Semiconductor device and method for manufacturing semiconductor device
The surface-activated pads on the semiconductor device protruding from the passivation film enable reliable bonding under vacuum conditions, addressing misalignment issues and improving assembly precision.
Patent Information
- Application Number
- JP2021143433
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2021-09-02
- Publication Date
- 2024-10-30
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing technologies face challenges in reliably bonding pads of a semiconductor chip to pads of a substrate without causing misalignment due to thermal stress and oxide film interference.
The semiconductor device employs surface-activated pads on both the chip and substrate, which are formed to protrude from the passivation film, allowing for direct contact and bonding under high vacuum at room temperature, eliminating the need for thermal processes.
This method ensures reliable and precise bonding of chip and substrate pads without misalignment, enhancing the reliability and efficiency of semiconductor device assembly.
Smart Images

Figure 2024153958000001_ABST
Abstract
Description
[Technical field]
[0001] FIELD An embodiment of the present invention relates to a semiconductor device and a method for manufacturing a semiconductor device. [Background technology]
[0002] There is a technology for bumplessly mounting a semiconductor chip onto a substrate, in which multiple pads on the semiconductor chip must be securely connected to multiple contact pads on the substrate, respectively. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2013 / 161891 Summary of the Invention [Problem to be solved by the invention]
[0004] An object of the embodiments is to provide a semiconductor device and a method for manufacturing the semiconductor device that can reliably bond pads of a semiconductor chip to pads of a substrate. [Means for solving the problem]
[0005] The semiconductor device of the embodiment comprises a semiconductor chip having a passivation film on a first surface, and a mounting substrate having a second surface opposite the first surface of the semiconductor chip, the semiconductor chip having a first pad formed on the first surface so as to protrude from a surface of the passivation film, the mounting substrate having a second pad on the second surface, and the first pad and the second pad are in contact with each other with any oxide film or adsorbed material removed from the contact area between the first pad and the second pad. [Brief description of the drawings]
[0006] [Figure 1]1 is a perspective view of a semiconductor chip and a substrate on which the semiconductor chip is mounted according to an embodiment; [Diagram 2] 1 is a cross-sectional view of a semiconductor chip and a mounting substrate in a state in which the semiconductor chip is mounted on the mounting substrate according to an embodiment. [Diagram 3] 2 is a cross-sectional view of one pad of a semiconductor chip in an embodiment. FIG. [Figure 4] 4 is a cross-sectional view of one pad of a semiconductor chip having a different configuration from that of FIG. 3 in the embodiment. [Diagram 5] 1A to 1C are diagrams for explaining a method for manufacturing pads of a semiconductor chip according to an embodiment. [Figure 6] 1A to 1C are diagrams for explaining a method for manufacturing pads of a semiconductor chip according to an embodiment. [Figure 7] 1A to 1C are diagrams for explaining a method of bumplessly mounting a semiconductor chip on a mounting substrate according to an embodiment. [Figure 8] 1A to 1C are diagrams for explaining a surface activation treatment for a semiconductor chip and a mounting substrate according to an embodiment. [Figure 9] 4A to 4C are diagrams for explaining bonding of a semiconductor chip and a mounting substrate according to an embodiment. [Figure 10] 4A to 4C are diagrams for explaining bonding between pads of a semiconductor chip and pads of a mounting substrate in an embodiment. [Figure 11] 4A to 4C are diagrams for explaining bonding between pads of a semiconductor chip and pads of a mounting substrate in an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] Hereinafter, an embodiment will be described with reference to the drawings.
[0008] In addition, in each drawing used in the following description, the scale of each component is different so that each component can be recognized on the drawing, and the present invention is not limited to only the quantity of components, the shapes of components, the size ratios of the components, and the relative positional relationships of each component depicted in these drawings. (composition)
[0009] Fig. 1 is a perspective view of a semiconductor chip 1 and a substrate 2 on which the semiconductor chip 1 is mounted in this embodiment. The semiconductor chip 1 is a bare chip cut out from a semiconductor wafer and separated into individual pieces. In Fig. 1, the semiconductor chip 1 is flip-chip mounted on the substrate 2.
[0010] For ease of explanation, an example will be described in which one semiconductor chip (hereinafter also referred to as chip) 1 is mounted on a substrate 2 which is a mounting substrate, but multiple semiconductor chips 1 may be mounted on the substrate 2. Furthermore, when multiple semiconductor chips 1 are mounted on the substrate 2, the multiple semiconductor chips 1 may be different types of devices.
[0011] The semiconductor chip 1 is a plate-shaped chip and has a plurality of pads (hereinafter referred to as chip pads) 3 for electrical connection with the substrate 2. The plurality of chip pads 3 are provided on one surface of the semiconductor chip 1 (the lower surface of the semiconductor chip 1 in FIG. 1).
[0012] Meanwhile, the substrate 2 also has a plurality of pads (hereinafter referred to as contact pads) 4 for electrical connection with the semiconductor chip 1 on the surface on which the semiconductor chip 1 is mounted. The plurality of contact pads 4 are provided on one surface of the substrate 2 (the upper surface of the substrate 2 in FIG. 1). As will be described later, the semiconductor chip 1 is bonded to the substrate 2 in a high vacuum environment.
[0013] 2 is a cross-sectional view of the semiconductor chip 1 and the substrate 2 in a state in which the semiconductor chip 1 is mounted on the substrate 2. FIG 2 shows a cross section of the semiconductor chip 1 and the substrate 2 taken along the line II-II in FIG.
[0014] A plurality of chip pads 3 of the semiconductor chip 1 are in contact with and electrically connected to contact pads 4 of the substrate 2 by flip-chip mounting.
[0015] Flip chip mounting has been widely adopted to replace wire bonding mounting in response to the demand for smaller and thinner semiconductor memory packages. In particular, flip chip mounting has been widely adopted in response to the increasing performance and functionality of mobile information terminals. Flip chip mounting is also used in MCPs (Multi-Chip-Packages) that stack multiple chips.
[0016] A substrate 2 on which a semiconductor chip 1 as shown in Fig. 2 is mounted is mounted in various devices. For example, the semiconductor chip 1 is a chip of a NAND type flash memory, which is a non-volatile memory, and / or a chip of a memory controller that controls the non-volatile memory. The substrate 2 on which one or more chips 1 are mounted is mounted in an SSD (Solid State Drive) device.
[0017] The semiconductor chip 1 has a passivation film 11 on one surface. The chip pads 3 of the semiconductor chip 1 are provided in a plurality of openings provided in the passivation film 11 of the semiconductor chip 1. Each chip pad 3 is electrically connected to a wiring in the semiconductor chip 1.
[0018] On the other hand, the multiple contact pads 4 on the substrate 2 are provided on the surface on which the semiconductor chip 1 is mounted. That is, the substrate 2 has the multiple contact pads 4 on the surface opposite to the surface having the multiple chip pads 3 of the semiconductor chip 1. A solder mask 5 is applied on the surface. The solder mask 5 is not applied on the surfaces of each of the multiple contact pads 4. (Chip pad configuration)
[0019] Each of the chip pads 3 is provided so as to protrude from the surface of the passivation film. Fig. 3 is a cross-sectional view of one chip pad 3.
[0020] The chip pad 3 is formed so as to protrude from an opening 11a of a passivation film 11 of the semiconductor chip 1. Specifically, as shown in FIG. 3, the chip pad 3 has an interlayer film 12 which is an insulating film, and an aluminum film 13 which is a conductive film. The chip pad 3 has the aluminum film 13 formed on the interlayer film 12. The aluminum film 13 is provided so as to cover the interlayer film 12. A top surface (upper surface in FIG. 3) 13a of the aluminum film 13 protrudes by a height d from a surface 11s of the passivation film 11. In other words, the protruding portion of the chip pad 3 is a part of the aluminum film 13.
[0021] FIG. 4 is a cross-sectional view of one chip pad 3A having a different configuration from that of FIG.
[0022] The chip pad 3A is formed so as to protrude from an opening 11a of a passivation film 11 of the semiconductor chip 1. Specifically, as shown in FIG. 4, the chip pad 3A has an aluminum film 14 which is a conductive film, and an additional aluminum film 15 which is also a conductive film. The additional aluminum film 15 is laminated on the aluminum film 14. If the aluminum film 14 is considered as a first conductive film, the additional aluminum film 15 is a second conductive film formed so as to cover the aluminum film 14 by a rewiring process. A top surface (upper surface in FIG. 4) 15a of the additional aluminum film 15 protrudes by a height d from a surface 11s of the passivation film 11. That is, the protruding portion of the chip pad 3A is a part of the additional aluminum film 15. (Method of manufacturing chip pad)
[0023] A method for manufacturing the chip pad 3 will now be described.
[0024] 5 is a diagram for explaining a method for manufacturing the chip pad 3. FIG 5 shows a cross section of one chip pad 3.
[0025] 5, an interlayer film 12, which is an insulating film, is formed on the surface of the semiconductor chip 1. Furthermore, a photoresist 21 for anisotropic etching (RIE) is patterned on the interlayer film 12 in accordance with the shape of the chip pad 3.
[0026] From the state of SS1, the interlayer film 12 is patterned to match the shape of the chip pad 3 by anisotropic etching (RIE) or the like.
[0027] As shown by SS2, after the photoresist 21 is removed, the aluminum film 13 and the passivation film 11 are laminated on the surface of the semiconductor chip 1 by sputtering, coating, or the like.
[0028] Thereafter, as shown by SS3, a protective film 22 is laminated by sputtering or the like. Thereafter, the protective film 22 and the passivation film 11 are entirely etched back by anisotropic etching (RIE), chemical mechanical polishing (CMP), or the like. As a result, a chip pad 3 as shown in FIG. 3 is formed.
[0029] A method for manufacturing the chip pad 3A will now be described.
[0030] Fig. 6 is a diagram for explaining a method for manufacturing a chip pad 3A. Fig. 6 shows a cross section of one chip pad 3A. After an aluminum film 14 for the chip pad is formed on the surface of the semiconductor chip 1, a passivation film 11 is applied. The passivation film 11 is patterned, and the aluminum film 14 is exposed at the bottom of a recess formed in the passivation film 11 of the semiconductor chip 1, as shown by SS11.
[0031] In other words, the passivation film 11 is formed so as to bulge around the aluminum film 14 at the bottom of the recess, as shown in FIG.
[0032] Next, as shown by SS12, an additional aluminum film 15 is deposited by sputtering, coating or the like.
[0033] Then, as indicated by SS13, a protective film 23 is laminated by sputtering, coating or the like.
[0034] Thereafter, the protective film 23 and the additional aluminum film 15 are etched back over the entire surface by anisotropic etching (RIE), chemical mechanical polishing (CMP), etc. As a result, a chip pad 3A as shown in FIG. (A method of mounting semiconductor chips on a substrate without bumps)
[0035] FIG. 7 is a diagram for explaining a method for mounting the semiconductor chip 1 on the substrate 2 in a bumpless manner.
[0036] The fabrication (S1) of the semiconductor chip 1 and the fabrication (S2) of the substrate 2 are performed separately from each other. The fabrication (S1) of the semiconductor chip 1 includes the fabrication (S3) of a plurality of chip pads 3 (or 3A). The fabrication (S3) of the plurality of chip pads 3 (or 3A) is as shown in FIG. 5 (or FIG. 6).
[0037] That is, a semiconductor chip (1) having a passivation film 11 on one surface of the semiconductor chip 1 is fabricated, and a plurality of chips 3 are fabricated so as to protrude from the surface of the passivation film 11. A substrate 2 having a plurality of contact pads 4 is fabricated separately from the semiconductor chip 1.
[0038] After the fabrication of the semiconductor chip 1 (S1) and the substrate 2 (S2), a surface activation process (S4) is performed. The surface activation process (S4) is performed under vacuum on the surfaces of the multiple chip pads 3 (or 3A) of the semiconductor chip 1 and the multiple contact pads 4 of the substrate 2. An oxide film may be formed on the surfaces of the multiple chip pads 3 (or 3A) and the multiple contact pads 4, or various adsorbed substances may be attached to them. The surface activation process (S4) removes these oxide films and the like.
[0039] Fig. 8 is a diagram for explaining the surface activation process for the semiconductor chip 1 and the substrate 2. As shown in Fig. 8, in the surface activation process (S4), in a space C under high vacuum, the surfaces of the chip pads 3 (or 3A) and the contact pads 4 are irradiated with a beam B (indicated by a dashed line) which is an ion beam or a neutron beam, thereby removing oxide films and the like on the surfaces of the bonding materials (the chip pads 3 (or 3A) and the contact pads 4).
[0040] After the surface activation process (S4), a bonding process (S5) is performed. Fig. 9 is a diagram for explaining bonding of the semiconductor chip 1 and the substrate 2. In the bonding process (S5), the chip pads 3 (or 3A) and the contact pads 4 are brought into contact with each other and bonded to each other in a high vacuum space C at room temperature.
[0041] Specifically, in the bonding process (S5), the chip pads 3 (or 3A) and the contact pads 4 are brought into contact with each other after being aligned with each other. By bringing the chip pads 3 (or 3A) and the contact pads 4 into contact with each other under high vacuum and at room temperature, the chip pads 3 (or 3A) and the contact pads 4 are instantly bonded to each other. Since the surfaces of the chip pads 3 (or 3A) and the surfaces of the contact pads 4 are subjected to surface activation processing, the chip pads 3 (or 3A) and the contact pads 4 are firmly bonded to each other. At this time, the chip pads 3 (or 3A) and the contact pads 4 are in contact with each other with the oxide film or adsorbed matter removed from the contact area of each chip pad 3 (or 3A) and each contact pad 4.
[0042] In the conventional method of mounting a semiconductor chip 1 on a substrate 2 using ball bumps, a thermal process is performed during the process, which causes misalignment between the semiconductor chip 1 and the substrate 2 due to thermal stress. However, in pad bonding using surface activation treatment, no thermal process is performed, so this type of misalignment problem does not occur.
[0043] 10 and 11 are diagrams for explaining the bonding between the chip pad 3A and the contact pad 4. Fig. 11 shows a state in which the top surface 15a of the additional aluminum film 15 is in contact with the surface 4a of the contact pad 4.
[0044] As shown in FIG. 10, the semiconductor chip 1 and the substrate 2 are aligned and bonded together so that the top surface 15a of the additional aluminum film 15 of the chip pad 3A comes into contact with the surface 4a of the contact pad 4.
[0045] 10, the surface 4a of the contact pad 4 may be at the bottom of a recess formed in the surface of the solder mask 5. Even in such a case, the top surface 15a of the additional aluminum film 15 protrudes from the surface of the passivation film 11. Therefore, as shown in FIG. 11, the top surface 15a of the additional aluminum film 15 fits into the recess of the solder mask 5.
[0046] That is, the substrate 2 has a solder resist 5 on the surface on which the semiconductor chip 1 is mounted. Each contact pad 4 is formed in a recess formed on the solder resist 5, and the protruding portion of each chip pad 3 (3A) fits into the recess.
[0047] Surface 4a of contact pad 4 and surface 15a of chip pad 3A (top surface 15a of additional aluminum film 15) are subjected to a surface activation process, and therefore are instantly and firmly bonded together upon contact.
[0048] As described above, according to the above-described embodiment, it is possible to provide a semiconductor device and a method for manufacturing the semiconductor device that can reliably bond the pads of the semiconductor chip to the pads of the substrate.
[0049] Since the multiple chip pads of a typical semiconductor chip are located lower than the surface of the passivation film (i.e., in a position where there is no passivation film), simply performing an activation process makes it difficult for the multiple contact pads 4 of the substrate 2 and the chip pads 3 of the semiconductor chip 1 to be bonded by simply coming into contact with each other.
[0050] In contrast, according to the embodiment described above, the chip pads 3 of the semiconductor chip 1 are formed so as to protrude from the surface of the passivation film 11, so that the pads that have been subjected to surface activation treatment are reliably and firmly bonded to each other.
[0051] In the above-described embodiment, aluminum is used as the material for each pad, but other conductive materials such as copper may also be used.
[0052] Although several embodiments of the present invention have been described, these embodiments are merely examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]
[0053] 1 semiconductor chip, 2 boards, 3, 3A chip pad, 4 contact pads, 4a contact pad surface; 5 solder mask, 11 Passivation film, 11a aperture, 11s surface, 12 Interlayer film, 13 Aluminum film, 13a top surface, 14 Aluminum film, 15 additional aluminum film, 15a top surface, 21 Photoresist, 22, 23 Protective membrane.
Claims
1. a semiconductor chip having a passivation film on a first surface; a mounting substrate having a second surface facing the first surface of the semiconductor chip, the semiconductor chip has a first pad formed on the first surface so as to protrude from a surface of the passivation film, the mounting substrate has second pads on the second surface; A semiconductor device, wherein the first pad and the second pad are in contact with each other in a state where an oxide film or adsorbed material is removed from the contact region between the first pad and the second pad.
2. the mounting board has a solder resist provided on the second surface, the second pad is formed in a recess formed on the solder resist, The semiconductor device according to claim 1 , wherein a protruding portion of said first pad fits into said recess.
3. the first pad has a conductive film formed on an insulating film, 2. The semiconductor device according to claim 1, wherein the protruding portion of said first pad is a part of said conductive film.
4. the first pad has a second conductive film laminated on a first conductive film; 2. The semiconductor device according to claim 1, wherein the protruding portion of said first pad is a part of said second conductive film.
5. 2. The semiconductor device according to claim 1, wherein the semiconductor chip is a nonvolatile memory chip or a controller chip that controls the nonvolatile memory.
6. 2. The semiconductor device according to claim 1, wherein said first pad is formed using aluminum as a conductive material.
7. A semiconductor chip is fabricated having a passivation film on a first surface thereof; forming a first pad on the first surface of the semiconductor chip so as to protrude from a surface of the passivation film; a mounting substrate having second pads on a second surface opposite to the first surface of the semiconductor chip; performing a surface activation treatment on the surfaces of the first pad and the second pad under vacuum; After the surface activation treatment, the first pad and the second pad are brought into contact with each other and bonded together under vacuum. A method for manufacturing a semiconductor device.
Citation Information
Patent Citations
Chip-on-wafer bonding method and bonding device, and structure comprising chip and wafer
WO2013161891A1