Electrolytic solvent capable of adjusting dissolution characteristic, and production method and application therefor

The electrolyte solvent with adjustable solubility characteristics addresses dendritic lithium growth and SEI issues in LMBs, improving battery performance and safety by forming a uniform SEI, thus extending cycle life and reducing costs.

JP2024155803AActive Publication Date: 2024-10-31NAT TAIWAN UNIV OF SCI & TECH
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024066385
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-19
Filing Date
2024-04-16
Publication Date
2024-10-31
Estimated Expiration
2044-04-16

AI Technical Summary

Technical Problem

Conventional lithium metal batteries (LMBs) face issues with uncontrollable dendritic lithium growth, irreversibility of lithium plating stripping, and interfacial incompatibility due to solvent-separated ion pairs and poor solid electrolyte interfaces, leading to reduced cycle life and coulombic efficiency.

Method used

Development of an electrolyte solvent with adjustable solubility characteristics, forming a strong and uniform conductive solid electrolyte interface (SEI) on the anode surface, using chemical structures represented by formulas (1), (2), and (3), synthesized through specific reaction steps to enhance solubility adjustment.

Benefits of technology

The electrolyte solvent improves battery performance by controlling lithium growth, enhancing safety during fast charging, and extending the life and reducing costs of lithium batteries, while maintaining high coulombic efficiency and capacity retention.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024155803000001_ABST
    Figure 2024155803000001_ABST
Patent Text Reader

Abstract

To provide an electrolytic solvent that can adjust dissolution characteristics, and its production method and application.SOLUTION: The present invention provides an electrolytic solvent that can adjust dissolution characteristics, including a chemical structure represented by the following formula. (In the formula, A is oxygen, sulfur, selenium, tellurium, or their combination, and B is one, two or three substituted halogens, nitrile groups, nitro groups, nitroso groups, amine groups, or their combination). According to the inventive electrolytic solvent, a solvent abundantly containing anions is adjusted so as to have a satisfactory dissolution action through an electrolyte process, leading to the development and synthesis of a solvent having a weak solubility characteristic, with greatly improved battery performance. The solvent achieves reduced production cost.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an electrolyte solvent, particularly an electrolyte solvent for application in electrochemical devices. The primary application of the electrolyte solvent described in the present invention is in various electrochemical batteries, which will be described and detailed below. However, the present invention is not limited to use in electrochemical batteries, and other applicable electrochemical devices are also within the scope of the present invention. [Background technology]

[0002] Lithium metal batteries (LMBs) have become an important research direction for next-generation electric vehicles and energy storage devices due to their high energy density. However, uncontrollable lithium dendritic growth, irreversible lithium plating delamination, and interface incompatibility quickly result in short cycle life and low coulombic efficiency, hindering the practical application of LMBs.

[0003] In conventional LMBs carbonate-based electrolyte solvents such as carbonate solvents, lithium ions can be dissolved by coordinating with carbonate solvent molecules, but the carbonate solvent contains excess free carbonate solvent, which forms a solvent-separated ion pair (SSIP) and a poor solid electrolyte interface (SEI) of organic oxides on the negative electrode surface, which significantly reduces the performance of the subsequent LMBs. Increasing the concentration of lithium salts and decreasing the free solvent will undoubtedly increase the cost of the electrolyte and cause further problems due to the high concentration of electrolyte.

[0004] In view of this, there is currently an urgent need to be able to solve the problem of electrical losses in electrochemical cells caused by conventional electrolyte solvents containing excessive free solvent. Summary of the Invention [Problem to be solved by the invention]

[0005] In view of this, to solve the above problems and extend the lifespan of LMBs, the most efficient way is to improve the electrolyte solvent process to form a strong and uniform conductive SEI layer on the anode surface, which can potentially improve the electrochemical performance of LMBs, realizing fast charging and a wide range of operating temperatures, and meeting various market requirements in the future. [Means for solving the problem]

[0006] The present invention provides an electrolyte solvent having adjustable solubility characteristics, comprising a chemical structure represented by the following formula (1): [ka] (Formula 1) In formula (1), A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof.

[0007] Furthermore, the present invention provides an electrolyte solvent with adjustable solubility properties, which is symmetrically formed by two formulas (1) and includes a chemical structure represented by the following formula (2): [ka] (Formula 2) where A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ) or a combination thereof.

[0008] Furthermore, the present invention provides another electrolyte solvent with adjustable solubility properties, comprising a chemical structure represented by the following formula (3): [ka] (Formula 3) where A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ) or a combination thereof.

[0009] Furthermore, the synthesis method of the electrolyte solvent having adjustable solubility properties of the above formula (1) is as follows: A step of reacting chemical structures of the following formula (4) and formula (5) to bond formula (5) and formula (4) at a double bond site to obtain a chemical structure of formula (6); In formula (6), a double bond is again formed at the bond between the original formula (5) and formula (4), and an ethyl group and A ‐ After removing the chemical structure represented by formula (7) formed by the above formula, a step of obtaining an electrolyte solvent with adjustable solubility characteristics as described in formula (1) of claim 1 is obtained; Includes. [ka] (Formula 4) [ka] (Formula 5) [ka] (Formula 6) C 2 H 5 A ‐ …Formula (7) where A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof.

[0010] Furthermore, a method for producing an electrolyte solvent capable of adjusting the solubility characteristics corresponding to the above formula (2) is as follows: A step of reacting the chemical structure of the following formula (8) with two chemical structures of formula (5) to combine formula (8) and formula (5) to obtain a chemical structure represented by formula (9); In formula (9), a double bond is again formed at the bond between the original formula (8) and formula (5), and two ethyl groups and A ‐ After removing the chemical structure represented by formula (7) formed by the above, a chemical structure according to formula (2) of claim 2 is obtained; Includes. [ka] (Formula 8) [ka] (Formula 9) where A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ) or a combination thereof.

[0011] The present invention applies the above-mentioned electrolyte solvent capable of adjusting the dissolution characteristics to various electrochemical devices, for example, various metal batteries.

[0012] Preferably, the metal batteries include lithium batteries, sodium batteries, magnesium batteries, zinc batteries, or aluminum batteries, as well as metal, metal ion, and mixed metal and metal ion batteries. Effect of the Invention

[0013] From the above description, it can be seen that the present invention has the following beneficial effects and advantages. 1. The present invention adjusts anion-rich solvents to have good solvation action through the electrolyte process, develops and synthesizes solvents with weak solubility characteristics, greatly improving battery performance, and the solvents have low manufacturing costs. The technology of the present invention can control the lithium growth pattern, which also helps improve the safety of lithium batteries during fast charging, and is extended to various electrochemical devices such as various metal / metal ion / metal and metal ion mixed batteries. 2. The electrolyte solvent provided by the present invention not only helps to deposit metal on the surface of the negative electrode and form a useful solid electrolyte interface, but also has good interaction with the anion of the metal salt, and produces a cathode electrolyte interface (CEI) that suppresses defects in the positive electrode. It does not require an increase in the concentration of the metal salt, greatly extending the life and safety of the metal / metal ion / metal and metal ion mixed battery, and reducing the overall cost of the electrolyte. [Brief description of the drawings]

[0014] [Figure 1] 1 is a flow chart of a preferred embodiment of a synthesis method according to the first preferred embodiment of the present invention; [Diagram 2] 1 is a flow chart of a preferred embodiment of a synthesis method according to a second preferred embodiment of the present invention; [Figure 3A] FIG. 2 is an electrostatic potential distribution (ESP) map of each atom of the chemical structures of corresponding Examples 2-1 and 2-2. [Figure 3B] FIG. 2 is an electrostatic potential distribution (ESP) map of each atom of the chemical structures of corresponding Examples 2-1 and 2-2. [Figure 4] FIG. 2 is a diagram showing the hydrogen nuclear magnetic resonance spectrum of Example 2-1 of the present invention. [Diagram 5] FIG. 1 is a diagram showing the results of the Coulombic efficiency and the electrostatic capacity retention rate when Example 2-1 of the present invention and a comparative example are applied to an anode-free lithium metal battery. [Figure 6] FIG. 13 is a diagram showing the cycle life performance when Example 2-1 of the present invention is applied to a Li||NMC lithium metal half cell. [Figure 7A] 6 is an electron microscope image of the negative electrode surface observed after charging and discharging using Example 2-1 of the present invention and a comparative example corresponding to the Cu∥NMC battery in FIG. 5. [Figure 7B] 6 is an electron microscope image of the negative electrode surface observed after charging and discharging using Example 2-1 of the present invention and a comparative example corresponding to the Cu∥NMC battery in FIG. 5. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] In order to more clearly describe the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings necessary for describing the embodiments. It should be understood that the drawings in the following description are merely some examples or embodiments of the present invention, and do not limit the technical scope of the present invention. Unless otherwise clear from the context or otherwise described, the same component symbols in the drawings represent the same structures or operations.

[0016] The present invention will be described in detail below with reference to some preferred embodiments. However, the drawings are merely exemplary representatives or embodiments of the present invention, and those skilled in the art can further apply the present invention to other similar situations based on these drawings without exerting any creative effort.

[0017] It should be understood that the terms "system", "apparatus", "unit" and / or "module" used herein are ways of distinguishing different components, members, parts, portions or assemblies of different classes. However, other terms may be substituted if the same purpose can be achieved by other terms. As shown in the present invention, unless the context clearly indicates otherwise, terms such as "a", "one", "a kind" and / or "the" are not limited to singular but may include plural. In general, the terms "comprising" and "including" only suggest the inclusion of specifically identified steps and elements, and these steps and elements do not constitute an exclusive list, and the method or system may also include other steps or elements.

[0018] In the present invention, a flowchart is used to describe the operations performed by the system according to the embodiment of the present invention. It should be understood that the operations are not necessarily performed in exact order. Conversely, each step may be processed in reverse order or simultaneously. At the same time, other operations may be added to these processes or one or more steps may be removed from these processes.

[0019] Dissolution or solvation in the present invention refers to a series of chemical reactions caused by the solvent in a chemical solution, which affects the reaction rate, reaction balance, solubility, stability, and even reaction mechanism of the chemical reactions. Therefore, the present invention is an electrolyte solvent with tunable properties for the overall reaction in the solution.

[0020] <Example 1 of electrolyte solvent with adjustable solubility characteristics> Example 1 of the electrolyte solvent capable of adjusting the solvation characteristics of the present invention has the chemical structure shown in formula (1) below. [ka] Formula (1) In formula (1), A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof.

[0021] The elements not shown in formula (1) are carbon elements (C). The halogens include fluorine (F), chlorine (Cl), bromine (Br), iodine (I), astatine (At), etc. The elements not shown in formula (1) are carbon elements (C), and unless otherwise indicated, the carbon elements are bonded to hydrogen (H), and at the same time, without affecting the characteristics of the present invention, these carbon elements can be bonded to other elements or functional groups by carbon single bonds, carbon double bonds, or carbon triple bonds, and are not limited here.

[0022] <Example 2 of electrolyte solvent with adjustable solubility characteristics> Example 2 of the electrolyte solvent capable of adjusting the solvation characteristics of the present invention has the chemical structure shown in formula (2) below, which is a symmetrical structure of formula (1) of Example 1 above. [ka] Formula (2) In formula (2), A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof.

[0023] The elements not shown in formula (2) are carbon elements (C), and unless otherwise indicated, the carbon elements are bonded to hydrogen (H); at the same time, these carbon elements can be bonded to other elements or functional groups by carbon single bonds, carbon double bonds, or carbon triple bonds without affecting the properties of the present invention, and are not limited thereto.

[0024] <Example 3 of electrolyte solvent with adjustable solubility characteristics> Example 3 of the electrolyte solvent capable of adjusting the solvation characteristics of the present invention has a chemical structure shown in formula (3) below. [ka] Formula (3) In formula (3), A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof.

[0025] The elements not shown in formula (3) are carbon elements (C), and unless otherwise indicated, the carbon elements are bonded to hydrogen (H); at the same time, these carbon elements can be bonded to other elements or functional groups by carbon single bonds, carbon double bonds, or carbon triple bonds without affecting the properties of the present invention, and are not limited thereto.

[0026] With reference to Table 1 below, the description of some preferred examples of chemical structure formulas and their names of the electrolyte solvents capable of adjusting the above-mentioned solvation properties in Examples 2 and 3 are shown. In each of the following examples, elements not shown are carbon (C), and unless otherwise indicated, carbon elements are bonded to hydrogen (H), and at the same time, these carbons can be bonded to other elements or functional groups by carbon single bonds, carbon double bonds, or carbon triple bonds without affecting the properties of the present invention, and are not limited here.

[0027] [Table 1]

[0028] <Example 1 of a method for producing an electrolyte solvent with adjustable solubility characteristics> In a preferred embodiment of the synthetic preparation method of preferred embodiment 1 of the present invention, the steps include: Step S1-1) Referring to FIG. 1, a reaction is carried out using the chemical structures of formula (4) and formula (5) to produce a negatively charged A ‐ and the positively charged double bond of formula (4) react to form a single bond at the positively charged double bond of formula (4), bonding formula (5) and formula (4) together to obtain the chemical structure of formula (6). [ka] Formula (4) [ka] Formula (5) [ka] Formula (6)

[0029] In step S1-2) formula (6), a double bond is again formed at the bond between the original formula (5) and formula (4), and an ethyl group and A ‐ After removing the chemical structure represented by formula (7) formed by the above, the compound of preferred embodiment 1 represented by formula (1) of the present invention is obtained. C 2 H 5 A - …Formula (7) where A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te) or a combination thereof, and B is a halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof, and the element not shown in the single bond is a carbon element (C). The AH group in formula (5) is a functional group formed by the element represented by the above-mentioned symbol A and hydrogen (H).

[0030] <Example 2 of a method for producing an electrolyte solvent with adjustable solubility characteristics> In a preferred embodiment of the synthetic preparation method of preferred embodiment 2 of the present invention, the steps include: Step S2-1) Referring to FIG. 2, a reaction is carried out using the chemical structures of formula (8) and formula (5) to produce a negatively charged A‐ and the positively charged double bonds of formula (8) react to form single bonds at the two positively charged double bonds of formula (8), bonding formula (8) and formula (5) together to obtain the chemical structure of formula (9). [ka] Formula (8) [ka] Formula (9)

[0031] In step S2-2) formula (8), a double bond is again formed at the bond between the original formula (8) and formula (5), and an ethyl group and A ‐ After removing the chemical structure represented by formula (7) formed by the above, the compound represented by formula (2) of the preferred embodiment 1 of the present invention is obtained. Similarly, in each chemical formula of this embodiment, A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te) or a combination thereof, and B is halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof, where the element not shown in the single bond is carbon (C).

[0032] A preferred embodiment of the manufacturing method of the present invention can be specifically carried out as follows. 12 g of DES, 10.05 g of 2,2-difluoroethanol, 2.75 g of triethylamine (TEA, Et3N) and 20 ml of anhydrous acetone are added to a 250 ml round-bottom flask, the solution is cooled to 0 °C and stirred in an ice bath for 10 min. The mixture is mixed with 10 ml of anhydrous dichloromethane (DCM) and added dropwise to the flask. Once the addition is complete, the ice bath is removed and the suspension is allowed to warm to room temperature. The reaction mixture is stirred at room temperature for 48 h. After the reaction is complete, 5 ml of deionized water is slowly added to the suspension to dissolve all solids. The DCM layer is separated, washed with brine and diluted with anhydrous magnesium sulfate (MgSO 4) and the solvent was removed under vacuum. The raw material was distilled three times at a temperature of about 80° C. to obtain a colorless liquid weighing about 19.62 g with a yield of 89%. After synthesis, the invention was mixed with 10 wt. % activated molecular sieves and stored at room temperature in an argon-filled glove box (Vigor, oxygen <0.5 ppm, water <0.1 ppm). The water content of the invention measured by Karl-Fisher titration is less than 70 ppm.

[0033] <Validity test> The electrolyte solvent with adjustable dissolution properties provided by the present invention is preferably used as an electrolyte solvent in an electrochemical device, for example, an electrochemical battery. Figures 3A and 3B are electrostatic potential distribution (ESP) maps of each atom of the chemical structures of Examples 2-1 and 2-2 in Table 1 above. The shading areas (red areas in the color diagrams) in Figures 3A and 3B have negative potential positions such as C=O and F, I, and the optimal position is between C=O and F, I, which are the metal ions in the solvent and electrolyte metal salt, for example, the ions in lithium salt (Li + The optimal solvation coordination of CH ions helps metal ions to create a dense and highly conductive solid electrolyte interface (SEI) on the negative electrode, which is favorable for metal precipitation. The darkest areas in Figure 3 (blue areas in the color diagram) are the CH 3 The positive potential position of the solvent molecule of the present invention is a positive potential position such as , which has a good interaction with the negative charge of the metal salt in the electrolyte such as lithium salt, and is useful for stabilization at the cathode electrolyte interface (CEI) at the positive electrode. In a similar concept, the cation (Li) and the corresponding anion of other lithium salts can be stabilized at the positive potential and negative potential of the solvent molecule of the present invention, respectively. By appropriately selecting the elements A and B, the present invention is useful for depositing metal on the negative electrode surface of an electrochemical device and forming a beneficial solid electrolyte interface (SEI), and at the same time, has a good interaction with the anion of the metal salt and suppresses the formation of a poor cathode electrolyte interface (CEI) at the positive electrode.

[0034] FIG. 4 shows a hydrogen nuclear magnetic resonance spectrum ( 1 4. H-NMR Spectrum. As can be seen from FIG. 4, the structures marked with X, Y, and Z in the chemical structures of the examples of the present invention certainly have corresponding chemical shift peaks, so it can be confirmed that the compounds of the present invention have been successfully synthesized by the above-mentioned synthesis preparation method and have the proposed chemical structures.

[0035] FIG. 5 shows the results of measuring the Coulombic efficiency and capacity retention rate by overcharging (4.5V) using an electrolyte solvent with adjustable dissolution characteristics corresponding to Example 2-1 of the present invention in Table 1 above and ethylene carbonate (EC) and diethyl carbonate (DEC) solvents as comparative examples, which is applied to an anodeless battery, a Cu||NMC lithium metal battery, and using lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) as the lithium salt in the electrolyte. As can be seen from the results shown in FIG. 5, the Coulombic efficiency of Example 2-1 of the present invention still maintains an average Coulombic efficiency (ACE) of nearly 100% after 40 charge / discharge cycles, even under the harsh test environment of overcharging, whereas the comparative example has a decrease to 90% or less. The capacity retention rate (CR) still maintains at least 55% after 40 charge / discharge cycles for the example of the present invention, while the capacity of the comparative example is 0%, indicating that the present invention can indeed maintain the electrical characteristics of a lithium metal battery.

[0036] FIG. 6 shows the cycle life performance under overcharge (4.5 V) when the electrolyte solvent with tunable solubility properties corresponding to Example 2-1 in Table 1 of the present invention is applied to a Li||NMC lithium metal half cell, and the lithium salt in the electrolyte is lithium bis(trifluoromethanesulfonyl)imide (LiTFSI). Even under the harsh condition of 4.5V overcharge, the battery still maintained an average coulomb rate (ACE) of 99.78% after 200 charge / discharge cycles, and a capacity retention (CR) of 77.54% at the 195th cycle, indicating that the present invention can indeed extend or maintain the electrical properties of the battery.

[0037] 7A and 7B are scanning electron microscope (SEM) images of the negative electrode surface observed after charging and discharging in a Cu||NMC battery corresponding to FIG. 5, using the electrolyte solvent with tunable dissolution characteristics of Example 2-1 of the present invention in Table 1 above, and ethylene carbonate (EC) and diethyl carbonate (DEC) solvents as comparative examples. The surface of the negative electrode of Example 2-1 of the present invention in FIG. 7A is smooth and dense, indicating the formation of a dense lithium metal and solid electrolyte interface (SEI), which is favorable for extending the electrical properties and life of the battery. On the other hand, the surface of the comparative example in FIG. 7B is rough and loose, indicating the formation of a significant amount of lithium dendrites or dead lithium, which cannot be used for electrochemical reactions and ultimately reduces the electrical properties and life of the battery.

[0038] <Application of electrolyte solvents with adjustable solubility properties> The electrolyte solvent with tunable dissolution properties provided by the present invention can be preferably used in electrochemical devices, such as electrolyte solvents in electrochemical batteries. Applicable electrochemical batteries include lithium batteries, sodium batteries, magnesium batteries, zinc batteries, aluminum batteries, etc., and preferably include the above-mentioned metal batteries, metal ion batteries, and mixed batteries.

[0039] In the above description, numbers are used to describe the quantities of components and attributes in some embodiments, but it should be understood that the numbers used to describe the embodiments are modified in some embodiments using the modifiers "about", "approximately", or "substantially". Unless otherwise specified, "about", "approximately", or "substantially" means that the numerical value described is allowed to vary by ±20%. Thus, in some embodiments, the numerical parameters used in the specification and claims are approximations that may vary depending on the desired properties of each embodiment. In some embodiments, the numerical parameters must be calculated using a methodology that takes into account the number of significant digits given and reserves the common digits. Although the numerical fields and parameters used to determine the breadth of the ranges in some embodiments of the present invention are approximations, in specific embodiments, such numerical values ​​are set to be as precise as possible within the limits practicable.

[0040] Finally, it should be understood that the embodiments described herein are used only to illustrate the principles of the embodiments of the present invention. Other variations may fall within the scope of the present invention. As such, the embodiments are intended to be illustrative rather than limiting, and alternative configurations of the embodiments of the present invention may be considered consistent with the teachings of the present invention. Correspondingly, the embodiments of the present invention are not limited to the embodiments explicitly introduced and described herein. [Explanation of symbols]

[0041] S1-1 Synthesis step of the first preferred embodiment S1-2 Synthesis step of the first preferred embodiment S2-1 Synthesis step of the second preferred embodiment S2-2 Synthesis step of the second preferred embodiment

Claims

1. An electrolyte solvent having adjustable solubility characteristics, comprising a chemical structure represented by the following formula (1): 【Chemistry 1】 (Formula 1) In formula (1), A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof; B is a substituted halogen atom, a nitrile group (CN), a nitro group (NO), or a combination thereof; 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof.

2. The electrolyte solvent capable of adjusting the solubility characteristics according to claim 1 , which is symmetrically formed by two formulas (1) and includes a chemical structure represented by the following formula (2): 【Chemistry 2】 (Formula 2) In formula (2), A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof; B is a mono-, di-, or tri-substituted halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ) or a combination thereof.

3. A step of reacting chemical structures of the following formula (4) and formula (5) to bond formula (5) and formula (4) at a double bond site to obtain a chemical structure of formula (6); In formula (6), a double bond is again formed at the bond between the original formula (5) and formula (4), and an ethyl group and A ‐ After removing the chemical structure represented by formula (7) formed by the above formula, an electrolyte solvent having tunable solubility properties according to formula (1) of claim 1 is obtained; A method for producing an electrolyte solvent having tunable solubility properties, comprising: 【Chemistry 3】 (Formula 4) 【Chemistry 4】 (Formula 5) 【Chemistry 5】 (Formula 6) C 2 H 5 A ‐ …Formula (7) where A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is one, two, or three substituted halogens, a nitrile group (CN), a nitro group (NO 2 ), nitroso group (NO), amine group (NH 2 ), or a combination thereof.

4. A step of reacting the chemical structure of the following formula (8) with two chemical structures of formula (5) to combine the formula (8) and the formula (5) to obtain a chemical structure represented by formula (9); In formula (9), a double bond is again formed at the bonding site of the original formula (8) and formula (5), and two ethyl groups and A ‐ obtaining a chemical structure according to formula (2) of claim 2 after removing the chemical structure represented by formula (7) formed by: The method for producing an electrolyte solvent with adjustable solubility characteristics according to claim 3, further comprising: 【Chemistry 6】 (Formula 8) 【Chemistry 7】 (Formula 9) where A is oxygen (O), sulfur (S), selenium (Se), tellurium (Te), or a combination thereof, and B is a mono-, di-, or tri-substituted halogen, a nitrile group (CN), hydrogen (H), a nitro group (NO), a nitroso group (NO), an amine group (NH), or a combination thereof.

5. 3. An electrochemical device comprising an electrolyte solvent with tunable solubility characteristics according to claim 1 or 2.

6. The electrochemical device of claim 5 , wherein the electrochemical device comprises a metal battery.

7. 7. The electrochemical device of claim 6, wherein the metal battery comprises a lithium battery, a sodium battery, a magnesium battery, a zinc battery, or an aluminum battery.

8. 8. The electrochemical device of claim 6 or 7, wherein the metal batteries include metal, metal ion, and mixed metal and metal ion batteries.

9. The electrochemical device of claim 5 , wherein the electrochemical device comprises an anode-free battery.

Citation Information

Patent Citations

  • Method for preparing fatty acid trifluoro-ethyl ester without catalysts or condensation agents

    CN106349071A

  • Nonaqueous electrolytic solution, and nonaqueous electrolytic solution battery

    JP2007258102A

  • Lithium-ion battery

    JP2014525667A

  • Lithium secondary battery

    JP2019537226A

  • Lithium anode battery

    JP2022191981A