Semiconductor device

The semiconductor device addresses the challenge of etching control in thin film transistors by exposing the insulating surface through controlled openings, facilitating easy electrical connections and reducing device deterioration.

JP2024156016AActive Publication Date: 2024-10-31SEMICON ENERGY LAB CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2024146270
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2007-03-26
Filing Date
2024-08-28
Publication Date
2024-10-31
Estimated Expiration
2028-03-11

AI Technical Summary

Technical Problem

The challenge in manufacturing semiconductor devices is controlling etching when forming openings in insulating layers to electrically connect wiring to the source or drain regions, particularly for thin film transistors with semiconductor layers thinner than 50 nm, which complicates the formation of contact holes.

Method used

The semiconductor device is designed with a structure that allows for controlled etching by forming openings in both the semiconductor layer and insulating layers, exposing the insulating surface, and using a conductive layer to connect electrically with the semiconductor layer, avoiding the need to stop etching at the semiconductor film surface.

Benefits of technology

This approach enables easy control of etching during contact hole formation, leading to the production of semiconductor devices with suppressed deterioration of characteristics and improved electrical connections.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024156016000001_ABST
    Figure 2024156016000001_ABST
Patent Text Reader

Abstract

To provide a technology for manufacturing a semiconductor device that facilitates etching control when a contact hole is formed.SOLUTION: A semiconductor device comprises: a semiconductor layer formed on at least an insulation surface; a first insulating layer formed on the semiconductor layer; a gate electrode formed on the first insulating layer; and a second insulating layer formed on the gate electrode. An opening is formed at least on the semiconductor layer and the second insulating layer to partially expose the insulation surface. The semiconductor device comprises a conductive layer formed on the second insulating layer via the opening. Here, the conductive layer is electrically connected with the semiconductor layer on a lateral face of the opening formed on the semiconductor layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor device and a manufacturing method thereof. This refers to any device that can function by utilizing the properties of semiconductors. [Background technology]

[0002] In recent years, thin film transistors (TFTs) have been formed on substrates with insulating surfaces such as glass, and The production of semiconductor devices that use thin film transistors as switching elements etc. is becoming more and more popular. The thin-film transistor is formed on a substrate having an insulating surface by a CVD method, a photolithography method, etc. A semiconductor film having an island shape is formed by a film forming process or the like, and a part of the semiconductor film is formed into a transistor. The semiconductor device is provided so as to be utilized as a channel formation region (eg, Patent Document 1).

[0003] A schematic diagram of a cross section of a thin film transistor is shown in FIG. The substrate 30 is provided with an insulating layer 31 that functions as a base film. a channel forming region 32a; an impurity region 32b functioning as a source region and a drain region; A semiconductor layer 32 having a gate insulating layer 32c is formed on the semiconductor layer 32 and the insulating layer 31. An insulating layer 33 functioning as a gate electrode is formed on the insulating layer 33. 34 is formed, an insulating layer 203 is formed on the conductive layer 34, and an impurity region is formed on the insulating layer 203. A wiring 204 is formed to electrically connect to 32b and 32c. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Application Publication No. 08-018055 Summary of the Invention [Problem to be solved by the invention]

[0005] In the structure of FIG. 21, in order to electrically connect the wiring to the surface of the source region or the drain region, It is considered necessary to form a semiconductor layer to be a source region or a drain region at the bottom of the opening. This made it difficult to control the etching process when forming an opening in the insulating layer. This is a particularly noticeable problem when the semiconductor layer is formed as a thin film having a thickness of 50 nm or less.

[0006] The present invention is a technology to solve such problems, and The present invention proposes a technique for manufacturing a semiconductor device capable of easily controlling switching. [Means for solving the problem]

[0007] The semiconductor device of the present invention comprises at least a semiconductor layer formed on an insulating surface, and a semiconductor layer formed on the semiconductor layer. a first insulating layer formed on the first insulating layer, a gate electrode formed on the first insulating layer, and a gate electrode formed on the gate electrode. and a second insulating layer formed on the semiconductor layer, and an opening is formed in at least the semiconductor layer and the second insulating layer. The insulating surface is partially exposed through the opening, and a metal oxide film is formed on the second insulating layer through the opening. and a conductive layer. Here, the conductive layer is formed on the side of a contact hole formed in the semiconductor layer. The surface of the semiconductor layer is electrically connected to the semiconductor layer. In other words, the upper area of ​​the opening formed in the semiconductor layer is The upper area of ​​the opening formed in the second insulating layer is smaller than the upper area of ​​the conductive layer and the semiconductor The layer is electrically connected to the side surface of the contact hole formed in the semiconductor layer and to the surface of the semiconductor layer. The input / output terminals may be electrically connected to each other.

[0008] The semiconductor device of the present invention includes a semiconductor layer formed on an insulating surface, and a first insulating layer formed on the semiconductor layer. forming a gate electrode on the first insulating layer; forming a second insulating layer on the gate electrode; an opening in at least the semiconductor layer and the second insulating layer that partially exposes the insulating surface; and forming a conductive layer on the insulating surface and the second insulating layer through the opening. It can be made by

[0009] The semiconductor device of the present invention further comprises a first insulating layer formed on a substrate, and a second insulating layer formed on the first insulating layer. forming an insulating layer, forming a semiconductor layer on the second insulating layer, and forming a third insulating layer on the semiconductor layer Then, a gate electrode is formed on the third insulating layer, a fourth insulating layer is formed on the gate electrode, and The first insulating layer surface is partially exposed to at least the second insulating layer, the semiconductor layer and the fourth insulating layer. and forming an opening through which a conductive layer is formed on the surface of the first insulating layer and the fourth insulating layer through the opening. It can be produced by forming.

[0010] The semiconductor device of the present invention further comprises a first insulating layer formed on a substrate, and a second insulating layer formed on the first insulating layer. forming an insulating layer, forming a semiconductor layer on the second insulating layer, and forming a third insulating layer on the semiconductor layer a gate electrode is formed on the third insulating layer, a fourth insulating layer is formed on the gate electrode, and A resist is formed on the insulating layer, and a semiconductor layer is formed on at least the fourth insulating layer using the resist as a mask. A first opening is formed to partially expose the surface of the conductor layer, and at least The second insulating layer, the semiconductor layer and the fourth insulating layer are etched to form a first insulating layer surface and and forming a second opening that partially exposes the surface of the semiconductor layer, and The semiconductor layer is fabricated by forming a conductive layer on the insulating layer surface, the semiconductor layer surface, and the fourth insulating layer. The first opening can be formed by wet etching, and the second opening can be formed by can be formed by dry etching.

[0011] The semiconductor device of the present invention further comprises a first insulating layer formed on a substrate, and a second insulating layer formed on the first insulating layer. forming an insulating layer, forming a semiconductor layer on the second insulating layer, and forming a third insulating layer on the semiconductor layer a gate electrode is formed on the third insulating layer, a fourth insulating layer is formed on the gate electrode, and A resist is formed on the insulating layer, and a semiconductor layer is formed on at least the fourth insulating layer using the resist as a mask. A first opening is formed to partially expose the surface of the conductor layer, and the resist is etched to expose the first opening. The resist is then retreated, and at least the second insulating layer, the semiconductor layer, and the fourth insulating layer are formed using the resist as a mask. The insulating layer is etched to partially expose the first insulating layer surface and the semiconductor layer surface. and a surface of the first insulating layer, a surface of the semiconductor layer, and a fourth insulating layer are formed through the second opening. The insulating layer may be formed by forming a conductive layer on the insulating layer. The second opening can be formed by dry etching. Effect of the Invention

[0012] In the present invention, since it is not necessary to stop etching at the surface of the semiconductor film, the contact hole The etching process for forming the contacts can be easily controlled. The side of the contact hole can be electrically connected to the source electrode or the drain electrode. Therefore, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured. [Brief description of the drawings]

[0013] [Figure 1] 1A and 1B are a top view and a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Diagram 2] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Diagram 3] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Figure 4] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Diagram 5] 1A and 1B are a top view and a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 6] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Figure 7] 1A and 1B are a top view and a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 8] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Figure 9] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Figure 10] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Figure 11] 1A and 1B are a top view and a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 12] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Figure 13] 1 is a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 14] 1 is a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 15] 1 is a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 16] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Figure 17] 1A to 1C are cross-sectional views illustrating a manufacturing process of a semiconductor device of the present invention. [Figure 18] 1 is a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 19] 1 is a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 20] 1A and 1B are a top view and a cross-sectional view illustrating a structure of a semiconductor device of the present invention. [Figure 21] FIG. 1 is a cross-sectional view illustrating a configuration of a conventional semiconductor device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] The present invention will be described below with reference to the drawings. The present invention is not limited to the above, and various modifications and variations in form and detail are possible without departing from the spirit and scope of the present invention. It will be readily understood by those skilled in the art that the present invention can be modified in the following manner. The present invention is not limited to the above-described embodiment. In the configuration, the same reference numerals may be used in common between different drawings.

[0015] (Embodiment 1) In this embodiment, etching can be easily controlled when forming contact holes. The structure and manufacturing method of the semiconductor device will be described.

[0016] FIG. 1 is a top view and a cross-sectional view for explaining the main configuration of a semiconductor device according to the present invention. FIG. 1(A) shows a top view of a thin film transistor in particular, and FIG. 1(B) shows A and B of FIG. 1(A). FIG. 1(C) shows a cross-sectional view taken along a dashed line connecting C and D in FIG. 1(A). 1 shows a cross-sectional view of the

[0017] The semiconductor device shown in this embodiment is a semiconductor device provided in an island shape on a substrate 30 with an insulating layer 31 interposed therebetween. A conductor layer 32, a gate insulating layer 33 formed on the semiconductor layer 32, and a gate insulating layer 34 formed on the semiconductor layer 32. A thin film including a conductive layer 34 that functions as a gate electrode and is provided via a gate insulating layer 33. A thin-film transistor 205 and an insulating layer 203 provided over the gate insulating layer 33 and the conductive layer 34. 03 and a conductive layer functioning as a source electrode or a drain electrode provided over the insulating layer 203 204 (FIGS. 1(A) to 1(C)). The semiconductor layer 32 has a channel formation region. The impurity regions 32a and 32b, 32c functioning as a source region and a drain region are added. In addition, the end of the semiconductor layer 32, in this case, the channel forming region 32a below the conductive layer 34 is contacted. and an insulating layer 36 formed on the portion.

[0018] The semiconductor device shown in this embodiment has an insulating layer 203, an impurity region 32b of a semiconductor layer 32, 32c is etched to form a contact hole (also called an opening) that reaches the insulating layer 31b. Then, a conductive layer 204 is formed so as to fill the contact hole. In the embodiment, the conductive layer 204 and the impurity regions 32b and 32c are , 32c are electrically connected to the side surface of a contact hole formed in the first electrode 32a.

[0019] In this embodiment, since it is not necessary to stop etching at the surface of the semiconductor layer, the contact In addition, the etching process for forming the holes in the semiconductor layer can be easily controlled. The side of the contact hole is electrically connected to the source electrode or the drain electrode. Therefore, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured.

[0020] Here, the insulating layer 36 formed on the edge of the semiconductor layer is not necessarily formed, but it is possible to form the insulating layer 36 on the edge of the semiconductor layer. The end of the conductive layer 32 and the conductive layer 34 functioning as the gate electrode are short-circuited, causing a leakage current to flow. Therefore, when the insulating layer 36 is provided, it is preferable to provide at least If it is formed on the side surface (exposed portion) of the channel formation region 32a of the semiconductor layer 32, However, it is of course acceptable for the wiring to be formed in other parts. In this embodiment, the insulating layer 36 is formed on the lower side (substrate side) of the gate insulating layer 33. It is formed in contact with

[0021] Next, an example of a method for manufacturing the semiconductor device shown in FIG. The fabrication process in the cross section taken along the dashed line connecting A and B in FIG. 1(A) is shown in FIG. 2(A) to (D). 3(A)-(C) and Fig. 4(A)-(B), the dashed line connecting C and D in Fig. 1(A) The cross-sectional fabrication process is shown in Fig. 2(E)-(H), Fig. 3(D)-(F), Fig. 4(C)-(D). This will be explained using:

[0022] First, an insulating layer 31 is formed on a substrate 30 (FIGS. 2(A) and 2(E)). In this embodiment, The insulating layer 31 is a first insulating layer 31a formed on the substrate 30 and a second insulating layer 31b formed on the first insulating layer 31a. The formed second insulating layer 31b has a two-layer structure.

[0023] The substrate 30 may be a glass substrate, a quartz substrate, a metal substrate (e.g., a ceramic substrate or a stainless steel substrate). Substrates such as silicon substrates and other semiconductor substrates can also be used. As the substrate, polyethylene terephthalate (PET), polyethylene naphthalate ( You can also choose substrates such as polyethersulfone (PEN), polyethersulfone (PES), and acrylic. Cut.

[0024] The insulating layer 31 is formed by depositing silicon oxide, silicon nitride, or the like by using, for example, a CVD method or a sputtering method. Silicon, silicon oxide nitride (SiOxNy) (x>y>0), silicon oxide nitride (SiN For example, the first insulating material may be A silicon nitride oxide film is formed as the insulating layer 31a, and a silicon oxynitride film is formed as the second insulating layer 31b. A silicon nitride film is preferably formed as the first insulating layer 31a, and a silicon nitride film is preferably formed as the second insulating layer 31b. Alternatively, a silicon oxide film may be formed as the second insulating layer 31b. This prevents impurities such as alkali metals from diffusing from the substrate 30 and contaminating the elements formed thereon. It is possible.

[0025] Next, a semiconductor film 201 is formed on the insulating layer 31. The semiconductor film 201 is an amorphous semiconductor film. Alternatively, the insulating layer 31 may be formed of a crystalline semiconductor film. The amorphous semiconductor film is crystallized by heat treatment or laser light irradiation. As the semiconductor material, silicon is preferable, and other silicon A germanium semiconductor or the like can also be used.

[0026] The semiconductor film 201 has a thickness of 10 nm to 200 nm, preferably 10 nm to 50 nm, and more preferably It is preferable to form the semiconductor layer with a thickness of about 10 nm to 30 nm. When forming a semiconductor film, after forming a semiconductor film with a thickness of 50 nm or more, the surface of the semiconductor film is dried. A semiconductor film with a thickness of about 10 nm to 50 nm is formed by dry etching. The etching gas used in this etching is Cl2, BCl3, Si Chlorine gases such as Cl4, fluorine gases such as CF4, NF3, SF6, CHF3, etc. is a mixed gas made by adding an appropriate amount of inert gas such as O2 gas, H2 gas, He, or Ar to a fluorine-based gas. Before dry etching, the surface of the semiconductor film is treated with dilute hydrofluoric acid. The natural oxide film formed on the semiconductor surface is then removed, and the semiconductor film surface is then irrigated with ozone water or the like. An oxide film may be formed on the surface of the semiconductor film by processing.

[0027] By forming the semiconductor film 201 as a thin film of about 50 nm or less, In addition, the semiconductor film is formed as a thin film. This allows the TFT to be made smaller. In addition, the threshold voltage of the TFT can be controlled. Even if the amount of impurity elements doped into the channel formation region is increased to obtain a By forming a thin film, it becomes easier to fabricate a fully depleted TFT, resulting in a good S value. In this way, it is possible to fabricate a TFT with a controlled threshold voltage.

[0028] In addition, a semiconductor film is formed by crystallizing or recrystallizing an amorphous semiconductor film by irradiating it with laser light. When used as the membrane 201, a continuous wave (CW) laser diode pumped as a laser light source is used. The second harmonic (YVO4, wavelength 532 nm) can be used. Although it is not necessary to be limited to the second harmonic, the second harmonic is more energy efficient than higher harmonics. When a semiconductor film is irradiated with a CW laser, the energy is continuously transferred to the semiconductor film. Therefore, once the semiconductor film is put into a molten state, it can remain in the molten state. In addition, the solid-liquid interface of the semiconductor film is moved by scanning the CW laser, and this movement It is possible to form long crystal grains along the direction of the laser pulse. The reason is that compared to gas lasers, etc., the output is highly stable and stable processing is expected. This is because, in addition to CW lasers, pulsed lasers with repetition rates of 10 MHz or more can also be used. It is also possible to use a pulsed laser with a high repetition rate. If the laser pulse interval is shorter than the time it takes for the film to melt and solidify, the semiconductor The film can be kept in a molten state, and the movement of the solid-liquid interface creates a structure of long crystal grains in one direction. It is possible to form a semiconductor film that can be used with other CW lasers and lasers with a repetition rate of 1 Pulsed lasers of 0 MHz or higher can also be used. For example, gas lasers include There are Ar lasers, Kr lasers, CO2 lasers, etc. As for solid-state lasers, YAG lasers Laser, YLF laser, YAlO3 laser, GdVO4 laser, KGW laser, KYW laser, Alexandrite laser, Ti:sapphire laser, Y2O3 laser Lasers such as YAG lasers, Y2O3 lasers, GdV lasers, etc. There are ceramic lasers such as O4 lasers and YVO4 lasers. Metal vapor lasers and Examples of such lasers include helium cadmium lasers. When the laser light is emitted in TEM00 (single transverse mode), the This is preferable because it can improve the energy uniformity of the linear beam spot. Alternatively, a pulsed excimer laser may be used.

[0029] Next, a resist 202 is selectively formed on the semiconductor film 201 (FIGS. 2(A) and 2(E)). Then, the semiconductor film 201 is dry-etched using the resist 202 as a mask to form island-like The semiconductor layer 32 is formed (FIGS. 2B and 2F). The resist 202 is removed by etching. It is used as a mask when The above-mentioned materials can be appropriately selected and used.

[0030] The etching gases used in dry etching are CF4, NF3, SF6, C Fluorine-based gas such as HF3, or the fluorine-based gas plus O2 gas, H2 gas, He, Ar, etc. A mixed gas containing an appropriate amount of inert gas can be used. mixed gas of SF6 and O2, mixed gas of CHF3 and He, or mixed gas of CF4 and H It is recommended to use a mixed gas of 2. Also, etching is not limited to dry etching, and wet etching is also possible. In this case, the semiconductor film 201 may be etched with TMAH (tetrahydrofuran). methylanmmonium hydroxide, tetramethylammonium hydroxide Wet etching using an organic alkaline aqueous solution, typically alkoxide, is used. As a result, island-shaped semiconductor layers 32 can be formed. When using the above-mentioned method, only the semiconductor film 201 is selectively etched, and the insulating layer 31 In this way, the insulating surface can be etched without damaging the By isolating the semiconductor layer into islands, multiple thin-film transistors and peripheral circuits can be formed on the same substrate. When the above-mentioned elements are formed, the elements can be separated from each other.

[0031] The semiconductor layer 32 may be formed so that the end portion is vertical, or the end portion is tapered. The shape of the end of the semiconductor layer 32 can be changed by changing the etching conditions, etc. Preferably, the end of the semiconductor layer 32 is tapered. The taper angle is preferably 45° or more and less than 95°, and more preferably 60° or more and less than 95°. By forming the end of the semiconductor layer 32 in a nearly vertical shape, a parasitic channel can be formed. can be reduced.

[0032] Subsequently, the resist 202 formed on the semiconductor layer 32 is removed.

[0033] Next, an insulating layer 107 (hereinafter also referred to as a third insulating layer 107) is formed so as to cover the semiconductor layer 32. The third insulating layer 107 is formed by a CVD method or a sputtering method. Using the above, silicon oxide, silicon nitride, silicon oxynitride, silicon nitride oxide, SiO It can be formed using materials such as F, SiOC, DLC, and porous silica.

[0034] Moreover, the third insulating layer 107 is formed to a thickness that can sufficiently cover the end portions of the semiconductor layer 32 . The thickness of the third insulating layer 107 is 1.5 to 3 times the thickness of the semiconductor layer 32 formed thereunder. It is preferable to form the insulating film with a thickness in the range of 100 to 200 mm.

[0035] Next, the third insulating layer 107 is anisotropically etched mainly in the vertical direction. The insulating layer 36 (hereinafter referred to as the fourth insulating layer 3) in contact with the side surface of the semiconductor layer 32 is selectively etched. 6) is formed (Figures 2(D) and (H)).

[0036] When the third insulating layer 107 is anisotropically etched mainly in the vertical direction, a semiconductor The third insulating layer 107 formed on one surface of the conductive layer 32 and on the insulating layer 31b is gradually The surface of the semiconductor layer 32 and the insulating layer 31b are etched away. A third insulating layer 107 having the same thickness is formed. Therefore, one surface of the semiconductor layer 106 is exposed. By stopping the etching at the point where the semiconductor layer 32 is exposed, The third insulating layer 107 can be left only on and around the third insulating layer 107. corresponds to the fourth insulating layer 36. Note that the end of the semiconductor layer 32 is formed in a shape close to a vertical shape. By doing so, the third insulating layer 107 is formed only in the region in contact with the side surface of the semiconductor layer 32 and in the vicinity thereof. In other words, the fourth insulating layer 36 can be easily formed.

[0037] The third insulating layer 107 is etched by anisotropic etching mainly in the vertical direction. For example, reactive ion etching (RIE) may be used. Reactive Ion Etching can also be used. The plasma generation method is parallel plate type, magnetron type, dual frequency type, EC type, etc. They are classified into R type, helicon type, ICP type, etc. The etching gas used in this case is Therefore, an etching selectivity can be obtained between the third insulating layer 107 and the other layers (semiconductor layer 32). When selectively etching an insulating film, for example, CHF3, C Fluorine gases such as F4, C4F8, C2F6, and NF3 can be used. Inert gases such as helium (He), argon (Ar), xenon (Xe), or O2 gas Gas, H2 gas may be added appropriately.

[0038] The shape of the fourth insulating layer 36 can be determined by appropriately selecting the material for forming the thin film, the etching conditions, etc. In this embodiment, the fourth insulating layer 36 is a bottom surface (insulating layer 3 1b) is formed so that its vertical height from the surface in contact with the semiconductor layer 32 is approximately equal to that of the semiconductor layer 32. In addition, the fourth insulating layer 36 has a curved surface that does not contact the side surface of the semiconductor layer. Specifically, the surface of the semiconductor layer 32 has a given curvature and is curved in a convex shape with respect to the side surface of the semiconductor layer 32 that is in contact with the surface of the semiconductor layer 32. Of course, the present invention is not particularly limited, and the fourth insulating layer 36 is formed in a rounded shape. The fourth insulating layer 36 may have a corner shape instead of a square shape. By making the shape of the insulating layer 33 gentle, the covering property of the layer (here, the insulating layer 33) laminated on the upper layer can be improved. The etching conditions are the type of etching gas, the flow rate ratio of each gas, In addition, the amount of power applied to the electrode on which the substrate is placed, the electrode temperature of the electrode on which the substrate is placed, Indicates pressure inside the bar, etc.

[0039] Next, an insulating layer 33 (hereinafter also referred to as a fifth insulating layer 33) is formed on the semiconductor layer 32 and the fourth insulating layer 36. The fifth insulating layer 33 is formed by a CVD method or a sputtering method (FIGS. 3A and 3D). Silicon oxide, silicon nitride, silicon oxynitride, silicon nitride oxide, and nitrogen are produced by the etching method. The fifth insulating layer 33 is formed of a material such as aluminum nitride. The fifth insulating layer 33 is formed of a single layer or a multilayer structure by using one or more of these. The thickness is 1 nm to 50 nm, preferably 1 nm to 20 nm, more preferably 1 nm to It is formed in the range of 10 nm.

[0040] The method for forming the insulating layer 36 is not limited to that shown in this embodiment. The edge of layer 32 is subjected to wet oxidation or plasma treatment in an atmosphere containing oxygen. In this case, after forming the insulating layer 33 on the semiconductor layer 32, the edge of the semiconductor layer 32 may be The insulating layer 33 covering the semiconductor layer 32 is removed, and the exposed portion of the semiconductor layer 32 is treated with plasma or wet acid. It is preferable to form the insulating layer 36 by curing.

[0041] In the case of wet oxidation, an aqueous solution containing ozone, an aqueous solution containing hydrogen peroxide, an aqueous solution containing sulfuric acid, The surface of the semiconductor layer 32 is treated with an aqueous solution, an aqueous solution containing iodic acid, or an aqueous solution containing nitric acid. By this treatment, the oxide film formed on the exposed portion of the semiconductor layer 32 is converted into the insulating layer 36. The aqueous solution containing ozone, the aqueous solution containing hydrogen peroxide, the aqueous solution containing sulfuric acid, The aqueous solution containing iodic acid or the aqueous solution containing nitric acid is preferably an aqueous solution containing acetic acid or oxalic acid. may also include

[0042] In addition, oxygen-containing atmospheres include oxygen (O2) and rare gases (He, Ne, Ar, K In a mixed gas atmosphere of oxygen, hydrogen (H2) and rare gas (r, xenon), In a mixed gas atmosphere of dinitrogen monoxide and rare gas, or in a mixed gas atmosphere of dinitrogen monoxide and rare gas The reaction can be carried out under a mixed gas atmosphere of nitrogen, hydrogen, and rare gases. For example, oxygen (O2), water A mixture of hydrogen (H2) and argon (Ar) can be used. In this case, the flow rate is: Oxygen at 0.1-100sccm, hydrogen at 0.1-100sccm, argon at 100-5 The oxygen:hydrogen:argon ratio should be 1:1:100. It is preferable to introduce a mixed gas. For example, oxygen at 5 sccm, hydrogen at 5 sccm, and arsenic at 5 sccm. Just introduce 500sccm of gon.

[0043] In addition, nitrogen-containing atmospheres include nitrogen (N2) and rare gases (He, Ne, Ar, K r, Xe) in a mixed gas atmosphere of nitrogen, hydrogen and rare gases It can be performed under a gas atmosphere or a mixture of ammonia (NH3) and rare gases. can.

[0044] The plasma treatment was carried out in an atmosphere of the above gas with an electron density of 1×1011 cm-3 More specifically, the plasma is used with an electron temperature of 1.5 eV or less. The electron density is between 1×1011cm-3 and 1×1013cm-3, and the electron temperature is 0.5 eV The plasma has a high electron density and is 1.5 eV or less. As a result, the electron temperature in the vicinity of the processing object (here, the semiconductor layer 32) formed on the substrate 30 is low. Therefore, damage to the object to be treated by the plasma can be prevented. Since the electron density of the ion beam is high at 1×1011cm-3 or more, the ion beam can be processed by plasma treatment. The oxide film or nitride film formed by oxidizing or nitriding the irradiated object is formed by a CVD method or Compared to films formed by sputtering, etc., it forms a dense film with excellent uniformity in film thickness. In addition, since the electron temperature of the plasma is low at 1.5 eV or less, Compared with the Zuma treatment and thermal oxidation method, the oxidation or nitridation treatment can be performed at a lower temperature. For example, even if plasma treatment is performed at a temperature 100 degrees or more lower than the distortion point of the glass substrate, oxidation is sufficient. In addition, the frequency for generating plasma is microwave (2 High frequencies such as 1.45 GHz can be used.

[0045] Next, a conductive layer 34 that functions as a gate electrode is formed on the gate insulating layer 33 (FIG. 3(B) Here, the conductive layer 34 is formed as a single layer. The conductive material may be laminated in two or three or more layers. However, the conductive layer 34 is formed by selectively etching the conductive layer formed covering the gate insulating layer 33. The insulating layer can be formed by:

[0046] The conductive layer 34 may be made of tantalum (Ta), tungsten (W), titanium (Ti), molybdenum (Mo), or the like. Mo, aluminum (Al), copper (Cu), chromium (Cr), niobium (Nb), etc. The elements selected from the above, or alloy materials or compound materials mainly composed of these elements, In addition, it is possible to form a polycrystalline silicon doped with an impurity element such as phosphorus. For example, the conductive layer 34 may be formed of a first conductive film and a second conductive film. When a laminated structure with a conductive film is formed, tantalum nitride is used as the first conductive film, and a second conductive film is The conductive layer may be formed using tungsten. When 34 is formed by laminating, the above materials can be freely combined.

[0047] Next, the impurity element 121 is introduced into the semiconductor layer 32 using the conductive layer 34 as a mask. Therefore, the semiconductor layer 32 does not have the impurity regions 32b and 32c and the impurity element 121 introduced therein. A channel forming region 32a is formed (FIGS. 3(B) and (E)). In order to form the conductive layer 32 so as to cross the island-shaped semiconductor layer 32 and then introduce the impurity element, Impurities are introduced into the regions of the semiconductor layer 32 that are not covered by the insulating layer 34 to form impurity regions 32b and 32c. c is formed, and the impurity element 121 is introduced into the region of the semiconductor layer 32 covered with the conductive layer 34. In this way, a channel formation region 32a that is not exposed to the ion beam is formed.

[0048] Here, the impurity element 121 is an impurity element that imparts n-type conductivity or an impurity element that imparts p-type conductivity. Impurity elements that exhibit n-type conductivity include phosphorus (P) and arsenic (As As impurity elements showing p-type, boron (B) and aluminum can be used. For example, the impurity element 121 may be aluminum (Al), gallium (Ga), or the like. The semiconductor layer is then doped with phosphorus (P) at a concentration of 1×1018 to 1×1021 / cm3. The impurity regions 32b and 32c are formed by introducing the impurity into the channel 32. Between the formation region 32a and the impurity regions 32b and 32c which are the source region and the drain region, The impurity is added at a lower concentration than the impurity regions 32b and 32c which are the source and drain regions. A low concentration impurity region (LDD region) may be formed by adding a low concentration impurity region. This reduces the electric field at the drain end, suppressing deterioration caused by repeated writing and erasing. It can be controlled.

[0049] In addition, the impurity doped in the channel forming region 32a is opposite to the impurity doped in the impurity regions 32b and 32c. Alternatively, an impurity element having a conductivity type other than that of the n-type TFT (eg, boron for an n-type TFT) may be added. By doping the channel forming region 32a with impurities of the opposite conductivity type, the threshold voltage of the TFT The voltage can be controlled. The impurity element can be doped through the gate electrode. Alternatively, it may be added in advance before the gate electrode is formed.

[0050] Next, an insulating layer 203 is formed so as to cover the conductive layer 34 and the gate insulating layer 33 (FIG. 3(C) , (F)). Next, a resist 207 is selectively formed on the insulating layer 203.

[0051] Then, the insulating layer 203, the gate insulating layer 33, and the semiconductor layer 32 are dry-etched. Contact holes are formed (FIGS. 4A and 4C). Next, a source electrode is formed on the insulating layer 203. A conductive layer 204 that functions as a gate or drain electrode is selectively formed (FIG. 4(B), (D)). Here, the conductive layer 204 is connected to the insulating layer 203, the gate insulating layer 33, and the semiconductor layer 32. The conductive layer 204 is formed so as to fill the contact hole. The impurity regions 32b and 32c functioning as a source region or a drain region are impurity regions 32b, 32c are electrically connected to the side of the contact hole. It is provided.

[0052] Here, the insulating layer 203 is made of silicon oxide, oxide film, or the like formed by a CVD method, a sputtering method, or the like. Silicon nitride (SiOxNy) (x>y>0), silicon oxide nitride (SiNxOy) ( x>y>0) can be used. Also, polyimide, polyamide, polyvinyl chloride, etc. can be used. Organic materials such as phenol, benzocyclobutene, acrylic, epoxy, etc., or siloxane resin The material is a single layer or laminated structure made of siloxane materials such as grease, oxazole resin, etc. It is possible to make a siloxane material. The skeleton of xane is composed of bonds between silicon (Si) and oxygen (O). For this purpose, an organic group containing at least hydrogen (for example, an alkyl group or an aromatic hydrocarbon) is used. A fluoro group can also be used as a substituent. Oxazole resins are, for example, photosensitive Photosensitive polybenzoxazole has a low dielectric constant (normal It has a dielectric constant of 2.9 at 1MHz and high heat resistance (differential thermal analysis / thermogravimetry (TG / DTA:T hermogravimetry-Differential Thermal Ana lysis) with a temperature rise of 5℃ / min, thermal decomposition temperature of 550℃, low water absorption rate (24 hours at room temperature) Oxazole resin is a material with a dielectric constant of 0.3%. It has a dielectric constant of 3.2 to 3.5%, similar to polyimide. 4), the dielectric constant is low (about 2.9), which suppresses the generation of parasitic capacitance. In this example, the insulating layer 203 is an oxide film formed by a CVD method. Silicon, silicon oxynitride (SiOxNy) (x>y>0) or silicon oxynitride (S iNxOy) (x>y>0) is formed as a single layer or a laminate. Organic materials such as polyamide, polyvinylphenol, benzocyclobutene, acrylic, and epoxy The material may be formed by laminating a siloxane material such as a siloxane resin or an oxazole resin. good.

[0053] The conductive layer 204 may be made of aluminum, tungsten, titanium, tantalum, molybdenum, A single layer made of an element selected from nickel and neodymium or an alloy containing multiple of the elements. For example, a conductive layer made of an alloy containing a plurality of the elements can be used. Aluminum alloys containing titanium and aluminum alloys containing neodymium as conductive films In the case of providing a laminated structure, for example, an aluminum layer or Alternatively, the aluminum alloy layer may be sandwiched between titanium layers to form a laminate structure. good.

[0054] Through the above steps, a semiconductor device including the thin film transistor 205 can be manufactured.

[0055] In this embodiment, since it is not necessary to stop etching at the surface of the semiconductor film, In addition, the etching process for forming the holes in the semiconductor layer can be easily controlled. The side of the contact hole is electrically connected to the source electrode or the drain electrode. Therefore, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured.

[0056] Also, a thick insulating layer may be selectively provided at the end of the channel formation region of the semiconductor layer. This can reduce the electric field concentration at the end of the channel formation region of the semiconductor layer. Therefore, it is possible to reduce gate leakage defects and improve the breakdown voltage of the gate electrode. .

[0057] (Embodiment 2) In this embodiment mode, a structure and a manufacturing method of a semiconductor device different from that in FIG. 1 will be described.

[0058] FIG. 5 is a top view and a cross-sectional view for explaining the configuration of the semiconductor device according to the present embodiment. FIG. 5(A) shows a top view of a thin film transistor, and FIG. 5(B) shows A and B of FIG. 5(A). FIG. 5(C) is a cross-sectional view taken along the dashed line connecting C and D in FIG. 5(A). A cross-sectional view is shown.

[0059] The semiconductor device shown in this embodiment is a semiconductor device provided in an island shape on a substrate 30 with an insulating layer 31 interposed therebetween. A conductor layer 32, a gate insulating layer 33 formed on the semiconductor layer 32, and a gate insulating layer 34 formed on the semiconductor layer 32. A thin film including a conductive layer 34 that functions as a gate electrode and is provided via a gate insulating layer 33. A thin-film transistor 205 and an insulating layer 203 provided over the gate insulating layer 33 and the conductive layer 34. 03 and a conductive layer functioning as a source electrode or a drain electrode provided over the insulating layer 203 204 (FIGS. 5A to 5C). The semiconductor layer 32 has a channel formation region. The impurity regions 32a and 32b, 32c functioning as a source region and a drain region are added. In addition, the end of the semiconductor layer 32, in this case, the channel forming region 32a below the conductive layer 34 is contacted. An insulating layer 36 is formed in the channel forming region 32a. Impurities of the opposite conductivity type to the impurities added to the pure regions 32b and 32c may be added. stomach.

[0060] The semiconductor device shown in this embodiment has an insulating layer 203, an impurity region 32b of a semiconductor layer 32, 32c, the insulating layer 31b is etched to form a contact hole reaching the insulating layer 31a. Then, a conductive layer 204 is formed so as to fill the contact hole. In this embodiment, the conductive layer 204 and the impurity regions 32b and 32c are They are electrically connected to the side surface of a contact hole formed in 2c.

[0061] Next, the manufacturing process in the cross section taken along the dashed line connecting A and B in FIG. 5(A) is shown in FIG. 6(A) to (B). The fabrication process for the cross section taken along the dashed line connecting C and D in FIG. 5(A) is shown in FIG. 6(C) to FIG. D) will be used to explain.

[0062] First, similarly to the first embodiment, insulating layers 31a and 31b are formed on a substrate 30, and insulating layer 31 A semiconductor layer 32, an insulating layer 36 and a gate insulating layer 33 are formed on the surface of the gate insulating layer 33. A conductive layer 34 that functions as a gate electrode is formed, and an insulating layer 203 is formed over the conductive layer 34. (FIGS. 6(A) and 6(C)). Here, a resist 207 is formed on the insulating layer 203. .

[0063] Next, the insulating layer 203, the gate insulating layer 33, and the semiconductor layer 32 are patterned using the resist 207 as a mask. The insulating layer 31b is etched to form a contact hole reaching the insulating layer 31a. (Figure 6(B) and (D)).

[0064] Next, the resist 207 is removed. The subsequent steps are the same as in the first embodiment, except that the contact holes are not removed. A conductive layer 204 is formed so as to fill the holes, thereby fabricating the semiconductor device shown in FIG. It is possible.

[0065] In this embodiment, since it is not necessary to stop etching at the surface of the semiconductor film, In addition, the etching process for forming the holes in the semiconductor layer can be easily controlled. The side of the contact hole is electrically connected to the source electrode or the drain electrode. Therefore, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured.

[0066] Also, a thick insulating layer may be selectively provided at the end of the channel formation region of the semiconductor layer. This can reduce the electric field concentration at the end of the channel formation region of the semiconductor layer. Therefore, it is possible to reduce gate leakage defects and improve the breakdown voltage of the gate electrode. .

[0067] (Embodiment 3) In this embodiment mode, a structure and a manufacturing method of a semiconductor device different from those shown in FIG. 1 or FIG. do.

[0068] FIG. 7 is a top view and a cross-sectional view for explaining the configuration of the semiconductor device according to the present embodiment. FIG. 7(A) shows a top view of a thin film transistor, and FIG. 7(B) shows A and B of FIG. 7(A). 7(A) and FIG. 7(C) is a cross-sectional view taken along the dashed line connecting C and D in FIG. 7(A). A cross-sectional view is shown.

[0069] As shown in FIG. 7, the semiconductor device of this embodiment has the structure shown in FIG. In other words, the shape of the contact hole is different in the semiconductor device shown in this embodiment. In this process, the insulating layer 203, the impurity regions 32b and 32c of the semiconductor layer 32, and the insulating layer 31b are etched. The contact hole reaching the insulating layer 31a formed by the etching is formed on the surface of the semiconductor layer 32. The impurity regions 32b and 32c are also formed so as to be exposed. In the embodiment, the conductive layer 204 and the impurity regions 32b and 32c are The side surface of the contact hole formed in the region c and the surfaces of the impurity regions 32b and 32c are electrically connected to the contact hole. In this embodiment, the insulating layer 31b is also electrically connected to the contact hole. However, no contact holes are formed in the insulating layer 31b. A contact hole may be formed so that the surface is exposed.

[0070] Next, the manufacturing process in the cross section taken along the dashed line connecting A and B in FIG. 7(A) is shown in FIG. 8(A) to (C). 9(A)-(B), the cross section taken along the dashed line connecting C and D in FIG. 7(A) was fabricated. The process will be described with reference to Figs. 8(D) to (F) and Figs. 9(C) to (D).

[0071] First, similarly to the first embodiment, insulating layers 31a and 31b are formed on a substrate 30, and insulating layer 31 A semiconductor layer 32, an insulating layer 36 and a gate insulating layer 33 are formed on the surface of the gate insulating layer 33. A conductive layer 34 that functions as a gate electrode is formed, and an insulating layer 203 is formed over the conductive layer 34. (FIGS. 8(A) and 8(D)). Here, a resist 207 is formed on the insulating layer 203. .

[0072] Next, the insulating layer 203 and the gate insulating layer 33 are dry etched using the resist 207 as a mask. Then, contact holes reaching the semiconductor layer 32 are formed (FIGS. 8(B) and 8(E)).

[0073] Next, the insulating layer 203 and the gate insulating layer 33 are removed by wet etching using the resist 207 as a mask. Then, the insulating layer 203 and the gate insulating layer 33 are recessed outward.

[0074] Next, the semiconductor layer 32 and the insulating layer 31b are dry etched using the resist 207 as a mask. Then, a contact hole is formed that reaches the insulating layer 31a. As a result, the impurity region 32 The contact holes 32b and 32c expose the side surfaces of the impurity regions 32b and 32c. It is possible to form a

[0075] The subsequent steps are performed to fill the contact holes in the same manner as in the first or second embodiment. By forming a conductive layer 204 on the insulating film 204, the semiconductor device shown in FIG. 7 can be manufactured.

[0076] Next, a manufacturing method different from the method shown in FIGS. 8 and 9 will be described with reference to FIG. The fabrication process for the cross section taken along the dashed line connecting A and B in (A) is shown in Fig. 10(A) to (C). The fabrication process in the cross section taken along the dashed line connecting C and D in FIG. 7(A) is shown in FIG. 10(D) to (F). I will use this to explain.

[0077] First, similarly to FIGS. 8B and 8E, insulating layers 31a and 31b are formed on a substrate 30, and insulating A semiconductor layer 32, an insulating layer 36 and a gate insulating layer 33 are formed on the layer 31b. A conductive layer 34 that functions as a gate electrode is formed on the insulating layer 203. The insulating layer 203 and the gate electrode 204 are formed by using the resist 207 formed on the insulating layer 203 as a mask. The insulating layer 33 is dry etched to form contact holes (FIGS. 10(A) and 10(D)). )).

[0078] Next, the resist 207 is dry etched to retreat outward (FIG. 1 0(B), (E)). Next, the resist 207 is used as a mask to form the insulating layer 203 and the gate insulating layer 204. The layer 33, the semiconductor layer 32, and the insulating layer 31b are dry etched to expose the insulating layer 31a. A contact hole is formed through the contact hole (FIGS. 10C and 10F). The contact holes 32b and 32c expose the side surfaces of the impurity regions 32b and 32c. It is possible to form a

[0079] In the subsequent steps, a conductive layer 204 is formed so as to fill the contact holes in the same manner as in the first embodiment. By forming the above, the semiconductor device shown in FIG. 7 can be manufactured.

[0080] In this embodiment, since it is not necessary to stop etching at the surface of the semiconductor film, In addition, the insulating layer 203 and the semiconductor Since a step is formed between the conductive layer 32 and the conductive layer 2 on the side surface of the contact hole, The coating property of 04 is improved, and the variation in the film thickness of the conductive layer 204 and the breakage of the conductive layer 204 are prevented. This makes it possible to suppress the variation in contact resistance. The side of the contact hole is electrically connected to the source electrode or the drain electrode. Therefore, a semiconductor device with suppressed deterioration of characteristics can be easily manufactured. do.

[0081] Also, a thick insulating layer may be selectively provided at the end of the channel formation region of the semiconductor layer. This can reduce the electric field concentration at the end of the channel formation region of the semiconductor layer. Therefore, it is possible to reduce gate leakage defects and improve the breakdown voltage of the gate electrode. .

[0082] (Embodiment 4) The semiconductor device according to the present invention is not limited to the configurations shown in the first to third embodiments, and may have various shapes. In this embodiment, a thin-film transistor in which a semiconductor layer is partially silicided is used. The structure and manufacturing method of the semiconductor device of this embodiment mode are described below. Figure 11(A) is a top view, and Figure 11(B) is a cross-sectional view taken along dashed line AB in Figure 11(A). 11(C) shows a cross-sectional view taken along dashed line CD in FIG. 11(A).

[0083] As shown in FIG. 11, the semiconductor device of the present embodiment includes a semiconductor layer 32 in addition to the configuration shown in FIG. A silicide region 1102 is formed on a part of the surface of the gate electrode. The conductive layer 34 is formed of a laminated structure of a first conductive layer 34a and a second conductive layer 34b. An insulating layer (also called a sidewall insulating layer) 1101 is formed on the side wall of the conductive layer 34. Furthermore, the impurity regions (high concentration impurity) functioning as source and drain regions are The impurity regions 32b and 32c are disposed between the channel forming region 32a and the impurity regions 32b and 32c. Regions 32d and 32c are doped with impurities at lower concentrations (also called low-concentration impurity regions). 2e is formed.

[0084] Next, a method for manufacturing the semiconductor device shown in FIG. 11 will be described.

[0085] First, similarly to the first embodiment, insulating layers 31a and 31b are formed on a substrate 30, and insulating layer 31 A semiconductor layer 32, an insulating layer 36 and a gate insulating layer 33 are formed on the surface of the gate insulating layer 33. A first conductive layer 34a and a second conductive layer 34b that function as a gate electrode are formed (FIG. 12). Next, an impurity source that imparts one conductivity type with a first concentration is implanted using the conductive layer 34b as a mask. After doping, the conductive layer 34a and the conductive layer 34b are used as a mask to dope the impurity element of a second concentration. By doping, a pair of high concentration impurity regions 32b and 32c and a pair of low concentration Impurity regions 32d and 32e and a channel forming region 32a are formed. The impurity element of the first concentration and the impurity element of the second concentration are doped with impurity elements of the same conductivity type, for example. Boron (B), aluminum (Al), and gallium (Ga ), and impurity elements such as phosphorus (P) and arsenic (As) that give n-type conductivity can be added. do.

[0086] In addition, the channel forming region 32a is given one conductivity type for controlling the threshold voltage of the transistor. The channel formation region 32a may be doped with an impurity element. This can be done before forming the conductive layer 34. Also, the impurity element that imparts one conductivity type After the doping, a heat treatment may be performed to activate the doped impurity element. The annealing can be performed by using a laser beam irradiation, or an RTA or furnace annealing oven. The heating may be performed at a temperature in the range of 00°C to 700°C, preferably 500°C to 650°C. The heat treatment is preferably carried out in a nitrogen atmosphere.

[0087] Next, a sidewall insulating layer 1101 is formed to contact the side surfaces of the conductive layer 34a and the conductive layer 34b. (Figure 12(B)).

[0088] The sidewall insulating layer 1101 forms an insulating layer on the conductive layer 34a and the conductive layer 34b. Selectively etching the insulating layer by anisotropic etching mainly in the vertical direction. For example, the silicon oxide film can be formed by a CVD method or a sputtering method. Inorganic materials such as silicon nitride, silicon oxynitride, silicon oxynitride, and silicon nitride oxide, and organic resins An insulating layer having a single layer structure or a laminated structure is formed using an organic material, and the insulating layer is selectively etched. The sidewall insulating layer 1101 can be formed by etching the silicide region. This is used as a silicide mask when forming the sidewall insulating layer. The layer 1101 has a curved surface that does not contact the side surfaces of the conductive layers 34a and 34b. The sidewall insulating layer 1101 is formed by the conductive layer 34a and the conductive layer 34 which form the gate electrode. It is formed so as to completely cover the side of b.

[0089] In this embodiment, the etching for forming the sidewall insulating layer 1101 is The insulating layer 33 underneath is also etched away, selectively exposing a portion of the semiconductor layer 32. Specifically, the high concentration impurity region 32 in the region not overlapping with the sidewall insulating layer 1101 is Depending on the etching conditions, the high concentration impurity regions 32b and 32c are exposed. The upper layer of 2c may also be etched, resulting in a decrease in film thickness (known as film loss).

[0090] Next, a metal layer 1103 is formed on the exposed surface of the semiconductor layer 32 (FIG. 12(C)).

[0091] The metal layer 1103 may be formed at least on the exposed semiconductor layer 32. The sidewall insulating layer 1101 is formed in a region of the conductor layer 32 that does not overlap the sidewall insulating layer 1101. In this embodiment, the metal layer 1103 is formed on the sidewall insulation layer 1102 and not only on the exposed surface of the semiconductor layer 32. The metal layer 1103 is formed so as to cover the edge layer 1101 and the conductive layer 34. The metal layer 1103 reacts with the semiconductor layer. The material is formed by using a material that forms a silicide by contacting the metal with the metal. For example, nickel (Ni), titanium (T i) Metal elements such as cobalt (Co) or platinum (Pt), or alloys containing such metal elements The metal layer 1103 is formed by sputtering using these materials. The metal layer 1103 is formed by a method such as deposition or plating. It is necessary to select the thickness appropriately depending on the film thickness of the side region. In this embodiment, the metal layer 1103 and In addition, when forming the metal layer 1103, the exposed If a natural oxide film is formed on the exposed semiconductor layer 32, the natural oxide film is removed. Then, a metal layer 1103 may be formed.

[0092] Next, a silicide region 1102 is formed in a part of the semiconductor layer 32 (FIG. 12(D)).

[0093] The silicide region 1102 is formed by heat treatment to remove the semiconductor layer 32 and the metal layer 1103. The silicide region 1102 is formed by a reaction between the metal layer 1103 and the silicide layer 1104. A part of the semiconductor layer 32 in the region where the semiconductor layer 32 contacts the semiconductor layer 32 is silicided. The high concentration impurity regions 32b and 32c formed in the semiconductor substrate 32 are partially silicided. It can also be said that a silicide region is formed in a part of the high-concentration impurity region. For example, when nickel is formed as the metal layer 1103, the silicide region 1102 is Similarly, titanium, cobalt, When platinum is formed, titanium silicide is formed as the silicide region 1102, and platinum is formed as the silicide region 1102. Cobalt silicide and platinum silicide are formed.

[0094] The heat treatment can be performed using an RTA or an annealing furnace. The temperature range is 00°C to 700°C, and the range is 10 seconds to 1 hour, preferably 20 seconds to 30 minutes. In this embodiment, the heat treatment is performed at 550° C. for 30 seconds to form nickel silicide. A silicide region 1102 made of silicide is formed.

[0095] In FIG. 12D, the silicide region 1102 is formed in the channel formation region of the semiconductor layer 32. The thickness of the sidewall 32a is smaller than that of the sidewall 32b. In the semiconductor layer 32 in the region not overlapping with the insulating layer 1101, The high concentration impurities 32b and 32c are formed on the side of the insulating layer 31b. A silicide region 1102 is formed in contact with the upper layer of 32b, 32c.

[0096] The shape, thickness, etc. of the silicide region 1102 depend on the thickness of the metal layer 1103 to be reacted, the thermal The selection can be made by appropriately controlling the treatment temperature, the heat treatment time, etc. As shown in FIG. 13B, the semiconductor in the region not overlapping with the sidewall insulating layer 1101 is In the layer 32, a part or the whole of the semiconductor layer 32 in the region is The upper surface may be a silicide region 1102 formed by silicidizing the semiconductor. The surface of the insulating layer 32 on which a metal layer for silicidation is formed is called the bottom surface. In addition, when the entire surface from the top to the bottom is silicided, A high-concentration impurity region is formed under the side wall insulating layer 1101. The present invention is not particularly limited, and a part of the silicide region is a half under the sidewall insulating layer 1101. The conductor layer 32 (excluding the channel forming region 32a) may be formed.

[0097] In addition, if an unreacted metal layer remains after the reaction between the semiconductor layer 32 and the metal layer 1103, The unreacted metal layer is removed by removing the insulating layer 36 and the sidewall insulating layer, which are not shown in the figure. The metal layer 1103 formed on the layer 1101, the conductive layer 34b and the insulating layer 31b is removed. In addition, if an unreacted metal layer remains on the formed silicide region 1102, the remaining metal layer is The unreacted metal layer is also removed by wet etching or dry etching. In this case, the etching gas or the etching solution is unreacted. The metal layer and other layers (e.g., insulating layer 36, sidewall insulating layer 1101, conductive layer 34) of the reaction b, the insulating layer 31b and the silicide region 1102) have a sufficient etching selectivity. In other words, the etching rate for the metal layer is high and the etching rate for other layers is low. For example, the metal layer 1103 may be made of nickel. When the sample was prepared, a mixture of hydrochloric acid (HCl), nitric acid (HNO3) and pure water (H2O) was used. It can be removed by wet etching. For example, the mixture ratio of the solution is HCl:H The ratio can be NO3:H2O=3:2:1.

[0098] In this embodiment, the insulating layer 36 is formed in contact with the side surface of the end of the semiconductor layer 32. Therefore, when the unreacted metal layer is etched away, the side surface of the semiconductor layer 32 is also etched. This can prevent the loss of data.

[0099] In addition, when forming a silicide region, the silicide region and the gate electrode are formed by using a conductive material. This is because the silicide region and the gate electrode must not come into contact with each other. If this happens, the gate electrode and the source or drain region will be shorted, resulting in poor switching characteristics. This is because the device will no longer function as a semiconductor device due to the loss of its on / off ratio. Therefore, in this embodiment, the width of the conductive layers 34a and 34b forming the gate electrode is The sidewall insulating layer 1101 is narrower than the insulating layer 33 which functions as a gate insulating layer. The end of the insulating layer 33 is made to substantially coincide with the end of the insulating layer 33 .

[0100] Next, an insulating layer 203 is formed so as to cover the insulating layer, the conductive layer, and the like provided on the substrate 30 ( Figure 13(A)).

[0101] The subsequent steps are the same as in the first embodiment, with the insulating layer 203 and the semiconductor layer 32, and the insulating layer 31b being A contact hole is formed to reach the contact hole, and a conductive layer 204 is formed to fill the contact hole. In this manner, the semiconductor device shown in FIG. 11 or FIG. 13A can be manufactured.

[0102] The semiconductor device of the present embodiment is not limited to the one shown in FIGS. 11 to 13, but may be the one shown in FIGS. 14 to 15. The shape shown in the figure may also be used.

[0103] The semiconductor device shown in FIG. 14A has the same structure as that shown in FIG. 13A and is filled with a conductive layer 204. The shape of the contact hole is different. That is, in the semiconductor device shown in FIG. The contact hole filled with the conductive layer 204 is filled with impurities of the insulating layer 203 and the semiconductor layer 32. The object regions 32b and 32c reach the insulating layer 31a formed by etching the insulating layer 31b. Therefore, in this embodiment, the conductive layer 204 and the impurity region 32 b and 32c are the side surfaces of the contact holes formed in the impurity regions 32b and 32c. The contact hole shown in FIG. 14(A) is the same as that in the third embodiment. It should be noted that the method is not limited to that shown in FIG. As shown in FIG. 14B, a part or the whole of the semiconductor layer 32 is shielded from the upper surface to the lower surface. Residualized silicide regions 1102 may be formed.

[0104] The semiconductor device shown in FIG. 15A has the same structure as that shown in FIG. 13A, except that a conductive layer 204 is filled in the semiconductor device. In other words, the semiconductor device shown in this embodiment has a different shape of the contact hole. In this case, the insulating layer 203, the impurity regions 32b and 32c of the semiconductor layer 32, and the insulating layer 31b are etched. The contact hole reaching the insulating layer 31a formed by etching is formed on the surface of the semiconductor layer 32. The impurity regions 32b and 31c are also exposed. In this embodiment, the conductive layer 204 and the impurity regions 32b and 32c are On the side surface of the contact hole formed in 2c and on the surfaces of the impurity regions 32b and 32c In the present embodiment, the insulating layer 31b is also provided with a contact hole. However, no contact holes are formed in the insulating layer 31b. A contact hole may be formed so that the surface is exposed. The hole can be formed in the same manner as in the third embodiment. It is not limited to the one shown in (A), but may be applied to a part or the whole of the semiconductor layer 32 as shown in FIG. Alternatively, a silicide region 1102 may be formed by silicidizing the entire surface from the top surface to the bottom surface. .

[0105] In this embodiment, since it is not necessary to stop etching at the surface of the semiconductor film, In addition, the etching process for forming the holes in the semiconductor layer can be easily controlled. The side of the contact hole is electrically connected to the source electrode or the drain electrode. Therefore, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured.

[0106] (Embodiment 5) The semiconductor device described in the first to fourth embodiments is a semiconductor device made of silicon oxide on a single crystal silicon substrate. An oxide film is formed, and the single crystal semiconductor thin film formed on the oxide film can be used as the active layer. In this embodiment, a semiconductor device using SOI technology called SIMOX is described. explain.

[0107] First, a single crystal silicon substrate 601 is prepared as a material for forming the single crystal silicon layer (FIG. 16). (A) Here, the case of using a P-type single crystal silicon substrate is explained, but the case of using an N-type single crystal silicon substrate is also explained. Of course, a single crystal silicon germanium substrate can also be used. can.

[0108] Next, oxygen ions are added to the single crystal silicon substrate 601 to form an oxygen-containing layer at a predetermined depth. A layer 602 is formed (FIG. 16B). The oxygen ions are, for example, 1×10 atoms / The oxygen-containing layer 602 may be formed at a dose of about 1 / 2 cm. The distance between the main surface of the crystalline silicon substrate 601 and the oxygen-containing layer 602 is determined by the distance between the main surface of the crystalline silicon substrate 601 and the oxygen-containing layer 602. This is the thickness of the single crystal silicon layer that functions as the active layer of the TFT.

[0109] Next, a heat treatment is performed at a temperature of 800 to 1200° C. to bury the oxygen-containing layer 602 and form the insulating layer 6 The width of the oxygen-containing layer 602 in the depth direction is changed to 03 by the distribution of oxygen ions at the time of ion addition. The concentration of oxygen ions is determined by the fabric. Therefore, the interface between the single crystal silicon substrate 601 and the buried insulating layer 603 decreases toward the Although the surface is unclear, the single crystal silicon substrate 601 and the buried insulating layer are The interface with 603 becomes clear (FIGS. 16(B) and (C)).

[0110] The thickness of the buried insulating layer 603 is set to 10 to 500 nm (typically 20 to 50 nm). In this embodiment, the interface between the single crystal silicon substrate 601 and the buried insulating layer 603 is stable. Since the material is bonded directly to the substrate, a thin buried insulating layer of 20 to 50 nm can be formed. Cut.

[0111] When the buried insulating layer 603 is formed in this manner, the buried insulating layer 603 is partially A portion of the single crystal silicon substrate remains, forming a single crystal silicon layer 604. The thickness of the crystalline silicon layer 604 is 10 to 200 nm (preferably 10 to 50 nm, more preferably The depth at which the oxygen-containing layer 602 is formed is adjusted so that the thickness is approximately 10 nm to 30 nm. good.

[0112] Next, a resist is selectively formed on the single crystal silicon layer 604, and the single crystal silicon layer 60 4 is selectively etched to form island-shaped single layers which will become the active layers of the TFTs to be formed later. A crystalline silicon layer 605 is formed. In this embodiment, a single island of single crystalline silicon is formed. Although only a single layer is shown, multiple layers may be formed on the same substrate. (FIG. 16(D) )

[0113] The subsequent steps are performed in the same manner as in the first to fourth embodiments to manufacture the semiconductor device according to the present invention. It can be manufactured.

[0114] In the semiconductor device according to the present embodiment, it is not necessary to stop etching at the surface of the semiconductor film. This makes it easy to control the etching process for forming the contact holes. The side of the contact hole formed in the layer is electrically connected to the source electrode or the drain electrode. Since the connection can be made, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured. In addition, the semiconductor device according to the present embodiment uses a single crystal semiconductor layer as an active layer. Therefore, the characteristics can be further improved.

[0115] (Embodiment 6) In this embodiment mode, an oxide film made of silicon oxide is formed on a single crystal silicon substrate. A semiconductor device using a single crystal semiconductor thin film formed on a substrate as an active layer will be described. In the embodiment, a semiconductor device using an SOI substrate formed by using the Smart-Cut method is The location will be explained.

[0116] First, a single crystal silicon substrate 801 is prepared as a material for forming the single crystal silicon layer. The following describes the case where a P-type single crystal silicon substrate is used, but the N-type single crystal silicon substrate is also used. Of course, a single crystal silicon germanium substrate can also be used.

[0117] Next, a thermal oxidation process is performed to form a silicon oxide film 802 on the main surface (corresponding to the element formation surface). The thickness of the film can be determined by the practitioner, but is generally in the range of 10 to 500 nm (typically 20 This silicon oxide film 802 will later be used as a buried insulating film for the SOI substrate. It functions as a part of the layer (Figure 17(A)).

[0118] Next, hydrogen ions are introduced from the main surface side of the single crystal silicon substrate 801 through the silicon oxide film 802. The hydrogen-containing layer 803 is formed by adding hydrogen (FIG. 17(B)). Depth to be formed (distance between the main surface of the single crystal silicon substrate 801 and the hydrogen-containing layer 803) is the thickness of the single crystal silicon layer that will later function as the active layer of the TFT. A single crystal silicon layer of 50 nm thickness is placed between the main surface of the silicon substrate 801 and the hydrogen-containing layer 803. The hydrogen ions are implanted at 1×1016 to 1×1 The doping can be performed at a dose of 017 atoms / cm2.

[0119] Next, the single crystal silicon substrate 801 and a supporting substrate are bonded together. A single crystal silicon substrate 804 is used as the plate, and a silicon oxide film for bonding is applied to the surface of the substrate. 805 is provided (FIG. 17(C)). Note that instead of the single crystal silicon substrate 804, A silicon substrate formed by the Z method, a polycrystalline silicon substrate, etc. may also be used. A quartz substrate Alternatively, a highly heat-resistant substrate such as a ceramic substrate or a crystallized glass substrate may be used.

[0120] At this time, the bonding interface is made up of highly hydrophilic silicon oxide films, so The adhesion occurs through a reaction with moisture.

[0121] Next, a heat treatment (first heat treatment) is performed at 400 to 600°C (for example, 500°C). As a result, a volume change occurs in the hydrogen-containing layer 803, and the hydrogen-containing layer 803 is broken along the hydrogen-containing layer 803. As a result, the single crystal silicon substrate 801 is divided, and the oxide is left on the support substrate. The etched silicon film 802 and the single crystal silicon layer 806 are left behind (FIG. 17(D)).

[0122] Next, in the second heat treatment step, the refractory metal is heated at a temperature in the range of 1050 to 1150°C (for example, 1100°C). A furnace annealing process is performed. In this process, Si-O-Si bonds are formed at the bonding interface. In other words, the single crystal silicon layer 806 is bonded to the substrate 802 by the bonding process. This is the process to completely bond the substrate to the support substrate. This stabilizes the bonding interface. Thus, a buried insulating layer 807 is formed (FIG. 17(E)). A hydrogen-containing layer 803 is formed, and a fracture surface is generated along the hydrogen-containing layer 803 to form a thin single crystal. Although a silicon layer 806 is formed, the present invention is not limited to this. The single crystal silicon substrate 801 is polished to form a thin single crystal silicon layer 806 may be formed.

[0123] Next, a process for planarizing the surface of the single crystal silicon layer 806 may be performed. Chemical mechanical polishing (CMP) and high temperature (90 0 to 1200°C) may be performed.

[0124] The final thickness of the single crystal silicon layer 806 is 10 to 200 nm (preferably 10 to 50 nm). , and more preferably 10 nm to 30 nm).

[0125] Next, a resist is selectively formed on the single crystal silicon layer 806, and the single crystal silicon layer 80 6 is selectively etched to form island-shaped single layers which will become the active layers of the TFTs to be formed later. A crystalline silicon layer 808 is formed. In this embodiment, an island-shaped single crystalline silicon Although only one layer is described, multiple island-shaped single crystal silicon layers are formed on the same substrate. (Fig. 17(F))

[0126] The subsequent steps are performed in the same manner as in the first to fourth embodiments to manufacture the semiconductor device according to the present invention. It can be manufactured.

[0127] In the semiconductor device according to the present embodiment, it is not necessary to stop etching at the surface of the semiconductor film. This makes it easy to control the etching process for forming the contact holes. The side of the contact hole formed in the layer is electrically connected to the source electrode or the drain electrode. Since the connection can be made, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured. In addition, the semiconductor device according to the present embodiment uses a single crystal semiconductor layer as an active layer. Therefore, the characteristics can be further improved.

[0128] (Embodiment 7) In this embodiment, the semiconductor device and the electroluminescence element described in the first embodiment are (hereinafter, also referred to as "EL element"), A semiconductor device that can be used in this embodiment mode will be described. The semiconductor device is not limited to that shown in the first embodiment, and may be any of the semiconductor devices described in the second to sixth embodiments.

[0129] In this embodiment, light from the electroluminescence element is taken from the first electrode 110 side. In order to form a structure in which the first electrode 110 is exposed, a film having light transmitting properties is used to form the first electrode 110. In this embodiment, indium tin oxide containing silicon oxide (ITSO) is used as the first electrode 110. Use.

[0130] First, as shown in FIG. 18, TFTs 1701 to 1703 and TFT An insulating layer 1710 that covers the TFTs 1701 to 1703 and the source regions or Next, wiring 1704 to 1709 are formed to electrically connect to the drain region. An insulating layer 109 is formed so as to cover 1709 to 1709, and wiring 1709 and a Next, the end of the first electrode 110 and the insulating layer are electrically connected to each other. An insulating film 111 (also called a bank, a partition wall, a barrier, a bank, etc.) is formed to cover the insulating film 109. Complete.

[0131] The insulating film 111 may be formed of silicon oxide, silicon nitride, silicon oxynitride, aluminum oxide, aluminum nitride, or the like. Aluminum, aluminum oxynitride and other inorganic insulating materials, or acrylic acid, methacrylic acid Acids and their derivatives, or polyimides, aromatic polyamides, poly Heat-resistant polymers such as polybenzimidazole, Among compounds consisting of silicon, oxygen, and hydrogen, inorganic siloxanes containing Si-O-Si bonds, silicon Organosiloxanes in which the hydrogen bonded to the atom is replaced with an organic group such as methyl or phenyl. Insulating materials such as acrylic and polyimide can be used. In this embodiment, a photosensitive polyimide is used to form a flat region. The insulating film 111 is formed to a thickness of 1.5 μm.

[0132] In addition, the insulating film 111 preferably has a shape in which the radius of curvature changes continuously. The covering property of the electroluminescent layer 112 (layer containing an organic compound) and the second electrode 113 is improved. It is possible to do so.

[0133] In order to further improve reliability, the first electrode 112 is formed before the electroluminescent layer 112 is formed. The insulating film 10 and the insulating film 111 are subjected to a nitriding process or an oxidizing process using a high density plasma device. The first electrode 110 may be nitrided or oxidized using a high-density plasma device. This reduces plasma damage during surface modification, resulting in a surface with fewer defects. Therefore, the display by the light emitting element of this embodiment mode is high definition and has little display unevenness. When the film 111 is nitrided, the surface of the insulating film 111 is modified, and the absorption of moisture into the insulating film is prevented. In addition, when the insulating film 111 is oxidized, the film becomes stronger, and the amount of the organic gas can be reduced. In this embodiment, the high density plasma device is used to suppress the emission of plasma. It is possible to perform processing with less Zuma damage. Whether to perform the oxidation treatment or the nitridation treatment can be appropriately selected in consideration of the material and effect of the insulating film. good.

[0134] Next, an electroluminescent layer 112 is formed on the first electrode 110. Note that in FIG. Although not shown in the figure, in this embodiment, the electric currents corresponding to the colors red (R), green (G), and blue (B) are In this embodiment, the electroluminescent layer 112 is made of red (R), green ( G) and blue (B) luminescent materials were selected by deposition using a deposition mask. The red (R), green (G), and blue (B) luminescent materials are formed by deposition masks. The method of selectively forming the layers by the deposition method used in the present invention and the method of forming the layers by the droplet discharge method are also used. The droplet ejection method allows for RGB color separation without using a mask. In this embodiment, materials that emit red (R), green (G), and blue (B) light are used. Each is formed by a vapor deposition method.

[0135] Before the deposition of EL, the main component was an inert gas, with an oxygen concentration of 5% or less and a water concentration of It is preferable to perform the heat treatment in an atmosphere with a temperature of 1% or less to remove moisture. In the form, heat treatment is performed at 300°C for 1 hour.

[0136] Next, a second electrode 113 made of a conductive film is formed on the electroluminescent layer 112. 113, materials with low work functions (Al, Ag, Li, Ca, or alloys of these) MgAg, MgIn, AlLi, CaF2, or calcium nitride) can be used. In this way, a light emitting element consisting of the first electrode 110, the electroluminescent layer 112 and the second electrode 113 is formed. It is done.

[0137] In the display device shown in FIG. 18, light emitted from a light emitting element is transmitted between a substrate 101 and a first electrode 11. 0 and is emitted in the direction of the arrow from the first electrode 110 side.

[0138] It is also effective to provide a passivation film so as to cover the second electrode 113. Passivation films include silicon nitride, silicon oxide, silicon oxynitride (SiON), and nitride. Silicon oxide (SiNO), aluminum nitride (AlN), aluminum oxynitride (AlON) ), aluminum oxide nitride (AlNO) or aluminum oxide, which has a nitrogen content higher than the oxygen content. Insulation materials including aluminum, diamond-like carbon (DLC), and nitrogen-containing carbon (CN) films The insulating film may be a single layer or a laminated layer of a combination of insulating films. Siloxane, whose skeletal structure is formed by bonds between silicon (Si) and oxygen (O), may also be used. Siloxanes are substituted with organic groups that contain at least hydrogen (e.g., alkyl groups, aromatic In addition, the substituents include fluoro groups or groups containing at least hydrogen. An organic group and a fluoro group may also be used.

[0139] In this case, it is preferable to use a film with good coverage as the passivation film. In particular, the use of DLC films is effective. DLC films can be used in the temperature range from room temperature to 100°C or less. Since the film can be formed easily, it can be easily formed above the electroluminescent layer 112, which has low heat resistance. In addition, the DLC film has a high blocking effect against oxygen, and the oxygen of the electroluminescent layer 112 can be prevented. Therefore, the electroluminescent layer can be prevented from being oxidized during the subsequent sealing step. This can prevent problems such as oxidation of 112.

[0140] Next, the substrate 101 on which the light emitting element is formed is fixed to a sealing substrate by a sealant, and the light emitting element is The element is sealed. The sealant prevents moisture from entering through the cut surface, so the light emitting element This prevents deterioration and improves the reliability of the display device. The container may be filled with a material, or nitrogen or the like may be enclosed by sealing under a nitrogen atmosphere. The filler may also be dropped in a liquid state to fill the inside of the display device. Since it is a bottom injection type, it is not necessary to use a filler with translucency. In the case of a structure in which light is extracted through the insulating layer, the filler needs to be made of a light-transmitting material. An example of a filler is a visible light cured, UV cured, or heat cured epoxy resin. Through the above steps, a display device having a light emitting element is completed.

[0141] In addition, it is preferable to place a desiccant inside the EL display panel to prevent deterioration of the element due to moisture. In this embodiment, a drying agent is applied to a recess formed in a sealing substrate so as to surround a pixel region. The dry adhesive is applied to the area corresponding to the gate wiring layer so as not to hinder the thinning. By installing the agent, the water absorption area can be made larger, and the water absorption effect is high. Since the desiccant is formed on the gate wiring layer, the light extraction efficiency is not reduced. None.

[0142] The process of sealing the light-emitting element is a process for protecting the light-emitting element from moisture. Methods of mechanically sealing with bar material, sealing with thermosetting resin or ultraviolet light curing resin, The method of sealing with a thin film with high barrier properties such as metal oxides or nitrides is used. The substrate or cover material is glass, ceramics, plastic or metal. However, if light is to be emitted toward the cover material, it must be translucent. The cover material and the substrate on which the light emitting element is formed are made of a thermosetting resin, an ultraviolet light curing resin, or the like. The plates are attached using a sealant, and the resin is hardened by heat treatment or ultraviolet light irradiation. A sealed space is formed. A moisture absorbent material such as barium oxide is placed in this sealed space. This moisture absorbing material may be provided on the sealing material, or may be provided on the light absorbing material from the light emitting element. The light emitting element may be provided on or around the partition wall so as not to interfere with the light emitting element. It is also possible to fill the space between the substrate and the substrate with a thermosetting resin or an ultraviolet light curing resin. In this case, a material such as barium oxide is added to the thermosetting resin or ultraviolet light curing resin. It is effective to add a moisture absorbent to prevent this.

[0143] The TFTs 1701 to 1703 shown in this embodiment are manufactured by any one of the methods of the first to sixth embodiments. Since there is no need to stop etching at the surface of the semiconductor film, the contact hole The etching process during the formation of the contacts can be easily controlled. The side of the tact hole can be electrically connected to the source electrode or drain electrode. Therefore, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured. An EL display device with good characteristics can be easily manufactured.

[0144] (Embodiment 8) In this embodiment mode, a transmission type liquid crystal display device is manufactured using the semiconductor device manufactured in the embodiment mode 1. A method for manufacturing the semiconductor device will be described. You can also be there.

[0145] First, as in the first embodiment, the TFTs 1701 to 1703 are The insulating layer 1710 covers the source region or drain region of the TFTs 1701 to 1703. Next, wirings 1704 to 1709 are formed to connect the wirings 1704 to 1709 to each other (FIG. 19). An insulating layer 109 is formed so as to cover the insulating layer 109, and the insulating layer 109 is electrically connected to the wiring 1709. In this embodiment, the first electrode 110 is formed from the following material: Indium tin oxide containing silicon oxide (ITSO) is used. Next, as shown in FIG. An alignment film 1801 is formed over the insulating layer 109 and the first electrode 110. In this embodiment, Polyimide is used for the alignment film 1801. Next, the opposing substrate 1802 is prepared. 02 is a glass substrate 1803, a counter electrode 1804 made of a transparent conductive film, an alignment film 1805, and It is composed of:

[0146] Next, the TFT substrate 1806 obtained in the above process and the opposing substrate 1802 are bonded together via a sealant. Here, in order to keep the distance between the two substrates constant, the alignment film 1801 and the alignment film 18 A spacer may be provided between the substrates 1805. Then, liquid crystal 1807 is injected between the two substrates and sealed. The transmissive liquid crystal display device shown in FIG. 19 is completed by sealing with a sealing material.

[0147] In the present embodiment, a transmissive liquid crystal display device has been described. The display device is not limited to this. A reflective electrode may be used as the first electrode 110. By providing a reflective film on the upper or lower surface of the first electrode 110, the liquid crystal display device can be used as a reflective liquid crystal display device. In addition, the present invention may be used in a semi-transmissive liquid crystal display device.

[0148] The TFTs 1701 to 1703 shown in this embodiment are manufactured by any one of the methods of the first to sixth embodiments. Since there is no need to stop etching at the surface of the semiconductor film, the contact hole The etching process during the formation of the contacts can be easily controlled. The side of the tact hole can be electrically connected to the source electrode or drain electrode. Therefore, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured. A liquid crystal display device with good characteristics can be easily manufactured.

[0149] (Embodiment 9) In this embodiment, the thin film transistor, the memory element, and the amplifier described in the first to sixth embodiments are A method for manufacturing a semiconductor device including a tena according to the present invention will be described with reference to the drawings.

[0150] The semiconductor device shown in this embodiment mode is shown in FIG. FIG. 20(B) shows a cross-sectional structure of a semiconductor device according to an embodiment of the present invention. It shows.

[0151] In this embodiment, a semiconductor device 1200 includes an integrated circuit portion 1201, a memory portion 1202, The antenna 1203 is shown in FIG. 20(A). In FIG. 20(B), 204 corresponds to a part of the cross-sectional structure of the integrated circuit portion 1201 in FIG. 20(A), and region 1205 corresponds to The region 1206 corresponds to a part of the cross-sectional structure of the memory section 1202 in FIG. ) corresponds to a part of the cross-sectional structure of antenna 1203.

[0152] In the semiconductor device of this embodiment, as shown in FIG. 20(B), an insulating layer 775 is formed on a first substrate 775. 03 and thin film transistors (TFTs) 744 to 748 provided through the thin film transistor An insulating film 750 is provided on the substrates 744 to 748, and a source is provided on the insulating film 750. The insulating film 752 to 761 function as a source electrode or a drain electrode. An insulating film 762 is provided on the conductive films 750 and 752 to 761. The conductive films 763 to 765 are formed by applying a conductive film 766 to the insulating film 762 and a part of the conductive films 763 to 764. The insulating film 766 is provided as shown in FIG. a conductive layer 786 functioning as an antenna provided over the conductive film 765; and an insulating film 766 An insulating film provided to cover the conductive film 771 and the conductive layer 786 functioning as an antenna The first substrate 772 and the second substrate 776 are provided on the insulating film 772. The substrate 775 and the second substrate 776 form an integrated circuit portion 1201 and a memory portion of the semiconductor device. 1202 and antenna 1203 are sealed.

[0153] The thin film transistors 744 to 748 shown in this embodiment are the same as those in any one of the first to sixth embodiments. Since there is no need to stop etching at the surface of the semiconductor film, The etching process for forming the holes can be easily controlled. The side of the contact hole is electrically connected to the source electrode or the drain electrode. Therefore, a semiconductor device in which deterioration of characteristics is suppressed can be easily manufactured. Thus, a semiconductor device capable of wireless communication and having good characteristics can be easily manufactured. [Explanation of symbols]

[0154] 30 Substrate 31 Insulating layer 32 Semiconductor layer 33 Gate insulating layer 34 Conductive layer 36 Insulating layer 203 Insulating layer 204 Conductive layer 205 Thin-film transistor 32a Channel formation region 32b Impurity region 32c impurity region

Claims

[Claim 1] a semiconductor layer formed on an insulating surface; a first insulating layer formed on the semiconductor layer; a gate electrode formed on the first insulating layer; a second insulating layer formed on the gate electrode; A semiconductor device comprising: a conductive layer formed on the second insulating layer through an opening that is formed in at least the semiconductor layer and the second insulating layer and reaches the insulating surface.

Citation Information

Patent Citations

  • Thin-film transistor and manufacture thereof

    JP1990220475A

  • Thin film transistor and its manufacture

    JP1998150198A

  • Active matrix type display device

    JP2000321603A

  • Liquid crystal display device and method of manufacturing liquid crystal display device

    JP2001264813A

  • Semiconductor device and its manufacturing method

    JP2007013091A