Flooring material

The laminated flooring material with a surface and cold press molding layer addresses the limitations of existing materials by maintaining intricate designs and allowing complex three-dimensional shapes, achieving high design quality and functional enhancements.

JP2024155958AActive Publication Date: 2024-10-31TOLI +1
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2024139106
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-10-31
Estimated Expiration
2040-09-07

AI Technical Summary

Technical Problem

Existing flooring materials with surface patterns are limited to sheet-like planar shapes and struggle to maintain intricate designs, such as three-dimensional structures and detailed patterns, due to manufacturing process constraints.

Method used

A flooring material composed of a laminated structure with a surface layer and a cold press molding layer, where the surface layer features a three-dimensionally formed uneven pattern and the cold press molding layer is molded into any shape during cooling, integrated by thermal fusion, ensuring high design quality and free formability.

Benefits of technology

The laminated structure maintains intricate surface patterns without deformation and allows for complex three-dimensional shapes, enhancing design quality, anti-slip properties, and providing sound insulation and drainage, while being efficiently manufactured in a single step.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024155958000001_ABST
    Figure 2024155958000001_ABST
Patent Text Reader

Abstract

To provide a flooring material capable of achieving both high design quality and free formability.SOLUTION: A flooring material 1A consists of a surface layer 2 and a cold-pressed molding layer 3 laminated together. The surface layer 2 and the cold-pressed molding layer 3 are made of the same type of material. The surface layer 2 has an uneven pattern and the uneven pattern is given to the surface layer before lamination. The cold-pressed molding layer 3 has a three-dimensional structure formed in a vertical or horizontal direction with respect to a lamination surface.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a flooring material having a pattern or design on its surface, and a method for manufacturing the flooring material. [Background technology]

[0002] Flooring materials with patterns or textured patterns on the surface have been known (see, for example, Patent Document 1). The flooring material in Patent Document 1 is composed of a laminate in which multiple layers are superimposed and passed between a pair of rolls to be fused and integrated by applying pressure and heat. This laminate is passed between an embossing roll and a receiving roll, and at that time, the textured pattern of the embossing roll is transferred to the surface of the laminate.

[0003] As a means for integrating multiple layers, in addition to the above-mentioned heat fusion, there are known methods for bonding multiple layers together, such as "cold pressing," in which multiple layers are stacked together with an adhesive interposed therebetween and pressed at room temperature, and "hot pressing," in which further heat is applied after cold pressing (see, for example, Patent Documents 2 and 3).

[0004] Regarding cold pressing, a method for producing a resin molded product has been put into practical use in which a resin material is heated to a plasticization temperature higher than the softening temperature (softening point) of the base thermoplastic resin to make it plastic, and then the resin material is placed inside a mold consisting of an upper mold and a lower mold, and then molded into a predetermined shape by applying pressure while being cooled in the mold (see, for example, Patent Document 4). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2017-20248 A [Patent Document 2] International Publication No. 2012 / 053036 [Patent Document 3] JP 2002-18807 A [Patent Document 4] JP 2017-177692 A Summary of the Invention [Problem to be solved by the invention]

[0006] The flooring material disclosed in Patent Document 1 can be given a certain degree of designability because an embossed pattern can be formed on the surface using an embossing roll. However, the laminate constituting the flooring material is formed by passing multiple layers, in a superimposed state, between a pair of rolls under pressure and heat, and therefore the formed product is limited to a flat sheet-like shape due to the constraints of the manufacturing process, and it is difficult to form it into a free three-dimensional shape, especially a three-dimensional shape that exceeds the thickness of the sheet.

[0007] Even in the integration method by cold pressing as disclosed in Patent Document 2, the molded product is limited to a flat sheet shape due to the constraints of the manufacturing process. In Patent Document 3, a hot pressing process is carried out in addition to the cold pressing process, so that, for example, if the surface layer is made of a polyvinyl chloride resin with a pattern or textured pattern, the pattern or textured pattern on the surface will be crushed by thermal deformation and pressure during the pressing process, making it impossible to maintain the design.

[0008] In the cold press molding used in the manufacturing method for resin molded products disclosed in Patent Document 4, a resin material in a plastic state is filled along the shape of a molding cavity formed by clamping an upper mold and a lower mold in a molding die, so that it is possible to mold into any shape according to the shape of the molding cavity, but it is not good at adding fine decoration such as patterns or textured patterns to the surface.

[0009] The present invention has been made in consideration of the above problems, and aims to provide a flooring material that can combine high designability with free formability, and a manufacturing method for said flooring material. [Means for solving the problem]

[0010] The characteristic configuration of the flooring material according to the present invention to solve the above problems is as follows: The sheet is formed by laminating a surface layer and a cold press molded layer.

[0011] According to the flooring material of this configuration, the surface layer and the cold press molded layer are laminated, so that a high design can be applied to the surface side of the surface layer. Examples of the design include a three-dimensional uneven pattern and a two-dimensional pattern. For example, the uneven pattern can be obtained by forming unevenness on the surface by embossing or the like. The pattern means a color or design, and can be obtained by providing a design layer made of a printed film or multicolor chips. The cold press molded layer is a layer formed by pressing the base material of the cold press molded layer, which has been brought to a state above its softening point, while cooling it with a mold. The boundary between the surface layer and the cold press molded layer is integrated by thermal fusion due to the heat of the base material of the cold press molded layer, which has been brought to a state above its softening point, and the pressure during the press process. In the flooring material of this configuration, the surface side of the surface layer is cooled by the mold, although the pressure during the press process acts on it. For this reason, the thermal deformation of the surface side of the surface layer can be suppressed, and as a result, the pattern or uneven pattern applied to the surface side of the surface layer remains without being crushed, and high design can be ensured. On the other hand, in the cold press molding layer, the base material, which is in a state above its softening point, can be molded into any shape until it solidifies by cooling. Therefore, it is possible to achieve both high designability and free moldability that could not be achieved with conventional flooring materials.

[0012] In the flooring material according to the present invention, The surface layer and the cold-press molded layer are preferably made of the same type of material.

[0013] In the flooring material of this configuration, the surface layer and the cold-press molded layer are made of the same type of material, so the boundary between the surface layer and the cold-press molded layer can be more firmly integrated by heat fusion.

[0014] In the flooring material according to the present invention, It is preferable that the surface layer and the cold-press molded layer are made of different materials, and that both layers are laminated via a bonding layer.

[0015] With the flooring material of this configuration, the surface layer and the cold-press molded layer are made of different materials and the two layers are laminated via a bonding layer, so that even if the surface layer and the cold-press molded layer are made of different materials, the surface layer and the cold-press molded layer can be firmly integrated via the bonding layer.

[0016] In the flooring material according to the present invention, The surface layer preferably has an uneven pattern.

[0017] In the flooring material of this configuration, the surface layer has an uneven pattern. This increases the eye-catching power in terms of design, and enhances the texture to create a sense of luxury. Meanwhile, in terms of functionality, the unevenness in the uneven pattern acts as an anti-slip agent, increasing the anti-slip properties. In addition, the elasticity and partial contact of the curved surfaces of the unevenness in the uneven pattern provide a comfortable feel that is not available on a smooth surface.

[0018] In the flooring material according to the present invention, The cold-press molded layer preferably has a three-dimensional structure formed in a vertical or horizontal direction relative to the lamination surface.

[0019] According to the flooring material of this configuration, the cold press molded layer has a three-dimensional structure formed in a vertical or horizontal direction relative to the lamination surface. Here, the "vertical or horizontal direction" includes not only the vertical or horizontal direction relative to the lamination surface, but also an oblique direction inclined relative to the lamination surface. Therefore, the three-dimensional structure includes at least one of a structure having a part extending in a vertical direction, a structure having a part extending in a horizontal direction, and a structure having a part extending in an oblique direction. As a result, in addition to the function of the surface layer, a specific function performed by the three-dimensional structure of the cold press molded layer is added, and the added value of the flooring material can be increased. In detail, in the technology disclosed in Patent Documents 1 to 3, as described above, due to the constraints of the manufacturing process, the molded product is limited to a sheet-like planar shape, and even if the member corresponding to the surface layer of the flooring material of the present invention can be molded, it is not possible to mold a protruding portion with a protruding length greater than the thickness of the surface layer. In the present invention, the cold press molded layer can be molded into a free shape until the base material, which is in a state of being at or above the softening point, is solidified by cooling. Therefore, by setting the shape of the molding cavity of the mold, it is possible to form a protrusion in the cold press molded layer with a protruding length equal to or greater than the thickness of the surface layer. Thus, the flooring material of this configuration has both the uneven pattern of the surface layer and the three-dimensional structure of the cold press molded layer, and can be formed by superimposing a relatively large three-dimensional structure and a small three-dimensional structure. This allows high levels of control over anti-slip properties and drainage properties. Furthermore, the effect of diffuse sound reflection by the curved surface of the uneven pattern and the three-dimensional structure can also be obtained, providing soundproofing, sound insulation and sound absorption effects.

[0020] Next, the characteristic configuration of the manufacturing method of the flooring material according to the present invention is as follows: A method for manufacturing a flooring material comprising laminating a surface layer and a cold-press molded layer, a first placement step of placing the surface layer in a mold; a second disposing step of disposing a thermoplastic resin in a state of not less than its softening point so as to be in contact with the surface layer; a pressing step of pressing the contents of the mold at a temperature lower than the softening point of the thermoplastic resin; a recovery step of removing the laminated molded body formed by the pressing step from the mold; The purpose of this study is to encompass the above.

[0021] According to the manufacturing method of the flooring material of this configuration, the surface layer is placed in the mold, and the thermoplastic resin, which is the base material of the cold press molded layer, which is in a state above the softening point, is placed so as to be in contact with the surface layer. Then, a pressing process is carried out in which the contents of the mold, i.e., the surface layer and the base material of the cold press molded layer, are pressed at a temperature lower than the softening point of the thermoplastic resin. As a result, while the molding of the cold press molded layer progresses with the pressing process, the boundary between the cold press molded layer and the surface layer during molding is integrated by thermal fusion due to the heat of the base material of the cold press molded layer, which is in a state above the softening point, and the pressure during the pressing process. In this way, the laminated molded body formed by the pressing process is removed from the mold and collected. In the manufacturing method of the flooring material of this configuration, the surface side of the surface layer is cooled by the mold, although the pressure during the pressing process acts on it. For this reason, it is possible to suppress thermal deformation of the surface side of the surface layer, and as a result, the uneven pattern imparted to the surface side of the surface layer remains without being crushed, and high designability can be ensured. On the other hand, in the cold press molded layer, the base material, which is in a state above the softening point, can be molded into any shape until it solidifies by cooling. Therefore, it is possible to achieve both high designability and free moldability that could not be achieved with conventional flooring materials. In addition, the manufacturing method of the flooring material of this configuration can be molded in one step compared to a method in which the surface layer and the cold press molded layer are molded separately and then joined together, so that it can be molded quickly and easily, and even complex configurations can be molded accurately, resulting in excellent manufacturing efficiency. [Brief description of the drawings]

[0022] [Figure 1] FIG. 1 is a cross-sectional view showing a schematic diagram of a laminated structure of a flooring material according to a first embodiment of the present invention. [Diagram 2] FIG. 2 shows a schematic diagram of the laminated structure of the surface layer, where (a) is a cross-sectional view of a surface layer with enhanced anti-slip properties, and (b) is a cross-sectional view of a surface layer with enhanced cushioning properties. [Diagram 3] FIG. 3 is a cross-sectional view showing a schematic diagram of a laminated structure of a flooring material according to a second embodiment of the present invention. [Figure 4] FIG. 4 shows a specific example (1) of a flooring material to which the present invention can be applied, where (a) is an overall perspective view of a flooring material for stairs, and (b) is an enlarged view of a main part of the cross section taken along line AA in (a). [Diagram 5] FIG. 5 shows a molding die for molding a staircase floor material, where (a) is a diagram showing a mold release state and (b) is a diagram showing a mold clamping state. [Figure 6] FIG. 6 shows the steps of a manufacturing method for a staircase flooring material, where (a) is an explanatory diagram of the surface layer arrangement process, (b) is an explanatory diagram of the thermoplastic resin arrangement process, (c) is an explanatory diagram of the pressing process, and (d) is an explanatory diagram of the recovery process. [Figure 7] FIG. 7 shows a specific example (2) of a flooring material to which the present invention can be applied, where (a) is a plan view of a flooring material for an entrance hall, and (b) is an enlarged view of a main part of the cut end surface taken along line BB in (a). [Figure 8] FIG. 8 shows a molding die for molding an entrance hall floor material, where (a) is a diagram showing the mold release state and (b) is a diagram showing the mold clamping state. [Figure 9] FIG. 9 shows the steps of the manufacturing method for molding entrance hall flooring, where (a) is an explanatory diagram of the surface layer arrangement process, (b) is an explanatory diagram of the thermoplastic resin arrangement process, (c) is an explanatory diagram of the pressing process, and (d) is an explanatory diagram of the recovery process. [Figure 10] Figure 10 shows the bonding layer arrangement step in the manufacturing method for flooring of the present invention, where (a) is an explanatory diagram of the bonding layer arrangement step in the manufacturing method for flooring for stairs, and (b) is an explanatory diagram of the bonding layer arrangement step in the manufacturing method for flooring for entranceways. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] The flooring material of the present invention and the method for manufacturing the flooring material will be described below with reference to the drawings. In each drawing, the flooring material of the present invention is shown to be composed of multiple layers, but the thickness relationship of each layer has been appropriately exaggerated or simplified for ease of explanation, and does not strictly reflect the size relationship (scale) of the thickness of each layer in the actual flooring material.

[0024] As used herein, the "top surface" or "above" of a layer refers to the surface or direction away from the floor surface (horizontal surface) on which the flooring is laid, and the "bottom surface" or "below" refers to the surface or direction on the opposite side (the side closer to the floor surface on which the flooring is laid).

[0025] First Embodiment <Overall composition of flooring materials> Fig. 1 is a cross-sectional view showing a laminated structure of a flooring material according to a first embodiment of the present invention. The flooring material 1A shown in Fig. 1 has a surface layer 2 and a cold-press molded layer 3, and the surface layer 2 and the cold-press molded layer 3 are laminated from top to bottom in this order.

[0026] <Surface layer> FIG. 2 shows a schematic laminated structure of the surface layer, where (a) is a cross-sectional view of a surface layer with enhanced anti-slip properties, and (b) is a cross-sectional view of a surface layer with enhanced cushioning properties. The surface layer 2 has an uneven pattern (not shown) formed thereon to enhance the design of the flooring material. Examples of the uneven pattern include embossing, a foam structure, debossing, and graining. For example, the surface layer 2A shown in FIG. 2(a) and the surface layer 2B shown in FIG. 2(b) can be used as the surface layer 2. When the anti-slip properties of the flooring material 1A are to be enhanced, the surface layer 2A shown in FIG. 2(a) is used, and when the cushioning properties of the flooring material 1A are to be enhanced, the surface layer 2B shown in FIG. 2(b) is used.

[0027] First, the surface layer 2A that can enhance the anti-slip properties of the flooring material 1A will be described with reference to Fig. 2(a). The surface layer 2A shown in Fig. 2(a) is made up of an abrasion-resistant layer 11, a protective layer 12, a design layer 13, an upper resin layer 14, a resin-impregnated glass sheet 15, and a lower resin layer 16 laminated in this order from top to bottom.

[0028] [Abrasion resistant layer] The abrasion-resistant layer 11 is the layer located on the outermost side, and is not an essential component of the surface layer 2A, but prevents scratches and improves abrasion resistance. The abrasion-resistant layer 11 may be transparent or opaque, but is preferably transparent so that the pattern of the design layer 13 and the like provided on the back side of the protective layer 12 can be seen. The abrasion-resistant layer 11 preferably has a layer thickness of 2 to 50 μm, more preferably 5 to 35 μm, for the reasons that it exhibits scratch resistance while not becoming brittle as a whole and has excellent impact resistance. In particular, a layer thickness of 2 μm or more provides sufficient scratch resistance, and a layer thickness of 50 μm or less provides the flooring material with a rigidity that is not too high as a whole, is less likely to crack, and is excellent in processability.

[0029] The wear-resistant layer 11 is preferably made of an ionizing radiation curable resin such as an ultraviolet curable resin, since it is versatile. Examples of the curable resin include, in addition to an ionizing radiation curable resin such as an ultraviolet curable resin, a thermosetting resin, and a resin cured by non-ionizing radiation. When an ionizing radiation curable resin composition is used, the wear-resistant layer 11 contains a polymerization initiator, various other additives, and an aggregate as necessary. As the resin cured by ionizing radiation, it is preferable to use an ultraviolet curable resin such as a urethane-based, epoxy-based, or acrylic-based resin, since it is easy to process and versatile, and a fluorine resin, silicone resin, or the like may be added. In addition, inorganic particles such as alumina can be used as the aggregate, which can improve anti-slip properties, wear resistance, and durability.

[0030] [Protective layer] The protective layer 12 is a layer provided to facilitate the removal of dirt adhering to the surface layer 2A. In other words, the protective layer 12 imparts dirt removability to the surface layer 2A. The protective layer 12 is provided as necessary. The protective layer 12 may be either transparent or opaque, but is preferably transparent so that the pattern and coloring of the design layer 13 provided on the back side of the protective layer 12 can be visually observed.

[0031] Resin materials are suitable as the material of the protective layer 12. Thermoplastic resins such as polyvinyl chloride resins, polyolefin resins, polyacrylic acid resins, and polyester resins are used as the resin materials, and among these, polyvinyl chloride resins are preferred. The thickness of the protective layer 12 is 0.03 to 1 mm, and preferably 0.1 to 0.8 mm.

[0032] [Design layer] The design layer 13 is a layer that expresses a desired pattern and imparts design to the surface of the surface layer 2A. For example, the design layer 13 is formed of a thermoplastic resin. Examples of the thermoplastic resin include vinyl chloride resin, olefin resin, acrylic resin such as ethylene-vinyl acetate copolymer and ethylene-methacrylate resin, amide resin, ester resin, vinyl acetate, olefin elastomer, styrene elastomer, and various elastomers, rubber, and the like. Among them, vinyl chloride resin is preferable because of its excellent durability and processability. In addition, various additives such as fillers, plasticizers, flame retardants, stabilizers, antioxidants, lubricants, colorants, and foaming agents may be blended into the thermoplastic resin.

[0033] The design layer 13 may be formed of a printed film, may be molded from a thermoplastic resin to which a coloring agent has been added, or may be formed by adding and kneading together resin chips of multiple colors.

[0034] The thickness of the design layer 13 is 0.50 to 1.50 mm, preferably 0.60 to 1.00 mm, and more preferably 0.65 to 0.80 mm.

[0035] In addition, when a pattern is to be expressed by adding a colorant or the like to the upper resin layer 14, the design layer 13 may be omitted.

[0036] [Upper resin layer and lower resin layer] The upper resin layer 14 and the lower resin layer 16 are the main components that determine the strength and weight of the surface layer 2A. The thicknesses of the upper resin layer 14 and the lower resin layer 16 are not particularly limited and can be set appropriately. The thickness of the upper resin layer 14 and the thickness of the lower resin layer 16 may be the same or different. The thickness of the upper resin layer 14 is 0.05 to 1.0 mm, and preferably 0.1 to 0.8 mm. The thickness of the lower resin layer 16 is 0.5 to 3.0 mm, and preferably 0.7 to 2.0 mm.

[0037] Thermoplastic resins are suitable as materials for the upper resin layer 14 and the lower resin layer 16. Examples of thermoplastic resins include polyvinyl chloride resins such as polyvinyl chloride and vinyl chloride-vinyl acetate copolymers; polyolefin resins; polystyrene resins; polyvinyl acetate resins such as ethylene-vinyl acetate copolymers; polyacrylate resins such as polymethyl methacrylate; polyamide resins; polyester resins; and various elastomers such as olefin elastomers and styrene elastomers. These may be used alone or in combination of two or more. At least one of the upper resin layer 14 and the lower resin layer 16 is preferably a resin layer mainly composed of polyvinyl chloride resin, since it has excellent flexibility and is easily bonded to the resin-impregnated glass sheet 15, and it is more preferable that both the upper resin layer 14 and the lower resin layer 16 are mainly composed of polyvinyl chloride resin. The surface layer 2A having a resin layer mainly composed of polyvinyl chloride resin has excellent flexibility, so that it feels good to walk on, and can be curved while being applied to the floor surface. In addition, polyvinyl chloride resin is inexpensive, and the use of this resin makes it easy to manufacture the surface layer 2A. When both the upper resin layer 14 and the lower resin layer 16 are mainly composed of polyvinyl chloride resin, the polyvinyl chloride resins may have the same or different monomer types and polymerization degrees.

[0038] In this specification, the main component refers to the resin component excluding additives, and when there are multiple components (excluding additives) constituting the layer, it refers to the component (weight ratio) with the largest content among them. Examples of the additives include plasticizers, fillers, stabilizers, etc. The content of the main component is more than 50% by mass, preferably 70% by mass or more, and more preferably 80% by mass or more, when the total components constituting the layer are taken as 100% by mass. The upper limit of the content of the main component is 100% by mass. When the content of the main component is less than 100% by mass, the components other than the main component contained in the layer are not particularly limited, and may include conventionally known components.

[0039] [Resin-impregnated glass sheet] The resin-impregnated glass sheet 15 is used to suppress the size variation of the surface layer 2A due to shrinkage and expansion over time, and is a glass sheet containing glass fibers impregnated with resin, although detailed illustrations are omitted. The resin-impregnated glass sheet 15 has the characteristics of glass fibers, such as high strength and small size variation due to temperature, and can increase the mechanical strength such as the size stability and rigidity of the surface layer 2A, and can suppress size change and warping due to temperature change, shrinkage over time, and expansion. The glass sheet, which is the base material of the resin-impregnated glass sheet 15, is made of a layer of multiple fibers overlapping each other, and can be made of glass nonwoven fabric, glass woven fabric, etc., but glass nonwoven fabric is preferably used. Since glass nonwoven fabric has excellent size stability, it greatly contributes to the overall size stability of the surface layer 2A, and can improve the bending strength and tensile strength of the surface layer 2A. In addition, since the fibers of the glass woven fabric are generally regularly arranged, the weave may appear on the surface of the surface layer 2A and affect the appearance of the uneven pattern, but when a glass nonwoven fabric is used, the uneven pattern of the surface layer 2A can be maintained as it is without affecting it. Note that the resin-impregnated glass sheet 15 may be omitted in cases where a large variation in size is acceptable or where the size variation can be suppressed by other configurations.

[0040] The resin to be impregnated into the glass sheet is not particularly limited as long as it adheres to both the upper resin layer 14 and the lower resin layer 16, and a conventionally known resin can be used. Examples of the resin include thermoplastic resins such as those exemplified for the upper resin layer 14 and the lower resin layer 16. When the upper resin layer 14 and the lower resin layer 16 are mainly composed of polyvinyl chloride resin, it is preferable that the resin to be impregnated into the glass sheet is also mainly composed of polyvinyl chloride resin, since it exhibits excellent adhesion to the upper resin layer 14 and the lower resin layer 16. Regarding the properties of the resin to be impregnated into the glass sheet, a paste-like resin is preferable because it is easy to impregnate and has excellent processability.

[0041] Next, the surface layer 2B that can improve the cushioning properties of the flooring material 1A will be described with reference to Fig. 2(b). The surface layer 2B shown in Fig. 2(b) includes a foam layer 23, a design layer 24 laminated on the upper surface of the foam layer 23, a protective layer 22 laminated on the upper surface of the design layer 24, and a glass fiber cloth 21 embedded and laminated in the foam layer 23. In the surface layer 2B, the glass fiber cloth 21 is embedded and laminated in the foam layer 23 on the upper side of the center line S of the entire thickness of the surface layer 2B. If necessary, a decorative layer (not shown) having design properties may be provided between the protective layer 22 and the glass fiber cloth 21.

[0042] [Glass fiber cloth] The glass fiber cloth 21 preferably has an appropriate gap so that it can be impregnated with the foamable resin composition. 2 The average thickness of the nonwoven or woven fabric may be in the form of a sheet or mat with a basis weight of 15 g / m2 or less. 2 When the weight is less than 80 g / m, the foamable resin composition easily enters the gaps between the fibers, but the strength of the foamable resin composition is mainly dependent on the strength of the foamable resin composition. 2 If the thickness exceeds this range, the foamable resin composition will be difficult to penetrate into the gaps between the fibers, and the entanglement between the fibers and the foamable resin composition will be insufficient. In either case, there is a risk that a sufficient anchor effect will not be obtained.

[0043] As a method for laminating the glass fiber cloth 21, any method can be applied, such as a method in which a paste-like foamable resin composition in which the glass fiber cloth 21 is embedded is foamed using a normal heater such as an infrared heater in a conventional manufacturing method for a foamed product, thereby embedding the glass fiber cloth 21 in the foamed product and laminating it; a method in which a foamable resin composition in a fluid state is coated on the glass fiber cloth 21 and forcedly impregnated; or a method in which a carrier such as release paper is coated with a foamable resin composition in a fluid state using a knife coater or the like, and then the glass fiber cloth 21 is placed on top of the carrier, impregnated with the foamable resin composition, and heated to foam.

[0044] [Protective layer] For the protective layer 22, the components exemplified in the description of the protective layer 11 above can be used.

[0045] <Cold press molding layer> In the flooring material 1A shown in FIG. 1, the cold press molded layer 3 is a layer formed by pressing the base material (resin) of the cold press molded layer 3, which is in a state above its softening point, while cooling it with the molding dies 60 (upper die 61, lower die 62) and 90 (upper die 91, lower die 92) described below. Here, the "softening point" is the temperature at which the resin becomes plastically deformable when subjected to external stress, and the softening point is usually between the glass transition temperature (Tg) and melting temperature (Tm) of the resin. As the base material of the cold press molded layer 3, the thermoplastic resins exemplified in the explanation of the components of the upper resin layer 14 and the lower resin layer 16 described above can be used, and polyvinyl chloride resins are particularly suitable. Incidentally, polyvinyl chloride, a representative example of polyvinyl chloride resin, has a glass transition point (Tg) of approximately 60 to 85°C and a melting temperature (Tm) of approximately 210°C, although this varies depending on the amount of plasticizer added. Therefore, the softening point can be estimated to be, for example, 60 to 200°C.

[0046] The cold-press molded layer may be formed only from a resin as a base material, but other materials such as wood or metal materials can be embedded or joined as a core material or substrate. As wood materials, plywood, MDF, particle board, hardboard, etc. are preferably used. As metal materials, iron, aluminum, stainless steel, etc. are preferably used. When the cold-press molded layer is formed on wood or metal materials as a substrate, it can be easily joined or incorporated into a building, improving convenience.

[0047] In the flooring material 1A of the first embodiment, the surface layer 2 and the cold-press molded layer 3 are made of the same type of material. Here, the term "same type of material" means that the main components are the same, and the term "same type of main components" means that the materials are the same material and that the materials are of the same system. Examples of materials of the same system include those in which the monomers constituting the repeating units of the resin are the same but have different degrees of polymerization, different degrees of crystallization, and different substituents on the side chains. By making the surface layer 2 and the cold-press molded layer 3 out of the same type of material, the boundary between the surface layer 2 and the cold-press molded layer 3 can be more firmly integrated by heat fusion.

[0048] The surface layer 2 and the cold press molded layer 3 may contain other components other than the resin as necessary. Examples of the other components include plasticizers, fibers, fillers, stabilizers, processing aids, antifungal agents, deodorants, antibacterial agents, flame retardants, antioxidants, lubricants, and colorants. Examples of the plasticizer include dioctyl phthalate (DOP), diheptyl phthalate (DHP), diisononyl phthalate (DINP), trioctyl phosphate (TOP), triphenyl phosphate (TPP), dioctyl terephthalate (DOTP), dioctyl isophthalate (DOIP), and diisononyl cyclohexyl phthalate (DINCH). Examples of the fibers include short fibers of resin, glass, and the like. Among them, short glass fibers are preferred, as they can suppress warping of the product and increase dimensional stability and strength. The fiber length is 0.5 to 10 mm, preferably 2 to 9 mm, and more preferably 4 to 8 mm. Examples of the filler include calcium oxide, barium carbonate, magnesium hydroxide, aluminum hydroxide, clay, talc, mica, heavy calcium carbonate, light calcium carbonate, silica sand, aluminum hydroxide, etc. In the cold-press molded layer 3, the plasticizer is 10 to 90 parts, and the filler is 0 to 400 parts.

[0049] <density> The densities of the surface layer 2 and the cold-press molded layer 3 are particularly affected by the type and amount of plasticizer and the type and amount of filler, but are also affected by temperature changes during cooling and solidification in cold press molding using molds 60 (upper mold 61, lower mold 62) and 90 (upper mold 91, lower mold 92) described later. That is, in cold press molding using molds 60 and 90 described later, the portion of the surface layer 2 that contacts the molds 60 and 90 (upper surface portion) is cooled by the molds 60 and 90 from the beginning, while the portion of the surface layer 2 that contacts the base material of the cold-press molded layer 3 (lower surface portion) is once raised to a temperature equal to or higher than the softening point of the base material of the cold-press molded layer 3 by contact with the base material, and then cooled to approach the temperature of the molds 60 and 90. In contrast, the cold-press molded layer 3 is rapidly cooled from a state in which the base material of the cold-press molded layer 3 is at or above its softening point to the mold 60, 90 when it comes into contact with the mold 60, 90 during the molding stage, so that the temperature approaches the temperature of the mold 60, 90. In this way, the temperature change of the cold-press molded layer 3 is greater than the temperature change of the surface layer 2, so that the density of the cold-press molded layer 3 tends to be greater than the density of the surface layer 2. This tendency is particularly noticeable when the surface layer 2 contains a foamed resin. As a result, the cold-press molded layer 3 makes the entire flooring structure strong, while softening the surface layer 2 that is directly stepped on by the sole of the foot, improving the comfort of stepping on it, and also providing the effect of reducing fatigue in the lower limbs.

[0050] <Interlaminar peel strength> The interlayer peel strength between the surface layer 2 and the cold press molded layer 3 measured in accordance with the interlayer peel strength test method of JIS A 1454 is 8 to 100 N / 50 mm, preferably 20 to 95 N / 50 mm, and more preferably 30 to 90 N / 50 mm. This can reliably prevent the surface layer 2 from peeling off from the cold press molded layer 3 during normal use of the floor material 1A, and the function of the floor material 1A can be stably maintained for a long period of time. If the interlayer peel strength is less than 8 N / 50 mm, there is a risk that the welded state of the surface layer 2 and the cold press molded layer 3 cannot be maintained for a long period of time. If the interlayer peel strength exceeds 100 N / 50 mm, the surface layer 2 and the cold press molded layer 3 formed of different materials cannot be separated, which is undesirable from the viewpoint of recyclability. In addition, when the surface layer 2 and the cold press molded layer 3 are formed of the same material, they may or may not be separated during recycling.

[0051] <Hardness> The hardness of the surface layer 2 and the cold press molded layer 3 refers to a type A durometer hardness measured in accordance with JIS K 6253. Specifically, it is a value measured using GS-719N manufactured by Tecrock Corporation. The hardness of the surface layer 2 is 30 to 118, preferably 35 to 100, and more preferably 40 to 98. If the hardness is less than 30, the flexibility of the surface layer 2 is improved and the comfort of stepping is improved, but the surface layer 2 becomes easily deformed, so there is a risk of the uneven pattern being destroyed. If the hardness exceeds 118, the uneven pattern of the surface layer 2 is less likely to be destroyed, but there is a risk of the comfort of stepping being deteriorated. The hardness of the cold press molded layer 3 is 75 to 115, preferably 90 to 100, and more preferably 94 to 96. If the hardness is less than 75, the flexibility of the cold-press molded layer 3 is improved and the comfort of stepping on the cold-press molded layer 3 is improved, but the cold-press molded layer 3 is easily deformed, so there is a risk that the three-dimensional structure may be easily crushed. If the hardness is more than 115, the three-dimensional structure of the cold-press molded layer 3 is not easily crushed, but there is a risk that the comfort of stepping on the cold-press molded layer 3 may be deteriorated.

[0052] Furthermore, by making the hardness of the cold-press molded layer 3 higher than that of the surface layer 2, the cold-press molded layer 3 makes the entire flooring structure strong, while the surface layer 2 that is directly stepped on by the soles of the feet is softened to improve comfort and reduce fatigue in the lower limbs. In this case, the difference in hardness between the cold-press molded layer 3 and the surface layer 2 is preferably 30 or more, more preferably 40 or more. The upper limit is preferably 65 or less, more preferably 50 or less. The hardness difference here is calculated by the following formula. Hardness difference = (hardness of cold press molded layer 3) - (hardness of surface layer 2)

[0053] [Modification (1) of the first embodiment] As a modified example (1) of the first embodiment, there is a flooring material in which a core material is contained in a cold-press molded layer. Examples of the core material include a member formed into a plate-like, lattice-like, mesh-like, or other shape made of metal, wood, resin, or a composite material thereof.

[0054] The core material may be entirely contained in the cold press molded layer, or may have a protruding portion protruding from the surface of the cold press molded layer in a required portion. An example of the protruding portion is a screw shaft having a male screw. By adopting a configuration in which the screw shaft protrudes from the surface of the cold press molded layer in this manner, the floor material can be easily and firmly fixed to the installation location by tightening the nut screwed onto the screw shaft of the floor material when the floor material is installed.

[0055] Alternatively, a required opening may be provided on the surface side of the cold-press molded layer to expose a required portion of the core material, and a female screw may be formed in the portion of the core material corresponding to the opening. In this manner, by adopting a configuration in which a bolt can be screwed into the female screw formed in the core material through the opening provided on the surface side of the cold-press molded layer, the floor material can be easily and firmly fixed to the installation location by tightening the bolt screwed into the female screw of the floor material when the floor material is installed.

[0056] By using a wooden board as the core material, the flooring can be easily and firmly fixed to the installation location using nails or wood screws. The required part of the wooden board may be exposed from the cold press molding layer. In this case, for example, if the floor surface to be installed is a wooden base, the flooring can be easily and firmly fixed to the installation location by a construction method in which an adhesive layer formed of a wood adhesive or the like is interposed between the exposed wooden part and the wooden base.

[0057] According to the flooring material of the above modification (1), the core material is contained in the cold press molded layer, so that the strength of the core material is added to the strength of the surface layer and the cold press molded layer, and the strength of the entire flooring material can be increased. Also, according to the flooring material of the above modification (1), the function of the core material is added to the functions of the surface layer and the cold press molded layer, respectively, so that added value can be increased. Also, according to the flooring material of the above modification (1), since the core material is contained in the cold press molded layer, it is not necessary to consider the bonding strength between the cold press molded layer and the core material, and it is possible to adopt a core material made of a different material such as metal or wood, which is different from the cold press molded layer made of a resin material, and the options for materials used as the core material can be increased.

[0058] The flooring material according to the above modification (1) can be manufactured by a manufacturing method including the following steps (1) to (6). (1) A first placement step of placing a surface layer on a mold (2) A second placement step of placing a thermoplastic resin at or above its softening point so as to be in contact with the surface layer. (3) A third arrangement step of arranging a core material so as to be in contact with the thermoplastic resin arranged in the second arrangement step (4) A fourth placement step of placing a thermoplastic resin in a state above its softening point so as to be in contact with the core material. (5) A pressing step in which the contents of the mold are pressed at a temperature below the softening point of the thermoplastic resin. (6) A recovery step of removing the laminated molded body formed by the pressing step from the mold.

[0059] According to the above manufacturing method, it is possible to easily incorporate a core material made of a different material, such as metal or wood, into the cold-press molded layer, which is made of a resin material, while achieving both high design quality and flexible formability that could not be achieved with conventional flooring materials.

[0060] [Modification (2) of the first embodiment] As a modified example (2) of the first embodiment, there is a flooring material formed by laminating a surface layer, a cold press molded layer, and a base material in the order described. In this way, by adopting a configuration in which a base material is laminated in addition to the surface layer and the cold press molded layer, the strength of the flooring material can be increased. Examples of the base material include members formed into a plate-like, lattice-like, mesh-like, etc. shape made of metal, wood, resin, etc., or a composite material thereof.

[0061] For example, if the floor surface to be installed has a wooden base, a wooden board can be used as the base material for the flooring, and an adhesive layer formed with a wood adhesive or the like can be interposed between the base material and the wooden base, allowing the flooring to be easily and firmly fixed to the installation location.

[0062] The flooring material according to the above modification (2) can be manufactured by a manufacturing method including the following steps (1) to (6). (1) A first placement step of placing a surface layer on a mold (2) A second placement step of placing a thermoplastic resin at or above its softening point so as to be in contact with the surface layer. (3) a third arrangement step of arranging a substrate so as to be in contact with the thermoplastic resin arranged in the second arrangement step (4) A pressing step in which the contents of the mold are pressed at a temperature below the softening point of the thermoplastic resin. (5) A recovery step of removing the laminated molded body formed by the pressing step from the mold.

[0063] According to the above manufacturing method, it is possible to easily laminate a base material made of a different material, such as metal or wood, which is made of a different material from the cold-press molded layer made of a resin material, to the surface layer and the cold-press molded layer, while achieving both high design quality and free formability that were not possible with conventional flooring materials.

[0064] Second Embodiment 3 is a cross-sectional view showing a laminated structure of a flooring material according to a second embodiment of the present invention. In the second embodiment, the same or similar parts as those in the first embodiment are denoted by the same reference numerals in the figure, and detailed descriptions thereof are omitted. In the following, the description will be focused on parts unique to the second embodiment.

[0065] As shown in Fig. 3, in the flooring material 1B of the second embodiment, a surface layer 2 and a cold-press molded layer 3 are laminated via a bonding layer 4. The surface layer 2 and the cold-press molded layer 3 are made of different types of thermoplastic resins.

[0066] The bonding layer 4 is not particularly limited as long as it is made of a material that can exert an anchor effect. Examples of materials for the bonding layer 4 include jute, glass fiber nonwoven fabric, spunbond nonwoven fabric, and foamed resin having a porous structure. As an example, a case where a spunbond nonwoven fabric is used for the bonding layer 4 will be described. In cold press molding using molding dies 60 (upper die 61, lower die 62) and 90 (upper die 91, lower die 92) described later, due to the heat of the base material of the cold press molded layer 3 that is in a state above its softening point and the pressure during pressing, a part of the side of the surface layer 2 facing the cold press molded layer 3 and a part of the base material of the cold press molded layer 3 facing the surface layer 2 each enter into the fiber gaps of the spunbond nonwoven fabric in a molten state, and then cool and solidify, and the surface layer 2 and the cold press molded layer 3 are firmly integrated via the bonding layer 4 (spunbond nonwoven fabric) by the anchor effect. When the surface layer 2 and the cold-press molded layer 3 are made of different materials, the bonding between the two may not be successful. However, by interposing the bonding layer 4 in this manner, the surface layer 2 and the cold-press molded layer 3 can be firmly integrated via the bonding layer 4, even if the surface layer 2 and the cold-press molded layer 3 are made of different materials.

[0067] <Examples of flooring materials (1)> Fig. 4 shows a specific example (1) of a flooring material to which the present invention is applied, where (a) is an overall perspective view of the staircase flooring material, and (b) is an enlarged view of the main part of the AA line cross section of (a). The staircase flooring material 31 shown in Fig. 4(a) has a surface layer 32 (the part hatched in the figure) formed in a rectangular sheet shape in a plan view, and a cold-press molded layer 33 that supports the surface layer 32 from below.

[0068] <Surface layer> 4(b), the surface layer 32 has a plurality of recesses 35 and protrusions 36 formed by applying uneven processing imitating a wood grain pattern to the surface (upper surface) of the surface layer 2. The recesses 35 and protrusions 36 mainly constitute the wood grain uneven pattern.

[0069] The recess 35 has an inclined surface that slopes downward from the boundary between the recess 35 and the protrusion 36 toward the bottom of the recess 35. The recess 35 has a low gloss and a rough feel. On the other hand, the surface of the protrusion 36 has a high gloss and a mirror-like feel. As a result, the surface of the protrusion 36 resembles the appearance and feel of late wood of natural wood, and the surface of the recess 35 resembles the appearance and feel of early wood of natural wood. In this way, the grain of natural wood is reproduced in the surface layer 32, and the feel is also close to that of natural wood.

[0070] <Cold press molding layer> The cold-press molded layer 33, in the cold-press molded layer 3 of the first embodiment, comprises a tread laying portion 41 laid on the tread of the staircase, a riser surface laying portion 42 laid on at least the upper part of the riser surface of the staircase, and a stair nosing laying portion 43 laid on the stair nosing portion of the staircase.

[0071] The surface layer 32 is placed integrally on the upper surface of the tread laying portion 41. The tread laying portion 41 and the nosing laying portion 43 are disposed integrally so as to be continuous in the horizontal direction. The nosing laying portion 43 and the riser surface laying portion 42 are disposed integrally so as to be substantially perpendicular to each other. The cold-press molded layer 33 has a three-dimensional structure including a portion extending vertically (the riser surface laying portion 42) and a portion protruding horizontally (the nosing laying portion 43) with respect to the tread laying portion 41 having a layering surface on which the surface layer 32 is layered.

[0072] The step nosing portion 43 is formed with a plurality of groove-shaped recesses 45 and a plurality of streak-shaped protrusions 46. The groove-shaped recesses 45 and streak-shaped protrusions 46 constitute the uneven portion 50. The groove-shaped recesses 45 and streak-shaped protrusions 46 extend in a horizontal direction perpendicular to the direction from the step nosing portion 43 toward the tread laying portion 41. The groove-shaped recesses 45 and streak-shaped protrusions 46 are arranged alternately in the direction from the step nosing portion 43 toward the tread laying portion 41. The depth of the groove-shaped recesses 45 is set to be equal to or greater than the thickness of the surface layer 32. The protruding length of the streak-shaped protrusions 46 when the upper surface of the tread laying portion 41 is taken as the reference plane is set to be equal to or greater than the thickness of the surface layer 32.

[0073] In order for the riser surface laying part 42 to cover at least the upper part of the riser surface of the staircase, the downward protruding length from the tread surface laying part 41 is set to 2 to 12 times, preferably 4 to 10 times, and more preferably 6 to 8 times the thickness of the surface layer 32.

[0074] <Molding for staircase flooring> Fig. 5 shows a mold for molding a staircase flooring material, (a) is a diagram of a mold release state, and (b) is a diagram of a mold clamping state. As shown in Fig. 5(a), a mold 60 for molding a staircase flooring material 31 includes an upper mold 61 having a convex portion 61a and a lower mold 62 having a concave portion 62a corresponding to the convex portion 61a. When the convex portion 61a and the concave portion 62a are combined in the mold clamping state shown in Fig. 5(b), a molding cavity 65 for molding the staircase flooring material 31 is formed between the convex portion 61a and the concave portion 62a.

[0075] As shown in Fig. 5(a), the upper die 61 has a pressing surface 66 for pressing the base material of the cold-press molded layer 33 that has been brought to a state above its softening point. The upper die 61 has a cutout portion 67 for forming the riser surface laying portion 42 (see Fig. 4(a)) in the cold-press molded layer 33. The lower die 62 has a surface layer mounting portion 68 on which the surface layer 32 (see Fig. 4(a)) can be mounted within a recess 62a. The lower die 62 has a concave-convex portion molding portion 69 for forming the concave-convex portion 50 (see Fig. 4(a)) in the cold-press molded layer 33, formed adjacent to the surface layer mounting portion 68.

[0076] <Manufacturing method for staircase flooring> FIG. 6 shows the steps of a manufacturing method for a staircase flooring material, where (a) is an explanatory diagram of the surface layer arrangement process, (b) is an explanatory diagram of the thermoplastic resin arrangement process, (c) is an explanatory diagram of the pressing process, and (d) is an explanatory diagram of the recovery process.

[0077] [Surface layer placement process] 6(a), in a state where the upper die 61 is positioned above the lower die 62 and the molding die 60 is open, the surface layer 32 is placed upside down, with the upper surface of the surface layer 32 facing downward and the lower surface facing upward, on the surface layer placement portion 68 of the lower die 62. This surface layer placement step corresponds to the "first placement step" of the present invention.

[0078] [Thermoplastic resin placement process] 6(b), the thermoplastic resin 33M, which is the base material of the cold-press molded layer 33 in a plasticized state, is placed on the surface layer 32 placed on the surface layer placement section 68 in an upside-down state. Note that "plasticization" here means that the thermoplastic resin 33M is heated to a plasticization temperature higher than its softening point (for example, in the case of polyvinyl chloride, about softening point (90 to 200°C) + (10 to 30°C)) to make it flowable. This thermoplastic resin placement step corresponds to the "second placement step" of the present invention.

[0079] [Pressing process] Next, while cooling the upper mold 61 and the lower mold 62 by a cooling means (not shown) such as circulating cooling water through each of the upper mold 61 and the lower mold 62, the upper mold 61 is lowered relative to the lower mold 62 as shown in FIG. 6(c) to be in a mold clamped state, and the surface layer 32, which is the content of the mold 60, and the thermoplastic resin 33M in a plastic state (base material of the cold press molded layer 33) are pressed at a temperature lower than the softening point of the thermoplastic resin 33M, for example, at room temperature or near room temperature. The pressing pressure in this pressing step is 0.1 to 20 MPa, preferably 0.2 to 15 MPa, and more preferably 0.5 to 10 MPa. Note that, according to JIS Z8703, "room temperature" is defined as 20°C±15°C, i.e., 5 to 35°C, but "room temperature or near room temperature" may include a temperature range wider than "room temperature", for example, 20 to 50°C. If the pressing pressure is less than 0.1 MPa, the thermoplastic resin 33M may not be able to fill the entire molding cavity 65, resulting in molding defects. If the pressing pressure exceeds 20 MPa, the mold releasability may deteriorate.

[0080] In the pressing process, the thermoplastic resin 33M pressed by the convex portion 61a of the upper die 61 is spread on the surface layer 32, a part of which fills the concave-convex portion forming portion 69 of the lower die 62, and the remaining part fills between the notch portion 67 of the upper die 61 and the concave portion 62a of the lower die 62. In this manner, the molding of the cold-press molded layer 33 proceeds as the pressing process progresses. During the molding of the cold-press molded layer 33, the boundary between the cold-press molded layer 33 and the surface layer 32 is integrated by thermal fusion due to the heat of the thermoplastic resin 33M that is at or above its softening point (plasticization temperature) and the pressure during the pressing process.

[0081] The surface side of the surface layer 32 (the lower side in Figs. 6(a) to (c)) is cooled by the lower die 62, although pressure is applied during press processing. Therefore, thermal deformation of the surface side of the surface layer 32 is suppressed, and the pattern or uneven pattern (in this example, a wood grain uneven pattern) provided on the surface side of the surface layer 32 remains without being crushed. Even if the surface layer 32 has a wood grain design layer, the pattern does not deform due to thermal deformation. In the cold press molded layer 33, the base material (thermoplastic resin 33M) that is in a plasticizing temperature state spreads along the shape of the mold cavity 65 (see Fig. 5(b)), and is solidified by cooling with the mold 60 (mainly the upper die 61), and is molded into a shape corresponding to the shape of the mold cavity 65. Therefore, high designability and free moldability with a three-dimensional feel can be achieved at the same time.

[0082] [Recovery process] Once the pressing step is complete, as shown in Figure 6(d), the upper die 61 is raised relative to the lower die 62 to open the molding die 60, and the laminated molded body (staircase flooring material 31) is removed and collected from the molding die 60. At this time, in order to facilitate the release of the laminated molded body from the molding die 60, the molding die 60 may be vibrated or the laminated molded body may be sucked with air.

[0083] [Joining layer placement process] FIG. 10(a) is an explanatory diagram of the bonding layer arrangement step in the manufacturing method of the staircase flooring material. The manufacturing method of the staircase flooring material 31 is applied when the surface layer 32 and the cold press molded layer 33 are made of the same type of thermoplastic resin. When the surface layer 32 and the cold press molded layer 33 are made of different types of thermoplastic resin, a bonding layer arrangement step is added between the surface layer arrangement step and the thermoplastic resin arrangement step. In the bonding layer arrangement step, the bonding layer 4 that exerts an anchor effect is arranged on the surface layer 32 that is placed on the surface layer placement part 68 in an upside-down state by the surface layer arrangement step. Then, in the thermoplastic resin arrangement step, the thermoplastic resin 33M (see FIG. 6(b)) in a plasticized state is arranged on the bonding layer 4.

[0084] A case where a spunbonded nonwoven fabric is used as the bonding layer 4 will be described. In the pressing process of cold press molding using a mold 60, a part of the side of the surface layer 32 facing the thermoplastic resin 33M and a part of the side of the thermoplastic resin 33M facing the surface layer 32 each enter into the fiber gaps of the spunbonded nonwoven fabric in a molten state due to the heat of the thermoplastic resin 33M that is in a state above its softening point and the pressure during the pressing process, and then the surface layer 32 and the cold press molding layer 33 are firmly integrated through the bonding layer 4 (spunbonded nonwoven fabric) by the anchor effect due to cooling and solidification. In this way, by interposing the bonding layer 4, even if the surface layer 32 and the cold press molding layer 33 are made of different materials, the surface layer 32 and the cold press molding layer 33 can be firmly integrated through the bonding layer 4. The bonding layer 4 may be laminated on the back surface of the surface layer 32 in advance.

[0085] <Specific examples of flooring materials (2)> Fig. 7 shows a specific example (2) of a flooring material to which the present invention is applied, where (a) is an overall perspective view of the entrance flooring material, and (b) is an enlarged view of the main part of the cut end surface along line BB in (a). The entrance flooring material 71 shown in Fig. 7(a) has a surface layer 72 formed in a rectangular sheet shape in a plan view, and a cold-press molded layer 73 that supports the surface layer 72 from below.

[0086] <Surface layer> As shown in Fig. 7(b), the surface layer 72 has a plurality of recesses 75 and a plurality of protrusions 76 formed by carrying out a cold press molding process described below. The plurality of recesses 75 and the plurality of protrusions 76 are arranged adjacent to each other vertically and horizontally. The plurality of recesses 75 are formed between adjacent protrusions 76. The plurality of recesses 75 and the plurality of protrusions 76 as a whole form a tile-like uneven pattern.

[0087] [Convex] The multiple protrusions 76 are formed in a substantially square shape in plan view. In this specification, the plan view refers to a view from a direction perpendicular to the surface of the surface layer 72, and the plan view shape refers to the outline in plan view. The multiple protrusions 76 all have the same size in plan view and are regularly arranged at equal intervals vertically and horizontally. This makes it possible to prevent the drainage and anti-slip properties of the entrance floor material 71 from varying from place to place.

[0088] Each of the protrusions 76 has a generally flat top surface at its protruding end. To enhance design and anti-slip properties, the top surface is provided with a mesh-like protrusion 78 that protrudes in a lattice net shape when viewed from above. The mesh-like protrusion 78 forms a lattice net-like uneven pattern.

[0089] [Concave] The recesses 75 are connected to each other to form a drainage groove 79, which is formed in a lattice shape in a plan view so as to surround each of the protrusions 76.

[0090] <Cold press molding layer> 7(a) and (b), the cold press molded layer 73 includes a rectangular floor laying portion 81 having a predetermined drainage gradient toward the drainage portion 80, a protruding portion 82 protruding horizontally from the floor laying portion 81 toward the drainage portion 80, and a water stop plate portion 83 erected on each of the remaining three sides of the floor laying portion 81 except for the side on which the protruding portion 82 is provided. As shown in FIG. 7(b), the surface layer 72 is integrally placed on the upper surface of the floor laying portion 81.

[0091] 7(b), a vertical surface 83a is formed on the outer side of the water stop portion 83, which extends perpendicular to the upper surface of the floor-laying portion 81, i.e., extends straight in the vertical direction. A sloping surface 83b is formed on the inner side of the water stop portion 83, which slopes outward in the direction away from the upper surface of the floor-laying portion 81, i.e., upward.

[0092] The cold press molded layer 73 has a three-dimensional structure formed in a vertical or horizontal direction relative to the lamination surface. That is, the cold press molded layer 73 has a three-dimensional structure including a part extending vertically (vertical surface 83a of the water stop portion 83), a part protruding horizontally (projecting portion 82), and a part extending obliquely (inclined surface 83b of the water stop portion 83) relative to the floor surface laying portion 81 having the lamination surface on which the surface layer 72 is laminated. In this way, the present invention can mold flooring materials with any three-dimensional structure. In particular, the three vertical surfaces 83 have a three-dimensional structure in which the surface layer 72 is surrounded from three sides, which is a three-dimensional structure that cannot be obtained by extrusion molding.

[0093] <Molding mold for entrance flooring> Fig. 8 shows a mold for molding an entrance floor material, where (a) is a diagram of the mold release state and (b) is a diagram of the mold clamping state. As shown in Fig. 8(a), the mold has an upper mold 91 having a convex portion 91a and a lower mold 92 having a concave portion 92a corresponding to the convex portion 91a. When the convex portion 91a and the concave portion 92a are combined as shown in the figure in the mold clamping state shown in Fig. 8(b), a molding cavity 95 for molding the entrance floor material 71 is formed between the convex portion 91a and the concave portion 92a.

[0094] The upper die 91 has a pressing surface 96 for pressing the base material of the cold-press molded layer 73, which has been brought to a state above its softening point. The lower die 92 has a surface layer mounting portion 98 on which the surface layer 72 can be mounted within a recess 92a. The lower die 92 is formed with a waterstop portion molding portion 99 for molding the waterstop portion 83 (see FIGS. 7(a) and (b)) in the cold-press molded layer 73, adjacent to the surface layer mounting portion 98.

[0095] <Manufacturing method for entrance flooring> FIG. 9 shows the steps of the manufacturing method for molding entrance hall flooring, where (a) is an explanatory diagram of the surface layer arrangement process, (b) is an explanatory diagram of the thermoplastic resin arrangement process, (c) is an explanatory diagram of the pressing process, and (d) is an explanatory diagram of the recovery process.

[0096] [Surface layer placement process] 9(a), in a state where the upper die 91 is positioned above the lower die 92 and the molding die 90 is open, the surface layer 72 is placed upside down, with the upper surface of the surface layer 72 facing downward and the lower surface facing upward, on the surface layer placement portion 98 of the lower die 92. This surface layer placement step corresponds to the "first placement step" of the present invention.

[0097] [Thermoplastic resin placement process] 9(b), the thermoplastic resin 73M, which is the base material of the cold-press molded layer 73 in a plasticized state, is placed on the surface layer 72 placed upside down on the surface layer placement part 98. This thermoplastic resin placement step corresponds to the "second placement step" of the present invention.

[0098] [Pressing process] Next, while cooling the upper mold 91 and the lower mold 92 by a cooling means (not shown) such as circulating cooling water through each of the upper mold 91 and the lower mold 92, the upper mold 91 is lowered relative to the lower mold 92 as shown in FIG. 9(c) to close the mold, and the surface layer 72, which is the content of the mold 90, and the thermoplastic resin 73M in a plastic state (base material of the cold press molded layer 73) are pressed at a temperature lower than the softening point of the thermoplastic resin 73M, for example, at or near room temperature. The pressing pressure in this pressing step is 0.1 to 20 MPa, preferably 0.2 to 15 MPa, and more preferably 0.5 to 10 MPa. If the pressing pressure is less than 0.1 MPa, the thermoplastic resin 73M may not be filled into the entire molding cavity 95, resulting in molding defects. If the pressing pressure is more than 20 MPa, the mold releasability may be deteriorated.

[0099] In the pressing process, the thermoplastic resin 73M pressed by the convex portion 91a of the upper die 91 is pressed and spread on the surface layer 72, and a part of it is filled into the waterstop portion molding portion 99 of the lower die 92. In this way, the molding of the cold-press molded layer 73 progresses as the pressing process progresses. Also, during the molding of the cold-press molded layer 73, the boundary between the thermoplastic resin 73M and the surface layer 72 is integrated by thermal fusion caused by the heat of the thermoplastic resin 73M that is at or above its softening point (plasticization temperature) and the pressure during the pressing process.

[0100] The surface side of the surface layer 72 (the lower side in Figs. 9(a) to (c)) is cooled by the lower die 92, although pressure is applied during press processing. Therefore, thermal deformation of the surface side of the surface layer 72 is suppressed, and the pattern or uneven pattern (in this example, a tile-like uneven pattern or a lattice-like uneven pattern) provided on the surface side of the surface layer 72 remains without being crushed. In the cold-press molded layer 73, the thermoplastic resin 73M, which is at a plasticizing temperature, spreads along the shape of the mold cavity 95, and is solidified by cooling with the mold 90 (mainly the upper die 91), thereby being molded into a shape corresponding to the shape of the mold cavity 95. Therefore, it is possible to achieve both high designability and free moldability with a three-dimensional feel.

[0101] [Recovery process] Once the pressing process is completed, as shown in Figure 9 (d), the upper die 91 is raised relative to the lower die 92 to open the molding die 90, and the laminated molded body (entrance hall flooring material 71) formed by the pressing process is removed from the molding die 90 and collected.

[0102] [Joining layer placement process] FIG. 10(b) is an explanatory diagram of the bonding layer arrangement step in the manufacturing method of the entrance floor material. The manufacturing method of the entrance floor material 71 is applied when the surface layer 72 and the cold press molded layer 73 are made of the same type of thermoplastic resin. When the surface layer 72 and the cold press molded layer 73 are made of different types of thermoplastic resin, a bonding layer arrangement step is performed between the surface layer arrangement step and the thermoplastic resin arrangement step. In the bonding layer arrangement step, a bonding layer 4 that exerts an anchor effect is arranged on the surface layer 72 that is placed on the surface layer placement part 98 in an upside-down state by the surface layer arrangement step. Then, in the thermoplastic resin arrangement step, a thermoplastic resin 73M (see FIG. 9(b)) in a plasticized state is arranged on the bonding layer 4.

[0103] A case where a spunbonded nonwoven fabric is used as the bonding layer 4 will be described. In the pressing process of cold press molding using a mold 90, a part of the surface layer 72 facing the thermoplastic resin 73M and a part of the thermoplastic resin 73M facing the surface layer 72 each enter into the fiber gaps of the spunbonded nonwoven fabric in a molten state due to the heat of the thermoplastic resin 73M that is in a state above its softening point and the pressure during the press processing, and then the surface layer 72 and the cold press molded layer 73 are firmly integrated via the bonding layer 4 (spunbonded nonwoven fabric) by the anchor effect due to cooling and solidification. In this way, by interposing the bonding layer 4, the surface layer 72 and the cold press molded layer 73 can be firmly integrated even if they are made of different materials.

[0104] The uneven pattern of the surface layer 32, 72 is preferably given to the surface layer 32, 72 before lamination. As described above, in the step of laminating the surface layer 32, 72 and the cold press molded layer 33, 73 so as to be integrated, a press process is performed to mold the cold press molded layer 33, 73. This press process is performed by contacting the uneven pattern given to the surface layer 32, 72 before lamination with the mold 60, 90. At this time, although the pressure during the press process acts on the uneven pattern, the uneven pattern is cooled by the mold 60, 90. Therefore, even if the uneven pattern is given to the surface layer 32, 72 before lamination, the thermal deformation of the uneven pattern can be suppressed and the shape of the uneven pattern can be maintained. According to the flooring material 31, 71, it is not necessary to perform a step of giving an uneven pattern to the surface layer 32, 72 by, for example, embossing after the press process, so that production efficiency can be improved.

[0105] [Another embodiment] The present invention can be implemented by partially modifying the configuration of the flooring material according to each of the above-described embodiments (including the modified examples). Such modified examples will be described below as other embodiments.

[0106] <Another embodiment 1> In the above second embodiment, as a specific example (1) of the flooring to which the present invention is applied, a flooring material for stairs in which the step nosing laying part 43 and the riser surface laying part 42 are substantially perpendicular to each other is shown, but the connection form between the step nosing laying part 43 and the riser surface laying part 42 can be changed in various ways. For example, in FIG. 4, the connection part between the step nosing laying part 43 and the riser surface laying part 42 can be curved so that the entire cold press molded layer 33 has a rounded shape without corners (not shown). In addition, the uneven part 50 consisting of a plurality of groove-like recesses 45 and streak-like protrusions 46 formed in the step nosing laying part 43 can also be curved along the longitudinal direction or the corners of the unevenness can be chamfered to emphasize a rounded and soft impression.

[0107] <Another embodiment 2> In the above second embodiment, as a specific example (2) of a flooring material to which the present invention is applied, a flooring material for an entrance hall having a cold-press molded layer 73 with a floor surface laying portion 81, an overhanging portion 82, and a waterstop portion 83 is shown, but the cold-press molded layer 73 can also be configured to include a frame of the flooring material (flooring). For example, in Fig. 7, if the waterstop portion 83 of the cold-press molded layer 73 is further extended vertically and connected to the edge of the flooring material (flooring), not shown, the waterstop portion 83 of the cold-press molded layer 73 can function as a frame of the flooring material (flooring). [Industrial Applicability]

[0108] The present invention can firmly integrate a cold-pressed layer that is hard and capable of three-dimensional formation with a surface layer that is flexible and has a fine uneven structure and is excellent in design. Therefore, the present invention is a technology that can be widely used in the construction industry, remodeling industry, etc., and is particularly useful in the construction of floor surfaces in various buildings such as ordinary houses, apartment buildings, condominiums, commercial malls, office buildings, factories, stores, stations, schools, hospitals, and public facilities. [Explanation of symbols]

[0109] 1A, 1B Flooring 2,2A,2B surface layer 3 Cold press molding layer 4 Bonding layer 31 Staircase flooring 32 Surface layer of staircase flooring 33 Cold-pressed layer of staircase flooring 35 Concave (wood grain pattern) 36 Convex part (wood grain pattern) 37 Short fiber-containing resin layer (wood-like uneven pattern) 42 Riser surface installation part (three-dimensional structure) 43 Nose laying part (three-dimensional structure) 60 Molding mold (for molding flooring for stairs) 71 Entrance flooring 72 Surface layer of entrance flooring 73 Cold-pressed layer of entrance flooring 75 Concave (tile-like uneven pattern) 76 Convex part (tile-like uneven pattern) 78 Net-like convex part (lattice-like uneven pattern) 82 Overhang (three-dimensional structure) 83 Water stop plate part (three-dimensional structure) 90 Molding mold (for molding entrance flooring)

Claims

1. A flooring material comprising a surface layer and a molding layer laminated thereon, The boundary between the surface layer and the molding layer is integrated by thermal fusion, The molding layer has a portion formed in a vertical or horizontal direction relative to the lamination surface, The vertically formed portion has a length greater than or equal to the thickness of the surface layer and is formed so as to bend from multiple points on the molding layer.

2. 2. The flooring material according to claim 1, wherein the vertically formed portions that are bent from a plurality of points of the molding layer are adjacent to each other and integrated together.

3. A flooring material comprising a surface layer and a molding layer laminated thereon, The boundary between the surface layer and the molding layer is integrated by thermal fusion, The molding layer has a portion formed in a vertical or horizontal direction relative to the lamination surface, The vertically formed portion has a length greater than or equal to the thickness of the surface layer and is formed so as to bend from the molding layer, with the surface layer being positioned on the inside of the bent portion.

4. The flooring material according to any one of claims 1 to 3, wherein the surface layer and the molding layer are made of the same material.

5. The molding layer has a higher hardness (type A durometer hardness measured in accordance with JIS K 6253) than the surface layer, The flooring material according to any one of claims 1 to 4, wherein the difference in hardness between the molding layer and the surface layer is 30 or more.

6. 6. The flooring material according to claim 1, wherein in the region where the surface layer and the molding layer are laminated, the molding layer is formed to be thicker than the surface layer.

Citation Information

Patent Citations

  • Bath tub installation type floor pan

    JP1992055563A

  • Decorated molding and its manufacture

    JP2001038758A

  • Floor pan for unit room

    JP2001182117A

  • Indoor interior-finishing panel, and floor panel and construction method for double floor

    JP2006249839A

  • Member for sanitary installation room

    JP2008223263A