Liquid crystal package and manufacturing method for the same, optical stack including the same, and smart window including the same
The liquid crystal package with a sealed structure and direct conductive layer on a polarizing plate addresses sealant-related defects and cost issues, enhancing transmittance and flexibility in lighting conditions.
Patent Information
- Application Number
- JP2024066730
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-21
- Filing Date
- 2024-04-17
- Publication Date
- 2024-10-31
AI Technical Summary
Conventional variable transmittance optical laminates face issues such as product defects due to uneven gaps and sealant rupture caused by sealants, and increased manufacturing costs due to the inclusion of additional base materials for forming conductive layers, leading to fixed transmittance issues that can cause glare or visibility problems depending on lighting conditions.
A liquid crystal package with a sealed structure that eliminates the need for a sealant and forms the conductive layer directly on a polarizing plate, using protective films and alignment films to maintain alignment without a separate base material, resulting in a thinner and more efficient laminate.
This design prevents product defects from sealant-related issues and reduces manufacturing costs while improving transmittance and bending characteristics, allowing for variable light transmittance based on voltage application.
Smart Images

Figure 2024155813000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a liquid crystal package and a manufacturing method thereof, an optical laminate including the same, and a smart window including the same. [Background technology]
[0002] In general, external light blocking coating is often applied to the window glass of a vehicle or other means of transportation. However, the window glass of a conventional means of transportation has a fixed transmittance, and the external light blocking coating also has a fixed transmittance. Therefore, the windows of such conventional means of transportation have a fixed overall transmittance, which may lead to accidents. For example, if the overall transmittance is set low, there is no problem during the day when there is sufficient light in the surroundings, but there is a problem that the driver may have difficulty in properly checking the surroundings of the means of transportation at night when there is insufficient light in the surroundings. Alternatively, if the overall transmittance is set high, there is a problem that the driver may be dazzled during the day when there is sufficient light in the surroundings. Therefore, a variable transmittance optical laminate capable of changing the transmittance of light when a voltage is applied has been developed.
[0003] The variable transmittance optical stack is driven by applying a voltage to drive the liquid crystal to change the transmittance. The variable transmittance optical stack developed to date has been fabricated by forming a liquid crystal layer in an area defined by an upper laminate, a lower laminate, and a sealant, forming a conductive layer for driving the liquid crystal on a separate substrate, and combining this with other elements such as a polarizing plate.
[0004] For example, Japanese Patent Publication No. 2018-010035 also discloses a variable transmittance optical laminate that forms a liquid crystal layer in an area defined by an upper laminate, a lower laminate, and a sealing material, and includes a transparent electrode layer formed on a polycarbonate (PC) substrate or the like having a predetermined thickness.
[0005] However, when a sealant is included to provide a space for the liquid crystal layer, the height of the sealant is not sufficiently compressed when the upper and lower laminates are joined, which can lead to product defects such as uneven gaps or sealant bursting. Also, when a separate substrate is included to form a conductive layer, the manufacturing process becomes complicated and the manufacturing costs increase, and the laminate becomes thick, which can cause a phase difference and thus change the transmittance.
[0006] Therefore, there is a need to develop a variable transmittance optical laminate that can prevent product defects caused by the use of a sealant, does not require a separate substrate for forming a conductive layer, simplifies the manufacturing process, and can reduce the thickness. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] Japanese Patent Application Publication No. 2018-010035 Summary of the Invention [Problem to be solved by the invention]
[0008] The present invention aims to minimize product defects caused by gap non-uniformity or sealant rupture that occurs due to the inclusion of a sealant for forming a liquid crystal layer.
[0009] Another object of the present invention is to solve the problem of increased manufacturing costs due to the inclusion of a separate base material for forming a conductive layer, and to further improve product quality, such as by making the product thinner or improving its transmittance.
[0010] However, the problems to be solved by the present invention are not limited to those mentioned above, and other problems not mentioned will be clearly understood by those skilled in the art from the following description. [Means for solving the problem]
[0011] The present invention relates to a liquid crystal package having a sealed structure with an outer circumferential surface sealed, the package including a first protective film, a first alignment film formed on one side of the first protective film, a second protective film facing the first alignment film, a second alignment film formed on one side of the second protective film and facing the first alignment film, and a liquid crystal layer provided between the first alignment film and the second alignment film.
[0012] In the first aspect of the present invention, the sealed structure may be a structure sealed by heat fusion sealing.
[0013] In a second aspect of the present invention, at least a partial area of the sealed outer circumferential surface may have a shape that protrudes outward from the liquid crystal package.
[0014] In a third aspect of the present invention, at least a partial area of the sealed outer circumferential surface may have a bent shape such that a curved surface is formed on the outer circumferential surface of the liquid crystal package.
[0015] In a fourth aspect of the present invention, at least one of the first protective film and the second protective film may include one or more selected from the group consisting of polyethylene terephthalate (PET), polyethylene isophthalate (PEI), polyethylene naphthalate (PEN), polybutylene terephthalate (PBT), diacetyl cellulose, triacetyl cellulose (TAC), polycarbonate (PC), polyethylene (PE), polypropylene (PP), polymethyl acrylate (PMA), polymethyl methacrylate (PMMA), polyethyl acrylate (PEA), polyethyl methacrylate (PEMA), and cyclic olefin polymer (COP).
[0016] In a fifth aspect of the present invention, at least one of the first protective film and the second protective film may have a thickness of 50 μm or less.
[0017] The present invention also relates to a method for manufacturing the liquid crystal package.
[0018] The present invention also relates to a variable transmittance optical laminate including a first transparent conductive layer and a first polarizing plate laminated on the upper surface of the first protective film, and a second transparent conductive layer and a second polarizing plate laminated on the upper surface of the second protective film.
[0019] In a sixth aspect of the present invention, at least one of the first transparent conductive layer and the second transparent conductive layer may be formed in direct contact with one of the first polarizing plate and the second polarizing plate.
[0020] In a seventh aspect of the present invention, at least one of the first transparent conductive layer and the second transparent conductive layer may contain one or more materials selected from the group consisting of transparent conductive oxides, metals, carbon-based materials, conductive polymers, conductive inks, and nanowires.
[0021] In an eighth aspect of the present invention, at least one of the first polarizing plate and the second polarizing plate may include one or more layers selected from the group consisting of a protective layer, a phase difference adjusting layer, and a refractive index adjusting layer.
[0022] In a ninth aspect of the present invention, at least one of the first polarizing plate and the second polarizing plate may have a thickness of 30 to 200 μm.
[0023] In a tenth aspect of the present invention, the variable transmittance optical laminate may further include one or more layers selected from the group consisting of an overcoat layer, an adhesive layer, and an ultraviolet absorbing layer.
[0024] The present invention also relates to a smart window comprising the variable transmittance optical laminate.
[0025] The present invention also relates to a means of transportation comprising said smart window.
[0026] The present invention also relates to an automobile in which the smart window is applied to at least one of a front window, a rear window, a side window, a sunroof window, and an interior partition.
[0027] The present invention also relates to a wearable device or building fixture including the smart window. Effect of the Invention
[0028] The liquid crystal package according to the present invention is advantageous in that it does not include a sealant, and therefore does not cause a gap non-uniformity caused by poor compression of the sealant or a product defect caused by sealant bursting.
[0029] In addition, according to the variable transmittance optical laminate of the present invention, the conductive layer is formed directly on one side of the polarizing plate, and a separate substrate for forming the conductive layer is not required, which is advantageous in terms of making the laminate thinner or improving the transmittance. [Brief description of the drawings]
[0030] [Figure 1] 1 illustrates a liquid crystal package in accordance with one or more embodiments of the present invention. [Diagram 2] 1 illustrates a liquid crystal package in accordance with one or more embodiments of the present invention. [Figure 3A] 2A to 2C are diagrams illustrating a manufacturing process of a liquid crystal package according to an embodiment of the present invention. [Figure 3B] 2A to 2C are diagrams illustrating a manufacturing process of a liquid crystal package according to an embodiment of the present invention. [Figure 3C] 2A to 2C are diagrams illustrating a manufacturing process of a liquid crystal package according to an embodiment of the present invention. [Figure 4] 1 is a diagram showing a variable transmittance optical stack according to an embodiment of the present invention. [Diagram 5] FIG. 2 illustrates a laminated structure of a smart window according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] The present invention includes a liquid crystal package and a manufacturing method thereof, which does not include a sealant for forming a liquid crystal layer and thus can prevent technical problems that may occur when a sealant is included, such as uneven gaps due to poor compression of the sealant or product defects due to sealant rupture; and the liquid crystal package.
[0032] More specifically, the present invention relates to a variable transmittance optical laminate in which a conductive layer for driving liquid crystal is directly formed on one side of a polarizing plate, thereby eliminating the need for a separate substrate for forming the conductive layer, thereby reducing the thickness of the laminate and improving the transmittance in the light-transmitting mode.
[0033] More specifically, the present invention relates to a liquid crystal package including a first protective film, a first alignment film formed on one side of the first protective film, a second protective film facing the first alignment film, a second alignment film formed on one side of the second protective film and facing the first alignment film, and a liquid crystal layer provided between the first alignment film and the second alignment film, and the liquid crystal package has a sealed structure with a sealed outer periphery, a manufacturing method thereof, and a variable transmittance optical laminate including the same.
[0034] The variable transmittance optical laminate of the present invention including the liquid crystal package is particularly suitable for technical fields in which light transmittance can be changed by applying a voltage, and can be used, for example, as a smart window.
[0035] A smart window is an optical structure that controls the amount of light or heat passing through by changing the light transmittance according to the application of an electrical signal. That is, a smart window can be changed to a transparent, opaque, or translucent state according to voltage, and is also called variable transmittance glass, light control glass, or smart glass.
[0036] A smart window can be used as a partition for dividing the interior space of a vehicle or building or for privacy protection, or as a light window placed in an opening of a building. It can also be used as a highway sign, bulletin board, scoreboard, clock or advertising screen, and can be used to replace windows in vehicles such as automobiles, buses, airplanes, ships or trains, or glass in vehicles such as sunroofs.
[0037] The variable transmittance optical laminate of the present invention can also be used as a smart window in the various technical fields described above, but since the conductive layer is directly formed on the polarizing plate, no separate substrate is required for forming the conductive layer, and the thickness is thin and the bending characteristics are advantageous, so that the variable transmittance optical laminate of the present invention can be particularly suitably used as a smart window for vehicles or buildings. In one or more embodiments, the smart window to which the variable transmittance optical laminate of the present invention is applied can be used in transportation, for example, front windows, rear windows, side windows and sunroof windows of automobiles, or building fixtures, and can be used for dividing the interior space of automobiles or buildings, such as interior partitions, or for protecting private life, in addition to blocking external light, and can also be used in wearable devices such as helmets, glasses, or watches.
[0038] Hereinafter, the present invention will be described in more detail with reference to the drawings. However, the following drawings attached to this specification are for illustrating preferred embodiments of the present invention and serve to further understand the technical concept of the present invention together with the above-mentioned content of the invention, so the present invention should not be interpreted as being limited only to the matters described in the drawings.
[0039] The terms used in this specification are for the purpose of describing the embodiments and are not intended to limit the present invention. In this specification, the singular form includes the plural form unless otherwise specified in the text. For example, the term "polarizing plate" used in this specification means at least one polarizing plate among the first polarizing plate and the second polarizing plate, the term "transparent conductive layer" means at least one transparent conductive layer among the first transparent conductive layer and the second transparent conductive layer, the term "protective film" means at least one protective film among the first protective film and the second protective film, and the term "alignment film" may mean at least one alignment film among the first alignment film and the second alignment film.
[0040] As used herein, the words "comprises" and "comprising" are used in a sense that does not exclude the presence or addition of one or more other components, steps, operations and / or elements other than the mentioned components, steps, operations and / or elements. The same reference numerals refer to the same components throughout the specification.
[0041] Spatially relative terms such as "below," "bottom," "lower," "upper," "top," "top" and the like can be used to readily describe the relationship of one element or component to another element or component as depicted in the drawings. Spatially relative terms should be understood in terms that include different orientations of elements in use or operation in addition to the orientation depicted in the drawings. For example, if an element depicted in the drawings is flipped over, an element described as "below" or "below" another element may be placed "above" the other element. Thus, the exemplary term "below" can include both an orientation of below and above. Elements can be oriented in other directions, whereby the spatially relative terms are interpreted accordingly.
[0042] As used herein, "planar direction" is interpreted as the thickness direction of the polarizer and / or transparent conductive layer, ie, the direction viewed from the user's viewing side.
[0043] As used in this specification, "substantially" is interpreted to include not only something that is completely identical or coincident with the physical object, but also something that is within the range of error in measurement or manufacturing process, for example, an error range of 1% or less.
[0044] <Liquid crystal package> 1 and 2 are diagrams illustrating a liquid crystal package according to one or more embodiments of the present invention.
[0045] Referring to Figures 1 and 2, a liquid crystal package 100 according to one embodiment of the present invention may include a first protective film 11, a second protective film 12, a first alignment film 21, a second alignment film 22, and a liquid crystal layer 30.
[0046] The protective films 11 and 12 are intended to provide a structural base for the formation of the alignment films 21 and 22 and the liquid crystal layer 30, and to act as members for forming a sealed structure by sealing, as described below.
[0047] The protective films 11 and 12 may be used in a single layer form as shown in Figures 1 and 2, but are not limited thereto, and may be used in a multi-layer form in which two or more protective films are continuously laminated according to the needs of the user.
[0048] In one or more embodiments, the protective films 11 and 12 may include one or more selected from the group consisting of polyethylene terephthalate (PET), polyethylene isophthalate (PEI), polyethylene naphthalate (PEN), polybutylene terephthalate (PBT), diacetyl cellulose, triacetyl cellulose (TAC), polycarbonate (PC), polyethylene (PE), polypropylene (PP), polymethyl acrylate (PMA), polymethyl methacrylate (PMMA), polyethyl acrylate (PEA), polyethyl methacrylate (PEMA), and cyclic olefin polymer (COP). In terms of availability and ease of processing, polyethylene terephthalate (PET) may be used. Of these, poly(ethylene terephthalate; PET), triacetyl cellulose (TAC), polycarbonate (PC), and cyclic olefin polymer (COP) can be preferably used.
[0049] In one or more embodiments, the protective films 11 and 12 may have a thickness of 50 μm or less, preferably 1 to 30 μm, and more preferably 1 to 10 μm. If the thickness of the protective film is too small, the durability of the liquid crystal package itself may be reduced, or it may be difficult to form a sealed structure by a sealing process described later, and if the thickness is too large, the distance between the transparent conductive layers disposed on the outside of the liquid crystal package for preparing a variable transmittance optical laminate described later may be too large, making it difficult to smoothly drive the optical laminate.
[0050] The alignment films 21 and 22 are located inside the liquid crystal package with respect to the protective films 11 and 12, and serve to impart alignment to the liquid crystal compound contained in the liquid crystal layer 30.
[0051] The alignment films 21 and 22 are not particularly limited as long as they can impart alignment to the liquid crystal compound. For example, a physical alignment film or a photoalignment film can be used.
[0052] The physical alignment film may refer to an alignment film that is provided with alignment properties through a rubbing process after coating an alignment material such as polyimide (PI).
[0053] The photo-alignment film may include a photo-alignment or photo-curable polymer, etc. For example, the photo-alignment film can be prepared by applying and curing an alignment film coating composition including a photo-alignment or photo-curable polymer, a photopolymerization initiator, and a solvent.
[0054] The photo-alignable or photo-curable polymer is not particularly limited, and may be a cinnamate-based polymer, a polyimide-based polymer, or the like. For example, poly(vinyl cinnamate) (PVCi), poly(siloxane cinnamate) (PSCN), poly(ω(4-chalconyloxy)alkoxyphenylmaleimide, 6-FDA-HAB-Cl, or the like. Conventional or later developed polymers exhibiting alignment may be used.
[0055] In one or more embodiments, the alignment films 21 and 22 may have a thickness of 30 to 100 nm, and more preferably, may have a thickness of 50 to 100 nm. When the thickness of the alignment film satisfies the above range, not only is it easy to impart alignment to the liquid crystal compound, but it may also be advantageous in terms of making the liquid crystal package thinner.
[0056] The liquid crystal layer 30 can adjust the transmittance of light incident from one or more directions by an electric field, and can change the driving mode of the optical laminate in combination with a polarizing plate, which will be described later.
[0057] The liquid crystal layer 30 may include a liquid crystal compound (not shown) and a spacer (not shown), and may be disposed, for example, between a first alignment film 21 and a second alignment film 22 provided between a first protective film 11 and a second protective film 12, and in some embodiments, may form an interface with the inner wall of the protective film joined by sealing.
[0058] The liquid crystal compound is not particularly limited as long as it is driven by an electric field and can control the light transmittance, and any conventional or later developed liquid crystal compound can be used.
[0059] The liquid crystal compound may refer to a compound that includes, for example, a mesogen skeleton and one or more polymerizable functional groups. Such liquid crystal compounds are variously known as reactive mesogens (RMs). The liquid crystal compound may be polymerized by light or heat to form a cured film in which a polymer network is formed while maintaining the liquid crystal alignment.
[0060] The liquid crystal compound may be a monofunctional or polyfunctional reactive liquid crystal compound. The monofunctional reactive liquid crystal compound is a compound having one polymerizable functional group, and the polyfunctional reactive liquid crystal compound is a compound having two or more polymerizable functional groups.
[0061] The liquid crystal behavior mode of the liquid crystal compound is not particularly limited, and for example, a twisted nematic (TN) mode, a super twisted nematic (STN) mode, a vertical alignment (VA) mode, an electrically controlled birefringence (ECB) mode, etc. can be used.
[0062] The spacer may include at least one of a ball spacer and a column spacer, and is preferably a ball spacer. The number of ball spacers may be one or more, and the ball spacer preferably has a diameter of 1 to 10 μm. In addition, the area of the ball spacer in the liquid crystal layer as viewed in the planar direction is preferably 0.01 to 10% of the area of the liquid crystal layer in terms of improving the visibility of the user and the transmittance in the light-transmitting mode.
[0063] In one embodiment, the liquid crystal package 100 of the present invention may have a sealed structure with a sealed outer periphery, and for example, the sealed structure may be sealed by a heat fusion seal.
[0064] The shape of the outer periphery of the sealed structure is not particularly limited, and may be, for example, as shown in Fig. 1, a shape that protrudes outward from at least a portion of the liquid crystal package 100. Also, as shown in Fig. 2, the outer periphery of the liquid crystal package 100 may be bent so that a curved surface is formed.
[0065] The liquid crystal package 100 of the present invention does not include a sealant for forming the liquid crystal layer 30, and is advantageous in that no gap non-uniformity due to poor compression of the sealant or product defects due to sealant rupture do occur.
[0066] FIG. 3 is a diagram showing a manufacturing process of a liquid crystal package according to an embodiment of the present invention.
[0067] Referring to Figure 3, a manufacturing process of a liquid crystal package according to one embodiment of the present invention may include a step of respectively preparing a first laminate and a second laminate (S1, see Figure 3A), a step of forming a liquid crystal layer 30 between the first laminate and the second laminate (S2, see Figure 3B), and a step of sealing the outer peripheral surface by a sealing process (S3, see Figure 3C).
[0068] The step (S1) may be a step of forming a first alignment film 21 on one surface of a first protective film 11 to prepare a first laminate.
[0069] The first alignment film 21 may be formed by applying a composition for forming a physical alignment film and then performing a rubbing process, as described above, or by applying and drying a composition for forming a photoalignment film and then irradiating UV light onto the dried coating film.
[0070] In one embodiment, in order to improve adhesion between the first protective film 11 and the first alignment film 21, the first alignment film 21 may be formed after a pretreatment such as a corona treatment or a plasma treatment is performed on the surface of the first protective film 11 on which the first alignment film 21 is to be formed.
[0071] In one embodiment, the first alignment layer 21 may be formed to be smaller than the area of the first protection film 11, i.e., to have a width narrower than the width of the first protection film 11, and preferably may not be formed on the outer edge of the first protection film 11. When the first alignment layer 21 is formed in this manner, the processability of sealing the outer periphery by sealing the protection films 11 and 12 in step S3 can be further improved.
[0072] On the other hand, although FIG. 3A does not show the second laminate, the second laminate can also be produced by substantially the same method as the first laminate.
[0073] The step (S2) may be a step of forming the liquid crystal layer 30 by injecting a liquid crystal layer forming composition between the first laminate and the second laminate.
[0074] In one embodiment, the liquid crystal layer 30 is formed by injecting a liquid crystal layer forming composition onto the first alignment film 21 of the first laminate by a one drop filling (ODF) method, and then bonding the first laminate and the second laminate at a predetermined pressure. The pressure for bonding the first laminate and the second laminate is not particularly limited, but is preferably 1.0 to 3.0 kg / cm. 2 More preferably, it is 1.5 to 2.0 kg / cm 2 may be also possible.
[0075] In one embodiment, step (S2) may include a step of dispersing ball spacers before injecting a liquid crystal layer forming composition for forming the liquid crystal layer 30.
[0076] The method for spraying the ball spacers is not particularly limited, but may be, for example, a method in which a mixed solvent is prepared by mixing the ball spacers with a solvent such as IPA, and then the ball spacers are sprayed onto the lower laminate, for example, the first alignment film 21 of the first laminate.
[0077] In another embodiment, the liquid crystal layer forming composition may contain ball spacers, and in this case, the step of dispersing the ball spacers may be omitted.
[0078] The step (S3) may be a step of sealing the protective films 11 and 12 to prepare a liquid crystal package.
[0079] In one embodiment, the sealing process may be a thermal sealing process, in which case the first protective film 11 and the second protective film 12 are heated and pressed.
[0080] The temperature at which the heat sealing is performed can be appropriately selected by the user depending on the type of protective film, and may be, for example, 30 to 400°C, and preferably 50 to 380°C.
[0081] In one embodiment, the pressing is performed by applying pressures P1 and P2 to the regions corresponding to the outer ends of the first and second protective films 11 and 12, respectively.
[0082] It is preferable that the pressure P1 applied to the first outer end portion of the first protective film 11 and the second protective film 12 and the pressure P2 applied to the second outer end portion are substantially the same as each other, or if different, the difference between them is relatively small.
[0083] <Variable transmittance optical laminate> FIG. 4 is a diagram showing a variable transmittance optical laminate according to an embodiment of the present invention.
[0084] 4, the variable transmittance optical stack according to an embodiment of the present invention may include the above-mentioned liquid crystal package 100, a first transparent conductive layer 210, a second transparent conductive layer 220, a first polarizing plate 310, and a second polarizing plate 320. For example, the first transparent conductive layer 210 and the first polarizing plate 310 may be sequentially laminated on an upper surface of a first protective film 11 provided in the liquid crystal package 100, or the first polarizing plate 310 and the first transparent conductive layer 210 may be sequentially laminated on an upper surface of the first protective film 11. The second transparent conductive layer 220 and the second polarizing plate 320 may be sequentially laminated on an upper surface of the second protective film 12, or the second polarizing plate 320 and the second transparent conductive layer 220 may be sequentially laminated on an upper surface of the second protective film 12.
[0085] The transparent conductive layers 210 and 220 are provided for driving the liquid crystal layer 30 provided in the liquid crystal package 100, and may be formed in direct contact with the polarizing plates 310 and 320. For example, as shown in Fig. 4, the first transparent conductive layer 210 and the second transparent conductive layer 220 may be formed in direct contact with the first polarizing plate 310 and the second polarizing plate 320, respectively.
[0086] Conventional optical laminates used in the manufacture of smart windows, etc., are manufactured by forming a conductive layer for driving liquid crystal on one side of a substrate and laminating the other side of the substrate with a polarizing plate. However, the variable transmittance optical laminate according to the present invention is characterized in that it does not include a separate substrate for forming a conductive layer, but directly forms a conductive layer on one side of a polarizing plate, thereby reducing the thickness of the laminate and improving the transmittance and bending characteristics in the light transmission mode.
[0087] In one embodiment, the transparent conductive layers 210 and 220 may be formed by being directly deposited on one surface of the polarizers 310 and 320. In this case, the transparent conductive layers 210 and 220 may be formed by directly contacting the pre-treated surface of the polarizers 310 and 320 after performing a pre-treatment such as a corona treatment or a plasma treatment on one surface of the polarizers 310 and 320 in order to improve adhesion between the polarizers 310 and 320. The pre-treatment is not limited to a corona treatment or a plasma treatment, and any conventional or later developed pre-treatment process may be used within a range that does not impede the object of the present invention.
[0088] In another embodiment, the transparent conductive layers 210, 220 may be formed in direct contact with the polarizers 310, 320 via an easy-adhesion layer (not shown) provided on one side of the polarizers 310, 320 to improve adhesion to the polarizers 310, 320.
[0089] The transparent conductive layers 210, 220 preferably have a visible light transmittance of 50% or more, and may include, for example, one or more selected from the group consisting of transparent conductive oxides, metals, carbon-based materials, conductive polymers, conductive inks, and nanowires, but are not limited thereto, and any conventional or later developed transparent conductive layer material may be used.
[0090] In one or more embodiments, the transparent conductive oxide may include one or more selected from the group consisting of indium tin oxide (ITO), indium zinc oxide (IZO), indium zinc tin oxide (IZTO), aluminum zinc oxide (AZO), gallium zinc oxide (GZO), fluorine tin oxide (FTO), zinc oxide (ZnO), etc. The metal may include one or more selected from the group consisting of gold (Au), silver (Ag), copper (Cu), aluminum (Al), platinum (Pt), palladium (Pd), chromium (Cr), titanium (Ti), tungsten (W), niobium (Nb), tantalum (Ta), vanadium (V), iron (Fe), manganese (Mn), cobalt (Co), nickel (Ni), zinc (Zn), and alloys containing at least one of them, for example, a silver-palladium-copper (APC) alloy or a copper-calcium (CuCa) alloy. The carbon-based material may include at least one selected from the group consisting of carbon nanotubes (CNTs) and graphene, and the conductive polymer may include at least one selected from the group consisting of polypyrrole, polythiophene, polyacetylene, PEDOT, and polyaniline. The conductive ink may be an ink in which a metal powder and a curable polymer binder are mixed, and the nanowire may be, for example, a silver nanowire (AgNW).
[0091] In addition, the transparent conductive layers 210 and 220 are formed in a two-layer structure by combining the above materials, for example, a two-layer structure including a metal layer and a transparent conductive oxide layer to reduce the reflectance and increase the transmittance of incident light.
[0092] The transparent conductive layers 210 and 220 may be formed by a method commonly used in the art, for example, a coating process such as spin coating, roller coating, bar coating, dip coating, gravure coating, curtain coating, die coating, spray coating, doctor coating, kneader coating, etc.; a printing process such as screen printing, spray printing, inkjet printing, letterpress printing, intaglio printing, lithographic printing, etc.; and a deposition process such as CVD (chemical vapor deposition), PVD (physical vapor deposition), PECVD (plasma enhanced chemical vapor deposition), etc.
[0093] The polarizing plates 310 and 320 may include a polarizer (not shown) and may further include functional layers such as a protective layer, a phase difference adjustment layer, and a refractive index adjustment layer on one or both sides of the polarizer. For example, the polarizing plates 310 and 320 may include a polarizer and a protective layer stacked on one or both sides of the polarizer, a polarizer, a protective layer stacked on one side of the polarizer, and a phase difference adjustment layer stacked on the other side opposite to the one side of the polarizer, a polarizer, a protective layer stacked on one side of the polarizer, and a phase difference adjustment layer and a refractive index adjustment layer stacked in sequence on the other side opposite to the one side of the polarizer, or a polarizer, a protective layer stacked on one side of the polarizer, and a protective layer and a phase difference adjustment layer stacked in sequence on the other side opposite to the one side of the polarizer.
[0094] The polarizer may be any conventional or later developed polarizer, such as a stretched type polarizer or a coated type polarizer.
[0095] In one embodiment, the stretched polarizer may include a stretched polyvinyl alcohol (PVA)-based resin. The polyvinyl alcohol (PVA)-based resin may be a polyvinyl alcohol-based resin obtained by saponifying a polyvinyl acetate-based resin. Examples of the polyvinyl acetate-based resin include polyvinyl acetate, which is a homopolymer of vinyl acetate, and copolymers of vinyl acetate and other monomers copolymerizable therewith. The other monomers may be unsaturated carboxylic acid-based, unsaturated sulfonic acid-based, olefin-based, vinyl ether-based, and acrylamide-based monomers having an ammonium group. The polyvinyl alcohol (PVA)-based resin may be modified, and may be, for example, polyvinyl formal or polyvinyl acetal modified with aldehydes.
[0096] In an embodiment, the coating type polarizer is formed by a liquid crystal coating composition, and the liquid crystal coating composition may include a reactive liquid crystal compound and a dichroic dye.
[0097] The reactive liquid crystal compound is not particularly limited as long as it is driven by an electric field and can control the light transmittance, and may be substantially the same as the liquid crystal compound described above for the liquid crystal layer.
[0098] The dichroic dye is a component contained in the liquid crystal coating composition to impart polarization properties, and has a property that the absorbance in the long axis direction of the molecule is different from that in the short axis direction. The dichroic dye may be any dichroic dye that has been used or will be developed later, and may include at least one dye selected from the group consisting of azo dyes, anthraquinone dyes, perylene dyes, merocyanine dyes, azomethine dyes, phthaloperylene dyes, indigo dyes, dioxadine dyes, polythiophene dyes, and phenoxazine dyes.
[0099] The liquid crystal coating composition may further include a solvent for dissolving the reactive liquid crystal compound and the dichroic dye, and may include, for example, propylene glycol monomethyl ether acetate (PGMEA), methyl ethyl ketone (MEK), xylene, chloroform, etc. Also, the liquid crystal coating composition may further include a leveling agent, a polymerization initiator, etc., within a range that does not inhibit the polarization properties of the coating film.
[0100] The protective layer serves to protect the polarization characteristics of the polarizer from post-processing and external environments, and may be in the form of a protective film.
[0101] The protective layer is formed on one or both sides of the polarizer in direct contact therewith, but is not limited thereto. For example, the protective layer may be used in a multi-layer structure in which one or more protective layers are continuously laminated, or may be formed on another member.
[0102] The protective layer may be substantially the same as that described above in the protective film for the liquid crystal package.
[0103] The retardation adjusting layer is for compensating for the optical properties of the optical laminate and can be realized in the form of a retardation film, etc., and conventional or later developed retardation films, etc. can be used. For example, a quarter wave plate (1 / 4 wave plate) or a half wave plate (1 / 2 wave plate) for delaying the phase of light can be used, and these can be used alone or in combination.
[0104] The retardation adjustment layer is formed on one side of the polarizer in direct contact therewith, but is not limited thereto. For example, the retardation adjustment layer may be formed on one side of the protective layer, and the polarizer, the protective layer, and the retardation adjustment layer may be laminated in sequence.
[0105] The retardation adjusting layer may be a polymer stretched film obtained by stretching a polymer film capable of imparting optical anisotropy by stretching in an appropriate manner, or a liquid crystal polymer film.
[0106] In one embodiment, the polymer stretched film may be a polymer layer including polyolefins such as polyethylene (PE) or polypropylene (PP), cycloolefin polymers (COP) such as polynorbornene, polyesters such as polyvinyl chloride (PVC), polyacrylonitrile (PAN), polysulfone (PSU), acrylic resins, polycarbonate (PC), and polyethylene terephthalate (PET), cellulose ester polymers such as polyacrylate, polyvinyl alcohol (PVA), and triacetyl cellulose (TAC), or copolymers of two or more monomers among the monomers forming the polymers.
[0107] The method for obtaining the polymer stretched film is not particularly limited, and for example, the polymer material can be formed into a film and then stretched. The method for forming the film is not particularly limited, and the film can be formed by known methods such as injection molding, sheet molding, blow molding, injection blow molding, inflation molding, extrusion molding, foam molding, and cast molding, and secondary processing molding methods such as compressed air molding and vacuum molding can also be used. Among them, extrusion molding and cast molding are preferably used. At this time, for example, an extruder equipped with a T-die, a circular die, or the like can be used to extrude the unstretched film. When obtaining a molded product by extrusion molding, a material in which various resin components, additives, etc. are melt-kneaded in advance may be used, or the product may be molded through melt-kneading during extrusion molding. In addition, the unstretched film may be cast molded by dissolving various resin components using a solvent common to the various resin components, such as chloroform or methylene dichloride, and then casting, drying, and solidifying the resin components.
[0108] The polymer stretched film may be produced by uniaxially stretching the formed film in the mechanical direction (MD; mechanical direction, lengthwise or longitudinal direction) or uniaxially stretching the formed film in the transverse direction (TD; transverse direction, widthwise or transverse direction) of the mechanical direction. Alternatively, a biaxially stretched film may be produced by stretching the formed film using a sequential biaxial stretching method of roll stretching and tenter stretching, a simultaneous biaxial stretching method using tenter stretching, a biaxial stretching method using tubular stretching, or the like.
[0109] The liquid crystal polymer film may include a reactive liquid crystal compound in a polymerized state. The reactive liquid crystal compound may be substantially the same as the liquid crystal compound of the liquid crystal layer described above.
[0110] In one or more embodiments, the thickness of the retardation adjusting layer may be 10 μm to 100 μm in the case of a polymer stretched film, and may be 0.1 μm to 5 μm in the case of a liquid crystal polymer film.
[0111] The refractive index adjustment layer is provided to compensate for the refractive index difference of the optical laminate due to the transparent conductive layers 210 and 220, and may play a role of improving visibility by reducing the refractive index difference. The refractive index adjustment layer may also be provided to correct a hue caused by the transparent conductive layers 210 and 220. Meanwhile, when the transparent conductive layer has a pattern, the refractive index adjustment layer can compensate for the transmittance difference between a patterned region where the pattern is formed and a non-patterned region where the pattern is not formed.
[0112] Specifically, the transparent conductive layers 210 and 220 are stacked adjacent to other members (e.g., polarizers) having different refractive indices, and the difference in light transmittance may be induced due to the difference in refractive index between adjacent layers, and in particular, when a pattern is formed on the transparent conductive layer, a problem may occur in which the patterned region and the non-patterned region are visually distinguished. Therefore, by including the refractive index adjustment layer, the refractive index is compensated to reduce the difference in light transmittance of the optical laminate, and in particular, when a pattern is formed on the transparent conductive layer, the patterned region and the non-patterned region are visually distinguished.
[0113] In one embodiment, the refractive index of the refractive index adjustment layer can be appropriately selected depending on the material of the adjacent other members, but is preferably 1.4 to 2.6, and more preferably 1.4 to 2.4. In this case, it is possible to prevent light loss due to a sharp difference in refractive index between the transparent conductive layers 210 and 220 and other members such as the polarizer.
[0114] The refractive index adjusting layer is not particularly limited as long as it can prevent a sharp refractive index difference between other components such as a polarizer and the transparent conductive layers 210 and 220, and a compound used to form a conventional or later developed refractive index adjusting layer can be used, and for example, it may be formed from a refractive index adjusting layer forming composition containing a polymerizable isocyanurate compound.
[0115] In one embodiment, the polarizing plates 310 and 320 may further include other functional layers to supplement or enhance the properties of the polarizer in addition to the above-mentioned functional layers. For example, the polarizing plates 310 and 320 may further include an overcoat layer to further improve mechanical durability.
[0116] In one or more embodiments, the polarizing plates 310 and 320 may have a thickness of 30 to 200 μm, preferably 30 to 170 μm, and more preferably 50 to 150 μm, in which case the polarizing plates 310 and 320 can be used to manufacture an optical laminate having a small thickness while maintaining optical properties.
[0117] The variable transmittance optical laminate of the present invention may further include other components within the scope of the present invention, for example, may further include an adhesive layer, an ultraviolet absorbing layer, a hard coat layer, etc.
[0118] The adhesive layer is formed using an adhesive or pressure sensitive adhesive, and preferably has an appropriate adhesive strength so as to prevent peeling, air bubbles, etc. from occurring when the optical laminate is handled, and at the same time, has transparency and thermal stability.
[0119] The adhesive may be any conventional or later developed adhesive, for example a light curable adhesive.
[0120] The photocurable adhesive exhibits strong adhesive strength by crosslinking and curing when exposed to active energy rays such as ultraviolet (UV) and electron beam (EB), and is made of reactive oligomers, reactive monomers, photopolymerization initiators, etc.
[0121] The reactive oligomer is an important component that determines the properties of the adhesive, and forms a polymer bond by photopolymerization to form a hardened coating. Usable reactive oligomers include polyester resins, polyether resins, polyurethane resins, epoxy resins, polyacrylic resins, silicone resins, etc.
[0122] The reactive monomer acts as a crosslinking agent or diluent for the reactive oligomer and affects the adhesive properties. Usable reactive monomers include monofunctional monomers, polyfunctional monomers, epoxy monomers, vinyl ethers, cyclic ethers, etc.
[0123] The photopolymerization initiator plays a role of initiating photopolymerization by absorbing light energy and generating radicals or cations, and a suitable one can be selected and used depending on the photopolymerizable resin.
[0124] The adhesive may be a conventional or later developed adhesive, and in one or more embodiments, may be an acrylic adhesive, a rubber adhesive, a silicone adhesive, a urethane adhesive, a polyvinyl alcohol adhesive, a polyvinylpyrrolidone adhesive, a polyacrylamide adhesive, a cellulose adhesive, a vinyl alkyl ether adhesive, etc. The adhesive is not particularly limited as long as it has adhesive strength and viscoelasticity, but in terms of availability, etc., it may be preferably an acrylic adhesive, and may contain, for example, a (meth)acrylate copolymer, a crosslinking agent, and a solvent.
[0125] The crosslinking agent may be a conventional or later developed crosslinking agent, and may include, for example, a polyisocyanate compound, an epoxy resin, a melamine resin, a urea resin, a dialdehyde, a methylol polymer, or the like, and may preferably include a polyisocyanate compound.
[0126] The solvent may include ordinary solvents used in the field of resin compositions, such as alcohol-based compounds such as methanol, ethanol, isopropanol, butanol, and propylene glycol methoxy alcohol; ketone-based compounds such as methyl ethyl ketone, methyl butyl ketone, methyl isobutyl ketone, diethyl ketone, and dipropyl ketone; acetate-based compounds such as methyl acetate, ethyl acetate, butyl acetate, and propylene glycol methoxy acetate; cellosolve-based compounds such as methyl cellosolve, ethyl cellosolve, and propyl cellosolve; and hydrocarbon-based compounds such as hexane, heptane, benzene, toluene, and xylene. These may be used alone or in combination of two or more.
[0127] The thickness of the adhesive layer can be appropriately determined depending on the type of resin acting as an adhesive, adhesive strength, the environment in which the adhesive is used, etc. In one embodiment, the adhesive layer may have a thickness of 0.01 to 50 μm, preferably 0.05 to 20 μm, and more preferably 0.1 to 10 μm, in order to ensure sufficient adhesive strength and minimize the thickness of the optical laminate.
[0128] The ultraviolet absorbing layer is not particularly limited as long as it is used to prevent deterioration of the optical laminate due to ultraviolet rays. For example, it may be a salicylic acid-based ultraviolet absorber (phenyl salicylate, p-tert-butyl salicylate, etc.), a benzophenone-based ultraviolet absorber (2,4-dihydroxybenzophenone, 2,2'-dihydroxy-4,4'-dimethoxybenzophenone, etc.), a benzotriazole-based ultraviolet absorber (2-(2'-hydroxy-5'-methylphenyl)benzotriazole, 2-(2'-hydroxy-3',5'-di-t 2-(2'-hydroxy-3'-tert-butyl-5'-methylphenyl)benzotriazole, 2-(2'-hydroxy-3',5'-di-tert-butylphenyl)-5-chlorobenzotriazole, 2-(2'-hydroxy-3'-(3”,4”,5”,6”-tetrahydrophthalimidomethyl)-5'-methylphenyl)benzotriazole, 2,2-methylenebis(4-(1,1,3,3-tetramethylbutyl)-6-(2H-benzotriazole- 2-yl)phenol), 2-(2'-hydroxy-3'-tert-butyl-5'-methylphenyl)-5-chlorobenzotriazole, 2-(2'-hydroxy-3'-tert-butyl-5'-(2-octyloxycarbonylethyl)-phenyl)-5-chlorobenzotriazole, 2-(2'-hydroxy-3'-(1-methyl-1-phenylethyl)-5'-(1,1,3,3-tetramethylbutyl)-phenyl)benzotriazole, 2-(2H-benzotriazol-2-yl)-6-(linear and and side chain dodecyl)-4-methylphenol, a mixture of octyl-3-[3-tert-butyl-4-hydroxy-5-(chloro-2H-benzotriazol-2-yl)phenyl]propionate and 2-ethylhexyl-3-[3-tert-butyl-4-hydroxy-5-(5-chloro-2H-benzotriazol-2-yl)phenyl]propionate, etc.), cyanoacrylate ultraviolet absorbers (2'-ethylhexyl-2-cyano-3,3-diphenylacrylate, ethyl-2-cyano-3-(3',4'-methylenedioxyphenyl)-acrylate, triazine-based ultraviolet absorbers, etc. can be used, and benzotriazole-based ultraviolet absorbers and triazine-based ultraviolet absorbers, which have high transparency and are excellent in preventing deterioration of the polarizing plate and the transmittance variable layer, are preferred, and benzotriazole-based ultraviolet absorbers with a more suitable spectral absorption spectrum are particularly preferred. The benzotriazole-based ultraviolet absorbers may be bis(Bis)-modified, and may be, for example, 6,6'-methylenebis(2-(2H-benzo[d][1,2,3]triazol-2-yl)-4-(2,4,4-trimethylpentan-2-yl)phenol), 6,6'-methylenebis(2-(2H-benzo[d][1,2,3]triazol-2-yl)-4-(2-hydroxyethyl)phenol), etc.,
[0129] The hard coat layer is not particularly limited as long as it is capable of protecting components such as a polarizing plate and a transmittance variable layer from external physical and chemical shocks, and any conventional or later developed hard coat layer can be used.
[0130] In one embodiment, the hard coat layer is formed by applying a composition for forming a hard coat layer onto another member and curing the composition with light or heat. The composition for forming a hard coat layer is not particularly limited and may include, for example, a photocurable compound and a photoinitiator.
[0131] The photocurable compound and photoinitiator can be any compound commonly used in the art without any restrictions. For example, the photocurable compound may be a photopolymerizable monomer, a photopolymerizable oligomer, etc., and examples of the photocurable compound include monofunctional and / or polyfunctional (meth)acrylates, and examples of the photoinitiator include oxime esters, etc.
[0132] <Smart windows and products that include them> FIG. 5 is a diagram showing a laminated structure of a smart window according to one embodiment of the present invention.
[0133] Referring to FIG. 5, a smart window according to one embodiment of the present invention may include the above-mentioned variable transmittance optical stack, a first glass member 510, and a second glass member 520. For example, the first glass member 510 may be stacked on an upper surface of a first polarizer 310 provided in the variable transmittance optical stack, and the second glass member 520 may be stacked on an upper surface of the second polarizer 320.
[0134] In some embodiments, adhesive layers 410, 420 may be disposed between the polarizers 310, 320 and the glass members 510, 520. The adhesive layers may be substantially the same as those described for the adhesive layer of the variable transmittance optical laminate described above, and may be realized in the form of an adhesive film commonly used in the industry, such as an EVA film, a PVB film, etc.
[0135] The glass members 510 and 520 are not particularly limited, and may be ordinary glass members used in transportation means, automobiles, wearable devices, building fixtures, and the like, which will be described later.
[0136] In one embodiment, in the case of a smart window used in an automobile, the window may be formed by bonding vehicle glass onto both sides of the variable transmittance optical laminate. For example, the window may be formed by placing vehicle glass on both sides of the optical laminate, and then heating the laminate in a press machine at a temperature of 90°C and a vacuum of 1 bar for 10 to 20 minutes. In this case, an adhesive film such as an EVA film or a PVB film can be used.
[0137] In other embodiments, in the case of a smart window used in architectural fittings, it may be formed by bonding building glass to one or both sides of the variable transmittance optical laminate. For example, it may be formed by bonding building glass to one side of the optical laminate using a lamination method, or it may be formed by applying a UV adhesive to both sides of the optical laminate, bonding and UV curing the glass.
[0138] The present invention also includes a means of transportation including the smart window, for example, an automobile in which the smart window is applied to at least one of the front window, rear window, side window, sunroof window, and interior partition, a wearable device including the smart window, and a building fixture.
Claims
1. A first protective film; a first alignment film formed on one surface of the first protective film; a second protective film facing the first protective film; a second alignment film formed on one surface of the second protective film and facing the first alignment film; a liquid crystal layer provided between the first alignment film and the second alignment film; A liquid crystal package having a sealed structure with a sealed outer periphery.
2. The liquid crystal package according to claim 1 , wherein the sealed structure is a structure sealed by heat fusion sealing.
3. The liquid crystal package according to claim 1 , wherein at least a portion of the sealed outer peripheral surface has a shape protruding outward from the liquid crystal package.
4. The liquid crystal package according to claim 1 , wherein at least a portion of the sealed outer periphery has a curved shape such that a curved surface is formed on the outer periphery of the liquid crystal package.
5. At least one of the first and second protective films may be made of polyethylene terephthalate (PET), polyethylene isophthalate (PEI), polyethylene naphthalate (PEN), polybutylene terephthalate (PBT), diacetyl cellulose, triacetyl cellulose (TAC), polycarbonate (PC), polyethylene (PE), polypropylene (PP), polymethyl acrylate (PC), or the like.
3. The liquid crystal package according to claim 1, comprising at least one selected from the group consisting of polymethyl methacrylate (PMA), polyethyl acrylate (PEA), polyethyl methacrylate (PEMA) and cyclic olefin polymer (COP).
6. The liquid crystal package according to claim 1 , wherein at least one of the first and second protective films has a thickness of 50 μm or less.
7. The method for manufacturing a liquid crystal package according to any one of claims 1 to 6.
8. A variable transmittance optical laminate including the liquid crystal package according to claim 1, a first transparent conductive layer and a first polarizing plate laminated on an upper surface of the first protective film; A variable transmittance optical laminate comprising: a second transparent conductive layer and a second polarizing plate laminated on the upper surface of the second protective film.
9. The variable transmittance optical laminate of claim 8 , wherein at least one of the first transparent conductive layer and the second transparent conductive layer is formed in direct contact with one of the first polarizing plate and the second polarizing plate.
10. 9. The variable transmittance optical stack of claim 8, wherein at least one of the first transparent conductive layer and the second transparent conductive layer comprises at least one selected from the group consisting of transparent conductive oxides, metals, carbon-based materials, conductive polymers, conductive inks, and nanowires.
11. The variable transmittance optical laminate according to claim 8, wherein at least one of the first polarizing plate and the second polarizing plate includes one or more selected from the group consisting of a protective layer, a phase difference adjusting layer, and a refractive index adjusting layer.
12. 9. The variable transmittance optical laminate according to claim 8, wherein at least one of the first polarizing plate and the second polarizing plate has a thickness of 30 to 200 μm.
13. The variable transmittance optical laminate according to claim 8 , further comprising at least one layer selected from the group consisting of an overcoat layer, an adhesive layer, and an ultraviolet absorbing layer.
14. A smart window comprising the variable transmittance optical laminate according to any one of claims 8 to 13.
15. A means of transportation comprising the smart window of claim 14.
16. 15. A car comprising the smart window of claim 14 applied to at least one of a front window, a rear window, a side window, a sunroof window, and an interior partition.
17. A wearable device comprising the smart window of claim 14.
18. Architectural fittings comprising the smart window of claim 14.
Citation Information
Patent Citations
Light control film
JP2018010035A