Secondary battery and manufacturing method of the secondary battery
The secondary battery's laminated structure with specific density and thickness ratios in the positive electrode sheet addresses uneven salt concentration issues, ensuring even electrolyte distribution and preventing short circuits.
Patent Information
- Application Number
- JP2023072920
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-27
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing secondary batteries face issues with uneven salt concentration between the positive and negative electrodes due to the presence of an insulating layer, which obstructs electrolyte flow and leads to potential short circuits.
The secondary battery design includes a positive electrode sheet with a laminated structure of high and low-density positive electrode active material layers and insulating layers, along with specific density and thickness ratios to ensure even electrolyte distribution and reduce salt concentration unevenness.
This design enhances electrolyte flow and reduces uneven salt concentration between electrodes, preventing short circuits and maintaining battery performance during rapid charging and discharging.
Smart Images

Figure 2024158068000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a secondary battery and a method for manufacturing a secondary battery. [Background technology]
[0002] Currently, secondary batteries such as lithium ion batteries are used in electric vehicles, hybrid vehicles, plug-in hybrid vehicles, etc. Patent Document 1 discloses an example of such a secondary battery, which aims to improve ion diffusibility near the current collector by providing low-density regions and high-density regions in a predetermined pattern on the surface of the electrode active material layer. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2022-133084 A Summary of the Invention [Problem to be solved by the invention]
[0004] In order to prevent such a short circuit in the secondary battery, an insulating layer may be provided at one end of the positive electrode sheet in the width direction of the secondary battery. However, when such an insulating layer is provided in the secondary battery disclosed in Patent Document 1, the flow of the electrolyte that has permeated the positive electrode sheet is hindered by the insulating layer, and there is a risk of unevenness in the salt concentration occurring between the positive electrode and the negative electrode.
[0005] The present disclosure has been made to solve such problems, and has an object to provide a secondary battery and a method for manufacturing a secondary battery that are capable of reducing unevenness in salt concentration between a positive electrode and a negative electrode. [Means for solving the problem]
[0006] A secondary battery including an electrode assembly formed by stacking a positive electrode sheet, a negative electrode sheet, and a separator according to an embodiment of the present invention includes: The positive electrode sheet includes a positive electrode active material layer and an insulating layer formed on both sides of a positive electrode current collector foil, the positive electrode active material layer is composed of a first positive electrode active material layer located on the positive electrode current collector foil side, and a second positive electrode active material layer located on the separator side and having a lower density than the first positive electrode active material layer; The insulating layer is composed of a first insulating layer located on the positive electrode current collector foil side, and a second insulating layer located on the separator side and having a lower density than the first insulating layer.
[0007] The negative electrode sheet includes a negative electrode active material layer, The average density of the positive electrode active material layer and the insulating layer may be within a range of not less than the average density of the negative electrode active material layer and not more than twice the average density of the negative electrode active material layer.
[0008] Furthermore, the thickness of the first positive electrode active material layer and the thickness of the first insulating layer are the same, The thickness of the first positive electrode active material layer and the thickness of the first insulating layer may be at least two-thirds of the combined thickness of the first positive electrode active material layer and the second positive electrode active material layer.
[0009] Furthermore, the density of the second insulating layer is greater than the density of the second positive electrode active material layer, The difference between the density of the second insulating layer and the density of the second positive electrode active material layer is 1 g / cm 3 It can be the following:
[0010] A method for manufacturing a secondary battery including an electrode assembly formed by stacking a positive electrode sheet, a negative electrode sheet, and a separator according to an embodiment of the present invention includes the steps of: a first positive electrode active material layer forming step of applying a positive electrode active material layer material to both sides of a positive electrode current collector foil to form a first positive electrode active material layer; a first insulating layer forming step of applying an insulating layer material to both sides of the positive electrode current collector foil to form a first insulating layer; a first pressurizing step of pressurizing the first positive electrode active material layer and the first insulating layer at a predetermined first pressure; a second positive electrode active material layer forming step of applying a positive electrode active material layer material to the first positive electrode active material layer to form a second positive electrode active material layer; a second insulating layer forming step of applying an insulating layer material to the first insulating layer to form a second insulating layer; a second pressurizing step of pressurizing the second positive electrode active material layer and the second insulating layer at a second predetermined pressure; The first pressure and the second pressure are pressures that make the density of the second positive electrode active material layer smaller than the density of the first positive electrode active material layer and that make the density of the second insulating layer smaller than the density of the first insulating layer.
[0011] The method for producing a secondary battery includes a negative electrode active material layer forming step of applying a negative electrode active material layer material to both sides of a negative electrode current collector foil to form a negative electrode active material layer; a third pressurizing step of pressurizing the negative electrode active material layer at a predetermined third pressure, The first pressure, the second pressure, and the third pressure may be pressures that make the average density of the positive electrode active material layer and the insulating layer equal to or greater than the average density of the negative electrode active material layer and equal to or less than twice the average density of the negative electrode active material layer.
[0012] Furthermore, in the second positive electrode active material layer forming step and the second insulating layer forming step, the positive electrode active material layer material and the insulating layer material can be applied to the first positive electrode active material layer and the first insulating layer, respectively, so that the thicknesses of the second positive electrode active material layer and the second insulating layer are less than one-third of the combined thickness of the first positive electrode active material layer and the second positive electrode active material layer.
[0013] Furthermore, in the second positive electrode active material layer forming step and the second insulating layer forming step, the density of the second insulating layer after pressing is greater than the density of the second positive electrode active material layer, and the difference between the density of the second insulating layer after pressing and the density of the second positive electrode active material layer is 1 g / cm 3 The positive electrode active material layer material and the insulating layer material may be applied to a first positive electrode active material layer and a first insulating layer, respectively, as follows:
[0014] According to another embodiment, a method for producing a secondary battery including an electrode assembly formed by laminating a positive electrode sheet, a negative electrode sheet, and a separator includes the steps of: a first positive electrode active material layer forming step of applying a first positive electrode active material layer material to both sides of a positive electrode current collector foil to form a first positive electrode active material layer; a first insulating layer forming step of applying a first insulating layer material to both sides of the positive electrode current collector foil to form a first insulating layer; a second positive electrode active material layer forming step of applying a second positive electrode active material layer material having a lower density than the first positive electrode active material layer material to the first positive electrode active material layer to form a second positive electrode active material layer; and a second insulating layer forming step of applying a second insulating layer material having a lower density than the first insulating layer material to the first insulating layer to form a second insulating layer.
[0015] The method for producing a secondary battery further includes a negative electrode active material layer forming step of applying a negative electrode active material layer material to a negative electrode current collector foil to form a negative electrode active material layer, The density of the first positive electrode active material layer material, the density of the second positive electrode active material layer material, the density of the first insulating layer material, the density of the second insulating layer material, and the density of the negative electrode active material layer material may be such that the average density of the positive electrode active material layers and insulating layers is equal to or greater than the average density of the negative electrode active material layers and is equal to or less than twice the average density of the negative electrode active material layers.
[0016] Furthermore, in the second positive electrode active material layer forming step and the second insulating layer forming step, the second positive electrode active material layer material and the second insulating layer material can be applied to the first positive electrode active material layer and the first insulating layer, respectively, so that the thicknesses of the second positive electrode active material layer and the second insulating layer are less than one-third of the combined thickness of the first positive electrode active material layer and the second positive electrode active material layer.
[0017] Furthermore, the density of the second positive electrode active material layer material and the density of the second insulating layer material are such that the density of the second insulating layer after compression is greater than the density of the second positive electrode active material layer, and the difference between the density of the second insulating layer after compression and the density of the second positive electrode active material layer is 1 g / cm 3 The density may be: Effect of the Invention
[0018] According to the present disclosure, it is possible to provide a secondary battery capable of reducing unevenness in salt concentration between a positive electrode and a negative electrode, and a method for manufacturing the secondary battery. [Brief description of the drawings]
[0019] [Figure 1] FIG. 1 is a diagram illustrating an example of a secondary battery according to an embodiment. [Diagram 2] FIG. 2 is a diagram showing an example of an electrode body according to an embodiment. [Diagram 3] 3 is a cross-sectional view showing a part of the electrode body taken along the line II in FIG. 2. [Figure 4] 3 is a diagram showing details of a cross section of a positive electrode sheet taken along the line II in FIG. 2. [Diagram 5] FIG. 4 is a diagram showing examples of the densities of a first positive electrode active material layer, a second positive electrode active material layer, a first insulating layer, and a second insulating layer. [Figure 6] 4 is a flowchart showing an electrode assembly manufacturing process included in a manufacturing method for a secondary battery according to one embodiment. [Figure 7] 4 is a flowchart showing details of a step S1 of producing a positive electrode sheet according to one embodiment. [Figure 8] FIG. 2 is a conceptual diagram showing the flow of an electrolyte in a secondary battery according to one embodiment. [Figure 9] 4 is a conceptual diagram showing the flow of an electrolyte in another secondary battery different from the secondary battery according to the embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] <First embodiment> FIG. 1 is a diagram showing an example of a secondary battery 1 according to an embodiment. The secondary battery 1 includes a battery case 2 and an electrode body (not shown) housed in the battery case 2. The battery case 2 is filled with an electrolyte. Specific examples of the electrolyte include a non-aqueous electrolyte in which a lithium salt is dissolved in an organic solvent. Lithium salts include LiClO4, LiPF6, LiAsF6, LiBF4, LiSO3CF3, and the like. The width direction shown in the figure refers to the width direction of the secondary battery 1 and the electrode body. Also, the thickness direction refers to the thickness direction of the secondary battery 1 and the electrode body.
[0021] 2 is a diagram showing an example of an electrode assembly 3 according to one embodiment. The electrode assembly 3 is formed by stacking and winding a positive electrode sheet, a negative electrode sheet, and a separator that insulates the positive electrode sheet and the negative electrode sheet. The secondary battery 1 may also include a non-wound electrode assembly.
[0022] Fig. 3 is a cross-sectional view showing a part of the electrode assembly 3 taken along the II cross-sectional line in Fig. 2. The electrode assembly 3 is formed by laminating a positive electrode sheet 10, a negative electrode sheet 20, and a separator 30 that insulates the positive electrode sheet 10 and the negative electrode sheet 20.
[0023] Fig. 4 is a diagram showing details of a cross section of the positive electrode sheet 10 taken along the II cross section line in Fig. 2. The positive electrode sheet 10 includes a positive electrode current collector foil 13, a positive electrode active material layer 11, and an insulating layer 12. The positive electrode current collector foil 13 is a metal foil such as aluminum foil. The positive electrode active material layer 11 and the insulating layer 12 are formed on both sides of the positive electrode current collector foil 13.
[0024] The positive electrode active material layer 11 is composed of a first positive electrode active material layer 111 and a second positive electrode active material layer 112. The first positive electrode active material layer 111 is located on the side of the positive electrode current collector foil 13. The second positive electrode active material layer 112 is located on the side of the separator 30 (not shown) and faces the separator 30. The density of the second positive electrode active material layer 112 is smaller than the density of the first positive electrode active material layer 111. The first positive electrode active material layer 111 and the second positive electrode active material layer 112 are composed of materials forming a positive electrode active material layer, such as a positive electrode active material, a solvent, and a binder (hereinafter referred to as "positive electrode active material materials"). Specific examples of the positive electrode active material include metal oxides such as cobalt, nickel, and manganese.
[0025] The insulating layer 12 is composed of a first insulating layer 121 and a second insulating layer 122. The first insulating layer 121 is located on the side of the positive electrode current collector foil 13. The second insulating layer 122 is located on the side of the separator 30 and faces the separator 30. The density of the second insulating layer 122 is smaller than the density of the first insulating layer 121. The first insulating layer 121 and the second insulating layer 122 are composed of materials such as an insulator, a solvent, and a binder (hereinafter, referred to as "insulating layer materials"). Specific examples of the insulator include boehmite and alumina. The insulating layer 12 has a function of preventing a short circuit between the positive electrode and the negative electrode and suppressing the intrusion of foreign matter into the positive electrode active material layer 11. The insulating layer 12 corresponds to a heat resistance layer (HRL).
[0026] 4, the thickness of the first positive electrode active material layer 111 is the same as the thickness of the first insulating layer 121. The thickness of the second positive electrode active material layer 112 is the same as the thickness of the second insulating layer 122. The thickness of the first positive electrode active material layer 111 and the thickness of the first insulating layer 121 are preferably at least two-thirds of the total thickness T of the first positive electrode active material layer 111 and the second positive electrode active material layer 112.
[0027] The density of the second insulating layer 122 is greater than the density of the second positive electrode active material layer 112. The difference between the density of the second insulating layer 122 and the density of the second positive electrode active material layer 112 is less than 1 g / cm. 3 It is preferable that:
[0028] Fig. 5 is a diagram showing an example of the densities of the first positive electrode active material layer 111, the second positive electrode active material layer 112, the first insulating layer 121, and the second insulating layer 122. The densities of the first positive electrode active material layer 111, the second positive electrode active material layer 112, the first insulating layer 121, and the second insulating layer 122 can be set to values within the ranges shown in Fig. 5. The densities of the second positive electrode active material layer 112, the first insulating layer 121, and the second insulating layer 122 may be values outside the ranges shown in Fig. 5.
[0029] The average density of the positive electrode active material layer 11 and the insulating layer 12 can be set within a range of not less than the average density of the negative electrode active material layer of the negative electrode sheet 20, and not more than twice the average density of the negative electrode active material layer. More specifically, the ratio of the average density of the positive electrode active material layer 11 and the insulating layer 12 to the average density of the negative electrode active material layer is preferably 2:1. The negative electrode active material layer is composed of materials forming the negative electrode active material layer, such as a negative electrode active material, a solvent, and a binder (hereinafter referred to as "negative electrode active material materials"). Specific examples of the negative electrode active material include carbon materials such as graphite.
[0030] 6 is a flowchart showing the steps of producing an electrode assembly 3, which are included in a method for producing a secondary battery according to one embodiment. The steps of producing the electrode assembly 3 include a step S1 of producing a positive electrode sheet 10, a step S2 of producing a negative electrode sheet 20, and a winding step S3.
[0031] The positive electrode sheet 10 preparation step S1 is a step of preparing the positive electrode sheet 10. Fig. 7 is a flowchart showing details of the positive electrode sheet preparation step S1. The positive electrode sheet 10 preparation step S1 includes a first positive electrode active material layer formation step S10, a first insulating layer formation step S11, a first pressurizing step S12, a second positive electrode active material layer formation step S13, a second insulating layer formation step S14, and a second pressurizing step S15.
[0032] The first positive electrode active material layer forming step S10 is a step of applying a positive electrode active material layer material to both sides of the positive electrode current collector foil 13 to form the first positive electrode active material layer 111. The first insulating layer forming step S11 is a step of applying an insulating layer material to both sides of the positive electrode current collector foil 13 to form the first insulating layer 121.
[0033] The first pressurizing step S12 is a step of pressing the first positive electrode active material layer and the first insulating layer with a predetermined first pressure. In the first pressurizing step S12, the first positive electrode active material layer and the first insulating layer are pressed by a pressing device such as a pair of pressure rollers so that the first positive electrode active material layer 111 and the first insulating layer 121 have the same thickness. The amounts of the positive electrode active material layer material and the insulating layer material are the amounts required for the first positive electrode active material layer 111 and the first insulating layer 121 to have the same thickness when pressed in the first pressurizing step S12.
[0034] The second positive electrode active material layer forming step S13 is a step of applying a positive electrode active material layer material to the first positive electrode active material layer 111 to form the second positive electrode active material layer 112. The second insulating layer forming step S14 is a step of applying an insulating layer material to the first insulating layer to form a second insulating layer.
[0035] In the second positive electrode active material layer forming step S13 and the second insulating layer forming step S14, the positive electrode active material layer material and the insulating layer material are applied to the first positive electrode active material layer 111 and the first insulating layer 121, respectively, so that the thicknesses of the second positive electrode active material layer 112 and the second insulating layer 122 are less than one-third of the thickness T obtained by adding the thicknesses of the first positive electrode active material layer 111 and the second positive electrode active material layer 112. In other words, the positive electrode active material layer material and the insulating layer material are applied to the first positive electrode active material layer 111 and the first insulating layer 121, respectively, so that the thicknesses of the first positive electrode active material layer 111 and the first insulating layer 121 are at least two-thirds of the thickness T obtained by adding the thicknesses of the first positive electrode active material layer 111 and the second positive electrode active material layer 112.
[0036] In the second positive electrode active material layer forming step S13 and the second insulating layer forming step S14, the density of the second insulating layer 122 after pressure application is greater than the density of the second positive electrode active material layer 112 after pressure application, and the difference between the density of the second insulating layer 122 after pressure application and the density of the second positive electrode active material layer 112 after pressure application is less than 1 g / cm 3 The positive electrode active material layer material and the insulating layer material are applied to the first positive electrode active material layer 111 and the first insulating layer 121, respectively, as described below.
[0037] The second pressurizing step S15 is a step of pressurizing the second positive electrode active material layer and the second insulating layer with a second predetermined pressure. In the second pressurizing step S15, the second positive electrode active material layer and the second insulating layer are pressed by a pressurizing device so that the second positive electrode active material layer 112 and the second insulating layer 122 have the same thickness. Note that the thicknesses of the first positive electrode active material layer 111 and the first insulating layer 121 remain the same.
[0038] The manufacturing process S2 of the negative electrode sheet 20 shown in FIG. 6 includes a negative electrode active material layer process in which a negative electrode active material layer material is applied to both sides of a negative electrode current collector foil such as a copper foil to form a negative electrode active material layer, and a third pressure process in which the negative electrode active material material is pressed at a predetermined third pressure using a pressure device. In this embodiment, the first pressure, the second pressure, and the third pressure are pressures that make the average density of the positive electrode active material layer 11 and the insulating layer 12 in a range of not less than the average density of the negative electrode active material layer and not more than twice the average density of the negative electrode active material layer. More specifically, it is preferable to adopt pressures that make the ratio of the average density of the positive electrode active material layer 11 and the insulating layer 12 to the average density of the negative electrode active material layer 2:1 as the first pressure, the second pressure, and the third pressure.
[0039] The winding step S3 is a step of stacking and winding the positive electrode sheet 10, the negative electrode sheet 20, and the separator 30. In another embodiment for producing a non-wound type electrode body, a stacking step of stacking the positive electrode sheet 10, the negative electrode sheet 20, and the separator 30 can be adopted instead of the winding step S3.
[0040] As described above, the positive electrode sheet 10 includes a positive electrode active material layer 11 and an insulating layer 12 formed on both sides of the positive electrode current collector foil 13. The positive electrode active material layer 11 is composed of a first positive electrode active material layer 111 located on the positive electrode current collector foil 13 side, and a second positive electrode active material layer 112 located on the separator 30 side and having a lower density than the first positive electrode active material layer 111. The insulating layer 12 is composed of a first insulating layer 121 located on the positive electrode current collector foil 13 side, and a second insulating layer 122 located on the separator 30 side and having a lower density than the first insulating layer 121.
[0041] FIG. 8 is a conceptual diagram showing the flow of the electrolyte that has permeated the positive electrode sheet 10 and the negative electrode sheet 20. As shown by the white arrows in FIG. 8, the electrolyte that has permeated the positive electrode sheet 10 and the negative electrode sheet 20 moves in the width direction. FIG. 9 is a conceptual diagram showing the flow of the electrolyte in a secondary battery including a positive electrode sheet 10 in which the positive electrode active material layer is composed of a single layer of positive electrode active material layer 111 and the insulating layer is composed of a single layer of insulating layer 121. As shown by the white arrows in FIG. 9, the electrolyte that has permeated the positive electrode sheet 10 moves in the width direction, but the flow of the electrolyte is hindered by the insulating layer 121, which has low electrolyte permeability.
[0042] In the above-described embodiment, the density of the second positive electrode active material layer 112 and the second insulating layer 122 facing the separator 30, that is, the density of the second positive electrode active material layer 112 and the second insulating layer 122 located on the surface layer of the positive electrode sheet 10 in the thickness direction, is smaller than the density of the first positive electrode active material layer 111 and the first insulating layer 121, respectively. Therefore, compared with the secondary battery shown in FIG. 9, in the secondary battery 1 according to the above-described embodiment, the fluidity of the electrolyte in the second positive electrode active material layer 112 and the second insulating layer 122 of the positive electrode sheet 10 is high. In addition, in the secondary battery 1, the flow of the electrolyte that has infiltrated into the second positive electrode active material layer 112 of the positive electrode sheet 10 can be prevented from being hindered by the second insulating layer 122. As a result, in the secondary battery 1, the salt contained in the electrolyte that has infiltrated into the positive electrode sheet 10 moves in the width direction and is easily discharged from the positive electrode sheet 10.
[0043] In conventional secondary batteries such as lithium ion batteries, the electrolyte in the positive electrode sheet is usually less fluid than that in the negative electrode sheet. In other words, since the fluidity of the salt contained in the electrolyte that has permeated the positive electrode sheet is low, unevenness in the salt concentration between the positive electrode and the negative electrode during rapid charging and discharging is likely to occur. On the other hand, in the secondary battery 1, the electrolyte that has permeated the positive electrode sheet 10 moves in the width direction and is likely to flow out of the positive electrode sheet 10. In other words, the salt contained in the electrolyte that has permeated the positive electrode sheet 10 moves in the width direction and is likely to flow out of the positive electrode sheet 10. Therefore, in the secondary battery 1, unevenness in the salt concentration between the positive electrode and the negative electrode during rapid charging and discharging can be reduced.
[0044] As described above, the thickness of the first positive electrode active material layer 111 and the thickness of the first insulating layer 121 are the same. The thickness of the first positive electrode active material layer 111 and the thickness of the first insulating layer 121 are two-thirds or more of the thickness T obtained by adding the thickness of the first positive electrode active material layer 111 and the thickness of the second positive electrode active material layer 112. As a result, the first positive electrode active material layer 111, which is a high-density layer, exists at two-thirds or more of the thickness T obtained by adding the thickness of the first positive electrode active material layer 111 and the thickness of the second positive electrode active material layer 112, so that the decrease in the capacity and input / output of the secondary battery due to the adoption of the second positive electrode active material layer 112, which is a low-density layer, can be reduced. In addition, since the first insulating layer 121, which is a high-density layer, is present at a thickness of more than two-thirds of the combined thickness T of the first positive electrode active material layer 111 and the second positive electrode active material layer 112, it is possible to reduce the deterioration in insulating performance and strength caused by the use of the second insulating layer 122, which is a low-density layer.
[0045] <Second embodiment> The second embodiment will be described below, focusing on the differences from the first embodiment. In the second embodiment, the density of the positive electrode active material layer may be adjusted by adjusting the amount or particle size of the positive electrode active material contained in the positive electrode active material layer. Specifically, the density of the positive electrode active material layer can be increased by increasing the amount of the positive electrode active material. On the other hand, the density of the positive electrode active material layer can be decreased by decreasing the amount of the positive electrode active material.
[0046] The density of the insulating layer may be adjusted by adjusting the amount or particle size of the insulator contained in the insulating layer. Specifically, the density of the insulating layer can be increased by increasing the amount of the insulator. On the other hand, the density of the insulating layer can be decreased by decreasing the amount of the insulator.
[0047] In the first positive electrode active material layer forming step S10, a first positive electrode active material layer material is applied to both sides of the positive electrode current collector foil 13 to form the first positive electrode active material layer 111. The first positive electrode active material layer material has a higher density than the second positive electrode active material layer material that forms the second positive electrode active material layer.
[0048] In the first insulating layer forming step S11, a first insulating layer material is applied to both sides of the positive electrode current collector foil to form the first insulating layer 121. The first insulating layer material has a higher density than the second insulating layer material.
[0049] In the first pressurizing step S12, similarly to the first embodiment, the first positive electrode active material layer 111 and the first insulating layer 121 are pressurized so that they have the same thickness.
[0050] In the second positive electrode active material layer forming step S13, a second positive electrode active material layer material having a lower density than the first positive electrode active material layer material is applied to the first positive electrode active material layer 111 to form the second positive electrode active material layer 112. In the second insulating layer forming step S14, a second insulating layer material having a lower density than the first insulating layer material is applied to the first insulating layer 121 to form the second insulating layer 122. In the second pressurizing step S15 according to the second embodiment, the second positive electrode active material layer 112 and the second insulating layer 122 are pressurized so that the second positive electrode active material layer 112 and the second insulating layer 122 have the same thickness.
[0051] The density of the second positive electrode active material layer material applied in the above step S13 and the density of the second insulating layer material applied in the above step S14 are such that the density of the second insulating layer 122 after compression is greater than the density of the second positive electrode active material layer 112, and the difference between the density of the second insulating layer 122 after compression and the density of the second positive electrode active material layer 112 is less than 1 g / cm 3 Preferably, the density is:
[0052] The manufacturing step S2 of the negative electrode sheet 20 includes a negative electrode active material layer forming step of applying a negative electrode active material layer material to a negative electrode current collector foil to form a negative electrode active material layer. In the second embodiment, the density of the first positive electrode active material layer material applied in the above step S10, the density of the second positive electrode active material layer material applied in the above step S13, the density of the first insulating layer material applied in the above step S11, the density of the second insulating layer material applied in the above step S14, and the density of the negative electrode active material layer material applied in the above step S2 are preferably densities that make the average density of the positive electrode active material layer 11 and the insulating layer 12 within a range of not less than the average density of the negative electrode active material layer and not more than twice the average density of the negative electrode active material layer.
[0053] The present invention is not limited to the above-described embodiment, and can be modified as appropriate without departing from the spirit and scope of the present invention. [Explanation of symbols]
[0054] 1 Secondary battery 2 battery case 3 Electrode body 10 Positive electrode sheet 11 Cathode active material layer 111 First positive electrode active material layer 112 Second positive electrode active material layer 12 Insulating layer 121 First insulating layer 122 Second insulating layer 13 Positive electrode current collector foil 20 Negative electrode sheet 30 Separator
Claims
1. A secondary battery including an electrode assembly formed by laminating a positive electrode sheet, a negative electrode sheet, and a separator, The positive electrode sheet includes a positive electrode active material layer and an insulating layer formed on both sides of a positive electrode current collector foil, the positive electrode active material layer is composed of a first positive electrode active material layer located on the positive electrode current collector foil side, and a second positive electrode active material layer located on the separator side and having a density lower than that of the first positive electrode active material layer, The insulating layer is composed of a first insulating layer located on the positive electrode current collector foil side and a second insulating layer located on the separator side and having a density lower than that of the first insulating layer. Secondary battery.
2. The negative electrode sheet includes a negative electrode active material layer, 2. The secondary battery according to claim 1, wherein the average density of the positive electrode active material layer and the insulating layer is within a range of equal to or higher than the average density of the negative electrode active material layer and equal to or lower than twice the average density of the negative electrode active material layer.
3. the thickness of the first positive electrode active material layer and the thickness of the first insulating layer are the same; 3. The secondary battery according to claim 1, wherein a thickness of the first positive electrode active material layer and a thickness of the first insulating layer are equal to or greater than two-thirds of a combined thickness of the first positive electrode active material layer and the second positive electrode active material layer.
4. the density of the second insulating layer is greater than the density of the second positive electrode active material layer, The difference between the density of the second insulating layer and the density of the second positive electrode active material layer is 1 g / cm 3 The secondary battery according to claim 1 or 2, wherein:
5. A method for manufacturing a secondary battery including an electrode assembly formed by laminating a positive electrode sheet, a negative electrode sheet, and a separator, comprising: a first positive electrode active material layer forming step of applying a positive electrode active material layer material to both sides of a positive electrode current collector foil to form a first positive electrode active material layer; a first insulating layer forming step of applying an insulating layer material to both sides of the positive electrode current collector foil to form a first insulating layer; a first pressurizing step of pressurizing the first positive electrode active material layer and the first insulating layer at a predetermined first pressure; a second positive electrode active material layer forming step of applying the positive electrode active material layer material to the first positive electrode active material layer to form a second positive electrode active material layer; a second insulating layer forming step of applying the insulating layer material to the first insulating layer to form a second insulating layer; a second pressurizing step of pressurizing the second positive electrode active material layer and the second insulating layer at a second predetermined pressure; the first pressure and the second pressure are pressures that make the density of the second positive electrode active material layer smaller than the density of the first positive electrode active material layer and make the density of the second insulating layer smaller than the density of the first insulating layer. A method for manufacturing a secondary battery.
6. a negative electrode active material layer forming step of applying a negative electrode active material layer material to both sides of a negative electrode current collector foil to form a negative electrode active material layer; a third pressurizing step of pressurizing the negative electrode active material layer at a third predetermined pressure, 6. The method for producing a secondary battery according to claim 5, wherein the first pressure, the second pressure, and the third pressure are pressures that make the average density of the positive electrode active material layer and the insulating layer within a range of not less than an average density of the negative electrode active material layer and not more than twice the average density of the negative electrode active material layer.
7. 7. The method for manufacturing a secondary battery according to claim 5, wherein in the second positive electrode active material layer forming step and the second insulating layer forming step, the positive electrode active material layer material and the insulating layer material are applied to the first positive electrode active material layer and the first insulating layer, respectively, so that thicknesses of the second positive electrode active material layer and the second insulating layer are less than one-third of a combined thickness of the first positive electrode active material layer and the second positive electrode active material layer.
8. In the second positive electrode active material layer forming step and the second insulating layer forming step, the density of the second insulating layer after compression is greater than the density of the second positive electrode active material layer after compression, and the difference between the density of the second insulating layer after compression and the density of the second positive electrode active material layer is 1 g / cm 3 7. The method for producing a secondary battery according to claim 5, wherein the positive electrode active material layer material and the insulating layer material are applied to the first positive electrode active material layer and the first insulating layer, respectively, so as to satisfy the following:
9. A method for manufacturing a secondary battery including an electrode assembly formed by laminating a positive electrode sheet, a negative electrode sheet, and a separator, comprising: a first positive electrode active material layer forming step of applying a first positive electrode active material layer material to both sides of a positive electrode current collector foil to form a first positive electrode active material layer; a first insulating layer forming step of applying a first insulating layer material to both sides of the positive electrode current collector foil to form a first insulating layer; a second positive electrode active material layer forming step of applying a second positive electrode active material layer material having a lower density than the first positive electrode active material layer material to the first positive electrode active material layer to form a second positive electrode active material layer; a second insulating layer forming step of applying a second insulating layer material having a lower density than the first insulating layer material to the first insulating layer to form a second insulating layer; Including, A method for manufacturing a secondary battery.
10. a negative electrode active material layer forming step of applying a negative electrode active material layer material to a negative electrode current collector foil to form a negative electrode active material layer; 10. The method for producing a secondary battery according to claim 9, wherein a density of the first positive electrode active material layer material, a density of the second positive electrode active material layer material, a density of the first insulating layer material, a density of the second insulating layer material, and a density of the negative electrode active material layer material are densities that make an average density of the positive electrode active material layer and the insulating layer within a range of not less than an average density of the negative electrode active material layer and not more than twice the average density of the negative electrode active material layer.
11. 11. The method for manufacturing a secondary battery according to claim 9 or 10, wherein in the second positive electrode active material layer forming step and the second insulating layer forming step, the second positive electrode active material layer material and the second insulating layer material are applied to the first positive electrode active material layer and the first insulating layer, respectively, so that thicknesses of the second positive electrode active material layer and the second insulating layer are less than one-third of a combined thickness of the first positive electrode active material layer and the second positive electrode active material layer.
12. The density of the second positive electrode active material layer material and the density of the second insulating layer material are such that the density of the second insulating layer after compression is greater than the density of the second positive electrode active material layer, and the difference between the density of the second insulating layer after compression and the density of the second positive electrode active material layer is 1 g / cm 3 The method for producing a secondary battery according to claim 9 or 10, wherein the density is equal to or less than the above.
Citation Information
Patent Citations