Semiconductor device, semiconductor module, and manufacturing method of semiconductor module
The semiconductor module employs a multi-layer sealing structure with varying elastic moduli to address bonding wire peeling and moisture ingress, ensuring reliability and stability under thermal stress.
Patent Information
- Application Number
- JP2023071123
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-24
- Publication Date
- 2024-11-06
AI Technical Summary
Semiconductor modules face issues with moisture resistance and reliability at the bonding portion between the bonding wire and the surface electrode due to thermal expansion and contraction, leading to peeling and connection failures.
A semiconductor module design that includes multiple sealing members with varying elastic moduli to reinforce the joint between the surface electrode and bonding wire, using a first sealing member with a higher elastic modulus than the second and third sealing members, and ensuring sufficient moisture resistance with dielectric breakdown strength, along with a protective coating for the surface electrode.
The design enhances the reliability and moisture resistance of the bonding portion by reducing thermal stress and preventing peeling, maintaining the integrity of the semiconductor module under repeated thermal cycles.
Smart Images

Figure 2024156552000001_ABST
Abstract
Description
[Technical field]
[0001] FIELD Embodiments of the present invention relate to a semiconductor device, a semiconductor module, and a method for manufacturing a semiconductor module. [Background technology]
[0002] A semiconductor module usually comprises a substrate having a conductor pattern, a semiconductor element mounted on the substrate, having a back electrode on one side (back side) that is joined to the conductor pattern, and a surface electrode on the other side (front side), and a bonding wire that electrically connects the surface electrode to the conductor pattern, etc. The semiconductor element is sealed with a sealing material such as a moisture-resistant thermosetting resin in order to provide stable performance in a high-temperature and high-humidity environment. However, when a current is repeatedly applied to the semiconductor element, the sealing material repeatedly expands and contracts due to heat generation from the semiconductor element, which causes problems such as the sealing material peeling off from the surface electrode and the connection between the bonding wire and the electrode, etc. being destroyed, resulting in poor connection.
[0003] Therefore, there is a demand for a semiconductor module that ensures sufficient moisture resistance of the semiconductor element while providing highly reliable junctions between the semiconductor element and the bonding wires, or between the bonding wires and the conductor pattern. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2018-182330 A Summary of the Invention [Problem to be solved by the invention]
[0005] An object of the present invention is to provide a semiconductor module having a semiconductor device with high moisture resistance and high reliability of the joint between the bonding wire provided on the semiconductor element and the surface electrode. [Means for solving the problem]
[0006] The present invention provides a semiconductor device including a semiconductor element, a surface electrode provided on the semiconductor element, and a bonding wire connected to the surface electrode, the semiconductor device comprising: a first sealing member provided to cover a joint between the surface electrode and the bonding wire; a second sealing member provided to cover a portion of the surface electrode that is not sealed by the first sealing member; and a third sealing member provided to cover the first sealing member and the second sealing member. [Brief description of the drawings]
[0007] [Figure 1] 1 is a cross-sectional view of a semiconductor module according to a first embodiment. [Diagram 2] 1 is a manufacturing method of a semiconductor module according to a first embodiment. [Diagram 3] 4 is a schematic cross-sectional view of the semiconductor module at step S3 of the semiconductor module manufacturing method according to the first embodiment. [Figure 4] 4 is a schematic cross-sectional view of the semiconductor module at step S4 of the semiconductor module manufacturing method according to the first embodiment. FIG. [Diagram 5] 1 is a cross-sectional view of a general semiconductor module according to a first embodiment. [Figure 6] 4A and 4B are diagrams showing a comparison between the accumulated inelastic strain acting on the bonding wire bonded portion and the normal stress acting on the second sealing member 5 according to the first embodiment. [Figure 7] FIG. 11 is a cross-sectional view of a semiconductor module according to a second embodiment. [Figure 8] 11 is a manufacturing method of a semiconductor module according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] Hereinafter, a semiconductor module and a method for manufacturing the semiconductor module according to an embodiment will be described with reference to the drawings. In this specification, when the arrangement and configuration of each part are described using a front side and a back side, the side opposite to the front side is referred to as the back side.
[0009] A semiconductor module and a method for manufacturing the semiconductor module according to the first embodiment will be described with reference to FIGS. 1 to 5. First, the structure of the semiconductor module according to the first embodiment will be described. FIG. 1 shows a cross-sectional view of the semiconductor module according to the first embodiment. As shown in FIG. 1, the semiconductor device 100 includes an insulating substrate 1, a semiconductor element 2 having a front electrode 2a and a back electrode (not shown) provided on the insulating substrate 1, a bonding wire 3 connected to the front electrode 2a provided on the semiconductor element 2, a first sealing member 4 provided so as to cover a joint between the front electrode 2a and the bonding wire 3, and a second sealing member 5 provided around the first sealing member 4 so as to contact the first sealing member 4. The semiconductor module 101 also includes a base plate 7 on which the semiconductor device 100 is mounted and which dissipates heat from the semiconductor element 2, and a case 8 provided on the outer periphery of the base plate 7 and surrounding the periphery so that the entire semiconductor device 100 mounted on the base plate 7 can be sealed with a third sealing member 6.
[0010] The insulating substrate 1 has an insulating layer 11 and a conductor pattern 12, which are laminated together. A plurality of conductor patterns 12 are provided on the insulating layer 11, and the conductor patterns 12 are electrically insulated from each other by spaces or by the insulating layer 11. For example, silicon nitride (SiN), alumina (Al2O3), or aluminum nitride (AlN) can be used as the insulating layer 11. The insulating layer 11 has a front surface 11a and a back surface 11b. The conductor patterns 12 are provided on the front surface 11a and the back surface 11b of the insulating layer 11, respectively. For example, copper (Cu) or aluminum (Al) can be used as the conductor pattern 12.
[0011] The semiconductor element 2 has a surface electrode 2a on the surface opposite to the insulating substrate 1. The semiconductor element 2 may be made of, for example, silicon, silicon carbide, or gallium nitride.
[0012] The surface electrode 2a may be made of, for example, an alloy of aluminum (Al) containing Si, copper (Cu), etc. The surface electrode 2a is electrically connected to an active region of the semiconductor element 2. The surface electrode 2a can be connected to a bonding wire 3 as described later. The surface electrode 2a may have a coating layer. For example, the coating layer is plating. By covering the surface electrode 2a with the coating layer, the surface electrode 2a can be protected from oxidation. Furthermore, the coating layer cushions the impact on the semiconductor element 2 when the bonding wire 3 is bonded. The coating layer may be, for example, a layer made of nickel (Ni), a layer made of gold (Au), an alloy layer, or a layer structure in which these are laminated. The back side of the semiconductor element 2, which is the surface opposite to the surface on which the surface electrode 2a is provided, is bonded to the conductor pattern 12 on the surface 11a side of the insulating substrate 1 via a first bonding member 9. For example, solder, a paste containing sintered silver particles, or the like can be used as the first bonding member 9.
[0013] The semiconductor element 2 has, for example, a vertical structure in which a current flows from the front electrode 2a side to the back side of the semiconductor element 2. Specifically, the semiconductor element 2 can be a switching element such as an IGBT (Insulated Gate Bipolar Transistor) or a vertical MOSFET (Metal Oxide Semiconductor Field Effect Transistor), or a rectifying element such as a Schottky barrier diode. For example, silicon (Si), silicon carbide (SiC), or gallium nitride (GaN) can be used as the semiconductor element 2.
[0014] The bonding wire 3 is joined to the surface electrode 2a at a joint 31. The joint 31 refers to the portion where the bonding wire 3 and the surface electrode 2a contact each other. A current flows to the surface electrode 2a via the bonding wire 3. The bonding wire 3 can be made of aluminum or copper.
[0015] The first sealing member 4 covers the periphery of the bonding portion 31 provided on the surface electrode 2a. The first sealing member 4 only needs to be in contact with the bonding portion 31, and the covering method is not important. The vertical thickness of the first sealing member 4 may be either thicker or thinner than the diameter of the bonding wire 3. The thicker the vertical thickness of the first sealing member 4, the greater the effect of the thermal stress exerted by the bonding wire 3 on the first sealing member 4, and the greater the force exerted on the first sealing member 4. When the thermal stress exerted from the bonding wire 3 to the first sealing member 4 increases, the first sealing member 4 becomes more likely to peel off from the surface electrode 2a. Therefore, for example, the vertical thickness of the first sealing member 4 can be made thinner than the diameter of the bonding wire 3. In general, in a semiconductor module, unnecessary portions between the semiconductor element 2 and the conductor pattern 12 are sealed with an insulating material so that they are not electrically conductive. However, since the second sealing member 5 described later covers the outer periphery of the first sealing member 4, even if the first sealing member 4 is conductive, no current flows except to the semiconductor element 2. Therefore, the first sealing member 4 does not necessarily have to be an insulating material, and a conductive material can also be used. For example, insulating materials such as polyimide resin, resin containing polyimide and silicone gel, epoxy resin, and phenol resin, and resin containing a conductive material filler can be used for the first sealing member 4. For example, metal or ceramics can be used for the filler. By adding a filler, it is possible to improve thermal conductivity and electrical conductivity. On the other hand, the physical properties of the first sealing member 4, such as hardness and linear expansion coefficient, can be easily changed compared to when the first sealing member 4 does not contain a filler. It is preferable that the first sealing member 4 has a glass transition temperature higher than the maximum operating temperature of the semiconductor module 101. When, for example, silicon carbide (SiC) or gallium nitride (GaN) is used as the semiconductor element 2, it can operate at a higher temperature than when silicon or the like is used, and therefore the temperature applied to the junction 31 is also higher. Therefore, when SiC or GaN is used as the semiconductor element 2, it is preferable that it has a glass transition temperature of, for example, 150 degrees or higher.
[0016] The second sealing member 5 seals the surface of the surface electrode 2a. A part of the second sealing member 5 is in contact with the first sealing member 4. The second sealing member 5 does not have to cover the entire first sealing member 4. However, the second sealing member 5 does not contact the bonding wire 3. As the second sealing member, it is preferable to use a member having insulating properties and moisture resistance, and for example, a resin containing polyimide or silicone gel, an epoxy resin, a polyolefin resin, or a fluorine resin can be used. The second sealing member 5 needs to have a sufficient thickness to ensure the moisture resistance of the surface electrode 2a. For example, the thickness of the second sealing member 5 can be 50 μm or more. Here, moisture resistance refers to resistance to the intrusion of moisture from the outside in a high humidity environment, and the higher the moisture resistance, the less moisture is likely to intrude from the outside even in a high humidity environment. For example, if the moisture resistance of the second sealing member 5 is low, moisture will intrude into the semiconductor module 101 in a high humidity environment, and the dielectric strength voltage of the second sealing member 5 will decrease. If the withstand voltage of the second sealing member 5 decreases, a leakage current occurs in the semiconductor element 2, leading to breakdown.
[0017] The third sealing member 6 is filled inside the semiconductor module 101 and seals the entire semiconductor element 2. Specifically, the third sealing member 6 is filled inside an area defined by a base plate 7 and a case 8 described later, and the third sealing member 6 seals the insulating substrate 1, the semiconductor element 2, and the bonding wires 3. The third sealing member 6 only needs to cover at least the second sealing member 5 and the first sealing member 4, and the third sealing member 6 does not need to seal all of the insulating substrate 1, the semiconductor element 2, and the bonding wires 3. As the third sealing member 6, an insulating material, for example, silicone gel, can be used.
[0018] Next, the relationship between the elastic modulus and the dielectric breakdown strength of the first sealing member 4, the second sealing member 5, and the third sealing member 6 will be described. Generally, a semiconductor element is repeatedly heated and cooled as electricity is passed through it. Since the thermal expansion coefficient of the bonding wire is different from that of the surface electrode to which the bonding wire is bonded, repeated heating and cooling may cause thermal stress due to the difference in thermal expansion coefficient, and the bonding wire may peel off from the surface electrode. As the bonding wire peels off, the moisture-resistant resin covering the surface electrode and the bonded portion between the surface electrode and the bonding wire also peels off. When the bonding wire peels off from the surface electrode, the reliability of the semiconductor module decreases. In addition, when the moisture-resistant resin peels off, moisture absorbed by the Si gel covering the entire semiconductor element may reach the surface electrode, causing a leak current to flow to the surface electrode, thereby reducing the reliability of the semiconductor module. Even if the bonding wire does not peel off from the surface electrode, the moisture-resistant resin itself may thermally shrink with the heat generated by the semiconductor element, causing the moisture-resistant resin to peel off from the surface electrode.
[0019] Therefore, in this embodiment, in order to reinforce the surface electrode 2a and the bonding portion 31 of the bonding wire 3, a first sealing member 4, a second sealing member 5, and a third sealing member 6 having different elastic moduli are used. The first sealing member 4 is made of a material having a higher elastic modulus than the second sealing member 5 and the third sealing member 6. The elastic modulus of the first sealing member 4 is desirably 1000 MPa or more. The elastic modulus of the second sealing member 5 is lower than that of the first sealing member 4 and higher than that of the third sealing member 6. The elastic modulus of the third sealing member 6 is lower than that of the second sealing member 5. For example, it can be 1 MPa or less. In other words, it is sufficient to use materials with the greatest elastic modulus in the order of the first sealing member 4, the second sealing member 5, and the third sealing member 6.In other words, it is sufficient that the sealing member closest to the joint 31 between the bonding wire 3 and the surface electrode 2a has the greatest elastic modulus and the sealing member sealing a position away from the joint 31 has the smallest elastic modulus; therefore, the number of types of sealing members is not limited to three.
[0020] When the first sealing member 4 has a higher elastic modulus than the second sealing member 5, the first sealing member 4 has a higher resistance to thermal contraction than the second sealing member 5. Therefore, the stress applied to the second sealing member 5 is reduced when the bonding portion 31 is sealed with the first sealing member 4 compared to when the bonding portion 31 is sealed without the first sealing member 4, so that the peeling of the second sealing member 5 can be prevented at the surface electrode 2a. Similarly, when the second sealing member 5 has a higher elastic modulus than the third sealing member 6, the second sealing member 5 has a higher resistance to thermal contraction than the third sealing member 6. Therefore, the third sealing member 6 can prevent peeling due to thermal stress caused by the difference in thermal expansion coefficient on the surface of the second sealing member 5. In other words, by sealing the semiconductor element 2 with three types of sealing members having different elastic moduli, the reliability and moisture resistance of the semiconductor module 101 can be maintained.
[0021] It is desirable that the second sealing member 5 and the third sealing member 6 have a higher dielectric breakdown strength than the first sealing member 4. The dielectric breakdown strength is an index that indicates how much voltage must be applied to an insulator before the insulator breaks down, loses its insulation, and allows current to flow. In order to make it difficult for current to flow outside the semiconductor element 2 and the bonding wires 3, it is desirable that the second sealing member 5 and the third sealing member 6 have a higher dielectric breakdown strength than the first sealing member 4. For example, it is desirable that the second sealing member 5 and the third sealing member 6 have a dielectric breakdown strength of 10 kV (1 mm).
[0022] The base plate 7 has a role of carrying heat generated from the semiconductor element 2 to a heat sink (not shown) and dissipating the heat. The heat carried to the heat sink is dissipated to the outside of the semiconductor module 101 according to the first embodiment via the rear surface of the heat sink. The base plate 7 has a front surface 7a and a rear surface 7b. The base plate 7 can be made of a material with high thermal conductivity. For example, aluminum or copper can be used for the base plate 7. A front surface 7a of the base plate 7 is bonded to a conductive pattern 12 provided on a rear surface 11b side of the insulating substrate 1. The base plate 7 is bonded to the conductive pattern 12 via a second bonding member 10. As the second bonding member 10, for example, solder, sintered silver particles, or the like can be used.
[0023] The case 8 has a side wall 81 and an inner wall 82. The case 8 is joined to the side surface 71 of the base plate 7 at the inner wall 82. For example, polyphenylene sulfide (PPS), polybutylene terephthalate (PBT), or the like can be used for the case 8. The base plate 7 and the case 8 form a housing for the semiconductor module 101.
[0024] Next, a description will be given of a manufacturing method of the semiconductor module 101. Fig. 2 shows a flowchart illustrating the manufacturing method of the semiconductor module 101 according to the first embodiment.
[0025] In step S1, the semiconductor element 2 is bonded to the insulating substrate 1. Specifically, the back surface of the semiconductor element 2 is bonded to the conductor pattern 12 on the front surface 11a of the insulating substrate 1 via a first bonding member 9. Next, the process proceeds to step S2.
[0026] In step S2, the bonding wires 3 are bonded to the surface electrodes 2a of the semiconductor element 2 by ultrasonic bonding or the like. After the bonding wires 3 are bonded to the surface electrodes 2a, the process proceeds to step S3.
[0027] In step S3, a first sealing member 4 is supplied to cover the bonding portion 31, and the bonding portion 31 is sealed with the first sealing member 4. Fig. 3 shows a schematic diagram of a partially enlarged cross section of the semiconductor module 101 in step S3 of the manufacturing method of the semiconductor module 101 according to the first embodiment. As shown in FIG. 3a, for example, a liquid first sealing member 4 is supplied near a joint 31 between a bonding wire 3 and a surface electrode 2a of a semiconductor element 2. Here, the vicinity of the joint 31 includes both the height (diameter) of the wire and the planar direction of the surface electrode 2a. The first sealing member 4 can be dropped from any position as long as it can reach the joint 31 and cover the joint 31 by the force of dropping or surface tension. When the first sealing member 4 is a resin, the first sealing member 4 can be supplied to the joint 31 by dropping a mixture of a base agent and a hardener or a mixture of a base agent and a solvent using air dispense or jet dispense. When the first sealing member 4 contains a solder alloy, molten solder can be supplied to the joint 31 using a soldering iron or the like.
[0028] After the first sealing member 4 is supplied to the joint 31, the supplied first sealing member 4 is hardened. When the first sealing member 4 is a resin, the first sealing member 4 can be hardened, for example, by holding the supplied liquid first sealing member 4 at room temperature or by heating it at a temperature equal to or lower than the melting point of the first joining member 9. When the first sealing member 4 contains a solder alloy, the first sealing member 4 can be hardened by cooling the supplied liquid first sealing member 4. As shown in FIG. 3b, the supplied first sealing member 4 is hardened, so that the joint 31 is sealed with the first sealing member 4. After sealing the joint 31 with the first sealing member 4, the process proceeds to step S4.
[0029] In step S4, the second sealing member 5 is supplied onto the front electrode 2a so as to be in contact with the first sealing member 4, thereby sealing the front and side surfaces of the front electrode 2a.
[0030] FIG. 4 shows a schematic diagram of a partially enlarged cross section of the semiconductor module in step S3 of the manufacturing method of the semiconductor module 101 according to the first embodiment. As shown in FIG. 4a, for example, a liquid second sealing member 5 is supplied to the surface electrode 2a of the semiconductor element 2 so as to contact the first sealing member 4 sealed in step S3. At this time, the application start position of the second sealing member 5 is not limited to the vicinity of the end of the bonding wire 3, and it can be applied from the vertically upward direction of the surface electrode 2a excluding the joint portion 31. If the second resin is applied from the vertically upward direction of the joint portion 31, a portion where the second sealing member 5 and the bonding wire 3 come into contact with each other is generated, and the bonding wire 3 is subjected to thermal stress due to the thermal contraction of the second sealing member 5. In order to prevent this, it is preferable to apply the second sealing member 5 from the vertically upward direction of the surface electrode 2a excluding the joint portion 31. When the second sealing member 5 is a resin, it can be supplied onto the surface electrode 2a by dripping a mixture of a base agent and a hardener or a mixture of a base agent and a solvent using air dispensing or jet dispensing in the same manner as when supplying the first sealing member 4. After the second sealing member 5 is supplied to the front surface electrode 2a, the supplied second sealing member 5 is cured. When the second sealing member 5 is a resin, the second sealing member 5 can be hardened, for example, by holding the supplied liquid second sealing member 5 at room temperature or by heating it at a temperature equal to or lower than the melting point of the first bonding member 9. As shown in Fig. 4b, after the surface electrode 2a is sealed with the second sealing member 5, the process proceeds to step S5.
[0031] In step S5, the insulating substrate 1 and the case 8 are bonded to the base plate 7. The base plate 7 is bonded to the conductor pattern 12 of the insulating substrate 1 via the second bonding member 10. The case 8 is bonded such that the inner wall 82 of the case 8 is in contact with the side surface 71 of the base plate 7. The base plate 7 and the case 8 form the housing of the semiconductor module 101. After the insulating substrate 1 and the case 8 are bonded to the base plate 7, the process proceeds to step S6.
[0032] In step S6, the third sealing member 6 is supplied into the housing of the semiconductor module 101 including the base plate 7 and the case 8. Similar to the second sealing member 5, the liquid third sealing member 6 is supplied into the housing of the semiconductor module 101, and the supplied third sealing member 6 is cured.
[0033] Next, the effect of the semiconductor module according to the first embodiment will be described. As described above, in the joint 31 between the surface electrode 2a and the bonding wire 3, thermal stress occurs repeatedly with current flow due to the difference in thermal expansion coefficient between the semiconductor element 2 on which the surface electrode 2a is provided and the bonding wire 3. FIG. 5 shows a cross-sectional view of a general semiconductor module according to the first embodiment. The joint 31 of the semiconductor module 201 shown in FIG. 5 is sealed with the second sealing member 5. On the other hand, the joint 31 of the semiconductor module 101 shown in FIG. 1 is sealed with the first sealing member 4. This first sealing member 4 has a higher elastic modulus than the second sealing member 5. Therefore, the stress from the bonding wire 3 applied to the joint 31 can be reduced when the joint 31 is sealed with the first sealing member 4 compared to when the joint 31 is sealed with the second sealing member 5. By reducing the stress applied to the joint 31, peeling of the bonding wire 3 bonded to the surface electrode 2a from the surface electrode 2a can be suppressed. In other words, according to the semiconductor module 101 of this embodiment, it is possible to prevent the bonding wires 3 from peeling off from the surface electrodes 2a, and it is possible to provide a semiconductor module with higher reliability.
[0034] In addition, the first sealing member 4, the second sealing member 5, and the third sealing member 6 also undergo repeated thermal expansion and contraction due to the heat generation and dissipation of the semiconductor element 2, generating thermal stress. The larger the vertical thickness of the second sealing member 5, which has moisture resistance, the more difficult it is for moisture entering from the third sealing member 6 to diffuse inside and the more difficult it is for moisture to reach the bonding portion 31. However, the thicker the vertical thickness of the second sealing member 5 is, the greater the effect of the thermal stress that the second sealing member 5 exerts on the bonding wire 3, and the greater the force exerted on the bonding portion 31 of the bonding wire 3. In the semiconductor module according to this embodiment, the first sealing member 4 covers the bonding portion 31, so that the thermal stress exerted on the second sealing member 5 can be alleviated. FIG. 6 shows a comparison of the accumulated inelastic strain exerted on the bonding wire bonding portion according to the first embodiment. Using the finite element method, a comparison was made between the accumulated inelastic strain near the joint 31 of the semiconductor module 101 shown in Fig. 1 and the accumulated inelastic strain near the joint 31 of the semiconductor module 201 shown in Fig. 5. Specifically, a comparison was made between the accumulated inelastic strain (mm / mm) for one cycle of the joint 31 when simulating a power cycle test in which the current was turned on for 2 seconds and off for 8 seconds. At this time, the thickness of the second sealing member 5 of the semiconductor module 101 and the semiconductor module 201 was both set to 100 μm. In addition, the diameter of the bonding wire 3 was set to Φ400 μm in both the semiconductor module 101 and the semiconductor module 201. 5, it can be seen that the semiconductor module 101 in which the joint 31 is sealed with the first sealing member 4 has a smaller cumulative inelastic strain on the joint 31 than the semiconductor module 201 in which the joint 31 is sealed with the second sealing member 5, the cumulative inelastic strain being reduced by about 35%. That is, according to the semiconductor module of the first embodiment, even if the second sealing member 5 is made thicker, peeling of the bonding wire 3 from the front electrode 2a and peeling of the second sealing member 5 from the front electrode 2a caused by inelastic strain can be suppressed. That is, it is possible to provide a semiconductor module in which the joint 31 is reinforced while ensuring the moisture resistance reliability of the semiconductor element 2.
[0035] Furthermore, the thinner the vertical thickness of the first sealing member 4, the smaller the portion of the bonding wire 3 that is subjected to stress due to thermal contraction of the first sealing member 4, making it possible to provide a semiconductor module in which the bonding wire 3 is even less likely to peel off from the surface electrode 2a.
[0036] Second Embodiment Next, a semiconductor module and a manufacturing method for the semiconductor module according to a second embodiment will be described with reference to Fig. 7 and Fig. 8. In this embodiment, the structure of the second sealing member 5 is different from that of the first embodiment. The above-mentioned differences will be specifically described.
[0037] In the semiconductor module according to the first embodiment, the second sealing member 5 is in contact with the surface electrode 2a and the first sealing member 4. However, in the semiconductor module according to the present embodiment, the second sealing member 5 is in contact with other than the surface electrode 2a and the first sealing member 4. FIG. 7 shows a cross-sectional view of the semiconductor module according to the second embodiment. As shown in FIG. 7, the second sealing member 5 according to the second embodiment is in contact with, for example, the insulating substrate 1 and the base plate 7 in addition to the surface electrode 2a of the semiconductor element 2. The second sealing member 5 can wet and spread outside the surface electrode 2a, and therefore has a larger thickness in the vertical direction than when applied only on the surface electrode 2a.
[0038] Fig. 8 shows a flowchart of the method for manufacturing the semiconductor module according to the second embodiment. Steps S7 to S9 can be performed in the same manner as steps S1 to S3 shown in Fig. 2. In step S9, the bonding portion 31 is sealed with the first sealing member 4, and then the process proceeds to step S10.
[0039] In step S10, the second sealing member 5 is supplied, for example, onto the surface electrode 2a so as to cover the surface electrode 2a, and seal it. At this time, since the second sealing member 5 is also supplied outside the surface electrode 2a, the application start position of the second sealing member 5 is not limited to the vertically upward position of the surface electrode 2a excluding the joint portion 31, but can be applied from the vertically upward position outside the surface electrode 2a. After sealing the surface electrode 2a with the second sealing member 5, the process proceeds to step S11.
[0040] Steps S11 and S12 can be performed in the same manner as steps S5 and S6 shown in FIG.
[0041] The thicker the second sealing member 5, the greater the thermal stress applied to the joint 31 and the second sealing member in the vicinity of the joint 31. However, since the first sealing member 4 seals the joint 31, the thermal stress applied to the joint 31 and the second sealing member in the vicinity of the joint 31 can be reduced. Therefore, according to the semiconductor module of this embodiment, the amount of the second sealing member supplied into the semiconductor module can be increased, and the thickness of the second sealing member, which is a moisture-resistant resin, can be increased. In other words, according to the semiconductor module of this embodiment, it is possible to provide a semiconductor module that prevents the intrusion of moisture into the semiconductor element while ensuring the reliability of the joint, and has a semiconductor element with high moisture-resistant reliability.
[0042] Although several embodiments of the present invention have been described, these novel embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]
[0043] 1...Insulating substrate 11...Insulating layer 11a…Surface 11b…Back side 12...Conductor pattern 2. Semiconductor element 2a…Surface electrode 3…Bonding wire 31…Joint part 4...First sealing member 5...Second sealing member 6...Third sealing member 7…Base plate 71...Side 7a…Surface 7b…Back 8. Case 81...Side wall 82…Inner wall 9...First joining member 10...Second joining member 100...Semiconductor device 101...Semiconductor module
Claims
1. A semiconductor device including a semiconductor element, a surface electrode provided on the semiconductor element, and a bonding wire connected to the surface electrode, a first sealing member provided to cover a joint between the surface electrode and the bonding wire; a second sealing member provided to cover a portion of the surface of the front electrode that is not sealed by the first sealing member; a third sealing member provided to cover the first sealing member and the second sealing member; and A semiconductor device comprising:
2. 2. The semiconductor device according to claim 1, wherein the elastic modulus of the sealing members is highest in the first sealing member, followed by the second sealing member and the third sealing member in that order.
3. The semiconductor device according to claim 2 , wherein the second sealing member has a higher moisture resistance than the third sealing member.
4. 4. The semiconductor device according to claim 3, wherein the thickness of the first sealing member in the vertical direction is smaller than a diameter of the bonding wire.
5. 4. The semiconductor device according to claim 3, wherein the second sealing member covers the entire first sealing member, and the third sealing member does not contact the first sealing member but only contacts the second sealing member.
6. A housing and The semiconductor device according to claim 3 , which is provided in the housing; A semiconductor module having the following:
7. A step of joining a bonding wire to a surface electrode provided on a semiconductor element; supplying a first sealing member to a joint between the surface electrode and the bonding wire; providing a second sealing member in contact with a surface of the front electrode and at least a portion of the first sealing member; providing a third sealing member over the second sealing member; A method for manufacturing a semiconductor module comprising the steps of:
Citation Information
Patent Citations
Semiconductor device
JP2018182330A