium, while a portion of the coating material is transferred and remains on the print medium, thereby printing a pattern on the print medium and completing the print. At this time, a portion of the back side of the coating material remains on the mask film 23 side. The coating material may be any of a variety of materials including, for example, metal materials and resin materials, and a variety of materials are used depending on the type of printing object, for example, electronic components, displays, etc.
[0045] According to the manufacturing method of the screen mask 20 configured as above, during the second exposure process, position information is detected from the alignment marks AM formed on the mesh 22 or the base layer 23b, thereby improving the positional accuracy. For example, in Comparative Example 1 in which the first base layer 23b and the second cover layer 23c are aligned only by the positioning pins AP, the alignment accuracy is 10 μm, whereas according to the manufacturing method of the above embodiment, the alignment is performed based on information detected by the alignment marks AM in addition to the positioning pins AP, resulting in an alignment accuracy of 3 μm, thereby improving the accuracy.
[0046] For example, in general, a screen mask is subjected to a thermal load during the manufacturing process, etc., which can cause misalignment due to thermal expansion, theta rotation, or overall expansion / contraction. Screen masks in particular are more susceptible to deformation than, for example, glass materials, due to tension being applied to the mesh, but according to the above embodiment, alignment marks are formed in advance on the first mesh or base layer, making it possible to effectively suppress misalignment during drawing on the second cover layer due to theta rotation or overall expansion / contraction.
[0047] For example, in this embodiment, the mask film 23 has a base layer 23b and a cover layer 23c, and an exposure pattern can be set for each of the multiple layers, so that a three-dimensional shape can be easily created.
[0048] Furthermore, according to this embodiment, since alignment is performed based on the alignment mark AM formed on the mesh 22 or the mask film 23, it is not necessary to consider positional deviation due to thermal expansion, and the need for seasoning can be reduced. That is, in the past, seasoning was necessary due to the effect of applying temperature to dry the emulsion after applying the cover layer, and it was difficult to adjust the positional accuracy, but according to this embodiment, alignment can be performed based on the alignment mark AM formed on the mesh 22 or the mask film 23, and the need for seasoning can be reduced.
[0049] In particular, in the case of a screen mask, there are areas where it is difficult to detect the position due to the presence of a mesh and a translucent emulsion, but by detecting the alignment mark AM formed on the mesh or mask film, the position can be easily detected.
[0050] The configuration and arrangement of the pattern openings 24 are not limited to the above, and can be changed as appropriate according to the printing shape, and the height can also be set. For example, an example with a step is shown, but this is not limited to this. As an example, the same opening may be formed in two layers, or the inner wall of the opening in the first layer may be formed in the second layer. Therefore, it is possible to form a three-dimensional pattern including a pattern opening 24 that opens in both directions, or a recess formed by partially removing only one layer, for example, the cover layer 23c.
[0051] For example, as another embodiment, a configuration may be made in which, in addition to the pattern opening 24, a recess 25 in which only the cover layer 23c is open, as in the screen mask 20A shown in FIG. 7 to FIG. 9. For example, in this embodiment, after performing the processes ST1 to ST4 in the same manner as in the first embodiment, the cover layer 23c forms an uncured region in a different position from the cured region of the base layer 23b as a second exposure process ST15 in addition to a position overlapping with the opening of the base layer 23b. For example, at the same time as the pattern opening 24, exposure is performed with an exposure pattern in which the portion that becomes the recess 25 is uncured. That is, the base layer 23b is cured by the second exposure process, and an uncured portion of the cover layer 23c is formed. By subsequently performing the development process ST16, the recess 25 and the step can be formed by etching in the same process as the pattern opening 24. For example, by forming an opening in the cover layer 23c overlapping the portion where the base layer 23b is cured, only the cover layer 23c is removed, and the recess 25 in which the base layer 23b remains can be formed. Furthermore, for example, by making the opening in the cover layer 23c wider than the opening in the base layer 23b, a step can be formed in which the opening expands, and conversely, by forming an opening in the cover layer 23c that is narrower than the opening in the base layer 23b, a step can be formed in which the opening shrinks.
[0052] According to this embodiment, by differentiating the exposure patterns of the layers 23b and 23c, it is possible to form any desired recess or step shape.
[0053] For example, in the above embodiment, the first layer is developed to open, and then the second layer is formed, but this is not limited to this. For example, as another embodiment, as shown in Fig. 10, after the first exposure process ST2, the first development process ST3 may be omitted, a cover layer 23c may be formed (ST4), and the uncured portions of the base layer 23b and the cover layer 23c may be simultaneously removed in the development process ST6 after the second exposure process ST5.
[0054] In the above embodiment, an example in which the alignment mark is formed as an opening in the mask film is shown, but the present invention is not limited to this. For example, it is sufficient if the exposure shape can be optically detected as an alignment mark. For example, as shown in FIG. 11, as another embodiment, the opening may be blocked with a cover layer 23c. That is, during the second exposure process, the alignment mark AM portion may be left blocked without being removed by etching. Even in this case, since the wall of the opening in the base layer 23b can be optically detected, position information can be detected by detecting the OD value, as in the case of the above opening. Furthermore, the position information is not limited to the OD value, and various position information such as color and brightness can be used.
[0055] In addition, the alignment mark AM is an opening in the mask film 23, but is not limited thereto. For example, the alignment mark AM may be provided on the mesh 22 instead of the mask film 23. The alignment mark AM may be formed on the support mesh 27. For example, in the example shown in FIG. 11 as another embodiment, after the first layer forming step ST1 (first film forming process) and before the first patterning step, a photosensitive coloring sheet SP such as Sun Art Paper is attached to the exposed surface of the mesh 22 (ST21). Then, in the first patterning step ST22 (first exposure process) in which the first emulsion layer is exposed in the same manner as the first exposure process of the first embodiment, the attached photosensitive coloring sheet SP is exposed at the same time. This exposure forms a photosensitive portion Sa and a non-photosensitive portion Sb on the photosensitive coloring sheet SP. Then, the photosensitive coloring sheet SP is subjected to a development process (ST23) to form an image that becomes the alignment mark AM. Specifically, an alignment mark AM is formed having a colored portion formed by the photosensitive portion Sa and a non-colored portion Sc formed by the non-photosensitive portion Sb, and position information can be detected by detecting the OD value. Thereafter, similar to the second layer forming step ST4, the second patterning step ST5, and the second etching step ST6 of the first embodiment, the second layer forming step ST24, the second patterning step ST25, and the second etching step ST26 are sequentially performed. The second layer forming step ST24, the second patterning step ST25, and the second etching step ST26 may not be performed on the area of the support mesh 27, or the same processes may be performed on the support mesh 27 at the same time as the processes ST24, ST25, and ST26 on the main mesh 26. Although the colored and non-colored parts are described, the present invention is not limited to this, and the position information may be indicated by other elements such as color saturation, brightness, or darkness depending on the part. In this embodiment, too, by detecting the positions of the alignment marks AM formed on the photosensitive color developing sheet SP on the mesh 22 during the second exposure process, the positional accuracy can be improved, similarly to the first embodiment and the like.
[0056] In addition, in each of the above embodiments, a so-called single mesh has been exemplified as the mesh 22, but the present invention is not limited to this. For example, the mesh 22 may have a so-called combination mesh structure including a main mesh 26 and a support mesh 27 provided on the outer periphery of the main mesh 26. Also, the mask film 23 may be formed only on a part of the center portion of the mesh 22, or the mask film 23 may be formed over the entire area.
[0057] The alignment mark AM may be formed in the area of the main mesh 26 or on the support mesh 27. For example, in the example shown in FIG. 12 and FIG. 13 as another embodiment, the mesh 22 may be a combination type, and the alignment mark AM may be formed on the support mesh 27. The method for manufacturing a screen mask according to this embodiment includes a first layer forming step ST1 (first film forming process), a first patterning step ST2 (first exposure process), a first etching step (first developing step) ST3, a second layer forming step ST4 (second film forming process), a second patterning step ST5 (second exposure process), and a second etching step (second developing step) ST6, similar to the first embodiment. In this embodiment, when performing the processes ST1, ST2, ST3, and ST4 of the first embodiment, an alignment mark AM is formed at the position of the support mesh 27. Furthermore, in ST5 and ST6, the second layer formation process ST4, the second patterning process ST5, and the second etching process ST6 are performed in the area of the main mesh 26. In this case, too, by detecting the position of the alignment mark AM on the support mesh 27, the positional accuracy can be improved, as in the first embodiment, etc.
[0058] Alternatively, alignment marks may be formed by making the optical characteristics of exposed and unexposed areas different from each other without forming openings by etching. For example, it is possible to make a difference in color characteristics, brightness characteristics, or OD values between exposed and unexposed areas, and detect the difference as position information.
[0059] In addition, the shapes of the pattern openings 24 and recesses 25 of the mask film 23 are not limited to those in the above embodiment. For example, the pattern openings 24 may be openings whose cross-sectional shape changes in the depth direction, and the depths of the pattern openings 24 and recesses 25 can be set. Alternatively, it is possible to form a protrusion continuous with the openings 24. For example, openings of different depths may be formed, and the coating amount of the coating material may be adjusted according to the depth of the pattern openings 24. That is, the coating height is high in the area where the pattern openings 24 are configured deep, and the coating height is low in the area where the pattern openings 24 are configured shallow. Therefore, the screen mask 20 can be used to print a pattern shape having regions of different thicknesses, and three-dimensional patterning can be realized.
[0060] Also, features of the different embodiments described above may be combined.
[0061] The present invention is not limited to the above-described embodiments, and in the implementation stage, the components can be modified and embodied without departing from the spirit of the invention.
[0062] In each of the above embodiments, when the first emulsion and the second emulsion are used, the first emulsion Pm1 and the second emulsion Pm2 may be made of different materials or the same material.
[0063] In addition, each component exemplified in the above embodiment may be deleted, and the shape, structure, material, etc. of each component may be changed. Various inventions can be formed by appropriate combinations of the multiple components disclosed in the above embodiment. By adjusting the dimensional ratio of the material, the difference in the amount of stretch between the length and width can be reduced, thereby improving printing accuracy. [Explanation of symbols]
[0064] 10...screen printing device, 13...squeegee, 20...screen mask, 21...frame, 22...mesh, 22a...warp thread, 22b...weft thread, 22c...hole portion, 23...mask membrane, 23b...base layer, 23c...cover layer, 24...pattern opening, 26...main mesh, 27...support mesh, AM...alignment mark, Pa1...first hardened portion, Pa2...second emulsion hardened portion, Pb1...first unhardened portion, Pb2...second unhardened portion, Pm1...first emulsion, Pm2...second emulsion.
Claims
1. a first film formation process for forming a first layer on a substrate; a first exposure process for exposing the first layer to light; a second deposition process for depositing a second layer on the first layer; an alignment process for forming an alignment mark on the substrate or the first layer; A detection process for detecting position information of the alignment mark; a second exposure process for exposing the second layer based on the position information; Equipped with A method for manufacturing a screen mask.
2. The substrate has holes through which a coating material can pass, The method for manufacturing a screen mask according to claim 1 , wherein openings having different patterns are formed in the first layer and the second layer by the first exposure process and the second exposure process, respectively.
3. The method of claim 1 , wherein the alignment mark is formed in the first layer by the first exposure process.
4. The alignment mark is formed on the substrate before a first film formation process. A method for manufacturing the screen mask according to claim 1 .
5. The method for manufacturing a screen mask according to claim 1 , wherein the first exposure process and the second exposure process are maskless exposures in which light is irradiated from one side of the base material.
6. The method for manufacturing a screen mask according to claim 4 , wherein the alignment marks are formed by a photosensitive color developing sheet attached to the base material.
7. The method of claim 1 , wherein the alignment mark is an opening formed in the first layer and is covered by the second layer.
Citation Information
Patent Citations
Manufacture of color filter
JP1997171106A
Metal mask and its manufacturing process
JP2008254344A
Screen printing mask manufacturing method for multilayer film structure
JP2009066932A
Mask and method of manufacturing the same
JP2010247500A
Method for manufacturing screen printing plate
JP2015064454A