Laser light source and manufacturing method of the same

The laser light source design with non-metallic support members and strategic metal films enhances heat utilization and bonding reliability, enabling higher output levels by addressing inefficiencies in existing technologies.

JP2024154537APending Publication Date: 2024-10-31NICHIA CORP +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023068396
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-19
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing laser light sources do not achieve high output levels due to inefficiencies in heat utilization and potential damage from excessive heat application during bonding processes.

Method used

A laser light source design featuring a support member made of non-metallic material with strategically placed metal films on its surfaces to enhance heat utilization efficiency and prevent bonding material scattering, using a method that includes irradiating specific surfaces with a heating laser beam to melt or sinter the bonding material.

Benefits of technology

The design allows for increased output capabilities while minimizing heat-related damage, ensuring reliable bonding and improved heat dissipation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154537000001_ABST
    Figure 2024154537000001_ABST
Patent Text Reader

Abstract

To provide a laser light source which is suitable for increasing the output, and to provide a manufacturing method of the laser light source.SOLUTION: A laser light source includes: a sub mount having a major surface; a semiconductor laser element supported by the major surface of the sub mount and having an end surface from which a laser beam is emitted; an optical member which is disposed facing the end surface of the semiconductor laser element; a support member supported by the major surface of the sub mount and supporting the optical member; and a joint member which joins the support member and the optical member to each other. The support member has: a body formed of a non-metal material and having a front surface joined to the optical member through the joint member, a back surface opposite to the front surface, a lower surface supported by the sub mount, an upper surface opposite to the lower surface, and two side surfaces intersecting with the front surface, the back surface, the lower surface, and the upper surface; and a first metal film provided on the upper surface.SELECTED DRAWING: Figure 1A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a laser light source and a method for manufacturing the same. [Background technology]

[0002] Patent Document 1 discloses a laser light source having an edge-emitting semiconductor laser element, a lens member, a lens support that supports the lens member, and a submount that supports the semiconductor laser element. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] International Publication No. 2021 / 131171 Summary of the Invention [Problem to be solved by the invention]

[0004] There is a demand for laser light sources with even higher output.

[0005] The present disclosure provides a laser light source suitable for achieving high output and a method for manufacturing such a laser light source. [Means for solving the problem]

[0006] In an exemplary embodiment, a laser light source of the present disclosure comprises a submount having a main surface, a semiconductor laser element supported on the main surface of the submount and having an end surface that emits a laser beam, an optical member arranged opposite the end surface of the semiconductor laser element, a support member supported on the main surface of the submount and supporting the optical member, and a joining member joining the support member and the optical member, wherein the support member is a main body formed of a non-metallic material and has a front surface joined to the optical member via the joining member, a back surface opposite the front surface, a bottom surface supported by the submount, an top surface opposite the bottom surface, and two side surfaces intersecting the front surface, the back surface, the bottom surface, and the top surface, and a first metal film provided on the top surface.

[0007] In an exemplary embodiment, a manufacturing method of a laser light source disclosed herein includes the steps of preparing a submount to which a semiconductor laser element and a support member are bonded, and an optical member, and bonding the optical member to the support member, wherein the support member is a main body formed of a non-metallic material and has a front surface bonded to the optical member, a back surface opposite the front surface, a bottom surface bonded to the submount, an upper surface opposite the bottom surface, and two side surfaces intersecting the front surface, the back surface, the bottom surface, and the upper surface, a first metal film provided on the top surface, and a second metal film provided on one of the back surface or the side surfaces, and the step of bonding the optical member to the support member includes irradiating the other of the back surface or the side surface on which the second metal film is not provided with laser light, and melting or sintering a bonding material arranged between the optical member and the support member. Effect of the Invention

[0008] According to the embodiments of the present disclosure, a laser light source suitable for achieving high output and a method for manufacturing the same are provided. [Brief description of the drawings]

[0009] [Figure 1A]FIG. 1A is an exploded perspective view illustrating a schematic configuration example of a laser light source according to an exemplary embodiment of the present disclosure. [Figure 1B] FIG. 1B is a schematic diagram for explaining a method for manufacturing a laser light source according to an exemplary embodiment of the present disclosure. [Figure 1C] FIG. 1C is an exploded perspective view that illustrates a schematic configuration example of a laser light source according to an exemplary embodiment of the present disclosure. [Figure 1D] FIG. 1D is a perspective view that illustrates a schematic configuration example of a support member included in a laser light source according to an exemplary embodiment of the present disclosure. [Figure 1E] FIG. 1E is a diagram illustrating a schematic configuration example of a support member included in a laser light source according to an exemplary embodiment of the present disclosure. [Diagram 2] FIG. 2 is an exploded perspective view that illustrates a schematic configuration example of a laser light source according to an exemplary embodiment of the present disclosure. [Figure 3A] FIG. 3A is a diagram illustrating a schematic configuration example of a support member included in a laser light source according to an exemplary embodiment of the present disclosure. [Figure 3B] FIG. 3B is a diagram illustrating a schematic configuration example of a support member included in a laser light source according to an exemplary embodiment of the present disclosure. [Figure 4A] FIG. 4A is an exploded perspective view that illustrates a schematic configuration example of a laser light source according to an exemplary embodiment of the present disclosure. [Figure 4B] FIG. 4B is a diagram illustrating a schematic configuration example of a support member included in a laser light source according to an exemplary embodiment of the present disclosure. [Figure 4C] FIG. 4C is a schematic diagram for explaining a method for manufacturing a laser light source according to an exemplary embodiment of the present disclosure. [Diagram 5] FIG. 5 is a diagram illustrating a schematic configuration example of a support member included in a laser light source according to an exemplary embodiment of the present disclosure. [Figure 6] FIG. 6 is an exploded perspective view illustrating a schematic configuration example of a laser light source according to an exemplary embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, a light emitting device according to an embodiment of the present disclosure will be described with reference to the drawings. Parts having the same reference numerals appearing in multiple drawings indicate the same or equivalent parts.

[0011] The following are examples to embody the technical ideas of the present invention, and the present invention is not limited to the following. Furthermore, the description of the size, material, shape, relative arrangement, etc. of components is intended to be illustrative, and not to limit the scope of the present invention. The size and positional relationship of the components shown in each drawing may be exaggerated to make it easier to understand.

[0012] In addition, in this specification or claims, when there are multiple elements that correspond to a certain element and each element needs to be expressed separately, the elements may be distinguished by adding "first" or "second" to the beginning of the element. If the objects or viewpoints distinguished between this specification and the claims are different, the same addition may not refer to the same object between this specification and the claims.

[0013] [Laser light source] (Embodiment 1) An example of a laser light source according to the first embodiment of the present disclosure will be described with reference to Fig. 1A. Fig. 1A is a schematic exploded perspective view showing an example of the configuration of a laser light source 100A according to the first embodiment of the present disclosure.

[0014] As shown in FIG. 1A, the laser light source 100A includes a submount 10, a semiconductor laser element 20, an optical member 40, a support member 30A, and a bonding member 52 that bonds the support member 30A and the optical member 40. The submount 10 has a main surface 10s1. The semiconductor laser element 20 is supported on the main surface 10s1 of the submount 10, and has an end surface 20e that emits a laser beam. The optical member 40 is disposed opposite the end surface 20e of the semiconductor laser element 20. The support member 30A is supported on the main surface 10s1 of the submount 10, and supports the optical member 40. The support member 30A has a main body 32 formed of a nonmetallic material, and a first metal film 34a. The body 32 of the support member 30A has a front surface 32f bonded to the optical member 40 via the bonding member 52, a back surface 32r opposite the front surface 32f, a bottom surface 32b supported by the submount 10, a top surface 32t opposite the bottom surface 32b, and two side surfaces 32s1 and 32s2 intersecting the front surface 32f, the back surface 32r, the bottom surface 32b, and the top surface 32t. The first metal film 34a is provided on the top surface 32t of the body 32. The body 32 of the support member 30A is formed from a nonmetallic material that transmits, scatters, or absorbs light, for example, from ceramics.

[0015] The reason why the laser light source 100A is suitable for high output will be described while explaining the manufacturing method of the laser light source 100A. Figure 1B is a schematic diagram for explaining the manufacturing method of the laser light source 100A.

[0016] First, the submount 10 to which the semiconductor laser element 20 and the support member 30A are bonded, and the optical member 40 are prepared.

[0017] 1B, the optical member 40 and the support member 30A are joined together. The white arrows in FIG. 1B diagrammatically represent the direction of incidence of a heating laser beam (hereinafter, referred to as "heating laser beam"). In the process of joining the support member 30A and the optical member 40, for example, the side surfaces 32s1 and 32s2 of the main body 32 of the support member 30A are irradiated with the heating laser beam. As a result, heat is transferred to the joining material disposed between the front surface 32f of the main body 32 and the optical member 40 via the main body 32, and the joining material is melted or sintered to form a joining member 52 that joins the support member 30A and the optical member 40.

[0018] In a high-power laser light source, the submount supporting the support member needs to have high heat dissipation. However, if the submount has high heat dissipation, when the heating laser light is irradiated, heat dissipation from the support member via the submount is promoted, and the heat utilization efficiency of the heating laser light in the bonding process between the optical member and the support member is reduced. If the output of the heating laser light is increased to compensate for the reduction in the heat utilization efficiency of the heating laser light, excessive heat may be applied to the bonding material, causing the bonding material to bump. If the bonding material bumps, it may scatter and adhere to the optical member. If the bonding material adheres to the position of the optical member where the laser light emitted from the semiconductor laser element 20 is irradiated, the bonding material may absorb the laser light, generate heat, and burn the optical member. In contrast, the laser light source 100A has a first metal film 34a on the support member 30A, and as described below, the heat utilization efficiency of the heating laser light can be improved. Therefore, even if a submount 10 with high heat dissipation properties is used, the support member 30A and the optical member 40 can be bonded while suppressing an increase in the output of the heating laser light. Since an increase in the output of the heating laser light is suppressed, scattering of the bonding material is suppressed. Since the laser light source 100A can use a submount 10 with high heat dissipation properties, it is possible to increase the output and is suitable for high output.

[0019] When the heating laser light is irradiated, the heating laser light is scattered on the surface of the main body 32, which may reduce the heat utilization efficiency of the heating laser light in the process of joining the optical member 40 and the support member 30A. If the main body 32 is made of alumina, for example, the heating laser light is scattered by crystal grain boundaries formed on the surface. Since the support member 30A has the first metal film 34a, the heating laser light scattered on the surface of the main body 32 can be absorbed by the first metal film 34a. Therefore, the utilization efficiency of the heat transferred from the heating laser light to the joining material is improved.

[0020] The first metal film 34a may be a single layer or may have a laminated structure including a plurality of layers. When the first metal film 34a is a single layer, the first metal film 34a is preferably formed of a metal having a high absorptivity of the heating laser light. For example, the absorptivity of the heating laser light is preferably 50% or more, more preferably 60% or more, and even more preferably 70% or more. When the absorptivity of the heating laser light is high, the effect of improving the utilization efficiency of the heat transferred from the heating laser light to the joining material is high. For example, when a YAG laser light source (wavelength 1064 nm) is used as the light source for emitting the heating laser light, the first metal film 34a is preferably formed of, for example, Ti. This is because Ti has a high absorptivity of the YAG laser light and can improve the utilization efficiency of the heat. Note that the heating laser light absorbed by the first metal film 34a is converted into heat, so even if the first metal film 34a is formed of a metal having a low absorptivity of the heating laser light, the utilization efficiency of the heat transferred from the heating laser light to the joining material can be improved compared to the case where the first metal film 34a is not provided. When the first metal film 34a includes a plurality of layers, the layer closest to the main body 32 is preferably formed of a metal having a high absorptivity of the heating laser beam. For example, the first metal film 34a may have a laminated structure including a Ti film. The first metal film 34a may have a laminated structure (Ti / Pd / Au) formed by laminating Ti, Pd, and Au in this order. Such a first metal film 34a may include, in order from the main body 32 side, a Ti film, a Pd film, and an Au film. Alternatively, the first metal film 34a may have a laminated structure (Ti / Pt / Au) formed by laminating Ti, Pt, and Au in this order. Such a first metal film 34a may include, in order from the main body 32 side, a Ti film, a Pt film, and an Au film. When the first metal film 34a includes a plurality of layers, it may have a layer of Cr, Ti, Ni, or the like as a base layer (layer on the main body 32 side) and a layer of Pt, Pd, Ru, or the like as an intermediate layer. The material of the first metal film 34a is not limited to the above example, and may be appropriately selected depending on, for example, the wavelength of the heating laser light.

[0021] In the manufacturing process of the laser light source 100A, the power density of the heating laser light irradiated in the process of joining the optical member 40 and the support member 30A is, for example, 10 kW / cm 2 More than 10000kW / cm 2 The irradiation time of the heating laser light may be, for example, 1 ms or more and 50 ms or less. The wavelength of the heating laser light is not particularly limited, and ultraviolet light, blue light, green light, red light, infrared light, etc. may be used. For example, a YAG laser light source (wavelength 1064 nm) may be used as a light source for emitting the heating laser light. In addition, when the side surfaces 32s1 and 32s2 of the support member 30A are irradiated with the heating laser light, as shown by the thick arrow in FIG. 1B, the support member 30A and the optical member 40 are pressed from opposite directions along one axis parallel to the optical axis (dotted line) of the laser light L1 emitted from the end surface 20e of the semiconductor laser element 20, thereby bonding the support member 30A and the optical member 40 via the bonding member 52.

[0022] The first metal film 34a is formed by, for example, a physical deposition method (for example, sputtering or vapor deposition). The first metal film 34a may be formed by plating. The thickness of the first metal film 34a is, for example, 0.5 μm or more and 10 μm or less. For example, if the thickness of the first metal film 34a is less than 0.5 μm, the first metal film 34a may not be formed uniformly depending on the surface condition of the main body 32 of the support member 30A. From the viewpoint of reducing manufacturing costs, it is preferable that the thickness of the first metal film 34a is small.

[0023] An example of the shape of the main body 32 of the support member 30A will be described with reference to FIG. 1C, FIG. 1D, and FIG. 1E. FIG. 1C is a schematic exploded perspective view showing an example of the configuration of the laser light source 100A, and is a perspective view seen from the front surface 32f side of the main body 32 of the support member 30A. FIG. 1D is a perspective view of the support member 30A seen from the rear surface 32r side of the main body 32. FIG. 1E is a diagram showing each surface of the support member 30A. As shown in FIG. 1C and FIG. 1D, the main body 32 of the support member 30A includes a pair of columnar parts 32A1 and 32A2, and a connecting part 32B that connects the upper parts of the pair of columnar parts 32A1 and 32A2. The dashed line shown in FIG. 1D represents an example of the boundary between the pair of columnar parts 32A1 and 32A2 and the connecting part 32B. The front surface 32f of the main body 32 of the support member 30A includes the front surfaces 32A1f and 32A2f of the pair of columnar portions 32A1 and 32A2 and the front surface 32Bf of the connecting portion 32B, as shown in FIG. 1C. The back surface 32r of the main body 32 includes the back surfaces 32A1r and 32A2r of the pair of columnar portions 32A1 and 32A2 and the back surface 32Br of the connecting portion 32B, as shown in FIG. 1D. The lower surface 32b of the main body 32 includes the lower surfaces 32A1b and 32A2b of the pair of columnar portions 32A1 and 32A2. The upper surface 32t of the main body 32 includes the upper surfaces 32A1t and 32A2t of the pair of columnar portions 32A1 and 32A2 and the upper surface 32Bt of the connecting portion 32B, as shown in FIG. 1D. The two side surfaces 32s1 and 32s2 (see FIG. 1A) of the main body 32 include outer surfaces 32A1so and 32A2so of a pair of columnar portions 32A1 and 32A2, as shown in FIGS. 1C and 1D.

[0024] As shown in FIG. 1C, the support member 30A further includes a metal film 34e (sometimes referred to as a "fifth metal film 34e") provided on the front surface 32f of the main body 32. The fifth metal film 34e may be provided between the support member 30A and a joining member 52 for joining the support member 30A and the optical member 40. In such a case, the fifth metal film 34e improves the joining strength between the support member 30A and the optical member 40. The fifth metal film 34e may be formed by a method similar to that of the first metal film 34a described above. The fifth metal film 34e may cover half or more of the area of ​​the front surface 32f of the main body 32. The fifth metal film 34e may be provided only in an area of ​​the front surface 32f of the main body 32 including a portion to be joined to the optical member 40.

[0025] The fifth metal film 34e has a laminated structure (Ti / Pd / Au) formed by laminating, for example, Ti, Pd, and Au in this order. When the first metal film 34a is formed of Ti, the Ti layer constituting the fifth metal film 34e is formed from the same Ti film as the Ti film for forming the first metal film 34a. The fifth metal film 34e is obtained by further laminating a Pd layer and an Au layer in this order on the Ti layer. In such a case, the manufacturing process and manufacturing costs can be reduced.

[0026] Alternatively, the fifth metal film 34e may be formed of a metal different from that of the first metal film 34a. When the fifth metal film 34e includes a plurality of layers, the layer closest to the main body 32 may be formed of a metal having a lower absorptance of the heating laser light than the first metal film 34a, or a metal having a higher reflectance of the heating laser light than the first metal film 34a. In such a case, in the bonding process between the optical member 40 and the support member 30A, the heat input to the entire support member 30A can be increased, but the heating laser light is difficult to be absorbed by the fifth metal film 34e or is easily reflected by the fifth metal film 34e, so that the sudden heat input to the bonding material can be suppressed. Therefore, the bonding material can be suppressed from being excessively heated and scattering. In addition, by providing a metal film on a surface that is not irradiated with the heating laser light and / or a surface that does not contribute to bonding with other members, such as the first metal film 34a, the heat is easily absorbed by a surface other than the front surface 32f of the main body 32, and the effect of suppressing the heat input to the bonding material is improved. Examples of metals with low absorptance of heating laser light (or metals with high reflectance of heating laser light) include Al and Ni when a YAG laser light source (wavelength 1064 nm) is used as a light source for emitting heating laser light. The fifth metal film 34e may have a laminated structure (Al / Pd / Au) formed by laminating Al, Pd, and Au in this order, or a laminated structure (Ni / Pd / Au) formed by laminating Ni, Pd, and Au in this order. When the fifth metal film 34e is a single layer, the fifth metal film 34e may be made of a metal with a lower absorptance of heating laser light than the first metal film 34a, or a metal with a higher reflectance of heating laser light than the first metal film 34a.

[0027] 1E, the support member 30A further has a metal film 34f (sometimes referred to as "sixth metal film 34f") provided on the lower surfaces 32A1b and 32A2b of the pair of columnar portions 32A1 and 32A2. The sixth metal film 34f may be provided between the support member 30A and the submount 10. The support member 30A and the submount 10 are joined by a joining member, and the sixth metal film 34f improves the joining strength between the support member 30A and the submount 10. The joining member for joining the support member 30A and the submount 10 may be formed from the same material as the joining member 52.

[0028] The sixth metal film 34f may be formed by the same method and with the same material as the first metal film 34a described above. The sixth metal film 34f may be formed of the same material as the fifth metal film 34e and may have the same layered structure as the fifth metal film 34e, for example.

[0029] The area and shape of the sixth metal film 34f are not limited to the example in which it is formed on a part of the lower surfaces 32A1b and 32A2b of the pair of columnar parts 32A1 and 32A2, and may be appropriately changed. The sixth metal film 34f may be provided on almost the entire surface of the lower surfaces 32A1b and 32A2b of the pair of columnar parts 32A1 and 32A2. When the area of ​​the sixth metal film 34f is small, when the heating laser light is irradiated, heat dissipation to the submount 10 is suppressed, so that the decrease in the efficiency of heat transfer from the heating laser light to the bonding material is suppressed. However, if the area of ​​the sixth metal film 34f is too small compared to the area of ​​the lower surfaces 32A1b and 32A2b of the pair of columnar parts 32A1 and 32A2, the bonding strength between the support member 30A and the submount 10 may not be sufficient, so the area of ​​the sixth metal film 34f is preferably large enough to obtain the bonding strength between the support member 30A and the submount 10. For example, the area of ​​the sixth metal film 34f provided on the lower surface 32A1b or 32A2b is preferably 70% or more of the area of ​​the lower surface 32A1b or 32A2b, respectively.

[0030] In the first embodiment, the front surface 32f and the back surface 32r of the main body 32 of the support member 30A are parallel to the XY plane, the lower surface 32b and the upper surface 32t of the main body 32 of the support member 30A are parallel to the XZ plane, and the two side surfaces 32s1 and 32s2 of the main body 32 of the support member 30A are parallel to the YZ plane. Therefore, the front surfaces 32A1f and 32A2f of the pair of columnar parts 32A1 and 32A2, the front surface 32Bf of the connecting part 32B, the back surfaces 32A1r and 32A2r of the pair of columnar parts 32A1 and 32A2, and the back surface 32Br of the connecting part 32B are parallel to the XY plane. The lower surfaces 32A1b and 32A2b of the pair of columnar parts 32A1 and 32A2, the lower surface 32Bb of the connecting part 32B, the upper surfaces 32A1t and 32A2t of the pair of columnar parts 32A1 and 32A2, and the upper surface 32Bt of the connecting part 32B are surfaces parallel to the XZ plane. The outer side surfaces 32A1so and 32A2so of the pair of columnar parts 32A1 and 32A2 are surfaces parallel to the YZ plane. The inner side surfaces 32A1si and 32A2si of the pair of columnar parts 32A1 and 32A2 are also surfaces parallel to the YZ plane. However, the illustrated example is merely one example of the support member of the laser light source according to the embodiment of the present disclosure, and the shape of the support member may be changed as appropriate.

[0031] In the laser light source 100A, the first metal film 34a is formed only on a part of the upper surface 32t of the main body 32 of the support member 30A. In this example, the first metal film 34a is provided on at least the upper surfaces 32A1t and 32A2t of the pair of columnar parts 32A1 and 32A2. In this example, no metal film is provided on the upper surface 32Bt of the connecting part 32B. The area and shape of the first metal film 34a are not limited to the example in which the first metal film 34a is formed on a part of the upper surfaces 32A1t and 32A2t of the pair of columnar parts 32A1 and 32A2, and may be changed as appropriate. It is preferable that the first metal film 34a is formed in a region including a region close to the position (here, two side surfaces 32s1 and 32s2 of the main body 32) of the upper surface 32t of the main body 32 where the heating laser light is irradiated, of the upper surface 32t of the main body 32. For example, a metal film is formed on almost the entire surface of the upper surface 32t of the main body 32 by physical deposition, and then the metal film is patterned into a desired shape to obtain the first metal film 34a formed only on a part of the upper surface 32t. Alternatively, the first metal film 34a may be formed by forming the metal film only on a desired region of the upper surface 32t of the main body 32 using a mask or the like. From the viewpoint of improving the thermal utilization efficiency of the heating laser light, the area of ​​the first metal film 34a is, for example, 20% or more of the area of ​​the upper surface 32t, and preferably, for example, 50% or more.

[0032] FIG. 2 is an exploded perspective view showing a schematic diagram of another example of the configuration of the laser light source according to the present embodiment. The laser light source 100A1 shown in FIG. 2 is different from the laser light source 100A having the support member 30A in that the first metal film 34a provided on the upper surface 32t of the main body 32 of the support member 30A1 is formed so as to cover almost the entire surface of the upper surface 32t. The laser light source 100A1 is suitable for high output for the same reason as the laser light source 100A. Since the area of ​​the first metal film 34a of the laser light source 100A1 is larger than that of the laser light source 100A, the laser light source 100A1 can improve the heat utilization efficiency of the heating laser light more effectively than the laser light source 100A.

[0033] (Embodiment 2) An example of a support member of a laser light source according to embodiment 2 of the present disclosure will be described with reference to FIG. 3A. FIG. 3A is a diagram showing each surface of a support member 30B of a laser light source according to embodiment 2. The exploded perspective view of the laser light source according to embodiment 2 seen from the optical member 40 side is the same as the exploded perspective view of the laser light source 100A shown in FIG. 1A, and is therefore omitted from the illustration. As shown in FIG. 3A, the support member 30B is different from the support member 30A of the laser light source 100A in that it further has a second metal film 34b1 provided on the rear surface 32r of the main body 32. The second metal film 34b1 can be formed by the same method and from the same material as the first metal film 34a described above.

[0034] A laser light source having the support member 30B is suitable for high output for the same reason as the laser light source 100A. In the laser light source having the support member 30B, the support member 30B has a second metal film 34b1 in addition to the first metal film 34a, so that the heat utilization efficiency of the heating laser light can be further improved. Here, no metal film is provided on the side surfaces 32s1 and 32s2 of the main body 32 to which the heating laser light is irradiated. The second metal film 34b1 may be provided on at least a part of the back surface 32r of the main body 32. In this example, the second metal film 34b1 is provided on at least the back surfaces 32A1r and 32A2r of the pair of columnar parts 32A1 and 32A2, and no metal film is provided on the back surface 32Br of the connecting part 32B.

[0035] The area and shape of the second metal film 34b1 may be changed as appropriate. For example, the second metal film 34b1 may cover more than half of the area of ​​the back surface 32r of the main body 32. That is, the area of ​​the second metal film 34b1 may be more than 50% of the area of ​​the back surface 32r. The second metal film 34b1 is preferably formed in a region of the back surface 32r of the main body 32 that includes a region close to the position where the heating laser light is irradiated (here, the two side surfaces 32s1 and 32s2 of the main body 32). Alternatively, as in the example shown in FIG. 3B, the second metal film 34b1 may be formed on almost the entire surface of the back surface 32r.

[0036] (Embodiment 3) An example of a laser light source according to the third embodiment of the present disclosure will be described with reference to FIGS. 4A and 4B. FIG. 4A is a schematic exploded perspective view showing a configuration example of a laser light source 100C according to the third embodiment. FIG. 4B is a diagram showing each surface of a support member 30C of the laser light source 100C. The support member 30C has a second metal film 34b2 provided on two side surfaces 32s1 and 32s2 of the main body 32, instead of the second metal film 34b1 provided on the back surface 32r of the support member 30B. In the illustrated example, the second metal film 34b2 is provided on the outer side surfaces 32A1so and 32A2so of a pair of columnar parts 32A1 and 32A2. The second metal film 34b2 can be formed by the same method and with the same material as the first metal film 34a described above.

[0037] FIG. 4C is a schematic top view for explaining the manufacturing method of the laser light source 100C. As described above, in the manufacturing method of the laser light source 100A according to the first embodiment, in the step of joining the optical member 40 and the support member 30A, the side surfaces 32s1 and 32s2 of the support member 30A are irradiated with a heating laser beam to melt or sinter the bonding material arranged between the optical member 40 and the support member 30A. In contrast, the manufacturing method of the laser light source 100C according to the present embodiment is different from the manufacturing method of the laser light source 100A in that, in the step of joining the optical member 40 and the support member 30C, the back surface 32r of the support member 30C is irradiated with a heating laser beam to melt or sinter the bonding material arranged between the optical member 40 and the support member 30C, as shown in FIG. 4C. The white arrow shown in FIG. 4C typically indicates the incident direction of the heating laser beam. In this example, the heating laser light is irradiated onto rear surfaces 32A1r and 32A2r of a pair of columnar portions 32A1 and 32A2.

[0038] The laser light source 100C is suitable for high output for the same reasons as the laser light source 100A.

[0039] In the laser light source 100C manufactured by the above-mentioned manufacturing method, it is preferable that the support member 30C does not have a metal film on the back surface 32r of the main body 32 irradiated with the heating laser light. In this example, as shown in Fig. 4B, the back surfaces 32A1r and 32A2r of the pair of columnar parts 32A1 and 32A2 irradiated with the heating laser light are not provided with a metal film. In this case, the back surface 32Br of the connecting part 32B, which is not irradiated with the heating laser light, may be provided with a metal film.

[0040] The area and shape of the second metal film 34b2 may be changed as appropriate. The second metal film 34b2 may be provided on at least a part of one of the side surfaces 32s1 and 32s2 of the main body 32.

[0041] (Embodiment 4) With reference to FIG. 5, an example of a support member included in a laser light source according to embodiment 4 of the present disclosure will be described. FIG. 5 is a diagram showing each surface of a support member 30D included in a laser light source according to embodiment 4. The exploded perspective view of the laser light source according to embodiment 4 seen from the optical member 40 side is the same as the exploded perspective view of the laser light source 100A shown in FIG. 1A, and therefore is not shown. As shown in FIG. 5, the support member 30D is different from the support member 30A included in the laser light source 100A in that it further includes a third metal film 34c provided on the lower surface 32Bb of the connecting portion 32B. The third metal film 34c can be formed by the same method and from the same material as the first metal film 34a described above. A laser light source including the support member 30D is manufactured by the same method as the laser light source 100A. A laser light source including the support member 30D is suitable for high output for the same reason as the laser light source 100A.

[0042] (Embodiment 5) An example of a laser light source according to the fifth embodiment of the present disclosure will be described with reference to FIG. 6. FIG. 6 is an exploded perspective view showing a laser light source 100E according to the fifth embodiment. The support member 30E of the laser light source 100E is different from the support member 30A of the laser light source 100A in that the support member 30E further includes a fourth metal film 34d provided on the inner side surfaces 32A1si and 32A2si of the pair of columnar parts 32A1 and 32A2. The fourth metal film 34d can be formed by the same method and from the same material as the first metal film 34a described above. The laser light source having the support member 30E is manufactured by the same method as the laser light source 100A. The laser light source having the support member 30E is suitable for high output for the same reasons as the laser light source 100A.

[0043] The above-mentioned embodiments 1 to 5 may be combined as appropriate.

[0044] The support member of the laser light source of the present disclosure has a metal film (including a first metal film provided on the upper surface) provided on at least one of the surfaces of the body formed from a nonmetallic material other than the surface irradiated with the heating laser light and the surface bonded to another member. By having such a metal film, the efficiency of heat utilization of the heating laser light is improved. Specifically, the metal film for improving the efficiency of heat utilization of the heating laser light is provided on at least a part of the surfaces of the body of the support member, such as the front surface bonded to the optical member, the back surface opposite the front surface, the bottom surface facing the submount, the top surface opposite the bottom surface, and two side surfaces, excluding the surface irradiated with the heating laser light (side surface or back surface) and the surface bonded to another member (front surface and bottom surface). The total area of ​​such metal films is preferably large from the viewpoint of improving the efficiency of heat utilization transmitted from the heating laser light to the bonding material. On the other hand, the surfaces (front surface and bottom surface) bonded to another member among the surfaces of the body of the support member are provided with a metal film for bonding the support member to the other member. The area of ​​the metal film for joining the support member to another member is preferably small within a range in which the joining strength with the other member is ensured. At least the surface (side or back) of the main body of the support member that is irradiated with the heating laser light is not provided with the metal film, and the surface of the main body made of a nonmetallic material is exposed.

[0045] The submount 10, the semiconductor laser element 20, the support member 30, the bonding member 52, and the optical member 40 will be described in detail below in terms of materials, shapes, sizes, and the like.

[0046] [Submount 10] The submount 10 may be, for example, a rectangular parallelepiped. A part or the whole of the submount 10 may be formed of at least one selected from the group consisting of AlN, SiC, alumina, CuW, Cu, a laminated structure of Cu / AlN / Cu, diamond, and a metal matrix composite (Metal Matrix Compound: MMC). The MMC includes, for example, at least one selected from the group consisting of Cu, Ag, and Al, and diamond. Alternatively, a part or the whole of the submount 10 may be formed of other common materials. In particular, the submount 10 is preferably formed of AlN or diamond. The thermal conductivity of the submount 10 made of AlN may be, for example, 150 [W / m·K] or more and 230 [W / m·K] or less, and the thermal conductivity of the submount 10 made of diamond may be, for example, 1200 [W / m·K] or more and 2000 [W / m·K] or less. With such a thermal conductivity, the submount 10 can efficiently transfer the heat generated from the semiconductor laser element 20 during operation to a package that houses the laser light source. The thermal expansion coefficient of the submount 10 is, for example, 2×10 -6 [1 / K] or more 2×10 -5 [1 / K] or less. Such a thermal expansion coefficient can suppress deformation of the submount 10 due to heat applied when bonding the semiconductor laser element 20 onto the submount 10 with a bonding material. The size of the submount 10 in the X direction is, for example, 1 mm or more and 3 mm or less, the size in the Y direction is, for example, 0.1 mm or more and 0.5 mm or less, and the size in the Z direction is, for example, 1 mm or more and 6 mm or less. The size of the submount 10 is designed with respect to the size and output of the semiconductor laser element 20. If the size of the semiconductor laser element 20 is increased, the output of the semiconductor laser element 20 will also increase, so it is preferable to increase the size of the submount 10 to improve heat dissipation.

[0047] The submount 10 has a main surface 10s1 parallel to the XZ plane, a bottom surface 10s4 opposite to the main surface 10s1, and a front surface 10s2 located on the optical member 40 side. A metal film having a thickness of, for example, 0.5 μm to 10 μm may be formed on the main surface 10s1 and the bottom surface 10s4 of the submount 10 by plating. The metal film formed on the main surface 10s1 of the submount 10 is useful when bonding the submount 10 and the semiconductor laser element 20 via a bonding member and when supplying power to the semiconductor laser element 20. The metal film formed on the bottom surface 10s4 of the submount 10 is useful when bonding the submount 10 and the base supporting the submount 10 via a bonding member.

[0048] [Semiconductor laser element 20] The semiconductor laser element 20 can emit a violet, blue, green or red laser beam in the visible region, or an infrared or ultraviolet laser beam in the invisible region. The emission peak wavelength of the violet light is preferably in the range of 350 nm to 420 nm, more preferably in the range of 400 nm to 415 nm. The emission peak wavelength of the blue light is preferably in the range of 420 nm to 495 nm, more preferably in the range of 440 nm to 475 nm. The emission peak wavelength of the green light is preferably in the range of 495 nm to 570 nm, more preferably in the range of 510 nm to 550 nm. Examples of laser diodes that emit violet, blue and green laser beams include laser diodes containing nitride semiconductor materials. Examples of nitride semiconductor materials that can be used include GaN, InGaN and AlGaN. The emission peak wavelength of the red light is preferably in the range of 605 nm to 750 nm, more preferably in the range of 610 nm to 700 nm. Examples of laser diodes that emit a red laser beam include laser diodes that include InAlGaP-based, GaInP-based, GaAs-based, and AlGaAs-based semiconductor materials.

[0049] The size of the semiconductor laser element 20 in the X direction may be, for example, 50 μm or more and 500 μm or less, the size in the Y direction may be, for example, 20 μm or more and 150 μm or less, and the size in the Z direction may be, for example, 50 μm or more and 4 mm or less. In face-down mounting, the distance in the Z direction between the end face 20e of the semiconductor laser element 20 and the front face 10s2 of the submount 10 may be, for example, 2 μm or more and 50 μm or less.

[0050] An electrode is provided on each of the upper and lower surfaces of the semiconductor laser element 20. In the above-mentioned semiconductor laminate structure of the semiconductor laser element 20, the electrode electrically connected to the p-type cladding layer is referred to as the "p-side electrode", and the electrode electrically connected to the n-type substrate is referred to as the "n-side electrode". By applying a voltage to the p-side electrode and the n-side electrode to pass a current equal to or greater than a threshold value, the semiconductor laser element 20 emits a laser beam from the end face 20e. The laser beam has a spread, and forms an elliptical far-field pattern (hereinafter referred to as "FFP") on a plane parallel to the end face 20e. The FFP is the shape and light intensity distribution of the emitted light at a position away from the end face 20e. In this light intensity distribution, the 1 / e power of the peak light intensity at the center of the beam is 1 / e 2 Light having an intensity equal to or greater than this is considered to be the main part of the light. e is the base of the natural logarithm.

[0051] The shape of the FFP of the laser beam emitted from the semiconductor laser element 20 is elliptical. In the elliptical shape, the long axis is parallel to the stacking direction of the semiconductor stacked structure, and the short axis is parallel to the extending direction of the end face 20e. The extending direction of the end face 20e is the horizontal direction of the FFP, and the stacking direction is the vertical direction of the FFP.

[0052] Based on the light intensity distribution of the FFP, the angle equivalent to the full width at half maximum of the light intensity distribution is defined as the spread angle of the laser beam emitted from the semiconductor laser element 20. In the FFP, the vertical and horizontal axes are called the fast axis and the slow axis, respectively.

[0053] [Support members 30A to 30E] Support members 30A to 30E are collectively referred to as support member 30. Main body 32 of support member 30 is formed from a nonmetallic material (e.g., ceramics) and may be formed from, for example, AlN, SiC, alumina, glass, Si, zirconia, etc. The size of each of a pair of columnar portions 32A1 and 32A2 of main body 32 in the X direction may be 0.05 mm or more and 1 mm or less, the size in the Y direction may be, for example, 0.5 mm or more and 3 mm or less, and the size in the Z direction may be, for example, 0.2 mm or more and 1 mm or less.

[0054] The thermal conductivity of the body 32 of the support member 30 is, for example, higher than that of the optical member 40 and equal to or lower than that of the submount 10. Due to this relationship in magnitude of thermal conductivity, heat applied to the joining member 52 is easily dissipated to the submount 10 via the body 32, and deterioration of the optical member 40 due to heat can be suppressed. When the lower surface 10s4 of the submount 10 is in contact with a heat sink, the heat of the heating laser light is transferred from the body 32 of the support member 30 to the heat sink via the submount 10. Therefore, in the step of bonding the optical member 40 to the support member 30, the optical member 40 can be bonded to the support member 30 with a good yield.

[0055] [Connecting member 52] The joining member 52 may be formed, for example, from a material that can be sintered. In sintering, metal particles or metal powder are heated at a temperature lower than the melting point of the metal and baked to join the members together. The sintering temperature is lower than the melting point of the metal that constitutes the particles, and may be, for example, 120°C or higher and 300°C or lower. The sintering temperature corresponds to the joining temperature of the joining material.

[0056] The sinterable material may be, for example, a metal paste containing at least one type of metal particles selected from the group consisting of Ag particles, Cu particles, Au particles, and other precious metal particles, and an organic binder. The metal paste containing the organic binder is flexible, so that the position of the optical member 40 can be finely adjusted when the support member 30 and the optical member 40 are joined together.

[0057] If there is no need to fine-tune the position of the optical member 40, the joining member 52 may be made of a material that can be soldered or brazed. In soldering or brazing, the solder material or brazing material is melted by increasing the temperature and solidified by decreasing the temperature, thereby joining the members together. The melting temperature of the solder material may be, for example, 180°C or higher and 300°C or lower. The melting temperature of the brazing material may be, for example, 500°C or higher and 900°C or lower. The melting temperature of the solder material or brazing material corresponds to the joining temperature of the joining material. When the joining member 52 is formed by melting the solder material or brazing material, the joining temperature is higher than when the joining member 52 is formed by sintering a sinterable material, so that the possibility of the joining material bumping and scattering can be reduced.

[0058] The solderable joining material may be, for example, at least one solder material selected from the group consisting of AuSn, SnCu, SnAg, and SnAgCu. The brazable joining material may be, for example, at least one brazing material selected from the group consisting of gold brazing material, tin brazing material, and silver brazing material.

[0059] The thickness of the bonding members 52 (i.e., the length of the bonding members 52 in the Z direction) can be, for example, 1 μm or more and 30 μm or less. This can increase the bonding strength. Also, the bonding can be completed in a short time.

[0060] In the illustrated example, the planar shape of the bonding members 52 (i.e., the shape of the bonding members 52 in the XY plane) is rectangular, but is not limited to a rectangle. The planar shape of the bonding members 52 may be, for example, a circle or an ellipse.

[0061] [Optical member 40] The optical member 40 may be made of at least one light-transmitting material selected from the group consisting of glass, quartz, synthetic quartz, sapphire, and light-transmitting ceramics, or may be made of other common materials.

[0062] The optical member 40 may be a collimating lens such as a fast axis collimating lens (FAC lens) or a slow axis collimating lens (SAC lens). When the optical member 40 is a collimating lens, the collimating lens can be provided at a position close to the end face 20e of the semiconductor laser element 20. As a result, the laser beam emitted from the semiconductor laser element 20 can be collimated before it spreads, so that the optical member 40 can be made compact.

[0063] A metal film may be formed by, for example, plating, vapor deposition, etc. on the surface of the optical member 40 that faces the pair of columnar portions 32A1 and 32A2 of the support member 30. The material of such a metal film may be the same as the material of the first metal film 34a described above.

[0064] The size of the optical member 40 in the X direction may be, for example, equal to the size of the support member 30 in the X direction, or may be larger or smaller than the size of the support member 30 in the X direction. However, the size of the optical member 40 in the X direction is larger than the distance in the X direction between the surfaces where the columnar portion 32A1 and the columnar portion 32A2 of the support member 30 face each other. The maximum size of the optical member 40 in the Y direction may be, for example, 0.2 mm or more and 3 mm or less, and the maximum size in the Z direction may be, for example, 0.2 mm or more and 3 mm or less.

[0065] The present disclosure includes laser light sources and methods for manufacturing laser light sources as described in the following items.

[0066] [Item 1] a submount having a major surface; a semiconductor laser element supported on the main surface of the submount and having an end surface from which a laser beam is emitted; an optical member disposed opposite the end face of the semiconductor laser element; a support member supported by the main surface of the submount and supporting the optical member; a joining member that joins the support member and the optical member; Equipped with The support member is A body formed from a non-metallic material, a front surface joined to the optical member via the joining member; a back surface opposite the front surface; and A lower surface supported by the submount; an upper surface opposite the lower surface; two side surfaces intersecting the front surface, the back surface, the bottom surface, and the top surface; a body having A first metal film provided on the upper surface; A laser light source having a

[0067] [Item 2] The main body includes a pair of columnar portions and a connecting portion that connects upper portions of the pair of columnar portions, The front surface of the main body includes front surfaces of the pair of columnar portions and a front surface of the connecting portion, The rear surface of the main body includes rear surfaces of the pair of columnar portions and a rear surface of the connecting portion, the lower surface of the main body includes lower surfaces of the pair of columnar portions, the upper surface of the main body includes upper surfaces of the pair of columnar portions and an upper surface of the connecting portion, 2. The laser light source according to claim 1, wherein the two side surfaces of the main body include outer surfaces of the pair of columnar portions.

[0068] [Item 3] 3. The laser light source according to item 2, wherein the first metal film is provided on the upper surfaces of at least the pair of columnar portions.

[0069] [Item 4] 3. The laser light source according to claim 2, wherein the support member further has a second metal film provided on the rear surface of the body or the side surface of the body.

[0070] [Item 5] the second metal film is provided on at least the back surfaces of the pair of columnar portions, 5. The laser light source according to item 4, wherein the two side surfaces are not provided with a metal film.

[0071] [Item 6] The second metal film is provided on the two side surfaces, 5. The laser light source according to item 4, wherein a metal film is not provided on the back surfaces of the pair of columnar portions.

[0072] [Item 7] 7. The laser light source according to any one of claims 2 to 6, wherein the support member further has a third metal film provided on a lower surface of the connecting portion and / or a fourth metal film provided on inner surfaces of the pair of columnar portions.

[0073] [Item 8] The support member further includes a fifth metal film provided on the front surface of the body, the first metal film and / or the second metal film is formed of Ti; 8. The laser light source according to any one of items 4 to 7, wherein the fifth metal film has a laminated structure formed by laminating Ti, Pd, and Au in this order.

[0074] [Item 9] The support member further includes a fifth metal film provided on the front surface of the body, 8. The laser light source according to any one of claims 1 to 7, wherein the fifth metal film has a laminated structure formed by laminating Al, Pd, and Au or Ni, Pd, and Au in this order.

[0075] [Item 10] 7. The laser light source according to any one of claims 1 to 6, wherein the area of ​​the first metal film is 20% or more of the area of ​​the top surface of the main body.

[0076] [Item 11] preparing a submount to which a semiconductor laser element and a support member are bonded, and an optical member; a step of joining the optical member and the support member; Equipped with The support member is a body formed of a non-metallic material, a front surface bonded to the optical member; a back surface opposite the front surface; and a lower surface to be bonded to the submount; an upper surface opposite the lower surface; two side surfaces intersecting the front surface, the back surface, the bottom surface, and the top surface; a body having A first metal film provided on the upper surface; A second metal film provided on one of the back surface and the side surface; having A method for manufacturing a laser light source, wherein the process of joining the optical member and the support member includes irradiating the other of the back surface or the side surface on which the second metal film is not provided with laser light, and melting or sintering a joining material arranged between the optical member and the support member.

[0077] [Item 12] the second metal film is provided on the back surface, Item 12. The method for manufacturing a laser light source according to item 11, wherein the step of joining the optical member and the support member includes irradiating the side surface with laser light to melt or sinter the joining material.

[0078] [Item 13] The second metal film is provided on the side surface, Item 12. The method for manufacturing a laser light source according to item 11, wherein the step of joining the optical member and the support member includes irradiating the rear surface with laser light to melt or sinter the joining material. [Industrial Applicability]

[0079] The laser light source and the manufacturing method thereof of the present disclosure can be applied to laser light sources used for various applications such as processing, projectors, displays, and lighting fixtures. [Explanation of symbols]

[0080] 10: submount, 20: semiconductor laser element, 30A to 30E: support member, 32: main body, 34a to 34f: metal films, 40: optical member, 52: joining member, 100A, 100A1, 100C, 100E: laser light source

Claims

1. a submount having a major surface; a semiconductor laser element supported on the main surface of the submount and having an end surface from which a laser beam is emitted; an optical member disposed opposite the end face of the semiconductor laser element; a support member supported by the main surface of the submount and supporting the optical member; a joining member that joins the support member and the optical member; Equipped with The support member is A body formed from a non-metallic material, a front surface joined to the optical member via the joining member; a back surface opposite the front surface; and A lower surface supported by the submount; an upper surface opposite the lower surface; two side surfaces intersecting the front surface, the back surface, the bottom surface, and the top surface; a body having A first metal film provided on the upper surface; A laser light source having a

2. The main body includes a pair of columnar portions and a connecting portion that connects upper portions of the pair of columnar portions, The front surface of the main body includes front surfaces of the pair of columnar portions and a front surface of the connecting portion, The rear surface of the main body includes rear surfaces of the pair of columnar portions and a rear surface of the connecting portion, the lower surface of the main body includes lower surfaces of the pair of columnar portions, the upper surface of the main body includes upper surfaces of the pair of columnar portions and an upper surface of the connecting portion, The laser light source according to claim 1 , wherein the two side surfaces of the main body include outer surfaces of the pair of columnar portions.

3. The laser light source according to claim 2 , wherein the first metal film is provided on the upper surfaces of at least the pair of columnar portions.

4. The laser light source according to claim 2 , wherein the support member further comprises a second metal film provided on the rear surface of the main body or on the side surface of the main body.

5. the second metal film is provided on at least the back surfaces of the pair of columnar portions, The laser light source according to claim 4 , wherein the two side surfaces are not provided with a metal film.

6. the second metal film is provided on the two side surfaces, The laser light source according to claim 4 , wherein no metal film is provided on the rear surfaces of the pair of columnar portions.

7. 7. The laser light source according to claim 2, wherein the support member further has a third metal film provided on a lower surface of the connecting portion and / or a fourth metal film provided on inner surfaces of the pair of columnar portions.

8. The support member further includes a fifth metal film provided on the front surface of the body, the first metal film and / or the second metal film is formed of Ti, The laser light source according to claim 4 , wherein the fifth metal film has a laminated structure formed by laminating Ti, Pd, and Au in this order.

9. The support member further includes a fifth metal film provided on the front surface of the body, The laser light source according to claim 1 , wherein the fifth metal film has a laminated structure formed by laminating Al, Pd, and Au, or Ni, Pd, and Au in this order.

10. The laser light source according to claim 1 , wherein an area of ​​the first metal film is 20% or more of an area of ​​the upper surface of the main body.

11. preparing a submount to which a semiconductor laser element and a support member are bonded, and an optical member; a step of joining the optical member and the support member; Equipped with The support member is a body formed of a non-metallic material, a front surface bonded to the optical member; a back surface opposite the front surface; and a lower surface to be bonded to the submount; an upper surface opposite the lower surface; two side surfaces intersecting the front surface, the back surface, the bottom surface, and the top surface; a body having A first metal film provided on the upper surface; A second metal film provided on one of the back surface and the side surface; having A method for manufacturing a laser light source, wherein the process of joining the optical member and the support member includes irradiating laser light to the other of the back surface or the side surface on which the second metal film is not provided, and melting or sintering a joining material arranged between the optical member and the support member.

12. the second metal film is provided on the back surface, The method for manufacturing a laser light source according to claim 11 , wherein the step of joining the optical member and the support member includes irradiating the side surface with laser light to melt or sinter the joining material.

13. The second metal film is provided on the side surface, The method for manufacturing a laser light source according to claim 11 , wherein the step of joining the optical member and the support member includes irradiating the rear surface with laser light to melt or sinter the joining material.