Method for manufacturing photoelectric conversion element and photoelectric conversion element

By forming a dielectric layer with neutralizing electrons and a transparent conductive layer using specific deposition methods, the method addresses charge-up issues in photoelectric conversion elements, reducing dark current and enhancing charge extraction efficiency.

JP2024148314APending Publication Date: 2024-10-18NIPPON HOSO KYOKAI
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023061348
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-05
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Existing photoelectric conversion elements face issues with increased dark current and reduced signal-to-noise ratio due to charge-up caused by ionic charges during transparent electrode formation, and reducing deposition time or rate to avoid charge-up results in insufficient conductivity and thickness of the transparent electrode.

Method used

A method involving the formation of a dielectric layer using electron beam evaporation and a transparent conductive layer using ion plating to neutralize positive charges, reducing charge-up and enhancing conductivity.

Benefits of technology

This method reduces dark current and increases the extraction efficiency of charges, maintaining high conductivity and preventing dielectric breakdown, thereby improving the signal-to-noise ratio.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024148314000001_ABST
    Figure 2024148314000001_ABST
Patent Text Reader

Abstract

To provide a method for manufacturing a photoelectric conversion element that reduces dark current and improves the extraction efficiency of the charge obtained by photoelectric conversion.SOLUTION: A method for manufacturing a photoelectric conversion element in accordance with an aspect of the disclosed technology includes a step for forming a first electrode on a substrate, a step for forming a photoelectric conversion layer on the first electrode, and a step for forming a second electrode on the photoelectric conversion layer, and the step for forming the second electrode includes forming a dielectric layer by electron beam deposition and a step for forming a transparent conductive layer by ion plating.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for manufacturing a photoelectric conversion element and the photoelectric conversion element. [Background technology]

[0002] Known photoelectric conversion elements such as imaging elements used in television cameras, digital cameras, etc. include multi-chip types that use multiple photoelectric conversion elements to obtain color images, and single-chip types that use only one photoelectric conversion element to obtain color images.

[0003] In multi-plate photoelectric conversion elements, a color separation prism separates the incident light into red (R), green (G), and blue (B), and multiple photoelectric conversion elements produce images of each color. This allows efficient use of the incident light, resulting in high-quality images. However, because a color separation prism is used, there is still room for improvement in miniaturizing the photoelectric conversion elements.

[0004] On the other hand, in a single-plate photoelectric conversion element, RGB color filters are arranged in-plane on one photoelectric conversion element to separate each color, which allows the photoelectric conversion element to be made smaller. However, since a color filter is used that absorbs all incident light except for light in a specific wavelength range, the light utilization efficiency is lower than that of a multi-plate photoelectric conversion element, and the quality of the image captured by the photoelectric conversion element may decrease.

[0005] There are advantages and disadvantages to both the multi-panel and single-panel types, and there is a demand for photoelectric conversion elements that can achieve both high image quality and compactness. Under these circumstances, a photoelectric conversion element has been proposed that alternately stacks photoelectric conversion layers that are sensitive to the RGB colors of light and readout circuits that use light-transmitting thin film transistors (TFTs) in order to achieve both high image quality and compactness.

[0006] Specifically, there have been disclosed three layers of organic photoelectric conversion layers and TFTs stacked alternately directly on a single glass substrate (see Patent Document 1), three photoelectric conversion elements each having an organic photoelectric conversion layer and a TFT stacked on a glass substrate (see Patent Document 2), and one in which the bottommost photoelectric conversion layer and readout circuit are replaced with a CMOS (Complementary Metal-Oxide-Semiconductor) sensor (see Patent Document 3).

[0007] Incidentally, in order to extract the electric charge generated by photoelectric conversion to the outside, the photoelectric conversion layer is sandwiched between two electrodes. Transparent electrodes including a transparent conductive film are used as the two electrodes. One method for forming transparent electrodes is the ion plating method, which can form a film with excellent adhesion and durability. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2002-217474 A [Patent Document 2] JP 2005-51115 A [Patent Document 3] JP 2019-102623 A Summary of the Invention [Problem to be solved by the invention]

[0009] When a transparent electrode is formed by ion plating, ion charges reaching the surface of the photoelectric conversion layer from the deposition material may cause charging of the photoelectric conversion element. Charging of the photoelectric conversion element may increase the dark current and reduce the signal-to-noise ratio (S / N) of the photoelectric conversion element. On the other hand, if the film formation time or film formation speed of the transparent electrode is reduced in order to avoid charging of the photoelectric conversion element, a transparent electrode with a specified film thickness may not be obtained and the conductivity may decrease.

[0010] The disclosed technique has an object to provide a method for manufacturing a photoelectric conversion element that reduces dark current and improves the efficiency of extracting charges obtained by photoelectric conversion. [Means for solving the problem]

[0011] A method for manufacturing a photoelectric conversion element according to one embodiment of the disclosed technology includes a step of forming a first electrode on a substrate, a step of forming a photoelectric conversion layer on the first electrode, and a step of forming a second electrode on the photoelectric conversion layer, the step of forming the second electrode including a step of forming a dielectric layer by an electron beam deposition method and a step of forming a transparent conductive layer by an ion plating method. Effect of the Invention

[0012] According to the disclosed technology, it is possible to reduce dark current and increase the efficiency of extracting charges obtained by photoelectric conversion. [Brief description of the drawings]

[0013] [Figure 1] 1 is a cross-sectional view of a photoelectric conversion element according to a first embodiment. [Diagram 2] 5A to 5C are cross-sectional views illustrating a step of forming a lower electrode according to the first embodiment. [Diagram 3] FIG. 2 is a cross-sectional view illustrating a step of forming a photoelectric conversion layer according to the first embodiment. [Figure 4] 5A to 5C are cross-sectional views illustrating a step of forming a dielectric layer according to the first embodiment. [Diagram 5] FIG. 2 is a schematic diagram showing a configuration of an electron beam evaporation apparatus for forming a dielectric layer according to the first embodiment. [Figure 6] FIG. 3 is a cross-sectional view illustrating a step of forming a transparent conductive layer according to the first embodiment. [Figure 7] FIG. 2 is a schematic diagram showing the configuration of an ion plating device for forming a transparent conductive layer according to the first embodiment. [Figure 8] FIG. 4 is a cross-sectional view of a photoelectric conversion element according to a second embodiment. [Figure 9] FIG. 11 is a cross-sectional view illustrating a step of forming a second dielectric layer according to the second embodiment. [Figure 10] FIG. 11 is a cross-sectional view illustrating a step of forming a second transparent conductive layer according to the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] Hereinafter, an embodiment of the present disclosure will be described with reference to the drawings. In each drawing, the same components may be denoted by the same reference numerals. In addition, in the description of each drawing, the description of components that are the same as those of components already described will be omitted as appropriate.

[0015] In each drawing, a rectangular coordinate system having an X-axis, a Y-axis, and a Z-axis is used to express directions. The X-axis, the Y-axis, and the Z-axis are mutually orthogonal. The X-direction along the X-axis indicates the width direction of the photoelectric conversion element according to the embodiment. The Y-direction along the Y-axis indicates the depth direction of the photoelectric conversion element according to the embodiment. The Z-direction along the Z-axis indicates the direction in which the first electrode, the photoelectric conversion layer, and the second electrode included in the photoelectric conversion element according to the embodiment are stacked. The X-direction and the Y-direction may be referred to as "in-plane directions". The Z-direction may be referred to as "direction perpendicular to the surface". However, these do not limit the orientation of the photoelectric conversion element according to the embodiment when used, and the orientation of the photoelectric conversion element according to the embodiment is arbitrary.

[0016] [First embodiment] <Configuration of photoelectric conversion element> A method for manufacturing a photoelectric conversion element according to the first embodiment will be described. First, the configuration of a photoelectric conversion element 1 manufactured by the method for manufacturing a photoelectric conversion element according to the first embodiment will be described with reference to Fig. 1. Fig. 1 is a cross-sectional view of the photoelectric conversion element 1 cut along the XZ plane.

[0017] 1, the photoelectric conversion element 1 includes a substrate 10, a lower electrode 20, a photoelectric conversion layer 30, and an upper electrode 40. The lower electrode 20 corresponds to a "first electrode." The upper electrode 40 corresponds to a "second electrode."

[0018] The substrate 10, the lower electrode 20, the photoelectric conversion layer 30, and the upper electrode 40 are stacked in this order from the lower side in the direction perpendicular to the surface. In the photoelectric conversion element 1, incident light may be incident from the substrate 10 side or from the upper electrode 40 side.

[0019] The substrate 10 is a flat plate-like member that serves as the base of the photoelectric conversion element 1. Examples of the substrate 10 include a glass substrate, a quartz substrate, a sapphire substrate, an alumina substrate, a spinel substrate, a quartz substrate, a silicon substrate, a germanium substrate, a polyethylene substrate, a polyethylene terephthalate substrate, and a polycarbonate substrate. Among these, a glass substrate or a quartz substrate having strength and translucency is preferable as the substrate 10. However, the type of the substrate 10 is not limited to these.

[0020] The lower electrode 20 is disposed on the substrate 10. When the photoelectric conversion element 1 is applied to an imaging element, the lower electrode 20 corresponds to an electrode called a counter electrode. The lower electrode 20 is connected to an external power source and applies a voltage to the photoelectric conversion layer 30.

[0021] The lower electrode 20 is preferably a transparent electrode including a transparent conductive film. Examples of the transparent conductive film include thin films of indium oxide, tin oxide, and zinc oxide. Examples of the indium oxide transparent conductive film include an ITO (tin-doped indium oxide) film containing tin as a dopant. Examples of the tin oxide transparent conductive film include an ATO (antimony-doped tin oxide) film containing antimony as a dopant and an FTO (fluorine-doped tin oxide) film containing fluorine as a dopant. Examples of the zinc oxide transparent conductive film include an AZO (aluminum-doped zinc oxide) film containing aluminum as a dopant and a GZO (gallium-doped zinc oxide) film containing gallium as a dopant. Among these, an ITO film or an FTO film having excellent conductivity and translucency are preferable. The lower electrode 20 may be a mixture or a laminate of two or more of these. However, the lower electrode 20 is not limited to these.

[0022] The thickness of the lower electrode 20 is preferably 5 nm or more from the viewpoint of ensuring electrical conductivity, etc. Also, the thickness of the lower electrode 20 is preferably 150 nm or less from the viewpoint of preventing a decrease in yield and ensuring light transmittance, etc. However, the thickness of the lower electrode 20 is not limited to these values.

[0023] The photoelectric conversion layer 30 is disposed on the lower electrode 20. The photoelectric conversion layer 30 absorbs light of a specific wavelength and converts it into electric charges depending on the material constituting the photoelectric conversion layer 30. The photoelectric conversion layer 30 may be a layer containing an organic material having excellent wavelength selectivity for selectively absorbing light of a specific wavelength and excellent photoelectric conversion characteristics.

[0024] Examples of organic materials include compounds such as triarylamine compounds, benzidine compounds, pyrazoline compounds, styrylamine compounds, hydrazone compounds, triphenylmethane compounds, carbazole compounds, polysilane compounds, thiophene compounds, phthalocyanine compounds, naphthalocyanine compounds, cyanine compounds, merocyanine compounds, oxonol compounds, polyamine compounds, indole compounds, pyrrole compounds, pyrazole compounds, and polyarylene compounds, as well as analogs of these compounds; derivatives such as carbazole derivatives, naphthalene derivatives, anthracene derivatives, chrysene derivatives, phenanthrene derivatives, pentacene derivatives, phenylbutadiene derivatives, styryl derivatives, quinoline derivatives, tetracene derivatives, pyrene derivatives, perylene derivatives, fluoranthene derivatives, quinacridone derivatives, coumarin derivatives, porphyrin derivatives, boron dipyrromethene derivatives, fullerene derivatives, phthalocyanine derivatives, and naphthalocyanine derivatives; and metal complexes (In complexes, Ir complexes, Pt complexes, Eu complexes, and the like).

[0025] From the viewpoint of increasing photoelectric conversion efficiency while preventing a short circuit between the lower electrode 20 and the upper electrode 40, the thickness of the photoelectric conversion layer 30 is preferably 10 nm or more. On the other hand, from the viewpoint of preventing a decrease in yield and an increase in cost, the thickness of the photoelectric conversion layer 30 is preferably 1 μm or less. However, the thickness of the photoelectric conversion layer 30 is not limited to this.

[0026] The photoelectric conversion layer 30 may be a mixture or a laminate of two or more of the above-mentioned materials. The photoelectric conversion layer 30 is not limited to an organic material and may contain an inorganic material. Examples of the inorganic material include various semiconductor materials and dielectric materials.

[0027] The upper electrode 40 is disposed on the photoelectric conversion layer 30. When the photoelectric conversion element 1 is applied to an imaging element, the upper electrode 40 is called a pixel electrode. The upper electrode 40 is connected to a readout circuit and outputs an electric signal based on the charge converted in the photoelectric conversion layer 30 to the readout circuit.

[0028] As shown in Fig. 1, the upper electrode 40 includes a dielectric layer 50 and a transparent conductive layer 60. The dielectric layer 50 and the transparent conductive layer 60 are stacked in a direction perpendicular to the surface. In the example shown in Fig. 1, the dielectric layer 50 is disposed on the photoelectric conversion layer 30, and the transparent conductive layer 60 is disposed on the dielectric layer 50. However, the positional relationship between the dielectric layer 50 and the transparent conductive layer 60 is not limited thereto, and the transparent conductive layer 60 may be disposed on the photoelectric conversion layer 30, and the dielectric layer 50 may be disposed on the transparent conductive layer 60.

[0029] The configuration of the upper electrode 40 is not limited to one having one each of the dielectric layer 50 and the transparent conductive layer 60, and may include a plurality of dielectric layers 50. The upper electrode 40 may also include a plurality of transparent conductive layers 60. Note that the configuration in which the upper electrode 40 includes a plurality of dielectric layers 50 and a plurality of transparent conductive layers 60 will be described in detail separately in the second embodiment.

[0030] The dielectric layer 50 transmits at least visible light. The dielectric layer 50 may be made of silicon monoxide (SiO), silicon dioxide (SiO 2 ), titanium dioxide (TiO 2 ), niobium pentoxide (Nb 2 O 5 ), Tantalum Pentoxide (Ta 2 O 5 ), molybdenum trioxide (MoO 3 ), germanium dioxide (GeO 2), aluminum oxide (Al 2 O 3 However, the type of the dielectric layer 50 is not limited to these.

[0031] The dielectric layer 50 is provided mainly to electrically neutralize the positive charge of the transparent conductive layer 60 and prevent charging up of the photoelectric conversion element 1. From the viewpoint of preventing charging up of the photoelectric conversion element 1, the thickness of the dielectric layer 50 is preferably 5 nm or more. On the other hand, from the viewpoint of preventing a decrease in translucency and an increase in cost, the thickness of the dielectric layer 50 is preferably 100 nm or less. In other words, the thickness of the dielectric layer 50 may be 5 nm or more and 100 nm or less. However, the thickness of the dielectric layer 50 is not limited to these values ​​and can be adjusted as appropriate.

[0032] The transparent conductive layer 60 is a layer having electrical conductivity and light transmissivity. Examples of the transparent conductive layer 60 include a layer including an indium oxide-based transparent conductive film, a tin oxide-based transparent conductive film, or a zinc oxide-based transparent conductive film. An example of the indium oxide-based transparent conductive film is an ITO film. Examples of the tin oxide-based transparent conductive film include an ATO film and an FTO film. Examples of the zinc oxide-based transparent conductive film include an AZO film and a GZO film. Among these, an ITO film or an FTO film, which has excellent electrical conductivity and light transmissivity, is preferable as the transparent conductive layer 60.

[0033] From the viewpoint of ensuring electrical conductivity, the thickness of the transparent conductive layer 60 is preferably 1 nm or more. On the other hand, from the viewpoint of preventing a decrease in yield and a decrease in light transmittance, the thickness of the transparent conductive layer 60 is preferably 50 nm or less. In other words, the thickness of the transparent conductive layer may be 1 nm or more and 50 nm or less. However, the film thickness of the transparent conductive layer 60 is not limited to these values.

[0034] The photoelectric conversion element 1 may appropriately include other components such as a charge transport layer, a charge blocking layer, etc. The charge transport layer and the charge blocking layer are disposed between the lower electrode 20 and the photoelectric conversion layer 30, and between the photoelectric conversion layer 30 and the upper electrode 40, respectively.

[0035] <Manufacturing method> Next, a method for manufacturing the photoelectric conversion element 1 according to the first embodiment will be described. The method for manufacturing the photoelectric conversion element 1 according to the first embodiment includes a step of forming a lower electrode 20 on the substrate 10, a step of forming a photoelectric conversion layer 30 on the lower electrode 20, and a step of forming an upper electrode 40 on the photoelectric conversion layer 30.

[0036] The process of forming the lower electrode 20 will be described below. FIG.

[0037] 2, a lower electrode 20 is formed on a substrate 10. Methods for forming the lower electrode 20 include dry processes such as vacuum deposition, ion plating, and sputtering, and wet processes such as inkjet, spin coating, and dipping. However, the method for forming the lower electrode 20 is not limited to these as long as it is possible to form a conductive layer.

[0038] Next, a description will be given of a process for forming the photoelectric conversion layer 30. FIG.

[0039] 3, the photoelectric conversion layer 30 is formed on the lower electrode 20. Methods for forming the photoelectric conversion layer 30 include dry processes such as vacuum deposition, ion plating, and sputtering, and wet processes such as inkjet, spin coating, and dipping. However, the method for forming the photoelectric conversion layer 30 is not limited to these as long as it is possible to form a layer having photoelectric conversion properties.

[0040] Next, a description will be given of the process of forming the upper electrode 40. The process of forming the upper electrode 40 includes a process of forming a dielectric layer 50 and a process of forming a transparent conductive layer 60.

[0041] The process of forming the dielectric layer 50 will be described with reference to Fig. 4 and Fig. 5. Fig. 4 is a cross-sectional view of a laminate 51 including a substrate 10, a lower electrode 20, a photoelectric conversion layer 30, and a dielectric layer 50. Fig. 5 is a schematic diagram showing the configuration of an electron beam evaporation apparatus 200 for forming the dielectric layer 50.

[0042] As shown in Fig. 4, a dielectric layer 50 is formed on the photoelectric conversion layer 30. Specifically, the dielectric layer 50 is formed by using an electron beam evaporation method. An electron beam evaporation apparatus 200 shown in Fig. 5 is used when forming the dielectric layer 50 by the electron beam evaporation method.

[0043] The configuration of the electron beam evaporation apparatus 200 will be described. The electron beam evaporation apparatus 200 includes a vacuum container 210, a crucible 220 filled with the evaporation material 50D, an electron gun 230 that emits an electron beam 231 for heating the evaporation material 50D, a holder 240 that holds the laminate 31 that is the object to be deposited, and a vacuum pump 250. The laminate 31 is held by the holder 240, so that the evaporation material 50D and the photoelectric conversion layer 30 face each other.

[0044] The deposition material 50D is also called a target, a pellet, or a tablet, and is a deposition source for the dielectric layer 50. Examples of the deposition material 50D include sintered bodies and crystals of metals, alloys, metal compounds, and the like. When a SiO film is deposited as the dielectric layer 50, a sintered body of SiO can be used as the deposition material 50D.

[0045] A process of depositing the dielectric layer 50 on the photoelectric conversion layer 30 using the electron beam deposition apparatus 200 will be described. First, the vacuum pump 250 of the electron beam deposition apparatus 200 is driven to evacuate the gas inside the vacuum vessel 210. Next, after the inside of the vacuum vessel 210 is in a vacuum state, an emission current and an acceleration voltage are applied to the electron gun 230, whereby an electron beam 231 is emitted from the electron gun 230.

[0046] The electron beam 231 emitted from the electron gun 230 irradiates the deposition material 50D and heats the surface of the deposition material 50D. A part of the deposition material 50D heated by the electron beam 231 is emitted as evaporated particles 50P and travels toward the photoelectric conversion layer 30 of the stack 31 facing the deposition material 50D. The evaporated particles 50P reach the photoelectric conversion layer 30. In this manner, the dielectric layer 50 is evaporated onto the photoelectric conversion layer 30.

[0047] On the other hand, electrons 230e, which are a part of the electron beam 231 irradiated to the deposition material 50D, are reflected by the deposition material 50D and proceed toward the photoelectric conversion layer 30 facing the deposition material 50D. That is, the electrons 230e reflected by the deposition material 50D reach the photoelectric conversion layer 30 together with the evaporated particles 50P. The electrons 230e reach the photoelectric conversion layer 30 together with the evaporated particles 50P, and are thereby accumulated in the dielectric layer 50 evaporated on the photoelectric conversion layer 30. The dielectric layer 50 includes a dielectric portion formed by the evaporated particles 50P and neutralizing electrons 230e. The neutralizing electrons 230e are electrons that electrically neutralize the positive charge of the transparent conductive layer 60 formed on the dielectric layer 50.

[0048] The amount of neutralizing electrons 230e contained in the dielectric layer 50 can be appropriately adjusted according to the emission current of the electron gun 230 and the emission time of the electron beam 231. By increasing the emission current of the electron gun 230 or increasing the emission time of the electron beam 231, the amount of neutralizing electrons 230e contained in the dielectric layer 50 can be increased.

[0049] Next, the process of forming the transparent conductive layer 60 will be described with reference to Fig. 6 and Fig. 7. Fig. 6 is a cross-sectional view of a laminate 61 including a substrate 10, a lower electrode 20, a photoelectric conversion layer 30, a dielectric layer 50, and a transparent conductive layer 60. The laminate 61 corresponds to a photoelectric conversion element 1. Fig. 7 is a schematic diagram showing the configuration of an ion plating apparatus 300 for forming the transparent conductive layer 60.

[0050] As shown in Fig. 6, a transparent conductive layer 60 is formed on a dielectric layer 50. Specifically, the transparent conductive layer 60 is formed by using an ion plating method. An ion plating device 300 shown in Fig. 7 is used when forming the transparent conductive layer 60 by the ion plating method.

[0051] The configuration of the ion plating device 300 will be described. The ion plating device 300 includes a vacuum container 310, a crucible 320 filled with a deposition material 60D, a plasma generating unit 330 that generates plasma 331 for ionizing the deposition material 60D, a holder 340 that holds a laminate 51 that is an object to be deposited, and a vacuum pump 350. The holder 340 holds the laminate 51, so that the deposition material 60D and the dielectric layer 50 face each other.

[0052] The deposition material 60D is a deposition source for the transparent conductive layer 60. The deposition material 60D is also called a target, a pellet, or a tablet. Examples of the deposition material 60D include sintered bodies and crystals of metals, alloys, metal compounds, and the like. When an ITO film is deposited as the transparent conductive layer 60, the deposition material 60D is In. 2 O 3 and SnO 2 A sintered body containing the above can be used.

[0053] The configuration of the ion plating device 300 is not limited to that shown in Fig. 7. The ion plating device 300 may include a resistance heating type heater for heating the deposition material 60D, a coil for generating plasma between the crucible 320 and the holder 340, and other components.

[0054] The process of depositing the transparent conductive layer 60 on the dielectric layer 50 using the ion plating device 300 will be described. First, the vacuum pump 350 of the ion plating device 300 is driven to evacuate the gas inside the vacuum container 310. Next, after the inside of the vacuum container 310 is in a vacuum state, the plasma generating unit 330 generates plasma 331 for ionizing the deposition material 60D.

[0055] When the deposition material 60D passes through the plasma 331 generated by the plasma generating unit 330, a part of the deposition material 60D becomes cationized evaporated particles 60P and moves toward the dielectric layer 50 of the laminate 51 facing the deposition material 60D. The evaporated particles 60P reach the dielectric layer 50 while reacting with the oxygen gas supplied into the vacuum vessel 310. As a result, the transparent conductive layer 60 is evaporated onto the dielectric layer 50. Here, since some of the evaporated particles 60P reach the dielectric layer 50 in the state of cations, the transparent conductive layer 60 has a positive charge based on the cations of the evaporated particles 60P. If the positive charge of the transparent conductive layer 60 is not electrically neutralized, the photoelectric conversion element 1 is charged up. The charge-up increases the dark current of the photoelectric conversion element 1, and the S / N ratio related to the detection of incident light having a specific wavelength decreases. The charge-up also induces an overcurrent, which may cause dielectric breakdown of the photoelectric conversion element 1. However, in this embodiment, the positive charges of the transparent conductive layer 60 are electrically neutralized by neutralizing electrons 230e in the dielectric layer 50 overlapping with the transparent conductive layer 60. As a result, in this embodiment, charge-up caused by the positive charges of the transparent conductive layer 60 can be reduced.

[0056] The upper electrode 40 is formed by forming the dielectric layer 50 and the transparent conductive layer 60 in this order. The order in which the dielectric layer 50 and the transparent conductive layer 60 are formed is not limited. That is, the transparent conductive layer 60 may be formed on the photoelectric conversion layer 30, and then the dielectric layer 50 may be formed on the transparent conductive layer 60. Even when the dielectric layer 50 is formed on the transparent conductive layer 60, the neutralizing electrons 230e of the dielectric layer 50 can electrically neutralize the positive charge of the transparent conductive layer 60.

[0057] Through the above steps, the photoelectric conversion element 1 is manufactured.

[0058] <Action and effect> As described above, the method for manufacturing the photoelectric conversion element 1 according to this embodiment includes a step of forming the lower electrode 20 (first electrode) on the substrate 10, a step of forming the photoelectric conversion layer 30 on the lower electrode 20, and a step of forming the upper electrode 40 (second electrode) on the photoelectric conversion layer 30. The step of forming the upper electrode 40 includes a step of forming the dielectric layer 50 by electron beam deposition and a step of forming the transparent conductive layer 60 by ion plating. By forming the dielectric layer 50 by electron beam deposition, the neutralizing electrons 230e can be contained in the dielectric layer 50. By overlapping the dielectric layer 50 containing the neutralizing electrons 230e and the transparent conductive layer 60 having a positive charge, the neutralizing electrons 230e electrically neutralize the positive charge of the transparent conductive layer 60. This reduces the charge-up caused by the positive charge of the transparent conductive layer 60, and reduces the dark current of the photoelectric conversion element 1. That is, the S / N ratio for detecting incident light having a specific wavelength can be increased. Furthermore, the charge-up caused by the positive charge of the transparent conductive layer 60 is reduced, thereby preventing dielectric breakdown of the photoelectric conversion element 1. Furthermore, the transparent conductive film can be continuously grown in a state in which the charge-up is reduced, and as a result, a thick transparent conductive layer 60 can be formed without damaging the photoelectric conversion element 1. In other words, the extraction efficiency of the charge obtained in the photoelectric conversion layer 30 can be improved. Furthermore, in addition to obtaining a transparent conductive layer 60 with excellent conductivity, a photoelectric conversion element 1 with excellent photoelectric conversion characteristics can be obtained.

[0059] [Second embodiment] <Configuration of photoelectric conversion element> A method for manufacturing a photoelectric conversion element according to the second embodiment will be described. First, the configuration of a photoelectric conversion element 1A manufactured by the method for manufacturing a photoelectric conversion element according to the second embodiment will be described with reference to Fig. 8. Fig. 8 is a cross-sectional view of the photoelectric conversion element 1A. Note that the same components as those in the first embodiment are given the same reference numerals, and duplicated descriptions will be omitted as appropriate.

[0060] The photoelectric conversion element 1A according to this embodiment differs from the photoelectric conversion element 1 according to the first embodiment in that the upper electrode includes a plurality of dielectric layers and a plurality of transparent conductive layers. Specifically, as shown in Fig. 8, the upper electrode 40A of the photoelectric conversion element 1A differs from the photoelectric conversion element 1 in that the upper electrode 40A includes a first dielectric layer 50A1 and a second dielectric layer 50A2 as the dielectric layers and a first transparent conductive layer 60A1 and a second transparent conductive layer 60A2 as the transparent conductive layers.

[0061] The number of dielectric layers is not limited to 2 and may be 3 or more. The number of transparent conductive layers is not limited to 2 and may be 3 or more. However, as the number of dielectric layers and transparent conductive layers increases, the number of interfaces between adjacent layers increases, which may reduce the light transmittance of the upper electrode 40A.

[0062] When the thickness of each dielectric layer is 5 nm to 100 nm and the thickness of each transparent conductive layer is 1 nm to 50 nm, the number of pairs of dielectric layers and transparent conductive layers is preferably 2 to 8. The number of pairs of dielectric layers and transparent conductive layers is more preferably 3 to 6. The number of pairs of dielectric layers and transparent conductive layers is more preferably 3 to 5.

[0063] The number of dielectric layers and the number of transparent conductive layers may be the same or different. From the viewpoint of suitably preventing charge-up, it is preferable that the number of dielectric layers and the number of transparent conductive layers are the same.

[0064] In the upper electrode 40A, the dielectric layers and the transparent conductive layers are alternately laminated. Specifically, a first dielectric layer 50A1 is disposed on the photoelectric conversion layer 30, and then a first transparent conductive layer 60A1, a second dielectric layer 50A2, and a second transparent conductive layer 60A2 are laminated in this order.

[0065] Alternatively, the first transparent conductive layer 60A1 may be disposed on the photoelectric conversion layer 30, and the first dielectric layer 50A1, the second transparent conductive layer 60A2, and the second dielectric layer 50A2 may be disposed in this order on the first transparent conductive layer 60A1.

[0066] The first dielectric layer 50A1 and the second dielectric layer 50A2 may be made of the same or different materials. When there are three or more dielectric layers, the materials of the dielectric layers may be the same or different. However, from the viewpoint of preventing a decrease in yield and simplifying the deposition process, it is preferable that the materials of the dielectric layers are the same.

[0067] The first transparent conductive layer 60A1 and the second transparent conductive layer 60A2 may be made of the same or different materials. When there are three or more transparent conductive layers, the materials of the respective transparent conductive layers may be the same or different. However, from the viewpoint of preventing a decrease in yield and simplifying the deposition process, it is preferable that the materials of the respective transparent conductive layers are the same.

[0068] <Manufacturing method> Next, a method for manufacturing the photoelectric conversion element 1A according to the second embodiment will be described. The method for manufacturing the photoelectric conversion element 1A according to the second embodiment includes the steps of forming a lower electrode 20 on the substrate 10, forming a photoelectric conversion layer 30 on the lower electrode 20, and forming an upper electrode 40A.

[0069] In the second embodiment, the process of forming the lower electrode 20 on the substrate 10 and the process of forming the photoelectric conversion layer 30 on the lower electrode 20 are similar to those in the first embodiment, and therefore the description thereof will be omitted. In addition, among the processes of forming the upper electrode 40A, the process of forming the first dielectric layer 50A1 and the process of forming the first transparent conductive layer 60A1 are similar to the processes of forming the dielectric layer 50 and the transparent conductive layer 60 in the first embodiment, and therefore the duplicated description thereof will be omitted.

[0070] The step of forming the second dielectric layer 50A2 will be described with reference to Fig. 9. Fig. 9 is a cross-sectional view of a laminate 71 including a substrate 10, a lower electrode 20, a photoelectric conversion layer 30, a first dielectric layer 50A1, a first transparent conductive layer 60A1, and a second dielectric layer 50A2.

[0071] As shown in Fig. 9, a second dielectric layer 50A2 is formed on the first transparent conductive layer 60A1. Specifically, the second dielectric layer 50A2 is formed by electron beam evaporation. The second dielectric layer 50A2 can be formed by using the electron beam evaporation apparatus 200 shown in Fig. 5. The second dielectric layer 50A2 also includes neutralizing electrons 230e, similar to the first dielectric layer 50A1.

[0072] The process of forming the second transparent conductive layer 60A2 will be described with reference to Fig. 10. Fig. 10 is a cross-sectional view of a laminate 81 including a substrate 10, a lower electrode 20, a photoelectric conversion layer 30, a first dielectric layer 50A1, a first transparent conductive layer 60A1, a second dielectric layer 50A2, and a second transparent conductive layer 60A2. The laminate 81 corresponds to the photoelectric conversion element 1A.

[0073] As shown in Fig. 10, a second transparent conductive layer 60A2 is formed on the second dielectric layer 50A2. Specifically, the second transparent conductive layer 60A2 is formed by using an ion plating method. The second transparent conductive layer 60A2 can be formed by using an ion plating apparatus 300 shown in Fig. 7.

[0074] Like the first transparent conductive layer 60A1, the second transparent conductive layer 60A2 also has a positive charge resulting from the positive ions of the evaporated particles 60P. However, by overlapping the second transparent conductive layer 60A2 with the second dielectric layer 50A2, the positive charge of the second transparent conductive layer 60A2 is electrically neutralized by the neutralizing electrons 230e in the second dielectric layer 50A2.

[0075] The upper electrode 40A is formed by sequentially forming the first dielectric layer 50A1, the first transparent conductive layer 60A1, the second dielectric layer 50A2, and the second transparent conductive layer 60A2. However, the order of forming the first dielectric layer 50A1, the first transparent conductive layer 60A1, the second dielectric layer 50A2, and the second transparent conductive layer 60A2 is not limited. That is, the first transparent conductive layer 60A1, the first dielectric layer 50A1, the second transparent conductive layer 60A2, and the second dielectric layer 50A2 may be sequentially formed on the photoelectric conversion layer 30.

[0076] Since the transparent conductive layers and the dielectric layers are alternately overlapped, the positive charges in the transparent conductive layers are electrically neutralized by the neutralizing electrons 230e in the dielectric layers, thereby suppressing charge-up in the photoelectric conversion element 1A.

[0077] Through the above steps, the photoelectric conversion element 1A is manufactured.

[0078] <Action and effect> As described above, in the manufacturing method of the photoelectric conversion element 1A according to the present embodiment, in the step of forming the upper electrode 40A (second electrode), the step of forming the dielectric layer and the step of forming the transparent conductive layer are each performed multiple times, and the step of forming the dielectric layer and the step of forming the transparent conductive layer are alternately performed. As a result, each of the multiple dielectric layers and each of the multiple transparent conductive layers are alternately overlapped, and the neutralizing electrons 230e in each dielectric layer can electrically neutralize the positive charges of the adjacent transparent conductive layers. As a result, the charge-up of the photoelectric conversion element 1A can be suppressed, and the dark current can be reduced. In addition, the thickness of the transparent conductive layer can be increased by stacking the multiple transparent conductive layers with the dielectric layer between them. This can increase the conductivity of the upper electrode 40A. That is, the extraction efficiency of the charge obtained in the photoelectric conversion layer 30 can be increased. Furthermore, the manufacturing method of the photoelectric conversion element 1A according to the second embodiment has almost the same effects as the manufacturing method of the photoelectric conversion element 1 according to the first embodiment.

[0079] [Example of application] The photoelectric conversion elements 1, 1A according to the embodiment can be applied to an imaging element that converts incident light from a subject into an electrical signal. The imaging element further includes a readout circuit that reads out the electrical signal obtained by the photoelectric conversion elements 1, 1A. The imaging element including the photoelectric conversion elements 1, 1A is preferably a multi-plate type, but may also be a single-plate type. The multi-plate type imaging element includes a plurality of photoelectric conversion elements 1, 1A. The plurality of photoelectric conversion elements 1, 1A are each connected to the readout circuit.

[0080] [Example] Specific examples of the above-described photoelectric conversion elements 1 and 1A will be described below, however, the present disclosure is not limited or restricted by the following examples.

[0081] <Example 1> As Example 1, a photoelectric conversion element was produced in which a lower electrode 20, a charge blocking layer, a photoelectric conversion layer 30, and an upper electrode 40A were stacked in this order on a substrate 10. The upper electrode 40A is a laminate in which a first dielectric layer 50A1, a first transparent conductive layer 60A1, a second dielectric layer 50A2, and a second transparent conductive layer 60A2 are stacked in this order.

[0082] The first dielectric layer 50A1 and the second dielectric layer 50A2 were each formed by electron beam deposition, and the first transparent conductive layer 60A1 and the second transparent conductive layer 60A2 were each formed by ion plating.

[0083] The configuration of each part of the photoelectric conversion element according to the first embodiment is as follows.

[0084] Substrate 10: Glass substrate Bottom electrode 20: ITO Charge blocking layer: B4PYMPM (thickness: 50nm) Photoelectric conversion layer 30: a laminate of tris(2-phenylpyrazole)iridium complex (thickness: 70 nm) and boron subphthalocyanine chloride (thickness: 200 nm) First dielectric layer 50A1: SiO (thickness: 30 nm) First transparent conductive layer 60A1: ITO (thickness: 10 nm) Second dielectric layer 50A2: SiO (thickness: 30 nm) · Second transparent conductive layer 60A2: ITO (thickness: 10 nm)

[0085] <Comparative Example 1> As Comparative Example 1, a photoelectric conversion element was produced in which a lower electrode 20, a charge blocking layer, a photoelectric conversion layer 30, and a transparent conductive layer as an upper electrode were laminated in this order on a substrate 10. The transparent conductive layer was formed by using an ion plating method.

[0086] The configuration of each part of the photoelectric conversion element according to Comparative Example 1 is as follows.

[0087] Substrate 10: Glass substrate Bottom electrode 20: ITO Charge blocking layer: B4PYMPM (thickness: 50nm) Photoelectric conversion layer 30: a laminate of tris(2-phenylpyrazole)iridium complex (thickness: 70 nm) and boron subphthalocyanine chloride (thickness: 200 nm) ·Transparent conductive layer: ITO (thickness: 20 nm)

[0088] <Differences between Example 1 and Comparative Example 1> The upper electrode 40A of Example 1 is composed of a first dielectric layer 50A1, a first transparent conductive layer 60A1, a second dielectric layer 50A2, and a second transparent conductive layer 60A2. In contrast, the upper electrode of Comparative Example 1 is composed of a single transparent conductive layer. The sum of the thickness of the first transparent conductive layer 60A1 and the thickness of the second transparent conductive layer 60A2 of Example 1 is the same as the thickness of the transparent conductive layer of Comparative Example 1.

[0089] <Evaluation of dark current and photocurrent> The measurement results of the dark current and the photocurrent in Example 1 and Comparative Example 1 are shown in Table 1. When measuring the dark current and the photocurrent, a voltage of 10 V was applied to each of Example 1 and Comparative Example 1. In addition, when measuring the photocurrent, a light having a wavelength of 550 nm and a power density of 50 μW / cm was applied from the substrate 10 side of each of Example 1 and Comparative Example 1. 2 The specimen was irradiated with monochromatic light of 1000 nm.

[0090] [Table 1]

[0091] As shown in Table 1, the photocurrent of Example 1 was approximately the same as that of Comparative Example 1. In contrast, the dark current of Example 1 was approximately one order of magnitude lower than the dark current of Comparative Example 1. It was found that by providing a pair of a dielectric layer and a transparent conductive layer in the upper electrode 40A, charge-up of the photoelectric conversion element was suppressed and the dark current was reduced.

[0092] Example 1 has two dielectric layers and two transparent conductive layers. Based on the measurement results, however, it is considered that the dark current will also be reduced in devices having one dielectric layer and one transparent conductive layer, or devices having three or more dielectric layers and three or more transparent conductive layers.

[0093] Although the embodiments have been described above, the present disclosure is not limited to the above-described embodiments, and various modifications and improvements are possible within the scope of the present disclosure. [Explanation of symbols]

[0094] 1,1A Photoelectric conversion element 10 Substrate 20 Lower electrode 30 Photoelectric conversion layer 40,40A Upper electrode 50 Dielectric Layer 50A1 First dielectric layer 50A2 Second dielectric layer 60 Transparent conductive layer 60A1 First transparent conductive layer 60A2 Second transparent conductive layer 200 Electron beam deposition equipment 230e neutralization electron 300 Ion plating equipment

Claims

1. forming a first electrode on a substrate; forming a photoelectric conversion layer on the first electrode; forming a second electrode on the photoelectric conversion layer; Including, The step of forming the second electrode includes: forming a dielectric layer by electron beam evaporation; forming a transparent conductive layer by an ion plating method; Including, A method for manufacturing a photoelectric conversion element.

2. In the step of forming the second electrode, the step of forming the dielectric layer and the step of forming the transparent conductive layer are each performed multiple times, and the step of forming the dielectric layer and the step of forming the transparent conductive layer are alternately performed. A method for producing the photoelectric conversion element according to claim 1 .

3. The thickness of the dielectric layer is 5 nm or more and 100 nm or less. A method for producing the photoelectric conversion element according to claim 1 or 2.

4. The transparent conductive layer has a thickness of 1 nm or more and 50 nm or less. A method for producing the photoelectric conversion element according to claim 1 or 2.

5. A substrate; A first electrode disposed on the substrate; A photoelectric conversion layer disposed on the first electrode; A second electrode disposed on the photoelectric conversion layer; Equipped with The second electrode comprises a dielectric layer and a transparent conductive layer stacked together. Photoelectric conversion element.

6. the second electrode comprises a plurality of the dielectric layers and a plurality of the transparent conductive layers; The dielectric layers and the transparent conductive layers are alternately laminated. The photoelectric conversion element according to claim 5 .

7. the dielectric layer contains neutralizing electrons that electrically neutralize positive charges of the transparent conductive layer; The photoelectric conversion element according to claim 5 or 6.

Citation Information

Patent Citations

  • Photoelectric conversion film and solid-state image sensor equipped with the same

    JP2002217474A

  • Thin film transistor, manufacturing method thereof, optical functioning element, and manufacturing method of optical functioning element

    JP2005051115A

  • Color imaging device and manufacturing method thereof

    JP2019102623A