Dye-sensitization type solar cell manufacturing kit and assembling method for dye-sensitization type solar cell
The dye-sensitized solar cell kit allows operators to freely draw or color on the solar cells, addressing the lack of design flexibility in existing kits, and maintains efficiency through a base layer and transparent components.
Patent Information
- Application Number
- JP2024069108
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-21
- Filing Date
- 2024-04-22
- Publication Date
- 2024-10-31
AI Technical Summary
Existing dye-sensitized solar cell production kits do not allow operators to freely color or draw characters and patterns on the solar cells.
A dye-sensitized solar cell kit comprising a dyeing substrate with a semiconductor layer, a writing instrument containing sensitizing dye, an electrolyte container, and a frame, allowing operators to color or draw on the substrate before assembling the cell, with a base layer to prevent bleeding and a transparent counter electrode for design visibility.
Enables operators to create personalized designs on the solar cells, enhancing their artistic appeal and functionality while maintaining photoelectric conversion efficiency.
Smart Images

Figure 2024155901000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a kit for producing a dye-sensitized solar cell and a method for assembling a dye-sensitized solar cell. [Background technology]
[0002] As the next generation of solar cells, there are high hopes for the development of organic solar cells that can be manufactured at low temperatures and at lower cost. Among organic solar cells, dye-sensitized solar cells are attracting particular attention because they have advantages not found in conventional solar cells, such as the possibility of significantly reducing manufacturing costs, their performance equivalent to that of amorphous silicon solar cells, and the ability to produce colored and transparent solar cells.
[0003] Dye-sensitized solar cells are generally composed of a semiconductor electrode made of semiconductor particles with sensitizing dye adsorbed on a conductive substrate, a counter electrode, and an electrolyte layer held between the semiconductor electrode and the counter electrode. The sensitizing dye increases the light absorption energy, improving the photoelectric conversion efficiency.
[0004] In addition, dye-sensitized solar cells are easy to fabricate and have an energy conversion efficiency close to that of thin-film silicon, so there is a growing demand for assembly kits for dye-sensitized solar cells as educational materials and for research purposes.
[0005] For example, Patent Document 1 describes a dye-sensitized solar cell production kit consisting of a photoelectrode member, a counter electrode member, and an electrolyte. In this dye-sensitized solar cell production kit, the counter electrode member is an opaque conductive substrate made of metal foil on which a conductive redox catalyst layer containing graphite is formed using a pencil. In addition, in the center of the photoelectrode member, a dye-sensitized semiconductor fine particle layer is formed on the conductive substrate. Then, using the dye-sensitized solar cell kit, the electrolyte is dropped onto the conductive redox catalyst layer using a dropper, and then the dye-sensitized semiconductor layer of the photoelectrode member and the conductive redox catalyst layer of the counter electrode member are placed so that they face each other, and the two electrode members are bonded together to produce a dye-sensitized solar cell. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Patent No. 5172166 Summary of the Invention [Problem to be solved by the invention]
[0007] However, in the dye-sensitized solar cell production kit described in Patent Document 1, the sensitizing dye is pre-adsorbed onto the semiconductor particles, and therefore the person constructing the dye-sensitized solar cell production kit cannot freely color or draw letters or patterns.
[0008] Therefore, an object of the present invention is to provide a dye-sensitized solar cell production kit that allows a craftsman of the kit to freely color or draw letters or patterns. [Means for solving the problem]
[0009] The above object of the present invention can be achieved by the following configuration [1] relating to a dye-sensitized solar cell production kit.
[0010] [1] A kit for producing a dye-sensitized solar cell, which is constructed by sandwiching an electrolyte layer between a semiconductor electrode having dye-sensitized semiconductor particles and a counter electrode, A dyeing substrate in which a semiconductor layer made of the semiconductor particles is formed on an electrode base material via a conductor; a writing instrument containing an ink having a sensitizing dye; an electrolyte container containing an electrolyte; A frame for sealing the electrolyte; A counter electrode, A dye-sensitized solar cell manufacturing kit comprising:
[0011] Further, preferred embodiments of the present invention relating to a dye-sensitized solar cell production kit relate to the following items [2] to [7].
[0012] [2] The dye-sensitized solar cell production kit described in [1], characterized in that the writing instrument is at least one of a marking pen filled with the ink, a brush pen filled with the ink, and a set of a brush and an ink container containing the ink. [3] The dye-sensitized solar cell production kit according to [1] or [2], characterized in that the writing implement is constituted by a multi-color set of inks having different colors. [4] The dye-sensitized solar cell production kit according to any one of [1] to [3], characterized in that the electrolyte solution contains an iodine-iodide redox couple and the ratio of the molar amount of triiodide ions to the molar amount of iodide ions is less than 1%. [5] The kit for producing a dye-sensitized solar cell according to any one of [1] to [4], wherein the electrode substrate constituting the counter electrode is transparent or semi-transparent. [6] The kit for producing a dye-sensitized solar cell according to any one of [1] to [5], wherein a solvent contained in the electrolytic solution is isopropanol or 3-methoxy-3-methylbutanol. [7] The dye-sensitized solar cell production kit according to any one of [1] to [6], further comprising a base layer formed on the semiconductor layer and made of a plurality of microparticles for preventing bleeding.
[0013] The above object of the present invention can be achieved by the following configurations [8] and [9] relating to a method for assembling a dye-sensitized solar cell.
[0014] [8] A method for assembling a dye-sensitized solar cell using the dye-sensitized solar cell production kit according to any one of [1] to [6], comprising the steps of: a method for assembling a dye-sensitized solar cell, comprising the steps of: coloring or drawing characters or a pattern using the writing instrument on the portion of the dyeing substrate where the semiconductor layer is formed; attaching the frame; filling the frame with the electrolyte; and then attaching the counter electrode to the frame. [9] A method for assembling a dye-sensitized solar cell using the dye-sensitized solar cell production kit according to [7], a method for assembling a dye-sensitized solar cell, comprising the steps of: coloring or drawing characters or a pattern using the writing instrument on the portion of the dyeing substrate where the undercoat layer is formed; attaching the frame; filling the frame with the electrolyte; and then attaching the counter electrode to the frame. Effect of the Invention
[0015] According to the present invention, it is possible to provide a dye-sensitized solar cell production kit on which a craftsman of the dye-sensitized solar cell production kit can freely color or draw letters or patterns. [Brief description of the drawings]
[0016] [Figure 1] FIG. 1 is a schematic diagram showing the main contents of a dye-sensitized solar cell kit according to one embodiment of the present invention, in which (A) shows a dyeing substrate, (B) shows a writing implement, (C) shows an electrolyte container, (D) shows a frame, and (E) shows a counter electrode. [Diagram 2] FIG. 2 is a cross-sectional view that illustrates a schematic configuration of a dyeing substrate that is a part of the dye-sensitized solar cell kit according to one embodiment of the present invention. [Diagram 3] FIG. 3 is a cross-sectional view that illustrates a counter electrode that is a part of the dye-sensitized solar cell kit according to one embodiment of the present invention. [Figure 4] FIG. 4 is a schematic diagram showing a procedure 1 for assembling a dye-sensitized solar cell using a dye-sensitized solar cell kit according to one embodiment of the present invention. [Diagram 5] FIG. 5 is a schematic diagram showing a procedure 2 for assembling a dye-sensitized solar cell using the dye-sensitized solar cell kit according to one embodiment of the present invention. [Figure 6] FIG. 6 is a schematic diagram showing a procedure 3 for assembling a dye-sensitized solar cell using the dye-sensitized solar cell kit according to one embodiment of the present invention. [Figure 7] FIG. 7 is a schematic diagram showing a procedure 4 for assembling a dye-sensitized solar cell using the dye-sensitized solar cell kit according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] Hereinafter, the embodiments of the present invention will be described in detail with reference to the drawings. Note that the present invention is not limited to the embodiments described below, and can be modified and implemented as desired without departing from the gist of the present invention.
[0018] [Dye-sensitized solar cell kit] FIG. 1 shows a schematic diagram of the main contents of the dye-sensitized solar cell kit. FIG. 1(A) shows a dyeing substrate 10, FIG. 1(B) shows a writing implement 20, FIG. 1(C) shows an electrolyte container 30, FIG. 1(D) shows a frame 40, and FIG. 1(E) shows a counter electrode 50. These contents are all contained in a kit container (not shown) such as a box or bag. Note that the dye-sensitized solar cell kit according to one embodiment of the present invention is only required to be composed of at least the dyeing substrate 10, the writing implement 20, the electrolyte container 30, the frame 40, and the counter electrode 50, and may further include other accessories as necessary.
[0019] (Substrate for dyeing 10) As shown in Fig. 2, the dyeing substrate 10 (semiconductor electrode) is configured by sequentially forming a semiconductor layer 14 made of countless semiconductor particles 13 (semiconductor fine particles) having a single or multiple particle diameters, and further a base layer 15 made of a plurality of fine particles 16 for preventing bleeding, on one surface of an electrode base material 11, via a conductor 12. Note that, although it is preferable for the dyeing substrate 10 in the dye-sensitized solar cell kit of the present invention to have the base layer 15, the base layer 15 is not necessarily essential.
[0020] The material of the electrode substrate 11 is not particularly limited, and for example, a glass plate, a plastic plate, a plastic film, a metal plate such as a stainless steel plate, etc. can be used.
[0021] The conductor 12 may be made of metals such as platinum, gold, silver, ruthenium, aluminum, nickel, cobalt, chromium, iron, molybdenum, titanium, tantalum, and alloys thereof, or carbon materials such as graphite, carbon black, glassy carbon, carbon nanotubes, and fullerenes. Metal oxides such as FTO, ITO, ATO, zinc oxide, IZO, GZO, and AZO may also be used.
[0022] The semiconductor particles 13 are preferably porous metal oxide semiconductors, such as titanium oxide, zinc oxide, and tin oxide, and are particularly preferably titanium dioxide, and more preferably anatase titanium dioxide. A semiconductor layer 14 made of the semiconductor particles 13 is then stacked, and a base layer 15 made of a plurality of fine particles 16 is then stacked thereon, thereby forming a printed semiconductor layer 17 as a whole. The portion on which this printed semiconductor layer 17 is formed becomes the printed region 10a (see FIG. 1, FIG. 4, etc.).
[0023] The semiconductor layer 14 is formed by stacking semiconductor particles 13 to a predetermined thickness. The semiconductor layer 14 may be formed by stacking semiconductor particles 13 of uniform particle size in layers, but is preferably formed as a two-layer structure in which the conductor 12 side is a layer of small diameter particles and a layer of large diameter particles is stacked on top of that, as shown in Fig. 2. With such a two-layer structure, it is possible to utilize the "light containment effect" that scatters incident light in a layer of large diameter particles to lengthen the optical path length. In this case, the average particle size of the small diameter particles is preferably 100 nm or less, and the average particle size of the large diameter particles is preferably 200 nm to 700 μm.
[0024] Furthermore, the semiconductor layer 14 may have a multi-layer structure of three or more layers, and may be laminated so that the particles have larger diameters in order from the side closer to the conductor 12. In this case, the optimum thickness of the semiconductor layer 14 varies depending on the oxide used and its average particle size, but it is preferable that the layer closest to the conductor 12 is 5 to 15 μm and the layer farthest from the conductor 12 is 3 to 10 μm.
[0025] The semiconductor layer 14 can be formed by, for example, a sol-gel method, coating of a dispersion paste, or electrodeposition or electrodeposition. The thickness of the semiconductor layer 14 is not particularly limited because the optimum value differs depending on the oxide used, but is 0.1 μm to 50 μm, preferably 3 to 30 μm, and more preferably 5 to 15 μm.
[0026] In addition, since letters and pictures are colored or drawn on the drawn semiconductor layer 17 using a writing instrument 20, a porous base layer 15 (porous layer) is formed on the semiconductor layer 14 to prevent the letters and pictures from bleeding and to prevent the letters and pictures from bleeding.
[0027] The underlayer 15 is made of inorganic or organic fine particles bound by a binder resin, and has a porous structure with many fine voids formed by the fine particles and the binder resin. Then, ink containing a sensitizing dye is applied to the underlayer 15, and the solvent in the ink is evaporated, so that the sensitizing dye is adsorbed to the semiconductor layer. At that time, the ink droplets that reach the underlayer 15 gradually penetrate into the fine voids formed by the fine particles 16 and the binder resin, and further penetrate into the voids of the semiconductor particles 13 of the semiconductor layer 14, and when the solvent in the ink evaporates, the sensitizing dye coats the semiconductor particles 13 of the semiconductor layer 14, and the sensitizing dye is adsorbed to the semiconductor particles 13. At the same time, the sensitizing dye remains in the voids of the underlayer 15 (the sensitizing dye adheres to the voids), so that the underlayer 15 reflects the pattern of the sensitizing dye. The sensitizing dye may be adsorbed onto the entire surface of the semiconductor particle 13, or may be adsorbed onto only a portion of the surface of the semiconductor particle 13.
[0028] In contrast, when the underlayer 15 is made of only a binder resin, there are no voids between the fine particles 16 and the binder resin, and the sensitizing dye does not penetrate into the voids, so that a small amount of the sensitizing dye reaches the semiconductor layer 14. In addition, the solvent contained in the droplets swells the binder resin, causing the pattern and color of the sensitizing dye to become blurred.
[0029] To form the underlayer 15, an ink containing inorganic or organic fine particles 16, a binder resin, and a crosslinking agent is applied to the semiconductor layer 14 and dried.
[0030] The type of inorganic fine particles is not particularly limited, and examples thereof include fine particles of silica, kaolinite, talc, light calcium carbonate, heavy calcium carbonate, zeolite, alumina, barium sulfate, carbon black, zinc oxide, zinc sulfate, zinc carbonate, titanium dioxide, satin white, aluminum silicate, diatomaceous earth, calcium silicate, aluminum hydroxide, hydrated halloysite, magnesium carbonate, magnesium hydroxide, etc. The type of organic fine particles is also not particularly limited, and examples thereof include fine particles of acrylic or methacrylic, vinyl chloride, vinyl acetate, nylon, styrene / acrylic, styrene / butadiene, polystyrene / acrylic, polystyrene / isoprene, methyl methacrylate / butyl methacrylate, melamine, polycarbonate, urea, epoxy, urethane, phenol, diallyl phthalate, polyester, etc. Among them, silica is preferred from the viewpoints of low refractive index, cost, etc., and synthetic amorphous silica having pores on the surface is more preferred.
[0031] Moreover, the particle diameter of the fine particles 16 is preferably 100 μm or less. If the fine particles 16 are larger than 100 μm, the surface of the underlayer 15 becomes rough, and the pattern of the sensitizing dye becomes disordered. There is no lower limit to the particle diameter, but the smaller the particle diameter, the denser the underlayer 15 becomes, and the narrower the voids become, making it difficult for the droplets to penetrate.
[0032] Furthermore, the fine particles 16 may be surface-modified. The surface modification improves the dispersibility of the fine particles 16 in the underlayer 15, and improves the adhesion to the binder resin. Examples of surface treatment include chemical treatment using organic silane, organic titanate, etc., and physical treatment of adhering paraffin wax or glycol to the surface.
[0033] The binder resin preferably has high binding ability with the fine particles 16 and the metal oxide semiconductor forming the semiconductor layer 14, and further preferably has excellent resistance to the solvent of the electrolyte layer. Examples of the binder resin include polyester resin, polyurethane resin, polyester urethane resin, acrylic resin, gum arabic, polyacrylamide, and styrene-butadiene rubber.
[0034] By using a crosslinking agent in combination, water resistance can be improved. As the crosslinking agent, for example, melamine resin, epoxy resin, isocyanate, glyoxal, isoban, borax, urea resin, etc. can be used. The amount of the crosslinking agent added is not particularly limited, but it is preferable to use 0.5 to 50 parts by mass of the crosslinking agent per 100 parts by mass of the binder resin. If the amount of the crosslinking agent is less than 0.5 parts by mass, the water resistance of the undercoat layer may be insufficient, and if it exceeds 50 parts by mass, the film quality and strength of the undercoat layer 15 tend to decrease. In addition, a catalyst compound having a reaction promoting effect of the crosslinking agent may be further added.
[0035] The content of the fine particles 16 in the underlayer 15 is preferably 150 to 250 parts by mass per 100 parts by mass of the binder resin. If the amount of the fine particles 16 is less than 150 parts by mass, a sufficient amount of voids is not formed. On the other hand, if the amount of the fine particles 16 exceeds 250 parts by mass, the amount of the binder resin is too small, which reduces the strength of the underlayer 15 and reduces the adhesion to the semiconductor layer 14. However, from the viewpoint of the writing feel when drawing and the strength of the base layer 15, it is preferable that the microparticles 16 are silica, and it is also preferable that the binder resin is a polyurethane-based resin. In this case, it is preferable that the silica content be 100 parts by mass or more and 150 parts by mass or less per 100 parts by weight of the binder resin.
[0036] In addition, various additives such as surfactants, fluorescent dyes, fluorescent brightening agents, plasticizers, UV absorbers, pigment dispersants, foam inhibitors, defoamers, preservatives, etc. may be added to the undercoat layer 15 in appropriate amounts depending on the purpose.
[0037] The thickness of the underlayer 15 is preferably 2 to 100 μm. As described above, the ink droplets penetrate the underlayer 15 and are adsorbed to the semiconductor layer 14. However, if the underlayer 15 is thinner than 2 μm, many droplets do not penetrate, and the pattern and color of the sensitizing dye become blurred. If the underlayer 15 is thicker than 100 μm, the ink droplets cannot penetrate the underlayer 15 and reach the semiconductor layer 14, and the dye becomes difficult to adsorb to the semiconductor layer 14. When silica fine particles are used as the fine particles 16, the thickness is preferably 5 to 50 μm.
[0038] (writing implements 20) The writing instrument 20 may be, for example, a pen that contains ink containing a sensitizing dye and a solvent, or a brush that is applied with ink. Specifically, the writing instrument 20 is preferably at least one of a marking pen (including a felt-tip pen) filled with ink, a brush pen filled with ink, and a set of a brush and an ink container that contains ink.
[0039] Examples of sensitizing dyes contained in writing instruments include metal complex dyes such as ruthenium complexes, iron complexes, and copper complexes, cyan dyes, porphyrin dyes, polyene dyes, coumarin dyes, cyanine dyes, squaric acid dyes, methine dyes, xanthene dyes, and indoline dyes. Although only one type of sensitizing dye may be used, a plurality of types may be mixed to express a desired color.
[0040] The solvent contained in the writing instrument is not limited as long as it is capable of dissolving the sensitizing dye, and examples of the solvent that can be used include alcohols such as ethanol, propanol, butanol, 3-methoxy-3-methylbutanol, and ethylene glycol, organic solvents such as toluene, acetone, acetonitrile, chloroform, dimethylformamide, γ-butyrolactone, and propylene carbonate, and water. However, it is also necessary for the solvent to be safe for the human body so that it will not cause harm to the human body if it is ingested or comes into contact with the skin. Therefore, alcohols such as ethanol and 3-methoxy-3-methylbutanol, which are safe for the human body, and water are preferred. In addition, the solvent contained in the writing instrument preferably has a high boiling point, since this reduces friction during drawing to make drawing easier and is highly effective in preventing peeling of the drawn semiconductor layer 17. However, if the boiling point is too high, it will take a long time for the ink to dry, so a solvent with an appropriately high boiling point, such as 3-methoxy-3-methylbutanol, is preferred.
[0041] The concentration of the sensitizing dye in the ink can be adjusted depending on the type of dye and solvent used, viscosity, etc., but is preferably 0.1 mM to 50 mM. If the sensitizing dye concentration is lower than 0.1 mM, the amount of the dye adsorbed to the semiconductor particles 13 is too small, resulting in insufficient light absorption effect. If the sensitizing dye concentration exceeds 50 mM, the dye may not be completely dissolved, which may cause clogging of the pen tips of marking pens and brush pens in particular. In addition to the sensitizing dye and the solvent, the ink for the writing instrument may contain, as appropriate, commonly used additives such as a sensitizing dye dissolving aid, a resin, a leveling agent, a surfactant, etc.
[0042] Furthermore, the writing instrument 20 can be a multi-color set consisting of a plurality of different ink colors, as shown in Fig. 1. For example, the writing instrument 20 can be composed of a writing instrument 20a containing ink containing a red sensitizing dye, a writing instrument 20b containing ink containing a yellow sensitizing dye, a writing instrument 20c containing ink containing a blue sensitizing dye, and so on.
[0043] Then, the worker of the dye-sensitized solar cell manufacturing kit uses the writing tool 20 to freely color or draw characters or patterns in the drawing area 10a of the dyeing substrate 10. At that time, the ink from the writing tool 20 soaks into the base layer 15 and further into the semiconductor layer 14, so that the sensitizing dye in the ink is adsorbed to the semiconductor layer 14. Therefore, in order to prevent the drawing semiconductor layer 17 from being damaged by the contact part (i.e., the pen tip or brush tip) of the writing tool 20 with the drawing semiconductor layer 17, it is preferable to use a writing tool 20 made of a relatively soft material such as the above-mentioned marking pen, brush pen, or brush and ink set. Note that the pen tip is preferably a porous molded product made of fiber bundle, felt, resin, etc., and ink is supplied to the pen tip by capillary action to enable writing.
[0044] (Electrolyte container 30) The electrolyte container 30 contains an electrolyte. The electrolyte is a solution in which a redox pair is dissolved in a solvent, and must be transparent or nearly transparent so that letters and patterns colored or drawn on the semiconductor layer 14 can be seen. The electrolyte must also be safe for the human body so that it will not cause harm to the human body even if it is ingested or comes into contact with the skin.
[0045] As the redox couple, an iodine-based redox couple with excellent photoelectric conversion efficiency can be used. Iodine is used in mouthwashes and disinfectants as well as in thyroid treatment, and is safe for the human body. However, the electrolyte has a brownish hue, so it is important to avoid the presence of iodide ions (I - ) to the molar amount of triiodide ion (I3 - ) molar ratio (I3 - / I - It is preferable that the "ratio" is less than 1%.
[0046] In addition, as the solvent contained in the electrolyte, a non-aqueous organic solvent, a room temperature molten salt, a protic organic solvent, etc. can be used. For example, nitrile compounds such as acetonitrile, methoxyacetonitrile, 3-methoxypropionitrile, etc., lactone compounds such as γ-butyrolactone and valerolactone, carbonate compounds such as ethylene carbonate and propylene carbonate, ester compounds such as ethyl acetate and polysorbate, ethers such as dioxane, diethyl ether, ethylene glycol dialkyl ether, and low polymerization degree polyethylene glycol, alcohols such as methanol and ethanol, sulfonic acids such as sulfolane, ethyl methyl sulfone, and ethyl isopropyl sulfone, dimethylformamide, imidazoles, etc. are also required to be excellent in safety to the human body so that they do not cause harm to the human body even if they are ingested or attached to the skin. In addition, the solvent contained in the electrolyte is preferably one that is in a range that is excellent in safety for the human body and has a melting point of 10° C. or less and has a low dissolving ability for the sensitizing dye. For example, in the case of alcohols, those with a large number of carbon atoms, particularly those with 3 or more carbon atoms, are preferred, and specifically, isopropanol or 3-methoxy-3-methylbutanol is more preferred than ethanol. These solvents also have the advantage of being less likely to fade.
[0047] The electrolyte container 30 itself may be a dropper, an eye dropper, or the like.
[0048] (Frame 40) The frame 40 is a member that surrounds the drawing area 10a of the dyeing substrate 10, and in FIG. 1, a rectangular frame is shown as an example. An electrolyte solution is injected into the frame of the frame 40. When the dyeing substrate 10 and the counter electrode 50 are bonded together, the electrolyte solution is sealed together with the frame 40 to form an electrolyte layer. The frame 40 can be made of, for example, resin.
[0049] (Counter electrode 50) As shown in FIG. 3, the counter electrode 50 is configured by forming a catalyst layer 58 on the surface of an electrode base material 55. The catalyst layer 58 in the figure is the electrolyte layer side. The electrode base material 55 is used as a support and current collector for the catalyst layer 58, so that an electrode substrate 56 having a conductor 57 formed on its surface is preferable. The electrode substrate 56 can be a glass plate or a plastic plate, and the conductor 57 can be a metal such as platinum, gold, silver, ruthenium, aluminum, nickel, cobalt, chromium, iron, molybdenum, titanium, tantalum, and alloys thereof, or a carbon material such as graphite, carbon black, glassy carbon, carbon nanotubes, or fullerene. Metal oxides such as FTO, ITO, ATO, zinc oxide, IZO, GZO, and AZO can also be used.
[0050] There are no particular limitations on the catalyst layer 58, so long as it has electrode properties that enable the rapid transfer of electrons to and from the electrolyte layer made of an electrolytic solution. For example, a platinum catalyst electrode coated with chloroplatinic acid and heat-treated, a platinum-deposited platinum catalyst electrode, a carbon material such as activated carbon, glassy carbon, or carbon nanotubes, an inorganic compound such as cobalt chloride, or a conductive polymer such as polythiophene, polypyrrole, or polyaniline can be used, with platinum catalyst electrodes and conductive polymers being preferred.
[0051] As described later in the assembly method of the dye-sensitized solar cell, it is preferable that the counter electrode 50 is transparent or semi-transparent so that the characters or pictures on the dyeing substrate 10 can be seen. For this reason, it is preferable that the electrode substrate 56 of the counter electrode 50 is a transparent glass plate or plastic plate, the conductor 57 is a metal oxide, and the catalyst layer 58 is a conductive polymer.
[0052] [How to assemble dye-sensitized solar cells] Hereinafter, steps 1 to 4 for assembling a dye-sensitized solar cell using a dye-sensitized solar cell kit according to one embodiment of the present invention will be described with reference to FIGS.
[0053] (Step 1) The dye-sensitized solar cell kit according to one embodiment of the present invention is composed of at least the above-mentioned contents. To assemble a dye-sensitized solar cell using this dye-sensitized solar cell kit, first, as shown in Fig. 4, a worker of the dye-sensitized solar cell manufacturing kit uses a writing implement 20 to freely color or draw characters or patterns on the drawing area 10a on the dyeing substrate 10 on which the drawing semiconductor layer 17 is formed.
[0054] (Step 2) 5, a frame 40 is attached so as to surround the drawing area 10a of the dyeing substrate 10. The frame 40 may be fixed to the dyeing substrate 10 using an adhesive or a double-sided adhesive tape.
[0055] (Step 3) Next, as shown in FIG. 6, the electrolyte 31 in the electrolyte container 30 is poured into the frame of the frame 40.
[0056] (Step 4) 7, the counter electrode 50 is attached to the frame 40 in a direction in which the catalyst layer 58 contacts the frame 40. In order to maintain the attached state, it is also preferable to clamp the dyeing substrate 10, the frame 40, and the counter electrode 50 in a stacked state with a clip 60 as shown in the figure. In addition, when attaching the counter electrode 50, it may be fixed to the frame 40 using an adhesive or a double-sided adhesive tape.
[0057] The dye-sensitized solar cell is completed by the above steps 1 to 4. Then, the dyeing substrate 10 and the counter electrode 50 of the completed dye-sensitized solar cell are electrically connected to a device 65 such as a light bulb or a motor with blades, and it can be confirmed that the solar cell generates electricity by irradiating the solar cell with light.
[0058] Although light may be irradiated from the dyeing substrate 10 side and the letters and patterns viewed from the same direction as the irradiation, there is a problem that the letters and patterns may appear inverted. Therefore, the electrode substrate 56, the conductor 57, and the catalyst layer 58 of the counter electrode 50 are made transparent or semi-transparent, and the letters and patterns are viewed by irradiating light from the counter electrode 50 side, so that the letters and patterns can be viewed without being inverted.
[0059] As described above, the completed dye-sensitized solar cell is colored or painted with letters and pictures by the craftsman, making it rich in design and artistic value. EXAMPLES
[0060] An example of the dye-sensitized solar cell produced using the above-mentioned dye-sensitized solar cell production kit will be described below.
[0061] (Preparation of dyeing substrate 10) Glass with a highly durable transparent conductive film manufactured by Geomatec Co., Ltd. was cut to a predetermined size, and ultrasonic cleaning was performed in the order of glass cleaning agent and pure water for 10 minutes each to prepare an electrode substrate 11. After drying, the electrode substrate 11 was immersed in a titanium tetrachloride aqueous solution (manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) at 70°C for 30 minutes. After immersion, it was washed with pure water and dried. Then, a titanium oxide paste ("Ti-Nanoxide T / SP" manufactured by Sоlarоnix) was applied to the surface of the transparent conductive film by a screen printing method, left to stand at 120°C for about 3 minutes, and dried to form a layer made of small diameter particles. On top of that, a titanium oxide paste ("Ti-Nanoxide D / SP" manufactured by Sоlarоnix) was applied by a screen printing method, left to stand at 120°C for about 3 minutes, and dried to form a layer made of large diameter particles. Then, it was fired at 500°C in the air to obtain a semiconductor layer 14 made of a porous metal oxide having a thickness of about 10 μm.
[0062] Next, a binder resin "IJ-200" manufactured by Takamatsu Oil Co., Ltd. was added to an inkjet receiving layer solution "MZ-480" manufactured by Takamatsu Oil Co., Ltd. to prepare a mixed solution. This mixed solution was applied to a thickness of about 100 μm on the semiconductor layer 14 by a bar coating method and dried at 120° C. for about 3 minutes to form the underlayer 15, thereby obtaining the drawn semiconductor layer 17. Note that "MZ-480" manufactured by Takamatsu Oil Co., Ltd. contains silica fine particles (fine particles 16), and the underlayer 15 is porous. At this time, the ratio of the amount of the inkjet receiving layer solution to the amount of the binder resin was changed, and the peel strength of the drawn semiconductor layer 17 was measured. The results are shown in Table 1.
[0063] (writing implements 20) A cyan dye ("Sensidizer SQ2" manufactured by Sоlarоnix) was dissolved in a solvent as a sensitizing dye to prepare an ink with a dye concentration of 2.0 mM, which was then filled into a marking pen to prepare a writing instrument 20. In this case, ethanol or 3-methoxy-3-methylbutanol was used as the solvent, and a writing test was carried out to evaluate the writing performance.
[0064] The writing test evaluated the peel strength of the drawn semiconductor layer 17 and the dynamic friction coefficient during drawing. For the measurement, a friction and wear tester "UMT_TriboLAB" manufactured by Bruker was used, and the marking pen was fixed at an angle of 90°. The test conditions were that the load was changed from 25 gf to 200 gf, the writing speed was 1 cm / sec, the writing distance was 3 cm, and the marking pen was moved back and forth twice at the same location, and the occurrence of peeling at the written location and the dynamic friction coefficient were measured. The results are shown in Table 1.
[0065] In addition, the photoelectric conversion characteristics of the dye-sensitized solar cell having the above-mentioned configuration were evaluated. The dyeing substrate 10 was dyed by filling an 8 mm square area on the drawing semiconductor layer 17 with the above-mentioned marking pen filled with a cyan dye dissolved in ethanol without applying an additional coat.
[0066] (Counter electrode 50) Glass with a highly durable transparent conductive film manufactured by Geomatec Co., Ltd. was cut to a predetermined size and ultrasonically cleaned with a glass cleaner and then with pure water for 10 minutes each to produce an electrode substrate 55. After drying, "Denatron PT-448" manufactured by Nagase ChemteX Co., Ltd. was applied using a bar coater and dried at 130°C for about 5 minutes to form a catalyst layer 58, which was used as a counter electrode 50.
[0067] (Electrolyte 31) An electrolyte solution 31 was prepared by dissolving sodium iodide in 3-methoxy-3-methylbutanol to a concentration of 0.2 M.
[0068] The electrolyte solution 31 was filled between the dyeing substrate 10 and the counter electrode 50 using the frame 40 to form an electrolyte layer, thereby producing a dye-sensitized solar cell. For the frame 40, Himilan "PECHM", a heat-sealable film manufactured by Peccell Technologies, was cut into a predetermined shape and used.
[0069] To evaluate the photoelectric conversion characteristics, a white LED light irradiation device "C-FLED2" manufactured by Nikon Corporation was used to measure the maximum output (Pmax) at approximately 700 lux. The results are shown in Table 2.
[0070] [Table 1]
[0071] [Table 2]
[0072] As shown in Table 1, the semiconductor layer 17 becomes more difficult to peel as the ratio of the binder resin increases, and it can be said that a ratio of the binder resin of 30 mass % or more is preferable. In addition, as for the solvent used in the writing implement 20, 3-methoxy-3-methylbutanol is more difficult to peel than ethanol, and the dynamic friction resistance is also smaller, so there is less catching when writing and the writing experience is smoother.
[0073] Furthermore, as shown in Table 2, the maximum output Pmax tends to decrease as the ratio of the binder resin increases, so the ratio of the binder resin is preferably 50 mass % or less, and more preferably 40 mass % or less. [Explanation of symbols]
[0074] 10. Dyeing Substrate 10a drawing area 11 Electrode base material 12 Conductors 13 Semiconductor particles 14 Semiconductor layer 15 Base layer 16 Fine particles 17 Drawing semiconductor layer 20 Writing instruments 30 Electrolyte container 31 Electrolyte 40 Frame 50 Counter electrode 55 Electrode base material 56 Electrode Substrate 57 Conductors 58 Catalyst layer 60 clips 65 Devices
Claims
1. A kit for producing a dye-sensitized solar cell, which is constructed by sandwiching an electrolyte layer between a semiconductor electrode having dye-sensitized semiconductor particles and a counter electrode, A dyeing substrate in which a semiconductor layer made of the semiconductor particles is formed on an electrode base material via a conductor; a writing instrument containing an ink having a sensitizing dye; an electrolyte container containing an electrolyte; A frame for sealing the electrolyte; A counter electrode, A dye-sensitized solar cell manufacturing kit comprising:
2. The dye-sensitized solar cell production kit according to claim 1, characterized in that the writing instrument is at least one of a marking pen filled with the ink, a brush pen filled with the ink, and a set of a brush and an ink container containing the ink.
3. 2. The dye-sensitized solar cell production kit according to claim 1, wherein the writing implement is constituted by a multi-color set having inks of different colors.
4. 2. The dye-sensitized solar cell production kit according to claim 1, wherein the electrolyte solution contains an iodine-iodide redox couple, and the ratio of the molar amount of triiodide ions to the molar amount of iodide ions is less than 1%.
5. 2. The kit for producing a dye-sensitized solar cell according to claim 1, wherein the electrode substrate constituting the counter electrode is transparent or semi-transparent.
6. 2. The dye-sensitized solar cell production kit according to claim 1, wherein a solvent contained in the electrolytic solution is isopropanol or 3-methoxy-3-methylbutanol.
7. 2. The dye-sensitized solar cell production kit according to claim 1, further comprising a base layer formed on the semiconductor layer and made of a plurality of fine particles for preventing bleeding.
8. A method for assembling a dye-sensitized solar cell using the dye-sensitized solar cell production kit according to any one of claims 1 to 6, comprising the steps of: a method for assembling a dye-sensitized solar cell, comprising the steps of: coloring or drawing characters or a pattern using the writing instrument on the portion of the dyeing substrate where the semiconductor layer is formed; attaching the frame; filling the frame with the electrolyte; and then attaching the counter electrode to the frame.
9. A method for assembling a dye-sensitized solar cell using the dye-sensitized solar cell production kit according to claim 7, comprising the steps of: a method for assembling a dye-sensitized solar cell, comprising the steps of: coloring or drawing characters or a pattern using the writing instrument on the portion of the dyeing substrate where the undercoat layer is formed; attaching the frame; filling the frame with the electrolyte; and then attaching the counter electrode to the frame.
Citation Information
Patent Citations
Shotsukiaraiki
JP1976072166A