Method and apparatus for repairing defect of lithographic mask
The method addresses the challenge of micro-defect repair in photolithographic masks by strategically placing repair elements with deviating parameters, simplifying the process and improving efficiency and cost-effectiveness in defect correction.
Patent Information
- Application Number
- JP2024113098
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-07-17
- Filing Date
- 2024-07-16
- Publication Date
- 2024-10-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The increasing complexity and cost of manufacturing photolithographic masks due to finer structural elements and the difficulty in repairing micro-defects, which are difficult to detect and correct, especially when deviations from design specifications are small.
A method and apparatus for repairing micro-defects in lithographic masks by determining repair shapes with parameters that deviate from predefined values, allowing for localized etching or deposition processes using focused particle beams and precursor gases, with repair elements placed strategically to compensate for defects without exact alignment, thus simplifying the repair process.
This approach significantly reduces the sensitivity of repair element placement, allowing for faster and more effective correction of micro-defects, maintaining mask quality without precise alignment requirements, and reducing the time and cost associated with defect repair.
Smart Images

Figure 2024153689000001_ABST
Abstract
Description
[Technical field]
[0001] This patent application claims the priority of German patent application DE 10 2020 208 980.9, filed on July 17, 2020 with the German Patent and Trademark Office and entitled "Verfahren und Vorrichtung zum Reparieren eines Dekts einer lithographischen Maske", which is incorporated by reference in its entirety into this patent application.
[0002] The present invention relates to a method and an apparatus for repairing at least one defect in a lithographic mask.Furthermore, the present invention relates to a method and an apparatus for repairing at least one pattern element in a lithographic mask. [Background technology]
[0003] As a result of increasing integration density in the semiconductor industry, lithography masks have to image smaller and smaller structures on the wafer. To take this trend into account, a possibility is to use lithography or photolithography masks whose light wavelengths are shifted towards shorter wavelengths. Currently, ArF (argon fluoride) excimer lasers emitting at a wavelength of about 193 nm are often used as light sources for photolithography. The use of masks for double or multiple exposure makes it possible to produce structures in the photoresist with dimensions that are not possible to realize in a single exposure step.
[0004] Currently, photolithography systems using electromagnetic radiation in the EUV (extreme ultraviolet) wavelength range (preferably 10 nm to 15 nm) are being developed. These EUV photolithography systems are based on a completely new beam guide concept using reflective optical elements, since no optically transparent materials are currently available in the EUV range. The technical challenges in developing EUV systems are numerous, and a significant development effort is required to bring the systems to an industrially applicable level.
[0005] Lithography masks, photolithography masks, exposure masks, photomasks, or simply masks, play a key role in imaging fine structures in the photoresist placed on the wafer. The higher the integration density, the more important it becomes to reduce the minimum feature size that the exposure mask can image. To ensure that the increasingly smaller mask features can be imaged in the photoresist applied to the wafer, resolution enhancement techniques (RET), such as optical proximity correction (OPC) techniques, are increasingly used. W.-M. Gan et al.: "Placement of sub-resolution assist features based on a generic algorithm", DOI 10.1109 / ACCESS.2019.2926102, IEEE ACCESS, P. Gupta et al.: "Manufacturing-aware design methodology for assist feature correctness", Design and Process Integration for Microelectronic Manufacturing III, Proc. of SPIE Vol. 4756, Bellingham, WA, 2005, doi: Exemplary documents such as U.S. Patent Application Publication No. 10.1117 / 12.604872, U.S. Patent Application Publication No. 2006 / 0046160, U.S. Patent No. 8,739,080 B1, U.S. Patent No. 8,498,469 B2, U.S. Patent Application Publication No. 2008 / 0077907, U.S. Patent Application Publication No. 2009 / 0258302, and U.S. Patent No. 10,318,697 B2 describe various aspects of RET or OPC techniques.
[0006] Due to the combination of smaller and smaller structural or pattern elements and the use of RET technology, the process of manufacturing photolithographic masks has become increasingly complex, time consuming and, as a result, more expensive.
[0007] Due to the small structural size of the pattern elements, even the smallest deviations from the design specifications of the pattern elements generated on the wafer during mask manufacturing appear as visible or "printable" errors. These need to be repaired whenever possible. Due to the small dimensional size of defects found on the wafer, e.g. values in the low double-digit nanometer range, the costs of detecting said defects are becoming prohibitively expensive. Furthermore, repairing smaller defects is becoming increasingly difficult. Firstly, positioning a repair tool relative to an identified defect is only possible by very complex metrology, and secondly, setting up the repair tool for a specific micro-defect requires a lot of time.
[0008] The present invention therefore specifically addresses the problem of defining a method and apparatus for improving the repair of micro-defects in lithographic masks. Summary of the Invention
[0009] According to an exemplary embodiment of the present invention, the above problem is solved by a method according to claim 1 and an apparatus according to claim 22. In another exemplary embodiment, the above problem is solved by a method according to claim 18 and an apparatus according to claim 23.
[0010] In one embodiment, a method for repairing at least one defect of a lithographic mask includes a step of determining a parameter of at least one repair feature for at least one defect, comprising assigning at least one numerical value to the parameter, the numerical value deviating from a predefined numerical value for said parameter by at least one defect. In particular, this may be advantageous for small defects, i.e. defects having at least one dimension size that is 10 times the resolution limit of the mask, 5 times the resolution limit, 3 times the resolution limit, or smaller than the resolution limit. It may be particularly advantageous when the small defect has at least one dimension size within a range of 2% to 50% of the resolution limit.
[0011] The parameters of the repair shape used to repair a defect are usually dictated by the defect to be repaired. The inventors have discovered through a comprehensive analysis that the compensation or repair of particularly very small defects, which could only be removed with great difficulty up until now, can be significantly simplified if at least one of the parameters of the repair shape is assigned a value different from the value actually required to repair the defect. In particular, this can be advantageous for small defects, i.e. defects having at least one dimension size within the range of 2% to 50% of the resolution limit of the mask.
[0012] In the following, a repair shape whose parameters only have values determined on the basis of measured values is also referred to as a nominal repair shape. The nominal repair shape is usually formed by the difference between a measured mask segment with a defect and an equivalent measured mask segment without a defect. Alternatively and / or additionally, it is also possible to generate the nominal repair shape by subtracting design data of the measured defective mask segment from the latter. The repair shape used in the method according to the invention differs from the nominal repair shape in that at least one parameter of the former has a value that deviates from the value determined by the measurement results.
[0013] In short, it can be advantageous to perform the repair (for example of an edge error) not only on the basis of a parameter whose value is predefined by each defect (for example in the case of an edge error due to the difference between an erroneous edge position and a target edge position predefined by the mask design). This is because the correction of this (small) defect requires a very precise repair, especially if the parameter's value is within or below the resolution limit (for example the edge position is only slightly in error). Small errors in the repair can have the effect that the repair does not involve a significant improvement. However, if each defect causes a targeted deviation from the predefined value for the corresponding parameter, the impact of the errors in the repair is significantly smaller, so that the requirements of the repair process can be relaxed, if necessary.
[0014] The method according to the invention will be described below on the basis of the example of edge placement errors of pattern elements. The deviation dx of the edge of a pattern element from the specification of the mask design is converted by the mask in the exposure process into an edge placement error EPE, which is given by the product of the deviation dx, a possible mask enhancement factor MEEF (Mask Error Enhancement Factor) for the defect or deviation, and the magnification or demagnification of the projection lens arranged downstream of the mask. The magnification of the projection lens of a photolithographic exposure system is often M=1 / 4 or M=1 / 5.
[0015] However, when the deviation dx of the edges of the pattern elements becomes smaller than the resolution limit of the photolithographic mask, the latter significantly reduces the deviation dx in the exposure process, resulting in smaller edge placement errors. This is due to the averaging of the photomask's light beam emission over structures whose dimensions are smaller than the resolving capability of the mask. The details of this averaging process depend on the structures considered and the details of the exposure process used to image these structure elements. This application exploits this importance to facilitate the repair of defects whose dimensions are below the resolution limit of the lithographic mask.
[0016] In this respect, for example in the case of an edge repair of a pattern element, if the parameters of the repair (or the parameters of the corresponding nominal repair shape) actually require the deposition of material from the measurement edge (numerically predefined by the defect) to the target edge, the material can be intentionally deposited at a distance from the measurement edge, and the material is optionally deposited short. Thus, errors in the exact positioning of the deposited material have little effect on the quality of the repaired mask (e.g. due to diffraction effects). This is equally true in the case of errors requiring etching of material, e.g. in the case of an edge error, the material can be etched at a distance from the measurement edge.
[0017] The repair shape is a combination of instructions that the repair tool executes to remove defects on the photomask. In the case of the example of a defect with excess material, the repair shape represents a local etching process that can be used to remove excess material from the mask. The repair shape usually has a reference area that is scanned by the particle beam as defined in the repair shape. This means that the repair shape defines the energy of the particles of the particle beam, the spot width at the focus of the particle beam, the residence time of the particle beam at a certain location, the distance between adjacent points of incidence of the particle beam on the mask or defect, and the time until the particle beam reaches the starting point again. The area scanned by the particle beam and the values of the above parameters can also be considered to change during the realization of the repair shape. In the case of a local etching process, the repair shape also defines the time progression of the supply of the etching gas. That is, the repair shape controls the gas volume flow rate of the etching gas during the processing of at least one defect.
[0018] In this application, the term lithographic mask includes photolithographic masks.
[0019] The at least one parameter may include at least one element from the group including at least one lateral dimension of the at least one repair feature, at least one height dimension of the at least one repair feature, a distance between the at least one repair feature and the at least one defect, a material composition of the at least one defect, a geometric shape of the at least one repair feature, and an environment of the at least one defect on the lithographic mask. The material composition of the at least one defect primarily determines its complex refractive index.
[0020] The facilitation or improvement of repair or compensation of small defects can be brought about by various means. In one respect, the defect does not need to be repaired 1:1, as predefined by the parameters of the nominal repair shape. In this respect, the nominal area of the repair shape can be smaller than the nominal area of the defect. In another respect, the height of the repair shape can be smaller than the height of the defect. Thus, the above-defined method allows for defect correction where the material removal from or material deposition on the mask can be smaller than the volume of the defect. This situation has a positive impact on the defect processing time.
[0021] In another aspect, the above-mentioned averaging of the light radiation over structures smaller than the resolving power allows the repair feature to be placed some distance away from the original defect location, resulting in a clear relaxation of the very stringent requirements for the positional accuracy when placing the repair feature of the defect, without significant adverse effects on the quality of the defect repair or compensation.
[0022] Furthermore, the geometry of the repair shape may deviate from the actual defect shape, which obviously simplifies the defect repair since the repair shape may be selected at least partially independent of the defect shape, which may result in a significantly simplified generation of the geometry.
[0023] At least one parameter may deviate by a predetermined absolute value from a predefined numerical value for said parameter due to at least one defect.
[0024] The deviation in the value of the at least one lateral parameter may be selected from a range with a lower limit greater than zero and an upper limit less than the resolution limit (of the defect-free area) of the lithographic mask.
[0025] The resolution limit of a lithography mask may be determined by the light wavelength of the lithography mask, the numerical aperture (NA), and the exposure settings suitable for projecting the pattern of the lithography mask onto the photoresist disposed on the wafer.
[0026] The numerical aperture may include the NA of a projection lens of an exposure system suitable for projecting a pattern of a lithography mask onto a photoresist. The NA of the projection lens is also referred to as the mask side numerical aperture (NA M ).
[0027] Lithography masks are usually designed to work in a particular exposure system, which depends on the wavelength of the light, the numerical aperture (NA) of the projection lens of the exposure system, etc. M ), and in particular the exposure settings used by the exposure system that projects the lithography mask's pattern into the photoresist. In this sense, the design of the lithography mask determines or defines its resolution limit.
[0028] The resolution limit of a lithographic mask may include the mask resolution limit of an exposure system suitable for exposing a wafer with the lithographic mask.
[0029] Mask side resolution limit (R M )teeth,
number
[0030] Mask side resolution limit R M is proportional to the light wavelength λ, and the mask side numerical aperture NA M Inversely proportional to NA M The value of can range from about 0.1 to 0.5. Furthermore, the resolution limit of a lithography mask is determined by the exposure setting σ of the exposure system that uses the lithography mask to expose the wafer. The value of σ ranges from 0 (for central illumination) to 1 (for maximum oblique illumination). In the technical field, oblique exposure is also called off-axis exposure.
[0031] Numerical aperture NAM Depending on the exposure setting σ, the resolution limit of a photomask exposed at a deep ultraviolet (DUV) wavelength λ = 193 nm is 150 nm ≤ R M For EUV masks with a light wavelength of λ = 13.5 nm, the resolution limit is currently 50 nm ≤ R M ≦100 nm. This means that as the wavelength of the light of the photolithography mask becomes shorter, the range in which the value of one or more parameters of the repair feature can be chosen shrinks. In other words, the method defined above allows new degrees of freedom to be used in the DUV wavelength range, which is wider than in the EUV wavelength range.
[0032] The deviation in the value of at least one parameter may be in the range of 2% to 80%, preferably 2% to 50%, most preferably 2% to 30% of the resolution limit of the lithographic mask.
[0033] The dimensional size of at least one dimension of the at least one repair feature may range from 10% to 90%, preferably 20% to 80%, more preferably 30% to 70%, and most preferably 40% to 60% of the dimensional size of the corresponding dimension of the at least one defect.
[0034] The dimensional size of at least one dimension of the at least one repair feature may include at least one lateral dimension and / or a height of the at least one repair feature.
[0035] The distance between the at least one repair feature and the at least one defect may be in the range of 2% to 80%, preferably 2% to 50%, more preferably 2% to 30%, and most preferably 2% to 10% of the resolution limit of the defect-free area of the lithography mask.
[0036] The repair shape may be laterally displaced relative to the nominal repair shape, may deviate laterally in its dimension size relative to the nominal repair shape, and may deviate in its height relative to the nominal repair shape such that the repair shape and the nominal repair shape produce substantially the same light intensity distribution in the photoresist. This means that the lateral dimension size and the height of the repair shape can be combined or correlated. As an example, if the height of the repair shape is small, this can be compensated by increasing one or both lateral dimensions, and vice versa. Furthermore, a correlation between the height or lateral dimension size of the repair shape relative to the defect and the lateral displacement of the repair shape is also possible. The details depend on the repair shape, the environment of the mask in which the repair shape is generated, and the exposure process.
[0037] The at least one defect may include at least one element from the group including edge placement error of a pattern element, interruption and / or cross-linking of a pattern element, edge roughness deviation of a pattern element, particle adhesion to a lithography mask, lateral defects with low printability, residual defects of a defect repair performed, sidewall angle error of a pattern element, centroid error of a pattern element and / or distance range between two pattern elements.
[0038] The step of determining the parameters of the at least one repair feature may include recording at least one aerial image of the at least one defect. The aerial image may be measurable by a mask inspection apparatus. The mask inspection apparatus may include an optical inspection apparatus and / or an inspection apparatus that scans the mask surface. The optical mask inspection apparatus may include, for example, a laser interferometer, and the mask inspection apparatus that scans the mask surface may include, for example, an atomic force microscope. The optical mask inspection apparatus may be designed to record an aerial image and / or aerial image focus synthesis of the photomask.
[0039] Recording at least one aerial image may include recording at least one aerial image of the at least one defect at a light wavelength of the lithography mask and / or recording an aerial image focus synthesis of the at least one defect. By recording an aerial image at a light wavelength, the aerial image shows details that are imaged in the subsequent exposure of the photomask in the photoresist. It is therefore advantageous to record an aerial image at a light wavelength of the mask. It is further advantageous to determine the imaging behavior of defective areas of the photolithography mask during adjustment through the focus of the mask.
[0040] Determining the parameter of the at least one repair feature may include scanning the at least one defect with a scanning particle microscope and / or a scanning probe microscope. Further, determining the parameter of the at least one repair feature may include recording at least one aerial image of the at least one defect and scanning the at least one defect with a scanning particle microscope and / or a scanning probe microscope.
[0041] The scanning particle microscope may include at least one member from the group including scanning electron microscope (SEM), scanning ion microscope (FIB (focused ion beam)), and scanning electron microscope with polarization assessment (SEMPA).
[0042] The scanning probe microscope may include at least one member from the group including a scanning tunneling microscope (STM), an atomic force microscope (AFM), a magnetic force microscope (MFM), a scanning near-field optical microscope (SNOM), and a scanning near-field acoustic microscope (SNAM).
[0043] The step of determining a parameter of the at least one repair shape may be further based on at least one element from the group including exposure settings for exposing the lithography mask during operation, design data of the lithography mask, refractive index data of the deposited material for repairing material loss defects, and RET techniques for resolution enhancement of the lithography mask.
[0044] Determining parameters of the at least one repair shape may include applying at least one algorithm to measurement data of the at least one defect and design data of the lithography mask.
[0045] The at least one algorithm can be implemented using hardware, software, firmware, or a combination thereof. Furthermore, the at least one algorithm can be stored in a non-volatile memory. In particular, the at least one algorithm can be stored in a semiconductor memory (SSD (Solid State Drive)).
[0046] Assigning a numerical value may include applying a trained machine learning model to determine deviations of the numerical value of at least one parameter from a predefined numerical value due to at least one defect for said parameter.
[0047] The machine learning model may include a transformation model having at least two transformation blocks, each of which includes at least a generically learnable function that transforms an input into an output that is used as an input for a subsequent transformation block. The machine learning model may include at least one member from the group including parametric mapping, artificial neural networks, deep neural networks, time-delay neural networks, convolutional neural networks, recurrent neural networks, long-term memory networks, developmental models, kernel density estimators, statistical models, decision trees, linear models, and time-invariant models.
[0048] The machine learning model may include (a) at least one encoder block that determines information-carrying characteristics of an image of at least one defect and design data assigned to the image of the at least one defect, and (b) at least one decoder block that generates at least one effect of the at least one defect from the determined information-carrying characteristics, wherein the at least one effect of the at least one defect indicates what a registration of the image of the at least one defect with the corresponding design data looks like.
[0049] The step of determining the parameters of the at least one repair shape may include applying a trained machine learning model to determine the parameters of the at least one repair shape.
[0050] In at least two embodiments of the above-mentioned method, a trained machine learning model can be used. First, a corresponding trained machine learning model can be used to assign one or more parameters of the repair shape with one or more numerical values that deviate as a result of at least one defect. However, it is also possible, and this is the currently preferred embodiment, that the corresponding trained machine learning model determines all parameters of the at least one repair shape for repairing at least one defect based on measurement data (e.g. one or more aerial images of the defect), design data of the mask, and optionally the structure of one or more RET techniques.
[0051] The method according to the invention may further comprise the step of generating at least one repair element on the lithographic mask according to the determined repair shape, whereby a repair element is generated on the photomask that is designed as far as possible to remove, i.e. repair or compensate for, the at least one defect by implementing the repair shape.
[0052] The at least one repair element may be prevented from being imaged during exposure of the photolithographic mask. The at least one repair element may change the imaging behavior of the at least one defect during exposure of the lithographic mask.
[0053] The generated repair elements typically deviate from the nominal repair shape below the resolution limit of the photolithography mask, and therefore may be considered not to be imaged into the photoresist and thus the wafer directly below during exposure of the mask with the light wavelength. However, the generated repair elements on the mask are designed to change the imaging behavior of the defective areas of the photomask, so that the combination of the defective areas and the repair elements results in imaging behavior that closely resembles a defect-free area with the same pattern placement. As a result, during the exposure process, the repaired mask produces edge positions that are substantially the same as the defect-free mask. The effect of the at least one repair element is based at least in part on the different effects of the light exposure radiation on the repair element.
[0054] The step of generating the at least one repair element may include performing at least one localized etching process and / or performing at least one localized deposition process with at least one focused particle beam and at least one precursor gas.
[0055] The at least one focused particle beam may include at least one member from the group including: a photon beam, an electron beam, an ion beam, an atomic beam, and a molecular beam.
[0056] The at least one precursor gas may include at least one member from the group including an etching gas, a deposition gas, and an additive gas.
[0057] Etching gases include halogens (F2, Cl2, Br2, J2), oxygen (O2), ozone (O3), hydrochloric acid (HCl), hydrogen fluoride (HF), xenon difluoride (XeF2), xenon tetrafluoride (XeF4), xenon hexafluoride (XeF6), xenon chloride (XeCl), argon fluoride (ArF), krypton fluoride (KrF), sulfur difluoride (SF2), sulfur tetrafluoride. The gas may include at least one member from the group including (SF4), sulfur hexafluoride (SF6), nitrosyl chloride (NOCl), phosphorus trichloride (PCl3), phosphorus pentachloride (PCl5), phosphorus trifluoride (PF3), nitrogen trifluoride (NF3), water vapor (H2O), hydrogen peroxide (H2O2), nitrous oxide (N2O), nitric oxide (NO), nitrogen dioxide (NO2), and nitric acid (HNO3).
[0058] The at least one deposition gas can include at least one member from the group including metal alkyls, transition element alkyls, main group element alkyls, metal carbonyls, transition element carbonyls, main group element carbonyls, metal alkoxides, transition element alkoxides, main group element alkoxides, metal complexes, transition element complexes, main group element complexes, and organic compounds.
[0059] The metal alkyls, transition element alkyls, and main group element alkyls may include at least one member from the group including cyclopentadienyl (Cp) trimethylplatinum (CpPtMe3), methylcyclopentadienyl (MeCp) trimethylplatinum (MeCpPtMe3), tetramethyltin (SnMe4), trimethylgallium (GaMe3), ferrocene (Co2Fe), and bisallylcuronium (Ar2Cr).
[0060] Metal carbonyls, transition element carbonyls, and main group element carbonyls include chromium hexacarbonyl (Cr(CO)6), molybdenum hexacarbonyl (Mo(CO)6), tungsten hexacarbonyl (W(CO)6), dicobalt octacarbonyl (Co2(CO)8), triruthenium dodecacarbonyl (Ru3(CO) 12 ), and iron pentacarbonyl (Fe(CO)5).
[0061] The metal alkoxides, transition element alkoxides, and main group element alkoxides may include at least one member from the group including tetraethylorthosilicate (TEOS, Si(OC2H5)4) and tetraisopropoxytitanium (Ti(OC3H7)4). The metal halides, transition element halides, and main group element halides may include at least one member from the group including tungsten hexafluoride (WF6), tungsten hexachloride (WCl6), titanium hexachloride (TiCl6), boron trichloride (BCl3), and silicon tetrachloride (SiCl4).
[0062] The metal complexes, transition element complexes, and main group element complexes may include at least one member from the group including copper bis(hexafluoroacetylacetonate) (Cu(C5F6HO2)2) and dimethylgold trifluoroacetylacetonate (Me2Au(C5F3H4O2)).
[0063] The organic compounds may include at least one member from the group including carbon monoxide (CO), carbon dioxide (CO2), aliphatic hydrocarbons, aromatic hydrocarbons, components of vacuum pump oil, and volatile organic compounds. The aromatic hydrocarbons may include styrene.
[0064] The at least one additive gas may include at least one member from the group including an oxidizer, a halide, and a reducing agent.
[0065] The oxidizing agent may include at least one element from the group including oxygen (O2), ozone (O3), water vapor (H2O), hydrogen peroxide (H2O2), nitrous oxide (N2O), nitric oxide (NO), nitrogen dioxide (NO2), and nitric acid (HNO3). The halide may include at least one element from the group including chlorine (Cl2), hydrochloric acid (HCl), xenon difluoride (XeF2), hydrogen fluoride (HF), iodine (I2), hydrogen iodide (HI), bromine (Br2), hydrogen bromide (HBr), nitrosyl chloride (NOCl), phosphorus trichloride (PCl3), phosphorus pentachloride (PCl5), and phosphorus trifluoride (PF3). The reducing agent may include at least one element from the group including hydrogen (H2), ammonia (NH3), and methane (CH4).
[0066] At least one generated repair element may at least partially overlap at least one defect. The deposited repair element may include the material of the lithography mask. The deposited repair element may include a metal (e.g., chromium (Cr)), a metal compound (e.g., tantalum nitride (TaN)), silicon (Si), silicon dioxide (SiO2), and molybdenum silicon oxynitride (Mo x SiO y N z )(0 < x ≤ 0.5, 0 ≤ y ≤ 2, and 0 ≤ z ≤ 4 / 3). The etched repair element may etch the material of the photolithography mask. The etched repair element may include the aforementioned mask material.
[0067] The method as defined above may include: (a) generating at least one repair element according to at least one repair shape defined by at least one defect, and (b) determining the parameters of the repair shape for the remaining residual defects, including assigning at least one numerical value to the parameters, where the numerical value deviates from the numerical value predefined by the remaining residual defects for the said parameters.
[0068] The method defined above can be used as a second step of a general defect repair process. In this case, in a first step, large defects, i.e. defects large relative to the resolution limit of the photomask, can be repaired by realizing a repair shape in the form of a local etching process or in the form of a local deposition process or by generating a corresponding repair element. The repaired mask is then inspected. If during the inspection of the mask it is noticed that the repaired location still does not necessarily meet the specifications, a repair shape is determined for the remaining residual defects, the parameters of which are determined according to the method according to the invention. Here, it is assumed that the remaining residual defects constitute small defects, i.e. defects having at least one dimensional size in at least one dimension smaller than the resolution capability or resolution limit of the photolithographic mask. The remaining residual defects can be repaired or compensated for later by generating a corresponding repair element based on the repair shape determined in the second step.
[0069] In a second embodiment, a method for repairing at least one defective pattern element of a lithography mask includes: (a) determining at least one repair element of the lithography mask that does not image the lithography mask during its exposure, the at least one repair element configured to change the imaging behavior of the at least one defective pattern element; and (b) generating the at least one repair element on the lithography mask with at least one focused particle beam and at least one precursor gas.
[0070] At least one repair element produced may have a dimensional size smaller than the resolution limit R of the photomask in at least one dimension. As already explained, the averaging of the light radiation over structures whose dimensional size is below the resolving ability of the mask reduces the effect of placement errors of the repair element. This situation greatly facilitates the positioning of the repair element relative to the location of the defect to be repaired. Furthermore, by being non-imaged of the repair element, its geometric shape may deviate significantly from the shape of the defect without significant adverse effects on the compensation of the defect. This fact greatly simplifies the repair or compensation of small defects.
[0071] However, the repair elements created on the mask locally change the diffraction behavior of the mask at the wavelength of the light, and the repair elements are then designed such that, in combination with the defective pattern elements, they substantially achieve the imaging behavior of the corresponding defect-free areas of the photolithographic mask.
[0072] The at least one repair element may have at least one dimension size that includes a range of 10% to 90% of the resolution limit of the lithographic mask, preferably 20% to 80%, more preferably 30% to 70%, and most preferably 40% to 60%.
[0073] The distance between the at least one repair element and the at least one defective pattern element may range from 2% to 80% of the resolution limit of the lithographic mask, preferably from 2% to 50%, more preferably from 2% to 30%, and most preferably from 2% to 10%.
[0074] At least one dimension size of the at least one repair element may be in the range of 10% to 90% of the resolution limit of the lithographic mask, preferably 20% to 80%, more preferably 30% to 70%, and most preferably 40% to 60%.
[0075] Other aspects of the repair element are as described above with respect to the first embodiment.
[0076] The computer program may include instructions which, when executed by a computer system, cause the computer system to perform the method steps of one of the aspects listed above.
[0077] In one embodiment, an apparatus for repairing at least one defect in a lithography mask includes means for determining a parameter of at least one repair shape for the at least one defect, the means comprising means for assigning a numerical value to the at least one parameter, the numerical value deviating from a predefined numerical value for said parameter due to the at least one defect.
[0078] The apparatus may further include means for generating at least one repair element on the lithographic mask according to the determined repair shape.
[0079] The means for determining the parameter of the at least one repair feature may comprise at least one co-processor configured to determine the parameter of the at least one repair feature from measurement data of the at least one defect and design data of the lithographic mask. Furthermore, the at least one co-processor is configurable to assign at least one numerical value to the at least one corresponding parameter that deviates from a predefined numerical value due to the at least one defect. The assignment of the deviating numerical value of the at least one corresponding parameter may be effected based on a resolution limit of the lithographic mask and a resolution limit in generating the at least one repair element.
[0080] The resolution limit in generating at least one repair element is essentially influenced by two parameters. The first parameter is the minimum spot diameter to which the particle beam generating the repair element can be focused. In the case of a photon beam, the achievable spot diameter depends on the wavelength of the photons. To generate repair elements in the DUV wavelength range on a mask by means of a photon beam, photons from the EUV wavelength range are required. EUV photon sources are currently still very expensive. Therefore, for the purpose of generating repair elements, it is advantageous to use a particle beam (for example an electron beam) with a mass whose resolution limit is given by the de Broglie wavelength. An electron beam can currently be focused to a spot diameter in the range of a few nanometers. The positioning accuracy of the electron beam is very high and extends into the sub-nanometer range.
[0081] The second parameter that determines the resolution limit in producing repair elements is the interaction area or scattering cone of secondary electrons generated by the massive particle beam. The diameter of said interaction area on the mask surface determines the extent of local chemical reactions initiated by the particle beam and at least one precursor gas. The size of the interaction area is determined by the energy of the particles incident on the photomask. Furthermore, the local material composition of the photomask at the interaction site has a large influence on the size of the interaction area. Currently, local chemical reactions can be limited to a lateral dimension of about 5 nm.
[0082] The means for determining the parameters of the at least one repair shape may include at least one algorithm embodied as an application specific integrated circuit (ASIC), a complex programmable logic device (CPLD), and / or a field programmable gate array (FPGA).
[0083] The means for determining at least one parameter of the repair shape may include at least one trained machine learning model, and further, the means for assigning a value to at least one corresponding parameter that deviates from a predefined value due to at least one defect may include a trained machine learning model.
[0084] The means for determining a parameter of the at least one repair feature may include at least one member from the group including a mask inspection apparatus, an interferometer, a confocal microscope, a scanning particle microscope, and a scanning probe microscope, said member being capable of recording measurement data from the at least one defect.
[0085] The means for generating the at least one repair element may include at least one focused particle beam and at least one precursor gas configured to carry out a localized chemical reaction.
[0086] In a second embodiment, an apparatus for repairing at least one defective pattern element of a lithography mask includes: (a) means for determining at least one repair element of the lithography mask that does not image the lithography mask during exposure, the repair element configured to change the imaging behavior of the at least one defective pattern element; and (b) means for providing a focused particle beam and at least one precursor gas configured to generate the at least one repair element on the lithography mask.
[0087] The means for determining the at least one repair element may comprise at least one co-processor configured to determine the at least one repair element from the measurement data of the at least one defect and the design data of the lithography mask. The determination of the at least one repair element may be based on a resolution limit of the lithography mask and a minimum spot size at the focus of the focused particle beam.
[0088] The means for determining at least one repair element of the lithographic mask may include at least one algorithm embodied as an application specific integrated circuit (ASIC), a complex programmable logic device (CPLD), and / or a field programmable gate array (FPGA).
[0089] The means for determining the at least one remedial element may include at least one trained machine learning model.
[0090] The means for determining the at least one repair element may include at least one element from the group including a mask inspection tool, an interferometer, a confocal microscope, a scanning particle microscope, and a scanning probe microscope.
[0091] Another embodiment includes a lithography mask repaired according to any of the methods described above. The repaired lithography mask is usable in an exposure system. Furthermore, the repaired lithography mask can be repaired based on at least one repair shape determined according to any of the aspects described above. Furthermore, the repaired lithography mask can include at least one repair element generated using the at least one repair shape determined. The lithography mask can be repaired by performing a particle beam induced local deposition process and / or a local etching process.
[0092] In another embodiment, the exposure system uses a lithographic mask that has been repaired according to any of the method steps described above.
[0093] The exposure system may be a photolithography exposure system. In particular, the exposure system may be a microlithography projection exposure system. The exposure system may be any kind of exposure system, for example an exposure system suitable for use with a transmission lithography mask and an exposure system suitable for use with a reflection lithography mask.
[0094] The resolution limit of an exposure system may be determined by the wavelength of the light source of the exposure system, the numerical aperture of the projection lens of the exposure system, and the exposure settings of the exposure system.
[0095] For an exposure system, at least two resolution limits can be defined, representing two ends of the projection lens or projection objective of the exposure system.
[0096] The resolution limit of the exposure system may be the wafer-side resolution limit of the projection lens of the exposure system.
[0097] The wafer side resolution limit is
number
[0098] The NA on the wafer side of the projection lens, i.e. NA W is typically chosen to be as large as possible to make the wafer-side resolution limit as small as possible. When using immersion liquid, NA W can be greater than 1, for example 1.3.
[0099] The mask-side resolution limit of the projection lens of the exposure system is
number
[0100] Mask side numerical aperture (NA M ) and wafer side numerical aperture (NA W ) defines the magnification M of the projection lens.
number
[0101] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS In the following detailed description, reference is made to the drawings and describes exemplary embodiments of the present invention that are currently preferred. [Brief description of the drawings]
[0102] [Figure 1] The top image is a schematic cross-sectional view of a pattern element of a photolithography mask having edges at locations predefined by the design, and the bottom image is a schematic representation of the effective dose distribution of light intensity around the mask segment shown in the top image in the photoresist during exposure of the photomask. [Diagram 2] The top image is a schematic cross-sectional view of a mask containing a defective pattern element, and the bottom image illustrates the effect of the defective pattern element on the effective dose distribution applied to the photoresist. [Diagram 3]The top image illustrates the repair of a defective pattern element of the photolithography mask of FIG. 2 according to the prior art, and the bottom image illustrates the effect of the defect repair on the light intensity distribution of the repaired mask segment of the top image. [Figure 4] The top image shows an ideal repair of a defective pattern element of the photolithography mask of FIG. 2 based on a method according to the present invention, and the bottom image shows the light intensity distribution produced by the optimally repaired photomask in the photoresist of a wafer. [Diagram 5] The top image shows the actual repair of a defective pattern element of the mask of FIG. 2 according to the method of the present invention, and the bottom image shows the effect of the repair photomask on the light intensity distribution generated in the photoresist. [Figure 6] FIG. 3 shows a schematic diagram of an alternative exemplary embodiment of a repair element for compensating for the defect of FIG. 2. [Figure 7] Top image 715 is a schematic diagram of a perfectly aligned edge of a pattern element, partial image 735 is a diagram illustrating a pattern element having a defect of excess absorber material, partial image 755 is a diagram illustrating repair of the defect in partial image 735 according to the prior art, partial image 775 is a diagram illustrating compensation of the defect in partial image 735 by creation of a repair element as described in the present application, and partial image 795 is a diagram illustrating a second exemplary embodiment of a repair element according to the present invention. [Figure 8] The top image 805 is a representation of a pattern element of a photolithographic mask with its edges positioned precisely where given by the design, the middle image 835 is a representation of the repair of a defect of lack of absorber material by the creation of a repair element in accordance with the present invention, and the bottom image 855 is a representation of the repair of a defect of excess absorber material by the creation of a repair element in accordance with the present invention. [Figure 9] The top image is a schematic plan view of a strip structure containing a defect, and the bottom image is a representation of the strip structure after repair of the defect according to the prior art. [Figure 10] The top image is a reproduction of the top image of FIG. 9, the middle image shows an exemplary repair of the defect in the top image by one of the methods described in this application, and the bottom image shows averaging of the complex amplitude of the light radiation at the length scale of the optical resolution. [Figure 11] Top image 1105 is a schematic diagram of a plan view of an absorbent angular pattern element, partial image 1125 is a diagram illustrating a pattern element having a defect of excess absorbent material, partial image 1145 is a diagram illustrating repair of the defect in partial image 1125 according to the prior art, partial image 1165 is a diagram illustrating compensation of the defect in partial image 1125 by creation of a repair element as described in the present application, and partial image 1185 is a diagram illustrating creation of a second example repair element according to the present invention. [Figure 12] FIG. 11 is a diagram showing the repair of a defect due to loss of absorber material according to the presented method. [Figure 13] The top image 1305 shows a stripe structure of a mask placed on a substrate, where the pattern element has a defect due to loss of absorber material, the middle image 1335 shows an exact simulation of the defective mask segment, and the bottom image 1365 shows the light intensity distribution of the defective mask segment. [Figure 14] FIG. 14 shows the mask segment of FIG. 13 after optimal repair of defects by the method according to the present invention. [Figure 15] 14 illustrates the mask segment of FIG. 13 after repair of the defect of FIG. 13 with a non-optimally positioned repair element. [Figure 16] The upper left image 1605 shows a mask segment having a defect measured by a scanning electron microscope, the upper right image 1635 shows a repair element in the mask segment of the upper left image that compensates for the defect, and the lower left image 1665 shows the repaired mask segment of the upper left image 1605. [Figure 17]Top image 1705 illustrates the normalized CD variation within the defective mask segment of the top left image of FIG. 16, and bottom image 1755 illustrates the normalized CD variation of the repaired mask segment of the bottom left image 1665 of FIG. [Figure 18] Top image 1805 is a schematic cross-sectional view of a strip structure including a defect, partial image 1825 is a diagram showing a mask segment of partial image 1805 around the repaired defect, partial image 1835 is a diagram showing the CD variation caused by the defect in the top image, and bottom image 1865 is a diagram showing the CD variation that remains after the defect is repaired. [Figure 19] 2 is a flowchart of a first embodiment of a method for repairing at least one defect in a lithography mask. [Figure 20] 4 is a flow diagram of a second embodiment of a method for repairing at least one defect in a lithography mask. [Figure 21] 1 is a schematic cross-sectional view of an apparatus for repairing one or more defects in a lithographic mask. [Figure 22] FIG. 1 shows a schematic cross-sectional view of an optical mask inspection apparatus and a comparison with a scanner of a photolithography exposure system. [Figure 23] 1 is a schematic cross-sectional view of an apparatus for repairing at least one defective pattern element of a lithographic mask; [Figure 24] FIG. 24 is a schematic cross-sectional view of an apparatus implementing the particle beam source and gas supply system of FIG. 23. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0103] In the following, currently preferred embodiments of the method according to the invention and the device according to the invention for repairing one or more defects in a lithographic mask are described in more detail. Furthermore, exemplary embodiments of the method according to the invention and the device according to the invention for repairing defective pattern elements in a lithographic mask are described in more detail. The methods according to the invention are described on the basis of the example of a binary photomask for the deep ultraviolet (DUV) wavelength range. However, they are not limited to improving the repair of defective DUV masks. Furthermore, the methods according to the invention are described mainly on the basis of edge placement errors of pattern elements. However, they are not limited to repairing errors of this type. Rather, they can be used for various photolithographic masks, in particular to facilitate the repair of any type of micro-defect. These masks can include transmissive and reflective photomasks. Furthermore, micro-defects in binary and / or phase-shift masks can be repaired, as well as micro-defects in masks for multiple exposures. Hereinafter, the term mask or photomask is also intended to encompass templates for nanoimprint lithography.
[0104] Furthermore, the device according to the invention for repairing one or more defects of a lithography mask is described based on the example of a modified scanning electron microscope. However, the device according to the invention can not only be realized based on a scanning electron microscope. Rather, the device according to the invention can be based on any scanning particle microscope. That is, the device defined in the present application can use any type of particles, preferably a type of particles having a mass and / or a type of particles that generate one or more repair elements of a photomask.
[0105] The top image 105 of FIG. 1 is a schematic cross-sectional view of a one-dimensional (1D) segment of a photolithography mask 100. The mask 100 can be a transmission or reflection mask 100. In the example of FIG. 1, the photomask 100 includes a binary transmission mask 100. The photolithography mask 100 includes a substrate 110 having a surface 115. On the surface 115 of the substrate 100, pattern elements 120 or structure elements 120 are arranged, having a surface 125. The substrate 110 can include a quartz substrate and / or a material with a low coefficient of thermal expansion (LTE (Low Thermal Expansion) substrate). In the case of a transmission photomask 100, the substrate 110 is substantially optically transparent to electromagnetic radiation of the light wavelength. The pattern elements 120 can be structure elements 120 of the binary photomask 100. In this case, the pattern elements 120 can include elements of an absorber structure 120, and can include, for example, chromium. The absorbing pattern elements 120 absorb substantially all of the optical wavelength electromagnetic radiation incident on the pattern elements 120. For DUV masks, the thickness of the pattern elements 120 ranges from 60 nm to 200 nm. Absorbing pattern elements for EUV masks currently range in layer thickness from 50 nm to 70 nm (not shown in FIG. 1).
[0106] Here, as well as elsewhere in this specification, the expression "substantially" refers to an indication of the measured variable within conventional measurement error when prior art measuring instruments are used to determine the measured variable.
[0107] Furthermore, pattern elements 120 may include structural elements 120 that both shift the phase of the optical radiation relative to the radiation incident on substrate 110 and absorb portions of the optical wavelengths of light incident on said pattern elements 120. Examples of such masks are AttPSMs (attenuated phase shift masks) based on molybdenum disilicide or silicon nitride. Such masks typically transmit 6-20% of the incident light intensity in dark areas with a phase shift of 180° compared to the clear areas of the photomask.
[0108] However, the pattern elements 120 can also be structural elements 120 of a pure phase-shifting photomask 100. A pure phase-shifting mask 100 can be produced, for example, by etching a corresponding pattern into a substrate 110 of the mask 100, which in this case essentially comprises quartz (SiO2). This type of mask is called a CPL (Chromeless Phase-Shift) mask. Another example of a type of pure phase-shifting mask is the AltPSM (Alternating Phase-Shift Mask) mask.
[0109] The top image 105 of Figure 1 shows an ideal edge 130 that is predefined by design and has a sidewall angle 135 of substantially 90°. Moreover, the edge 130 is precisely located in a location that is predefined by design.
[0110] The bottom image 155 of FIG. 1 shows a schematic of the effective dose distribution of light intensity 160 during exposure of a pattern element 120 of a photomask 100. The pattern element 120 absorbs radiation incident on the mask 100 from above, so that at a distance from the edge 130 below the pattern element 120, substantially no light intensity is visible in the photoresist of the wafer. At a distance from the edge 130 of the pattern element 120, in the transparent substrate region 110 of the mask 100, the photoresist applied to the wafer is exposed with maximum light intensity. The edge 130 of the pattern element 120 is usually defined as the location where the light intensity in the photoresist reaches 50% of the maximum light intensity or maximum effective dose. This is shown in the bottom image 155 of FIG. 1 by the intersection of the dashed vertical line 180 and the horizontal line 170.
[0111] In the upper image 205 of FIG. 2, the edge 230 of the pattern element 220 is not located at a position predefined by the design. Rather, the edge 230 is at a distance dx indicated by a horizontal double arrow 240. The distance dx from the target position of the edge 230 predefined by the design can result from a misplacement of the pattern element 220 whose dimension size has a value predefined by the design. In this case, the pattern element 220 can be corrected by defining two repair shapes and generating two repair elements by said repair shapes. On the one hand, a first repair shape defines the deposition of missing absorbent material in the area identified by the double arrow 240 in FIG. 2. On the other hand, a second repair shape defines the removal of excess absorbent material of the pattern element 220 or absorbent material that is not positioned in the correct place (not shown in FIG. 2).
[0112] In the following, it is assumed that the edges of the pattern element 220, which are not reproduced in the 1D representation of Fig. 2, are correctly positioned and that the pattern element 220 needs to be corrected by depositing the missing absorber material only in the region of the edge 230. Furthermore, in the following, it is assumed that the defect 240 is a micro-defect, meaning that the dimensional size dx of the one-dimensional defect 240 is smaller than the resolution limit of the photolithography mask 200 at the light wavelength. The accuracy of the positioning or placement of the edges 130, 230 of the pattern elements 120, 220 is extremely important, especially considering the overlay issues of lithography systems that perform multiple exposure steps to fix the pattern elements in the photoresist.
[0113] The bottom image 255 of FIG. 2 shows a light intensity distribution 260 or effective dose distribution 260 generated by a misplacement or positioning of an edge 230 of a pattern element 220 in a photoresist arranged on a wafer during exposure of a photolithography mask 200 with optical electromagnetic radiation. During exposure of the wafer, a position error of the edge 230 of the pattern element 220 (described by dx in the one-dimensional example of FIG. 2) is converted by the mask 200 into an edge placement error EPE, which is shown diagrammatically by a double arrow 280 in the bottom image 255 of FIG. 2. The relationship between the EPE 280 on the wafer and the mask defect 240 is described by the relationship EPE=mask error·MEEF·M. In this case, in the example represented in FIG. 2, the mask defect 240 or mask error 240 indicates the fact that the edge 230 of the pattern element 220 is misplaced by dx. The mask enhancement factor MEEF (mask error enhancement factor) refers to the enlargement or increase of the mask defect 240 that can be caused by the mask 200. For simplicity, in the following it is assumed that MEEF=1. The factor M indicates the magnification or demagnification with which the projection lens of the exposure system images the pattern elements 220 of the mask 200 onto the wafer. For currently used projection lenses, M=1 / 4 or M=1 / 5. In FIG. 2 and the following figures, the relationship between the mask defects 240 and the EPEs 280 is not shown to scale.
[0114] An ideal repair of mask defect 240 with perfect realization of the perfect repair shape would be to place a repair element at defect edge 230 of pattern element 220, such that defective pattern element 220 would look like pattern element 120 shown in Figure 1. However, this requires ideal positioning of a repair tool relative to edge 230 of defective pattern element 220. Furthermore, perfect repair of defect 240 assumes that the resolution limit of the repair tool is very small, ideally zero.
[0115] The top image 305 of FIG. 3 shows the actual repair of defect 240 of FIG. 2 according to the prior art. Given the finite positioning accuracy of the repair tool, the repair tool is never perfectly aligned with edge 230 of defective pattern element 220. Thus, the repair feature produces a repair element 310 that does not ideally correspond to the 1D dimension dx of defect 240. Rather, given the limited positioning accuracy of the repair tool, the repair feature of defect 240 produces an infinitesimal portion 320 of repair element 310 on surface 125 of defective pattern element 220. Thus, edge 330 of repair element 310 deviates from its predefined position by design. The remaining defect 340 has a dimension dx′.
[0116] The bottom image 355 of Fig. 3 shows the change in light intensity distribution 360 or EPE in the photoresist upon exposure of the repaired mask segment 300 with respect to the top image of Fig. 3. Compared to the exposure of the unrepaired mask 200, the repaired mask 300 comes much closer to the pattern shape predefined by the design of Fig. 1. However, there still remains a discrepancy or EPE 380, indicated by the double arrow 380, which results in a CD (critical dimension) deviation of the repaired pattern element 220 outside the tolerance budget of the mask 300. The defect 340 remaining after the prior art repair can be repaired or compensated for as explained below. However, it is more convenient to repair the defect 240 directly, i.e. in a single step, as will be explained below with reference to Fig. 4.
[0117] FIG. 4 shows in the top image 405 the best possible repair of the defective pattern element 220 of FIG. 2 according to one of the methods described in this application. The repair shape correcting the defective pattern element 220 of FIG. 2 is designed such that the realization of the repair shape generates a repair element 410 at a distance 420 from the edge 230 of the defective pattern element 220. The ideal distance 420 between the edge 230 of the defective pattern element 220 and the repair element 410 is approximately dx / 2, i.e. half the distance between the edge 230 and the vertical line 170 or the edge error 240 of the defective pattern element 220. For the corresponding height 430 of the repair element 410 being substantially identical to the height of the pattern element 220, the repair element 410 and thus the repair shape below the repair element 410 have a dimensional size corresponding to approximately 80% of the distance 240 between the edge 230 and the vertical line 170 of the pattern element 220. As already explained above, the mask-side resolution limit of a DUV mask is in the range of 150 nm to approximately 300 nm, and the mask-side resolution limit of an EUV mask is in the range of approximately 50 nm to 100 nm.
[0118] The bottom image 455 of Fig. 4 presents a light intensity distribution 460 of a repair photomask 400 having a repair element 410 located at a distance 420 from the edge 230 of the defective pattern element 220 of the photomask 200. Comparing Figs. 1 and 4, it is clear that the light intensity distribution 460 resulting from the combined effect of the defective pattern element 220 and the repair element 410 produces a pattern element in the photoresist that exactly realizes the edge 130 predefined by design. Even though the repair element 410 is not adjacent to the edge 230 and even though the extent of the defect 240 does not correspond to the one-dimensional size 440 of the repair element 410, the repair element 420 produces an ideal production in the photoresist and thus the wafer of the pattern element predefined by design.
[0119] The repair elements 410 can be generated by a repair tool (described below in conjunction with FIGS. 21-24) based on corresponding repair features on the photomask 400. To this end, the repair tool can perform a localized chemical deposition reaction by means of a particle beam and at least one precursor gas. The material composition of the repair elements 410 can correspond to the material composition of the pattern elements 220. However, the material composition of the repair elements 410 can also deviate from the material of the pattern elements 220, as long as the material of the repair elements 410 substantially completely absorbs the light wavelength of the photolithography mask 420.
[0120] FIG. 4 illustrates a perfect compensation of the defective pattern element 220 by the generation of a repair element 410 at a distance 420 from the edge 230 of the defective pattern element 220. The upper image 505 of FIG. 5 illustrates a realistically feasible repair of the defective pattern element 220. Considering the finite positioning accuracy of the repair tool, the determined repair shape does not allow the repair element 510 to be positioned exactly at a location that provides an optimal compensation of the defective pattern element. In the example shown in FIG. 5, the distance 520 from the edge 230 of the defective pattern element 220 is shorter than in the case of the optimal repair of the defective pattern element 220 shown in FIG. 4. As is evident from the lower image 555 of FIG. 5, the placement error 540 of the repair element 510 results in almost no deviation of the light intensity distribution 560 in the photoresist applied to the wafer compared to the ideal light intensity distribution 460 of FIG. 4. This means that after the repair of said mask by the generation of the repair element 510, the EPE of the mask 500, indicated by the arrow 580 in FIG. 5, is negligibly small.
[0121] This is because during transfer to the photoresist, the placement error 540 of the repair element 510 is approximately a factor of 1 / R M This is because the value is gradually decreased by R Mrepresents the resolution limit of the photolithographic mask. This is one of the great advantages of the method described herein for repairing micro-defects in a photolithographic mask. The sensitivity of the placement of the repair element 410, 510 to the EPE 580 is significantly reduced when the method according to the present invention is performed. This reduction in the sensitivity of the placement of the one or more repair elements 410, 510 reduces the resolution limit R of the photolithographic mask 400, 500. M The repair element 410, 510 is designed to be able to reach the resolution limit R of the photolithography mask 400, 500 without the EPE 580, i.e., the repair or compensation of the pattern element 220, deviating by more than 10% from the best possible light intensity distribution 460 of FIG. M The distance can be set to approximately 1% to 30% of the distance.
[0122] FIG. 6 shows a second example of a repair element 610 that can be used to repair or compensate for the defective pattern element 220 of FIG. 2. Unlike the height 530 of the repair element 510 of FIG. 5, the height 630 of the repair element 610 of the upper image 605 of FIG. 6 is smaller than the height or thickness of the pattern element 220 of the mask 600. To compensate for the lower height 630 of the repair element 610, the repair element 610 has a larger 1D dimension size 635 than the repair element 510 of FIG. 5. As can be inferred from the lower image 655 of FIG. 6, the modified repair element 610 has a substantially unchanged light intensity distribution 660 in the photoresist. The EPE 680 is negligibly small, similar to FIG. 5.
[0123] In addition to reducing the placement sensitivity of the repair elements 410, 510, 610, the implementation of a defined repair shape also allows the creation of repair elements 410, 510, 610 whose lateral size 435, 535, 635 deviates significantly from the 1D size dx of the defect 240. Thus, the defect repair method presented in this application significantly reduces the sensitivity of the parameterized repair shape to transfer one or more lateral size dimensions of the defect 240 to the repair elements 410, 510, 610. This is a second major advantage of the method for repairing micro-defects in photolithography masks as described in this application, apart from the mitigation of placement sensitivity. In particular, the repair elements 410, 510, 610 can be significantly smaller than the defect 240 to be repaired. This situation has a positive impact on the time required for defect repair, i.e., for the creation of the repair elements 410, 510, 610.
[0124] 1 to 6 illustrate the application of the methods presented in this application to repair defects of absorber material loss, i.e. clear defects. Fig. 7 illustrates how these methods can be used for repair of defects of material excess, i.e. so-called dark defects. The top image 705 of Fig. 7 presents a pattern element 720 disposed on the surface 715 of the substrate 710 of the mask 700. The edge 730 of the pattern element 720 is given by design and is precisely positioned at the location identified by the dashed vertical line 170.
[0125] In the second partial image 735 from the top, pattern element 740 has an excess material defect 750. The defect 750 has a 1D dimension 725 that extends beyond the edge 730 of a defect-free pattern element 720. The defect 750 may result from a misplacement of the pattern element 720 whose dimension is the exact size given by design. However, as discussed above in conjunction with FIG. 2, it is also possible that too little absorber material was removed from the area of edge 730 during patterning of mask 700.
[0126] Partial image 755 illustrates the prior art repair of defect 750. If ideal generation of repair elements 760 were achieved, defect 750 could be completely repaired, as shown in partial image 755. Problems with the prior art, particularly with regard to repairing small defects 750, were discussed in the discussion of FIG.
[0127] Partial image 775 illustrates the repair of material excess defect 750 by the creation of repair element 770, in accordance with the present invention. Repair element 770 is not designed to remove the excess material of defect 750 by performing a localized etching process. Rather, the creation of repair element 770 removes a portion of defect 750 and a small portion of defective pattern element 740. After creation of repair element 770, the remaining residual defect 780, in combination with repaired pattern element 740, affects the imaging behavior of repair mask 700 in the region of the repair pattern element such that it has imaging behavior like pattern element 720.
[0128] Finally, the bottom image 795 of Fig. 7 presents a second repair element 790 that can be generated as an alternative to the repair element 770. The generation of the repair element 790 removes a portion of the material of the defective pattern element 740 in the region of the edge 730 of the error-free pattern element 720. The repair element 790 has a larger 1D dimension than the repair element 770. The larger 1D dimension of the repair element 790 is compensated for by the fact that the realization of the repair shape below the repair element 790 does not result in etching of the pattern element 740 below the surface 715 of the substrate 710 of the mask 700.
[0129] Implementation of repair elements 770, 790 for repairing defect 740 allows for additional degrees of freedom as described above in conjunction with FIGS.
[0130] Figure 8 presents in a top image 805 an absorbing pattern element 720 having a surface 725 that is disposed on a surface 715 of a substrate 710 that is optically transparent to the light wavelength of the photolithography mask 800. An edge 730 of the pattern element 720 is positioned precisely at a location given by the design, which is clearly indicated in Figure 8 by a dashed vertical line 170.
[0131] The central image 835 of FIG. 8 represents a defective pattern element 840. The edge 830 of the pattern element 840 is not positioned at the location given by the mask design. As a result, the pattern element 840 constitutes a clear defect, namely a defect of absorber material loss. In the partial image 835, the defect is compensated by the realization of a corresponding repair shape that produces a repair element 850. In the example of FIG. 8, the repair element 850 is adjacent to the edge 830 of the defective pattern element 840. The repair element 850 is a deposition of absorber material whose 1D dimension size extends beyond the boundary of the absorber material loss. The height of the exemplary repair element 850 is approximately half the height of the pattern elements 820, 840.
[0132] The bottom image 855 of Fig. 8 presents a pattern element 860 having an absorber material excess defect. The material excess defect is repaired by removing the top of the excess absorber material by generating a repair shape 870. An edge 880 of the repaired pattern element 860 does not correspond to the location predefined by the design and indicated by the dashed line 170 in Fig. 8. Nevertheless, the repair element 870 removes the effect of the material excess defect from a negligibly small portion.
[0133] Given the reduced placement requirements of the repair tool, the creation of repair elements 850, 870 can be accomplished at less expense than the creation of prior art repair elements 310, 760.
[0134] The top image 905 of Figure 9 is a schematic plan view of a mask segment 900 having a strip structure ("line-space pattern") with two absorbing strips 920 and 930 disposed on an optically transparent substrate 910. In the example shown in Figure 9, the left-hand pattern element 920 has a two-dimensional (2D) defect 940 of excess absorber material.
[0135] The bottom image 955 of FIG. 9 illustrates the repair of defect 940 by performing a local etching process with particle beam and etching gas. In the example of the repair process depicted in the bottom image 955 of FIG. 9, the defect 940 is almost completely removed from the negligible residual defect 950. In general, the laterally extending defect 940 cannot be removed exactly as depicted in the bottom image 955 of FIG. 9. As already explained, the accuracy with which a repair tool or a repair shape of the defect 940 can be positioned relative to the defect 940 or the pattern element 920 is finite. Furthermore, during the generation of the repair element, both the photomask 900 and the repair shape are subject to drift (e.g., thermal drift). Thus, the repaired pattern element 920 often has an edge roughness outside a predetermined error interval (not shown in FIG. 9) along the processed right edge. Therefore, the generation of a corresponding repair shape to remove the defect 940 extending along the pattern element 930 is a very complex and time-consuming process.
[0136] FIG. 10 shows the repair of the 2D defect 940 of FIG. 9 by one of the methods presented in this application. The top image 1005 of FIG. 10 reproduces the top image 905 of FIG. 9. The center image 1035 of FIG. 10 shows the compensation of the defect 940 of excess material by the creation of repair elements 1010. The repair elements 1010 create local etching structures in the defect 940 in a part of the substrate 910 and in a part of the pattern element 920 of the mask 900. The different repair elements 1010 can be created based on a single repair shape created at different positions along the defect extending at the right edge of the pattern element. However, it is also possible to determine a single repair shape that creates the different repair elements 1010, as shown in the center image 1035 of FIG. 10.
[0137] A major advantage of repairing the defect 940 as depicted in the partial image 1035 is that the placement or positioning of the repair element 1010 relative to the defect 940 is much less sensitive. The lower image 1065 of FIG. 10 shows the reduced sensitivity during placement of the repair element 1010 in a schematic manner. The dashed ellipse 1050 shows the area or length scale of the photolithography mask 900 over which the mask 900 averages the complex amplitude of the optical electromagnetic radiation. When structures are present on the photomask whose dimensional size in one or two dimensions is smaller than the resolution limit of the photomask, the optical radiation is averaged over the details of said structures. This means that the minute irregularities of the pattern elements have no or little effect on the imaging behavior of the photolithography mask, while the complex amplitude of the optical electromagnetic radiation averaged over the dimensional size of the area of the resolution limit does affect the imaging behavior of the photomask.
[0138] The dashed ellipse 1050 indicates the area of the mask that contributes light intensity portions to the mask's image points in the photoresist. The scale of this averaging area is the resolution limit R of the photolithographic mask, as already explained above. M The dimension size of the repair element 1010 is determined by the resolution limit R MAs long as the size and positioning of the restorative element are small relative to the size and positioning of the restorative element according to the prior art, the size and positioning of the restorative element may be reduced by a factor of up to 1 / R. M This means that a very large range of different repair elements 1010 will give identical or very similar results in terms of the imaging behavior of the photolithographic mask. The method described in this application exploits this situation to improve the repair of small defects that have been particularly difficult to repair so far.
[0139] The resolution limits of modern DUV and EUV masks are as stated above.
[0140] 11 and 12 illustrate the repair of absorber material excess and absorber material loss defects, where the repair elements may have a different geometric shape than the defect being repaired. Partial image 1105 shows a mask segment 1100 that includes a square pattern element 1120 disposed on a mask substrate 1110 and whose shape meets the design specifications. In partial image 1125 of FIG. 11, pattern element 1130 has an absorber material excess defect 1140 disposed inside a corner region of the pattern element 1130.
[0141] The partial image 1145 of Fig. 11 presents the repair of a defect by realization of a repair shape assigned to the defect according to the prior art, which repair shape generates a repair element 1150 in the area of the defect 1140. The problems associated with this have already been fully explained above in the light of Figs. 3 and 9.
[0142] The partial image 1165 of FIG. 11 shows a first example of the generation of a repair element 1170 for compensating for the defect 1140, which is much less sensitive than the repair element 1150 of the partial image 1145, both firstly with respect to the positioning of the repair element 1170 relative to the defect 1140 and secondly with respect to the lateral size of the repair element 1170 relative to the lateral size of the defect 140. Finally, the partial image 1185 shows a repair element 1190 whose geometry is very different from the shape of the defect to be repaired. A circular or circular repair element 1190 is much easier to generate than a rectangular or square repair element 1170. Nevertheless, the repair element 1190 of the partial image 1185 provides a compensation of the defect 1140 that is no less than that of the repair element 1170. The reasons for this have been explained when discussing FIG. 10.
[0143] Repair of a defect of missing absorber material will now be described with reference to Fig. 12. Partial image 1205 of Fig. 12 shows a square pattern element 1220 disposed on an optically transparent substrate 1210 of a photolithographic mask 1200. In pattern element 1230 of partial image 1225, a portion 1240 of pattern element 1230 is missing. This means that pattern element 1230 has a distinct defect 1240, namely, defect 1240 of missing absorber material.
[0144] 12 shows the realization of a repair shape determined for a material loss defect 1240, and the repair of the defect by application of a corresponding repair element 1250 to the entire defect 1240. The repair element 1250 is realized according to the prior art.
[0145] 12 shows a first example of a repair element 1270 generated according to one of the methods described herein, which avoids the sensitivity of the repair method on the partial image 1245. Moreover, a repair element 1290 shows a second exemplary embodiment that is even easier to generate than the repair element 1270, since it only partially reproduces the complex contours of the defect 1240.
[0146] The top image 1305 of Fig. 13 is a plan view of a mask segment 1300 with a strip structure in which absorbing strip-like pattern elements 1320 are applied to the substrate 1310 of the photomask 1300. The second pattern element 1320 from the left has a material loss defect 1330. The width of the defect 1330 is chosen as 15% of the half pitch of the strip structures. The center image 1335 of Fig. 13 presents a rigorous simulation of the imaging behavior of the mask segment 1300 of the top image 1305. In the center image 1335, the defect 1330 is clearly visible as defect 1340.
[0147] The bottom image 1365 of Fig. 13 represents the light intensity distribution of the defective mask segment 1300. The dashed horizontal line 1360 indicates the maximum of the light intensity distribution or effective dose distribution of an error-free mask segment. The intersection of the intensity distribution with the dashed horizontal line 1370 represents the point where the photoresist is considered to be exposed. Said intersection thus represents the width of the strip-like pattern element produced on the wafer by the mask segment 1300. The defect 1330 is mirrored in the wider central pattern element produced on the wafer. The variation in the width of the pattern element imaged in the photoresist by the mask segment 1300 results in a variation in the CD (critical dimension) along the imaged pattern structure.
[0148] 14 depicts a defective mask segment 1300 repairing defect 1330 in top image 1405 by the creation of repair element 1440. In the example shown in FIG. 14, repair element 1440 is not placed on defect 1330 as in the prior art, but rather is positioned immediately next to absorber material missing defect 1330. As can be inferred from center image 1435, repaired defect 1330 is no longer visible in the imaging simulation. It is also evident from bottom image 1465 that there is no variation in light intensity over the entire length of pattern element 1320, since repair element 1450 has completely repaired defect 1330.
[0149] Figure 15 shows in top image 1505 the repair of defect 1330 of Figure 13, where repair element 1540 is located at a distance of 15% of half pitch from pattern element 1320. No deviation from a defect-free mask structure is discernible in the imaging simulation shown in center image 1535 of Figure 15. In bottom image 1565 of Figure 15, a slight reduction in the maximum of the light intensity distribution is seen, resulting in a smaller width of the central pattern element on the wafer. However, this width deviation is still within the predefined error budget for mask 1300.
[0150] The top left image of Figure 16 shows a mask segment 1600 recorded by a scanning particle microscope, which has a stripe pattern (pattern line width and space) with a half pitch of 152 nm on the mask 1600. As shown by the dashed vertical line 1625 with a bend, a pattern element 1620 of the mask segment 1600 has a defect 1630 of missing absorber material. The example defect 1630 in Figure 16 spans a 10 nm area perpendicular to the pattern element 1620. This span is within the resolution limit R of the photolithography mask 1600. M Much smaller than that.
[0151] In the top right image 1635, a repair element 1640 is shown that is designed to compensate for the defect 1630 by combining with adjacent pattern elements 1620. The bottom left image 1665 of Figure 16 represents the repaired mask segment of the top left image 1605 as a difference image relative to the top right image 1635. As indicated by vertical line 1645, the defect 1630 is no longer visible in the recording of the mask segment 1600.
[0152] The top image 1705 of FIG. 17 shows the CD variation along the pattern element for the various pattern elements of the top left image 1605 of FIG. 16. The dashed lines 1710 indicate The pattern elements produced on the wafer by the mask 1600 have a specified CD (predefined by design), which in the example shown in FIG. 17 is CD=37.68 nm. The dashed horizontal lines 1720 and 1730 represent the lower and upper limits of the allowable CD variation (ΔCD), respectively. In the example of FIG. 17, the CD variation range ΔCD is ±2.5%. From the curves in the top image 1705, it is clear that the curve 1750 touches the upper limit of the CD tolerance interval, and the CD curve 1760 runs well outside the ±2.5% CD tolerance interval over most of its profile. The maximum normalized CD variation of the curve 1760 is ΔCD / CD=8.6%.
[0153] The bottom image 1755 of Fig. 17 presents the CD variations of the different pattern elements 1620 of the repair mask segment of the left bottom image 1665 of Fig. 16. The CD curve profiles are all within the tolerance interval, i.e., the CD curves all meet the requirement of ΔCD / CD<±2.5%, which means that the repair element 1640 perfectly compensates for the defect 1630.
[0154] The top image 1805 of FIG. 18 shows a 1D cross-section of a mask segment 1800 including eight pattern elements 1820 in the form of strip structures arranged on an optically transparent substrate 1810 of the mask 1800. The eight pattern elements 1820 produce seven optically transparent strips numbered consecutively from 0 to 6 in the partial image 1805. The half pitch of the strip structures on the mask 1800 is 152 nm or 38 nm on the wafer. In the top image 1805, the second pattern element 1820 from the left has an excess defect 1840 of absorbing phase-shifting molybdenum silicide (MoSi) material at its right edge. To analyze the effect of the defect 1840, the strip structure of the defective mask segment 1800 represented in the partial image 1805 is simulated. The simulation parameters are NA=1.35, λ=193 nm, outer σ value: 1.0, inner σ value: 0.88, exposure setting: Disar, polarization: Y direction, pattern: L&S (line and space) MoSi (absorption at the light wavelength is 6%). The electromagnetic radiation incident on the mask 1800 is assumed to be coherent.
[0155] The center image 1835 of FIG. 18 presents the CD variation of seven optically transparent strips 0-6 along the strip direction, i.e., perpendicular to the paper, in the simulation. Also, the shift of the center of gravity (CoG) of the light intensity distribution is determined by the simulation. The dashed horizontal line 1870 represents the predefined target CD for the mask 1800. The curves in the center image 1835 represent the critical dimension variation (i.e., ΔCD) along the pattern element 1820. The table in the center image 1835 summarizes the ΔCD and ΔCoG for optically transparent strips 0, 1, and 2. The table shows that the CD variation of the 0th strip is 3.1 nm, which is much larger than the error budget of the mask 1800 of 2.5%. The effect of the defect 1840 on the second optically transparent strip is the result of exposure of the mask 1800 to coherent radiation. The simulations were carried out with the rigorous optical imaging program DrLitho at the Fraunhofer Institute for Integrated Circuits (IISB) in Erlangen.
[0156] The magnification segment 1825 shows the pattern element 1820 around the defective transparent strip 1 after repairing the defect by realizing the corresponding repair shape determined for the defect 1840. When realizing the repair shape for the local etching of the defect 1840, it is assumed that the local etching process produces a sidewall angle 1850 with a negative angle of -20°. The negative sidewall angle 1860 causes amplitude defects in the aerial image or exposure of the wafer. This is taken into account by the magnification factor MEEF=1.4. The negative sidewall angle 1850 is compensated by a (positive) shift of the origin 1860 of the edge 1830 so that the extent or width of the strip 1 corresponds approximately to half the size of the nominal width of the optically transparent strip. The error in the sidewall angle for an angle range of about ±20° can be substantially completely compensated by a corresponding shift of the origin of the edge 1830 of the repaired pattern element 1820. The lateral shift required for this is in the range of about ±3.3 nm for λ=193 nm.
[0157] Bottom image 1865 shows the simulated variation of CD for optically transparent strips 0-6 along the strip direction. Additionally, the CoG shift of the light intensity distribution is determined by simulation. Dashed horizontal line 1870 represents the target value of CD on the wafer. Comparing the set of curves in partial images 1835 and 1865, it is immediately evident that repair of defect 1840 has drastically reduced the CD variation. The table in bottom image 1865, as well as the table in center image 1865, summarizes the ΔCD and ΔCoG for optically transparent strips 0, 1, and 2. Compared to the table in center image 1835, repair of defect 1840 has reduced the CD variation by more than an order of magnitude.
[0158] The repair of an excess material defect 1840 was discussed in relation to Figure 18, where the defect abuts an edge 1820 of a pattern element without completely covering the transparent strip. Of course, excess material defects that completely bridge two pattern elements can also be repaired. Additionally, the method described in conjunction with Figure 18 can also be used to repair missing material defects.
[0159] 19 illustrates a first exemplary embodiment of a method described herein for repairing at least one defect 240, 750, 940, 1140, 1240, 1330, 1630, 1840 in a lithography mask 200, 400, 500, 600, 700, 800, 900, 1100, 1200, 1300, 1600, 1800. The method begins at step 1910. In a next step 1920, parameters of at least one repair shape for the at least one defect 240, 750, 940, 1140, 1240, 1330, 1630, 1840 are determined, where determining the parameters includes assigning a numerical value to the at least one corresponding parameter that deviates from a numerical value predefined by the at least one defect 240, 750, 940, 1140, 1240, 1330, 1630, 1840. The method ends in step 1930.
[0160] 20 presents steps of a second exemplary embodiment of a method for repairing at least one defective pattern element 220, 740, 840, 860, 920, 1130, 1230, 1320, 1620, 1820 of a lithographic mask 200, 400, 500, 600, 700, 800, 900, 1000, 1100, 1200, 1300, 1600, 1800. The method begins at step 2010. In a next step 2020, at least one repair element 410, 510, 610, 770, 790, 850, 870, 1010, 1170, 1190, 1270, 1290, 1440, 1540, 1640 of the lithography mask that does not image the lithography mask during exposure is determined, the repair element changing the imaging behavior of at least one defective pattern element.
[0161] Thereafter, at least one repair element is created on the lithographic mask with the focused particle beam and at least one precursor gas in step 2030. The method ends in step 2040.
[0162] FIG. 21 shows a cross-section of an apparatus 2100 designed to determine parameters of a repair shape for at least one defect 240. To this end, the apparatus 2100 comprises an optical mask inspection apparatus 2110. FIG. 22 shows the principle of an optical mask inspection apparatus designed to record an aerial image of a transmission mask 200. In the left image 2205 of FIG. 22, some components of the scanner are shown diagrammatically. The exposure system focuses electromagnetic radiation of optical wavelengths onto a photolithography mask. The projection optical unit or projection lens projects the radiation, which has passed through the photomask, onto a wafer or onto a photoresist arranged on the wafer, with a large numerical aperture (NA). W ) to form a reduced image (usually 1:4 or 1:5).
[0163] The right image 2255 of Fig. 22 shows some components of an optical mask inspection tool 2110 designed for the light wavelength of the scanner of the left image 2205. The exposure systems of the scanner and the optical mask inspection tool 2110 are substantially identical. This means that the image generation is substantially the same in both systems. The optical mask inspection tool 2110 therefore images a segment of the light intensity distribution of the mask as it is incident on the photoresist placed on the wafer. However, unlike the scanner, in the case of the optical mask inspection tool 2110, a lens images a small segment of the light intensity distribution of the photomask with high magnification onto a CCD (charge-coupled device) camera. As a result, it is possible to represent defects that the photomask has in its aerial image at the light wavelength and to detect said defects by a CCD sensor or a CCD camera.
[0164] The optical mask inspection device 2110 of the apparatus 2100 can provide measurement data of one or more aerial images to the computer system 2130 of the apparatus 2100 via the connection 2120. The computer system 2130 of the apparatus 2100 can determine parameters of repair shapes assigned to defects in the aerial images from the measurement data of the aerial images. To this end, the computer system 2130 can comprise a coprocessor 2140 specifically designed to efficiently execute an algorithm for determining parameters of repair shapes assigned to defects from the aerial images of the optical mask inspection device. Furthermore, the computer system 2130 of the apparatus 2100 can have a second algorithm designed to assign values or numerical values to one or more parameters of the repair shapes that deviate from a predefined numerical value due to the defects. The second algorithm can be executed by the coprocessor 2140 as well.
[0165] However, the computer system 2130 may also have a dedicated hardware component 2150 for executing one or both of the above-mentioned algorithms. The computer system hardware component 2150 may be implemented in the form of an Application Specific Integrated Circuit (ASIC), a Complex Programmable Logic Device (CPLD), and / or a Field Programmable Gate Array (FPGA).
[0166] Additionally or alternatively, the computer system 2130 may comprise a dedicated graphics processor 2160 designed to implement a trained machine learning model. It is also possible to train the machine learning model in at least two ways, or the graphics processor may implement two different trained machine learning models designed for each formulated problem. First, the machine learning model can be trained to determine parameters of one or more repair shapes realized to repair or compensate defects, i.e. to generate one or more repair elements 410, 510, 610, from measurement data of the optical mask inspection device 2110, design data of the lithographic mask 200, settings of the exposure device, and optionally settings of the RET structures generated on the mask 200.
[0167] Alternatively or additionally, the machine learning model may assign different values to one or more parameters of the parameterized repair shape for purposes of determining the above-described repair element 410, 510, 610 in accordance with the present invention. However, in a currently preferred embodiment, the machine learning model directly predicts the parameters of the repair shape from the input data for purposes of forming one of the repair elements 410, 510, 610 described in this application. The process of training the machine learning model is not discussed in this application.
[0168] Additionally, the computer system 2130 may include a non-volatile memory 2170 in which the algorithms, the machine learning models, and / or the trained machine learning models are stored. The non-volatile memory 2170 may include a semiconductor memory (SSD (Solid State Drive)).
[0169] Additionally, the computer system 2130 may include a control device 2180 designed to control the optical mask inspection apparatus 2110 .
[0170] Additionally, the apparatus 2100 may include a scanning particle microscope, a scanning probe microscope, and / or a confocal microscope designed to scan the photolithographic mask 200 for defects 240 and generate a graphical representation of the measurement data. If the apparatus 2100 includes one or more of these measurement tools, the control device 2180 may control these measurement devices as well.
[0171] Fig. 23 presents a schematic cross-section of an apparatus 2300 capable of repairing at least one defective pattern element 220. To this end, the apparatus 2300 comprises an optical mask inspection apparatus 2310. A measurement tool of this kind has already been described above in light of the description of Fig. 22.
[0172] The optical mask inspection device 2310 of the apparatus 2300 can provide measurement data of one or more aerial images or aerial image composites to a computer system 2330 of the apparatus 2300 via a connection 2320. The computer system 2330 of the apparatus 2300 can be similar to the computer system 2130 of the apparatus 2100 of Fig. 21. To avoid lengthy text, a description of the computer system 2330 is omitted. Instead, please refer to the description of Fig. 21.
[0173] The apparatus 2300 further comprises a particle source 2350 capable of providing a focused particle beam. The focused particle beam of the particle source 2350 can firstly be used to analyze the defect 240 of the photolithography mask 200. Based on the measurement data of the focused particle beam and / or the measurement data of the optical mask inspection device 2310, a repair shape of the defect can be determined by one or more algorithms or one or more machine learning models. The focused particle beam of the particle source 2350 can secondly be used to repair the analyzed defect 240 in combination with a gas supply system 2370 of the apparatus 2300. Both the particle source 2450 and the gas supply system 2370 can exchange data with the computer system 2330 via connections 2340 and 2360. Furthermore, the control unit 2370 of the computer system 2330 can control the optical mask inspection device 2310, the particle source 2350, and the gas supply system 2370.
[0174] Fig. 24 is a schematic cross-sectional view of an apparatus 2400 combining a particle source 2350 and a gas supply system 2370 of the apparatus 2300. The apparatus 2400 allows the generation of repair elements 410, 510, 610 for repairing defects 240. The exemplary apparatus 2400 of Fig. 24 comprises a modified scanning particle microscope 2410 in the form of a scanning electron microscope (SEM) 2410. The apparatus 2400 comprises a particle source 2350 in the form of an electron beam source 2405 generating an electron beam 2415 as a particle beam 2415 having mass. The electron beam 2415 can be focused to a spot much smaller than the focal diameter of a photon beam. Considering the short de Broglie wavelength of electrons, the electron beam 2415 can be focused to a spot diameter in the range of a few nanometers. Thus, as an analytical or measuring tool, the electron beam 2415 has a very good lateral resolution.
[0175] Additionally, the electron beam 2415 has the advantage over an ion beam in that electrons incident on the sample 2425 (e.g., photolithography mask 200) do not substantially damage the sample 2425 or the photomask 200. However, the apparatus 2400 may also use an ion beam, atomic beam, or molecular beam (not shown in FIG. 24) for processing the sample 2425.
[0176] The scanning particle microscope 2410 comprises an electron beam source 2405 and a mirror body 2420 in which a beam optical unit 2413, for example in the form of an electron optical unit of the SEM 2410, is arranged. In the SEM 2410 of Fig. 24, the electron beam source 2405 generates an electron beam 2415 which is guided as a focused electron beam 2415 by imaging elements (not shown in Fig. 24) arranged in the mirror body 2420 towards a sample 2425 (which may include a photolithography mask 200) at a position 2422. The beam optical unit 2413 thus constitutes an imaging system 2413 of the electron beam source 2405 of the apparatus 2400.
[0177] Additionally, the imaging elements of the mirror 2420 of the SEM 2410 can scan the electron beam 2415 over the sample 2425. The sample 2425 can be interrogated using the electron beam 2415 of the apparatus 2400. Typically, the electron beam 2415 is normally incident on the sample 2425.
[0178] Backscattered and secondary electrons generated by the electron beam 2415 in the interaction area or scattering cone of the sample 2425 are recorded by the detector 2417. The detector 2417 arranged in the electron mirror body 2420 is called an "in-lens detector". In various embodiments, the detector 2417 can be mounted in the mirror body 2420. The detector 2417 converts the secondary electrons generated by the electron beam 2415 and / or the electrons backscattered from the sample 2425 at the measurement point 2422 into an electrical measurement signal and transmits it to the evaluation unit 2480 of the device 2400. The evaluation unit 2480 analyzes the measurement signals from the detectors 2417 and 2419 to generate an image of the sample 2425. The image is displayed on a display 2495 of the evaluation unit 2480. The detector 2417 may also additionally include a filter or a filter system for distinguishing electrons with respect to energy and / or solid angle (not shown in FIG. 24).
[0179] The exemplary device 2400 may comprise a second detector 2419. The second detector 2419 may be designed to detect electromagnetic radiation, particularly in the X-ray range. As a result, the detector 2419 allows an analysis of the material composition of the radiation generated from the sample 2425 during the examination. The detectors 2417 and 2419 may be controlled by a control unit 2370 of the computer system 2330. In an alternative embodiment, the device 2400 comprises a dedicated control unit (not shown in FIG. 24).
[0180] Additionally, the apparatus 2400 may include a third detector (not shown in FIG. 24). The third detector may be embodied in the form of an Everhart-Thornley detector, typically located outside the mirror body 2420. It is typically used for detecting secondary electrons.
[0181] The apparatus 2400 may include an ion source that provides ions with low kinetic energy in the region of the sample 2425 (not shown in FIG. 24). The low kinetic energy ions can compensate for the charging of the sample 2425.
[0182] The sample 2425 is placed on a sample stage 2430 or sample holder 2430 for inspection. In the art, the sample stage 2430 is also known as a "stage." As symbolized by the arrows in FIG. 24, the sample stage 2430 can be moved in three spatial directions relative to the mirror body 2415 of the SEM 2410, for example by a micromanipulator, not shown in FIG. 24.
[0183] The sample stage 2430 is capable of translation as well as rotation about at least an axis oriented parallel to the beam direction of the particle source 2405. The sample stage 2430 can be further embodied such that it is also capable of rotation about one or two other axes arranged in the plane of the sample stage 2430. The two or three rotation axes preferably form a Cartesian coordinate system.
[0184] The sample 2425 to be inspected can be any microstructured component or device requiring analysis and, if necessary, subsequent processing (e.g., repair of a local defect 240 in a pattern element 220 of a photolithographic mask 200).
[0185] Additionally, the apparatus 2400 of FIG. 24 may include one or more scanning probe microscopes, for example in the form of an atomic force microscope (AFM) (not shown in FIG. 24), that can be used to analyze and / or process the sample 2425.
[0186] The example scanning electron microscope 2410 shown in Figure 24 operates in a vacuum chamber 2470. To create and maintain the reduced pressure required in the vacuum chamber 2470, the SEM 2410 of Figure 24 includes a pumping system 2472.
[0187] In the following, the gas supply system 2370 implemented by the apparatus 2400 will be discussed. As already explained above, the sample 2425 is placed on the sample stage 2430. The imaging element of the mirror body 2420 of the SEM 2410 can focus and scan an electron beam 2415 on the sample 2425. The electron beam 2415 of the SEM 2410 can be used to induce a particle beam induced deposition process (EBID (electron beam induced deposition)) and / or a particle beam induced etching process (EBIE (electron beam induced etching). The exemplary apparatus 2400 of FIG. 24 has three different supply vessels 2440, 2450, and 2460 that store various precursor gases for carrying out these processes.
[0188] The first supply container 2440 stores a precursor gas (e.g., a metal carbonyl (e.g., chromium hexacarbonyl (Cr(CO)6)) or a main group metal alkoxide (e.g., TEOS, etc.)). The precursor gas stored in the first supply container 2440 can deposit missing material from the photolithography mask 200, for example, within a localized chemical deposition reaction. Missing material in the mask 200 can include missing absorber material (e.g., chromium), missing substrate material 210 (e.g., quartz), missing material in an OMOG mask (e.g., molybdenum silicide), or missing material in a multi-layer structure (e.g., molybdenum and / or silicon) of a reflective photomask.
[0189] The electron beam 2415 of the SEM 2410 acts as an energy source for splitting a precursor gas stored in a first supply container 2440 at the site where material is intended to be deposited on the sample 2425. This means that the combined supply of the electron beam 2415 and the precursor gas performs an EBID process for local deposition of missing material (e.g., material missing from the photomask 20). A modified SEM 2410 of the apparatus 2400 may comprise an apparatus for producing repair elements 410, 510, 610 on the photolithography mask in combination with a precursor gas stored in the first supply container 2440.
[0190] As already explained above, the electron beam 2415 can be focused to a spot diameter in the range of a few nanometers. The interaction area or scattering cone, where the electron beam 2415 generates secondary electrons, depends firstly on the energy of the electron beam 2415 and secondly on the composition of the material it impinges on. The diameter of the interaction area is in the low single-digit nanometer range. The diameter of the scattering cone of the electron beam 2415 therefore restricts the resolution limit that can be realized during the production of the repair elements 410, 510, 610 by realizing the corresponding repair shapes. Said resolution limit is currently in the single-digit nanometer range.
[0191] In the apparatus 2400 shown in FIG. 24, the second supply container 2450 stores an etching gas that allows for the execution of a localized electron beam induced etching (EBIE) process. The electron beam induced etching process can remove excess material from the sample 2425. For example, excess material of the pattern elements 860 can be removed from the photolithography mask 800. By way of example, the etching gas can include xenon difluoride (XeF2), halogens, or nitrosyl chloride (NOCl). Thus, the particle beam source 2350 in combination with the gas supply system 2370 constitutes the apparatus 2400 for producing the repair elements 410, 510, 610.
[0192] The third supply container 2460 can store an additive or additive gas that can be added, as needed, to the etching gas kept available in the second supply container 2450 or the precursor gas stored in the first supply container 2440. Alternatively, the third supply container 2460 can store a second precursor gas or a second etching gas.
[0193] 24, each of the supply vessels 2440, 2450, and 2460 has its own control valve 2442, 2452, and 2462 for monitoring or controlling the amount of corresponding gas supplied per unit time, i.e., the gas volumetric flow rate at the site 2422 of incidence of the electron beam 2415 on the sample 2425. The control valves 2442, 2452, and 2462 can be controlled and monitored by a control unit 2370 of the computer system 2330. Thus, the partial pressure ratio of one or more gases provided to the processing location 2422 for performing the EBID and / or EBIE processes can be set over a wide range.
[0194] Additionally, in the exemplary apparatus 2400 of FIG. 24, each supply vessel 2440 , 2450 , and 2460 has its own gas supply line system 2445 , 2455 , and 2465 terminating in a nozzle 2447 , 2457 , and 2467 near the point of incidence 2422 of the electron beam 2415 on the sample 2425 .
[0195] Each of the supply vessels 2440, 2450, and 2460 has its own temperature setting element and / or control element, allowing both cooling and heating of the corresponding supply vessel 2440, 2450, and 2460. This allows the storage and especially the delivery of the precursor gases at their respective optimal temperatures (not shown in FIG. 24). The control unit 2370 can control the temperature setting elements and temperature control elements of the supply vessels 2440, 2450, and 2460. In the EBID and EBIE treatment processes, the temperature setting elements of the supply vessels 2440, 2450, and 2460 can further be used to set the vapor pressure of the stored precursor gases by selecting the appropriate temperature.
[0196] The apparatus 2400 may include two or more supply vessels 2440 for storing two or more precursor gases. Additionally, the apparatus 2400 may include two or more supply vessels 2450 for storing two or more etching gases (not shown in FIG. 24).
Claims
1. 1. A method (1900) for repairing at least one defect (240, 750, 940, 1140, 1240, 1330, 1630, 1840) in a lithography mask (200, 400, 500, 600, 700, 800, 900, 1100, 1200, 1300, 1600, 1800), comprising: determining at least one repair feature parameter for the at least one defect, comprising assigning at least one numerical value to the parameter, the numerical value deviating from a predefined numerical value for the parameter by the at least one defect, the deviation of the numerical value of the at least one parameter being selected from a range with a lower limit greater than zero and less than a resolution limit of the lithography mask; The method (1900),
2. 2. The method (1900) of claim 1 , wherein the at least one parameter comprises at least one element from a group comprising: at least one lateral dimension size of the at least one repair shape, a height dimension size of the at least one repair shape, a distance between the at least one repair shape and the at least one defect, a material composition of the at least one defect, a geometric shape of the at least one repair shape, and an environment of the at least one defect on the lithography mask.
3. The method (1900) according to claim 1 or 2, wherein said at least one parameter deviates by a predetermined absolute value from said predefined numerical value for said parameter due to said at least one defect.
4. The method (1900) of any one of claims 1 to 3, wherein the resolution limit of the lithography mask is determined by a light wavelength of the lithography mask, a numerical aperture, and an exposure setting suitable for projecting a pattern of the lithography mask onto a photoresist disposed on a wafer.
5. 5. The method (1900) of claim 4, wherein the numerical aperture comprises a numerical aperture of a projection lens of an exposure system suitable for projecting the pattern of the lithography mask onto the photoresist.
6. The method (1900) of any one of claims 1 to 5, wherein the resolution limit of the lithography mask comprises a mask-side resolution limit of an exposure system suitable for exposing a wafer with the lithography mask.
7. The mask side resolution limit is [0010] where λ is the light wavelength of the lithography mask, and NA M 7. The method (1900) of claim 6, wherein: σ is the mask-side numerical aperture of the projection lens of the exposure system; and σ is an exposure setting of the exposure system suitable for exposing the lithography mask.
8. The method (1900) according to any one of the preceding claims, wherein the deviation of the numerical value of the at least one corresponding parameter comprises a range of 2% to 80%, preferably 2% to 50%, most preferably 2% to 30% of the resolution limit of the lithographic mask.
9. 9. The method (1900) of any one of claims 1 to 8, wherein a dimensional size of at least one dimension of the at least one repair feature comprises a range of 10% to 90%, preferably 20% to 80%, more preferably 30% to 70%, and most preferably 40% to 60% of a dimensional size of a corresponding dimension of the at least one defect.
10. The method (1900) of any one of claims 1 to 9, wherein the at least one defect comprises at least one element from the group comprising: edge placement error (240) of a pattern element (220), interruption and / or cross-linking of a pattern element, deviation in edge roughness of a pattern element, particle adhesion to the lithography mask, lateral defects with low printability, residual defects of a performed defect repair (340), sidewall angle error (1850) of a pattern element (1820), centroid error of a pattern element and / or distance range between two pattern elements.
11. The method (1900) of any one of claims 1 to 10, wherein determining the parameters of the at least one repair shape comprises recording at least one aerial image of the at least one defect.
12. 12. The method (1900) of claim 11, wherein recording the at least one aerial image comprises recording the at least one aerial image of the at least one defect at a light wavelength of the lithography mask and / or recording an aerial image focus synthesis of the at least one defect.
13. 13. The method (1900) of any one of claims 1 to 12, wherein assigning the numerical value comprises applying a trained machine learning model that determines the deviation of the numerical value of the at least one parameter from a predefined numerical value for the at least one defect.
14. 14. The method (1900) of any one of claims 1 to 13, wherein determining the parameters of the at least one repair shape comprises applying a trained machine learning model to determine the parameters of the at least one repair shape.
15. The method (1900) of any one of claims 1 to 14, further comprising the step of generating at least one repair element (410, 510, 610, 770, 790, 850, 870, 1010, 1170, 1190, 1270, 1290, 1440, 1540, 1640) on the lithographic mask according to the determined repair shape.
16. 20. The method (1900) of claim 15, wherein the step of producing at least one repair element comprises performing at least one localized etching process and / or performing at least one localized deposition process with at least one focused particle beam and at least one precursor gas.
17. generating at least one repair element (310) according to at least one repair shape, said parameters of which are defined by said at least one defect (240); b. determining parameters of the repair shape for the remaining residual defects (340), comprising assigning at least one numerical value to the parameter, said numerical value deviating from a predefined numerical value for said parameter by said remaining residual defects; The method (1900) of any one of claims 1 to 16, comprising:
18. 1. A method (2000) for repairing at least one defective pattern element (220, 740, 840, 860, 920, 1130, 1230, 1320, 1620, 1820) of a lithographic mask (200, 400, 500, 600, 700, 800, 900, 1100, 1200, 1300, 1600, 1800), comprising: a. determining at least one repair element (410, 510, 610, 770, 790, 850, 870, 1010, 1170, 1190, 1270, 1290, 1440, 1540, 1640) of the lithographic mask that does not image the lithographic mask during its exposure, the at least one repair element being configured to change an imaging behavior of the at least one defective pattern element; b. creating said at least one repair element on said lithographic mask by at least one focused particle beam (2415) and at least one precursor gas; The method (2000).
19. 20. The method (2000) of claim 18, wherein the at least one repair element has at least one dimension size that includes a range of 10% to 90%, preferably 20% to 80%, more preferably 30% to 70%, and most preferably 40% to 60% of the resolution limit of the lithographic mask.
20. 20. The method (2000) of claim 18 or 19, wherein a distance (420, 520, 620) between the at least one repair element (410, 510, 610) and the at least one defective pattern element (220) is comprised in a range of 2% to 80%, preferably 2% to 50%, more preferably 2% to 30%, and most preferably 2% to 10% of the resolution limit of the lithographic mask.
21. A computer program comprising instructions which, when executed by a computer system, cause the computer system to perform the method steps of claims 1 to 20.
22. 1. An apparatus (2100) for repairing at least one defect (240, 750, 940, 1140, 1240, 1330, 1630, 1840) in a lithography mask (200, 400, 500, 600, 700, 800, 900, 1100, 1200, 1300, 1600, 1800), comprising: means for determining parameters of at least one repair shape for the at least one defect, the means including means for assigning a numerical value to at least one parameter, the numerical value deviating from a predetermined numerical value for the parameter by the at least one defect, the deviation of the numerical value of the at least one parameter being selected from a range having a lower limit greater than zero and less than a resolution limit of the lithography mask.
23. 1. An apparatus (2300) for repairing at least one defective pattern element (220, 740, 840, 860, 920, 1130, 1230, 1320, 1620, 1820) of a lithographic mask (200, 400, 500, 600, 700, 800, 900, 1100, 1200, 1300, 1600, 1800), comprising: a. means for determining at least one repair element (410, 510, 610, 770, 790, 850, 870, 1010, 1170, 1190, 1270, 1290, 1440, 1540, 1640) of the lithographic mask that does not image the lithographic mask during its exposure, the at least one repair element being configured to change an imaging behavior of the at least one defective pattern element; b. a means for providing a focused particle beam (2415) and at least one precursor gas configured to create the at least one repair element on the lithographic mask; An apparatus (2300).
24. A lithographic mask repaired according to any of the method steps of claims 1 to 20 and used in an exposure system.
25. An exposure system using a lithography mask repaired according to any of the method steps of claims 1-20.
26. 26. The exposure system of claim 25, wherein a resolution limit of the exposure system is determined by a wavelength of a light source of the exposure system, a numerical aperture of a projection lens of the exposure system, and an exposure setting of the exposure system.
27. 27. The exposure system of claim 26, wherein the resolution limit comprises a wafer-side resolution limit of the projection lens.
28. The wafer-side resolution limit is [0025] where λ is the light wavelength of the lithography mask, and NA W 28. The exposure system of claim 27, wherein: σ is the wafer-side numerical aperture of the projection lens of the exposure system, and σ is an exposure setting of the exposure system suitable for exposing the lithography mask to project a pattern of the lithography mask onto a photoresist disposed on a wafer.
Citation Information
Patent Citations
Method for correcting defect in gray tone part in gray tone mask
JP2002107913A
Method for correcting defect of mask and device for correcting defect
JP2003140321A
Method and apparatus for analyzing and removing defects in EUV photomasks
JP2014521230A
Method of defect repairing in graytone part in graytone mask
US20030186130A1
Method and apparatus for evaluating an unknown effect of defects of an element of a photolithography process
WO2019219826A1