Optical modulator element, optical transmitter, and optical transceiver

The optical modulator element addresses higher-order mode interference by using a rib-type waveguide with distinct electron affinity thin films and heavily doped regions to suppress electric field spread, enhancing signal quality and reducing optical loss.

JP2024154317APending Publication Date: 2024-10-30FUJITSU OPTICAL COMPONENTS LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023068091
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-30

AI Technical Summary

Technical Problem

In optical modulator elements, the expansion of the electric field waveguide mode generates higher-order modes, leading to inter-mode interference, decreased extinction ratio and optical modulation intensity, increased bit errors, and optical loss, which deteriorates signal quality.

Method used

The optical modulator element incorporates a rib-type optical waveguide with a PN junction, a first thin film on the P-type slab region and a second thin film on the N-type slab region, both having different electron affinities from the slab regions, and heavily doped regions connected to metal electrodes outside the slab regions, limiting the thin films' lateral extent to suppress electric field spread and reduce optical loss.

Benefits of technology

This design effectively suppresses higher-order modes, reduces optical loss, and enhances signal quality by minimizing electric field distribution, thereby improving the extinction ratio and optical modulation intensity while maintaining high mobility and reducing electrical resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154317000001_ABST
    Figure 2024154317000001_ABST
Patent Text Reader

Abstract

To provide an optical modulator element, etc., with which it is possible to suppress the occurrence of high-order modes and suppress the quality degradation and light loss of optical signals.SOLUTION: An optical modulator element comprises a rib-type optical waveguide, a first thin-film, a first high-concentration dope region, and a first metal electrode. The rib-type optical waveguide includes: a rib part having a PN junction; a P-type slab region which is continuous with a P-type region of the rib part; and an N-type slab region which is continuous with an N-type region of the rib part. The first thin-film is formed on the P-type slab region, and is different in electron affinity from the material of the P-type slab region. The first high-concentration dope region is a region in the P-type slab region located away from the rib part. The first metal electrode is electrically connected to the first high-concentration dope region located outside the P-type slab region in which the first thin-film is formed at an upper layer.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an optical modulator element, an optical transmitter, and an optical transceiver. [Background technology]

[0002] In recent years, the demand for high-capacity optical fiber communications has increased due to the increase in communication capacity in data centers, 5G fronthaul and backhaul, etc., and optical transceivers using optical modulator elements that modulate electrical signals into optical signals have become widespread. The optical modulator elements used in optical transceivers achieve high-speed communications while reducing optical loss. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] US Patent Application Publication No. 2022 / 0187635 [Patent Document 2] US Patent Application Publication No. 2022 / 0026747 [Patent Document 3] US Patent Application Publication No. 2022 / 0252911 Summary of the Invention [Problem to be solved by the invention]

[0004] In an optical modulator element, when the electric field of the waveguide mode is expanded, a higher-order mode is generated, and the inter-mode interference of the higher-order mode reduces the extinction ratio and optical modulation intensity of the optical modulated signal, increasing bit errors and degrading the quality of the optical signal. Moreover, when a higher-order mode is generated, optical energy is transferred from the fundamental mode to the higher-order mode, causing optical loss.

[0005] In one aspect, an object of the present invention is to provide an optical modulator element etc. capable of suppressing degradation in optical signal quality and optical loss while suppressing the occurrence of higher-order modes. [Means for solving the problem]

[0006] An optical modulator element according to one embodiment includes a rib-type optical waveguide, a first thin film, a first highly doped region, and a first metal electrode. The rib-type optical waveguide includes a rib portion having a PN junction, a P-type slab region continuous with the P-type region of the rib portion, and an N-type slab region continuous with the N-type region of the rib portion. The first thin film is formed on the P-type slab region and includes a material having a different electron affinity from the material of the P-type slab region. The first highly doped region is a highly doped region in the P-type slab region located away from the rib portion. The first metal electrode is electrically connected to the first highly doped region located outside the P-type slab region on which the first thin film is formed. Effect of the Invention

[0007] According to one aspect, it is possible to provide an optical modulator element etc. capable of suppressing degradation in optical signal quality and optical loss while suppressing the occurrence of higher-order modes. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is an explanatory diagram showing an example of a schematic cross-sectional portion of an optical modulator element according to a first embodiment. [Diagram 2] FIG. 2 is an explanatory diagram showing an example of a dopant arrangement configuration of the optical modulator element according to the first embodiment. [Figure 3A] FIG. 3A is an explanatory diagram showing an example of an electric field distribution in a waveguide mode of the optical modulator element according to the first embodiment. [Figure 3B] FIG. 3B is an explanatory diagram showing an example of an electric field distribution in a waveguide mode of an optical modulator element of a comparative example. [Figure 4] FIG. 4 is an explanatory diagram showing an example of the electric field profile of the fundamental mode in the optical modulator element of the comparative example and the optical modulator element of the first embodiment. [Diagram 5] FIG. 5 is an explanatory diagram showing an example of the band gap of Si and Ge. [Figure 6] FIG. 6 is a diagram illustrating an example of the relationship between the mobility of electrons and holes and the impurity concentration. [Figure 7] FIG. 7 is an explanatory diagram showing an example of the correspondence relationship between the RF frequency and the EO response. [Figure 8] FIG. 8 is an explanatory diagram showing an example of a dopant arrangement configuration of an optical modulator element according to a second embodiment. [Figure 9] FIG. 9 is an explanatory diagram showing an example of a schematic cross-sectional portion of a thin film of an optical modulator element according to the second embodiment. [Figure 10] FIG. 10 is an explanatory diagram showing an example of a dopant arrangement configuration of an optical modulator element according to a third embodiment. [Figure 11] FIG. 11 is an explanatory diagram showing an example of a schematic cross-sectional portion of an optical modulator element according to a third embodiment. [Figure 12] FIG. 12 is an explanatory diagram showing an example of a schematic cross-sectional portion of another optical modulator element. [Figure 13] FIG. 13 is a block diagram showing an example of an optical transceiver according to this embodiment. [Figure 14] FIG. 14 is an explanatory diagram showing an example of a schematic cross-sectional portion of an optical modulator element of a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Fig. 14 is an explanatory diagram showing an example of a schematic cross-sectional portion of an optical modulator element 100 of a comparative example. The optical modulator element 100 shown in Fig. 14 has a rib-type waveguide 101 and a metal electrode 103 that is electrically connected to the rib-type waveguide 101 and is connected to a signal electrode 104. The rib-type waveguide 101 is configured with a rib-shaped core 102 and has an upper clad layer 106 and a lower clad layer 105 that sandwich the core 102. The core 102 has a rib portion 111, a slab portion 112 that is continuous with both sides of the rib portion 111, and a thin film 113 formed on the slab portion 112.

[0010] The rib portion 111 has a P-type region 111A and an N-type region 111B that form a horizontal PN junction. The slab portion 112 has a P-type slab region 112A that is continuous with the P-type region 111A, and an N-type slab region 112B that is continuous with the N-type region 111B. The thin film 113 has a first thin film 113A formed on the P-type slab region 112A, and a second thin film 113B formed on the N-type slab region 112B. The metal electrode 103 has a first metal electrode 103A that is electrically connected to the first thin film 113A, and a second metal electrode 103B that is electrically connected to the second thin film 113B. The first metal electrode 103A is electrically connected to a first signal electrode 104A in the signal electrode 104, and the second metal electrode 103B is electrically connected to a second signal electrode 104B in the signal electrode 104.

[0011] The first thin film 113A is made of a semiconductor material having a different electron affinity from the material of the P-type slab region 112A. The electron affinity of a semiconductor is the energy obtained when one electron moves from the external vacuum level to the bottom of the semiconductor conductor.

[0012] The second thin film 113B is made of a semiconductor material having a different electron affinity from the material of the N-type slab region 112B. The first thin film 113A is formed on the P-type slab region 112A across a gap g11 from the sidewall of the P-type region 111A of the rib portion 111. The second thin film 113B is formed on the N-type slab region 112B across a gap g12 from the sidewall of the N-type region 111B of the rib portion 111.

[0013] A heterojunction between Si and Ge is formed at the interface between the first thin film 113A and the P-type slab region 112A. Also, a heterojunction between Si and Ge is formed at the interface between the second thin film 113B and the N-type slab region 112B.

[0014] Therefore, in the optical modulator element 100 of the comparative example, the electrical resistance between the first signal electrode 104A and the second signal electrode 104B is reduced by the high-mobility carriers formed at the heterojunction. As a result, the RC time constant given by the product of the series electrical resistance R and the electrostatic capacitance C can be reduced.

[0015] In the optical modulator element 100 of the comparative example, the first thin film 113A and the second thin film 113B extend to just below the metal electrode 103. In order to form a heterojunction and increase the mobility of electrons and holes, a material having a higher refractive index than that of the material forming the rib-shaped core 102 is used as the material forming the first thin film 113A and the second thin film 113B. When designed and manufactured using silicon photonics suitable for mass production as a platform, the core 102 is made of, for example, silicon crystal, and the first thin film 113A and the second thin film 113B are made of, for example, germanium crystal or silicon-germanium mixed crystal. That is, the refractive index of the first thin film 113A and the second thin film 113B is higher than that of the core 102. As a result, the electric field of the waveguide mode extends to the metal electrode 103 and the slab portion 112 just below the metal electrode 103, and light absorption by metal electrons and carriers occurs, resulting in light loss. For example, if the slab portion 112 directly below the metal electrode 103 is a highly doped region, the electric field extends to the highly doped region, causing light absorption by metal electrons and highly doped carriers, resulting in optical loss.

[0016] Even if a material other than silicon and germanium, for example GaAs, which is one of the III-V group, is used for the optical modulator element 100, the core 102 will be an AlGaAs mixed crystal, and the first thin film 113A and the second thin film 113B will be configured to include GaAs crystal. However, since the refractive index of GaAs crystal is higher than that of AlGaAs mixed crystal, optical loss will still occur.

[0017] Moreover, in the optical modulator element 100, when the electric field of the waveguide mode is expanded, a higher-order mode is generated, and the inter-mode interference of the higher-order mode reduces the extinction ratio and optical modulation intensity of the optical modulated signal, increases bit errors, and reduces the quality of the optical signal. Moreover, when a higher-order mode is generated, optical energy is transferred from the fundamental mode to the higher-order mode, causing optical loss.

[0018] In addition, in the optical modulator element 100, the first thin film 113A and the second thin film 113B are present directly under the metal electrode 103, so in order to achieve low resistance contact with the metal electrode 103, it is necessary to provide high conductivity to the first thin film 113A and the second thin film 113B. Therefore, it is necessary to distribute a high concentration of dopant by ion implantation into the first thin film 113A and the second thin film 113B and activate the dopant by annealing. In the case of a heterojunction having lattice distortion, lattice relaxation occurs due to the temperature increase caused by annealing, and crystal defects occur at the heterojunction interface. As a result, the electrical resistance increases due to scattering caused by the crystal defects, making it impossible to reduce the RC time constant. The crystal defects occurring at the heterojunction interface tend to be irregularly distributed on the wafer and increase with long-term use, which reduces the mass productivity of the optical modulator element 100 and impairs its reliability.

[0019] Therefore, there is a demand for the optical modulator element of this embodiment that can suppress the degradation of optical signal quality and optical loss while suppressing the occurrence of higher-order modes.

[0020] Hereinafter, the embodiments of the optical modulator element and the like disclosed in the present application will be described in detail with reference to the drawings. Note that the present invention is not limited to these embodiments. In addition, the following examples may be appropriately combined as long as no contradiction occurs. EXAMPLES

[0021] FIG. 1 is an explanatory diagram showing an example of a schematic cross-sectional portion of an optical modulator element 1 according to a first embodiment. FIG. 1 is a cross section perpendicular to the direction in which the fundamental mode of the optical modulator element 1 propagates. The optical modulator element 1 shown in FIG. 1 has a rib-type waveguide 2 and a metal electrode 3 electrically connected to both ends of the rib-type waveguide 2 and electrically connected to a signal electrode 16. The rib-type waveguide 2 has a rib-shaped core 10, and an upper clad layer 14 and a lower clad layer 13 sandwiching the core 10. For convenience of explanation, the lower clad layer 13 is laminated on a support substrate, but the support substrate is not shown. The core 10 has a rib portion 11, a slab portion 12 continuous with both sides of the rib portion 11, and a thin film 15 formed on the slab portion 12. The rib portion 11 has a P-type region 11A and an N-type region 11B. The slab portion 12 has a P-type slab region 12A that is continuous with the P-type region 11A in the rib portion 11, and an N-type slab region 12B that is continuous with the N-type region 11B in the rib portion 11. The thin film 15 has a first thin film 15A formed on the P-type slab region 12A, and a second thin film 15B formed on the N-type slab region 12B.

[0022] The metal electrode 3 includes a first metal electrode 3A that vertically penetrates the upper cladding layer 14 and electrically connects to the P-type slab region 12A, and a second metal electrode 3B that vertically penetrates the upper cladding layer 14 and electrically connects to the N-type slab region 12B. The first metal electrode 3A is electrically connected to a first signal electrode 16A in the signal electrode 16. The second metal electrode 3B is electrically connected to a second signal electrode 16B in the signal electrode 16.

[0023] FIG. 2 is an explanatory diagram showing an example of the dopant arrangement configuration of the optical modulator element 1 of Example 1. The core 10 shown in FIG. 2 has a P region 12A1, a P+ region 12A2, a P++ region 12A3, an N region 12B1, an N+ region 12B2, and an N++ region 12B3. The P region 12A1 is composed of a P-type region 11A and a part of a P-type slab region 12A continuous with the P-type region 11A. The P+ region 12A2 is a high-doped region formed by a part of the P-type slab region 12A connected to the P region 12A1. The P++ region 12A3 is a high-concentration doped region formed by a part of the P-type slab region 12A connected to the P+ region 12A2. The doping concentration has the relationship of P region 12A1 < P+ region 12A2 < P++ region 12A3. The P++ region 12A3, which is a high-concentration doped region, can be said to be the region with the highest doping concentration among the P-type slab regions continuous with the P-type region of the rib portion.

[0024] The first metal electrode 3A is electrically connected to the P++ region 12A3 located outside the P-type slab region 12A where the first thin film 15A is formed on the upper layer. That is, the first metal electrode 3A is electrically connected to the P++ region 12A3 located outside the P-type slab region 12A where the first thin film 15A is formed on the upper layer and on the side far from the rib portion 11. The P++ region 12A3 is in contact with the bottom of the first metal electrode 3A to form a P-side contact region. The P++ region 12A3 is in contact with and overlaps the first thin film 15A in the horizontal direction. As a result, holes are drawn into and distributed in the undoped first thin film 15A, which has a higher electron affinity for holes compared to the P-type slab region 12A, and high-mobility holes exist as two-dimensional carriers in the first thin film 15A, enabling the reduction of the series electrical resistance. The horizontal overlap between the P++ region 12A3 and the first thin film 15A is about 50 nm. Also, considering the alignment accuracy of patterning by an optical mask in the processing step, the horizontal overlap between the P++ region 12A3 and the first thin film 15A is preferably about 100 nm.

[0025] The N region 12B1 is composed of the N-type region 11B and a part of the N-type slab region 12B continuous with the N-type region 11B. The N+ region 12B2 is a part of the N-type slab region 12B connected to the N region 12B1 and forms a highly doped region. The N++ region 12B3 is a part of the N-type slab region 12B connected to the N+ region 12B2 and forms a high-concentration doped region. The second metal electrode 3B is electrically connected to the N++ region 12B3 located outside the N-type slab region 12B where the second thin film 15B is formed on the upper layer. That is, the second metal electrode 3B is electrically connected to the N++ region 12B3 located outside the N-type slab region 12B where the second thin film 15B is formed on the upper layer and on the side far from the rib portion 11. The N++ region 12B3 is in contact with the bottom of the second metal electrode 3B to form an N-side contact region. The doping concentration has the relationship of N region 12B1 < N+ region 12B2 < N++ region 12B3. The N++ region 12B3, which is a high-concentration doped region, can be said to be the region with the highest doping concentration among the N-type slab regions continuous with the N-type region of the rib portion.

[0026] The N++ region 12B3 is in contact with the second thin film 15B and overlaps in the horizontal direction. The horizontal overlap between the N++ region 12B3 and the second thin film 15B is about 50 nm. Also, considering the alignment accuracy of patterning by the optical mask in the processing step, the horizontal overlap between the N++ region 12B3 and the second thin film 15B is preferably about 100 nm.

[0027] In addition, the doping concentration of each region is set as follows, for example. The P region 12A1 is, for example, 5×10^17 cm^-3, the P+ region 12A2 is, for example, 5×10^18 cm^-3, and the P++ region 12A3 is, for example, 1×10^20 cm^-3. The N region 12B1 is, for example, 2×10^17 cm^-3, the N+ region 12B2 is, for example, 5×10^18 cm^-3, and the N++ region 12B3 is, for example, 1×10^20 cm^-3. However, the arrangement and setting of these doping densities are only examples and are not limited thereto, and can be changed as appropriate.

[0028] The first metal electrode 3A penetrates the upper cladding layer 14 vertically and is electrically connected to the P++ region 12A3 in the P-type slab region 12A. The second metal electrode 3B penetrates the upper cladding layer 14 vertically and is electrically connected to the N++ region 12B3 in the N-type slab region 12B.

[0029] If the thickness of the first thin film 15A and the second thin film 15B is hOL, the thickness of the slab portion 12 is hslab, and the thickness of the rib portion 11 is hrib, the thickness of the rib portion 11 of the optical modulator element 1 is thicker than the combined thickness of the slab portion 12 and the first thin film 15A (or the second thin film 15B). In other words, the thickness of the rib portion 11 is hrib>hslab+hOL.

[0030] A gap region 17 is formed between the rib portion 11 and the thin film 15. A first gap region 17A having a width g1 is formed between the rib portion 11 and the first thin film 15A. A second gap region 17B having a width g2 is also formed between the rib portion 11 and the second thin film 15B. However, the first gap region 17A and the second gap region 17B do not have to be provided and can be changed as appropriate depending on the optical loss required for the optical modulator element 1.

[0031] A gap region 18 is formed between the metal electrode 3 and the thin film 15. The gap region 18 has a third gap region 18A with a width g3 formed between the first thin film 15A and the first metal electrode 3A, and a fourth gap region 18B with a width g4 formed between the second thin film 15B and the second metal electrode 3B.

[0032] The core 10, the first thin film 15A, and the second thin film 15B are covered with an upper cladding layer 14. Thus, the upper cladding layer 14 is also present in the first gap region 17A, the second gap region 17B, the third gap region 18A, and the fourth gap region 18B.

[0033] Since the third gap region 18A exists between the first thin film 15A and the first metal electrode 3A, the first thin film 15A is finite in the horizontal direction. Furthermore, since the fourth gap region 18B exists between the second thin film 15B and the second metal electrode 3B, the second thin film 15B is also finite in the horizontal direction. That is, the first thin film 15A and the second thin film 15B are finite in the horizontal direction. Therefore, the electric field of the fundamental mode propagating through the core 10 is suppressed from extending in the horizontal direction, and is also suppressed from extending to the highly doped regions (P++ region 12A3 and N++ region 12B3) directly below the first metal electrode 3A and the second metal electrode 3B. As a result, it is possible to reduce optical loss and suppress higher modes.

[0034] In the optical modulator element 1A, the first thin film 15A and the second thin film 15B are arranged undoped without being intentionally doped, thereby reducing the series electrical resistance and shortening the RC time constant.

[0035] The width wrib of the rib portion 11 is set to, for example, 450 to 500 nm, thereby suppressing the generation of higher-order modes in the rib portion 11 and forming a core 10 with reduced effects of sidewall roughness, which can be used as a basic structure for an optical modulator with low optical loss. The core 10 is, for example, silicon crystal, and the upper clad layer 14 and the lower clad layer 13 are both silica. The first metal electrode 3A and the second metal electrode 3B are formed by forming an aluminum film, optical drawing, or etching. The thickness hrib of the rib portion 11 is, for example, 220 nm, the thickness hslab of the P-type slab region 12A and the N-type slab region 12B is, for example, 100 nm, and the thickness hOL of the first thin film 15A and the second thin film 15B is, for example, 10 nm. The first thin film 15A and the second thin film 15B are separated from the first metal electrode 3A and the second metal electrode 3B, and are located above the bottom surfaces of the first metal electrode 3A and the second metal electrode 3B.

[0036] The width g1 of the first gap region 17A and the width g2 of the second gap region 17B are, for example, 50 to 200 nm. For example, assume that the width g1 of the first gap region 17A and the width g2 of the second gap region 17B are narrower than 50 nm. In this case, the electric field of the fundamental mode spreads to the P-type slab region 12A and the N-type slab region 12B by the first thin film 15A and the second thin film 15B of germanium crystal having a higher refractive index than the core 10. Therefore, taking into consideration the alignment accuracy in processing, the width g1 of the first gap region 17A and the width g2 of the second gap region 17B are preferably within the range of, for example, 50 to 200 nm.

[0037] In order to avoid polarization rotation while maintaining the symmetry of the shape of the core 10, the widths of the first thin film 15A and the second thin film 15B are set to, for example, 700 nm. The width g3 of the third gap region 18A and the width g4 of the fourth gap region 18B are also set to, for example, 500 nm. When the width g3 of the third gap region 18A and the width g4 of the fourth gap region 18B are set to 500 nm, the electric field of the fundamental mode can be suppressed from spreading to the P++ region 12A3 and the N++ region 12B3.

[0038] FIG. 3A is an explanatory diagram showing an example of the electric field distribution of the guided mode of the optical modulator element 1 of the first embodiment. FIG. 3B is an explanatory diagram showing an example of the electric field distribution of the guided mode of the optical modulator element 100 of the comparative example. The core 10 of the optical modulator element 1 is, for example, made of silicon crystal, and the first thin film 15A and the second thin film 15B are, for example, made of germanium crystal. The core 102 of the optical modulator element 100 is, for example, made of silicon crystal, and the first thin film 113A and the second thin film 113B are, for example, made of germanium crystal. The refractive index of the silicon crystal is 3.48, and the refractive index of the germanium crystal is 4.28. It can be seen that the electric field distribution of the guided mode of the optical modulator element 1 shown in FIG. 3A is suppressed in the horizontal direction compared to the electric field distribution of the guided mode of the optical modulator element 100 of the comparative example shown in FIG. 3B.

[0039] Fig. 4 is an explanatory diagram showing an example of the electric field profile of the fundamental mode in the optical modulator element 100 of the comparative example and the optical modulator element 1 of the embodiment 1. In the electric field distribution shown in Fig. 4, the waveform at the position y=50 nm is extracted and displayed with respect to the vertical direction of the fundamental mode profile in Fig. 3A and Fig. 3B, that is, the y axis indicating the vertical position.

[0040] In the optical modulator element 1 of the first embodiment, as shown in Fig. 4, the spread of the electric field distribution of the fundamental mode is suppressed in the direction along the boundary surface (horizontal surface) between the core 10 and the lower cladding layer 13, i.e., along the x-axis. In the optical modulator element 1 of the first embodiment, the spread of the electric field distribution can be suppressed compared to the optical modulator element 100 of the comparative example, so that it is possible to reduce optical loss and suppress higher modes. Moreover, since the slab portion 12 in contact with the metal electrode 3 is a highly doped region of the P++ region 12A3 and the N++ region 12B3, the optical absorption by metal electrons and high-concentration carriers can be reduced to half or less compared to the comparative example.

[0041] FIG. 5 is an explanatory diagram showing an example of the band gap of Si and Ge. In the case where the core 10 is made of, for example, silicon crystal, and the first thin film 15A and the second thin film 15B are made of, for example, germanium crystal, the band arrangement of the heterojunction becomes Type II as shown in FIG. 5. Electrons are distributed on the silicon side, which has a lower band edge energy than germanium (higher electron affinity than germanium). However, since the band offset of the conduction band is small (the difference in electron affinity is small), at room temperature, electrons are also distributed in germanium. Therefore, the mobility is increased by conducting through both the silicon and undoped germanium paths.

[0042] FIG. 6 is an explanatory diagram showing an example of the relationship between the mobility of electrons and holes and the impurity concentration. The comparative example shown in FIG. 6 is an optical modulator element without the thin film 15. The first metal electrode 3A and the second metal electrode 3B are not directly connected to the first thin film 15A and the second thin film 15B in which high-mobility two-dimensional holes and electrons are distributed, but are connected to the P++ region 12A3 and the N++ region 12B3, and the dopant configuration shown in FIG. 2 is adopted. As a result, it is possible to simultaneously achieve optimization of the electrical characteristics (high speed due to reduced electrical resistance) and optimization of the optical characteristics (reduction of optical loss due to suppression of mode broadening and suppression of higher-order modes).

[0043] Since impurity ions due to dopants are not distributed in the first thin film 15A and the second thin film 15B, scattering due to ionized impurities does not occur, and the mobility of electrons and holes increases. The increase in mobility can be estimated from the characteristic curve in Figure 6. In the silicon-germanium heterojunction, the mobility of holes increases significantly due to the conduction of holes through undoped germanium. However, when the increase in the mobility of holes and electrons is taken into consideration, the electrical resistance of the optical modulator element 1 can be reduced to less than half compared to the case where the first thin film 15A and the second thin film 15B are not present.

[0044] Furthermore, since the optical modulator element 1 does not have the first thin film 15A and the second thin film 15B directly below the metal electrode 3, it is not necessary to provide the first thin film 113A and the second thin film 113B with high conductivity in order to achieve low resistance contact with the metal electrode 3. As a result, no crystal defects are generated, which improves the mass productivity and reliability of the optical modulator element 1A.

[0045] In the optical modulator element 1 of the first embodiment, since the first thin film 15A and the second thin film 15B are finite in the horizontal direction, the first metal electrode 3A and the P-type slab region 12A are directly connected, and the second metal electrode 3B and the N-type slab region 12B are directly connected. As a result, the horizontal spread of the electric field distribution is suppressed, thereby reducing optical loss and suppressing higher-order modes. Moreover, for example, the first metal electrode 3A and the second metal electrode 3B are arranged to overlap with the high-concentration doped region, so that optical absorption can be reduced compared to the optical modulator element 100 of the comparative example. In other words, the occurrence of higher-order modes due to the electric field extension of the waveguide mode can be suppressed, and the deterioration of the quality of the optical signal and optical loss can be suppressed.

[0046] In the optical modulator element 1, the P++ region 12A3, which has a higher carrier density than the P region 12A1 and the P+ region 12A2, contacts the first thin film 15A and overlaps with it in the horizontal direction. As a result, carriers present in the P+ region 12A2, the P++ region 12A3, etc. are diffused and distributed in the first thin film 15A. Therefore, the mobility of the first thin film 15A can be increased to reduce the electrical resistance.

[0047] In the optical modulator element 1, the N++ region 12B3, which has a higher carrier density than the N region 12B1 and the N+ region 12B2, contacts the second thin film 15B and overlaps it in the horizontal direction. As a result, carriers present in the N+ region 12B2, the N++ region 12B3, etc. are diffused and distributed in the second thin film 15B. Therefore, the mobility of the second thin film 15B can be increased to reduce the electrical resistance.

[0048] The boundary between P region 12A1 and P+ region 12A2 is located directly below first thin film 15A and overlaps with first thin film 15A in the horizontal direction. However, this is not necessarily required, and the boundary between P region 12A1 and P+ region 12A2 may be located outside first thin film 15A in the horizontal direction, that is, closer to central rib portion 11 than first thin film 15A, and can be changed as appropriate.

[0049] Furthermore, the boundary between N region 12B1 and N+ region 12B2 is located directly below second thin film 15B and overlaps with second thin film 15B in the horizontal direction. However, this is not necessarily required, and the boundary between N region 12B1 and N+ region 12B2 may be located outside second thin film 15B in the horizontal direction, that is, closer to central rib portion 11 than second thin film 15B, and can be changed as appropriate.

[0050] Incidentally, an optical modulator such as a phase modulation section may be configured by using two optical modulator elements 1 of this embodiment and arranging them on two arms of a Mach-Zehnder interferometer, and modifications can be made as appropriate. FIG. 7 is an explanatory diagram showing an example of a simulation result of the electro-optical frequency response of an optical modulator using the optical modulator element 1 of this embodiment. Incidentally, the simulation result of the optical modulator using the optical modulator element 100 of the comparative example is shown by a solid line, the simulation result of the optical modulator using the optical modulator element 100 of the comparative example without a thin film is shown by a dotted line, and the simulation result of the optical modulator using the optical modulator element without a thin film of the comparative example is shown by a dotted line. The optical modulator element 100 of the comparative example is the optical modulator element 100 shown in FIG. 14. The optical modulator element without a thin film is configured with a rib-type core in which a high mobility layer equivalent to the first thin film 113A and the second thin film 113B in which high mobility holes or electrons are distributed is not arranged directly above the slab part. For convenience of explanation, an optical modulator employing the optical modulator element 100 of the comparative example will be referred to as a first optical modulator, and an optical modulator employing the optical modulator element without a thin film of the comparative example will be referred to as a second optical modulator.

[0051] The simulation parameters for each optical modulator are as follows: The dimensions of the waveguide of the optical modulator are rib width Wrib of 500 nm, rib thickness hrib of 220 nm, and waveguide length of 3 mm.

[0052] The optical loss in the waveguide of the optical modulator of this embodiment can be estimated to be 0.4 dB / mm. In contrast, the optical loss in the waveguide of the first optical modulator and the second optical modulator of the comparative example can be estimated to be 0.6 dB / mm, taking into account the loss due to higher-order modes.

[0053] That is, in the simulation, the electrical characteristics were numerically analyzed as an electrical circuit consisting of a series electrical resistance R and a capacitance C, and the obtained electrical characteristics were input as the frequency characteristics of the phase modulation section, which is an optical modulator, to derive the frequency response of the optical interference intensity. The following values ​​were used for the series electrical resistance R and the capacitance C. As a result, the series electrical resistance R of the optical modulator of this embodiment and the first optical modulator of the comparative example is, for example, 1.7Ω, and the series electrical resistance R of the second optical modulator is, for example, 3.5Ω. Furthermore, the capacitance C of the optical modulator of this embodiment and the first optical modulator and the second optical modulator of the comparative example are all 1.2pF (DC reverse bias 3V).

[0054] Therefore, as can be seen from the simulation results shown in FIG. 7, the optical loss of the optical modulator of this embodiment can be further improved by 2 dB compared to the optical loss of the first optical modulator of the comparative example.

[0055] In the optical modulator element 1 of the first embodiment, the material is a silicon-germanium material, but the present invention is not limited thereto, and may be a GaAs or InP material of III-V compounds. These may be combined with silicon-germanium materials, and may be modified as appropriate. When the optical modulator element 1 is made of a GaAs material, the rib portion 11, the P-type slab region 12A, and the N-type slab region 12B may be made of, for example, AlGaAs, and the first thin film 15A and the second thin film 15B may be made of, for example, GaAlAs. When the optical modulator element 1 is made of an InP material, the rib portion 11, the P-type slab region 12A, and the N-type slab region 12B may be made of, for example, InP, and the first thin film 15A and the second thin film 15B may be made of, for example, GaInAs, and may be modified as appropriate.

[0056] In this embodiment, it is possible to provide an optical modulator element 1 capable of suppressing the occurrence of higher-order modes due to electric field extension of the waveguide mode, and suppressing deterioration in the quality of the optical signal and optical loss.

[0057] In the optical modulator element 1 of the first embodiment, the first thin film 15A and the second thin film 15B are made of germanium crystals. However, since germanium crystals have a large lattice mismatch with silicon crystals, it is desirable that the critical thickness at which lattice relaxation does not occur is 1 nm or less. However, when forming a germanium crystal film, lattice relaxation may occur. In addition, the optical absorption edge wavelength of germanium is 1600 nm or more, and loss due to optical absorption may occur in the C band or O band of optical communication.

[0058] Therefore, an embodiment for dealing with such a situation will be described below as Example 2. Note that the same components as those of the optical modulator element 1 of Example 1 are given the same reference numerals, and descriptions of the overlapping components and operations will be omitted. Fig. 8 is an explanatory diagram showing an example of a dopant arrangement configuration of the optical modulator element 1 of Example 2. EXAMPLES

[0059] For example, when a silicon-germanium mixed crystal is used, the critical film thickness can be increased and the optical absorption edge wavelength can be shortened, which may reduce the loss due to optical absorption. Therefore, as shown in Figure 8, a silicon-germanium mixed crystal is used as the first thin film 15A1 and the second thin film 15B1 instead of germanium crystal.

[0060] Fig. 9 is an explanatory diagram showing an example of a schematic cross-sectional portion of the thin film 15 of the optical modulator element 1 of Example 2. The first thin film 15A1 (second thin film 15B1) which is the thin film 15 using a silicon-germanium mixed crystal of the optical modulator element 1 shown in Fig. 9 has a high mobility layer 21 of a silicon-germanium mixed crystal and a covering layer 22 of a silicon crystal instead of the thin film 15 of a germanium crystal.

[0061] The higher the composition ratio of germanium crystals, the smaller the effective mass of holes, which increases mobility and reduces electrical resistance. It is possible to achieve both a reduction in electrical resistance due to increased mobility, i.e., faster operation, a reduction in optical loss, and an increase in critical film thickness. For example, a preferable composition ratio of germanium crystals:silicon crystals is 0.3:0.7. In this case, the silicon-germanium mixed crystal can be laminated to a film thickness of about 10 nm without defects. If this film thickness can be secured, the variation in film thickness during film formation is small, and the variation that affects optical properties can also be reduced.

[0062] The high mobility layer 21 has a thickness of, for example, 10 nm, and the covering layer 22 has a thickness of, for example, 5 nm. The covering layer 22 can suppress the occurrence of ionization defects and the like on the surface of the high mobility layer 21. Since the covering layer 22 is formed of silicon crystals, highly mobile electrons exist as two-dimensional carriers in the covering layer 22 of silicon crystals, making it possible to further reduce the electrical resistance.

[0063] The thin film 15 (first thin film 15A1, second thin film 15B1) of the optical modulator element 1 of the second embodiment has a high mobility layer 21 of silicon-germanium mixed crystal and a covering layer 22 of silicon crystal. As a result, the critical film thickness can be increased and at the same time, the optical absorption edge wavelength is shortened, so that the loss due to optical absorption can be reduced.

[0064] In the optical modulator element 1 of the second embodiment, the high mobility layer 21 is made of a silicon-germanium mixed crystal, and the covering layer 22 is made of silicon crystal, but the present invention is not limited to this and can be applied to germanium crystal or III-V semiconductors. When a GaAs-based material is used, the high mobility layer 21 is made of GaAs, and the covering layer 22 is made of GaAlAs. When an InP-based material is used, the high mobility layer 21 may be made of GaInAs, and the covering layer 22 may be made of InP, and these can be changed as appropriate. EXAMPLES

[0065] FIG. 10 is an explanatory diagram showing an example of a dopant arrangement configuration of an optical modulator element 1A of Example 3. FIG. 11 is a schematic cross-sectional view showing an example of an optical modulator element 1A of Example 3. The same components as those of the optical modulator element 1 of Example 1 are given the same reference numerals, and the description of the overlapping components and operations is omitted. The rib portion 11 of the optical modulator element 1A shown in FIG. 10 and FIG. 11 has a P-type region 11A and an N-type region 11B. A first compensation doped region 31A doped with a low concentration of N impurities is provided on the sidewall portion of the P-type region 11A in the rib portion 11. The first compensation doped region 31A reduces optical loss by canceling out carrier concentrations on the sidewall of the P-type region 11A. In addition, a second compensation doped region 31B doped with a low concentration of P impurities is provided on the sidewall portion of the N-type region 11B in the rib portion 11. The second compensating doped region 31B reduces optical loss by canceling out carrier concentrations on the sidewalls of the N-type region 11B.

[0066] In the optical modulator element 1A of the third embodiment, the first compensation doped region 31A is disposed on the sidewall of the P-type region 11A, and the second compensation doped region 31B is disposed on the sidewall of the N-type region 11B, thereby suppressing optical loss.

[0067] Incidentally, the core 10 in the optical modulator element 1A of the third embodiment is configured as a PN junction of a horizontal structure, but is not limited thereto and can be appropriately changed. FIG. 12 is an explanatory diagram showing an example of a schematic cross-sectional portion of another optical modulator element 1B. The core 10X in the optical modulator element 1B shown in FIG. 12 is a core of a PN junction of a vertical structure. The core 10X configured as a PN junction of a vertical structure has a long interface between the P-type region 11A and the N-type region 11B, and therefore has high light modulation efficiency. In the optical modulator element 1B, even if the core 10X is configured as a PN junction of a vertical structure, the horizontal spread of the electric field distribution is suppressed, thereby reducing optical loss and suppressing high-order modes. Moreover, for example, the first metal electrode 3A and the second metal electrode 3B are arranged so as to overlap with the high-concentration doped region, so that the optical absorption can be reduced compared to the optical modulator element 100 of the comparative example.

[0068] Next, an optical transceiver 50 employing the optical modulator element 1 of this embodiment will be described. FIG. 13 is a block diagram showing an example of the optical transceiver 50 of this embodiment. The optical transceiver 50 shown in FIG. 13 includes an optical transmitter / receiver 51 and a DSP (Digital Signal Processor) 52. The optical transmitter / receiver 51 includes an optical modulator element 54, a driver circuit 55, an optical receiver element 56, and a TIA (Transimpedance Amplifier) ​​57. The DSP 52 controls the entire optical transmitter / receiver 51. The DSP 52 is an electrical component that performs digital signal processing, such as IQ modulation processing of a transmission signal and demodulation processing of a reception signal.

[0069] The DSP 52 executes processing such as encoding of transmission data, generates an electrical signal including the transmission data, and outputs the generated electrical signal to the driver circuit 55. The driver circuit 55 drives the optical modulator element 54 in response to the electrical signal from the DSP 52. The optical modulator element 54 optically modulates the signal light.

[0070] The optical receiver element 56 converts the signal light into an electric signal. The TIA 57 amplifies the electric signal after the electric conversion, and outputs the amplified electric signal to the DSP 52. The DSP 52 performs processing such as decoding the electric signal obtained from the TIA 57 to obtain received data.

[0071] In the optical modulator element 54, since the first thin film 15A and the second thin film 15B are finite in the horizontal direction, the first metal electrode 3A is directly connected to the P-type slab region 12A, and the second metal electrode 3B is directly connected to the N-type slab region 12B. As a result, the horizontal spread of the electric field distribution is suppressed, thereby reducing optical loss and suppressing higher-order modes. Moreover, for example, the first metal electrode 3A and the second metal electrode 3B are arranged to overlap with the highly doped region, so that optical absorption can be reduced compared to the optical modulator element 100 of the comparative example.

[0072] For ease of explanation, the optical transceiver 50 has been illustrated as incorporating an optical modulator element 54 and an optical receiver element 56, but the optical transceiver 50 may be an optical transmitter incorporating only the optical modulator element 54, and may be modified as appropriate.

[0073] Furthermore, each component of each unit shown in the figure does not necessarily have to be physically configured as shown in the figure. In other words, the specific form of distribution and integration of each unit is not limited to that shown in the figure, and all or part of them can be functionally or physically distributed and integrated in any unit depending on various loads, usage conditions, etc.

[0074] Furthermore, the various processing functions performed by each device may be executed in whole or in part on a CPU (Central Processing Unit) (or a microcomputer such as an MPU (Micro Processing Unit) or an MCU (Micro Controller Unit)). It goes without saying that the various processing functions may be executed in whole or in part on a program analyzed and executed by a CPU (or a microcomputer such as an MPU or an MCU), or on hardware using wired logic.

[0075] The following supplementary notes are further disclosed regarding the above-described embodiments including the present example.

[0076] (Note 1) A rib-type optical waveguide having a rib portion having a PN junction, a P-type slab region continuous with the P-type region of the rib portion, and an N-type slab region continuous with the N-type region of the rib portion; a first thin film formed on the P-type slab region and having an electron affinity different from that of a material of the P-type slab region; a first highly doped region of the P-type slab region spaced from the rib portion; a first metal electrode electrically connected to the first highly doped region located outside the P-type slab region on which the first thin film is formed; An optical modulator element comprising:

[0077] (Additional Note 2) The first thin film is 2. The optical modulator element according to claim 1, wherein the optical modulator element is formed on the P-type slab region across a gap from the first metal electrode.

[0078] (Additional Note 3) The first thin film is 2. The optical modulator element according to claim 1, comprising a material having a smaller electron affinity than a material of the P-type slab region.

[0079] (Additional Note 4) The first thin film is 2. The optical modulator element according to claim 1, which is in an undoped state, that is, not intentionally doped.

[0080] (Additional Note 5) The first thin film is 2. The optical modulator element according to claim 1, wherein the optical modulator element is formed on the P-type slab region across a gap from a sidewall of the rib portion.

[0081] (Appendix 6) The optical modulator element according to appendix 1, wherein at least a portion of the first thin film is formed on the first highly doped region.

[0082] (Appendix 7) A second thin film formed on the N-type slab region and having a different electron affinity from the material of the N-type slab region; a second highly doped region of the N-type slab region spaced from the rib portion; a second metal electrode electrically connected to the second highly doped region located outside the N-type slab region on which the second thin film is formed; 2. The optical modulator element according to claim 1, further comprising:

[0083] (Appendix 8) The second thin film is 8. The optical modulator element according to claim 7, wherein the optical modulator element is formed on the N-type slab region across a gap from the second metal electrode.

[0084] (Appendix 9) The second thin film is 8. The optical modulator element according to claim 7, comprising a material having a smaller electron affinity than the material of the N-type slab region.

[0085] (Appendix 10) The second thin film is 8. The optical modulator element according to claim 7, which is in an undoped state, that is, not intentionally doped.

[0086] (Appendix 11) The second thin film is 8. The optical modulator element according to claim 7, wherein the optical modulator element is formed on the N-type slab region across a gap from a sidewall of the rib portion.

[0087] (Appendix 12) The optical modulator element according to appendix 7, wherein at least a portion of the second thin film is formed on the second highly doped region.

[0088] (Additional Note 13) The rib-type optical waveguide includes silicon, 8. The optical modulator element according to claim 7, wherein the first thin film and the second thin film contain germanium.

[0089] (Appendix 14) The optical modulator element according to appendix 13, wherein the first thin film and the second thin film are made of silicon-germanium having a germanium composition ratio of at least 0.2 to 0.4.

[0090] (Appendix 15) The optical modulator element according to appendix 13, wherein the surfaces of the first thin film and the second thin film are covered with a covering layer containing silicon.

[0091] (Appendix 16) An optical transmitter having an optical modulator element that optically modulates light using a transmission signal and transmits transmission light, The optical modulator element includes: a rib type optical waveguide having a rib portion having a PN junction, a P-type slab region continuous with the P-type region of the rib portion, and an N-type slab region continuous with the N-type region of the rib portion; a first thin film formed on the P-type slab region and having an electron affinity different from that of a material of the P-type slab region; a first highly doped region of the P-type slab region spaced from the rib portion; a first metal electrode electrically connected to the first highly doped region located outside the P-type slab region on which the first thin film is formed; 1. An optical transmitter comprising:

[0092] (Supplementary Note 17) The optical modulator element comprises: a second thin film formed on the N-type slab region and having an electron affinity different from that of a material of the N-type slab region; a second highly doped region of the N-type slab region spaced from the rib portion; a second metal electrode electrically connected to the second highly doped region located outside the N-type slab region on which the second thin film is formed; 17. The optical transmitter according to claim 16, further comprising:

[0093] (Appendix 18) An optical modulator element that optically modulates light using a transmission signal and transmits a transmission light; an optical receiver element for receiving a received signal from the received light using light; An optical transceiver having: The optical modulator element includes: a rib type optical waveguide having a rib portion having a PN junction, a P-type slab region continuous with the P-type region of the rib portion, and an N-type slab region continuous with the N-type region of the rib portion; a first thin film formed on the P-type slab region and having an electron affinity different from that of a material of the P-type slab region; a first highly doped region of the P-type slab region spaced from the rib portion; a first metal electrode electrically connected to the first highly doped region located outside the P-type slab region on which the first thin film is formed; 1. An optical transceiver comprising:

[0094] (Supplementary Note 19) The optical modulator element comprises: a second thin film formed on the N-type slab region and having an electron affinity different from that of a material of the N-type slab region; a second highly doped region of the N-type slab region spaced from the rib portion; a second metal electrode electrically connected to the second highly doped region located outside the N-type slab region on which the second thin film is formed; 19. The optical transceiver of claim 18, further comprising: [Explanation of symbols]

[0095] 1 Optical modulator element 2 Rib-type waveguide 3A First metal electrode 3B Second metal electrode 11 Rib section 11A P type region 11B N-type region 12A P-type slab area 12A3 P++ area 12B N-type slab region 12B3 N++ area 17A First Gap Region 17B Second gap region 18A Third Gap Region 18B Fourth Gap Region 22 Covering layer 50 Optical Transceiver 54 Optical Modulator Element 56 Optical receiver element

Claims

1. a rib type optical waveguide having a rib portion having a PN junction, a P-type slab region continuous with the P-type region of the rib portion, and an N-type slab region continuous with the N-type region of the rib portion; a first thin film formed on the P-type slab region and having an electron affinity different from that of a material of the P-type slab region; a first highly doped region of the P-type slab region spaced from the rib portion; a first metal electrode electrically connected to the first highly doped region located outside the P-type slab region on which the first thin film is formed; An optical modulator element comprising:

2. The first thin film comprises:

2. An optical modulator element according to claim 1, wherein said first metal electrode is formed on said P-type slab region across a gap.

3. The first thin film comprises:

2. An optical modulator element according to claim 1, further comprising a material having a smaller electron affinity than the material of said P-type slab region.

4. 2. The optical modulator element according to claim 1, wherein the first thin film is in an undoped state, that is, is not intentionally doped.

5. The first thin film comprises:

2. The optical modulator element according to claim 1, wherein the rib portion is formed on the P-type slab region with a gap therebetween from a sidewall of the rib portion.

6. 2. The optical modulator element of claim 1, wherein at least a portion of said first thin film is formed on said first highly doped region.

7. a second thin film formed on the N-type slab region and having an electron affinity different from that of a material of the N-type slab region; a second highly doped region of the N-type slab region spaced from the rib portion; a second metal electrode electrically connected to the second highly doped region located outside the N-type slab region on which the second thin film is formed; 2. The optical modulator element according to claim 1, further comprising:

8. the rib-type optical waveguide comprises silicon; 8. The optical modulator element according to claim 7, wherein the first thin film and the second thin film contain germanium.

9. 9. The optical modulator element according to claim 8, wherein the first thin film and the second thin film are made of silicon-germanium having a germanium composition ratio of at least 0.2 to 0.

4.

10. 1. An optical transmitter having an optical modulator element that optically modulates light using a transmission signal and transmits transmission light, The optical modulator element includes: a rib type optical waveguide having a rib portion having a PN junction, a P-type slab region continuous with the P-type region of the rib portion, and an N-type slab region continuous with the N-type region of the rib portion; a first thin film formed on the P-type slab region and having an electron affinity different from that of a material of the P-type slab region; a first highly doped region of the P-type slab region spaced from the rib portion; a first metal electrode electrically connected to the first highly doped region located outside the P-type slab region on which the first thin film is formed; 1. An optical transmitter comprising:

11. an optical modulator element that optically modulates light using a transmission signal and transmits the transmission light; an optical receiver element for receiving a received signal from the received light using light; An optical transceiver having: The optical modulator element includes: a rib type optical waveguide having a rib portion having a PN junction, a P-type slab region continuous with the P-type region of the rib portion, and an N-type slab region continuous with the N-type region of the rib portion; a first thin film formed on the P-type slab region and having an electron affinity different from that of a material of the P-type slab region; a first highly doped region of the P-type slab region spaced from the rib portion; a first metal electrode electrically connected to the first highly doped region located outside the P-type slab region on which the first thin film is formed; 1. An optical transceiver comprising:

Citation Information

Patent Citations

  • Apparatus and method for a silicon modulator with strong gradient slab doping

    US20220026747A1

  • Methods to improve modulation efficiency in silicon optical modulator

    US20220187635A1

  • Carrier depletion-based silicon photonic modulator using capacitive coupling

    US20220252911A1