Method and apparatus for producing compact as well as compact
The method and apparatus for producing fiber-reinforced resin materials with holes address the issue of fiber breakage and region control, enabling high-strength molded bodies with defined fiber-free areas through strategic mold deformation and resin application.
Patent Information
- Application Number
- JP2023067336
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-17
- Publication Date
- 2024-10-29
AI Technical Summary
Existing methods for producing fiber-reinforced resin materials with holes result in broken reinforcing fibers and difficulty in controlling regions without fibers, leading to potential breakage of the molded article.
A method and apparatus that involves winding reinforcing fibers around a core portion crossing the stretching direction, using molds with protrusions positioned to avoid contact before deformation, and applying resin between opposing molds to form holes without breaking fibers, allowing regions with and without reinforcing fibers to be easily defined.
Enables the production of high-strength molded bodies with holes by preventing fiber breakage and facilitating regions with and without reinforcing fibers, enhancing manufacturing efficiency and recyclability.
Smart Images

Figure 2024153438000001_ABST
Abstract
Description
[Technical field]
[0001] The technology disclosed herein belongs to the technical field of a method and apparatus for producing a molded body, and a method and apparatus for producing a molded body. [Background technology]
[0002] Molded bodies containing fiber-reinforced resin materials are used in various fields as lightweight and high-strength products. In general, fiber-reinforced resin materials are produced by impregnating a bundle of reinforcing fibers into a resin. Molded bodies are produced by press molding such fiber-reinforced resin materials, but some molded bodies require the formation of holes.
[0003] A method for manufacturing a molded body containing a fiber-reinforced resin material and having holes is disclosed, for example, in Patent Document 1. Patent Document 1 discloses a method for manufacturing FRP leaf springs, in which a cylindrical mold is provided with protrusions, and when a bundle of reinforcing fibers impregnated with resin is wound around the mold, the bundle is wound while avoiding the protrusions, thereby forming holes through the protrusions. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 60-132140 Summary of the Invention [Problem to be solved by the invention]
[0005] If holes are drilled after press molding, the reinforcing fibers will break at the hole formation area. In the method of Patent Document 1, it is possible to prevent the reinforcing fibers from breaking, but fine adjustments are required to wind the fiber-reinforced resin material while avoiding the protrusions. In addition, by providing an area around the hole that contains reinforcing fibers and an area that does not contain reinforcing fibers, the molded body can be made to be easily broken when removed while still having the strength required for a part. However, in the method of Patent Document 1, it is difficult to control the area around the protrusion to not contain reinforcing fibers.
[0006] The technology disclosed herein has been made in consideration of these points, and its purpose is to provide a manufacturing method and manufacturing apparatus that can easily manufacture a high-strength molded body containing a fiber-reinforced resin material and having holes, and that can also easily manufacture a high-performance molded body that does not contain reinforcing fibers in a specified region around the hole. [Means for solving the problem]
[0007] In order to solve the above-mentioned problems, the technology disclosed herein is a manufacturing method for a molded body containing reinforcing fibers and a resin material, the method comprising: a winding step of winding a fiber-reinforced resin material, in which a bundle of reinforcing fibers is impregnated with a resin material, around a core portion extending in a direction intersecting the extension direction of the reinforcing fibers to form a wound body; and a molding step of forming a molded body by deforming the wound body by providing a fixed mold and a movable mold having opposing surfaces facing each other, and disposing the wound body between the fixed mold and the movable mold and then bringing the movable mold closer to the fixed mold to butt the opposing surfaces together, wherein at least one of the fixed mold and the movable mold has a protrusion for forming a hole in the molded body, and the protrusion extends from one opposing surface to the other opposing surface at a position that is not in contact with the wound body before deformation and is in contact with the wound body after deformation.
[0008] According to the above configuration, the protrusion extends to a position that is not in contact with the wound body before deformation and to a position that is in contact with the wound body after deformation, so that the hole is formed by being surrounded on the outer periphery by the fiber reinforced resin material that flows due to the deformation of the wound body. Therefore, it is possible to prevent the reinforcing fibers in the fiber reinforced resin material from breaking, and to easily manufacture a high-strength molded body having a hole. In addition, by being provided at such a position, the protrusion restricts the movement of the reinforcing fibers that flow due to the deformation of the wound body, so that it is possible to easily provide an area that includes reinforcing fibers and an area that does not include reinforcing fibers around the hole of the molded body.
[0009] In one embodiment, the configuration may include a resin adding process of adding resin material between the opposing surfaces before the movable mold and the fixed mold reach a molding bottom dead center position in the molding process or after they reach a molding bottom dead center position.
[0010] According to the above-mentioned configuration, by adding the resin material, the molded body can be molded more reliably than if it were molded only with the resin that seeps out from the wound body when the wound body is deformed.
[0011] In one embodiment, the method may further include a core portion removal step in which the core portion is pulled out from the wound body before the movable die and the fixed die reach a bottom dead center position in the molding step.
[0012] According to the above configuration, the core portion is pulled out while the movable mold is moving toward the fixed mold, so that multiple processes are carried out consecutively or partially in parallel, thereby improving manufacturing efficiency.
[0013] In one embodiment, the fixed mold and the movable mold have a concave portion on one side and a convex portion on the other side, and the concave portion and the convex portion each have a top plate forming portion and a side wall forming portion extending from both ends of the top plate forming portion, so that the wound body can be molded into a hat-shaped cross section, and after the wound body is placed on the convex portion, the opposing surfaces are butted together to cause the wound body to flow outward from the convex portion, and the protrusion may be provided outer than the convex portion.
[0014] According to the above-mentioned configuration, a molded body having a high strength and a hat-shaped cross section can be easily manufactured. In addition, by providing the protrusion on the outside of the convex portion, which is the direction in which the reinforcing fibers and the resin material constituting the wound body flow, it becomes easy to provide an area including and an area not including the reinforcing fibers on the outer periphery of the protrusion, i.e., on the outer periphery of the hole of the molded body.
[0015] In one embodiment, the wound body may be configured to be positioned in the top plate forming portion so that the extension direction of the reinforcing fibers follows the extension direction of the corner formed between the top plate forming portion and the side wall forming portion.
[0016] According to the above configuration, by aligning the extension direction of the reinforcing fibers with the extension direction of the corner between the top plate forming portion and the side wall forming portion, the reinforcing fibers flow outward together with the resin material from the top plate forming portion through the side wall forming portion, making it easier to reach the protrusion, so that it is possible to more reliably provide areas on the outer periphery of the hole that contain and do not contain reinforcing fibers.
[0017] Furthermore, in order to solve the above-mentioned problems, the technology disclosed herein is a manufacturing apparatus for a molded body containing reinforcing fibers and a resin material, the manufacturing apparatus comprising: a core portion having a rotation axis extending in a direction intersecting the extension direction of the reinforcing fibers, the core portion being configured to be able to wind a fiber-reinforced resin material, in which a bundle of reinforcing fibers is impregnated with a resin material, around the outer periphery of a plurality of spaced-apart folding members; a fixed mold and a movable mold having opposing surfaces facing each other, the fixed mold and the movable mold sandwiching and deforming a wound body of the fiber-reinforced resin material wound by the core portion between the opposing surfaces; and a protrusion provided on at least one of the fixed mold and the movable mold, the protrusion extending from one opposing surface to the other opposing surface at a position not in contact with the wound body before deformation and in contact with the wound body after deformation.
[0018] According to the above configuration, the protrusion extends to a position that is not in contact with the wound body before deformation and to a position that is in contact with the wound body after deformation, so that the hole is formed by being surrounded by the fiber reinforced resin material that has flowed due to the deformation of the wound body. Therefore, it is possible to prevent the reinforcing fibers in the fiber reinforced resin material from breaking, and to easily manufacture a high-strength molded body having a hole. In addition, by being provided at such a position, the protrusion restricts the movement of the reinforcing fibers that flow due to the deformation of the wound body, so that it is possible to easily provide an area that includes reinforcing fibers and an area that does not include reinforcing fibers around the hole of the molded body.
[0019] In one embodiment, the fixed mold and the movable mold have a concave portion on one side and a convex portion on the other side, and have a top plate forming portion, side wall forming portions extending from both ends of the top plate forming portion, and a flange forming portion extending from the side wall forming portion, so that the wound body can be formed into a hat-shaped cross section, and the protrusion may be configured to be provided on the flange forming portion.
[0020] According to the above-mentioned configuration, a molded body having a hat-shaped cross section with high strength can be easily manufactured. In addition, by providing the protrusion on the flange forming portion, it becomes possible to more easily provide an area including reinforcing fibers and an area not including reinforcing fibers on the outer periphery of the hole.
[0021] Furthermore, in order to solve the above-mentioned problems, the technology disclosed herein is a molded body containing reinforcing fibers and a resin material, comprising a top plate portion, side wall portions extending from both ends of the top plate portion, and flange portions extending from both sides of the side wall portions, and has a hat-shaped cross section with a hole in the flange portion, the reinforcing fibers extend along the extension direction of a ridge portion formed between the top plate portion and the side wall portions and are folded back multiple times in that extension direction to form a reinforcing portion, and the flange portion is configured to have a non-reinforced portion that does not contain the reinforcing fibers on the outer periphery of the hole in a direction away from the top plate portion.
[0022] According to the above configuration, the molded body includes, on the outer periphery of the hole, a region that contains reinforcing fibers and a region that does not contain reinforcing fibers, so that while the molded body has the strength required for a part, it is easy to break when removed. Effect of the Invention
[0023] As described above, the manufacturing method and manufacturing apparatus for molded bodies disclosed herein make it possible to easily produce highly functional molded bodies that contain fiber-reinforced resin material but do not contain reinforcing fibers in a specified area around the outer periphery of the hole. [Brief description of the drawings]
[0024] [Figure 1] FIG. 2 is a schematic diagram illustrating an example of a manufacturing apparatus for a molded body. [Diagram 2] FIG. 2 is a schematic cross-sectional view of a press machine. [Diagram 3] FIG. 3 is a view taken along the line III-III in FIG. 2. [Figure 4] FIG. 2 is a schematic cross-sectional view of a press machine before a molding process. [Diagram 5] FIG. 5 is a view taken along the arrows VV in FIG. 4. [Figure 6] FIG. 11 is a schematic cross-sectional view of a press machine in a protruding portion insertion step. [Figure 7] 7 is a cross-sectional view taken along line VII-VII in FIG. 6. [Figure 8] FIG. 11 is a schematic cross-sectional view of the press machine after a core portion removal process. [Figure 9] 9 is a cross-sectional view taken along line IX-IX in FIG. 8. [Figure 10] 11 is a schematic cross-sectional view of a press machine in a resin adding step and a curing step. FIG. [Figure 11] FIG. 4 is a plan view of the fixed mold and the molded body after the curing step. [Figure 12] FIG. [Figure 13] 1 is a flowchart showing an example of a method for producing a molded body. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0025] Hereinafter, exemplary embodiments will be described in detail with reference to the drawings. In the following description, terms indicating directions such as left and right, up and down, and front and back are used, but these terms indicating directions do not limit the arrangement of components or the driving direction of the manufacturing device. In addition, for the convenience of explanation, the scale of each component is appropriately changed, and is not necessarily strictly illustrated.
[0026] X, Y, and Z in the drawings indicate the X-axis direction, the Y-axis direction, and the Z-axis direction. In the following embodiments, the X-axis direction indicates the left-right direction, the Y-axis direction indicates the front-back direction, and the Z-axis direction indicates the up-down direction. These directions can be changed depending on the embodiment, and do not limit the driving direction of the manufacturing apparatus.
[0027] 1 is an exemplary schematic diagram of a manufacturing apparatus for a molded body. The manufacturing apparatus 1 is a manufacturing apparatus for a molded body including reinforcing fibers and a resin material, and is a manufacturing apparatus for a molded body in which a fiber-reinforced resin material 2, in which a bundle of reinforcing fibers is impregnated with a resin material, is molded into a predetermined shape and holes are formed. The manufacturing apparatus 1 includes an unwinding roll 3 that unwinds the fiber-reinforced resin material 2, a core unit 4 configured so that the fiber-reinforced resin material 2 can be wound around it, and a press machine 5 that molds the molded body.
[0028] The reinforcing fibers are not particularly limited as long as they can be used as a fiber-reinforced resin material, and for example, carbon fibers, glass fibers, or fibers made from acrylic, bamboo, or hemp can be used. The thickness of the reinforcing fibers is, for example, 1 to 350 μmm, and preferably 1 to 50 μmm. The reinforcing fibers may be of any color. In addition, the hardness of the reinforcing fibers is not important as long as they can be wound up, but for example, it is preferable that the minimum bending radius is 1 mm or more. The reinforcing fibers are bundled with the resin material to generate a fiber-reinforced resin material 2 that extends along the extension direction of the reinforcing fibers (the X-axis direction in FIG. 1).
[0029] The resin material is not particularly limited as long as it can be used as a fiber-reinforced resin material, and may be, for example, either a thermosetting resin or a thermoplastic resin. Only a thermosetting resin, only a thermoplastic resin, or both a thermosetting resin and a thermoplastic resin may be used. A colorant or other additives may be added to the resin material.
[0030] As the thermosetting resin, for example, an epoxy resin, a vinyl ester resin, a phenol resin, an acrylate resin, a phenoxy resin, a urethane resin, a cyanate resin, etc., can be used. The thermosetting resin may be one type or a combination of two or more types. The thermosetting resin preferably has a viscosity of 100 to 10,000 Pa·sec.
[0031] Examples of the thermoplastic resin that can be used include polypropylene, polyamide, polyester resin, styrene resin, fluororesin, and olefin resin. The thermoplastic resin may be one type or a combination of two or more types. The thermoplastic resin preferably has an MFR (melt flow rate) of 5 to 60 g / 10 min.
[0032] The unwinding roll 3 is cylindrical, and has a fiber reinforced resin material 2, which is a bundle of reinforcing fibers impregnated with a resin material, wound around its outer periphery. The unwinding roll 3 unwinds the fiber reinforced resin material 2 while rotating, and the unwound fiber reinforced resin material 2 is wound around the core portion 4. The extension direction of the reinforcing fibers is approximately parallel to the extension direction of the fiber reinforced resin material 2, which is the X-axis direction in this embodiment. The installation of the unwinding roll 3 is optional, and for example, the fiber reinforced resin material 2 may be wound around the core portion 4 continuously from a process in which the bundle of reinforcing fibers is impregnated with the resin to produce the fiber reinforced resin material 2.
[0033] The core portion 4 is disposed in the unwinding direction of the unwinding roll 3. The fiber reinforced resin material 2 is wound around the core portion 4 to form a wound body 10. The core portion 4 is provided extending in a direction intersecting the extension direction of the reinforcing fibers. Specifically, the core portion 4 includes a rotating shaft 4a extending in a direction intersecting the extension direction of the reinforcing fibers, and a plurality of turn-up members 41, 41 spaced apart from each other on both sides of the rotating shaft 4a. The core portion 4 rotates around the rotating shaft 4a, thereby winding the fiber reinforced resin material 2 around the outer periphery of the turn-up members 41, 41. In this embodiment, the core portion 4 is provided extending in a direction substantially perpendicular to the extension direction of the reinforcing fibers, and the extension direction is the Y-axis direction.
[0034] The multiple folded members 41, 41 are provided extending in a direction intersecting the stretching direction of the reinforcing fibers. The folded members 41 are long and thin cylindrical members. The fiber reinforced resin material 2 is wound around the outer circumference of the multiple folded members 41, 41 to form the wound body 10. This process of winding the fiber reinforced resin material 2 around the core portion 4 to form the wound body 10 is called the winding process. As shown in FIG. 1, the folded members 41, 41 form the wound body 10 having a predetermined width in the extension direction of the folded members 41 by winding the fiber reinforced resin material 2 while shifting its position little by little in the extension direction of the folded members 41.
[0035] In the wound body 10, the fiber reinforced resin material 2 is folded back multiple times in its extension direction, and is wound and arranged in a direction intersecting the extension direction of the fiber reinforced resin material 2 (Y-axis direction in FIG. 1). By increasing the amount of the fiber reinforced resin material 2 wound around the turn-up member 41, the wound body 10 can increase the amount of the fiber reinforced resin material 2 contained in the molded body and increase the amount of reinforcing fibers wound in the molded body, making it easy to increase the strength of the molded body. The fiber reinforced resin material 2 is wound around the outer periphery of the multiple turn-up members 41, 41, so that turn-up parts 2a, 2a of the reinforcing fiber and the fiber reinforced resin material 2 are formed in the turn-up members 41, 41. A plurality of turn-up parts 2a, 2a are formed in the extension direction of the reinforcing fiber and the fiber reinforced resin material 2.
[0036] The press machine 5 is disposed adjacent to the core part 4. The press machine 5 includes a movable die 51 and a fixed die 52 having opposing surfaces 510, 520 opposed to each other, and a resin injection device 55. The core part 4 can enter between the movable die 51 and the fixed die 52, and can retreat to the outside from between the movable die 51 and the fixed die 52. The press machine 5 places the wound body 10 between the movable die 51 and the fixed die 52, and then moves the movable die 51 close to the fixed die 52 to butt the opposing surfaces 510, 520 together, thereby sandwiching and deforming the wound body 10 to mold a molded body. This process of sandwiching and deforming the wound body 10 between the movable die 51 and the fixed die 52 to mold a molded body is called a molding process.
[0037] Fig. 2 is a schematic cross-sectional view of movable die 51 and fixed die 52, and Fig. 3 is a view taken along the line III-III in Fig. 2. As shown in Fig. 2, movable die 51 in this embodiment is a die that is disposed above fixed die 52 and can move up and down. Fixed die 52 is a die that is fixed below movable die 51. Movable die 51 and fixed die 52 are configured to be able to mold wound body 10 into a molded body having a hat-shaped cross section that has a top plate portion and side wall portions extending from both ends of the top plate portion.
[0038] The opposing surface 510 of the movable mold 51 has a recessed portion recessed upward. The recessed portion is composed of a top plate forming portion 51a and side wall forming portions 51b, 51b inclined downward from both front-rear end portions of the top plate forming portion 51a. A corner portion 51d extends at the boundary between the top plate forming portion 51a and the side wall forming portion 51b. In this embodiment, the corner portion 51d extends in the left-right direction. A flange forming portion 51c extends outward in the front-rear direction from the lower end portion of the side wall forming portion 51b. The top plate forming portion 51a forms the upper surface of the top plate portion of the molded body, the corner portion 51d forms the outer surface of the ridge portion of the molded body, the side wall forming portion 51b forms the outer surface of the side wall portion of the molded body, and the flange forming portion 51c forms the upper surface of the flange portion of the molded body.
[0039] The movable die 51 has a protrusion 53 for forming a hole in the molded body. The protrusion 53 extends in a direction intersecting with the extension direction of the core part 4. The protrusion 53 extends downward from the opposing surface 510 of the movable die 51 to the opposing surface 520 of the fixed die 52 at a flange forming part 51c, which is a position where the protrusion 53 is not in contact with the wound body 10 before deformation and is in contact with the wound body 10 after deformation. The protrusion 53 is needle-shaped and tapers at the lower end. It is preferable that a plurality of protrusions 53 are provided at least in the extension direction of the core part 4. At each of the two flange forming parts 51c, 51c at the front and rear positions, two protrusions 53 are formed in the extension direction of the fiber reinforced resin material 2 (X-axis direction in FIG. 1), that is, in the left-right direction. The protrusion 53 moves relatively from the movable die side to the wound body 10 with the vertical movement of the movable die 51. The movable die 51 has a resin injection hole 51e. The resin injection hole 51e communicates with the opposing surface 510 of the top plate forming portion 51a to the opposite surface thereof.
[0040] The facing surface 520 of the fixed mold 52 has a convex portion protruding upward. The convex portion is composed of a top plate forming portion 52a and side wall forming portions 52b, 52b inclined downward from both ends of the top plate forming portion 52a in the front-rear direction. A corner portion 52e is formed extending in the left-right direction at the boundary between the top plate forming portion 52a and the side wall forming portion 52b. In the embodiment, the corner portion 52e is formed extending in the left-right direction. A flange forming portion 52c extends outward in the front-rear direction from the lower end of the side wall forming portion 52b. An abutting portion 52d is formed on the outer side of the flange forming portion 52c and above the flange forming portion 52c. As shown in FIG. 3, the abutting portion 52d is formed on the outer circumferential edge portion of the facing surface 520. The top plate forming portion 52a forms the lower surface of the top plate portion of the molded body, the corner portion 52e forms the inner surface of the ridge portion of the molded body, the side wall forming portion 52b forms the inner surface of the side wall portion of the molded body, and the flange forming portion 52c forms the lower surface of the flange portion of the molded body. The abutment portion 52d abuts on the outer peripheral edge portion of the flange forming portion 51c of the movable die 51 at the bottom dead center of molding.
[0041] A long and thin receiving hole 54 extending downward is provided in the flange forming portion 52c of the fixed die 52. The receiving hole 54 is provided at a position facing the protruding portion 53. When the movable die 51 descends, the protruding portion 53 is inserted into the receiving hole 54.
[0042] The resin injection device 55 is provided above the movable mold 51. Additional resin material is stored in the resin injection device 55. The resin injection device 55 is configured to be able to inject resin between the movable mold 51 and the fixed mold 52 through the resin injection hole 51e.
[0043] In this embodiment, the fixed mold has a receiving hole, and the movable mold has a protruding portion for forming a hole in the molded body, but the protruding portion may be provided on at least one of the fixed mold and the movable mold. Also, the protruding portion may be movable relative to the wound body from either the fixed mold side or the movable mold side. For example, the movable mold may have a receiving hole, and the fixed mold may have a protruding portion, and the protruding portion may move relative to the wound body from the fixed mold side. Also, for example, the protruding portion and the receiving hole may be provided on both the movable mold and the fixed mold. In this embodiment, the fixed mold has a convex portion, and the movable mold has a concave portion, but it is sufficient that one of the fixed mold and the movable mold has a concave portion and the other has a convex portion. In this embodiment, the resin injection hole is provided on the movable mold, but it may be provided on the fixed mold, and the resin injection device may also be provided on the fixed mold side.
[0044] Next, a method for forming the wound body 10 using the manufacturing apparatus 1 will be described.
[0045] Fig. 4 is a schematic cross-sectional view of the press machine before the molding process, and Fig. 5 is a view taken along the line VV in Fig. 4. As shown in Figs. 4 and 5, when the movable die 51 and the fixed die 52 are spaced apart from each other in the vertical direction and the protruding portion 53 is spaced apart from the top plate forming portion 52a of the fixed die 52 and positioned above it, the core portion 4 can enter between the movable die 51 and the fixed die 52. The core portion 4 enters between the movable die 51 and the fixed die 52 with the wound body 10 wound around it. In this embodiment, the core portion 4 moves in parallel in the front-rear direction to enter between the movable die 51 and the fixed die 52. The core portion 4 enters between the movable mold 51 and the fixed mold 52 at an angle such that the direction in which the corners 51d, 52e, which are the boundaries between the top plate forming portions 51a, 52a and the side wall forming portions 51b, 52b, extend (the X-axis direction in Figure 1) and the extension direction of the core portion 4 (the Y-axis direction in Figure 1) are approximately perpendicular.
[0046] The core portion 4 places the wound body 10 on the top plate forming portion 52a. The wound body 10 is placed so that the extension direction of the reinforcing fiber and fiber reinforced resin material 2 is approximately parallel to the extension direction of the corners 51d and 52e formed by the top plate forming portions 51a and 52a and the side wall forming portions 51b and 52b. The folded members 41 and 41 are placed at both left and right ends of the top plate forming portion 52a. The folded portions 2a and 2a of the reinforcing fiber and fiber reinforced resin material 2 are located at both left and right ends of the top plate forming portion 52a.
[0047] Fig. 6 is a schematic cross-sectional view of the press in the protruding portion insertion step, and Fig. 7 is a cross-sectional view taken along line VII-VII in Fig. 6. As movable die 51 descends from the state shown in Fig. 4, protruding portion 53 descends and is inserted into receiving hole 54 of fixed die 52. At this time, protruding portion 53 is not in contact with undeformed wound body 10 arranged on top plate forming portion 51a. This step of inserting protruding portion 53 into receiving hole 54 is called a protruding portion insertion step.
[0048] In the protrusion insertion step, the wound body 10 may be placed on the opposing surfaces 510, 520 of either the movable die 51 or the fixed die 52. In this embodiment, the wound body 10 is placed on the top plate forming part 52a of the fixed die 52, but is not limited thereto, and may be placed on the top plate forming part 51a of the movable die.
[0049] From the state shown in Fig. 6, the movable die 51 descends further, and before the opposing surface 510 of the movable die 51 collides with the core part 4, the core part 4 is removed from between the movable die 51 and the fixed die 52. More specifically, while the protruding part 53 is inserted into the receiving hole 54, the core part 4 is pulled out from the wound body 10 by the time the movable die 51 and the fixed die 52 reach the bottom dead center position of the molding. The core part 4 is removed from between the movable die 51 and the fixed die 52, leaving the wound body 10 on the top plate forming part 52a. This process of pulling out the core part 4 from the wound body 10 is called a core part removal process.
[0050] FIG. 8 is a schematic cross-sectional view of the press machine after the core portion removal step, and FIG. 9 is a cross-sectional view taken along line IX-IX in FIG. 8, with the movable die omitted.
[0051] FIG. 10 is a schematic cross-sectional view of the press machine in the resin adding step and the curing step. After the core portion 4 is pulled out, a part of the flange forming portion 51c of the movable mold 51 abuts against the abutting portion 52d of the fixed mold 52, and the position is the bottom dead center of molding shown in FIG. 10. Before the movable mold 51 and the fixed mold 52 reach the bottom dead center of molding, or after they reach the bottom dead center of molding, additional resin material is injected from the resin injection device 55 into the space between the movable mold 51 and the fixed mold 52 through the resin injection hole 51e. This step of adding resin material between the opposing surfaces 510 and 520 is called the resin adding step. Thereafter, at the bottom dead center of molding, the movable mold 51 and the fixed mold 52 are heated, so that the wound body 10 is deformed and cured to become the molded body 100. This step of curing the wound body 10 is called the curing step. In the curing step, the fiber reinforced resin material is cured by a curing method according to the type of resin material used, such as by heating or leaving it at room temperature for a long time.
[0052] FIG. 11 is a plan view of the fixed mold and the molded body after the curing step. After the wound body 10 is placed on the convex portion, the fixed mold 52 and the movable mold 51 butt the opposing surfaces 510, 520 together to cause the reinforcing fibers and the resin material to flow outward from the convex portion, thereby deforming the wound body 10. Before the curing step, the fiber-reinforced resin material 2 is placed on the top plate forming portion 52a of the fixed mold 52 as the wound body 10, but is pressed by the movable mold 51 and the fixed mold 52 and heat is applied, so that the reinforcing fibers and the resin material flow and harden to become the molded body 100. The reinforcing fibers in the fiber-reinforced resin material 2 flow in the arrangement direction of the reinforcing fibers. In the wound body 10 of this embodiment, the reinforcing fibers are folded back with the direction in which the corners 51d, 52e extend as the extension direction, and are wound back to be arranged in a direction approximately perpendicular to the direction in which the corners 51d, 52e extend. Therefore, the reinforcing fibers in the fiber-reinforced resin material 2 flow together with the resin material in a direction substantially perpendicular to the direction in which the corners 51d and 52e extend, that is, from the top plate forming portion 52a to the flange forming portion 52c, to form the molded body 100. The protruding portion 53 is provided on the flange forming portion 51c, which is outside the convex portion, that is, outside (downstream) the top plate forming portion 51a and the side wall forming portion 51b in the flow direction of the reinforcing fibers and the resin material. The reinforcing fibers that flow from the top plate forming portion 52a to the flange forming portion 51c are restricted in flow by the protruding portion 53, and flow outward in the area where the protruding portion 53 is not present. The molded body 100 has a hole 104 at the location where the protruding portion 53 is removed.
[0053] 12 is a perspective view of a molded body. The molded body 100 manufactured by the above-mentioned manufacturing apparatus 1 has a top plate portion 101, side wall portions 102 extending downward from both ends of the top plate portion 101, a ridge portion 105 formed between the top plate portion 101 and the side wall portions 102, and a flange portion 103 extending outward from the lower end portion of the side wall portions 102. The molded body 100 is a member having a hat-shaped cross section that is used, for example, for automobile pillars, etc.
[0054] The molded body 100 has a reinforced portion 100a and a non-reinforced portion 100b. The reinforced portion 100a is a region in which the reinforced fibers are folded back multiple times in the extension direction and wound around the extension direction to be arranged in a direction intersecting the extension direction. In the reinforced portion 100a, the reinforced fibers extend along the extension direction of the ridge portion 105 formed by the top plate portion 101 and the side wall portion 102. The non-reinforced portion 100b is a region that does not include the reinforced fibers. The flange portion 103 has a hole 104. In this embodiment, the fiber reinforced resin material 2 flows from the top plate portion 101 to the flange portion 103, so that the reinforced portion 100a exists from the top plate portion 101 to the flange portion 103, but in the flange portion 103, the protruding portion 53 restricts the flow of the reinforced fibers, so that a part of the region of the flange portion 103 is the non-reinforced portion 100b. The flange portion 103 has a non-reinforced portion 100b that does not contain reinforcing fibers on the outer periphery of the hole 104 in a direction away from the top plate portion 101, i.e., on the outer side in the flow direction of the reinforcing fibers. The hole 104 is located at the boundary between the reinforced portion 100a and the non-reinforced portion 100b. The boundary between the reinforced portion 100a and the non-reinforced portion 100b is wavy. The molded body 100 has strength as a part due to the reinforced portion 100a, and can be easily broken when removed due to the non-reinforced portion 100b formed on part of the outer periphery of the hole 104.
[0055] 13 is a flowchart showing an example of a method for manufacturing a molded body. As described above, the method for manufacturing a molded body of the present disclosure includes a winding step S10 and a molding step S20. The molding step S20 includes a protrusion insertion step S11, a core removal step S12, a resin addition step S13, and a curing step S14.
[0056] The winding step S10 is a step of winding a fiber-reinforced resin material 2, which is a bundle of reinforcing fibers impregnated with a resin material, around a core portion 4 extending in a direction intersecting the extension direction of the reinforcing fibers to produce a wound body 10. This step makes it possible to form the wound body 10, which is the raw material for the molded body, without cutting the reinforcing fibers in the fiber-reinforced resin material 2.
[0057] The protruding portion insertion step S11 is a step of inserting the protruding portion 53 into the receiving hole 54. In the protruding portion insertion step S11, the protruding portion 53 is not in contact with the undeformed wound body 10 arranged on the top plate forming section 51a. The protruding portion 53 is arranged before the curing step S14, and after the curing step S14, the protruding portion 53 is pulled out to form a hole 104 at the position of the protruding portion 53. This step makes it possible to easily form the portion of the molded body 100 that will become the hole 104, and prevents breakage of the reinforcing fibers.
[0058] The core portion removal step S12 is a step in which, after the protrusion insertion step S11 and before the hardening step S14, the core portion 4 is pulled out from the wound body before the fixed die 52 and the movable die 51 reach the molding bottom dead center position in the hardening step S14. By pulling out the core portion 4 while the movable die 51 is moving toward the fixed die 52, a plurality of steps are performed consecutively or partially in parallel, thereby improving manufacturing efficiency.
[0059] The resin adding step S13 is a step in which additional resin material is injected from a resin injection device 55 through a resin injection hole 51e into the space between the movable die 51 and the fixed die 52 before or after the movable die 51 and the fixed die 52 reach the molding bottom dead center. Although it is possible to mold the molded body 100 using only the resin material that seeps out from the wound body 10 when the wound body 10 is pressed, the molded body 100 can be molded more reliably by adding resin material.
[0060] The curing step S14 is a step of curing the wound body 10 with the holes formed therein. In this embodiment, the wound body 10 is molded and thermally cured by the press machine 5. The wound body 10 is deformed by the press machine 5, and is cured in a state in which the reinforcing fibers and the resin material flow to the outer periphery of the protruding portion 53.
[0061] According to the manufacturing method and manufacturing apparatus configured as described above, it is possible to easily manufacture a high-strength molded body having holes by preventing the reinforcing fibers in the fiber-reinforced resin material from breaking. In addition, by being provided at such a position, the protrusion restricts the movement of the reinforcing fibers that flow due to the deformation of the wound body, so that it is possible to easily provide an area containing reinforcing fibers and an area not containing reinforcing fibers around the holes of the molded body. Furthermore, since the reinforcing fibers are not cut and the reinforcing fibers are folded back and wound to form the reinforcing portion, when the molded body manufactured by this manufacturing method and manufacturing apparatus is recycled, the reinforcing fibers are easily dissolved when the resin material is melted, and long reinforcing fibers can be recovered, so that the recyclability is very high.
[0062] The above-described embodiments are merely illustrative and should not be construed as limiting the scope of the present disclosure. The scope of the present disclosure is defined by the claims, and all modifications and variations within the scope of the claims are within the scope of the present disclosure. [Industrial Applicability]
[0063] The technology disclosed herein is suitable for use as a manufacturing method and manufacturing apparatus for a molded article including a fiber-reinforced resin material and having holes. [Explanation of symbols]
[0064] 1 Manufacturing equipment 2. Fiber-reinforced resin materials 2a Folded part 3 Unwinding roll 4 Core 4a Rotation axis 5 Press machine 10 Winding body 41 Folding member 51 Movable type 52 Fixed type 53 Protrusion 54 Receptacle 55 Resin injection device 100 Molded body 100a Reinforcement 100b Non-reinforced part 101 Top plate 102 Side wall 103 Flange part 104 holes 105 Ridge S10 Winding process S11 Protruding part insertion process S12 Core removal process S13 Resin addition process S14 Curing process S20 Molding process
Claims
1. A method for producing a molded body containing reinforcing fibers and a resin material, comprising: A winding process in which a fiber-reinforced resin material obtained by impregnating a bundle of reinforcing fibers with a resin material is wound around a core portion extending in a direction intersecting the extension direction of the reinforcing fibers to form a wound body; a molding step of providing a fixed mold and a movable mold having opposing surfaces facing each other, disposing the wound body between the fixed mold and the movable mold, and then moving the movable mold toward the fixed mold to butt the opposing surfaces together, thereby deforming the wound body and forming a molded body, A method for manufacturing a molded body, wherein at least one of the fixed mold and the movable mold has a protrusion for forming a hole in the molded body, and the protrusion extends from one opposing surface to the other opposing surface at a position that is not in contact with the wound body before deformation and at a position that contacts the wound body after deformation.
2. The method for producing a molded article according to claim 1, A method for manufacturing a molded body, comprising a resin adding process of adding resin material between the opposing surfaces before the movable mold and the fixed mold reach a molding bottom dead center position in the molding process or after they reach a molding bottom dead center position.
3. The method for producing a molded article according to claim 1, A method for manufacturing a molded body, comprising a core portion removal step in which the core portion is pulled out from the wound body before the movable mold and the fixed mold reach a bottom dead center position in the molding step.
4. The method for producing a molded article according to claim 1, one of the fixed mold and the movable mold has a recess and the other has a protrusion, the recess and the protrusion each having a top plate forming portion and a side wall forming portion extending from both ends of the top plate forming portion, and the wound body can be molded into a hat-shaped cross section, and after the wound body is placed on the protrusion, the opposing surfaces are butted together to cause the wound body to flow outward from the protrusion, The method for manufacturing a molded body, wherein the protrusion is provided outside the protrusion.
5. The method for producing a molded article according to claim 4, A method for manufacturing a molded body, wherein the wound body is placed on the top plate forming portion so that the extension direction of the reinforcing fibers follows the extension direction of a corner formed between the top plate forming portion and the side wall forming portion.
6. An apparatus for manufacturing a molded body containing reinforcing fibers and a resin material, A core portion having a rotation axis extending in a direction intersecting the extension direction of the reinforcing fibers, and configured so that a fiber-reinforced resin material obtained by impregnating a bundle of the reinforcing fibers with a resin material can be wound around the outer periphery of a plurality of turn-up members spaced apart from each other; A fixed mold and a movable mold have opposing surfaces facing each other, and sandwich and deform the wound body of the fiber reinforced resin material wound around the core portion between the opposing surfaces; A molded body manufacturing apparatus comprising: a protrusion provided on at least one of the fixed mold and the movable mold, the protrusion extending from one opposing surface to the other opposing surface at a position that is not in contact with the wound body before deformation and at a position that is in contact with the wound body after deformation.
7. The apparatus for producing a molded body according to claim 6, the fixed die and the movable die have a concave portion on one side and a convex portion on the other side, and the fixed die and the movable die have a top plate forming portion, side wall forming portions extending from both ends of the top plate forming portion, and flange forming portions extending from the side wall forming portions so that the wound body can be formed into a hat-shaped cross section; The protrusion is provided on the flange forming portion.
8. A molded body including reinforcing fibers and a resin material, The container has a top plate portion, side walls extending from both ends of the top plate portion, and flanges extending from both sides of the side walls, and has a hat-shaped cross section with a hole in the flange portion, The reinforcing fibers extend along a direction in which a ridge portion formed between the top plate portion and the side wall portion extends, and are folded back multiple times in the extension direction to form a reinforcing portion, The flange portion has a non-reinforced portion that does not contain the reinforcing fibers in a direction away from the top plate portion on the outer periphery of the hole.
Citation Information
Patent Citations
Fiber reinforced plastic laminated spring and manufacture thereof
JP1985132140A